Porcelain wood male and female type composite structure
By combining the edge treatment of porcelain plates and the compound glue of the wooden board, combined with the design of the buckle groove and buckle blocks, the problems of the porcelain board and wooden board are solved. Composite board.
Patent Information
- Application Number
- CN202421174118.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-05-28
- Publication Date
- 2025-01-24
- Estimated Expiration
- 2034-05-28
AI Technical Summary
The existing porcelain boards and wooden boards have problems such as hollowing, fragile, prone to moisture and deformation, and insufficient fire and insect resistance during use, and are difficult to match and keep flat during laying, and are complex in installation.
Design a porcelain-wood male-female composite structure. The porcelain plates are edge-processed to make the edges appear in an "L" shape. Composite glue is used to combine the porcelain plates with the wooden boards. Fastening grooves and fastening blocks are provided for connection.
It has achieved facilitation of processing composite boards, overcoming the defects of porcelain boards and wooden boards, avoiding empty drums and fragile problems, improving the ability to crack and damage, and simplified the installation process, enhancing the stability and service life of the board.
Smart Images

Figure CN222390870U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of composite boards, and more specifically to a ceramic-wood male-female composite structure. Background Art
[0002] With the improvement of people's living standards, the requirements for the boards used for interior decoration are getting higher and higher. At present, there are two types of boards on the market: wooden boards and ceramic boards. Ceramic boards are prone to hollowing when posted, and ceramic tiles are brittle. If the hollowed-out places are subjected to external force, they are easy to break. The surface of ceramic boards is cold, so they are not suitable for the north where the temperature is lower; wooden boards give people a sense of warmth, and are easily affected by moisture, deformed, and cracked. They have a short service life and are not fireproof or insect-proof. Therefore, they are not suitable for the warm and humid south; and when laying ceramic wood floors, it is inconvenient to install them. It is difficult for adjacent boards to match and level them when posted, and it often requires experienced masters to construct them. Moreover, the spliced boards are not stable, and over time, the adjacent boards cannot be leveled.
[0003] The utility model can facilitate the processing of composite boards, overcome the defects of wooden boards and ceramic boards, and connect composite boards. Utility Model Content
[0004] The utility model aims to solve the technical problems raised by the above-mentioned background technology and provide a ceramic-wood male-female composite structure to facilitate the processing of composite boards, overcome the defects of wooden boards and ceramic boards, and connect composite boards.
[0005] To achieve the above-mentioned purpose, the utility model provides the following technical solutions: a ceramic-wood male-female composite structure, comprising: a ceramic plate, a wooden board is installed on the top of the ceramic plate, and the four sides or two adjacent sides of the ceramic plate are edge-treated, and the treated ceramic plate is in an "L" shape.
[0006] A further preferred solution is that the ceramic plate and the wood plate are combined into a composite plate by using a composite adhesive.
[0007] A further preferred solution is that a groove is provided in the center of the bottom end of the wooden board to fit with the "L"-shaped edge of the ceramic plate.
[0008] A further preferred solution is that two adjacent edges of the wooden board fit with the ceramic board, and the other two adjacent edges protrude outwards.
[0009] A further preferred solution is that two adjacent edges of the wooden board match the ceramic board, and the other two adjacent edges protrude outwards.
[0010] A further preferred solution is that two adjacent edges of the filler and the wooden board match the ceramic board, and the other two adjacent edges protrude outwards.
[0011] A further preferred solution is that the two outwardly protruding edges of the composite plate are processed to form snap-fit blocks, and the two non-outwardly protruding edges of the composite plate are provided with snap-fit grooves.
[0012] Beneficial effects:
[0013] 1. By processing the edge of the ceramic plate, it is easy to process the composite plate. The ceramic plate is hard and brittle, which is inconvenient to process, while the wood board is relatively soft and easy to process. If the ceramic plate and the wood board are not processed and the two wood boards are directly composited, the center of the composite plate will be hard on one side and soft on the other side, which is difficult to process with the same tool. After pre-processing the ceramic plate in advance, it forms a composite plate with the wood board. During processing, only the easy-to-process wood board or filler needs to be processed;
[0014] 2. By combining the ceramic plate and the wooden board with composite glue, the defects of the wooden board and the ceramic plate can be overcome. First, the ceramic plate of the composite plate is close to the wooden board, which avoids the problem of hollowing when the ceramic plate is posted; second, the wooden board is warm and the ceramic plate is cold, and the combination of the two uses different surfaces to make it suitable for more regions; finally, because the composite plate is bonded with composite glue, the composite plate is like explosion-proof glass, which not only makes the ceramic plate less likely to break, but also will be bonded by the composite glue even if the ceramic plate breaks, so that the ceramic plate will not split and scatter;
[0015] 3. The effect of connecting the composite panels is achieved by providing the buckle groove and the buckle block. The buckle block is inserted into the buckle groove of another composite panel to connect the two composite panels, making the composite panels easy to install, stable in connection, and convenient to replace damaged composite panels. Both the front and back sides can be used. The composite panels can be combined into different patterns by using different surfaces, and the use effect is greatly improved;
[0016] 4. In summary, this kind of porcelain-wood male-female composite structure can facilitate the processing of composite panels, overcome the defects of wooden boards and porcelain panels, and connect composite panels by processing the edges of porcelain panels, combining porcelain panels and wooden boards with composite glue, and providing connecting grooves and connecting blocks. BRIEF DESCRIPTION OF THE DRAWINGS
[0017] Figure 1 It is a schematic diagram of the three-dimensional structure of the porcelain plate of the present utility model.
[0018] Figure 2 This is a schematic diagram of the three-dimensional structure of a composite board of the utility model.
[0019] Figure 3 This is a schematic cross-sectional structure diagram of a composite board according to the utility model.
[0020] Figure 4 This is a schematic diagram of the three-dimensional structure of the second composite board of the utility model.
[0021] Figure 5It is a schematic diagram of the cross-sectional three-dimensional structure of the style 2 composite board of the present utility model.
[0022] Figure 6 It is a schematic diagram of the overall three-dimensional structure of the utility model.
[0023] Figure 7 It is a three-dimensional structural schematic diagram of the two composite plate connection structure of the utility model.
[0024] Figure 1-7 In: 1. Porcelain plate; 2. Wooden board; 3. Filler; 4. Snap-fit groove; 5. Snap-fit block. DETAILED DESCRIPTION
[0025] The following will be combined with the attached embodiment of the utility model Figure 1-Figure 7 , clearly and completely describe the technical solutions in the embodiments of the utility model.
[0026] Embodiment 1:
[0027] See also Figure 1-7 In an embodiment of the utility model, a ceramic-wood male-female composite structure includes: a ceramic plate 1, a wooden board 2 installed on the top of the ceramic plate 1, and the four sides or two adjacent sides of the ceramic plate 1 are edge-treated. The processed edges of the ceramic plate 1 are in an "L" shape to facilitate subsequent processing of the composite plate. In addition, the processing procedures for the four sides of the ceramic plate 1 and the two adjacent sides are similar, and the structures after processing are also similar. The utility model takes the composite plate with the four sides of the ceramic plate 1 as an example for description and drawing, and the composite plate with the two adjacent sides of the ceramic plate 1 being edge-treated will not be repeated.
[0028] In the embodiment of the utility model, the ceramic plate 1 and the wooden board 2 are combined into a composite board by composite glue, so as to overcome the defects of the wooden board 2 and the ceramic plate 1. Firstly, the ceramic plate 1 of the composite board is close to the wooden board 2, so as to avoid the problem of hollowing when the ceramic plate 1 is posted; secondly, the wooden board 2 is warm and the ceramic plate 1 is cold, and the combination of the two is suitable for more regions by using different surfaces; finally, because the composite board is bonded with composite glue, the composite board is like explosion-proof glass, which not only makes the ceramic plate 1 less likely to break, but also makes it bonded by the composite glue even if the ceramic plate 1 breaks, so that the ceramic plate 1 will not split and scatter.
[0029] In the embodiment of the utility model, a groove is opened in the center of the bottom end of the wooden board 2 to match the "L"-shaped edge of the ceramic plate 1. Two adjacent edges of the wooden board 2 match the ceramic plate 1, and the other two adjacent edges protrude outward. The ceramic plate 1 and the wooden board 2 are combined to form a style 2 composite board, which is easy to process. The two edges protruding outward are the easy-to-process wooden board 2, so that the protruding edges can be directly processed into the snap-fitting blocks 5, without the need to process the difficult-to-process ceramic plate 1.
[0030] In the embodiment of the utility model, the two outwardly protruding edges of the composite board are processed to form snap-fit blocks 5, and the two non-outwardly protruding edges of the composite board are provided with snap-fit grooves 4, so as to achieve the effect of connecting the two composite boards. The snap-fit blocks 5 are inserted into the snap-fit grooves 4 of another composite board to connect the two composite boards, so that the composite boards are easy to install, the connection is stable, and it is convenient to replace damaged composite boards. Both the front and back sides can be used. The composite boards can be combined into different patterns by using different surfaces, and the use effect is greatly improved.
[0031] Embodiment 2:
[0032] See also Figure 1-7 In this embodiment, only the composite board composite style is different, and no groove is provided in the center of the bottom end of the wooden board 2. The same structure is not repeated here. The difference from the first embodiment is that:
[0033] In the embodiment of the utility model, the four sides of the wooden board 2 are connected with fillers 3 that match the "L"-shaped edges of the ceramic plate 1. The filler 3 is made of an easy-to-process material. Two adjacent edges of the filler 3 and the wooden board 2 match the ceramic plate 1, and the other two adjacent edges protrude outward. The filler 3, the ceramic plate 1 and the wooden board 2 are combined to form a composite board, which is easy to process.
[0034] Working principle: When producing composite boards, firstly, one edge of the ceramic board 1 is processed. The ceramic board 1 is hard and brittle, which is inconvenient to process, while the wooden board 2 is relatively soft and easy to process. If the ceramic board 1 and the wooden board 2 are not processed, and the two wooden boards are directly compounded, the composite board will have a hard material on one side and a soft material on the other side in the middle, which is difficult to process with a tool. After the ceramic board 1 is pre-treated in advance, it is formed into a composite board with the wooden board 2. During processing, only the easy-to-process wooden board 2 needs to be processed; then the ceramic board 1 and the wooden board 2 are compounded into a composite board with composite glue. The composite board overcomes the defects of wooden board 2 and ceramic board 1. Firstly, the ceramic board 1 of the composite board is close to wooden board 2, which avoids the problem of hollowing when the ceramic board 1 is posted; secondly, The wooden board 2 is warm while the ceramic board 1 is cold. The combination of the two is suitable for more regions by using different surfaces. Finally, because the composite board is bonded by composite glue, the composite board is like explosion-proof glass, which not only makes the ceramic board 1 less likely to break, but also will be bonded by the composite glue even if the ceramic board 1 breaks, so that the ceramic board 1 will not split and scatter. Finally, the composite board is processed by grooving and the like to complete the processing of the composite board. The snap-fit block 5 is inserted into the snap-fit groove 4 of another composite board to connect the two composite boards, so that the composite board is easy to install, the connection is stable, and it is easy to replace the damaged composite board. Both the front and back sides can be used. The composite board can be combined into different patterns by using different surfaces, and the use effect is greatly improved.
Claims
1. A ceramic-wood male-female composite structure, comprising: A ceramic plate (1) is characterized in that a wooden board (2) is installed on the top of the ceramic plate (1), and four sides or two adjacent sides of the ceramic plate (1) are edge-treated, so that the treated edges of the ceramic plate (1) are in an "L" shape.
2. The ceramic-wood male-female composite structure according to claim 1, characterized in that: The ceramic plate (1) and the wooden plate (2) are combined into a composite plate by using composite glue.
3. The ceramic-wood male-female composite structure according to claim 2, characterized in that: A groove is provided at the center of the bottom end of the wooden board (2) and is matched with the "L"-shaped edge of the ceramic board (1).
4. The ceramic-wood male-female composite structure according to claim 3, characterized in that: Two adjacent edges of the wooden board (2) are aligned with the ceramic board (1), and the other two adjacent edges protrude outwards.
5. The ceramic-wood male-female composite structure according to claim 2, characterized in that: The four sides of the wooden board (2) are connected with fillers (3) that fit the "L"-shaped sides of the ceramic board (1), and the fillers (3) are made of an easy-to-process material.
6. The ceramic-wood male-female composite structure according to claim 5, characterized in that: Two adjacent edges of the filler (3) and the wooden board (2) are aligned with the ceramic board (1), and the other two adjacent edges protrude outwards.
7. A ceramic-wood male-female composite structure according to claim 4 or 6, characterized in that: The two outwardly protruding edges of the composite plate are processed to form snap-fit blocks (5), and the two non-outwardly protruding edges of the composite plate are provided with snap-fit grooves (4).