Chimney inner wall composite anti-corrosion structure of fluorine-containing rubber material surface layer
By adopting a composite anti-corrosion structure with a surface layer of fluoroelastic material on the inner wall of the chimney, the problem of unsatisfactory corrosion resistance and high temperature resistance in the prior art is solved, a longer service life and better anti-corrosion performance are achieved, and blockage is avoided through the cleaning system.
Patent Information
- Application Number
- CN202421224733.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-05-31
- Publication Date
- 2025-03-07
- Estimated Expiration
- 2034-05-31
AI Technical Summary
The existing composite anti-corrosion structure of the inner wall of the chimney has not yet achieved ideal results in corrosion resistance and high temperature resistance, resulting in a decline in material performance and a shortened service life.
A composite anticorrosion structure is adopted for the fluoro-rubber material surface layer, including a primer layer, a heat insulation layer, abrasion-resistant layer, an anticorrosion layer and a fluoro-rubber material surface layer, which is made of fluoro-rubber material and is coated on the outermost layer to increase weather resistance.
It improves the corrosion resistance and high temperature resistance of the composite anti-corrosion structure of the chimney inner wall, extends the service life of the chimney, and uses the design of the spray head and flow tank to facilitate the cleaning of the chimney inner wall and avoids the accumulation of impurities and cause clogging.
Smart Images

Figure CN222578277U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of anti-corrosion structures, in particular to a chimney inner wall composite anti-corrosion structure containing a fluorine rubber material surface layer. Background Art
[0002] The composite anti-corrosion structure of the chimney inner wall usually refers to an anti-corrosion system that combines a variety of anti-corrosion materials and technologies on the inner wall of the chimney. It is used to cope with complex working conditions such as high temperature, high pressure, and corrosive media, so as to extend the service life of the chimney and ensure its safe and stable operation.
[0003] The composite anti-corrosion structure currently used on the inner wall of the chimney has not yet achieved ideal results in terms of corrosion resistance and high temperature resistance. This structure may experience problems such as decreased material performance and shortened service life under long-term exposure to high temperature and corrosive gases.
[0004] Therefore, it is necessary to develop a composite anti-corrosion structure for the inner wall of a chimney containing a fluorine rubber surface layer, which can improve the corrosion resistance and high temperature resistance and extend the service life of the chimney. Utility Model Content
[0005] The utility model aims to provide a composite anti-corrosion structure for the inner wall of a chimney containing a fluorine rubber material surface layer, so as to solve the technical problems of unsatisfactory corrosion resistance and high temperature resistance proposed in the above background technology.
[0006] To achieve the above-mentioned purpose, the utility model provides the following technical solutions: a composite anti-corrosion structure for the inner wall of a chimney with a fluorine-containing rubber surface layer, comprising a chimney body, a primer layer coated on the chimney body, a heat insulation layer connected to the primer layer, a wear-resistant layer connected to the heat insulation layer, an anti-corrosion layer fixedly connected to the wear-resistant layer, a fluorine-containing rubber surface layer fixedly connected to the anti-corrosion layer, and a topcoat layer coated on the fluorine-containing rubber surface layer.
[0007] Preferably, support columns are arranged in an array on the chimney body, and the support columns are penetrated inside the primer layer, the thermal insulation layer, the wear-resistant layer and the anti-corrosion layer, and one end of the support column is fixedly connected to the fluororubber surface layer, thereby supporting and connecting the primer layer, the thermal insulation layer, the wear-resistant layer, the anti-corrosion layer and the fluororubber surface layer.
[0008] Preferably, water flow grooves are embedded inside the anti-corrosion layer and the fluorine-containing rubber surface layer.
[0009] Preferably, the water flow trough is provided with water spray heads in an array, and the water spray heads extend to the interior of the topcoat layer.
[0010] Compared with the prior art, the beneficial effects of the utility model are:
[0011] 1. The utility model can improve the protective performance of the composite anti-corrosion structure of the inner wall of the chimney with the fluorine-containing rubber surface layer installed. The fluorine-containing rubber surface layer is the outermost layer of the composite anti-corrosion structure and is made of fluorine-containing rubber material. The fluorine-containing rubber has excellent chemical resistance, especially in terms of acid resistance, alkali resistance, heat resistance, etc., and can effectively resist the erosion of the acid gas, corrosive steam and other media discharged from the chimney. The topcoat layer is used to protect the fluorine-containing rubber surface layer, increase the aesthetics and weather resistance. The topcoat is usually a high-performance coating that is resistant to ultraviolet rays and aging, thereby making the composite anti-corrosion structure of the inner wall of the chimney with the fluorine-containing rubber surface layer have the characteristics of aging resistance, high temperature resistance and corrosion resistance, thereby extending the service life of the chimney;
[0012] 2. The utility model has a water spray head installed, and the input end of the water trough is connected with the external delivery pipeline. The external cleaning agent can flow into the inside of the water trough through the pipeline. When the inner wall of the chimney needs to be cleaned, the chemical agent is prepared according to the condition of the inner wall of the chimney. After the chemical agent is transported to the inside of the water trough through the pipeline, the chemical agent is rushed to the inner wall of the chimney through the water spray head, thereby facilitating the cleaning of the inner wall of the chimney and effectively avoiding blockage caused by excessive impurities adsorbed inside the chimney. BRIEF DESCRIPTION OF THE DRAWINGS
[0013] Figure 1 It is a schematic diagram of the overall structure of the utility model;
[0014] Figure 2 This is a schematic diagram of the surface structure of the fluorine-containing rubber material of the utility model;
[0015] Figure 3 For this utility model Figure 1 A magnified schematic diagram of the structure in the middle.
[0016] In the figure: 1. Primer layer; 2. Heat insulation layer; 3. Wear-resistant layer; 4. Anti-corrosion layer; 5. fluororubber surface layer; 6. Topcoat layer; 7. Support column; 8. Chimney body; 9. Water flow channel; 10. Sprinkler head. DETAILED DESCRIPTION
[0017] The following will be combined with the drawings in the embodiments of the utility model to clearly and completely describe the technical solutions in the embodiments of the utility model. Obviously, the described embodiments are only part of the embodiments of the utility model, not all of the embodiments. Based on the embodiments in the utility model, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the utility model.
[0018] See also Figure 1 , Figure 2 and Figure 3A composite anti-corrosion structure for the inner wall of a chimney with a fluorine-containing rubber surface layer comprises a chimney body 8, a primer layer 1 is coated on the chimney body 8, a heat insulation layer 2 is connected to the primer layer 1, a wear-resistant layer 3 is connected to the heat insulation layer 2, an anti-corrosion layer 4 is fixedly connected to the wear-resistant layer 3, a fluorine-containing rubber surface layer 5 is fixedly connected to the anti-corrosion layer 4, a topcoat layer 6 is coated on the fluorine-containing rubber surface layer 5, the primer layer 1 is a polyurethane primer, which has excellent weather resistance and chemical resistance, and has good adhesion to metal and non-metallic materials, so that the composite anti-corrosion structure of the inner wall of the chimney with the fluorine-containing rubber surface layer can be tightly connected to the chimney body 8, the heat insulation layer 2 is refractory concrete, which contains a high proportion of refractory aggregate, can withstand high temperatures, and has good heat insulation performance, the wear-resistant layer 3 is made of glass flake resin, which has high strength and good corrosion resistance, and can form a solid layer. The hard wear-resistant protective layer is used to protect the inner wall of the chimney from wear and corrosion. The anti-corrosion layer 4 is an anti-corrosion coating such as polyurea, epoxy resin, polyvinyl chloride, etc., which has good corrosion resistance and can form a tough protective film to protect the inner wall of the chimney. The fluororubber surface layer 5 is the outermost layer of the composite anti-corrosion structure and is made of fluororubber material. Fluororubber has excellent chemical resistance, especially in terms of acid resistance, alkali resistance, heat resistance, etc., and can effectively resist the erosion of media such as acidic gases and corrosive steam emitted from the chimney. The topcoat layer 6 is used to protect the fluororubber surface layer 5, increase the aesthetics and weather resistance. The topcoat is usually a high-performance coating that is resistant to UV rays and aging, so that the composite anti-corrosion structure of the chimney inner wall with the fluororubber surface layer has the characteristics of aging resistance, high temperature resistance and corrosion resistance, thereby extending the service life of the chimney.
[0019] See also Figure 1 and Figure 3 A support column 7 is arranged in an array on the chimney body 8, and the support column 7 is penetrated inside the primer layer 1, the heat insulation layer 2, the wear-resistant layer 3 and the anti-corrosion layer 4. One end of the support column 7 is fixedly connected to the fluororubber surface layer 5, thereby supporting and connecting the primer layer 1, the heat insulation layer 2, the wear-resistant layer 3, the anti-corrosion layer 4 and the fluororubber surface layer 5. The support column 7 improves the tightness of the connection between the composite anti-corrosion structure of the chimney inner wall of the fluororubber surface layer.
[0020] See also Figure 3The anti-corrosion layer 4 and the fluorine-containing rubber surface layer 5 are inlaid with a water flow trough 9. The composite anti-corrosion structure of the chimney inner wall of the fluorine-containing rubber surface layer provides an installation space for the water flow trough 9 through the anti-corrosion layer 4 and the fluorine-containing rubber surface layer 5. The input end of the water flow trough 9 is connected with the external conveying pipeline. The external cleaning agent can flow into the inside of the water flow trough 9 through the pipeline. When the inner wall of the chimney needs to be cleaned, chemical agents are prepared according to the condition of the inner wall of the chimney. After the chemical agents are transported to the inside of the water flow trough 9 through the pipeline, the chemical agents are rushed to the inner wall of the chimney through the water nozzle 10, which facilitates the cleaning of the inner wall of the chimney and effectively avoids blockage caused by excessive impurities adsorbed inside the chimney.
[0021] See also Figure 3 A water spray head 10 is arranged in an array on the water flow trough 9, and the water spray head 10 extends to the inside of the topcoat layer 6, and the medium inside the water flow trough 9 flows to the outside through the water spray head 10.
[0022] Working principle: first, the primer layer 1 is a polyurethane primer, which has excellent weather resistance and chemical resistance, and has good adhesion to metal and non-metal materials, so that the composite anti-corrosion structure of the chimney inner wall with the fluorine rubber surface layer can be tightly connected with the chimney body 8. The heat insulation layer 2 is refractory concrete, which contains a high proportion of refractory aggregates, can withstand high temperatures, and has good heat insulation performance. The wear-resistant layer 3 is made of glass flake resin, which has high strength and good corrosion resistance. It can form a hard wear-resistant protective layer to protect the inner wall of the chimney from wear and corrosion. The anti-corrosion layer 4 is an anti-corrosion coating such as polyurea, epoxy resin, polyvinyl chloride, etc., which has good corrosion resistance. It can form a tough protective film to protect the inner wall of the chimney. The fluororubber surface layer 5 is the outermost layer of the composite anti-corrosion structure and is made of fluororubber material. Fluororubber has excellent chemical resistance, especially in terms of acid resistance, alkali resistance, heat resistance, etc. It can effectively resist the erosion of media such as acidic gases and corrosive steam emitted from the chimney. The topcoat layer 6 is used to protect the fluororubber surface layer 5 to increase the aesthetics and weather resistance. The topcoat is usually a high-performance coating that is resistant to UV rays and aging, so that the composite anti-corrosion structure of the inner wall of the chimney with the fluororubber surface layer has the characteristics of aging resistance, high temperature resistance and corrosion resistance, thereby extending the service life of the chimney.
[0023] It is obvious to those skilled in the art that the present invention is not limited to the details of the exemplary embodiments described above, and that the present invention can be implemented in other specific forms without departing from the spirit or essential features of the present invention. Therefore, the embodiments should be regarded as exemplary and non-restrictive from any point of view, and the scope of the present invention is defined by the appended claims rather than the above description, and it is intended that all changes falling within the meaning and scope of the equivalent elements of the claims be included in the present invention. Any reference numeral in a claim should not be regarded as limiting the claim to which it relates.
Claims
1. A composite anti-corrosion structure for the inner wall of a chimney with a fluorine-containing rubber surface layer, comprising a chimney body (8), characterized in that: The chimney body (8) is coated with a primer layer (1), the primer layer (1) is connected to a heat insulation layer (2), the heat insulation layer (2) is connected to a wear-resistant layer (3), the wear-resistant layer (3) is fixedly connected to an anti-corrosion layer (4), the anti-corrosion layer (4) is fixedly connected to a fluorine-containing rubber surface layer (5), and the fluorine-containing rubber surface layer (5) is coated with a topcoat layer (6).
2. The composite anti-corrosion structure for the inner wall of a chimney with a fluorine-containing rubber surface layer according to claim 1, characterized in that: The chimney body (8) is provided with support columns (7) in an array, and the support columns (7) are inserted into the primer layer (1), the heat insulation layer (2), the wear-resistant layer (3) and the anti-corrosion layer (4), and one end of the support column (7) is fixedly connected to the fluorine-containing rubber surface layer (5), thereby supporting and connecting the primer layer (1), the heat insulation layer (2), the wear-resistant layer (3), the anti-corrosion layer (4) and the fluorine-containing rubber surface layer (5).
3. The composite anti-corrosion structure for the inner wall of a chimney with a fluorine-containing rubber surface layer according to claim 2, characterized in that: The anti-corrosion layer (4) and the fluorine-containing rubber surface layer (5) are inlaid with water flow grooves (9) inside.
4. The composite anti-corrosion structure for the inner wall of a chimney with a fluorine-containing rubber surface layer according to claim 3, characterized in that: The water flow channel (9) is provided with water spray heads (10) in an array, and the water spray heads (10) extend to the interior of the topcoat layer (6).