Salient point structure, chip and packaging structure
By designing the lock finger structure in the bump structure of the flip chip, the problem of layering risk between the bump structure and the plastic seal body is solved, the reliability of the packaging structure is improved, and the requirements of moisture sensitivity level 1 are met.
Patent Information
- Application Number
- CN202421249983.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-03
- Publication Date
- 2025-03-07
- Estimated Expiration
- 2034-06-03
AI Technical Summary
There is a risk of layering between the convex structure of the flip chip and the plastic seal, which reduces the reliability of the packaging structure and is difficult to meet the reliability requirements of moisture-sensitive level 1.
A bump structure is designed in which the first metal layer, the second metal layer and the solder block are stacked sequentially on the substrate, and the second metal layer laterally protrudes the side walls of the first metal layer to form a step difference to form a locking finger structure to enhance the bonding strength with the plastic seal body.
Through the design of the lock finger structure, the risk of layering between the convex structure and the plastic seal body is reduced, the reliability of the packaging structure is improved, and the reliability requirements of moisture-sensitive level 1 are met.
Smart Images

Figure CN222581162U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of semiconductor packaging, in particular to a convex point structure, a chip and a packaging structure. Background Art
[0002] Flip chip (FC) packaging is an advanced integrated circuit packaging technology that mainly achieves electrical connection through bump structures. In recent years, more and more semiconductor packaging customers require that the reliability of integrated circuit chips must meet the requirements of Moisture Sensitivity Level 1 (MSL1). For flip chips, there is a risk of delamination between the bump structure and the plastic package after reliability testing, which reduces the reliability of the packaging structure. Utility Model Content
[0003] One of the purposes of the utility model is to provide a bump structure, a chip and a packaging structure, which can reduce the risk of delamination between the bump structure and the plastic package body and improve the reliability of the packaging structure.
[0004] In order to achieve the above object, the utility model provides a bump structure, which includes a first metal layer, a second metal layer and a solder block stacked in sequence on a substrate, wherein the second metal layer laterally protrudes from the side wall of the first metal layer.
[0005] Optionally, the second metal layer covers the first metal layer and an edge portion of the second metal layer extends out of a side wall of the first metal layer.
[0006] Optionally, the first metal layer is columnar.
[0007] Optionally, a surface of the solder block away from the second metal layer is a curved surface.
[0008] Optionally, the bump structure further includes a seed layer, and the seed layer is located between the substrate and the first metal layer.
[0009] Optionally, the material of the first metal layer is copper, and the material of the second metal layer is nickel.
[0010] The utility model also provides a chip, which comprises a substrate and the above-mentioned convex point structure, wherein the convex point structure is located on the surface of the substrate.
[0011] Optionally, a pad is provided on the surface of the substrate, an insulating protective layer is provided on the substrate, the insulating protective layer has a window exposing the pad, and the bump structure is formed on the pad.
[0012] The utility model also provides a packaging structure, which comprises a plastic packaging body and the chip, wherein the plastic packaging body wraps the chip and covers the side wall of the bump structure on the surface of the chip.
[0013] Optionally, the packaging structure further includes a substrate; the bump structure of the chip is welded on the substrate, and the plastic package body is formed on the substrate.
[0014] The utility model provides a bump structure comprising a first metal layer, a second metal layer and a solder block stacked in sequence on a substrate, wherein the second metal layer protrudes laterally from the side wall of the first metal layer, so that a step difference is formed between the side wall of the first metal layer and the side wall of the second metal layer, and the bump structure becomes a finger-locking structure, which is beneficial for the bump structure to lock the plastic package body wrapped around the bump structure, enhance the bonding strength between the bump structure and the plastic package body, reduce the risk of delamination between the bump structure and the plastic package body, and improve the reliability of the packaging structure. BRIEF DESCRIPTION OF THE DRAWINGS
[0015] Figure 1 A schematic diagram of a bump structure provided in one embodiment of the utility model.
[0016] Figure 2 A schematic diagram of a chip provided in accordance with an embodiment of the present invention.
[0017] Figure 3 A schematic diagram of a packaging structure provided in one embodiment of the utility model.
[0018] Explanation of the reference numerals: 100 - bump structure; 101 - first metal layer; 102 - second metal layer; 103 - solder block; 201 - substrate; 202 - insulating protective layer; 301 - base plate; 302 - plastic package. DETAILED DESCRIPTION
[0019] In order to reduce the risk of delamination between a bump structure and a plastic package body and improve the reliability of a packaging structure, the utility model provides a bump structure, a chip including the bump structure and a packaging structure including the chip.
[0020] The bump structure of the present application includes a first metal layer, a second metal layer and a solder block stacked in sequence on a substrate, wherein the second metal layer protrudes laterally from the side wall of the first metal layer, so that a step difference is formed between the side wall of the first metal layer and the side wall of the second metal layer, and the bump structure becomes a locking finger structure, which is beneficial for the bump structure to lock the plastic package wrapped around the bump structure, enhance the bonding strength between the bump structure and the plastic package, reduce the risk of delamination between the bump structure and the plastic package, and improve the reliability of the packaging structure.
[0021] The bump structure proposed by the utility model is further described in detail below in conjunction with the accompanying drawings and specific embodiments. According to the following description, the advantages and features of the utility model will become clearer. It should be noted that the accompanying drawings are all in a very simplified form and use non-precise proportions, which are only used to conveniently and clearly assist in explaining the purpose of the embodiments of the utility model.
[0022] The terms used in the present invention are only for the purpose of describing specific embodiments and are not intended to limit the present invention. Unless otherwise defined in the present application document, the technical terms or scientific terms used in the present invention should be the common meanings understood by people with ordinary skills in the field to which the present invention belongs. The words "first", "second" and similar words used in the present invention specification do not indicate any order, quantity or importance, but are only used to distinguish different components. Similarly, words such as "one" or "one" do not indicate quantity restrictions, but indicate the existence of at least one. "Multiple" or "several" means two or more. Unless otherwise specified, words such as "upper / upper layer" and / or "lower / lower layer" are only for the convenience of explanation and are not limited to one position or one spatial orientation. Words such as "include" or "comprise" mean that the elements or structures appearing in front of "include" or "comprise" include the elements or structures listed after "include" or "comprise" and their equivalents, and do not exclude other elements or structures. Words such as "connect" or "connected" are not limited to physical or mechanical connections, and can include electrical connections, whether direct or indirect. It should also be understood that the term "and / or" used herein refers to and encompasses any and all possible combinations of one or more of the associated listed items.
[0023] Figure 1 A schematic diagram of a bump structure provided by an embodiment of the utility model. Figure 1 As shown, the bump structure 100 includes a first metal layer 101 , a second metal layer 102 , and a solder bump 103 sequentially stacked on a substrate 201 , wherein the second metal layer 102 laterally protrudes from a sidewall of the first metal layer 101 .
[0024] In this embodiment, the first metal layer 101 is close to the substrate 201 and the solder block 103 is far away from the substrate 201 , and the second metal layer 102 is located between the first metal layer 101 and the solder block 103 .
[0025] refer to Figure 1 As shown, the second metal layer 102 covers the first metal layer 101 and the edge of the second metal layer 102 extends out of the side wall of the first metal layer 101 , and the side wall of the first metal layer 101 and the side wall of the second metal layer 102 form a stepped morphology.
[0026] The first metal layer 101 may be columnar, the second metal layer 102 covers the end surface of the first metal layer 101 away from the substrate 201, and the edge of the second metal layer 102 protrudes laterally from the first metal layer 101. Exemplarily, the cross section of the first metal layer 101 parallel to the surface of the substrate 201 may be circular, but is not limited thereto.
[0027] In this embodiment, the bump structure further includes a seed layer (not shown in the figure), and the seed layer is located between the substrate 201 and the first metal layer 101. The end surface of the columnar first metal layer 101 close to the substrate 201 is located on the seed layer.
[0028] Exemplarily, the seed layer serves as an adhesion layer of the bump structure 100 to enhance the bonding force between the bump structure 100 and the substrate 201, and the seed layer serves as a conductive layer during the electroplating process of forming the bump structure 100. The first metal layer 101 can provide electrons during the electroplating process of forming the solder bump, that is, the first metal layer 101 serves as a current-carrying layer. The second metal layer 102 can have solder wettability and serve as a diffusion barrier layer to prevent the formation of compounds between the solder bump 103 and the first metal layer 101.
[0029] In one embodiment, the material of the seed layer may include titanium, the material of the first metal layer 101 may include copper, the material of the second metal layer 102 may include nickel, and the material of the solder block 103 may include tin, but is not limited thereto. The material of the solder block 103 is, for example, tin-silver.
[0030] In this embodiment, the seed layer, the first metal layer 101 and the second metal layer 102 may all be referred to as an Under Bump Metallurgy (UBM).
[0031] refer to Figure 1 As shown, the solder block 103 is formed on the second metal layer 102, and the surface of the solder block 103 away from the second metal layer 102 is a curved surface.
[0032] The utility model also provides a chip. Figure 2 Schematic diagram of a chip provided by an embodiment of the utility model. Figure 2 As shown, the chip includes a substrate 201 and a bump structure 100, wherein the bump structure 100 is located on the surface of the substrate 201, and the bump structure 100 includes a first metal layer 101, a second metal layer 102 and a solder block 103 stacked in sequence on the substrate 201, wherein the second metal layer 102 laterally protrudes from the side wall of the first metal layer 101.
[0033] like Figure 2 As shown, a plurality of bump structures 100 may be disposed on the surface of the substrate 201 .
[0034] In this embodiment, the substrate 201 may be a silicon substrate. The substrate 201 may also be a germanium substrate, a silicon germanium substrate, a silicon on insulator (SOI) or a germanium on insulator (GOI), etc. Certain doping particles may be injected into the substrate 201 according to design requirements to change electrical parameters.
[0035] The surface of the substrate 201 may have a pad (not shown in the figure), Figure 2 As shown, the substrate 201 has an insulating protection layer 202 , the insulating protection layer 202 has a window exposing the pad, and the bump structure 100 is formed on the pad.
[0036] The material of the insulating protective layer 202 may be an insulating material such as a polymer. In this embodiment, the window of the insulating protective layer 202 exposing the pad may be a window that is larger at the top and smaller at the bottom, that is, the sidewall of the window is an inclined sidewall, but is not limited thereto. The seed layer of the bump structure may conformally cover the sidewall of the window and the surface of the pad in the window; the columnar first metal layer 101 partially fills the window.
[0037] Exemplarily, the chip may be a flip chip, and the bump structure 100 may be disposed on the front side of the chip.
[0038] This embodiment also provides a method for forming a bump structure on a substrate. The method for forming a bump structure comprises: referring to Figure 2 As shown, a seed layer is formed on the substrate 201 by sputtering or the like, and the seed layer covers the insulating protective layer 202, the side walls of the windows in the insulating protective layer 202, and the pads exposed on the surface of the substrate 201; a photoresist material is coated on the substrate 201 to form a photoresist layer; the photoresist layer is exposed; the photoresist layer is developed to form a patterned photoresist layer; an electroplating process is performed using the patterned photoresist layer as a mask to sequentially form a first metal layer 101, a second metal layer 102, and a solder block 103 on the seed layer; the patterned photoresist layer is removed; the seed layer covered by the patterned photoresist layer is etched away; a reflow process is performed to melt and reshape the solder block 103, i.e., a solder block 103 with an arc-shaped surface is obtained.
[0039] It should be noted that, taking the example of the first metal layer 101 being made of copper and the second metal layer 102 being made of nickel, in order to obtain a bump structure with a locking finger structure, in one embodiment, in the process of etching the seed layer, an etching solution with different side etching rates for nickel and copper can be selected. Under the same etching time, the etching amount for copper is greater than that for nickel, so that the shrinkage amount of the side wall of the first metal layer 101 is greater than the shrinkage amount of the second metal layer 102, so that the edge portion of the second metal layer 102 extends out of the first metal layer 101, and a locking finger morphology appears at the connection between the first metal layer 101 and the second metal layer 102 on the side wall of the bump structure 100.
[0040] The utility model also provides a packaging structure. Figure 3 This is a schematic diagram of a packaging structure provided by an embodiment of the utility model. Figure 3 As shown, the packaging structure includes a plastic package 302 and the above-mentioned chip, and the plastic package 302 wraps the chip and covers the side wall of the bump structure 100 on the surface of the chip.
[0041] like Figure 3 As shown, the packaging structure may further include a substrate 301, the chip is mounted on the substrate 301 with the front side facing downward, the bump structure 100 on the front side of the chip is welded on the substrate 301, the plastic package 302 is formed on the substrate 301, and the plastic package 302 fills the gap between the front side of the chip and the substrate 301 and wraps the bump structure 100. Since the side wall of the bump structure 100 is a locking finger structure, the bonding strength between the bump structure 100 and the plastic package 302 is high, and the bump structure 100 and the plastic package 302 are not easy to delaminate in a high humidity and high temperature environment, and the packaging structure can meet the reliability requirements of moisture sensitivity level 1.
[0042] In this embodiment, the substrate 301 includes but is not limited to a printed circuit board. The material of the plastic package 302 includes but is not limited to epoxy molding compound (EMC). The plastic package 302 can be formed by transfer molding, compression molding or lamination.
[0043] In the bump structure, the chip including the bump structure and the packaging structure including the chip provided by the utility model, the bump structure 100 includes a first metal layer 101, a second metal layer 102 and a solder block 103 stacked in sequence on a substrate 201, wherein the second metal layer 102 protrudes laterally from the side wall of the first metal layer 101, so that a step difference is formed between the side wall of the first metal layer 101 and the side wall of the second metal layer 102, and the bump structure 100 becomes a locking finger structure, which is beneficial for the bump structure 100 to lock the plastic package 302 wrapped around the bump structure 100, enhance the bonding strength between the bump structure 100 and the plastic package 302, reduce the risk of delamination between the bump structure 100 and the plastic package 302, and improve the reliability of the packaging structure.
[0044] It should be noted that this specification adopts a progressive description method. The chip and packaging structure described later focus on the differences from the bump structure described earlier, and the same and similar parts between the various parts can be referenced to each other.
[0045] The above description is only a description of the preferred embodiment of the utility model, and is not any limitation on the scope of rights of the utility model. Any technical personnel in this field can make possible changes and modifications to the technical solution of the utility model by using the methods and technical contents disclosed above without departing from the spirit and scope of the utility model. Therefore, any simple modifications, equivalent changes and modifications made to the above embodiments based on the technical essence of the utility model without departing from the content of the technical solution of the utility model are within the protection scope of the technical solution of the utility model.
Claims
1. A bump structure, characterized in that: The invention comprises a first metal layer, a second metal layer and a solder block which are sequentially stacked on a substrate, wherein the second metal layer laterally protrudes from a side wall of the first metal layer.
2. The bump structure according to claim 1, characterized in that: The second metal layer covers the first metal layer, and an edge portion of the second metal layer extends out of a sidewall of the first metal layer.
3. The bump structure according to claim 1, characterized in that: The first metal layer is columnar.
4. The bump structure according to claim 1, characterized in that: The surface of the solder block away from the second metal layer is a curved surface.
5. The bump structure according to claim 1, characterized in that: The bump structure further includes a seed layer, and the seed layer is located between the substrate and the first metal layer.
6. The bump structure according to claim 1, characterized in that: The material of the first metal layer is copper, and the material of the second metal layer is nickel.
7. A chip, characterized in that: It comprises a substrate and a bump structure as claimed in any one of claims 1 to 6, wherein the bump structure is located on the surface of the substrate.
8. The chip according to claim 7, characterized in that: The surface of the substrate is provided with a pad, the substrate is provided with an insulating protective layer, the insulating protective layer has a window exposing the pad, and the convex point structure is formed on the pad.
9. A packaging structure, characterized in that: It comprises a plastic package and the chip according to any one of claims 7 to 8, wherein the plastic package wraps the chip and covers the side walls of the bump structure.
10. The packaging structure according to claim 9, characterized in that: The packaging structure also includes a substrate; the bump structure of the chip is welded on the substrate, and the plastic package is formed on the substrate.