Methods for the heat treatment of silicon single crystal wafers
Patent Information
- Application Number
- DE112015004850
- Authority / Receiving Office
- DE · DE
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2014-11-26
- Filing Date
- 2015-09-17
- Publication Date
- 2024-10-02
- Estimated Expiration
- 2035-09-17
Smart Images

Figure 00000000_0000_ABST
Abstract
Description
TECHNICAL FIELDThe present invention relates to a method for heat treatment of a silicon single crystal wafer.PRIOR ARTRapid thermal annealing (RTA) treatment has been conducted to provide silicon single crystal wafers having gettering capability.Such RTA treatment has been widely applied to silicon single crystal wafers in which the entire plane is a neutral (hereinafter also referred to as N) region having almost equal amounts of vacancies that are point defects (Vacance (vacancy), hereinafter also referred to as Va) and interstitial point defects that are referred to as interstitial silicon (hereinafter also referred to as I-Si). Specifically, this has been applied to wafers having a Ni region in which I-Si predominates, an Nv region in which Va predominates, and an Nv region for the entire plane of each wafer as the N region including an oxidation-induced stack defect (OSF) region.As an example of such RTA treatment, JP 2009-212 537 A describes a method for imparting getterability by performing RTA treatment under an atmosphere containing NH 3- to form a nitride layer on a wafer surface to provide voids for a wafer. However, when such a method is used for the RTA treatment of a silicon single crystal wafer in which the entire plane is an Nv region or is an Nv region including an OSF region, the wafer may have larger BMD sizes and an excessively higher BMD density with respect to the oxygen concentration of the wafer, and the time-dependent dielectric breakdown (TDDB) properties are thereby deteriorated. DE 11 2008 000 486 T5 discloses a method for manufacturing a single crystal silicon wafer, wherein a single crystal silicon wafer, which is produced based on a Czochralski method and in which an entire plane in a radial direction is formed from an N region, is subjected to rapid thermal annealing in an oxidizing atmosphere, an oxide film formed in the rapid thermal annealing in the oxidizing atmosphere is removed, and then rapid thermal annealing is performed in a nitriding atmosphere, an Ar atmosphere, or a mixed atmosphere of these atmospheres.SUMMARY OF THE INVENTIONPROBLEM TO BE SOLVED BY THE INVENTIONThe present invention has been made to solve the above-described problem. An object of the present invention is to provide a method for heat-treating a silicon single crystal wafer that can impart getterability to a silicon single crystal wafer even without impairing TDDB characteristics, which has an Nv region for the entire plane of the silicon single crystal wafer or has an Nv region including an OSF region for the entire plane of the silicon single crystal wafer.PROBLEM SOLVING MEANSTo solve the above-described problems, the present invention provides a method for heat-treating a silicon single crystal wafer by a rapid thermal annealing treatment, comprising:introducing a silicon single crystal wafer having an Nv region for the entire plane of the silicon single crystal wafer or having an Nv region including an OSF region for the entire plane of the silicon single crystal wafer into a rapid thermal annealing furnace,Performing preheating at a temperature higher than the temperature 25° C. and lower than the temperature 600° C. lower than the temperature at which silicon reacts with NH 3 while supplying gas containing NH 3- to the rapid thermal annealing furnace, and thenStopping the supply of the NH 3- containing gas and starting the supply of Ar gas to start rapid thermal annealing treatment under Ar gas atmosphere in which the NH 3- gas remains as defined in the claims.Such a heat treatment method can cause a nitride film formed on the surface of a silicon single crystal wafer to have a thinner film thickness than that formed by a prior method. This can suppress the amount of vacancies supplied, whereby excessive oxygen precipitation can be avoided to prevent the formation of oxide precipitates on the surface portion even in a silicon single crystal wafer in which the entire plane is an Nv region or an Nv region including an OSF region. Accordingly, gettering capability can be given without impairing TDDB characteristics.Preferably, the rapid thermal annealing (RTA) treatment is performed under conditions of 1000 to 1275° C. for 10 to 30 seconds.By the RTA treatment, voids can be easily implanted appropriately under such conditions, whereby the gettering capability can be more reliably given. Also, occurrence of slip dislocation and contamination with heavy metals can be prevented by equipment.The preheating is performed at a temperature higher than the temperature 25° C. and lower than the temperature 600° C. as defined in the claims.The preheating at such a temperature provides a uniform NH 3- concentration in a furnace, whereby formation of a nitride layer upon preheating can be more reliably prevented.Also, the silicon single crystal wafer preferably has an Nv range for the entire plane of the silicon single crystal wafer and has an oxygen concentration of 10 to 12 ppma (parts per million atoms); or the silicon single crystal wafer has an Nv range for the entire plane of the silicon single crystal wafer containing an OSF range and has an oxygen concentration of 9 to 11 ppma.The inventive heat treatment method is particularly effective in heat treatment of a silicon single crystal wafer having such an oxygen concentration. The inventive heat treatment method can improve TDDB properties and simultaneously and reliably impart getterability even though the oxygen concentration is in such a range.In the rapid thermal annealing (RTA) treatment, an NH 3- concentration in the rapid thermal annealing furnace is preferably set to 0.5 volume percent or above and 3 volume percent or below when heated to a temperature at which the silicon reacts with NH 3.When the NH 3- concentration in an RTA furnace is such a concentration, a nitride layer having a uniform layer thickness can be more reliably formed on the wafer level.EFFECT OF THE INVENTIONAs described above, the inventive method for heat treatment of a silicon single crystal wafer can impart getterability even to a silicon single crystal wafer without impairing TDDB characteristics having an Nv region for the entire plane of the silicon single crystal wafer or having an Nv region including an OSF region for the entire plane of the silicon single crystal wafer.Accordingly, the inventive method for heat treating a silicon single crystal wafer may form a defect-free zone (DC) layer without generating a crystal defect from the wafer surface to a certain depth of an activated region of a device. A silicon single crystal wafer can also be obtained which can form oxide precipitates, which may be gettering sites, in the wafer by heat treatment for oxygen precipitation, etc.BRIEF DESCRIPTION OF THE DRAWINGSFIG. 1 is a flow chart illustrating an example of the inventive method for heat treatment of a silicon single crystal wafer. FIG. 2 is a graph showing the thickness of nitride films for comparing a nitride film formed by the inventive heat treatment method with a nitride film formed by a prior heat treatment method; FIG. 3 is a graph showing TDDB (y mode) obtained from measured values of each wafer whose entire plane is an Nv region including an OSF region subjected to heat treatment by the heat treatment method according to Example 1 or Comparative Example 1; FIG. 4 is a graph showing BMD densities obtained from measured values of each wafer whose entire plane is an Nv region including an OSF region subjected to the heat treatment by the heat treatment method according to Example 1 or Comparative Example 1.DESCRIPTION OF THE EMBODIMENTSIn a silicon single crystal wafer in which the entire plane is a Ni region, RTA treatment in an NH 3- atmosphere does not promote formation of BMD and thus does not affect TDDB characteristics. On the other hand, in a silicon single crystal wafer in which the entire plane is an Nv region or an Nv region including an OSF region, RTA treatment in an NH 3- atmosphere causes formation of BMD to promote when the oxygen concentration is high to some extent. This produces oxide precipitates on the surface portion to deteriorate the TDDB properties.Accordingly, the inventors have found that a silicon single crystal wafer in which the entire plane is an Nv region or an Nv region including an OSF region can be provided with gettering capability without degrading the TDDB characteristics by thinning the thickness of a nitride layer formed on the wafer surface to suppress the amount of voids supplied in the RTA treatment in an atmosphere containing NH 3-.Specifically, the inventors found that a thinner nitride layer can be formed by supplying NH 3- containing gas only upon preheating which has been supplied in the prior art in both preheating and RTA treatment, and controlling the temperature in a manner such that no nitride layer is formed upon preheating, and by performing the subsequent RTA treatment in which the supply of NH 3- containing gas is stopped and the gas to be supplied is changed to Ar gas, thereby forming a thin nitride layer from the NH 3- containing gas which has been supplied upon preheating and remained in the RTA furnace, thereby completing the present invention.That is, the present invention is a method for heat-treating a silicon single crystal wafer by rapid thermal annealing treatment, comprising:introducing a silicon single crystal wafer having an Nv region for the entire plane of the silicon single crystal wafer or having an Nv region including an OSF region for the entire plane of the silicon single crystal wafer into a rapid thermal annealing furnace,Performing preheating at a temperature lower than the temperature at which silicon reacts with NH 3 while supplying gas containing NH 3- to the rapid thermal annealing furnace, and thenStopping the supply of the NH 3- containing gas and starting the supply of Ar gas to start rapid thermal annealing treatment under Ar gas atmosphere in which the NH 3- gas remains.Hereinafter, the present invention will be described in more detail, but the present invention is not limited thereto.The following are shown: FIG. 1 is a flow chart illustrating an example of the inventive method for the heat treatment of a silicon single crystal wafer.In the heat treatment method in FIG. 1, first, a silicon single crystal wafer in which the entire plane is an Nv region or an Nv region including an OSF region is prepared (FIG. 1( a)). Then, this silicon single crystal wafer is placed in an RTA furnace, and subjected to preheating at a temperature lower than the temperature at which silicon reacts with NH 3 while supplying gas containing NH 3- to the RTA furnace (FIG. 1( b)). Subsequently, the supply of NH 3- containing gas is stopped, the supply of Ar gas is started (FIG. 1( c) ), and RTA treatment is started under Ar gas atmosphere in which NH 3- gas remains to perform the RTA treatment (FIG. 1( d)).In the inventive heat treatment method, the temperature in the preheating is controlled to a temperature lower than the temperature at which silicon reacts with NH 3 to supply gas containing NH 3-. Accordingly, a nitride layer is not formed on a wafer surface before the RTA treatment. Since the NH 3- containing gas is supplied only upon preheating and the RTA treatment is performed after stopping the supply of the NH3-containing gas and starting the supply of the Ar gas, the NH 3- containing gas remaining in the RTA furnace is uniformly diffused in the furnace by concentration gradient to reduce the NH 3- concentration in the furnace. The uniformly diffused NH 3- containing gas (nitriding gas) reacts with silicon during temperature elevation and maintaining the higher temperature during the RTA treatment to form a nitride layer having a thin and uniform layer thickness. As a result, the amount of vacancies implanted by the RTA treatment can be suppressed to reduce an effect that promotes oxide precipitation to prevent the generation of the oxide precipitates on the surface portion, as compared with previous heat treatment methods in which NH 3- gas is continuously supplied throughout the process (both preheating and RTA treatment).Hereinafter, the present invention will be described in more detail.[Silicon Single Crystal Wafer]The inventive heat treatment method relates to a silicon single crystal wafer having an Nv region for the entire plane of the silicon single crystal wafer or having an Nv region including an OSF region for the entire plane of the silicon single crystal wafer. Such a wafer can be cut from a silicon single crystal produced, for example, by the Czochralski method. In a wafer having such a defect region as described above, the TDDB characteristics are deteriorated by previous heat treatment in which NH3-containing gas is supplied in both preheating and RTA treatment. However, the inventive heat treatment method can provide gettering capability even for such a wafer without compromising TDDB characteristics.The silicon single crystal wafer is preferably a silicon single crystal wafer having an Nv range for the entire plane of the silicon single crystal wafer and having an oxygen concentration of 10 to 12 ppma, or a silicon single crystal wafer having an Nv range for the entire plane of the silicon single crystal wafer containing an OSF range and having an oxygen concentration of 9 to 11 ppma. The inventive heat treatment method is particularly effective in heat treatment of a silicon single crystal wafer having such an oxygen concentration. Deterioration of the TDDB characteristics can be more reliably avoided while forming the BMD density in an appropriate range.Incidentally, in the present invention, "ppma" refers to "ppma (JEITA)" (using a conversion factor of Japan Electronics and Information Technology Industries Association (JEITA)).[Preheating]Then, the silicon single crystal wafer is placed in an RTA furnace, and subjected to preheating at a temperature lower than the temperature at which silicon reacts with NH 3 while supplying gas containing NH 3- to the RTA furnace. At this time, the heating temperature is set to a temperature lower than the temperature at which silicon reacts with NH 3 preferably a temperature higher than ordinary temperature and 600° C. or below, and no nitride layer is formed on a wafer surface upon preheating.In the inventive heat treatment method, the thickness of the nitride layer formed during the RTA treatment is almost independent of the conditions in the preheating, such as the heating temperature, the heating time, and the flow rate of NH 3- containing gas, as long as the heating temperature in the preheating is at the above temperature. Accordingly, the conditions of preheating are not particularly limited, and may be set to a heating temperature higher than the ordinary temperature (about 25° C.) and 600° C. or below, a heating time of 10 to 60 seconds, and a flow rate of NH 3- containing gas of 0.1 to 5 I / min.As the NH 3- containing gas, which is not particularly limited, Ar gas containing NH 3 may be preferably used, for example. As described later, during the RTA treatment in the present invention, the NH 3- concentration in the RTA furnace is preferably set to 0.5 volume percent or above and 3 volume percent or below when heated to a temperature at which the silicon reacts with NH 3. Accordingly, the NH 3- concentration of the NH 3- containing gas supplied during preheating is preferably a concentration at which the NH 3- concentration in the RTA furnace during the RTA treatment is in the above-described range, specifically, for example, 1 volume percent or above and 6.5 volume percent or below.[Stopping Supply of NH3-containing Gas and Starting Supply of Ar Gas]After performing the preheating, the supply of NH 3- containing gas is stopped, and the supply of Ar gas is started. At this time, the stopping of the supply of NH 3- containing gas and the starting of the supply of Ar gas may be performed in any order, and may be performed simultaneously. Moreover, stopping the supply of NH 3- containing gas and starting the supply of Ar gas may be performed before the start of the RTA treatment described later, and may be performed simultaneously with the start of the RTA treatment.[RTA treatment]Then, the RTA treatment is started under Ar gas atmosphere in which NH 3- gas remains. Incidentally, in the inventive heat treatment method including the step of stopping the supply of NH3-containing gas and starting the supply of Ar gas, the NH 3- concentration in the RTA furnace is not limited when the temperature is raised to the temperature at which silicon reacts with NH 3 during the RTA treatment. However, by setting this concentration to 0.5 volume percent or above and 3 volume percent or below, it becomes easier to form the nitride layers to have the same thickness even if the conditions of the RTA treatment, such as the temperature, the time, and the flow rate of the Ar gas, are different. Accordingly, the conditions for the RTA treatment are not particularly limited. However, it is preferable that the RTA treatment is performed under the conditions such as a heating temperature of 1000 to 1275° C. and a heating time of 10 to 30 seconds, because this can impart reliable gettering capability. This can also prevent generation of slip dislocation and contamination with heavy metals.In this regard, the thickness of a nitride layer formed by the prior heat treatment method was compared with a nitride layer formed by the inventive heat treatment method, thereby achieving the results shown in FIG. 2. Incidentally, as the former heat treatment method, preheating was performed at 210 to 350° C. for 10 seconds while supplying Ar gas containing 3 volume percent NH 3 and then RTA treatment was performed at the maximum temperature of 1175° C. for 10 seconds while supplying Ar gas containing 3 volume percent NH 3. On the other hand, in the inventive heat treatment method, preheating was performed in the same manner as in the former heat treatment method, followed by stopping the supply of Ar gas containing NH 3- starting the supply of Ar gas and RTA treatment performed at the same temperature and time as in the former heat treatment method.As shown in FIG. 2, the nitride film formed by the former heat treatment method has a thickness of about 2.5 nm. On the other hand, the nitride film formed by the inventive heat treatment method has a thickness of about 2.4 nm, which is about 0.1 nm thinner. This small difference in nitride layer thickness substantially affects the amount of implanted vacancies during RTA treatment. Accordingly, with the nitride layer formed by the inventive heat treatment method to have a thickness thinner than the former, the amount of implanted vacancies can be effectively suppressed to suppress the formation of oxygen precipitates on the wafer surface.The inventors' studies further revealed that the nitride layer can be more reliably formed with a layer thickness uniform on the plane by setting the NH 3- concentration to 0.5 volume percent or more and 3 volume percent or less as the NH 3- concentration in an RTA furnace in the inventive heat treatment method when the temperature is raised to the temperature at which silicon reacts with NH 3. It has also been disclosed that the uniformity of the thickness of the nitride layer is significantly dependent on the above NH 3- concentration in an RTA furnace during the RTA treatment and is almost independent of the other conditions of preheating and RTA treatment.The TDDB characteristics, the BMD size and the BMD density were evaluated on a wafer which was heat-treated by the former heat treatment method in which NH 3- containing gas was continuously supplied in both preheating and RTA treatment, to disclose that the TDDB characteristics are particularly preferable when the BND size is 22 nm or below and the BMD density is 3×10 9 / cm 3 or less. On the other hand, it has been found that the wafer may have particularly preferable gettering capability when the BMD density is 5×10 8 / cm 3 or above, particularly 1×10 9 / cm 3 or above. This discloses that a wafer having the BMD size of 22 nm or less and the BMD density of 1×10 9 / cm 3 to 3×10 9 / cm 3 may be a wafer having particularly preferred TDDB characteristics and gettering capability.The inventive heat treatment method can suppress the amount of voids supplied to a wafer having the above-described preferred BMD size and BMD density, and thereby can provide a wafer having particularly preferred TDDB properties and gettering capability.As described above, in the inventive method for heat treatment of a silicon single crystal wafer, the temperature in the preheating is controlled so that a nitride layer is not formed, and the nitride layer is formed of NH 3- gas remaining in an RTA furnace during the RTA treatment. Accordingly, the thickness of a nitride film formed on a wafer surface can be made thinner by RTA treatment as compared with the former heat treatment methods. Thereby, the amount of voids supplied can be suppressed to impart getterability to even a silicon single crystal wafer having an Nv region for the entire plane of the silicon single crystal wafer or having an Nv region for the entire plane of the silicon single crystal wafer including an OSF region in which the TDDB characteristics have been impaired in the former heat treatment method without impairing the TDDB characteristics.EXAMPLEHereinafter, the present invention will be described in detail by way of Example, Comparative Example and Reference Example, but the present invention is not limited thereto.(Single Crystal Silicon Wafer)As the silicon single crystal wafer to be subjected to the heat treatment of Example 1 and Comparative Example 1, there were prepared silicon single crystal wafers in which each entire plane was an Nv region and silicon single crystal wafers in which each entire plane was an Nv region containing an OSF region, each oxygen concentration being different. These wafers were each prepared to have an oxygen concentration of 6.0 ppma, 8.0 ppma, 9.0 ppma, 10.0 ppma, 11.0 ppma, 12.0 ppma, and 14.0 ppma.[Example 1]The prepared wafers were subjected to preheating under the following conditions. Then, the supply of NH 3- containing gas was stopped and the supply of Ar gas was started, and then the RTA treatment was started under the following conditions in Ar gas atmosphere in which the NH 3- gas remained.(Preheating conditions)Heat treatment temperature: 350° C. or below Heat treatment time: 10 seconds Supplied gas: Ar gas containing 3 volume percent NH 3 Amount of gas supply: 0.6 L / min (conditions of RTA treatment) Heat treatment temperature (maximum temperature): 1175° C. Heat treatment time: 10 seconds Supplied gas: Ar gas Amount of gas supply: 20 L / min NH 3 Concentration in the RTA furnace (NH 3 Concentration in the RTA furnace when the temperature is raised to the temperature at which silicon reacts with NH 3 (600° C.)): 0.6 volume percent[Comparative Example 1]The prepared wafers were subjected to preheating under the following conditions. Subsequently, RTA treatment was carried out under the following conditions while the supply of NH 3- containing gas was continued.(Preheating conditions)Heat treatment temperature: 350° C. or below Heat treatment time: 10 seconds of supplied gas: Ar gas containing 3 volume percent of NH 3 Amount of gas supply: 0.6 L / min (conditions of RTA treatment) Heat treatment temperature (maximum temperature): 1175° C. Heat treatment time: 10 seconds of supplied gas: Ar gas containing 3 volume percent of NH 3 Amount of gas supply: 20 L / min of NH 3- Concentration in the RTA furnace: 3 volume percent (continuously supplied)Subsequently, the TDDB characteristics and the BMD density of each wafer subjected to the above-described heat treatment by the heat treatment method of Example 1 or Comparative Example 1 were evaluated as follows.(Evaluation of TDDB properties)Each TDDB (γ-mode) was measured under the conditions of the thickness of the gate oxide layer: 25 nm, the electrode area: 4 mm 2, and the criterion of the TDDB (γ-mode): 5 C / cm 2 or more, and evaluated based on the following criteria. Good: 93% ≤ TDDB (γ-mode) Reasonable: 80% ≤ TDDB (γ-mode) < 93% Poor: TDDB (γ-mode) < 80% (BMD density evaluation)Each wafer was subjected to oxygen precipitation treatment at 800° C. for 4 hours and 1000° C. for 16 hours, cleaved, and etched. The BMD density at the split surface was measured and evaluated based on the following criteria. Excellent: 3×10 9 / cm 3 ≤ BMD density Good: 1×10 9 / cm 3 ≤ BMD density<3×10 9 / cm 3 Appropriate: 5×10 8 / cm 3 ≤ BMD density <1×10 9 / cm 3 Poor: BMD density <5×108 / cm3The evaluation results for each silicon single crystal wafer in which the entire plane was an Nv region are shown in Table 1, and the evaluation results for each silicon single crystal wafer in which the entire plane was an Nv region including an OSF region are shown in Table 2. [Table 1] Table 1] [Table 1] Table 1]A silicon single crystal wafer in which the entire plane was an Nv region6,0Good results are obtainedAppropriately, appropriateGood results are obtainedAppropriately, appropriate8,0Good results are obtainedGood results are obtainedGood results are obtainedGood results are obtained9,0Good results are obtainedGood results are obtainedAppropriately, appropriateGood results are obtained10,0Good results are obtainedGood results are obtainedAppropriately, appropriateDraw down11,0Good results are obtainedGood results are obtainedPoor Quality TestExcellent Excellent Performance12,0Good results are obtainedExcellent Excellent PerformancePoor Quality TestExcellent Excellent Performance14,0Appropriately, appropriateExcellent Excellent PerformancePoor Quality TestExcellent Excellent Performance [Table 2][Table 2]Oxygen concentration Oi (ppma)Heat treatment method in Example 1Heat treatment method in Comparative Example 1TDDB propertyBMD DensityTDDB propertyBMD Density6,0Good results are obtainedAppropriately, appropriateGood results are obtainedAppropriately, appropriate8,0Good results are obtainedGood results are obtainedGood results are obtainedGood results are obtained9,0Good results are obtainedGood results are obtainedGood results are obtainedGood results are obtained10,0Good results are obtainedGood results are obtainedGood results are obtainedExcellent Excellent Performance11,0Good results are obtainedGood results are obtainedAppropriately, appropriateExcellent Excellent Performance12,0Appropriately, appropriateExcellent Excellent PerformanceAppropriately, appropriateExcellent Excellent Performance14,0Poor Quality TestExcellent Excellent PerformancePoor Quality TestExcellent Excellent PerformanceBased on the measured values for each wafer in which the entire plane was an Nv region including an OSF region and the heat treatment was performed by the heat treatment method of Example 1 or Comparative Example 1 as described above, the graph of TDDB (γ mode) and the graph of BMD densities shown in FIG. 3 and FIG. 4, respectively, were obtained.[Reference Example 1]As the wafers for the reference example, silicon single crystal wafers in which each entire plane was a Ni region different from Example 1 and Comparative Example 1 were prepared. These wafers were each prepared to have an oxygen concentration of 6.0 ppma, 8.0 ppma, 9.0 ppma, 10.0 ppma, 11.0 ppma, 12.0 ppma, and 14.0 ppma.The prepared wafers were subjected to preheating followed by the RTA treatment under the same conditions as in Example 1 and Comparative Example 1, respectively. The results are shown in Table 3. [Table 3] [Table 3]Oxygen concentration Oi (ppma)Heat treatment method in Example 1Heat treatment method in Comparative Example 1TDDB propertyBMD DensityTDDB propertyBMD Density6,0Good results are obtainedPoor Quality TestGood results are obtainedPoor Quality Test8,0Good results are obtainedPoor Quality TestGood results are obtainedPoor Quality Test9,0Good results are obtainedAppropriately, appropriateGood results are obtainedAppropriately, appropriate10,0Good results are obtainedAppropriately, appropriateGood results are obtainedAppropriately, appropriate11,0Good results are obtainedGood results are obtainedGood results are obtainedGood results are obtained12,0Good results are obtainedGood results are obtainedGood results are obtainedGood results are obtained14,0Good results are obtainedGood results are obtainedGood results are obtainedGood results are obtainedAs shown in Tables 1 and 2, and FIGS. 3 and 4, it was found that the heat treatment by the heat treatment method of Example 1 can completely reduce the BMD densities, and can suppress the deterioration of the TDDB characteristics as compared with the heat treatment by the heat treatment method of Comparative Example 1, while ensuring the BMD densities to the extent that they have gettering capability. Specifically, in silicon single crystal wafers in which each entire plane was an Nv region, the TDDB characteristics were remarkably improved when the oxygen concentrations were 10 to 12 ppma; in silicon single crystal wafers in which each entire area was an Nv region containing an OSF region, the TDDB characteristics were remarkably improved when the oxygen concentrations were 9 to 11 ppma. In the above oxygen concentration, the BMD densities were particularly preferred, and the excellent gettering capability could be obtained.On the other hand, in silicon single crystal wafers in which each entire plane was a Ni region, the preheating and the RTA treatment of Example 1 and Comparative Example 1 did not show any substantial difference in BMD densities and TDDB characteristics as shown in Table 3.Accordingly, Example 1, Comparative Example 1 and Reference Example 1 disclosed that the present invention exerts an extremely high effect on the improvement of the TDDB characteristics when the heat treatment is applied to a silicon single crystal wafer in which the entire plane is an Nv region or the entire plane is an Nv region including an OSF region as in the present invention.From the above results, it can be disclosed that the inventive method for heat treatment of a silicon single crystal wafer can control the BMD density to an appropriate value without degrading the TDDB properties even in a silicon single crystal wafer in which the entire plane is an Nv region or the entire plane is an Nv region including an OSF region, and accordingly can produce a silicon single crystal wafer having gettering capability while ensuring that the DC layer has excellent TDDB properties.
Claims
A method for heat treating a silicon single crystal wafer by a rapid thermal annealing treatment, comprising: placing a silicon single crystal wafer having an Nv range for the entire plane of the silicon single crystal wafer or having an Nv range containing an OSF range for the entire plane of the silicon single crystal wafer in a rapid thermal annealing furnace; performing preheating at a temperature greater than the temperature 25°C and less than the temperature 600°C which is lower than the temperature at which silicon reacts with NH 3, while supplying NH 3- containing gas into the rapid thermal annealing furnace, and then stopping supply of the NH 3- containing gas and starting supply of Ar gas to start rapid thermal annealing treatment under Ar gas atmosphere in which the NH 3- gas remains.The method for the heat treatment of a silicon single crystal wafer according to claim 1, wherein the rapid thermal annealing treatment is performed under conditions of 1000 to 1275°C for 10 to 30 seconds.The method for heat treatment of a silicon single crystal wafer according to claim 1 or 2, wherein the silicon single crystal wafer has an Nv region for the entire plane of the silicon single crystal wafer and has an oxygen concentration of 10 to 12 ppma.The method for heat treatment of a silicon single crystal wafer according to claim 1 or 2, wherein the silicon single crystal wafer has an Nv region including an OSF region and an oxygen concentration of 9 to 11 ppma for the entire plane of the silicon single crystal wafer.The method for heat treatment of a silicon single crystal wafer according to any one of claims 1 to 4, wherein in the rapid thermal annealing treatment, an NH 3- concentration in the rapid thermal annealing furnace is set to 0.5 volume percent or above and 3 volume percent or below when heated to the temperature of 600°C at which silicon reacts with NH 3.
Citation Information
Patent Citations
Method for producing silicon wafer and silicon wafer
JP2009212537A
Method for producing a single-crystal silicon wafer
DE112008000486T5