Method for manufacturing a superjunction semiconductor device

DE112020003068B4Active Publication Date: 2024-10-17SUZHOU ORIENTAL SEMICONDUCTOR CO LTD
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
DE112020003068
Authority / Receiving Office
DE · DE
Patent Type
Patents
Current Assignee / Owner
Priority Date
2020-05-06
Filing Date
2020-09-22
Publication Date
2024-10-17
Estimated Expiration
2040-09-22

Smart Images

  • Figure 00000000_0000_ABST
    Figure 00000000_0000_ABST
Patent Text Reader

Abstract

Method for fabricating a super-junction semiconductor device, comprising: forming a hard mask layer (30) on an n-doped epitaxial layer (20), determining a position of a p-doped column (23) via a lithography process, etching the hard mask layer (30) and forming at least one opening (31) in the hard mask layer (30), wherein the at least one opening (31) corresponds to the position of the p-doped column (23);Etching the n-doped epitaxial layer (20) with the hard mask layer (30) as a mask and forming a first trench (32) in the n-doped epitaxial layer (20), wherein a width of the first trench (32) is greater than a width of an opening (31) of the at least one opening (31) corresponding to the first trench (32), and the first trench (32) comprises a p-doped column region (32a) lying below the opening (31) corresponding to the first trench (32), and a gate region (32b) lying on two sides of the p-doped column region (32a); forming a first insulating layer (21) on a surface of the first trench (32), depositing a first conductive layer, and back-etching the first conductive layer to form a gate (22) in the gate region (32b) of the first trench (32);Forming an insulating sidewall (33) on an exposed sidewall of the gate (22), etching the n-doped epitaxial layer (20) with the hard mask layer (30) and the insulating sidewall (33) as masks, and forming a second trench (34) in the n-doped epitaxial layer (20), wherein the second trench (34) lies below the p-doped column region (32a) corresponding to the first trench (32); and forming the p-doped column (23) in the p-doped column region (32a) and in the second trench (34), and forming a pn transition structure between the p-doped column (23) and the n-doped epitaxial layer (20), wherein the p-doped column (23) is separated from the gate (22) by the insulating sidewall (33).
Need to check novelty before this filing date? Find Prior Art

Description

TECHNICAL FIELDThe present disclosure relates to the technical field of a super junction semiconductor device and, for example, to a method of manufacturing a super junction semiconductor device.From US 2017 / 0 062 586 A1, a method for manufacturing a split-gate power device is known. In the method for manufacturing a split-gate power device, lateral etching is added to form lateral recesses of a control gate groove below a first insulating layer in a process of forming the control gate groove by etching, and therefore, after depositing a first conductive layer, the first conductive layer can be directly etched by using the first insulating layer as a mask to form control gates.BACKGROUNDA super junction semiconductor device is based on a charge balancing technology and can reduce the on-state resistance and parasitic capacitance, so that the super junction semiconductor device has an extremely fast switching capability, the switching loss can be reduced, and a higher power conversion efficiency is achieved. A main manufacturing method of the prior art super junction semiconductor device includes: First, as shown in Fig. 1, a hard mask layer 11 is formed on an n-doped epitaxial layer 10, the hard mask layer 11 is then etched and etched by photoetching, an opening is formed in the hard mask layer 11, and a trench 12 is formed in the n-doped epitaxial layer 10; Next, as shown in Fig. 2, a p-doped pillar 13 is formed in the formed trench by an epitaxial process, and a planarization treatment is performed on the p-doped pillar 13, then, as shown in Fig. 3, a gate dielectric layer 14 and a gate 15 are formed again by a photoetching process and an etching process, and finally, a p-doped main portion 16 and an n-doped source region 17 located in the p-doped main portion 16 are formed in the n-doped epitaxial layer 10. The photo-etching process must be performed once when the p-doped pillar is formed, and then the photo-etching process must be performed again when the gate is formed, regardless of whether it is a planar super junction semiconductor device or a trench super junction semiconductor device, and since the photo-etching process is expensive and there is a risk of alignment deviation, the manufacturing cost and risks in manufacturing the super junction semiconductor device are relatively high.SUMMARYThe present disclosure provides a method of manufacturing a super junction semiconductor device that reduces the manufacturing cost of the super junction semiconductor device and reduces the risks in manufacturing the super junction semiconductor device.The present disclosure provides a method of manufacturing a super junction semiconductor device. The method comprises the following steps.A hard mask layer is formed on an n-doped epitaxial layer, a position of a p-doped pillar is determined via a photoetching process, then the hard mask layer is etched and at least one opening is formed in the hard mask layer, wherein the at least one opening corresponds to the position of the p-doped pillar.The n-doped epitaxial layer is etched with the hard mask layer as a mask, and a first trench is formed in the n-doped epitaxial layer, wherein a width of the first trench is larger than a width of an opening corresponding to the first trench, and the first trench has a p-doped pillar region under the opening corresponding to the first trench and a gate region located on two sides of the p-doped pillar region.A first insulating layer is formed on a surface of the first trench, a first conductive layer is deposited, and the first conductive layer is etched back to form a gate in the gate region of the first trench.An insulating sidewall is formed on an exposed sidewall of the gate, the n-doped epitaxial layer is etched with the hard mask layer and the insulating sidewall as masks, and a second trench is formed in the n-doped epitaxial layer, the second trench underlying a p-doped pillar region corresponding to the second trench.The p-doped pillar is formed in the p-doped pillar region and second trench, and a pn junction structure is formed between the p-doped pillar and the n-doped epitaxial layer, with the p-doped pillar separated from the gate by the insulating sidewall.Optionally, the method for manufacturing a super junction semiconductor device further comprises the following steps.A p-doped main region is formed in the n-doped epitaxial layer.An n-doped source region is formed in the p-doped main region.Optionally, the hard mask layer is a layer composite of a silicon oxide layer, a silicon nitride layer and a silicon oxide layer.Optionally, when the first trench is formed by etching, an etching process that combines anisotropic etching and isotropic etching is used.Optionally, the first insulating layer is made of silicon oxide.Optionally, the first conductive layer is made of polycrystalline silicon.Optionally, the formed first conductive layer fills at least the gate region of the first trench when the first conductive layer is deposited.Optionally, a width of the second trench is larger than a width of a p-doped pillar region corresponding to the second trench.Optionally, when the second trench is formed by etching, an etching process that combines anisotropic etching and isotropic etching is used.Optionally, the insulating sidewall has a silicon nitride layer.Optionally, the p-doped column is made of p-doped polycrystalline silicon.According to the method of manufacturing the super junction semiconductor device provided in the present disclosure, the first trench is formed by performing the photo-etching once, the gate is formed by self-alignment in the gate region of the first trench, then the n-type epitaxial layer is etched with the hard mask layer and the insulating sidewall covering a sidewall of the gate as masks to form the second trench, and then the p-type pillar is formed in the first trench and the second trench. According to the method of manufacturing the super junction semiconductor device, the photo-etching once is only required when the gate and the p-type pillar are formed, whereby the manufacturing cost of the super junction semiconductor device can be greatly reduced and the risks in manufacturing the super junction semiconductor device can be reduced.SHORT DESCRIPTION OF THE DRAWINGSFigs. 1 to 3 are simplified structural representations of main structures in cross section in a manufacturing process for a super-junction semiconductor device according to the prior art; and 4 to 10 are simplified structural diagrams of main structures in cross section in a manufacturing process of an embodiment of a method for manufacturing a super junction semiconductor device provided in the present disclosure.DETAILED DESCRIPTIONA technical solution of the present disclosure will now be described in conjunction with the accompanying drawings in embodiments of the present disclosure in a specific manner. Terms such as "having," "comprising," and "comprising" as used in the present disclosure do not exclude the presence or addition of one or more other elements or combinations thereof. Moreover, in the simplified drawings, the thickness of layers and regions of the present disclosure is shown enlarged to illustrate certain embodiments of the present disclosure, and the dimensions in the drawings do not represent actual dimensions.4 to 10 are simplified structural diagrams of main structures in cross section in a manufacturing process of an embodiment of a method for manufacturing a super junction semiconductor device provided in the present disclosure.First, as shown in Fig. 4, a hard mask layer 30 is formed on a provided n-doped epitaxial layer 20, wherein the n-doped epitaxial layer 20 is typically a silicon and the hard mask layer 30 is typically a layer composite of a silicon oxide layer, a silicon nitride layer and a silicon oxide layer. A position of a p-doped pillar is determined by a photoetching process, then the hard mask layer 30 is etched, at least one opening 31 is formed in the hard mask layer 30, and the at least one opening 31 corresponds to the position of the p-doped pillar, and a number of the openings 31 (i.e., a number of the p-doped pillars) is predetermined by requirements of the designed super junction semiconductor device. In the embodiment of the present disclosure, two openings 31 are shown merely by way of example.Next, as shown in Fig. 5, the n-doped epitaxial layer 20 is etched with the hard mask layer 30 as a mask, a first trench 32 is formed in the n-doped epitaxial layer 20, the first trenches 32 have a one-to-one correspondence with the openings in the hard mask layer 30, and the first trench 32 has a p-doped pillar region 32a underlying a corresponding opening and a gate region 32b underlying two sides of the p-doped pillar region 32a. When the first trench 32 is formed by etching, a method in which anisotropic etching and isotropic etching are combined may be adopted, for example, the p-doped pillar region 32a of the first trench 32 is formed by an anisotropic etching method and then the gate region 32b of the first trench 32 is formed by an isotropic etching method.Next, as shown in Fig. 6, a first insulating layer 21 is formed on a surface of the first trench, and the first insulating layer 21 is typically a silicon oxide and is formed by a thermal oxidation process. Then, a first conductive layer is deposited and etched back to form a gate 22 in the gate region of the first trench. When the first conductive layer is deposited, an entire first trench may be filled with the first conductive layer, or the entire first trench may not be filled with the first conductive layer, but the gate region of the first trench may be filled with the first conductive layer.Next, as shown in Fig. 7, an insulating sidewall 33 is formed on an exposed sidewall of the gate 22, and the insulating sidewall 33 typically comprises a silicon nitride layer. Next, the exposed first insulating layer is first etched, then the n-doped epitaxial layer 20 is further etched with the hard mask layer 30 and the insulating sidewall 33 as masks, and a second trench 34 is formed in the n-doped epitaxial layer 20, which is located under the first trench. Optionally, as shown in Fig. 8, a width of the second trench 34 may be larger than a width of a corresponding p-doped pillar region, and accordingly, when the second trench 34 is formed by etching, an etching process in which anisotropic etching and isotropic etching are combined may be applied, for example, the anisotropic etching process may be applied for etching first and then the isotropic etching process may be applied for etching so that the width of the second trench 34 is increased and thus a width of the n-doped epitaxial layer between adjacent second trenches 34 is reduced.The insulating sidewall 33 may extend on an exposed sidewall of the hard mask layer 30, as shown in Fig. 7 and Fig. 8.Next, as shown in Fig. 9, a p-doped pillar 23 is formed in the first trench and the second trench, and a pn junction structure is formed between the p-doped pillar 23 and the n-doped epitaxial layer 20 so that charge equalization occurs, and the p-doped pillar 23 is separated from the gate 22 via the insulating sidewall 33. The p-doped pillar 23 is a p-doped polysilicon formed by an epitaxial process, may be made of a p-doped polycrystalline silicon, and is typically formed by an epitaxial process. Optionally, a one-time p-doping by ion implantation may be performed before the p-doped pillar 23 is formed to form a p-doped equalization region under the second trench or in the n-doped epitaxial layer 20 under the second trench and on two sides of the second trench, thereby achieving better charge equalization between the p-doped pillar 23 and the n-doped epitaxial layer 20.Next, as shown in Fig. 10, a p-doped main region 24 is formed in the n-doped epitaxial layer 20 by a conventional method, and an n-doped source region 25 is formed in the p-doped main region 24.Finally, a dielectric insulation layer, a metal layer, and the like are formed by a conventional method to obtain the super junction semiconductor device.

Claims

A method of manufacturing a super junction semiconductor device, comprising: forming a hard mask layer (30) on an n-doped epitaxial layer (20), defining a position of a p-doped pillar (23) via a lithography process, etching the hard mask layer (30), and forming at least one opening (31) in the hard mask layer (30), wherein the at least one opening (31) corresponds to the position of the p-doped pillar (23); Etching the n-doped epitaxial layer (20) with the hard mask layer (30) as a mask and forming a first trench (32) in the n-doped epitaxial layer (20), wherein a width of the first trench (32) is greater than a width of an opening (31) of the at least one opening (31) corresponding to the first trench (32), and the first trench (32) comprises a p-doped pillar region (32a) located beneath the opening (31) corresponding to the first trench (32) and a gate region (32b) located on two sides of the p-doped pillar region (32a); forming a first insulating layer (21) on a surface of the first trench (32), depositing a first conductive layer, and etching back the first conductive layer to form a gate (22) in the gate region (32b) of the first trench (32); Forming an insulating sidewall (33) on an exposed sidewall of the gate (22), etching the n-doped epitaxial layer (20) with the hard mask layer (30) and the insulating sidewall (33) as masks and forming a second trench (34) in the n-doped epitaxial layer (20), the second trench (34) underlying the p-doped pillar region (32a) corresponding to the first trench (32); and forming the p-doped pillar (23) in the p-doped pillar region (32a) and in the second trench (34) and forming a pn junction structure between the p-doped pillar (23) and the n-doped epitaxial layer (20), the p-doped pillar (23) being separated from the gate (22) via the insulating sidewall (33).A method of manufacturing a super junction semiconductor device according to claim 1, further comprising: forming a p-doped main region (24) in the n-doped epitaxial layer (20); and forming an n-doped source region (25) in the p-doped main region.A method for producing a super junction semiconductor component according to claim 1, wherein the hard mask layer (30) is a layer composite of a silicon oxide layer, a silicon nitride layer and a silicon oxide layer.A method for producing a super junction semiconductor device according to claim 1, wherein during the formation of the first trench (32) by etching, an etching method is used in which anisotropic etching and isotropic etching are combined.A method of manufacturing a super junction semiconductor device according to claim 1, wherein the first conductive layer is made of a polycrystalline silicon.A method for producing a super junction semiconductor device according to claim 1, wherein the first conductive layer formed fills at least the gate region (32b) of the first trench (32) during the deposition of the first conductive layer.A method for manufacturing a super junction semiconductor device according to claim 1, wherein a width of the second trench (34) is greater than a width of the p-doped pillar region (32a) corresponding to the second trench (34).A method for producing a super junction semiconductor device according to claim 7, wherein during the formation of the second trench (34) by etching, an etching method is used in which anisotropic etching and isotropic etching are combined.A method of manufacturing a super junction semiconductor device according to claim 1, wherein the insulating sidewall (33) comprises a silicon nitride layer.A method for producing a super junction semiconductor device according to claim 1, wherein the p-doped column (23) is made of a p-doped polycrystalline silicon.

Citation Information

Patent Citations

  • Method for manufacturing split-gate power device

    US20170062586A1