METHOD FOR MANUFACTURING A STRUCTURE COMPRISING CAVITIES
The method of forming hollowed areas, vacuum welding, and hot isostatic compression enables the production of complex cavity structures with improved mechanical properties and reduced costs, addressing deformation and machining challenges in existing methods.
Patent Information
- Application Number
- FR2023002883
- Authority / Receiving Office
- FR · FR
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-27
- Publication Date
- 2024-10-04
- Estimated Expiration
- 2043-03-27
AI Technical Summary
Existing methods for manufacturing structures with cavities, such as heat exchangers, face challenges in achieving complex shapes without deformation, displacement, or offset, and often require costly and complex machining processes.
A method involving forming hollowed areas in a substrate, depositing a plate on the substrate, performing transparency welding under vacuum around the hollowed areas, and then applying hot isostatic compression to form sealed cavities, which includes steps like resistance, electron beam, or laser welding to ensure a watertight junction.
This method allows for the production of structures with complex cavity shapes while avoiding deformation and reducing machining costs, ensuring a uniform weld with minimal residual stresses and improved mechanical properties.
Smart Images

Figure 00000000_0000_ABST
Abstract
Description
Title of the invention: METHOD FOR MANUFACTURING A STRUCTURE COMPRISING CAVITIES Technical field
[0001] The present invention relates to the field of heat exchangers, and more generally to structures comprising cavities, for example fluid circulation channels.
[0002] The invention relates to a method of manufacturing a structure comprising cavities.
[0003] The invention also relates to a structure comprising cavities.
[0004] The invention finds applications in numerous industrial fields and, in particular, for the manufacture of heat exchangers.
[0005] The invention is particularly interesting since it makes it possible to obtain elements comprising cavities, the cavities being able to be of simple or complex shapes. STATE OF THE PRIOR ART
[0006] Currently, to produce a structure comprising hollowed-out parts, several methods are possible.
[0007] A first solution is to manufacture the component by additive manufacturing (or 3D printing). Parts with complex geometric shapes with good mechanical characteristics can be obtained. However, dimensional and geometric tolerances are often not respected.
[0008] A second solution consists of forming channels by removing material from a solid elementary part. However, such a machining technique does not allow all the desired channel geometries, sections and lengths to be obtained.
[0009] A third solution consists of assembling elementary parts together using various techniques, such as fusion welding, brazing, or diffusion welding.
[0010] Diffusion welding is currently one of the most promising avenues, and more particularly Hot Isostatic Compression (HIC) welding. The compressive force is obtained by applying a pressurized gas to all the walls of the components to be assembled. To produce a component with hollowed-out parts using this technique, three methods exist.
[0011] The first method, shown in [Fig.l], consists of using tubes 1 which are sandwiched between two grooved plates 2, 3. The shape of the grooves is identical to the tubes. The tubes can be pre-deformed to obtain different sections (example: square, rectangular) or to have different curvatures in length.
[0012] However, with this first method, only hollowed parts of simple geometric shapes can be obtained.
[0013] The second method, shown in [Fig. 2], consists of producing an assembly by means of two diffusion welding cycles. Such a method is described in document WO 2011 / 026925 A1. Several plates 4, 5, including at least one grooved plate, are superimposed. A bead is arranged between the two plates. A treatment step is carried out to obtain diffusion welding of the bead of material on the plates 4, 5. The first cycle is carried out at low pressure. The hollowed-out parts are closed at the ends. As the gas cannot penetrate at the interface, diffusion welding is carried out. The junction is watertight. However, large pores remain and the assembly has low mechanical strength. Thus, the method then comprises a step of consolidating the assembly by hot isostatic compression, to obtain diffusion welding of its elements.This cycle is started at high pressure, the hollowed parts are opened to close the pores and make the junction disappear.
[0014] The main disadvantage of this second method is that it is almost impossible to manufacture hollowed parts without deforming them. Indeed, since no pressure is present inside the channels, during the first cycle, they can deform.
[0015] In order to prevent deformation / collapse of the channels, it is possible to introduce a material into the channels that can subsequently be eliminated or removed, for example, chemically or mechanically. Such a solution is for example described in JP 2006 / 263746 A. However, it can be difficult not only to find the right filling material, but also to successfully remove it completely.
[0016] A third method consists of laser welding thin plates 6 onto the channels formed in a substrate 7, then welding a cover 8 onto the resulting assembly. This method is for example shown in [Fig. 3]. Such a method is also described in document WO 2006 / 067349 AL More particularly, this method comprises the following steps:
[0017] - providing a substrate 7 in which grooves have been made in order to constitute the bottom of the hollowed-out part ([Fig.4A]),
[0018] - place thin blades 6 at the top of the grooves in order to close the hollowed out part ([Fig.4B]),
[0019] - weld the blades 6 to the substrate 7 by edge / edge laser welding in order to guarantee a sealing ([Fig.4C]),
[0020] - place a cover 8 above the assembly formed by the substrate 7 and by the blades 6 ([Fig.4D]),
[0021] - weld the substrate 7 and the cover 8 by diffusion by isostatic compression to hot ([Fig.4E]).
[0022] However, this latter method has many disadvantages. In particular, the fitting of thin blades into the grooves requires strict width tolerances (0.1 mm), which not only increases the machining costs but complicates the process because it remains difficult to fit and weld the thin blades into the sockets without deformation, displacement and / or offset, particularly when it comes to hollowed parts of complex shapes. Statement of the invention
[0023] An aim of the present invention is to propose a method overcoming the drawbacks of the prior art, and in particular, a method making it possible to form a structure comprising cavities, the cavities being able to be of simple or complex shape, while avoiding the phenomena of deformation, displacement and / or offset.
[0024] For this, the present invention proposes a method of manufacturing a structure comprising cavities, the method comprising the following steps:
[0025] a) forming recessed areas in a first face of a substrate made of a first material,
[0026] b) depositing a plate made of a second material on the first face of the substrate, so as to cover the hollowed-out areas of the substrate,
[0027] c) performing resistance welding, electron beam welding or laser transparency welding, preferably under vacuum, around the recessed areas, whereby the plate is welded to the substrate and cavities are formed,
[0028] d) carrying out a diffusion welding step in hot isostatic compression on the assembly obtained.
[0029] The invention is fundamentally distinguished from the prior art by the deposition of a plate on the substrate and by the implementation of a step of transparency welding, preferably under vacuum, of the plate on the substrate over the entire contour of the hollowed-out areas of the substrate to form sealed cavities. The welding may be transparency resistance welding, transparency electron beam welding or transparency laser welding. This step ensures sealing at the substrate / plate junction. Thus, not only is the perimeter of the cavities made watertight, but in addition, this step limits or even avoids pollution / oxidation of the trapped surfaces.
[0030] The use of a vacuum environment allows, at the same beam power than under neutral gas, to obtain a finer and more penetrating weld bead. Welding takes place at the plate / substrate interface through the plate.
[0031] The hot isostatic compression diffusion welding step allows the assembly to be finalized.
[0032] Advantageously, during step c), laser welding is also carried out by transparency on the contour of the plate.
[0033] As the weld bead is thinner under vacuum and the atmosphere is homogeneous (it is not necessary to have gas protection next to the fusion as during welding under neutral gas), it is possible to weld cavities of small widths and / or at the bottom of a narrow and deep well.
[0034] Advantageously, after step c), a degassing step is carried out at the plate / substrate interface.
[0035] According to this advantageous variant, the method comprises, between step c) and step d), the following successive steps:
[0036] - place a cover on the plate,
[0037] - weld the cover onto the plate,
[0038] Advantageously, after having welded the cover to the plate, the method comprises a step during which a degassing step is carried out at the plate / cover interface.
[0039] Advantageously, the cover is welded to the plate by laser welding, by transparency, preferably under vacuum.
[0040] Advantageously, the first material and the second material are independently chosen from copper and its alloys, titanium and its alloys, aluminum and its alloys, steels and vanadium. The first material and the second material may be identical or different.
[0041] The process has many advantages:
[0042] - obtain a uniform weld (in terms of chemical composition and micro structure) almost free of residual stresses.
[0043] - assembling identical materials together (such as steels, alloys aluminum, titanium alloys, copper alloys) or assemble materials with very different chemical compositions (for example steel / copper, steel / vanadium assemblies, etc.),
[0044] - present a lower implementation cost compared to the methods of the art previous, and in particular a lower machining cost,
[0045] - being able to manufacture structures having cavities of complex shapes,
[0046] - avoid deformation phenomena,
[0047] - do not implement a nesting step.
[0048] The invention also relates to a structure obtained by such a method. The structure comprises:
[0049] - a substrate made of a first material comprising hollowed-out areas in a first face of the substrate,
[0050] - a plate made of a second material covering the hollowed-out areas of the substrate, the plate being welded to the substrate around the hollowed-out areas by a weld obtained by transparency, preferably under vacuum, by resistance welding, by laser welding or by electron beam welding and by diffusion in hot isostatic compression, the hollowed-out areas delimited by the substrate and the plate forming cavities,
[0051] - possibly, a cover welded onto the plate.
[0052] Advantageously, the first material and the second material are independently chosen from copper and its alloys, titanium and its alloys, aluminum and its alloys, steels, and vanadium. The first material may be identical to or different from the second material.
[0053] Advantageously, the structure is a heat exchanger comprising cavities arranged to circulate a fluid, the cavities forming channels for circulation of a fluid: gas or liquid (example: N2, water, mixture of molten metals).
[0054] Other characteristics and advantages of the invention will emerge from the additional description which follows.
[0055] It goes without saying that this additional description is given only as an illustration of the subject of the invention and must in no case be interpreted as a limitation of this subject. Brief description of the drawings
[0056] The present invention will be better understood on reading the description of exemplary embodiments given purely for informational purposes and in no way limiting, with reference to the appended drawings in which:
[0057] [Fig.l]
[0058] [Fig.2]
[0059] [Fig.3] previously described, represent different embodiments according to the prior art.
[0060] [Fig.4A]
[0061] [Fig.4B]
[0062] [Fig.4C]
[0063] [Fig.4D]
[0064] [Fig.4E] previously described, represent different steps of a method according to the prior art.
[0065] [Fig.5A]
[0066] [Fig.5B]
[0067] [Fig.5C]
[0068] [Fig.5D] represent different steps of a method according to a particular embodiment of the invention.
[0069] [Fig.6A]
[0070] [Fig.6B]
[0071] [Fig.6C]
[0072] [Fig.6D]
[0073] [Fig.6E] represent different steps of a method according to another particular embodiment of the invention.
[0074] [Fig.7A]
[0075] [Fig.7B] are three-dimensional schematic representations of different substrates used to implement the method according to different particular embodiments of the invention,
[0076] [Fig.8] is a photographic image of different substrates used to implement the method according to another particular embodiment of the invention.
[0077] [Fig.9] is a photographic image of different structures obtained after laser welding under vacuum by transparency of a plate on the different substrates of [Fig.8], according to another particular embodiment of the invention.
[0078] [Fig. 10] is a metallographic section of the weld of one of the structures shown in [Fig.9].
[0079] The different parts represented in the figures are not necessarily on a uniform scale, in order to make the figures more readable.
[0080] The different possibilities (variants and embodiments) must be understood as not being mutually exclusive and can be combined with each other.
[0081] Furthermore, in the following description, terms that depend on the orientation, such as "above", "below", etc. of a structure apply with the assumption that the structure is oriented as illustrated in the figures.
[0082] DETAILED DESCRIPTION OF PARTICULAR EMBODIMENTS
[0083] Although this is in no way limiting, the invention is particularly suitable for manufacturing a structure comprising fluid circulation channels intended in particular, but not exclusively, for the exchange of heat between two fluids.
[0084] We will now describe in more detail a method of manufacturing a structure comprising cavities with reference to the appended figures 5A to 5F. The method comprises the following steps:
[0085] a) forming hollowed-out areas 110 in a first face 101 of a substrate 100 made of a first material ([Fig.5A]),
[0086] b) depositing a plate 200 made of a second material on the first face 101 of the substrate 100, so as to cover the hollowed-out areas of the substrate 100 ([Fig.5B]),
[0087] c) performing resistance welding, electron beam welding or laser welding by transparency, preferably under vacuum, around the hollowed-out areas, whereby the plate 200 is welded to the substrate 100 and sealed cavities are formed ([Fig.5C]),
[0088] d) carrying out a diffusion welding step in hot isostatic compression on the assembly obtained ([Fig.5D]).
[0089] According to an alternative embodiment, the method further comprises, between step c) and step d), the steps of depositing a cover 300 on the plate 200 and of welding the cover 300 to the plate 200. Thus, according to this alternative embodiment, represented for example in the appended FIGS. 6A to 6E, the method comprises the following steps:
[0090] a) forming hollowed-out areas 110 in a first face 101 of a substrate 100 made of a first material ([Fig.6A]),
[0091] b) depositing a plate 200 made of a second material on the first face 101 of the substrate 100, so as to cover the hollowed-out areas 110 of the substrate 100 ([Fig.6B]),
[0092] c) carrying out transparency welding such as resistance welding, laser welding or electron beam welding, preferably under vacuum around the hollowed-out areas 110, whereby the plate 200 is welded onto the substrate 100 and sealed cavities are formed ([Fig.6C]),
[0093] - place a cover 300 on the plate 200,
[0094] - weld the cover 300 onto the plate 200 ([Fig.6D]),
[0095] d) carrying out a diffusion welding step in hot isostatic compression on the assembly obtained ([Fig.6E]).
[0096] The substrate 100 comprises a first face 101 and a second face 102. The first face 101 may be parallel to the second face 102. It may also not be parallel to the second face 102. For example, the first face 101 may be flat ([Fig.7A]) or have reliefs ([Fig.7B]).
[0097] During step a), the substrate 100 is machined to form recessed areas. The recessed areas 110 may be of simple shapes (for example, longitudinal shapes). The recessed areas are, for example, grooves (i.e., longitudinal notches that may be narrow). The recessed areas may also be of complex shapes (for example, they may have turns, zigzags).
[0098] The hollowed-out areas 110 may have a very varied section and path. In particular, they may have a rectangular, polygonal, or semi-circular section. They may also have a section that varies according to their length. Their path may or may not be straight. It may have back-and-forths and / or tight turns.
[0099] The hollowed-out areas can be in 2D (i.e. in the same plane (x, y)) or in 3D (i.e. their position can vary in a plane (x, y, z)).
[0100] Advantageously, each hollowed-out zone 110 opens at least at one of its ex ends. Preferably, the recessed areas have two ends and both ends are open.
[0101] In a particular embodiment, it is possible to form hollowed-out areas 110 in the first face 101 and in the second face 102 of the substrate 100. It is then possible to arrange another plate on the second face 102 of the substrate 100, the substrate being sandwiched between the two plates. This embodiment makes it possible to form a compact structure.
[0102] All surfaces to be joined are advantageously cleaned and / or pre-treated (for example by chemical stripping or light machining) in order to obtain a clean surface and in order to improve the characteristics of the joint (for example mechanical or electrical characteristics).
[0103] The plate 200 used during step b) is chosen so as to be able to weld the plate to the substrate by transparency. The plate 200 is deposited and aligned on the substrate 100. This adjustment is simple to implement because the plate 200 is a solid plate. The surface of the plate 200 covers at least all of the recessed areas 110. It preferably covers the entire first face 101 of the substrate 100.
[0104] Advantageously, before being assembled, the plate 200 and the substrate 100 are cleaned and / or machined to remove the surface oxide which may be present on the surface of these parts and / or have good roughness. The cleanliness of the junctions to be assembled is thus guaranteed. This step leads to an improvement in the mechanical properties at the junction.
[0105] According to a first embodiment, the plate 200 can act as a cover. This makes it possible to reduce the number of steps and elements necessary for implementing the method. The costs are thus reduced. The thickness of the plate 200 will be chosen so as to be sufficiently low to obtain a sealed weld with the substrate 100.
[0106] According to another embodiment, a cover 300 is subsequently welded onto the plate 200. The cover 300 acts as a lid. The surface area of the cover 300 is at least equal to the surface area of the plate 200. The cover 300 is the counter-form which allows the material to be added where necessary.
[0107] According to this embodiment variant, the plate 200 may also comprise hollowed-out areas. The hollowed-out areas of the plate may be closed by the cover 300. The cover 300 may be without hollowed-out areas or with hollowed-out areas.
[0108] According to this variant embodiment, the thickness of the plate 200 may be thinner than in the variant embodiment where the plate also acts as a cover.
[0109] The first material of the substrate 100 and the second material of the plate 200 may be identical (i.e. it is a homogeneous assembly).
[0110] Otherwise, the first material and the second material may be different (i.e. it is a heterogeneous assembly).
[0111] The first material and the second material can be chosen independently of each other from: copper and its alloys, titanium and its alloys, aluminum and its alloys, steels and vanadium. During step c), the face of the plate 200 arranged opposite the first face 101 of the substrate 100 and the first face 101 of the substrate 100 form the interface to be welded by diffusion.
[0112] The plate 200 is welded to the substrate 100. The welding is carried out over the entire contour of the hollowed-out areas 110. The weld 210 obtained follows the contour of the hollowed-out areas 110 ([Fig.5C], 6C). The periphery of the interface is welded in a sealed and degassed manner.
[0113] Welding eliminates the use of solder. The maximum temperature at which the resulting element can be used is therefore increased.
[0114] Transparency welding can be performed by laser, electron beam or resistance. Advantageously, for resistance welding, the thicknesses of the elements to be welded will typically be less than 3 mm. Resistance welding can be performed in air, in a controlled atmosphere or in a vacuum.
[0115] This step is preferably carried out by laser welding, and even more preferably it is a laser welding by transparency under vacuum.
[0116] It is possible to form two weld beads for each recessed area 110. However, if the recessed areas are very close to each other, a single weld bead may be sufficient.
[0117] The welding conditions are chosen so as to obtain a seal at the substrate / plate junction.
[0118] Thus, the pressurized gas which will be applied during the Hot Isostatic Compression (HIC) cycle and which will enter the hollowed-out parts will not be present at the substrate 100 / plate 200 interface between two laser weld beads.
[0119] Advantageously, a metallographic cut can be carried out on test samples in order to verify the full penetration of the bead and the absence of any prohibitive defect in the weld beads as defined in standard NF EN ISO 13919 but this control is destructive.
[0120] Advantageously, a helium leak test with a leak detection limit of 1.10 10 mbar.ls 1 according to standard NF EN ISO 20485 can be carried out to guarantee the good leaktightness of the vacuum welding by transparency of each channel of the substrate 100. This control is non-destructive.
[0121] Advantageously, a radiograph or an X-ray tomography can be carried out to check the absence of a redhibitory defect in the weld beads as defined in standard NF EN ISO 13919. This control is non-destructive.
[0122] Advantageously, during step c), the contour of the substrate 100 / plate 200 interfaces is also welded. The weld 220 makes the assembly watertight ([Fig.5D]). If necessary, the contour of the cover 300 / plate 200 interfaces is also welded. The weld 310 makes the assembly watertight ([Fig.6D]). The welding of the contours is preferably carried out by vacuum welding.
[0123] At the end of step c), the cavities formed are watertight.
[0124] To implement step d), the cavities are open at least at one of their ends so that the gas can thus circulate inside the hollowed-out parts. Thus, during step d), the pressure inside the cavities can increase and there is no deformation of the channels during the implementation of this step. This opening can be provided during the step of machining the substrate 100, prior to the CIC cycle.
[0125] Advantageously, before step d), the substrate 100 / plate 200 and / or cover 300 / plate 200 interfaces are degassed under secondary vacuum.
[0126] In step d), CIC diffusion welding is carried out. Sealing the recessed areas 110 by means of the plate 200 welded in step c) makes CIC diffusion welding possible without significant deformation of the formed channels.
[0127] This diffusion welding is done in solid phase. A temperature of approximately 0.5 to 0.9.Tf the melting temperature of the material and high pressure are applied to the components to be assembled.
[0128] For steels and nickel alloys, the welding temperature is typically chosen between 900°C and 1250°C. The pressure is typically between 700 bars and 1500 bars (i.e. between 8.107 Pa and 1.5.108 Pa). The welding time is for example between 1 h and 10 h, preferably between 2 h and 5 h.
[0129] Initially, contact is made at the rough peaks of material. Then, various diffusion mechanisms as well as a migration of the grain boundary seal close the pores. Thus, the interface between the two parts to be assembled disappears.
[0130] If the vacuum of the laser welding of step c) is not satisfactory, it is possible to carry out, before the CIC diffusion welding step, a step during which holes are formed, for example, by drilling and tails (i.e. tubes which allow the substrate / plate and / or plate / cover interfaces to be pulled under vacuum). The greater the vacuum at the interfaces to be welded, the better the mechanical characteristics of the junction.
[0131] Diffusion welding does not produce any deformation of the channels.
[0132] In a particular embodiment, after the diffusion welding step, it is possible to reduce the thickness of the different elements of the structure in order to obtain the desired dimensions of the part to be produced.
[0133] Illustrative and non-limiting examples of an embodiment
[0134] In this example, a substrate 100 with zigzag recessed areas 110, and more particularly M-shaped recessed areas, was manufactured ([Fig.8]). The substrate 100 is made of steel.
[0135] A steel plate 200 was placed on the substrate. Then, the following steps are carried out:
[0136] - a vacuum transparency laser welding step is carried out to weld the plate 200 on the substrate 100, by means of a weld 210, and thus form sealed cavities; the outline of the substrate 100 and the plate 200 has also been welded by transparent laser welding,
[0137] - a step of diffusion welding in hot isostatic compression of the set obtained.
[0138] [Fig.9] represents the part obtained after the vacuum transparency laser welding step.
[0139] A helium test was carried out to check the tightness of the laser weld. The test is that described in paragraph A.3 of the ISO 20485:2018 standard (“Non-destructive testing — Leakage testing — Tracer gas method”). The part has a good seal.
[0140] A metallographic section confirms that the solder 210 penetrates the substrate 100 ([Fig. 10]).
Claims
Claims
1. A method of manufacturing a structure comprising cavities, the method comprising the following steps: a) forming recessed areas (110) in a first face (101) of a substrate (100) made of a first material, b) depositing a plate (200) made of a second material on the first face (101) of the substrate (100), so as to cover the recessed areas (110) of the substrate (100), c) carrying out resistance welding, electron beam welding or laser transparency welding, preferably in a vacuum, around the recessed areas, whereby the plate (200) is welded to the substrate (100) and cavities are formed, d) carrying out a diffusion welding step in hot isostatic compression on the assembly obtained.
2. Method according to claim 1, characterized in that, during step c), laser welding is also carried out by transparency on the contour of the plate (200).
3. Method according to any one of the preceding claims, characterized in that, after step c), a degassing step is carried out at the plate (200) / substrate (100) interface.
4. Method according to any one of the preceding claims, characterized in that the method comprises, between step c) and step d), the following successive steps: - depositing a cover (300) on the plate (200), - welding the cover (300) on the plate (200).
5. Method according to the preceding claim, characterized in that, after having welded the cover (300) onto the plate (200), the method comprises a step during which a degassing step is carried out at the plate (200) / cover (300) interface.
6. Method according to one of claims 4 and 5, characterized in that the cover (300) is welded to the plate (200) by laser welding, preferably under vacuum.
7. Method according to any one of the preceding claims, characterized in that the first material and the second material are independently chosen from copper and its alloys, titanium and its alloys, aluminum and its alloys, steels and vanadium, the first material and the second material possibly being identical or different.
8. Structure comprising: - a substrate (100) made of a first material comprising hollowed-out areas (110) in a first face (101) of the substrate (100), - a plate (200) made of a second material covering the hollowed-out areas (110) of the substrate (100), the plate (200) being welded to the substrate (100) around the hollowed-out areas (110) by a weld (210) obtained by transparency, preferably under vacuum, by resistance welding, by laser welding or by electron beam welding and by diffusion in hot isostatic compression, the hollowed-out areas (110) delimited by the substrate (100) and the plate (200) forming cavities, - optionally, a cover (300) welded to the plate (200).
9. Structure according to claim 8, characterized in that the first material and the second material are independently chosen from copper and its alloys, titanium and its alloys, aluminum and its alloys, steels and vanadium, the first material being able to be identical or different from the second material.
10. Structure according to one of claims 8 and 9, characterized in that the structure is a heat exchanger comprising cavities arranged to circulate a fluid, the cavities forming channels for circulation of a fluid, such as a gas or a liquid.
Citation Information
Patent Citations
Production method of heat exchanger
JP2006263746A
Method for production of an element comprising fluid circulation channels
WO2006067349A1
PROCEED DE REALIZATION D'UN ELEMENT COMPORTANT DES CANAUX DE CIRCULATION DE FLUIDE
FR2879489A1
Cooler
JP2000310470A
Method for manufacturing a module having hollow area, preferably for the circulation of fluid
WO2011026925A1