Antenna cover
The antenna cover employs a planar heating device with comb-shaped electrodes and PTC resistors to efficiently melt obstructions like snow and rain, addressing the challenge of radio wave attenuation by quickly raising the temperature of the radome.
Patent Information
- Application Number
- JP2023046581
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-23
- Publication Date
- 2024-10-04
AI Technical Summary
Existing antenna devices struggle to quickly raise the temperature of the radome to effectively suppress the attachment of obstructions such as snow and rain, leading to potential radio wave attenuation.
An antenna cover equipped with a planar heating device comprising comb-shaped electrodes and PTC resistors made of polyolefin wax, conductive particles, and a binder resin, which heats the cover body to melt and remove obstructions without interfering with radio wave propagation.
The antenna cover reliably suppresses the attachment of snow and rain, ensuring stable radio wave transmission by efficiently melting obstructions using minimal power and maintaining radio wave transparency.
Smart Images

Figure 2024135741000001_ABST
Abstract
Description
[Technical field]
[0001] The present disclosure relates to an antenna cover. [Background technology]
[0002] Radar devices that transmit and receive radio waves have been put to practical use. The radar device is mounted on, for example, a vehicle and detects obstacles around the vehicle by transmitting and receiving radio waves from an antenna. If snow, rain, or other obstructions adhere to an antenna cover such as a radome that covers the antenna, the radio waves may be attenuated, and the propagation of the radio waves may be impeded and attenuated.
[0003] As a technique for preventing obstructions from adhering to the antenna cover, for example, Patent Document 1 proposes an antenna device that prevents deterioration of electrical performance during snowfall and eliminates the need for regular maintenance. This antenna device has an internal heater that raises the temperature of the radome surface, allowing the snow adhering to the radome to melt and be removed. [Prior art documents] [Patent documents]
[0004] [Patent Document 1] Patent No. 6804966 Summary of the Invention [Problem to be solved by the invention]
[0005] However, the antenna device of Patent Document 1 cannot quickly increase the temperature of the radome, and it is difficult to reliably prevent adhesion of obstructions such as snow and rain.
[0006] An object of the present disclosure is to provide an antenna cover that reliably prevents the adhesion of obstructions such as snow and rain. [Means for solving the problem]
[0007] The antenna cover according to the present disclosure comprises a cover body formed to be permeable to radio waves in order to cover an antenna that transmits radio waves, and a sheet-shaped heating element arranged along the cover body and heating the cover body by passing current through it, the sheet-shaped heating element having a first comb electrode having a first main electrode and a first comb-like electrode, a second comb electrode having a second main electrode and a second comb-like electrode, and a plurality of line-shaped PTC resistors arranged between the first comb-like electrode and the second comb-like electrode, the plurality of line-shaped PTC resistors being arranged at intervals, the PTC resistors comprising conductive particles, a binder resin, and a wax, the wax comprising a naturally derived wax and / or a polyolefin-based wax having one or two melting peaks observed in a DSC curve obtained by heating from 25°C to 150°C at a heating rate of 10°C / min using a differential scanning calorimeter. Effect of the Invention
[0008] According to the antenna cover of the present disclosure, it is possible to reliably prevent the adhesion of obstructions such as snow and rain. [Brief description of the drawings]
[0009] [Figure 1] FIG. 1 is a schematic cross-sectional view showing a configuration of a radar device including an antenna cover according to an embodiment of the present disclosure. [Diagram 2] 2A is a front view of the antenna cover, FIG. 2B is a plan view of the antenna cover, FIG. 2C is a cross-sectional view along line AA in FIG. 2B, FIG. 2D is a side view of the antenna cover, and FIG. 2E is a bottom view of the antenna cover. [Diagram 3] FIG. 3 is an enlarged view of a cross section taken along line BB in FIG. 2B. [Figure 4] FIG. 4 is a bottom view of the sheet heating element. [Diagram 5] FIG. 5 is a diagram showing a state in which the sheet heating element is disposed on the cover main body. [Figure 6] FIG. 6 is a diagram showing a radar device mounted on a vehicle. [Figure 7] FIG. 7 is a diagram showing a step in a method for manufacturing an antenna cover. [Figure 8] FIG. 8 is a diagram showing a step in a method for manufacturing an antenna cover. [Figure 9] FIG. 9A is a graph showing an example of a DSC curve of a polyolefin wax in a PTC resistor used in a heating device (sheet heating element) for an antenna cover, and FIG. 9B is a graph showing another example of the DSC curve. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0010] Hereinafter, embodiments of the present disclosure will be described with reference to the accompanying drawings.
[0011] 1 shows a schematic cross-sectional view of a radar device including an antenna cover according to an embodiment of the present disclosure. The radar device includes a support 1, an antenna substrate 2, an antenna 3, an antenna control unit 4, and an antenna cover 5.
[0012] The support part 1 is a member for supporting each part of the radar device, and together with the antenna cover 5 forms an accommodation chamber R for accommodating the antenna substrate 2 and the antenna 3. The support part 1 is made of, for example, a resin material. The antenna substrate 2 is a member for supporting the antenna 3, and is fixed to the support portion 1 in the accommodation chamber R. The antenna substrate 2 is made of, for example, a resin material.
[0013] The antenna 3 is disposed on the antenna board 2, and is configured to transmit radio waves W of a predetermined frequency, for example millimeter waves, toward the front in response to a control signal from the antenna control unit 4. The antenna 3 also receives reflected waves that are the transmitted radio waves W reflected back by an external object, and outputs a received signal to the antenna control unit 4 according to the intensity of the reflected waves.
[0014] The antenna control unit 4 is configured to control the antenna 3, and is electrically connected to the antenna 3. The antenna control unit 4 outputs a preset control signal to the antenna 3 so that radio waves W are transmitted from the antenna 3 at a predetermined timing. The antenna control unit 4 also receives a reception signal from the antenna 3 according to the intensity of the reflected wave. The antenna control unit 4 calculates the position of an object present outside based on the change in the frequency of the reflected wave relative to the frequency of the transmitted radio waves W, and the like.
[0015] The antenna cover 5 has a cover body (so-called radome) that protects the antenna 3, and a heating device (sheet heating element) 7 that removes obstructions such as snow and rain that adhere to the radar device by heating. The structure of the antenna cover 5 is shown in Figs. 2A to 2E. Fig. 2A is a front view of the antenna cover 5, Fig. 2B is a plan view, Fig. 2C is a cross-sectional view taken along line AA in Fig. 2B, Fig. 2D is a side view, and Fig. 2E is a bottom view. Fig. 3 shows an enlarged view of the cross-section taken along line BB in Fig. 2B.
[0016] The cover body 6 is disposed so as to completely cover the antenna substrate 2 and the antenna 3. The cover body 6 is disposed in front of the antenna 3, i.e., on the transmitting side of the radio waves W, and is therefore formed to be transparent to the radio waves W. In this case, the cover body 6 is formed so as to be curved convexly in the transmitting direction with a thickness according to the frequency of the radio waves W so as not to impede the propagation of the radio waves W. The cover body 6 can be made of a material having radio wave transparency, such as a resin material.
[0017] On the other hand, the heating device 7 is disposed on the bottom side of the antenna cover 5, and disposed so as to curve along the cover body 6. As shown in Fig. 2D and Fig. 3, the heating device 7 includes a first comb electrode 8, a second comb electrode 9, and a plurality of linear PTC resistors 10, and heats the cover body 6 by passing current through it.
[0018] FIG. 4 shows an enlarged view (bottom view) of the heating device 7. In FIG. 4, the PTC resistor 10 is indicated by a dotted line so that the structures of the first comb electrode 8 and the second comb electrode 9 can be easily distinguished. As shown in FIG. 4, the first comb electrode 8 includes a first main electrode 8a and a plurality of first comb-shaped electrodes 8b branched from the first main electrode 8a. Similarly, the second comb electrode 9 includes a second main electrode 9a and a plurality of second comb-shaped electrodes 9b branched from the second main electrode 9a. The comb-shaped electrodes 8b of the first comb electrode 8 and the comb-shaped electrodes 9b of the second comb electrode 9 correspond to each other one-to-one, and are arranged approximately parallel to each other. Furthermore, the PTC resistor 10 is arranged in a line between the corresponding first comb electrode 8b and second comb electrode 9b. The plurality of linear PTC resistors 10 are arranged at a predetermined interval to allow the radio wave W to pass therethrough. According to the heating device 7 having such a configuration, the propagation of the radio waves W is not impeded.
[0019] Here, the first comb electrode 8 and the second comb electrode 9 may be made of any material capable of conducting electricity. The first comb electrode 8 and the second comb electrode 9 are usually made of metal, such as aluminum. The PTC resistor 10 will be described in detail later.
[0020] As shown in FIGS. 5 and 6, the heating device 7 is directly or indirectly connected to a power source 11 provided in the radar device or the vehicle V, a power source control unit 12 connected to the power source 11, and a detection unit 13.
[0021] The power supply 11 is configured to supply power to the first comb electrode 8 and the second comb electrode 9 of the heating device 7, and is configured to switch the power supply on and off under the control of a power supply control unit 12.
[0022] The detection unit 13 is configured to detect obstructions such as snow and rain that adhere to the surface of the cover body 6. The detection unit 13 can be configured, for example, from a thermometer that measures the outside temperature, or a detector that directly detects outside snow, rain, etc. with a sensor.
[0023] The power supply control unit 12 is configured to switch the power supply 11 on and off based on the detection result of the detection unit 13, and to control the heating of the cover body 6 by the heating device .
[0024] This radar device can be mounted on a vehicle V as shown in Fig. 6, and can be arranged, for example, so that the cover body 6 is exposed to the outside from a front panel F of the vehicle V. An example of the vehicle V is a work vehicle such as a snowplow.
[0025] Next, a method for manufacturing the antenna cover 5 will be described.
[0026] The manufacturing method of the antenna cover 5 is not particularly limited. For example, the cover body 6 may be formed in advance, and the first comb electrode 8, the second comb electrode 9, and the PTC resistor may be sequentially formed on the back surface of the cover body 6. In this case, the method of forming the cover body 6 is not particularly limited, and various molding methods can be applied. Meanwhile, the first comb electrode 8 and the second comb electrode 9 can be formed by bonding aluminum foil or the like formed in a pattern to the cover body 6. Furthermore, the PTC resistor 10 can be formed by screen printing or the like.
[0027] 7, the first comb electrode 8 and the second comb electrode 9 may be fabricated on a substrate 21, the PTC resistor 10 may be formed thereon by screen printing or the like, and then the substrate 21 may be attached to the cover body 6 by a known method (for example, adhesion with an adhesive, fusion, etc.). At this time, the substrate 21 may be attached so as to be in contact with the cover body 6, or the PTC resistor 10 may be attached so as to be in contact with the cover body 6.
[0028] 7, the first comb electrode 8, the second comb electrode 9, and the PTC resistor 10 may be formed on the surface of the substrate 21, and then the substrate 21 may be placed in a cavity C of a mold M and molten resin Ra may be poured therein to form the cover body 6, as shown in FIG. 8. At this time, the first comb electrode 8, the second comb electrode 9, and the PTC resistor 10 may be placed so as to be exposed in the cavity C, or may be placed so as to be located outside the cavity C. According to this method, no gap is generated between the cover body 6 and the heating device 7, and the heating device 7 can be placed at a desired position.
[0029] The operation of the above radar device will be described with reference to Fig. 6. The above radar device is disposed so that the cover body 6 of the antenna cover 5 is exposed to the outside from the front panel F of the vehicle V. Then, as shown in Fig. 1, when radio waves W of a predetermined frequency are transmitted from the antenna 3 under the control of the antenna control unit 4, the radio waves W propagate forward of the vehicle V via the antenna cover 5. The radio waves W propagated forward of the vehicle V are reflected by an object present in front of the vehicle V. Then, this reflected wave returns via the antenna cover 5 and is received by the antenna 3.
[0030] When the reflected wave is received by the antenna 3, the received signal is output from the antenna 3 to the antenna control unit 4. Then, the antenna control unit 4 calculates the frequency of the reflected wave based on the received signal, and calculates the position of the object with respect to the vehicle V based on the change in the frequency of the reflected wave relative to the frequency of the transmitted radio wave W, etc.
[0031] Next, when an obstruction such as snow adheres to the surface of the cover body 6, the detection unit 13 detects the adhesion of the obstruction to the cover body 6 as shown in Fig. 5. The detection unit 13 detects the adhesion of the obstruction by, for example, detecting it with a raindrop sensor or the like in the external environment of the vehicle V, or by predicting the adhesion by measuring the temperature. The detection unit 13 outputs the measured temperature to the power supply control unit 12.
[0032] The power supply control unit 12 determines whether an obstruction is attached to the cover body 6 based on the temperature measured by the detection unit 13. When the temperature measured by the detection unit 13 is higher than a predetermined value, the power supply control unit 12 determines that an obstruction is not attached and turns off the power supply 11.
[0033] On the other hand, when the temperature measured by the detection unit 13 is equal to or lower than a predetermined value, the power supply control unit 12 determines that an obstruction is attached and turns on the power supply 11. When the power supply 11 is turned on, power is supplied from the power supply 11 to the heating device 7, which heats the cover body 6. This increases the temperature of the cover body 6, and obstructions such as snow attached to the surface of the cover body 6 can be melted or evaporated and removed. In addition, since the heating device 7 directly heats the cover body 6, obstructions can be removed with little power.
[0034] In this way, the heating device 7 heats the cover body 6 to suppress the adhesion of obstructions, so that radio waves W can be transmitted smoothly to the front of the vehicle V regardless of changes in the external environment, and objects present in front of the vehicle V can be reliably detected.
[0035] According to this embodiment, the heating device 7 includes a PTC resistor, which will be described later, and therefore the temperature can be raised stably in a short time. Also, as described above, the PTC resistor is arranged so as not to interfere with the transmission and reception of radio waves W, and therefore the radar device can be used stably.
[0036] In the above embodiment, the heating device 7 is described as being arranged on the bottom side (antenna 3 side) of the cover body 6, but the heating device 7 may also be located on the top side (outside) of the cover body.
[0037] In the above embodiment, the cover body 6 is disposed so as to be exposed to the outside from the front panel F of the vehicle V, but the present invention is not limited to this as long as obstructions can be removed. For example, the cover body 6 can be disposed so as to abut against the front panel F, and obstructions attached to the front panel F can be removed by heat conducted from the cover body 6 to the front panel F.
[0038] (About PTC resistors) The PTC resistor used in the heating device 7 of the antenna cover 5 described above will be described in detail. The PTC resistor contains a specific polyolefin wax or a natural wax together with conductive particles and a binder resin. In the PTC resistor, the wax melts near its melting point when the temperature rises. The volume increase caused by the melting of the wax is much larger than that of a typical resin. In addition, since they melt easily, the resistance value increases significantly in a short time. Therefore, the heating device 7 using the PTC resistor can reliably suppress the adhesion of obstacles such as rain and snow.
[0039] Hereinafter, the above PTC resistor will be described separately for a case where it contains a polyolefin wax (first embodiment) and a case where it contains a naturally derived wax (second embodiment).
[0040] (1) First aspect of the PTC resistor The PTC resistor of the first embodiment contains a polyolefin wax having one or two melting peaks observed in a differential scanning calorimeter (hereinafter also referred to as "DSC") curve when the DSC curve is created by heating from 25°C to 150°C at a heating rate of 10°C / min, a binder resin, and conductive particles. Each component will be described below.
[0041] Polyolefin wax In this specification, the term "wax" refers to an organic material that is solid or semi-solid at room temperature and melts without decomposition when heated. In addition, the term "polyolefin wax" refers to a wax containing 50% by mass or more of an olefin-derived component. The polyolefin wax used in this embodiment has one or two melting peaks observed in a DSC curve when the temperature is raised from 25°C to 150°C at a heating rate of 10°C / min by DSC. It is more preferable that the melting peak observed is one. In this specification, the melting peak in the DSC curve refers to an endothermic peak whose absolute value of the peak height is 0.5 mW or more, and does not include noise whose height is less than 0.5 mW. Note that all DSC curves in this specification are values obtained using 5 mg of sample.
[0042] In this specification, the peak height is a value obtained as follows. First, in the DSC curve, the falling position of the line and the rising position of the line in the downward convex region (region where endothermic reaction occurs) are confirmed. If both of these can be confirmed, they are connected with a line, and this is set as the baseline. In this specification, the baseline is drawn only for the large mountain region where the rising and falling exceeds 1 mW. For example, as shown in FIG. 9B, when a small peak (B, C, and D) with a rising or falling of 1 mW or less is included in one large mountain region (region that is convex downward), only one baseline is drawn for the large mountain region. Also, as shown in FIG. 9B, when there are two or more large mountain regions (regions that are convex downward), a baseline is drawn for each of them (two in FIG. 9B). On the other hand, as shown in FIG. 9A, when either the rising position or the falling position of the line in the downward convex region cannot be confirmed, a straight baseline is drawn along the hem of the side where the rising position or the falling position can be confirmed.
[0043] Then, a line perpendicular to the X-axis is drawn from each peak top of the melting peak of the DSC curve (A in FIG. 9A, and B, C, D, and E in FIG. 9B), and the distance from the intersection of the perpendicular line with the baseline to the peak top is defined as the height of each peak.
[0044] The absolute value of the melting peak height in the DSC curve obtained by the above method is preferably 5 mW or more. When the absolute value of the melting peak height is 5 mW or more, many polyolefin waxes tend to melt at the melting peak temperature. When there are two melting peaks in the DSC curve, it is sufficient that the absolute value of either one of the melting peaks is 5 mW or more.
[0045] The melting peak in the DSC curve of the polyolefin wax is preferably in the range of 80° C. to 150° C., more preferably in the range of 90° C. to 140° C., and even more preferably in the range of 100° C. to 130° C. This provides a PTC resistor that shows an increase in resistance value at 80° C. to 150° C.
[0046] The weight average molecular weight of the above-mentioned polyolefin wax is preferably 1,000 to 1,500,000, more preferably 3,000 to 20,000. When the weight average molecular weight of the polyolefin wax is within this range, it is likely to have a melting peak in the above-mentioned temperature range. The weight average molecular weight is a polystyrene-equivalent value measured by gel permeation chromatography (GPC).
[0047] The PTC resistor may contain only one type of the polyolefin wax, or may contain two or more types. Examples of polyolefin waxes include homopolymers of olefins, copolymers of two or more types of olefins, copolymers of olefins and monomers other than olefins, etc. More specific examples of polyolefin waxes include polyethylene waxes such as low-density polyethylene wax, medium-density polyethylene wax, and high-density polyethylene wax, polypropylene wax, polybutene wax, ethylene-propylene copolymer wax, and ethylene-propylene-butene copolymer wax. In addition, oxidized polyolefin waxes obtained by oxidizing these waxes by a known method may be used. Among these, polyethylene waxes are preferred from the viewpoints of availability and PTC characteristics.
[0048] The amount of polyolefin wax in the PTC resistor is preferably 6% by mass or more and 24% by mass or less, more preferably 12% by mass or more and 20% by mass or less. When the amount of polyolefin wax in the PTC resistor is 6% by mass or more, the PTC magnification of the PTC resistor is further increased, and the rate of increase in the resistance value after the PTC resistor is heated and reaches a certain temperature is likely to be further increased. On the other hand, when the amount is 24% by mass or less, the amount of conductive particles becomes sufficiently large relatively, and the PTC characteristics are likely to be further improved.
[0049] Binder resin The binder resin may be any resin capable of binding the polyolefin wax and the conductive particles described below, or binding them to a substrate or the like, but is preferably one that does not prevent the volume change caused by melting the polyolefin wax. The binder resin itself may expand with increasing temperature, and may contribute to an increase in the resistance value of the PTC resistor. The PTC resistor may contain only one type of binder resin, or may contain two or more types.
[0050] Examples of the binder resin include known thermoplastic resins. Specific examples include thermoplastic polyurethane resin, polyester resin, polyacrylate resin, polysiloxane resin, vinyl halide resin, vinylidene resin, polyimide resin, phenoxy resin, polyether resin, polyketone resin, polyvinyl butyral resin, polyvinylpyrrolidone resin, polyacrylate resin, SEBS resin (styrene-ethylene-butylene-styrene copolymer) and its hydrogenated product, SEPS resin (styrene-ethylene-propylene-styrene copolymer) and its hydrogenated product, etc. Among these, SEBS resin and hydrogenated SEPS resin are preferred from the viewpoint of being easily deformable and not hindering the volume change of the above-mentioned polyolefin wax.
[0051] The amount of binder resin in the PTC resistor is preferably 6% by mass or more and 30% by mass or less, more preferably 15% by mass or more and 28% by mass or less. When the amount of binder resin in the PTC resistor is 6% by mass or more, it becomes easier to print conductive resin, polyolefin wax, and a composition containing the binder resin, and the fixing property after printing becomes good. Furthermore, the strength of the PTC resistor is also likely to be further increased. On the other hand, when the amount of binder resin is 30% by mass or less, the amount of conductive particles becomes relatively sufficiently large, and the PTC characteristics tend to be further improved.
[0052] Conductive particles The conductive particles are not particularly limited as long as they are conductive. -6 / °C or less, and -6 / °C or less is more preferable. The thermal expansion coefficient of the conductive particles can be determined from the material of the conductive particles. The PTC resistor may contain only one type of conductive particles or may contain two or more types of conductive particles.
[0053] Examples of conductive particles include carbon-based particles such as graphite, carbon black, carbon nanotubes, and graphene; metal-based particles such as nickel powder, copper powder, silver powder, and tungsten powder; etc. Among these, nickel powder, silver powder, tungsten powder, and graphite are preferred from the viewpoint of high affinity with the above-mentioned polyolefin wax and binder resin, and of being unlikely to precipitate in the composition for producing the PTC resistor.
[0054] The shape of the conductive particles is not particularly limited, and may be, for example, spherical, amorphous, tubular, rod-like, flat, crushed, etc. The specific surface area of the conductive particles is 5 m 2 The specific surface area is a value measured by a gas adsorption method.
[0055] The size of the conductive particles is appropriately selected depending on the type of conductive particles, etc. For example, when the conductive particles are spherical or close to spherical, the average particle diameter is preferably 30 μm or less, and more preferably 1 μm or more and 10 μm or less. When the average particle diameter is 30 μm or less, the PTC magnification of the PTC resistor tends to be better. The average particle diameter is a value measured by a laser diffraction / scattering method, and is the median (D50) in the cumulative particle size distribution.
[0056] The content of the conductive particles in the PTC resistor is preferably 45% by mass or more and 80% by mass or less, more preferably 50% by mass or more and 70% by mass or less, and even more preferably 55% by mass or more and 67.5% by mass or less. When the amount of the conductive particles in the PTC resistor is 45% by mass or more, the PTC characteristics tend to be more stable. On the other hand, when the amount of the conductive particles in the PTC resistor is 80% by mass or less, the amount of the polyolefin wax and binder resin increases, and the resistance value when heated tends to increase.
[0057] ·others In addition to the polyolefin wax, the binder resin, and the conductive particles, the PTC resistor may contain other components as necessary within the scope of the purpose and effect of the present embodiment. Examples of the other components include various additives such as antioxidants and flame retardants.
[0058] ·Manufacturing method of PTC resistor The PTC resistor of this embodiment can be produced by applying a composition containing the polyolefin wax, the binder resin, the conductive particles, and optionally a solvent, and then heating and curing the composition.
[0059] The type of solvent is not particularly limited as long as it can uniformly dissolve or disperse the above-mentioned polyolefin wax, binder resin, conductive particles, etc. However, the boiling point of the solvent is preferably 100° C. or higher, more preferably 100 to 330° C., and even more preferably 150 to 250° C. When the boiling point of the solvent is within this range, the storage stability of the composition is improved, and the composition is easy to apply.
[0060] The solvent is appropriately selected depending on the type of polyolefin wax, the type of binder resin, etc. Examples include alcohols, ketones, esters, glycol esters, glycol ethers, ethers, aromatic hydrocarbons, and mixtures thereof, with terpineol, butyl carbitol acetate, tetralin, toluene, and mixtures thereof being preferred.
[0061] The amount of the solvent is appropriately selected according to the desired viscosity of the composition, and is usually preferably about 20 to 70 parts by mass, and more preferably 25 to 65 parts by mass, per 100 parts by mass of the total amount of the composition (ink). When the amount of the solvent is within this range, the viscosity of the composition (ink) tends to fall within the desired range.
[0062] The preferred viscosity of the composition is appropriately selected depending on the method for forming the PTC resistor. For example, when the composition is printed by screen printing and cured to obtain the PTC resistor, the viscosity of the composition is preferably 100 to 400 dPa·s. The viscosity is a value measured at 25°C using a cylindrical rotational viscometer (manufactured by Rion Co., Ltd.). When the viscosity of the composition is within this range, the composition can be applied to a desired thickness and can form a film without unevenness.
[0063] The method for preparing the composition is not particularly limited, and the polyolefin wax, resin binder, conductive particles, and solvent may be mixed at once, or the resin binder and solvent may be mixed first, and then the polyolefin wax and conductive particles may be mixed. stomach.
[0064] The method for applying the composition is not particularly limited, and examples thereof include screen printing, roll coating, and application with a dispenser.
[0065] The composition can be cured by heating to about 100 to 200° C. In this case, the heating time is preferably about 1 to 30 minutes. When the composition is heated to the above degree, the solvent in the composition is removed.
[0066] (2) PTC resistor according to the second embodiment The PTC resistor of the second embodiment includes a naturally occurring wax, a binder resin, and conductive particles. Each component will be described below.
[0067] Natural wax In this specification, wax refers to an organic material that is solid or semi-solid at room temperature (25°C) and melts without decomposition when heated. Natural wax refers to plant wax derived from plants or animal wax derived from animals. Also, plant wax refers to wax made from plants. Animal wax refers to wax derived from animals. A PTC resistor may contain only one type of naturally derived wax, or may contain two or more types. The type of naturally derived wax contained in a PTC resistor is not particularly limited, but a resistance value increase at 40°C or higher and 100°C or lower is usually required for a PTC resistor. Therefore, the melting point of the naturally derived wax is preferably 40°C or higher and 100°C or lower, more preferably 50°C or higher and 90°C or higher.
[0068] The wax ester component contained in the naturally occurring wax is preferably 10% by mass or more. When the wax ester component is 10% by mass or more, the melting point of the naturally occurring wax is likely to fall within the above range. In addition, melting near the melting point is likely to proceed in a shorter time.
[0069] Here, the wax ester component refers to an ester in which a higher fatty acid and a higher monohydric alcohol are bonded in a 1:1 ratio. The wax ester component is, for example, an ester of a higher fatty acid having 10 to 50 carbon atoms and a higher monohydric alcohol having 10 to 50 carbon atoms. The total number of carbon atoms constituting the wax ester component is preferably 20 to 100, more preferably 30 to 50.
[0070] The naturally occurring wax may further contain free saturated fatty acids (the above-mentioned higher fatty acids) and free alcohols (the above-mentioned higher monohydric alcohols). The amount of free saturated fatty acids is preferably 20% by mass or less based on the total mass of the naturally occurring wax. On the other hand, the amount of free alcohols is more preferably 15% by mass or less based on the total mass of the naturally occurring wax.
[0071] The iodine value of the naturally derived wax is preferably 80 or less, more preferably 30 or less, and even more preferably 25 or less. The iodine value represents the amount of unsaturated bonds in the hydrocarbon chain of the components contained in the naturally derived wax. The iodine value in the naturally derived wax, i.e., the amount of unsaturated double bonds, is preferably small. If the amount of unsaturated double bonds is large, the naturally derived wax is difficult to melt even when the temperature of the PTC resistor increases. In other words, if the iodine value exceeds 80, the resistance value is difficult to increase when the temperature increases. On the other hand, if the iodine value is 80 or less, the naturally derived wax is easy to melt when the temperature of the PTC resistor increases, and the resistance value is easy to increase.
[0072] Examples of the plant-based wax, which is one type of naturally occurring wax, include candelilla wax, carnauba wax, rice wax, Japan wax wax, hydrogenated jojoba wax, etc. Among these, carnauba wax, candelilla wax, and rice wax are preferred from the viewpoints of availability and ease of increasing the PTC multiplier.
[0073] On the other hand, examples of animal waxes, which are a type of naturally derived wax, include beeswax and lanolin wax.
[0074] The amount of naturally occurring wax in the PTC resistor is preferably 5% by mass or more and 50% by mass or less, more preferably 7% by mass or more and 40% by mass or less. When the amount of naturally occurring wax in the PTC resistor is 5% by mass or more, the resistance value of the PTC resistor when the temperature rises is likely to be further increased. On the other hand, when the amount is 50% by mass or less, the amount of conductive particles described below becomes relatively large enough, and the PTC characteristics of the PTC resistor are likely to be further improved.
[0075] Binder resin The binder resin may be any resin capable of binding the above-mentioned naturally occurring wax and the conductive particles described below, and binding them to a substrate or the like, but is preferably one that does not prevent the volume change caused by melting the above-mentioned naturally occurring wax. The binder resin itself may also expand with increasing temperature, and contribute to an increase in the resistance value of the PTC resistor. The PTC resistor may contain only one type of binder resin, or may contain two or more types. The binder resin is the same as the binder resin of the PTC resistor of the first embodiment.
[0076] The amount of binder resin in the PTC resistor of this embodiment is preferably 5% by mass or more and 50% by mass or less, more preferably 10% by mass or more and 40% by mass or less. When the amount of binder resin in the PTC resistor is 5% by mass or more, it becomes easier to print the conductive resin, the naturally derived wax, and the composition containing the binder resin, and the fixing property after printing becomes good. Furthermore, the strength of the PTC resistor is also likely to be further increased. On the other hand, when the amount of binder resin is 50% by mass or less, the amount of conductive particles becomes relatively sufficiently large, and the PTC characteristics tend to be further improved.
[0077] Conductive particles The conductive particles are not particularly limited as long as they are particles having electrical conductivity, and are the same as the conductive particles in the PTC resistor of the first embodiment described above.
[0078] The content of the conductive particles in the PTC resistor of this embodiment is preferably 45% by mass or more and 80% by mass or less, and more preferably 50% by mass or more and 70% by mass or less. When the amount of the conductive particles in the PTC resistor is 45% by mass or more, the PTC characteristics tend to be more stable. On the other hand, when the amount of the conductive particles in the PTC resistor is 80% by mass or less, the amount of the naturally derived wax and binder resin increases, and the resistance value when heated tends to increase.
[0079] ·others In addition to the naturally occurring wax, the binder resin, and the conductive particles, the PTC resistor may contain other components as necessary within the scope of the purpose and effect of the present embodiment. Examples of the other components include various additives such as antioxidants and flame retardants.
[0080] ·Manufacturing method of PTC resistor The PTC resistor of this embodiment can be produced by applying a composition containing the naturally occurring wax, the binder resin, the conductive particles, and, if necessary, a solvent, and then heating and curing the composition.
[0081] The type of solvent is not particularly limited as long as it can uniformly dissolve or disperse the above-mentioned naturally derived wax, binder resin, conductive particles, etc. However, the boiling point of the solvent is preferably 100° C. or higher, more preferably 100 to 330° C., and even more preferably 150 to 250° C. When the boiling point of the solvent is within this range, the storage stability of the composition is improved, and further, the composition is easier to apply.
[0082] The solvent is appropriately selected depending on the type of naturally occurring wax, the type of binder resin, etc. Examples of the solvent include alcohols, ketones, esters, glycol esters, glycol ethers, ethers, aromatic hydrocarbons, and mixtures thereof, with terpineol, butyl carbitol acetate, tetralin, toluene, and mixtures thereof being preferred.
[0083] The amount of the solvent is appropriately selected according to the viscosity of the desired composition (ink), and is usually preferably about 40 to 90 parts by mass, and more preferably 40 to 85 parts by mass, per 100 parts by mass of the total amount of the composition (ink). When the amount of the solvent is within this range, the viscosity of the composition tends to fall within the desired range.
[0084] The preferred viscosity of the composition is appropriately selected depending on the method for forming the PTC resistor. For example, when the composition is printed by screen printing and cured to obtain the PTC resistor, the viscosity of the composition is preferably 100 to 400 dPa·s. The viscosity is a value measured at 25°C using a cylindrical rotational viscometer (manufactured by Rion Co., Ltd.). When the viscosity of the composition is within this range, the composition can be applied to a desired thickness and can form a film without unevenness.
[0085] The method for preparing the composition is not particularly limited, and the naturally occurring wax, resin binder, conductive particles, and solvent may be mixed at once, or the resin binder and solvent may be mixed first, and then the naturally occurring wax and conductive particles may be mixed. stomach.
[0086] The method for applying the composition is not particularly limited, and examples thereof include screen printing, roll coating, and application with a dispenser.
[0087] The composition can be cured by heating to about 100 to 200° C. In this case, the heating time is preferably about 1 to 30 minutes. When the composition is heated to the above degree, the solvent in the composition is removed.
[0088] In addition, the above-mentioned embodiments are merely examples of the embodiment of the present invention, and the technical scope of the present invention should not be interpreted as being limited by them. In other words, the present invention can be implemented in various forms without departing from the gist or main features of the present invention. For example, the disclosure of the shapes and numbers of each part described in the above-mentioned embodiments is merely an example, and can be implemented by appropriately changing them. [Industrial Applicability]
[0089] The antenna cover according to the present disclosure can be used as a cover for covering an antenna that transmits radio waves. [Explanation of symbols]
[0090] 1 Support part 2 Antenna Board 3 Antennas 4 Antenna control section 5 Antenna cover 6 Cover body 7 Heating device (surface heating element) 8 First comb-shaped electrode 8a, 9a main electrode 8b,9b comb-shaped electrode 9 Second comb-shaped electrode 10 PTC resistor 11 Power supply 12 Power supply control unit 13 Detection section 21 Substrate C Cavity F. Front Panel M mold R Containment Room Ra Molten Resin V Vehicle
Claims
1. a cover body formed to be permeable to radio waves in order to cover an antenna that transmits radio waves; a sheet heating element disposed along the cover body and configured to heat the cover body by energizing the cover body; Equipped with The sheet heating element is a first comb electrode including a first main electrode and a first comb electrode; a second comb electrode including a second main electrode and a second comb electrode; a plurality of linear PTC resistors disposed between the first comb-like electrode and the second comb-like electrode; having The plurality of linear PTC resistors are arranged at intervals, The PTC resistor includes conductive particles, a binder resin, and a wax, The wax includes a naturally occurring wax and / or a polyolefin wax having one or two melting peaks observed in a DSC curve obtained by heating from 25° C. to 150° C. at a heating rate of 10° C. / min using a differential scanning calorimeter. Antenna cover.
2. The conductive particles have a thermal expansion coefficient of 20×10 -6 / ° C. or less, The antenna cover according to claim 1 .
3. The conductive particles have an average particle size of 30 μm or less. The antenna cover according to claim 1 .
4. The conductive particles have a specific surface area of 5 m 2 / g or less, The antenna cover according to claim 1 .
5. The wax includes the polyolefin wax, The absolute value of at least one melting peak height in the DSC curve is 5 W or more; The antenna cover according to any one of claims 1 to 4.
6. The wax comprises a naturally occurring wax, The naturally occurring wax contains 10% by mass or more of a wax ester component. The antenna cover according to any one of claims 1 to 4.
7. The naturally occurring wax has an iodine value of 80 or less. The antenna cover according to claim 6.
Citation Information
Patent Citations
Positive temperature coefficient characteristic thermistor
JP1994069001A
Radar device for vehicle
JP1998132921A
Organic positive temperature coefficient thermistor
JP2000200704A
Ptc planar heating element with fuse function
JP2002313541A
Positive temperature coefficient composition
JP2017535964A