Method for evaluating bonding condition of light-emitting element and method for manufacturing light-emitting device

By evaluating the bonding state of light-emitting elements using a transparent substrate and metal film observation, the method addresses bonding defects in light-emitting device manufacturing, improving productivity.

JP2024137029APending Publication Date: 2024-10-04NICHIA CORP
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
JP2023048379
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-03-24
Publication Date
2024-10-04

AI Technical Summary

Technical Problem

Existing methods for manufacturing light-emitting devices face frequent bonding defects due to inappropriate bonding conditions, leading to reduced productivity.

Method used

A method for evaluating the bonding state of light-emitting elements by bonding them to an evaluation substrate with a metal film on a transparent substrate, observing the electrode through the substrate to determine bonding states, and adjusting conditions based on observed appearances to ensure proper bonding.

Benefits of technology

This method allows for accurate setting of bonding conditions, reducing defects and enhancing the productivity of light-emitting device manufacturing.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024137029000001_ABST
    Figure 2024137029000001_ABST
Patent Text Reader

Abstract

To provide a method for evaluating the bonding state of a light-emitting element, which enables conditions for bonding a light-emitting element to a mounting substrate to be set with high accuracy, and a method for manufacturing a light-emitting device with high productivity.SOLUTION: A method for evaluating a bonding condition of a light-emitting element includes the steps of preparing a light-emitting element having a semiconductor laminate having an upper surface and a lower surface opposite to the upper surface, and an electrode arranged on the lower surface of the semiconductor laminate, preparing an evaluation substrate having a first surface and a second surface opposite to the first surface of a light-transmitting substrate, the first surface being provided with a metal film arranged on the first surface, bonding the electrode of the light-emitting element to the metal film of the evaluation substrate, and determining the bonding condition between the electrode and the metal film by observing the electrode overlapping the metal film from the second surface side of the light-transmitting substrate.SELECTED DRAWING: Figure 4
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The embodiments relate to a method for evaluating a bonding state of a light-emitting element and a method for manufacturing a light-emitting device. [Background technology]

[0002] Patent Document 1 discloses a method for manufacturing a light emitting device in which a large number of light emitting elements are bonded to a single mounting substrate. In such a method for manufacturing a light emitting device, if the conditions for bonding the light emitting elements to the mounting substrate are not properly set, bonding defects occur frequently, significantly reducing the productivity of the light emitting device. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] JP 2020-074005 A Summary of the Invention [Problem to be solved by the invention]

[0004] The embodiments have been made in consideration of the above-mentioned problems, and aim to provide a method for evaluating the bonding state of a light-emitting element, which enables the conditions for bonding a light-emitting element to a mounting substrate to be set with high accuracy, and a method for manufacturing a light-emitting device with high productivity. [Means for solving the problem]

[0005] A method for evaluating the bonding condition of a light-emitting element according to an embodiment includes the steps of: preparing a light-emitting element having a semiconductor laminate having an upper surface and a lower surface opposite to the upper surface, and an electrode arranged on the lower surface of the semiconductor laminate; preparing an evaluation substrate having a first surface and a second surface opposite to the first surface of a light-transmitting substrate, the first surface having a metal film arranged on the first surface; bonding the electrode of the light-emitting element to the metal film of the evaluation substrate; and determining the bonding condition between the electrode and the metal film by observing the electrode overlapping the metal film from the second surface side of the light-transmitting substrate. Effect of the Invention

[0006] According to the embodiment, it is possible to realize a method for evaluating the bonding state of a light emitting element, which allows the conditions for bonding a light emitting element to a mounting substrate to be set with high accuracy, and a method for manufacturing a light emitting device with high productivity. [Brief description of the drawings]

[0007] [Figure 1] 5A to 5C are cross-sectional views showing a method for evaluating the bonding state of the light-emitting element according to the first embodiment. [Diagram 2] 5A to 5C are cross-sectional views showing a method for evaluating the bonding state of the light-emitting element according to the first embodiment. [Diagram 3] 5A to 5C are cross-sectional views showing a method for evaluating the bonding state of the light-emitting element according to the first embodiment. [Figure 4] 4A to 4C are bottom views illustrating a method for evaluating the bonding state of the light-emitting element according to the first embodiment. [Diagram 5] FIG. 13 is a diagram showing an optical path and a waveform in an evaluation sample. [Figure 6] FIG. 13 is a diagram showing an optical path and a waveform in an evaluation sample. [Figure 7] FIG. 13 is a diagram showing an optical path and a waveform in an evaluation sample. [Figure 8] FIG. 13 is a diagram showing the relationship between the bonding state and the brightness of the appearance of the electrode. [Figure 9] 4 is a schematic diagram showing the results of observing electrodes of a light-emitting element through a light-transmitting substrate. FIG. [Figure 10] 10 is a flowchart showing a method for manufacturing a light emitting device according to a second embodiment. [Figure 11] 5A to 5C are cross-sectional views illustrating a method for manufacturing the light emitting device according to the second embodiment. [Figure 12] FIG. 4 is a bottom view showing the first member. [Figure 13] FIG. [Figure 14] 5A to 5C are cross-sectional views illustrating a method for manufacturing the light emitting device according to the second embodiment. [Figure 15] 15 is a partially enlarged cross-sectional view showing an area XV in FIG. 14. [Figure 16] 5A to 5C are cross-sectional views illustrating a method for manufacturing the light emitting device according to the second embodiment. [Figure 17] 5A to 5C are cross-sectional views illustrating a method for manufacturing the light emitting device according to the second embodiment. [Figure 18] 5A to 5C are cross-sectional views illustrating a method for manufacturing the light emitting device according to the second embodiment. [Figure 19] 5A to 5C are cross-sectional views illustrating a method for manufacturing the light emitting device according to the second embodiment. [Figure 20] 5A to 5C are cross-sectional views illustrating a method for manufacturing the light emitting device according to the second embodiment. [Figure 21] FIG. 4 is a top view showing a light emitting device according to a second embodiment. [Figure 22] 22 is a cross-sectional view taken along line XXII-XXII shown in FIG. 21. [Figure 23] 10 is a flowchart showing a method for manufacturing a light emitting device according to a third embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0008] Hereinafter, the embodiments will be described with reference to the drawings. The drawings are schematic or conceptual, and are simplified or emphasized as appropriate. The relationship between the thickness and width of each part, the ratio of the sizes between the parts, etc. are not necessarily the same as in reality. Even when the same part is shown, the dimensions and ratios of each part may be shown differently depending on the drawing. Furthermore, in this specification and each drawing, elements similar to those described with respect to the previous drawings are given the same reference numerals, and detailed descriptions are omitted as appropriate. In addition, an end view showing only the cut surface may be used as a cross-sectional view.

[0009] <First embodiment> The first embodiment is an example of a method for evaluating the bonding state of a light-emitting element. 1 to 3 are cross-sectional views illustrating a method for evaluating the bonding state of the light-emitting element according to this embodiment. FIG. 4 is a back view illustrating a method for evaluating the bonding state of the light emitting element according to this embodiment.

[0010] (Process for preparing light-emitting element) As shown in Fig. 1, a light emitting element 50 is prepared. The light emitting element 50 is, for example, a light emitting diode (LED). When viewed from above, the shape of the light emitting element 50 is rectangular, for example, a square with a side length of 45 µm. It is preferable to prepare a plurality of light emitting elements 50 having the same specifications.

[0011] The light emitting element 50 has a semiconductor laminate 51 and an electrode 52. In the semiconductor laminate 51, a p-type layer, an active layer, and an n-type layer are laminated in this order. The semiconductor laminate 51 has an upper surface 51a and a lower surface 51b opposite to the upper surface 51a. The electrode 52 is disposed on the lower surface 51b of the semiconductor laminate 51. At least the surface of the electrode 52 is made of gold (Au), and for example, the electrode 52 is entirely made of gold. For example, in one light emitting element 50, two electrodes 52 are provided, one electrode 52 is connected to the p-type layer of the semiconductor laminate 51, and the other electrode 52 is connected to the n-type layer of the semiconductor laminate 51. In this specification, "connection" means electrical connection. On the lower surface of the semiconductor laminate 51, the two electrodes are separated from each other, and a groove 53 is formed between the two electrodes 52. The groove 53 is recessed with respect to the lower surface 52b of the electrode 52. The light emitting element 50 may have three or more electrodes 52.

[0012] (Process of preparing the evaluation board) As shown in Fig. 2, an evaluation substrate 60 is prepared. The evaluation substrate 60 has a light-transmitting substrate 61 and a metal film 62. The light-transmitting substrate 61 is made of a light-transmitting insulating material, such as sapphire, quartz, or glass. The light-transmitting substrate 61 has a first surface 61a and a second surface 61b opposite to the first surface 61a.

[0013] The metal film 62 is disposed on the first surface 61a of the light-transmitting substrate 61. For example, the metal film 62 is disposed continuously over the entire first surface 61a. The metal film 62 has a thickness that allows at least 50% of visible light to pass through. The metal film 62 has a film made of gold on the surface, for example. In one example, the metal film 62 is a two-layer film in which a titanium layer having a thickness of 5 nm and a gold layer having a thickness of 20 nm are laminated, and the titanium layer is in contact with the first surface 61a of the light-transmitting substrate 61. The metal film 62 may be divided into regions to which the light-emitting element 50 is bonded in a bonding process described later.

[0014] 1 and the process of preparing the evaluation substrate 60 shown in Fig. 2 can be carried out independently of each other, and the order of the processes is not limited. The light emitting element 50 and the evaluation substrate 60 may be prepared by fabrication, or may be prepared by purchasing or receiving from another person.

[0015] (Step of bonding the light emitting element to the evaluation substrate) As shown in Fig. 3, certain bonding conditions are determined, and the electrode 52 of the light-emitting element 50 is bonded to the metal film 62 of the evaluation substrate 60. For example, while the electrode 52 and the metal film 62 are heated, the light-emitting element 50 is pressed against the evaluation substrate 60 for a predetermined time. In this way, the light-emitting element 50 is bonded to the evaluation substrate 60. In the example shown in Fig. 3, a plurality of light-emitting elements 50 are bonded to one evaluation substrate 60. In this way, an evaluation sample 70 is produced.

[0016] The evaluation sample 70 includes one evaluation substrate 60 and a plurality of light-emitting elements 50, and the electrode 52 of each light-emitting element 50 is bonded to the metal film 62 of the evaluation substrate 60. As will be described later, the evaluation sample 70 may include light-emitting elements 50 with poor bonding.

[0017] In this specification, "bonding" means being electrically connected and mechanically connected. Furthermore, "bonding conditions" refers to a combination of options when performing bonding, including, for example, the heating temperature of the electrode 52 and the metal film 62, the pressing force and time for pressing the light emitting element 50 against the evaluation substrate 60, whether or not ultrasonic waves are applied, and, if ultrasonic waves are applied, the frequency and strength of the ultrasonic waves. The bonding conditions may include parameters other than those mentioned above, such as whether or not pretreatment such as plasma treatment is performed on the bonding surfaces.

[0018] (Step for determining the bonding state between the electrode and the metal film) As shown in FIG. 4, the electrode 52 overlapping the metal film 62 of the evaluation sample 70 is observed from the second surface 61b side of the light-transmitting substrate 61 of the evaluation substrate 60. At this time, the light-transmitting substrate 61 transmits visible light, and the metal film 62 also transmits visible light, so that the electrode 52 can be observed with visible light through the light-transmitting substrate 61 and the metal film 62. This observation can be performed, for example, by an optical microscope with coaxial illumination. The observation light may be visible light, and may be monochromatic light having a single wavelength or mixed color light such as white light. If the size of the light-emitting element 50 is sufficiently large, the observation may be performed with the naked eye or a magnifying glass.

[0019] The appearance of the electrode 52 through the light-transmitting substrate 61 and the metal film 62 (hereinafter simply referred to as "the appearance of the electrode 52") varies depending on the bonding state between the metal film 62 and the electrode 52. Therefore, by observing the electrode 52, the bonding state between the electrode 52 and the metal film 62 can be determined.

[0020] The effect of the bonding state between the metal film 62 and the electrode 52 on the appearance of the electrode 52 will be described below. 5 to 7 are diagrams showing the optical path and waveform of light in the evaluation sample. FIG. 8 is a diagram showing the relationship between the bonding state and the brightness of the appearance of the electrode.

[0021] As shown in FIG. 5, when the electrode 52 is in contact with the metal film 62, the light 80 incident from the second surface 61b of the light-transmitting substrate 61 is mainly reflected at the interface between the light-transmitting substrate 61 and the metal film 62. This reflected light is called light 80c. The light 80 is visible light. In this case, since there is substantially only one interface that reflects the light 80, interference of the light 80c reflected at the interface between the light-transmitting substrate 61 and the metal film 62 does not occur, and the appearance of the electrode 52 is observed through the light-transmitting substrate 61. The color of the electrode 52 at this time is determined as the "first color", the area where the electrode 52 appears to be the first color is determined as the "first area 81", and the bonding state between the electrode 52 and the metal film 62 at this time is determined as the "first state". The first state is a state in which the electrode 52 and the metal film 62 are in contact with each other.

[0022] As shown in FIG. 6, when the electrode 52 is slightly separated from the metal film 62, an air layer 71 is interposed between the electrode 52 and the metal film 62. In this case, the light 80 is mainly reflected at the interface between the metal film 62 and the air layer 71 and the interface between the air layer 71 and the electrode 52. Hereinafter, of the light 80 incident from the second surface 61b of the light-transmitting substrate 61, the light reflected at the interface between the metal film 62 and the air layer 71 is referred to as light 80a, the light reflected at the interface between the air layer 71 and the electrode 52 is referred to as light 80b, and the light obtained by combining the light 80a and the light 80b is referred to as light 80d. The distance at which the electrode 52 is slightly separated from the metal film 62 is, for example, a distance smaller than half the wavelength λ of the light 80. When the light 80 includes light of multiple wavelengths, the distance at which the electrode 52 is slightly separated is a distance smaller than at least half the wavelength λ of the light with the longest wavelength. Furthermore, since the metal film 62 is thin enough to transmit visible light, when an air layer 71 is interposed between the electrode 52 and the metal film 62, the light reflected at the interface between the translucent substrate 61 and the metal film 62 (i.e., light 80c shown in Figure 5) is very weak, and its effect can be essentially ignored.

[0023] In general, when light incident on material A is reflected on the surface of material B, the refractive index of material A, n A is the refractive index n of material B B When the refractive index is greater than n, the light is reflected without any phase change. A is the refractive index n BWhen the phase difference is smaller than n, the light is reflected with a phase shift of π. A >n B When the phase difference is 0, n A <n B When , the phase difference is π.

[0024] When the wavelength λ of light 80 is 500 nm or more, the refractive index n of gold Au is less than 1. For example, when the wavelength λ of light 80 is 517 nm, the refractive index of air n AIR is approximately 1, and the refractive index of gold, n Au is about 0.608, which is smaller than the refractive index of air, which is about 1. Therefore, n AIR >n Au Therefore, when light 80 incident from the metal film 62 is reflected at the interface with the air layer 71, the phase difference between light 80a and light 80b is π. When light 80 incident from the air layer 71 is reflected at the interface with the electrode 52, the phase difference between light 80a and light 80b is 0. On the other hand, when the wavelength λ of light 80 is 480 nm or less, the refractive index n of gold Au is greater than 1. For example, when the wavelength λ of light 80 is 450 nm, the refractive index of gold, n Au is greater than 1, and n AIR <n Au In this case, the phase difference between the light 80a and the light 80b is 0. Furthermore, when the light 80 incident from the air layer 71 is reflected at the interface with the electrode 52, the phase difference between the light 80a and the light 80b is π.

[0025] Therefore, when the electrode 52 is slightly separated from the metal film 62, specifically, when the distance d between the metal film 62 and the electrode 52 is sufficiently smaller than the wavelength λ of the light 80, the light 80a reflected at the interface between the metal film 62 and the air layer 71 and the light 80b reflected at the interface between the air layer 71 and the electrode 52 cancel each other out because the phase difference is about π, and the appearance of the electrode 52 appears dark. The color of the electrode 52 at this time is determined as the "second color". The brightness of the second color is lower than the brightness of the first color. The region where the electrode 52 appears to be the second color is determined as the "second region 82", and the bonding state between the electrode 52 and the metal film 62 at this time is determined as the "second state". The bonding strength between the metal film 62 and the electrode 52 in the second state is lower than that in the first state. For example, the second state is a state in which the electrode 52 and the metal film 62 are separated from each other by a sufficiently small distance (for example, a distance smaller than half the wavelength λ of the light 80).

[0026] 7, when the electrode 52 is far away from the metal film 62, specifically, when the distance d between the metal film 62 and the electrode 52 is greater than about half the wavelength λ of the light 80, interference fringes appear according to the relationship between the distance d and the wavelength λ. When the distance d satisfies the following mathematical formula 1, where m is a natural number, the phase difference between the light 80a and the light 80b is 0, so that the light 80a and the light 80b constructively interact with each other, and when the distance d satisfies the following mathematical formula 2, the phase difference between the light 80a and the light 80b is π, so that the light 80a and the light 80b destructively interact with each other.

[0027]

number

[0028]

number

[0029] In the appearance of the electrode 52, a region where interference fringes are observed is defined as a "third region 83." If the third region 83 is recognized, the third region 83 is determined to be in a "third state" in which the distance d between the electrode 52 and the metal film 62 is larger than in the second state.

[0030] The above determinations are summarized as shown in FIG. 8. As shown in FIG. 8, when the electrode 52 is in contact with the metal film 62 and the distance d is 0, a first region 81 of a first color appears on the exterior of the electrode 52. When the distance d is sufficiently smaller than the wavelength λ of the light 80, a second region 82 of a second color appears on the exterior of the electrode 52. The brightness of the second color is lower than the brightness of the first color. In FIG. 8, the brightness changes sharply at the boundary between the first region 81 and the second region 82, but when the first region 81 and the second region 82 are mixed microscopically, the brightness may appear to change continuously between the first region 81 and the second region 82 macroscopically. When the distance d is about half the wavelength λ or more, a third region 83 in which interference fringes 85 are recognized appears on the exterior of the electrode 52. Typically, the second region 82 appears around the first region 81, and the third region 83 appears around the second region 82.

[0031] 9(a) to 9(i) are schematic diagrams showing the results of observing the electrodes of the light-emitting element through a light-transmitting substrate. The electrode 52 of the evaluation sample 70 shown in Fig. 4 has a rectangular appearance, for example, as shown in Fig. 9(a) to (i). Fig. 9(a) to (i) are schematic diagrams based on photographs of the electrode 52 taken by an optical microscope through the light-transmitting substrate 61. Fig. 9(a) to (i) show the area ratios of the first region 81, the second region 82, and the third region 83. Note that Fig. 9(a) to (i) show only typical observation results and do not cover all patterns of the observation results.

[0032] 9(a) to 9(i), in the appearance of electrode 52, groove 53 does not contact metal film 62, so the region corresponding to groove 53 appears darker than other regions. Furthermore, if there is a recessed region such as a contact hole due to a device structure such as an electrode of a light-emitting element on the surface of electrode 52, this region also does not contact metal film 62 and appears dark. Hereinafter, the region of the appearance of electrode 52 excluding groove 53 and recessed regions such as contact holes will be referred to as the "electrode region." Hereinafter, the area of ​​the electrode region will be regarded as the area of ​​electrode 52.

[0033] FIG. 9(a) shows an example in which the entire electrode region is observed as a first region 81 that appears in a first color. In this case, the bonding state between the electrode 52 and the metal film 62 is determined to be the first state for the entire electrode 52. The area ratio of the first region 81 in the electrode region is about 100%. That is, in the example shown in FIG. 9(a), it can be determined that the electrode region is in the first state in which almost the entire electrode region is in contact with the metal film 62. The first state is a state in which a sufficient load is applied during bonding and the electrode 52 and the metal film 62 are bonded well. When almost the entire electrode region is in the first state, it is estimated that, for example, the shape of the electrode 52 before bonding is changed by pressing, so that it matches the shape of the metal film 62 and is bonded with almost no gaps.

[0034] FIG. 9(b) shows an example in which the vicinity of one corner of a rectangular electrode region is observed as a second region 82 that appears to be a second color that is lower in brightness than the first color, and the other regions are observed as a first region 81 that appears to be the first color. The area ratio of the first region 81 in the electrode region is about 78%, and the area ratio of the second region 82 is about 22%. That is, in this example, it can be determined that about 78% of the electrode region is in the first state in which it is in contact with the metal film 62, and the other about 22% is in the second state in which it is slightly separated from the metal film 62. The interface between the first region 81 and the second region 82 is curved so as to be convex toward the second region 82. The fact that the electrode region includes the first state and the second state suggests that, for example, the electrode 52 generally maintains the surface shape (unevenness) before bonding (pressing), and only a load was applied to the extent that only a part of the region (convex portion) is bonded. It is estimated that this causes the electrode 52 and the metal film 62 to be bonded more weakly than in the state shown in FIG. 9(a).

[0035] FIG. 9(c) shows an example in which the second region 82 is observed along two sides sharing one corner of a rectangular electrode region, and the other region is observed as the first region 81. The area ratio of the first region 81 in the electrode region is about 65%, and the area ratio of the second region 82 is about 35%. In this example, it is determined that about 65% of the electrode region, including one corner, is in the first state in which it is in contact with the metal film, and the remaining about 22% is in the second state in which it is slightly separated from the metal film 62. The interface between the first region 81 and the second region 82 is curved so as to be convex toward the second region 82 side. It is estimated that the state shown in FIG. 9(c) has a weaker bonding strength than the state shown in FIG. 9(b).

[0036] FIG. 9(d) is an example in which the boundary between the first region 81 and the second region 82 is observed as a straight line across two opposing sides of the rectangular electrode region. The area ratio of the first region 81 is about 60%, and the area ratio of the second region 82 is about 40%. In this example, it is determined that about 60% of the electrode region is in the first state in contact with the metal film, and about 40% is in the second state in which it is slightly separated from the metal film 62. As in the example shown in FIG. 9(d), when the boundary between the first region 81 and the second region 82 is straight, there is a possibility that a foreign object is caught or a load is tilted. In such a case, it may be possible to identify the occurring phenomenon by judging it together with the observation results of the surrounding light-emitting element 50.

[0037] 9(e) is an example in which a first region 81 is observed in the center of the electrode region, and a second region 82 is observed around the first region 81. The second region 82 surrounds the first region 81. The area ratio of the first region 81 in the electrode region is about 25%, and the area ratio of the second region 82 is about 75%. In this example, it is determined that about 25% of the center of the electrode region is in the first state in contact with the metal film, and the other about 75% is in the second state slightly separated from the metal film 62.

[0038] FIG. 9(f) shows an example in which a first region 81 is observed in the center of the electrode region, a second region 82 is observed around the first region 81, and a third region 83 is observed around the second region 82 as an interference pattern. The second region 82 surrounds the first region 81, and the third region surrounds the second region. The area ratio of the first region 81 in the electrode region is about 4%, the area ratio of the second region 82 is about 36%, and the area ratio of the third region 83 is about 60%. In this example, it is determined that about 4% of the center of the electrode region is in a first state in contact with the metal film 62, about 36% of the periphery is in a second state in which the metal film 62 is slightly separated from the metal film 62, and about 60% of the periphery is in a third state in which the metal film 62 is separated from the metal film 62 and the distance between the metal film 62 and the third state is greater than the second state.

[0039] FIG. 9(g) is an example in which a first region 81 is observed at one corner of a rectangular electrode region, a second region 82 is observed around the first region 81, and a third region 83 is observed around the second region 82. In other words, the first region 81, the second region 82, and the third region 83 are observed in this order from one corner to the other corner. The area ratio of the first region 81 in the electrode region is about 4%, the area ratio of the second region 82 is about 36%, and the area ratio of the third region 83 is about 60%. In this example, it is determined that about 4% of the corner in the electrode region is in a first state in contact with the metal film 62, about 36% of the periphery is in a second state in which it is separated from the metal film 62, and about 60% of the periphery is in a third state in which it is separated from the metal film 62 and the distance from the metal film 62 is greater than in the second state.

[0040] 9(h) is an example in which the second region 82 is observed over the entire electrode region. The area ratio of the second region 82 in the electrode region is approximately 100%. In this example, it can be determined that almost the entire electrode region is in the second state in which it is slightly separated from the metal film.

[0041] 9(i) is an example in which a second region 82 is observed in one corner of the electrode region, and a third region 83 is observed in another region. The area ratio of the second region 82 in the electrode region is about 30%, and the area ratio of the third region 83 is about 70%. In this example, it can be determined that about 30% of the electrode region is in the second state where it is slightly separated from the metal film 62, and about 70% is in the third state where it is separated from the metal film 62 by a larger distance.

[0042] Among the examples shown in Figs. 9(a) to (i), the example shown in Fig. 9(a) has the highest bonding strength between the electrode 52 and the metal film 62, and it is estimated that the bonding strength decreases from Fig. 9(b) to Fig. 9(g). In the examples shown in Figs. 9(f) and 9(g), the area ratios of the first region, the second region, and the third region are the same, but Fig. 9(f), in which the first region is observed in the center, is determined to have a higher bonding strength. In the examples shown in Figs. 9(h) and (i), it is estimated that the electrode 52 and the metal film 62 are not bonded. In the examples shown in Figs. 9(h) and (i), it is estimated that the electrode 52 and the metal film 62 are not bonded, but the light-emitting element 50 is held by the light-transmitting substrate 61 by van der Waals forces, atmospheric pressure, friction at the interface, and the like.

[0043] Next, the effects of this embodiment will be described. In this embodiment, in the process shown in Fig. 3, certain bonding conditions are determined and the electrode 52 of the light-emitting element 50 is bonded to the metal film 62 of the evaluation substrate 60. Then, in the process shown in Fig. 4, the bonding state between the electrode 52 and the metal film 62 is judged by observing the appearance of the electrode 52 through the light-transmitting substrate 61 and the metal film 62. As a result, it can be easily judged whether the bonding conditions are appropriate. By repeating this process, it is possible to efficiently search for suitable bonding conditions.

[0044] <Second embodiment> The second embodiment is an example of manufacturing a light emitting device using the results of the method for evaluating the bonding state of the light emitting element according to the first embodiment. FIG. 10 is a flowchart showing a method for manufacturing a light emitting device according to this embodiment. FIG. 11 is a cross-sectional view showing a method for manufacturing a light emitting device according to this embodiment. FIG. 12 is a bottom view showing the first member. FIG. 13 is a top view showing the second member. FIG. 14 is a cross-sectional view showing a method for manufacturing a light emitting device according to this embodiment. FIG. 15 is a partially enlarged cross-sectional view showing an area XV in FIG. 16 to 20 are cross-sectional views showing a method for manufacturing a light emitting device according to this embodiment. FIG. 21 is a top view showing the light emitting device according to this embodiment. FIG. 22 is a cross-sectional view taken along line XXII-XXII shown in FIG.

[0045] (Step of determining first and second bonding conditions) First, as shown in step S1 of Fig. 10, the method for evaluating the bonding state of the light-emitting element according to the first embodiment is carried out. That is, in the step shown in Fig. 3, bonding conditions are determined and the light-emitting element 50 is bonded to the evaluation substrate 60, and in the step shown in Fig. 4, the electrode 52 is observed through the light-transmitting substrate 61 and the metal film 62 to evaluate the bonding state. Then, the first embodiment is repeated with different bonding conditions to determine appropriate bonding conditions.

[0046] Specifically, the condition under which 70% to 100% of the area of ​​electrode 52 (area of ​​the electrode region) is in the first state is defined as the "first bonding condition," and the condition under which 0.1% to 5% of the area of ​​the electrode region is in the first state is defined as the "second bonding condition." Among the examples shown in Figures 9(a) to (i), the examples shown in Figures 9(a) and 9(b) correspond to the "first bonding condition," and the examples shown in Figures 9(f) and 9(g) correspond to the "second bonding condition."

[0047] (Preparing the first and second members) As shown in step S2 of FIG. 10, and in FIGS. 11 and 12, a first member 10 is prepared. The first member 10 includes one support substrate 11 and a plurality of first light-emitting elements 12. The plurality of first light-emitting elements 12 include a light extraction surface and a first bonding portion 13 disposed on a surface located opposite to the light extraction surface. The plurality of first light-emitting elements 12 are disposed on the support substrate 11 such that the light extraction surface faces the support substrate 11. Each of the first light-emitting elements 12 has a first bonding portion 13. The first bonding portion 13 contains gold. For example, at least the outermost surface of the first bonding portion 13 is made of gold. The light extraction surface of the first light-emitting element 12 is a surface from which light from the first light-emitting element 12 is mainly extracted.

[0048] The multiple first light-emitting elements 12 are arranged, for example, in a matrix on the first surface 11a of the support substrate 11. However, the arrangement of the first light-emitting elements 12 is not limited to a matrix and is arbitrary. The first light-emitting elements 12 are, for example, light-emitting diodes. Each of the first light-emitting elements 12 has, for example, two first bonding portions 13. The two first bonding portions 13 of the first light-emitting element 12 function as an anode electrode or a cathode electrode of the first light-emitting element 12. The first light-emitting element 12 preferably has the same configuration as the light-emitting element 50 in the first embodiment, and the first bonding portion 13 preferably has the same configuration as the electrode 52.

[0049] The support substrate 11 is, for example, a jig for transfer, and includes, for example, silicon, glass, or sapphire. The support substrate 11 preferably includes an adhesive layer on the first surface 11a. In this case, the first light-emitting element 12 is adhered to the adhesive first surface 11a of the support substrate 11. For example, the support substrate 11 may be a member in which an adhesive resin is provided on the surface of a sapphire substrate.

[0050] Meanwhile, a second member 20 is prepared as shown in Fig. 11 and Fig. 13. The second member 20 includes one mounting substrate 21 and a plurality of second bonding portions 22. The plurality of second bonding portions 22 are disposed on the mounting substrate 21. The second bonding portions 22 include gold. For example, at least the outermost surface of the second bonding portion 22 is made of gold. It is preferable that the outermost surface of the second bonding portion 22 is made of the same material as the outermost surface of the metal film 62 in the first embodiment.

[0051] The multiple second bonding portions 22 are arranged, for example, in a matrix on the second surface 21a of the mounting substrate 21. However, the arrangement of the second bonding portions 22 is not limited to a matrix and may be any arrangement. The multiple first bonding portions 13 and the multiple second bonding portions 22 are arranged at positions where one first bonding portion 13 faces one second bonding portion 22 when the first surface 11a of the support substrate 11 and the second surface 21a of the mounting substrate 21 are opposed to each other.

[0052] In the example shown in FIG. 11 and FIG. 13, the mounting board 21 includes an insulating base material 23 and conductive wiring 24 arranged on at least the surface of the base material 23. Here, the mounting board 21 has a plurality of openings 25 arranged in the base material 23 on the second surface 21a, and the wiring 24 is exposed in each of the plurality of openings 25. The area of ​​the surface of the wiring 24 that is not exposed in the opening 25 is covered by the base material 23. The second joint portion 22 is arranged on the second surface 21a of the mounting board 21, and is connected to the wiring 24 at the opening 25. The upper surface of the second joint portion 22 is approximately flat. Each of the second joint portions 22 is connected to each of the wiring 24 at the opening 25. Note that the upper surface of the second joint portion 22 is not limited to being approximately flat, and may have a recess reflecting the shape of the opening 25, for example.

[0053] (Step of bonding the first light emitting element to the mounting substrate under the second bonding condition) 10, 14, and 15, the first bonding portion 13 and the second bonding portion 22 are bonded under the second bonding condition determined in step S1 of Fig. 10. Then, the support substrate 11 is separated from the first light-emitting element 12. The first bonding portion 13 and the second bonding portion 22 are bonded by facing the first surface 11a of the support substrate 11 to the second surface 21a of the mounting substrate 21 and bringing the first bonding portion 13 into contact with the second bonding portion 22.

[0054] In the second bonding condition, for example, the first bonding portion 13 and the second bonding portion 22 are heated, and a load is applied in a direction in which they approach each other. In the second bonding condition, for example, it is preferable to heat the first bonding portion 13 and the second bonding portion 22 so that the temperature is 80 degrees or more and 200 degrees or less. The temperature in the second bonding condition is, for example, 140 degrees. In the second bonding condition, the load to be applied is, for example, preferably 10 MPa or more and less than 150 MPa, more preferably 10 MPa or more and less than 100 MPa, and even more preferably 10 MPa or more and less than 40 MPa. The load in the second bonding condition is, for example, 30 MPa. In the second bonding condition, the time for which the load is applied is, for example, preferably 0.1 seconds or more and 10 seconds or less. In the second bonding condition, the time for which the load is applied is, for example, 0.5 seconds.

[0055] Before the first bonding portion 13 is brought into contact with the second bonding portion 22, a plasma treatment may be performed on the first surface 11a of the support substrate 11 of the first member 10 on which the first light emitting element 12 is arranged, and on the second surface 21a of the mounting substrate 21 of the second member 20 on which the second bonding portion 22 is arranged. This activates the surfaces of the first bonding portion 13 and the second bonding portion 22, and can further improve the bonding between the first bonding portion 13 and the second bonding portion 22. Under the second bonding condition, it is preferable not to apply ultrasonic waves.

[0056] In this step, the first bonding portion 13 and the second bonding portion 22 are bonded to each other at a part of their surfaces while the first bonding portion 13 and the second bonding portion 22 generally maintain their shapes before bonding. For example, if a recess is formed on the upper surface of the second bonding portion 22 before bonding, a gap may remain between the recess of the first bonding portion 13 and the second bonding portion 22. By bonding the first bonding portion 13 and the second bonding portion 22 under the second bonding condition, the first bonding portion 13 and the second bonding portion 22 are connected, but the mechanical bonding strength is lower than the bonding strength under the first bonding condition. Hereinafter, such a state realized under the second bonding condition is referred to as a "temporary bonding state". As a result, the first light emitting element 12 is bonded to the mounting substrate 21. Then, the support substrate 11 is separated from the first light emitting element 12.

[0057] (Step of Determining the First Light Emitting Element) Next, as shown in step S4 of FIG. 10 and FIG. 16, power is supplied to the first light-emitting elements 12 via the mounting board 21, and the characteristics of the first light-emitting elements 12 are evaluated. The characteristic to be evaluated is, for example, the luminance of light emitted from the first light-emitting elements 12 when a voltage is applied to each of the first light-emitting elements 12. By evaluating such characteristics, the first light-emitting elements 12 bonded to the mounting board 21 can be classified into good products and bad products. For example, the first light-emitting elements 12 having a luminance equal to or higher than a reference value are determined as "good products", and the first light-emitting elements 12 having a luminance lower than the reference value are determined as "bad products". Hereinafter, the first light-emitting elements 12 determined as bad products are also referred to as "first light-emitting elements 12x". In addition, the second bonding portion 22 to which the first light-emitting elements 12 determined as bad products in the process of evaluating the characteristics of the first light-emitting elements 12 are bonded is referred to as "second bonding portion 22r".

[0058] (Step of removing defective first light emitting elements from a mounting substrate) Next, as shown in step S5 of Fig. 10, Fig. 17 and Fig. 18, the first bonding portion 13 of the first light-emitting element 12x determined to be defective is separated from the second bonding portion 22r of the mounting substrate 21, thereby removing the first light-emitting element 12x determined to be defective from the mounting substrate 21. For example, in this embodiment, the first light-emitting element 12x is heated by irradiating the first light-emitting element 12x with laser light 32. As a result, thermal stress is applied to the interface between the first bonding portion 13 and the second bonding portion 22r, and the first bonding portion 13 of the first light-emitting element 12x is detached from the second bonding portion 22r.

[0059] For example, the upper surface of the semiconductor laminate of the first light-emitting element 12x is irradiated with the laser light 32. When the first light-emitting element 12x includes a sapphire substrate and a semiconductor laminate disposed on the sapphire substrate, the laser light 32 is irradiated from the sapphire substrate side, and the laser light 32 is transmitted through the sapphire substrate and condensed on the upper surface of the semiconductor laminate. As a result, the semiconductor laminate on which the laser light 32 is condensed expands thermally, generating thermal stress between the second bonding portion 22r, and the bonding between the first bonding portion 13 and the second bonding portion 22r is released.

[0060] The first light emitting element 12x may be removed by, for example, adhering the first light emitting element 12x to an adhesive jig. The first light emitting element 12x may also be removed by sucking it with a suction device. The first light emitting element 12x may also be removed by blowing it off with an air blower or the like.

[0061] (Step of arranging the second light emitting element on the mounting board) Next, as shown in step S6 of Fig. 10 and Fig. 19, the second light-emitting element 15 is prepared. The second light-emitting element 15 is, for example, an element having the same structure as the first light-emitting element 12. The second light-emitting element 15 has a third bonding portion 16. The third bonding portion 16 contains gold. For example, the second light-emitting element 15 has two third bonding portions 16. The two third bonding portions 16 of the second light-emitting element 15 function as an anode electrode or a cathode electrode of the second light-emitting element 15.

[0062] Next, the second light emitting element 15 is held by the jig 34, and the second light emitting element 15 is placed in the area of ​​the mounting substrate 21 where the removed first light emitting element 12x was placed. This brings the third bonding portion 16 of the second light emitting element 15 into contact with the second bonding portion 22r. Then, the second light emitting element 15 is bonded to the mounting substrate 21. This bonding is preferably performed under the second bonding condition described above. Next, the jig 34 is separated from the second light emitting element 15.

[0063] Before the third bonding portion 16 of the second light-emitting element 15 is brought into contact with the second bonding portion 22r, the mounting substrate 21 and the second light-emitting element 15 may be subjected to a plasma treatment. This activates the surface of the second bonding portion 22r and the surface of the third bonding portion 16 of the second light-emitting element 15. At this time, the plasma penetrates between the mounting substrate 21 and the first light-emitting element 12, and the surfaces of the first bonding portion 13 of the first light-emitting element 12 determined to be a non-defective product and the second bonding portion 22 temporarily bonded to this first bonding portion are also activated. This allows the first bonding portion 13 and the second bonding portion 22 to be bonded more firmly in the step of bonding under the first bonding conditions described later.

[0064] Furthermore, before the third bonding portion 16 of the second light-emitting element 15 and the second bonding portion 22r are brought into contact with each other, the surface of the second bonding portion 22r may be irradiated with laser light. This makes it possible to remove metal residues or the like that remain on the surface of the mounting substrate 21 after the step of removing the first light-emitting element 12x determined to be a defective product from the mounting substrate 21. As a result, in the step of bonding under the first bonding condition described later, the third bonding portion 16 of the second light-emitting element 15 and the second bonding portion 22r can be bonded more firmly.

[0065] (Step of bonding the first light emitting element and the second light emitting element to the mounting substrate under the first bonding condition) 10 and 20, a load toward the mounting substrate 21 is applied to the first light-emitting element 12 and the second light-emitting element 15 using a jig 35. This bonds the first bonding portion 13 and the second bonding portion 22 in a temporarily bonded state, and bonds the third bonding portion 16 of the newly placed second light-emitting element 15 to the second bonding portion 22r to which the first bonding portion 13 of the removed first light-emitting element 12x had been bonded. The jig 35 may have the same configuration as the support substrate 11, or the support substrate 11 may be used again.

[0066] In this step, the first bonding portion 13 and the second bonding portion 22 and the third bonding portion 16 and the second bonding portion 22r are bonded under the first bonding condition determined in step S1 of FIG. 10. The first bonding condition has at least one of the temperature and the load higher than the second bonding condition. That is, the temperature of the first bonding condition is higher than the temperature of the second bonding condition, the load of the first bonding condition is higher than the load of the second bonding condition, or the temperature of the first bonding condition is higher than the temperature of the second bonding condition and the load of the first bonding condition is higher than the load of the second bonding condition. In addition, it is preferable that the time for applying the load under the first bonding condition is longer than the time for applying the load under the second bonding condition. Note that at least one of the load and temperature under the first bonding condition and the load and temperature under the second bonding condition may be the same, and the time for applying the load under the first bonding condition may be longer than the time for applying the load under the second bonding condition.

[0067] For example, under the first bonding condition, it is preferable that the temperature is 100 degrees or more and 300 degrees or less. For example, the temperature under the first bonding condition is 200 degrees. Moreover, under the first bonding condition, it is preferable that the load applied to the first bonding portion 13 and the second bonding portion 22 is 40 MPa or more and 200 MPa or less. Under the first bonding condition, it is preferable that the load applied is 120 MPa, for example. Furthermore, under the first bonding condition, it is preferable that the bonding time is 1 second or more and 60 seconds or less. Under the first bonding condition, the bonding time is, for example, 30 seconds. Note that, under the first bonding condition, it is preferable that ultrasonic waves are not applied, as under the second bonding condition. Moreover, under the first bonding condition, it is not necessary to apply a load.

[0068] As a result, the first bonding portion 13 and the second bonding portion 22 are bonded more firmly, and the third bonding portion 16 and the second bonding portion 22r are bonded. At this time, the two bonding portions bonded to each other are integrated, and most of the interface disappears. Also, if a gap occurs at the interface, most of the gap disappears. As a result, the third bonding portion 16 and the second bonding portion 22r are electrically bonded, and the mechanical bonding strength between the first bonding portion 13 and the second bonding portion 22 and the mechanical bonding strength between the third bonding portion 16 and the second bonding portion 22r become higher than in the temporary bonding state. Hereinafter, such a state realized by the first bonding condition is referred to as a "main bonding state." By bonding under the first bonding condition, the first light-emitting element 12 and the second light-emitting element 15 determined to be non-defective are firmly bonded to the mounting board 21. Next, the jig 35 is separated from the first light-emitting element 12 and the second light-emitting element 15. In this manner, the light-emitting device 1 is manufactured.

[0069] In addition, if all of the first light-emitting elements 12 are determined to be good products in the evaluation process of the characteristics of the first light-emitting elements 12 shown in Figure 16, the removal process of the first light-emitting elements 12x shown in Figures 17 and 18 and the placement process of the second light-emitting elements 15 shown in Figure 19 are not performed, and a bonding process under the first bonding conditions shown in Figure 20 is carried out.

[0070] (Light emitting device) 21 and 22, the light emitting device 1 according to this embodiment includes a mounting substrate 21, a first light emitting element 12 on which a fourth bonding portion 36 is arranged, and a second light emitting element 15 on which the fourth bonding portion 36 is arranged. The mounting substrate 21 includes an insulating base material 23 and a plurality of conductive wirings 24 arranged in the base material 23. The first light emitting element 12 and the second light emitting element 15 are arranged on a second surface 21a of the mounting substrate 21, for example, in a matrix form.

[0071] The first light emitting element 12 and the second light emitting element 15 are, for example, elements having the same structure, such as light emitting diodes. The first light emitting element 12 and the second light emitting element 15 are electrically and mechanically joined to the wiring 24 of the mounting substrate 21 via the fourth joint 36. The fourth joint 36 is formed by integrating the first joint 13 and the second joint 22, or the third joint 16 and the second joint 22r. Therefore, the fourth joint 36 contains gold.

[0072] In this embodiment, as a first bonding step, in the step shown in FIG. 14 and FIG. 15, the first bonding portion 13 of the plurality of first light-emitting elements 12 is bonded to the second bonding portion 22 of the mounting substrate 21, and then, in the step shown in FIG. 16, a step of evaluating the characteristics of each of the first light-emitting elements 12 is performed. Next, the first light-emitting element 12x determined to be a defective product in the step of evaluating the characteristics of the first light-emitting element 12 is removed in the step shown in FIG. 17 and FIG. 18. Next, in the step shown in FIG. 19, the second light-emitting element 15 is placed in the area of ​​the mounting substrate 21 after the first light-emitting element 12x is removed. Then, as a second bonding step, in the step shown in FIG. 20, the first bonding portion 13 of the first light-emitting element 12 determined to be a non-defective product is bonded to the second bonding portion 22, and the newly placed second light-emitting element 15 is bonded to the second bonding portion 22r to which the first light-emitting element 12x determined to be a defective product was bonded.

[0073] As a result, in the first bonding step, the multiple first light-emitting elements 12 are connected to the mounting substrate 21 at once, and the characteristics of the multiple first light-emitting elements 12 can be evaluated via the mounting substrate 21. Then, after removing only the first light-emitting elements 12x determined to be defective as a result of evaluating the characteristics of the first light-emitting elements 12, the second light-emitting element 15 is placed in the region of the mounting substrate 21 from which the first light-emitting elements 12x have been removed. Thereafter, by performing the second bonding step, the non-defective first light-emitting elements 12 are bonded to the mounting substrate 21, and new second light-emitting elements 15 are also bonded to the mounting substrate 21. As a result, the defective first light-emitting elements 12x can be efficiently replaced, and the productivity of the light-emitting device 1 is improved.

[0074] In this embodiment, the first bonding step is performed under the second bonding condition, and the second bonding step is performed under the first bonding condition. The first bonding condition has a higher bonding strength than the second bonding condition. Specifically, the second bonding condition is a bonding condition in which the first bonding portion 13 is connected to the second bonding portion 22, but the mechanical bonding strength is a temporary bonding state lower than the actual bonding state. Therefore, it is easy to remove the first light-emitting element 12x determined to be defective while evaluating the characteristics of the first light-emitting element 12. On the other hand, the first bonding condition is a bonding condition in which the actual bonding state is higher than the temporary bonding state. This allows the first light-emitting element 12 and the second light-emitting element 15 (that is, the second light-emitting element 15 arranged in the area where the first light-emitting element 12x determined to be defective has been removed) to be bonded to the mounting substrate 21 under the first bonding condition in which the actual bonding state is achieved.

[0075] In this embodiment, the first and second bonding conditions can be determined in advance with high accuracy by the method according to the first embodiment, which can reduce the occurrence of bonding defects in the first bonding step shown in Figs. 14 and 15 and the second bonding step shown in Fig. 20.

[0076] Furthermore, in this embodiment, by heating the first light-emitting element 12x determined to be defective, thermal stress is generated between the first bonding portion 13 of the first light-emitting element 12x and the second bonding portion 22r of the mounting substrate 21. This makes it possible to release the bonding between the first bonding portion 13 and the second bonding portion 22r while suppressing damage to the mounting substrate 21. Also, by irradiating the first light-emitting element 12x with laser light 32, it is possible to precisely heat only the first light-emitting element 12x determined to be defective among the multiple first light-emitting elements 12.

[0077] Furthermore, in this embodiment, the first bonding portion 13, the second bonding portion 22, and the third bonding portion 16 contain gold. In a first bonding step, a portion of the first bonding portion 13 containing gold and a portion of the second bonding portion 22 containing gold are bonded together. For example, the outermost surface of the first bonding portion 13 made of gold and the outermost surface of the second bonding portion 22 made of gold are bonded together. Thereafter, thermal stress is generated at the bonding interface between the first bonding portion 13 and the second bonding portion 22 to remove the first light-emitting element 12x determined to be defective.

[0078] In the first bonding step, for example, when the first bonding portion 13 and the second bonding portion 22 are bonded via a bonding material, there is a risk that residues of the bonding material remain on the surface of the second bonding portion 22r after removing the first light-emitting element 12x determined to be defective. In addition, in the first bonding step, for example, when the first bonding portion 13 and the second bonding portion 22 are bonded by forming plating, there is a risk that residues of the plating remain on the surface of the second bonding portion 22r after removing the first light-emitting element 12x determined to be defective. In this case, when the second light-emitting element 15 is bonded to the second bonding portion 22r on which the first light-emitting element 12x was placed, the bonding strength between the second light-emitting element 15 and the second bonding portion 22r may be reduced due to residues of the bonding material or plating material. In bonding via a bonding material or bonding by forming plating, it is difficult to remove the bonding material or plating material after bonding.

[0079] In this embodiment, in the process of removing the first light-emitting element 12x determined to be defective, the bonding is released at the interface between the gold-containing portion of the first bonding portion 13 and the gold-containing portion of the second bonding portion 22, so that residue is unlikely to remain on the surface of the second bonding portion 22. Therefore, when the second light-emitting element 15 is bonded to the second bonding portion 22r on which the first light-emitting element 12x was placed, no residue is present between the second light-emitting element 15 and the second bonding portion 22r, so that the bonding strength can be increased. In the second bonding process, the gold-containing portion of the third bonding portion 16 is bonded to the gold-containing portion of the second bonding portion 22r. When the second light-emitting element 15 is bonded to the second bonding portion 22, there is no need to place a bonding material or form a plating, so that the process can be simplified while improving the bonding accuracy.

[0080] In the present embodiment, ultrasonic waves are not applied in the first and second bonding steps, which reduces misalignment of the first light-emitting element 12 and the second light-emitting element 15 that occurs when bonding the first light-emitting element 12 and the second light-emitting element 15 to the mounting substrate 21.

[0081] After the third bonding portion 16 of the second light-emitting element 15 is brought into contact with the second bonding portion 22r of the mounting substrate 21, a process of evaluating the characteristics of the second light-emitting element 15 via the mounting substrate 21 may be performed. If the second light-emitting element 15 is determined to be defective by this process, the second light-emitting element 15 may be removed by a method similar to that used to remove the first light-emitting element 12x. At this time, before evaluating the characteristics of the second light-emitting element 15, the third bonding portion 16 may be bonded under a second bonding condition, and the bonding state between the third bonding portion 16 and the second bonding portion 22r may be a temporary bonding state.

[0082] <Third embodiment> Similarly to the second embodiment, the third embodiment is an example of manufacturing a light emitting device using the results of the evaluation method of the bonding state of the light emitting element according to the first embodiment. However, unlike the second embodiment, the third embodiment does not perform temporary bonding and characteristic evaluation of the light emitting element. FIG. 23 is a flowchart showing a method for manufacturing a light emitting device according to this embodiment.

[0083] (Step of determining first bonding conditions) 23, the method for evaluating the bonding state of the light-emitting element according to the first embodiment is performed to determine a first bonding condition. As described above, the first bonding condition is a condition under which 70% to 100% of the area of ​​the electrode 52 (area of ​​the electrode region) is in the first state.

[0084] (Preparing the first and second members) Next, as shown in step S12 of Fig. 23, the first member 10 and the second member 20 are prepared. This method is similar to that in the second embodiment.

[0085] (Step of bonding a light emitting element to a mounting substrate under a first bonding condition) Next, as shown in step S13 of Fig. 23, the light emitting element is bonded to the mounting substrate. This bonding is performed under the first bonding conditions determined in step S11. The configuration of the light emitting element in this embodiment is the same as the configuration of the first light emitting element 12 in the second embodiment. In this manner, the light emitting device according to this embodiment is manufactured.

[0086] In this embodiment, the method according to the first embodiment is carried out in step S11 in Fig. 23 to determine the first bonding condition, and the light emitting element is bonded to the mounting substrate using this first bonding condition in step S13 in Fig. 23. This allows the first bonding condition to be determined in advance with high accuracy, and the occurrence of bonding defects can be suppressed. The method and effects of this embodiment other than those described above are the same as those of the second embodiment.

[0087] The above-described embodiments are examples of the present invention, and the present invention is not limited to these embodiments. For example, the present invention also includes the addition, deletion, or modification of some components or steps in the above-described embodiments.

[0088] The present invention includes the following aspects.

[0089] (Appendix 1) preparing a light emitting element having a semiconductor laminate having an upper surface and a lower surface opposite to the upper surface, and an electrode disposed on the lower surface of the semiconductor laminate; preparing an evaluation substrate in which a metal film is disposed on a first surface of a light-transmitting substrate having a first surface and a second surface opposite to the first surface; bonding the electrode of the light-emitting element to the metal film of the evaluation substrate; a step of determining a bonding state between the electrode and the metal film by observing the electrode overlapping the metal film from the second surface side of the light-transmitting substrate; A method for evaluating a bonding state of a light-emitting element comprising the steps of:

[0090] (Appendix 2) The method for evaluating the bonding state of a light-emitting element described in Appendix 1, wherein the determining step determines a first region in which the electrode appears to be a first color as a first state, and determines a second region in which the electrode appears to be a second color that is lower in brightness than the first color as a second state having a bonding strength lower than the first state.

[0091] (Appendix 3) A method for evaluating the bonding state of a light-emitting element described in Appendix 2, in which, in the determining step, the first state is determined as a state in which the electrode and the metal film are in contact, and the second state is determined as a state in which the electrode and the metal film are separated.

[0092] (Appendix 4) A method for evaluating the bonding state of a light-emitting element as described in Appendix 3, in which, if a third region in which interference fringes are observed is found in the determining step, the third region is determined to be in a third state in which the distance between the electrode and the metal film is greater than in the second state.

[0093] (Appendix 5) determining a first bonding condition such that 70% or more and 100% or less of the area of ​​the electrode is in the first state by the method for evaluating the bonding state of a light-emitting element according to any one of Supplementary Notes 2 to 4; bonding the light emitting element to a mounting substrate under the first bonding condition; A method for manufacturing a light emitting device comprising the steps of:

[0094] (Appendix 6) determining a first bonding condition under which 70% to 100% of the area of ​​the electrode is in the first state, and a second bonding condition under which 0.1% to 5% of the area of ​​the electrode is in the first state, by a method for evaluating a bonding state of a light-emitting element according to any one of Supplementary Notes 2 to 4; bonding a first light emitting element to a mounting substrate under the second bonding condition; evaluating characteristics of the first light emitting element through the mounting substrate to determine whether the first light emitting element is a non-defective product or a defective product; removing the first light emitting element determined to be a defective product from the mounting substrate; arranging a second light-emitting element in an area of ​​the mounting board after the first light-emitting element determined to be defective has been removed; bonding the first light emitting element and the second light emitting element determined to be non-defective under the first bonding condition to the mounting substrate; A method for manufacturing a light emitting device comprising the steps of:

[0095] (Appendix 7) 7. The method for manufacturing a light emitting device according to claim 6, wherein in the step of arranging the second light emitting element, the second light emitting element is bonded to the mounting substrate under the second bonding condition. [Industrial Applicability]

[0096] The present invention can be used, for example, as a headlamp for a vehicle and a light source for a display device. [Explanation of symbols]

[0097] 1: Light emitting device 10: First member 11: Support substrate 11a: Front page 12, 12x: first light-emitting element 13: 1st joint 15: Second light-emitting element 16: Third joint 20: Second member 21: Mounting board 21a: 2nd side 22, 22r: 2nd joint 23: Base material 24: Wiring 25: Opening 32: Laser light 34: Jig 35: Jig 36: 4th joint 50: Light emitting element 51: Semiconductor laminate 51a:Top surface 51b: Bottom surface 52: Electrode 52b: Bottom surface 53: Groove 60: Evaluation board 61: Translucent substrate 61a: 1st page 61b: 2nd side 62: Metal film 70: Evaluation sample 71: Air layer 80, 80a, 80b, 80c, 80d: light 85: Interference fringes d: distance

Claims

1. preparing a light emitting element having a semiconductor laminate having an upper surface and a lower surface opposite to the upper surface, and an electrode disposed on the lower surface of the semiconductor laminate; preparing an evaluation substrate in which a metal film is disposed on a first surface of a light-transmitting substrate having a first surface and a second surface opposite to the first surface; bonding the electrode of the light-emitting element to the metal film of the evaluation substrate; a step of determining a bonding state between the electrode and the metal film by observing the electrode overlapping the metal film from the second surface side of the light-transmitting substrate; A method for evaluating a bonding state of a light-emitting element comprising the steps of:

2. 2. The method for evaluating the bonding state of a light-emitting element as described in claim 1, wherein the determining step determines a first region in which the electrode appears to be a first color as a first state, and a second region in which the electrode appears to be a second color that is less bright than the first color as a second state having a bonding strength lower than that of the first state.

3. 3. The method for evaluating the bonding state of a light-emitting element according to claim 2, wherein, in the determining step, the first state is determined as a state in which the electrode and the metal film are in contact, and the second state is determined as a state in which the electrode and the metal film are separated.

4. 4. The method for evaluating the bonding state of a light-emitting element as described in claim 3, wherein, if a third region in which interference fringes are observed is found in the determining process, the third region is determined to be in a third state in which the distance between the electrode and the metal film is greater than in the second state.

5. determining a first bonding condition such that 70% or more and 100% or less of the area of ​​the electrode is in the first state by the method for evaluating the bonding state of a light-emitting element according to any one of claims 2 to 4; bonding the light emitting element to a mounting substrate under the first bonding condition; A method for manufacturing a light emitting device comprising the steps of:

6. A step of determining a first bonding condition under which 70% to 100% of the area of ​​the electrode is in the first state, and a second bonding condition under which 0.1% to 5% of the area of ​​the electrode is in the first state, by the method for evaluating the bonding state of a light-emitting element according to any one of claims 2 to 4; bonding a first light emitting element to a mounting substrate under the second bonding condition; a step of evaluating characteristics of the first light emitting element through the mounting substrate to determine whether the first light emitting element is a non-defective product or a defective product; removing the first light emitting element determined to be a defective product from the mounting substrate; arranging a second light-emitting element in an area of ​​the mounting board after the first light-emitting element determined to be defective has been removed; bonding the first light emitting element and the second light emitting element determined to be non-defective under the first bonding condition to the mounting substrate; A method for manufacturing a light emitting device comprising the steps of:

7. The method for manufacturing a light emitting device according to claim 6 , wherein in the step of arranging the second light emitting element, the second light emitting element is bonded to the mounting substrate under the second bonding condition.

Citation Information

Patent Citations

  • Image forming element and manufacturing method

    JP2020074005A