Composite substrate
By using SiC or AlN as a support substrate for a thin InP substrate, the composite substrate addresses heat dissipation issues, enhancing thermal conductivity and reducing defects for semiconductor applications.
Patent Information
- Application Number
- JP2023056664
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-30
- Publication Date
- 2024-10-11
AI Technical Summary
The composite substrate in existing technologies using a silicon substrate as a support for an indium phosphide substrate faces issues with heat dissipation due to both materials having low thermal conductivity.
The composite substrate is redesigned with an indium phosphide substrate supported by a SiC or AlN support substrate, with the InP substrate thickness of 10 μm or less, and optionally a bonding layer of SiO2, to enhance thermal conductivity and reduce warping and cracking during epitaxial processes.
This configuration improves heat dissipation and reduces warping and cracking, making the composite substrate suitable for semiconductor devices like laser light sources and optical modulators.
Smart Images

Figure 2024143786000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a composite substrate. [Background technology]
[0002] Conventionally, InP (indium phosphide) has been known as a semiconductor material suitable for laser light sources, optical modulators, photodiodes, driver ICs, etc. used in optical communications. Patent Document 1 describes a composite substrate having an indium phosphide substrate, a barrier layer formed directly on the indium phosphide substrate, and a silicon substrate, in which the barrier layer and the silicon substrate are directly bonded to each other, and an amorphous layer is formed at the bonding interface between the barrier layer and the silicon substrate. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] Patent Publication No. 2023-500 Summary of the Invention [Problem to be solved by the invention]
[0004] The composite substrate of Patent Document 1 has a silicon substrate as a support substrate, and an indium phosphide substrate bonded onto the support substrate. However, both the indium phosphide substrate and the silicon substrate have low thermal conductivity, and therefore the composite substrate of Patent Document 1 has a problem with heat dissipation.
[0005] The present invention has been made in view of the above, and a main object of the present invention is to improve the heat dissipation properties of a composite substrate using an indium phosphide substrate. [Means for solving the problem]
[0006] A composite substrate according to the present invention comprises an InP substrate made of an InP material and a support substrate supporting the InP substrate, the support substrate being made of SiC or AlN, and the InP substrate having a thickness of 10 μm or less. Effect of the Invention
[0007] According to the present invention, it is possible to improve the heat dissipation properties of a composite substrate using an indium phosphide substrate. [Brief description of the drawings]
[0008] [Figure 1] 1 is a schematic cross-sectional view showing a schematic configuration of a composite substrate according to a first embodiment of the present invention. [Diagram 2] FIG. 4 is a schematic cross-sectional view showing a schematic configuration of a composite substrate according to a second embodiment of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0009] Hereinafter, the embodiments of the present invention will be described with reference to the drawings, but the present invention is not limited to these embodiments. In addition, in order to clarify the description, the width, thickness, shape, etc. of each part may be shown more diagrammatically than in the embodiment, but these are merely examples and do not limit the interpretation of the present invention.
[0010] (First embodiment) 1 is a schematic cross-sectional view showing a schematic configuration of a composite substrate according to a first embodiment of the present invention. The composite substrate 100 in this embodiment is used as a material for semiconductor elements mounted on various semiconductor devices (laser light sources, optical modulators, photodiodes, driver ICs, etc.) constituting, for example, an optical transceiver, and has a structure in which an InP substrate 10 is bonded to a support substrate 30.
[0011] The InP substrate 10 is made of InP (indium phosphide). Here, the thickness of the InP substrate 10 is 10 μm or less. More preferably, it is 5 μm or less, and further preferably, it is 1 μm or less. The thinner the InP substrate 10, the more the occurrence of cracks can be suppressed in the epitaxial step of forming an epitaxial layer on the InP substrate 10. Therefore, it is preferable to form the InP substrate 10 as thin as possible within the range that can be processed.
[0012] Moreover, the surface roughness Ra of the InP substrate 10 is preferably, for example, 1 nm or less. The smaller the surface roughness Ra, the more likely it is that cracks will be prevented from occurring during the epitaxial process. Therefore, it is preferable to form the surface of the InP substrate 10 as smoothly as possible within the scope of processability.
[0013] The support substrate 30 supports the InP substrate 10. The material of the support substrate 30 preferably has a high thermal conductivity from the viewpoint of heat dissipation, and has a thermal expansion coefficient as close as possible to that of the InP substrate 10 at the temperature (approximately 500°C to 700°C) at which the epitaxial process is carried out in order to suppress the occurrence of warping or cracks in the epitaxial process. Specifically, the material constituting the support substrate 30 may be, for example, SiC (silicon carbide) or AlN (aluminum nitride).
[0014] The thickness of the support substrate 30 is, for example, 50 μm to 1 mm, preferably 100 μm to 800 μm, and more preferably 200 μm to 600 μm. The thicker the support substrate 30, the more warping and cracking can be suppressed, but if the support substrate 30 is too thick, the cost increases. Therefore, the thickness of the support substrate 30 can be appropriately set from the viewpoint of the balance between these factors.
[0015] The magnitude of warpage of composite substrate 100 after the epitaxial process is preferably 100 μm or less when the wafer size has a diameter of, for example, 2 inches. In composite substrate 100, the thicknesses of InP substrate 10 and supporting substrate 30 can be set so as to satisfy this condition.
[0016] The support substrate 30 may be made of a single crystal or a polycrystal. For example, when the support substrate 30 is made of a single crystal of SiC, the crystal polytype is typically 3C, 4H, or 6H, and 4H is more preferable. This can further suppress the occurrence of cracks.
[0017] The composite substrate 100 may be manufactured in any suitable shape. In one embodiment, the composite substrate 100 may be manufactured in the form of a so-called wafer. The size of the composite substrate 100 may be appropriately set depending on the purpose, for example, with the diameter of the wafer (substrate) being between 2 inches and 6 inches.
[0018] In the composite substrate 100 of this embodiment, the InP substrate 10 and the support substrate 30 are bonded to each other by direct bonding. For example, the bonding surfaces of the InP substrate 10 and the support substrate 30 are each subjected to an activation treatment, and then the bonding surfaces are directly bonded to each other, thereby forming the composite substrate 100 having the structure of FIG. 1. Examples of the activation treatment method include a method of irradiating each bonding surface with a neutral atomic beam at room temperature to activate and directly bond the surfaces, and a method of irradiating each bonding surface with plasma to activate (make hydrophilic) the surfaces and directly bond the surfaces (plasma activation bonding). In this embodiment, direct bonding using a neutral atomic beam is preferred.
[0019] Second Embodiment Fig. 2 is a schematic cross-sectional view showing a schematic configuration of a composite substrate according to a second embodiment of the present invention. A composite substrate 110 in this embodiment has a structure in which a bonding layer 20 is disposed between an InP substrate 10 and a support substrate 30, and the InP substrate 10 and the support substrate 30 are bonded to each other via the bonding layer 20, in comparison with the composite substrate 100 in Fig. 1 described in the first embodiment. In other respects, the composite substrate 110 is similar to the composite substrate 100 described in the first embodiment.
[0020] The material of the bonding layer 20 is, for example, any metal or SiO2. When the composite substrate 110 is used as a material for a laser light source, an optical modulator, or the like, it is preferable to form the bonding layer 20 using a material with a low refractive index such as SiO2 from the viewpoint of the light confinement effect. In addition, from the viewpoint of heat dissipation, it is preferable to make the thickness of the bonding layer 20 as thin as possible.
[0021] The bonding layer 20 can be formed on the supporting substrate 30 by any appropriate method. For example, the bonding layer 20 can be formed by physical vapor deposition such as sputtering, vacuum deposition, or ion beam assisted deposition (IAD), chemical vapor deposition, or atomic layer deposition (ALD), etc. The bonding layer 20 can be formed at room temperature (25°C) to 300°C, for example.
[0022] In the composite substrate 110 of the present embodiment, the InP substrate 10 and the support substrate 30 are bonded to each other via a bonding layer 20. For example, the bonding layer 20 is formed on the support substrate 30, and the bonding surfaces of the InP substrate 10 and the bonding layer 20 are each subjected to a plasma activation process, and then the bonding surfaces are directly bonded to each other, thereby forming the composite substrate 110 having the structure shown in FIG.
[0023] According to the embodiment of the present invention described above, the composite substrate 100, 110 has a structure in which the InP substrate 10 is supported by the support substrate 30 formed using SiC or AlN as a material. SiC and AlN are materials that have a thermal conductivity close to that of InP and a thermal expansion coefficient close to that of InP near the temperature at which the epitaxial process is performed. Therefore, it is possible to improve heat dissipation and suppress the occurrence of warping and cracks during the epitaxial process. Therefore, it is possible to provide the composite substrate 100, 110 that is suitable for use as a material for laser light sources, optical modulators, photodiodes, driver ICs, etc. used in optical communications.
[0024] The present invention is not limited to the above-described embodiment, and can be implemented using any components without departing from the spirit of the present invention.
[0025] The above-mentioned embodiments and modifications are merely examples, and the present invention is not limited to these contents as long as the characteristics of the invention are not impaired. In addition, although various embodiments and modifications have been described above, the present invention is not limited to these contents. Other aspects that are conceivable within the scope of the technical idea of the present invention are also included in the scope of the present invention. [Explanation of symbols]
[0026] 10: InP substrate 20: Bonding layer 30: Support substrate 100, 110: Composite board
Claims
1. An InP substrate made of an InP material; a support substrate supporting the InP substrate; the material of the support substrate is SiC or AlN; A composite substrate, wherein the thickness of the InP substrate is 10 μm or less.
2. 2. The composite substrate according to claim 1 , A composite substrate, wherein the thickness of the InP substrate is 5 μm or less.
3. The composite substrate according to claim 2, A composite substrate, wherein the thickness of the InP substrate is 1 μm or less.
4. The composite substrate according to claim 1 , The InP substrate and the support substrate are bonded to each other by direct bonding.
5. The composite substrate according to claim 1 , a bonding layer disposed between the InP substrate and the support substrate; The InP substrate and the support substrate are bonded to each other via the bonding layer.
Citation Information
Patent Citations
Composite substrate
JP2023000500A