Powdered silica production device and production method for short-time evaporation and solidification
The described method and equipment address the inefficiencies of instant coffee production by rapidly evaporating and solidifying liquefied silicon, achieving rapid production of water-soluble silica suitable for health foods.
Patent Information
- Application Number
- JP2023068872
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-04-03
- Publication Date
- 2024-10-16
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Existing methods for producing instant coffee require large-scale equipment, significant man-hours, and a long manufacturing period, limiting convenience and efficiency.
A method and equipment for producing highly water-soluble powdered silica involves a granulation/drying device that instantly evaporates and solidifies liquefied silicon at high temperatures, utilizing a six-unit system to control temperature and airflow for rapid production.
The method enables the production of water-soluble silica in a short time, suitable for use as a health food with improved absorbency.
Smart Images

Figure 2024147470000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to an apparatus and method for producing water-soluble powdered silica from liquid silicon. [Background technology]
[0002] Generally, as a method for obtaining granules from a liquid, there is a known technique for obtaining powdered instant coffee (Patent Documents 1 and 2).
[0003] Normally, coffee has a much better flavor when freshly brewed, but is less convenient in terms of the work of brewing it, waste disposal, etc. To improve this convenience, instant coffee and the like have been developed and are widely used, but in recent years, instant coffee with added value from a perspective other than convenience has been proposed.
[0004] However, these instant coffee manufacturing methods require large-scale equipment, a great deal of labor, and a long manufacturing period. [Prior art documents] [Patent documents]
[0005] [Patent Document 1] Patent Publication No. 2007-54057 [Patent Document 2] Patent Publication JP 2007-54058 A Problem to be Solved by the Invention
[0006] In order to solve these problems, the present invention has been made in consideration of the above-mentioned circumstances of the prior art, and has an object to provide a method and equipment for obtaining powdered silica having high water solubility in the shortest possible time. Summary of the Invention [Means for solving the problem]
[0007] The present invention is a method for producing powdered silica, which includes a granulation and drying device (1), which is the main part that instantly evaporates and solidifies liquefied silicon, and heats the silicon to a high temperature of 257°C or higher through equipment consisting of six units: a raw material input unit (2), an air intake unit for heating the device (3), an air intake and heating unit for the classifier (4), an exhaust unit (5), and a finished product recovery unit (6). The equipment is then used to evaporate and solidify the silicon in a short period of time.
[0008] A raw material input section (2) for the first step, in which water-soluble silicon (raw material) is input into a raw material tank (21) and sent to the granulation and drying apparatus (1) through a supply pump (22); This device takes in outside air and keeps the temperature inside the granulation and drying device (1) at 257°C. an air intake section (3) for heating the equipment in the second step, which blows air taken in from the intake fan (32) through a coarse dust filter (31) into an air heater (33) to heat the air to a high temperature of 257°C or higher and sends the air to the granulation drying equipment section (1); The classifier (61) in the finished product recovery section (6) is an air blowing section for returning silicon particles smaller than expected to the granulation and drying device (1), The third process is the classifier air intake and heating section (4), in which outside air is taken in by an intake fan, heated to 257°C or higher by an air heater, and the heated air is purified by a filter and sent to the classifier. This is the part that discharges air whose temperature has dropped below the specified level. an exhaust section (5) for the fourth step, which allows the air accumulated in the upper part of the granulation and drying device section (1) due to the force of spray from the granulation and drying device section (1) to be exhausted in a clean state to the outside through an exhaust fan (52) via a bag filter (51); This is the part that collects the granulated silicon (product) after spraying. The granulated silicon is sucked into the classifier (61) and simultaneously This granulation and drying apparatus is characterized by being composed of six units, including a finished product recovery section (6) in the fifth process, in which air is sprayed from below to collect particles within a specified size range (100 μm or more and less than 250 μm) and place them directly into a finished product tank (62). Effect of the Invention
[0009] The water-soluble silica of the present invention can be instantly liquefied and can be used as a health food with good absorbency. [Brief description of the drawings]
[0010] [Figure 1] 1 is a flow chart illustrating the manufacturing process of the instant coagulation component preservation method of the present invention. [Diagram 2] 1 is a schematic diagram of a manufacturing apparatus for the instantaneous solidification component preservation method of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0014] Hereinafter, an embodiment of the present invention will be described in detail with reference to the accompanying drawings (see FIG. 1 and FIG. 2). The present invention relates to a granulation and drying device section (1), Heated air is charged and adjusted in the equipment heating air suction section (3) to stabilize the temperature inside the granulation dryer section (1). After the temperature has stabilized, water-soluble silicon is sprayed in a spray form from the raw material input section (2) and evaporated instantly inside the chamber. Approximately 10 seconds after being sprayed inside the granulation dryer section (1), the water-soluble silicon solidifies and is collected from the finished product recovery air suction section (3). Granules smaller than the specified size are blown back into the granulation dryer section (1) and spray drying is repeated again until the specified size is reached. The excess air inside the chamber is sucked in through the exhaust section (5) at the top of the granulation dryer section (1) and exhausted.
[0015] In the granulation and drying device section (1), In order to spray the water-soluble silicon (raw material) entering through the raw material inlet section (2), the spray air entering through the device heating air intake section (3) is taken in together with the silicon and sent into the granulation dryer section (1), where the silicon is sprayed into particles of 30 μm or less in size from a spray nozzle installed inside the granulation dryer section (1).
[0016] In the device heating air intake section (3), In order to keep the temperature inside the granulation drying equipment (1) constant at 257℃, the air volume is automatically adjusted under computer control.
[0017] In the classifier air intake and heating section (4), Outside air is taken in by an intake fan and heated to over 257°C by an air heater. The heated air is then purified by a filter and sent to the classifier.
[0018] In the finished product recovery section (6), The granulated silicon is sucked into the classifier (61) and simultaneously Air is sprayed from below, and particles smaller than the specified size are returned to the main body of the granulation and drying device section (1) again, where they are sprayed and dried to form particles of the specified size. Particles within the specified size range (100 μm or more and less than 250 μm) are placed directly into the finished product tank (62). [Explanation of symbols]
[0020] 1...Pelletization / drying equipment section 2...Raw material input section 21: Bottom of raw material tank, 22...Supply pump, 3. Air intake for heating the device 31... Coarse dust filter 32... Intake fan 33 Air heater 4 Classifier air intake and heating section 5 Exhaust section 51 Bag filter 52 Exhaust fan 6. Finished Product Collection Department 61...Classifier 62...Classifier
Claims
1. This method for producing powdered silica is characterized in that it includes a granulation and drying device section (1), which is the main section for instantly evaporating liquefied silicon and solidifying the evaporated gas, and then raises the temperature to a high temperature of 257°C or higher through equipment consisting of six units: a raw material input section (2), an air intake section for heating the device (3), an air intake and heating section for a classifier (4), an exhaust section (5), and a finished product recovery section (6), thereby evaporating and solidifying the silicon in a short period of time.
2. In the above-mentioned manufacturing method, A raw material input section (2) for the first step, in which water-soluble silicon (raw material) is placed in a raw material tank (21) and sent to the granulation and drying apparatus (1) through a supply pump (22); This device takes in outside air and keeps the temperature inside the granulation and drying device (1) at 257°C. an air intake section (3) for heating the second process device, which blows air taken in from a suction fan (32) through a coarse dust filter (31) into an air heater (33), raises the temperature to a high temperature of 257°C or higher, and sends the air to the granulation drying device section (1); The classifier (61) in the finished product recovery section (6) is an air blowing section for returning silicon particles smaller than expected to the granulation and drying device (1), The third process is an air intake and heating section (4) for the classifier, in which outside air is taken in by an intake fan, heated to 257°C or higher by an air heater, the heated air is purified by a filter, and sent to the classifier; This is the part that discharges air whose temperature has dropped below the specified level. a fourth step exhaust section (5) in which the air accumulated in the upper part of the granulation drying device section (1) due to the force of spraying from the granulation drying device section (1) can be exhausted in a clean state to the outside through an exhaust fan (52) via a bag filter (51); This is the part that collects the granulated silicon (product) after spraying. The granulated silicon is sucked into the classifier (61) and simultaneously separated into the classifier (61). The granulation and drying apparatus is characterized by being composed of six units, including a finished product recovery section (6) in the fifth process, in which air is sprayed from below to collect particles within a specified size range (100 μm or more to less than 250 μm) and the particles can be directly placed in a finished product tank (62). A method for producing instant coffee comprising the steps of:
3. In the granulation and drying device section (1), This method for producing powdered silica is characterized in that heated air is charged and adjusted in the device heating air suction section (3) to keep the temperature inside the granulation dryer section (1) constant, and after the temperature has been stabilized, water-soluble silicon is sprayed in a spray form from the raw material input section (2) and evaporated instantly inside the chamber, the water-soluble silicon solidifies about 10 seconds after being sprayed inside the granulation dryer section (1) and is recovered from the finished product recovery air suction section (3), and granules smaller than the specified size are blown back into the granulation dryer section (1) and spray drying is repeated again until the specified size is reached, and the excess air inside the chamber that is sucked in from the exhaust section (5) at the top of the granulation dryer section (1) is exhausted.
4. In the granulation and drying device section (1), The method for producing powdered silica is characterized in that the water-soluble silicon (raw material) entering through the raw material inlet section (2) is turned into a spray form by taking in the atomizing air entering through the device heating air inlet section (3) together with the water-soluble silicon (raw material) and sending it into the chamber of the granulation and drying device section (1), and the resulting product is sprayed into particles having a size of 30 μm or less from a spray nozzle installed inside the chamber of the granulation and drying device section (1).
5. In the device heating air suction section (3), The method for producing powdered silica, wherein the air volume is automatically adjusted under computer control to keep the temperature inside the granulation and drying device (1) constant at 257°C.
6. In the classifier air intake and heating section (4), A method for producing powdered silica, comprising the steps of: taking in outside air with an intake fan; heating the air to 257°C or higher with an air heater; cleaning the heated air with a filter; and sending the cleaned air to a classifier.
7. In the finished product recovery section (6), The granulated silicon is sucked into the classifier (61) and simultaneously separated into the classifier (61). A method for producing powdered silica, characterized in that air is sprayed from below, particles smaller than a specified size are returned to the main body of the granulation and drying device (1) again, and sprayed and dried to produce particles of a specified size, while particles within the specified size range (100 μm or more and less than 250 μm) are placed directly into a finished product tank (62).
Citation Information
Patent Citations
Method for producing coffee composition
JP2007054057A
Method for producing coffee composition
JP2007054058A