The method and machine for butt welding plastic parts address the issue of undetected cavities by using a camera to inspect molten areas, ensuring high-quality welds through early detection and correction, thus minimizing material waste and process time.

JP2024154424APending Publication Date: 2024-10-30GEORG FISCHER ROHRLEITUNGSSYSTEME AG
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
JP2024066998
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-04-18
Filing Date
2024-04-17
Publication Date
2024-10-30

AI Technical Summary

Technical Problem

Existing butt welding methods for plastic parts, particularly in conduit components, fail to detect cavities in weld seams during the process, leading to undesirable joints.

Method used

A method and machine that uses a camera to inspect the molten area of the plastic parts after melting, allowing early detection of weld quality without interrupting the process, and includes a planer to remove irregularities and a hot plate for non-contact heating, with image correction for evaluation.

Benefits of technology

Enables real-time quality assessment of welds, reducing material loss and time by identifying defects early, and ensuring high-quality welds without full seam separation.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024154424000001_ABST
    Figure 2024154424000001_ABST
Patent Text Reader

Abstract

To provide a method for quality evaluation of a butt welded zone of conduit components.SOLUTION: Disclosed is a method for quality evaluation of a butt welded zone of plastic members, preferably, conduit components by a butt welding machine, wherein the method includes: fastening two plastic members to each other at a coaxial position by using a fastening device for position fixing; flatly cutting end faces of plastic members positioned while facing each other by using a planar which can approach therebetween; fusing plastic member end parts by using a hot plate which can approach therebetween, followed by bonding each other subsequently after the fusing; and inspecting fusion regions formed at the end faces of the plastic member end parts after fusing by using at least one camera.SELECTED DRAWING: Figure 2
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a method for quality assessment of butt welds between plastic parts, preferably between piping components, made by a butt welding machine, in which both plastic parts are clamped and fixed in position in a coaxial position with respect to each other by clamping devices, the end faces of the plastic parts located opposite each other are planed by a planer that can be inserted between them, the plastic part ends are melted by a hot plate that can be inserted between them, and following melting they are joined to each other, and to a butt welding machine comprising a base unit, a planer, a hot plate, a control device, and at least two clamping devices that are located opposite each other coaxially and can be adjusted along the longitudinal axis of the plastic parts to be welded, and in which both opposing clamping devices of the both plastic part ends to be welded to each other have front sides that face each other.

[0002] Methods and butt welding machines for welding plastic parts together are known from the prior art and are often used to weld pipes and piping components used in industry or supply. Non-contact welding machines, for example IR welding machines, are often used when high demands are made on the cleanliness of the piping and therefore also on the welds.

[0003] EP 0899085 discloses a method for welding plastic parts together, in which the cooling process is monitored by an infrared sensor and the cooling time is controlled to obtain an optimum weld.

[0004] The document states that even if an optimal cooling process is maintained, there is nevertheless the disadvantage that voids occur in the weld seam, which voids cannot be recognized and which lead to undesirable welded joints being incorporated into the installation.

[0005] The object of the invention is to propose a method and an associated butt-welding machine, by which the quality of a welded joint can be checked early on, without the welding process having to be interrupted.

[0006] This problem is solved according to the invention in that after melting, the molten area occurring on the end face of the end of the plastic part is inspected by means of at least one camera, and for this purpose at least one camera is arranged on the butt welding machine for imaging the end face of the plastic part.

[0007] In the method according to the invention for quality assessment of butt welds between plastic parts, preferably between ducting components, by a butt welding machine, both plastic parts are clamped in a coaxial position with respect to each other by a clamping device. The ducting components include pipes, fittings, as well as fittings and valves, which can be welded to each other. In the method according to the invention, the end faces of the plastic parts lying opposite each other are planed by a planer which can be inserted between them. This removes irregularities or impurities, which are important for the quality of the welded joint. The plastic part ends are then melted by a hot plate which can be inserted between them. This hot plate is placed between the plastic part ends instead of the planer used previously, and heats them without contact, preferably by means of an infrared hot plate.

[0008] Following melting, the plastic part ends are joined together. For this purpose, the hot plates arranged between them are moved away and the plastic parts are pressed together. Immediately after melting, the resulting melted area on the end surface of the plastic part ends is inspected by at least one camera. This is done during the movement of the hot plates and in a short time window before the plastic part ends are brought together.

[0009] Preferably, the inspection of the melted area by means of a camera is carried out before joining of both plastic part ends, so that the inspection does not require additional time and is carried out during the welding process, so that the welded area is no longer cooled before joining.

[0010] It has been found to be advantageous if the imaging of the edge of the plastic part by the camera is performed at an oblique viewing angle, which makes it possible to first avoid the need to bring the camera in front between the edge faces of the plastic part ends, but to place the camera stationary outside or offset relative to the edge faces, thereby making it possible to create an image of the edge with the melted area immediately after melting.

[0011] It has proven advantageous if the image of the camera is corrected for the evaluation. The correction of the image converts the obliquely detected image into a frontal image. This makes it possible to evaluate the image with the aid of an image evaluation system and classify the quality of the melted area of ​​the end face as sufficient or insufficient for the weld. Advantageously, if the quality is classified as insufficient, the welding process is stopped, the plastic component ends are again planed and a new melting is carried out or the component to be welded is removed from the welding machine and replaced by another component. This early inspection and recognition of the quality of the melted area can, on the one hand, save material losses, since it is not necessary to cut off the entire weld seam, but only to over-plan both individual end faces again, and, on the other hand, also save time, since unnecessary steps can be avoided when defects or insufficient quality in the melted area are recognized early.

[0012] Of course, the camera can already be used to recognize the clamped plastic parts, so that, autonomously, for example, the dimensions, material and other properties of the plastic parts to be welded can be identified and transmitted to the butt welding machine or control device, so that manual input can be avoided, which also contributes to reducing defects.

[0013] Advantageously, the image from the oblique viewing angle of the camera is converted into a front image. As already mentioned above, only the front image is used for the image evaluation after the conversion. The corrected image from the conversion or the front image allows cavities, inclusions, bubble formations, combustions, impurities and other undesirable texture changes to be recognized and evaluated. Preferably, an image evaluation system and an algorithm evaluate which melted areas correspond to the required quality and which do not. Advantageously, the algorithm is optimized on the basis of empirical values ​​itself or can be optimized or self-learned on the basis of empirical values ​​entered by the operator.

[0014] It is advantageous if the imaging is performed obliquely from below towards the oppositely situated end faces of the plastic component ends.

[0015] The butt welding machine of the present invention for carrying out a method for welding plastic parts at their end faces and for evaluating the quality of the butt welds between the plastic parts has a base unit, a planar, a hot plate, a control device, at least two fastening devices positioned coaxially opposite each other, and two front planes facing each other, and at least one camera is arranged on the butt welding machine for imaging the end faces of the plastic parts.

[0016] The butt welding machine according to the invention has a stable base unit, on which the planar and the hot plate are preferably arranged so as to be pivotable and movable along the longitudinal axis. As a result, at the time of each method step, the planar or the hot plate can be pivoted between the plastic part ends to carry out the corresponding process step. To control the welding process, the butt welding machine has a control device which controls the time flow of the process as well as the temperature. The plastic parts to be welded together, preferably the tube components, are clamped in a number of coaxially arranged clamping devices of the butt welding machine. Preferably, at least one clamping device of a clamped plastic part can be moved along the longitudinal axis or on one side of the butt welding machine in order to position the end faces of the plastic part ends in accordance with the method steps and finally to join the plastic parts together. The butt welding machine according to the invention has two front planes located opposite each other, between which the planar and the welding plate can be pivoted.

[0017] The plastic parts end portions protrude or overhang beyond the front plane so as to be joined together. The two front planes are located opposite each other and constitute a front plane facing the welding area of ​​the two clamping units of the butt welding machine. In order to weld the plastic parts together, one plastic part is arranged on each clamping unit. The front plane is formed by both facing end faces of the clamping units of the butt welding machine. The front plane is preferably formed by two facing clamping devices of the two plastic parts or by a base unit. At least one camera is arranged on the butt welding machine to image the plastic part end faces. It is advantageous if this camera is arranged on a non-rotatable, rigid unit of the butt welding machine, preferably not on a planar or welding plate.

[0018] It is advantageous if the camera is arranged stationary on the welding machine, since the camera does not perform any movement while taking the image, resulting in extremely clear and sharp images.

[0019] Preferably, the camera is arranged in a front plane of the butt welding machine, so that the camera can be directed toward the end faces of the plastic part ends. In order to protect the camera, it is advantageous if the camera is arranged in a recess in the front plane. Furthermore, it is advantageous if the camera is arranged obliquely with respect to the vertically extending front plane in order to achieve an oblique direction of the camera toward the mutually facing end faces of the plastic part ends.

[0020] It has been found to be a preferred embodiment for the camera to be offset relative to the longitudinal axis and have an oblique viewing angle for imaging the end face of the plastic part end, so that the camera is not pointed directly in front of or perpendicular to the end face, but offset relative to the centre of the cross section of the plastic part.

[0021] Preferably, the camera is positioned laterally offset relative to the end face of the plastic member.

[0022] Preferably, at least two cameras are arranged on the butt welding machine, each of which is arranged on one front plane of the butt welding machine and is directed toward mutually facing end faces of the plastic parts.

[0023] It has proven to be advantageous if the camera is arranged in the front plane below the plastic components to be welded, so that the camera can image the welding area with an oblique viewing angle directed upwards towards the end faces lying opposite each other.

[0024] All possible constructional means are freely combinable with one another.

[0025] An embodiment of the present invention will be described with reference to the drawings, however, the present invention is not limited to this embodiment. [Brief description of the drawings]

[0026] [Figure 1] FIG. 2 is a three-dimensional view of two fastened plastic part ends positioned opposite each other. [Diagram 2] FIG. 2 is a three-dimensional view of two plastic part ends located opposite each other, in which the melted area can be seen. [Diagram 3] FIG. 2 is a front view of a portion of a butt welding machine;

[0027] In FIG. 1, a partial area of ​​a butt welding machine 1 according to the invention is shown with a clamped plastic part 2, preferably a pipe component 2, to be welded. The butt welding machine 1 has a base unit 9, a planer (not shown) and a welding plate (not shown). Furthermore, the butt welding machine 1 according to the invention has clamping devices 3 arranged coaxially with one another, which fix the plastic parts 2. The butt welding machine 1 has two front planes 11 facing one another, beyond which the ends 6 of the plastic parts 2 to be welded extend. The front planes 11 are preferably formed by the facing end faces of the two clamping devices 3 or the base unit 9. The front planes 11 form the vertically extending front faces of both clamping areas of the butt welding machine 1, which immovably clamp the respective plastic parts 2 to be welded to one another. A camera 7 is arranged in each case in the front planes 11 for imaging the end faces 4 of the plastic parts 2. The oblique viewing angle 8 of the camera 7 is clearly visible in the drawing. The camera 7 is preferably arranged obliquely with respect to the front plane 11 of the welding machine 1. Due to the immobile arrangement of the camera 7 on the front plane 11, an image of the melting area 6 from the oblique viewing angle 9 is taken as soon as the melting phase is terminated by moving the hot plate away. Of course, an image of the end face 4 of the plastic part 2 can also be taken for inspection or part recognition of the surface immediately after or immediately before planing the material. This allows an autonomous positioning of the butt welding machine 1 based on the plastic parts to be welded. By means of the control device and the stored data, the machine recognizes the parts to be welded and automatically carries out all necessary adjustments, and the welding process also proceeds automatically. Furthermore, a welding protocol can be directly created by the detected images and their evaluation using an image evaluation system which compares the captured and corrected images with predefined values ​​or images and classifies them as pass or fail. [Explanation of symbols]

[0028] 1. Butt welding machine 2 Plastic parts / pipe components 3 Fastening device 4 End face of plastic parts 5 Plastic component end 6. Melting Zone 7. Camera 8 Diagonal viewing angles 9 Basic Unit 10 Longitudinal axis 11 Anterior plane

Claims

1. A method for quality assessment of butt welds between plastic parts (2), preferably between piping components (2), made by a butt welding machine (1), comprising the steps of clamping two plastic parts (2) in a coaxial position with respect to each other with a clamping device (3), planing the opposing end faces (4) of the plastic parts (2) with a planer that can be inserted between them, melting the plastic part ends (5) with a hot plate that can be inserted between them, and joining them together following the melting, A method according to claim 1, further comprising inspecting, after said melting, the resulting melted area (6) on said end face (4) of said plastic part end (5) by means of at least one camera (7).

2. 2. The method according to claim 1, characterized in that the inspection of the melted area (6) by means of a camera (7) is performed before the joining of both plastic part ends (5).

3. 3. The method according to claim 1 or 2, characterized in that the imaging of the end face (4) of the plastic component (5) by the camera (7) is performed at an oblique viewing angle (8).

4. 4. The method according to claim 3, characterized in that the images of the camera (7) are corrected for the evaluation.

5. 4. The method according to claim 3, characterized in that the image is transformed from an oblique viewing angle (8) of the camera (7) into a frontal image.

6. 6. The method according to claim 1, wherein the corrected image or the image converted into a front image of the molten area (6) at the end face (4) is classified as of good or bad quality by an image evaluation system.

7. A butt-welding machine (1) for carrying out the method according to any one of claims 1 to 6, comprising a base unit (9), a planar, a hot plate, a control device, at least two clamping devices (3) located coaxially opposite each other, and two front planar surfaces (11) facing each other, The butt welding machine (1) is characterized in that at least one camera (7) for imaging an end surface (4) of a plastic member is disposed in the butt welding machine (1).

8. 9. The butt welding machine (1) according to claim 8, characterized in that the camera (7) is arranged stationary on the butt welding machine (1).

9. 10. The butt welding machine (1) according to claim 8 or 9, characterized in that the camera (7) is arranged in the front plane (11) of the butt welding machine (1).

10. 10. The butt welding machine (1) according to claim 7, wherein the camera is arranged offset with respect to the longitudinal axis and has an oblique viewing angle (8) for imaging the end face (4) of the plastic part end (5).

11. 11. The butt welding machine (1) according to claim 7, characterized in that at least two cameras (7) are arranged on the butt welding machine (1), the cameras (7) being arranged on each of the front planes (11) of the butt welding machine (1) and directed towards the mutually facing end faces (4) of the plastic parts (2).