Method for manufacturing rotor
By heating resin injection from both ends of the rotor core, the method addresses deformation risks in thermoplastic resin injection, simplifying the manufacturing process and apparatus configuration.
Patent Information
- Application Number
- JP2023071631
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-04-25
- Publication Date
- 2024-11-07
AI Technical Summary
Conventional rotor manufacturing methods using thermoplastic resin injection risk deforming the rotor core due to high injection pressure, necessitating complex manufacturing apparatus configurations.
A method involving a rotor core with magnet housing holes on both ends, using a first mold to heat the resin injection from one end and a second mold to heat the resin flow path from the other end, reducing resin viscosity and injection pressure without needing slide core molds.
This approach prevents rotor core deformation and simplifies the manufacturing apparatus by maintaining resin temperature and reducing pressure, ensuring efficient filling without complex equipment.
Smart Images

Figure 2024157332000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a method for manufacturing a rotor. [Background technology]
[0002] Conventionally, a rotor with embedded magnets includes a rotor core having magnet accommodating holes, and magnets accommodated in the magnet accommodating holes. The magnets are fixed to the rotor core via a resin filled in the magnet accommodating holes.
[0003] The resin filled in the magnet accommodating holes is mainly a thermosetting resin or a thermoplastic resin. Generally, a thermoplastic resin has a higher viscosity when melted than a thermosetting resin. Therefore, the injection pressure when filling the magnet accommodating holes with a thermoplastic resin using an injection device is more likely to be higher than when filling with a thermosetting resin. As a result, the rotor core may be deformed by the injection pressure of the thermoplastic resin.
[0004] Patent Document 1 discloses a method for manufacturing a rotor in which a thermoplastic resin is injected into magnet housing holes while the outer peripheral surface of the rotor core is heated by a heating mold. The heating mold has multiple slide core molds that are slidable in the radial direction of the rotor core. Each slide core mold heats the outer peripheral surface of the rotor core while pressing the outer peripheral surface of the rotor core from the outside in the radial direction.
[0005] The rotor core is heated by the heating mold, so that the temperature of the thermoplastic resin is less likely to drop. Therefore, the thermoplastic resin is filled into the magnet housing holes while the increase in the viscosity of the thermoplastic resin is suppressed. This suppresses the increase in the injection pressure of the thermoplastic resin, and thus suppresses deformation of the rotor core. [Prior art documents] [Patent documents]
[0006] [Patent Document 1] JP 2015-192575 A Summary of the Invention [Problem to be solved by the invention]
[0007] The rotor manufacturing method described in Patent Document 1 requires a heating mold having a plurality of slide core dies, which may complicate the configuration of the manufacturing device for manufacturing the rotor. [Means for solving the problem]
[0008] A manufacturing method for a rotor to solve the above problem is a manufacturing method for a rotor including a rotor core having magnet accommodating holes that open to each of a first end face and a second end face located opposite the first end face, and magnets that are accommodated in the magnet accommodating holes and fixed to the rotor core via a thermoplastic resin, the manufacturing method including an injection process of contacting a first mold with the first end face of the rotor core with the magnet accommodated in the magnet accommodating hole, and injecting the resin into the magnet accommodating hole through the flow path while contacting a second mold having a flow path through which the resin flows with the second end face, and injecting the resin into the magnet accommodating hole through the flow path while the first mold is heated in the injection process.
[0009] According to the above method, the magnet accommodating hole is filled with thermoplastic resin through the flow path of the second mold in contact with the second end face of the rotor core. At this time, the temperature of the injected resin is likely to decrease from the second end face to the first end face inside the magnet accommodating hole. In the injection process, the resin is injected into the magnet accommodating hole while the rotor core is heated by the first mold in contact with the first end face of the rotor core. As a result, the temperature of the resin is unlikely to decrease when the resin approaches the first end face from the second end face side inside the magnet accommodating hole. Therefore, the viscosity of the resin is unlikely to increase. As a result, the injection pressure of the resin can be suppressed from increasing, and deformation of the rotor core can be suppressed. From the above, equipment such as a slide core mold that presses the outer peripheral surface of the rotor core is not required to suppress deformation of the rotor core. Therefore, the configuration of the manufacturing device for manufacturing the rotor can be suppressed from becoming complicated. [Brief description of the drawings]
[0010] [Figure 1] FIG. 1 is a perspective view showing a rotor manufactured by a rotor manufacturing method according to one embodiment. [Diagram 2] FIG. 2 is a cross-sectional view showing the rotor of FIG. [Diagram 3] FIG. 3 is a cross-sectional view showing a rotor manufacturing apparatus according to one embodiment. [Figure 4] FIG. 4 is a cross-sectional view showing the state in which the dowel is crushed. [Diagram 5] FIG. 5 is a cross-sectional view showing a state in which the rotor core is placed on the first die. [Figure 6] FIG. 6 is a cross-sectional view showing a state in which the first and second dies are clamped together. [Figure 7] FIG. 7(a) is a cross-sectional view showing a state before the rotor core is pressed by a second die, and FIG. 7(b) is a cross-sectional view showing a state in which the rotor core is pressed by the second die. [Figure 8] FIG. 8 is a cross-sectional view showing a state in which resin has been injected into the magnet accommodating hole. [Figure 9] FIG. 9 is a cross-sectional view showing a first type of the modified example. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0011] Hereinafter, one embodiment of a method for manufacturing a rotor will be described with reference to FIGS. (Rotor 10) 1 and 2, the rotor 10 includes a rotor core 11, a plurality of magnets 30, and a plurality of resins 31. The rotor 10 is, for example, a magnet-embedded rotor.
[0012] Rotor core 11 has a generally cylindrical shape with its central axis coincident with axis C. Rotor core 11 is formed, for example, by laminating a plurality of core pieces 20 punched out of electromagnetic steel sheets.
[0013] Hereinafter, the stacking direction of the multiple core pieces 20 will be simply referred to as the stacking direction. The radial direction centered on the axis C of the rotor core 11 will be simply referred to as the radial direction. The circumferential direction centered on the axis C of the rotor core 11 will be simply referred to as the circumferential direction.
[0014] Rotor core 11 has a first end face 11a and a second end face 11b located on opposite sides to each other in the stacking direction. Rotor core 11 has a central hole 12 into which a shaft (not shown) is inserted, and a plurality of magnet accommodating holes 13 in which magnets 30 are housed. Central hole 12 and each magnet accommodating hole 13 penetrate rotor core 11 in the stacking direction. That is, central hole 12 and each magnet accommodating hole 13 open to each of first end face 11a and second end face 11b.
[0015] The multiple core pieces 20 include a first core piece 21 and a second core piece 22. The rotor core 11 is formed, for example, by stacking the multiple first core pieces 21 and one second core piece 22. The second core piece 22 forms one end face of the rotor core 11 in the stacking direction. The second core piece 22 forms, for example, a first end face 11a of the rotor core 11.
[0016] 2, each first core piece 21 has a plurality of dowels 21a that bulge out to one side in the stacking direction. The plurality of dowels 21a are provided at equal intervals in the circumferential direction of the first core piece 21. The first core pieces 21 adjacent in the stacking direction are joined to each other by crimping the dowels 21a.
[0017] The second core piece 22 has a plurality of through holes 22a penetrating in the stacking direction. The plurality of through holes 22a are provided at equal intervals in the circumferential direction of the second core piece 22. The first core piece 21 and the second core piece 22 are joined to each other by fitting the dowel 21a into the through hole 22a.
[0018] The magnets 30 are respectively housed in the magnet housing holes 13. Each magnet 30 has an elongated shape extending in the stacking direction. The cross-sectional shape of the magnet 30 perpendicular to the stacking direction is substantially rectangular.
[0019] The length of magnet 30 in the lamination direction is shorter than the lamination height, which is the height from first end face 11a to second end face 11b of rotor core 11. One end face of the magnet 30 in the stacking direction is flush with, for example, the first end face 11a. The other end face of the magnet 30 opposite to the one end face in the stacking direction is located, for example, more inward in the stacking direction than the second end face 11b.
[0020] The magnet 30 is fixed to the rotor core 11 via resin 31 filled in the magnet accommodating hole 13. The resin 31 is interposed between the outer peripheral surface of the magnet 30 and the inner peripheral surface of the magnet accommodating hole 13. The resin 31 covers the other end face of the magnet 30.
[0021] The resin 31 may be, for example, a thermoplastic resin such as a liquid crystal polymer. (Manufacturing equipment 40) The manufacturing apparatus 40 for manufacturing the rotor 10 will now be described.
[0022] The manufacturing apparatus 40 is an apparatus for filling the magnet accommodating holes 13 of the rotor core 11, in which the magnets 30 are accommodated, with resin 31 and solidifying it. As shown in FIG. 3, the manufacturing apparatus 40 includes a first mold 50 and a second mold 60 .
[0023] (1st type 50) The first mold 50 is, for example, a fixed mold. The first die 50 has a first contact surface 51 that contacts the first end face 11a of the rotor core 11. The first contact surface 51 is flat. The first contact surface 51 has a size sufficient to cover the openings of all of the magnet accommodating holes 13 that open to the first end face 11a.
[0024] Inside the first die 50, for example, a first heater 52 that generates heat when electricity is applied is disposed. (2nd type 60) The second die 60 includes a die body 61 and a gate plate 65. The die body 61 and the gate plate 65 are, for example, configured as separate bodies. The die body 61 is, for example, a movable die configured to be movable toward and away from the first die 50.
[0025] The mold body 61 has a sprue 62 through which the resin 31 injected from the injection device 100 flows. Inside the mold body 61, for example, a second heater 63 that generates heat when electricity is applied is disposed.
[0026] (Gate Plate 65) The gate plate 65 is disposed between the die body 61 and the rotor core 11. The gate plate 65 has a second contact surface 66 that contacts the second end face 11b of the rotor core 11. The second contact surface 66 is flat. The second contact surface 66 has a size sufficient to cover the openings of all of the magnet accommodating holes 13 that open to the second end face 11b.
[0027] The gate plate 65 has a runner 67 that communicates with the sprue 62 and a plurality of gates 68 extending from the runner 67 . The runners 67 open to a surface of the gate plate 65 opposite to the second contact surface 66. The runners 67 extend radially from the center of the gate plate 65. Each gate 68 opens to the second contact surface 66. Each gate 68 communicates between an end of the runner 67 and the magnet accommodating hole 13.
[0028] (Method of manufacturing rotor 10) The manufacturing method of the rotor 10 includes a crushing step, a first arranging step, a second arranging step, a third arranging step, a pressing step, a heating step, an injection step, and a solidification step. The crushing step, the first arranging step, the second arranging step, the third arranging step, the pressing step, the heating step, the injection step, and the solidification step are performed in this order.
[0029] (Crushing process) As shown by the dotted line in Figure 4, when the first core piece 21 and the second core piece 22 are crimped to each other, the tip of the dowel 21a of the first core piece 21 adjacent to the second core piece 22 may protrude to the outside from the through hole 22a of the second core piece 22.
[0030] In the crushing process, the tip of the dowel 21a protruding from the through hole 22a of the second core piece 22 is pressed by a pressing jig 70, thereby crushing the dowel 21a. In the crushing process, the dowel 21a is crushed so that the tip of the dowel 21a is positioned inside the through hole 22a.
[0031] (1st placement process) As shown in FIG. 5, in the first arrangement step, the rotor core 11 with the magnets 30 accommodated in each magnet accommodating hole 13 is placed on the first contact surface 51 of the first die 50. At this time, the first contact surface 51 covers the entire first end face 11a. That is, the first contact surface 51 closes the openings of all the magnet accommodating holes 13 that open to the first end face 11a. At this time, the lower surface of each magnet 30 is in contact with the first contact surface 51. In addition, the upper surface of each magnet 30 is located below the second end face 11b. Note that in the first arrangement step, the rotor core 11 may be placed on the first die 50 so that the second end face 11b is in contact with the first contact surface 51.
[0032] (Second placement process) 6, in the second arrangement step, the gate plate 65 is placed on the second end face 11b of the rotor core 11. At this time, the second contact surface 66 covers the entire second end face 11b, and each gate 68 communicates with the magnet accommodating hole 13. Each gate 68 is disposed at a position facing the upper surface of the magnet 30, for example.
[0033] (Third placement process) In the third arrangement step, the die body 61 comes into contact with the gate plate 65 from the side opposite to the rotor core 11. As a result, the sprue 62 of the die body 61 communicates with the runner 67 of the gate plate 65.
[0034] (Pressing process) In the pressing process, as the first die 50 and the second die 60 are clamped together, the second die 60 presses the second end face 11b, thereby pressing the first end face 11a against the first die 50. In the pressing process, the die body 61 presses the second end face 11b via the gate plate 65.
[0035] Here, in the rotor core 11 that is stacked with the dowels 21a crimped together, a small gap may occur between adjacent core pieces 20. When the second end face 11b of the rotor core 11 is pressed by the second die 60, the core pieces 20 are brought into close contact with each other so that the gaps between the core pieces 20 are filled. This reduces the stacking height of the rotor core 11.
[0036] 7(a) and 7(b), as the stacking height of the rotor core 11 decreases, the distance H1 in the stacking direction from the second end face 11b of the rotor core 11 to the upper face of the magnet 30 decreases to a distance H2. That is, in the pressing step, the second end face 11b is pressed by the second die 60, thereby generating a flow space S through which the resin 31 flows in the stacking direction between the gate plate 65 and the magnet 30 while the stacking height of the rotor core 11 decreases. The resin 31 discharged from the gate 68 is introduced into the magnet accommodating hole 13 through the flow space S.
[0037] Incidentally, if the pressing force by the second die 60 is small in the pressing process, there is a risk that the resin 31 will leak out of the magnet accommodating hole 13 through the gaps between the iron core pieces 20 in the injection process. On the other hand, if the pressing force by the second die 60 is large, there is a risk that the stacking height of the rotor core 11 will increase due to springback of the iron core pieces 20 when the pressing force is released after the resin 31 filled in the magnet accommodating hole 13 has solidified. At this time, gaps due to springback are generated between the iron core pieces 20. For this reason, the pressing force by the second die 60 is set to a value that does not cause leakage of the resin 31 from the magnet accommodating hole 13 and does not cause gaps between the iron core pieces 20 due to springback.
[0038] (Heating process) In the heating process, the first mold 50 is heated by passing current through the first heater 52, and the mold body 61 of the second mold 60 is heated by passing current through the second heater 63. The heating temperatures of the first mold 50 and the mold body 61 are set to, for example, the same temperature. The heating temperatures of the first mold 50 and the mold body 61 are set to, for example, the glass transition temperature of the resin 31 or lower.
[0039] In the heating step, the first die 50 and the die body 61 are heated for a predetermined period of time. The gate plate 65 is heated through the die body 61. (injection process) 8, in the injection process, the injection device 100 injects the resin 31 into each magnet accommodating hole 13 through the flow path P of the second mold 60. More specifically, the resin 31 injected from the injection device 100 is injected into the magnet accommodating hole 13 through the sprue 62, the runner 67, and the gate 68. As a result, the magnet accommodating hole 13 is filled with the resin 31.
[0040] In the injection process, the resin 31 is injected while the pressing of the second die 60 in the pressing process is continued. That is, in the injection process, the resin 31 is injected while the first end face 11a of the rotor core 11 is pressed against the first contact surface 51 of the first die 50.
[0041] In the injection step, the resin 31 is injected while the first mold 50 and the mold body 61 are continuously heated in the heating step. (solidification process) In the solidification process, for example, the heating of the first die 50 and the die body 61 is stopped to air-cool the rotor core 11. This causes the resin 31 filled in the magnet accommodating holes 13 to solidify. In this manner, the rotor 10 is manufactured.
[0042] Finally, the rotor 10 is removed from between the first die 50 and the second die 60. The operation of this embodiment will be described. Thermoplastic resin 31 is filled into magnet accommodating hole 13 through flow path P of second die 60 in contact with second end face 11b of rotor core 11. At this time, the temperature of injected resin 31 is likely to decrease from second end face 11b to first end face 11a inside magnet accommodating hole 13. In the injection process, resin 31 is injected into magnet accommodating hole 13 while rotor core 11 is heated by first die 50 in contact with first end face 11a of rotor core 11. As a result, when resin 31 moves from second end face 11b side to first end face 11a side inside magnet accommodating hole 13, the temperature of resin 31 is unlikely to decrease. Therefore, viscosity of resin 31 is unlikely to increase. As a result, the injection pressure of resin 31 can be suppressed from increasing, and deformation of rotor core 11 can be suppressed.
[0043] The effects of this embodiment will be described. (1) In the injection step, the resin 31 is injected into the magnet accommodating hole 13 while the first die 50 is in a heated state.
[0044] According to the above method, equipment such as a slide core mold that presses the outer peripheral surface of rotor core 11 is not required to suppress deformation of rotor core 11. Therefore, the configuration of manufacturing apparatus 40 that manufactures rotor 10 can be prevented from becoming complicated.
[0045] (2) In the injection process, the resin 31 is injected into the magnet accommodating hole 13 while the second die 60 is in a heated state. According to the above method, by heating the second die 60, the temperature of the resin 31 is less likely to decrease when the resin 31 passes through the flow path P. Therefore, the temperature of the resin 31 is less likely to decrease until the resin 31 reaches the magnet accommodating hole 13. Therefore, an increase in the injection pressure of the resin 31 can be further suppressed.
[0046] (3) In the injection step, the resin 31 is injected into the magnet accommodating hole 13 with the first end face 11a pressed against the first die 50. According to the above method, the first end face 11a of the rotor core 11 is pressed against the first die 50, thereby increasing the contact area between the first die 50 and the first end face 11a and reducing the air space between the first die 50 and the first end face 11a. This makes it easier for the temperature of the heated first die 50 to be transferred to the rotor core 11. This makes it possible to shorten the time required to raise the rotor core 11 to a desired temperature.
[0047] (4) In the pressing process, the stacking height of the rotor core 11 is reduced by tightly contacting the multiple core pieces 20 in the stacking direction, while the second end face 11b is pressed so as to create a flow space S between the second die 60 and the magnet 30 in the stacking direction.
[0048] If there is a gap between the core pieces 20 adjacent to each other in the stacking direction, the resin 31 may leak from the gap during the injection process. In this case, it is possible to perform the injection process while pressing the rotor core 11 in order to fill the gap between the core pieces 20. However, if the stacking height of the rotor core 11 becomes excessively small by pressing the rotor core 11, the second die 60 may come into contact with the end face of the magnet 30 accommodated in the magnet accommodating hole 13. In this case, the flow path P of the second die 60 is blocked by the end face of the magnet 30, so that the resin 31 may not be filled in the magnet accommodating hole 13. The problem of the resin 31 leaking from the gap between the core pieces 20 is particularly noticeable in the case of a thermoplastic resin, which is more likely to be injected at a higher pressure than a thermosetting resin.
[0049] In this regard, according to the above method, the rotor core 11 is pressed so that the core pieces 20 come into close contact with each other, thereby reducing the stacking height of the rotor core 11 and generating a flow space S between the second die 60 and the magnets 30. Therefore, the resin 31 can be filled into the magnet accommodating holes 13 while suppressing leakage of the resin 31 from the gaps between the core pieces 20.
[0050] (5) In the crushing step, the dowel 21a is crushed so that the tip of the dowel 21a protruding from the through hole 22a is positioned inside the through hole 22a. If the dowel 21a protrudes from the through hole 22a opening in the first end face 11a of the rotor core 11, a gap may be generated between the first die 50 and the first end face 11a when the first die 50 is brought into contact with the first end face 11a. If the dowel 21a protrudes from the through hole 22a opening in the second end face 11b of the rotor core 11, a gap may be generated between the second die 60 and the second end face 11b when the second die 60 is brought into contact with the second end face 11b. In these cases, there is a risk that the resin 31 will leak out from the gap between the rotor core 11 and the first die 50 or the second die 60 during the injection process.
[0051] In this regard, according to the above method, before the injection step, the dowel 21a is crushed so that the tip of the dowel 21a is located inside the through hole 22a. This makes it difficult for a gap to be generated between the rotor core 11 and the first die 50 or the second die 60, thereby making it possible to suppress leakage of the resin 31 from the gap.
[0052] Furthermore, according to the above method, the contact area between the first die 50 and the first end face 11a can be increased compared to when the injection step is performed with the dowel 21a protruding from the through hole 22a opening in the first end face 11a of the rotor core 11. As a result, the temperature of the heated first die 50 is easily transferred to the rotor core 11. Therefore, the time required to raise the rotor core 11 to a desired temperature can be shortened.
[0053] <Example of change> This embodiment can be modified as follows: This embodiment and the following modifications can be combined with each other to the extent that there is no technical contradiction.
[0054] As shown in FIG. 9, the first die 50 may have a plurality of accommodating recesses 51a formed in the first contact surface 51. Each accommodating recess 51a accommodates the tip of the dowel 21a protruding from the through hole 22a opening in the first end surface 11a. In this case, in the injection process, the resin 31 is injected into the magnet accommodating hole 13 in a state in which the tip of the dowel 21a protruding from the through hole 22a is accommodated in the accommodating recess 51a. According to this method, when the first die 50 contacts the first end surface 11a of the rotor core 11, the tip of the dowel 21a is accommodated in the accommodating recess 51a. This makes it possible to increase the contact area between the first die 50 and the first end surface 11a, compared to a case in which the first die 50 does not have the accommodating recess 51a. As a result, the temperature of the heated first die 50 is easily transferred to the rotor core 11. Therefore, the time required to raise the rotor core 11 to a desired temperature can be shortened. In addition, the crushing process in the above embodiment can be omitted.
[0055] The rotor core 11 may be configured by stacking a plurality of laminated blocks, each of which is configured by stacking a plurality of first core pieces 21 and one second core piece 22. In this case, the laminated blocks are fixed to each other by, for example, resin 31.
[0056] The core pieces 20 do not have to be joined to each other by crimping the dowels 21a. The core pieces 20 may be joined to each other by, for example, the resin 31.
[0057] In the pressing step, the flow space S does not have to be generated between the second die 60 and the magnet 30. In this case, the position of the gate 68 is preferably set to a position in the magnet accommodating hole 13 where the magnet 30 is not present.
[0058] The pressing step does not have to be carried out before the injection step. The heating temperature of the first die 50 may be higher than the heating temperature of the die body 61. In this case, the temperature gradient in the stacking direction of the magnet accommodating hole 13 becomes smaller, so that the temperature of the resin 31 injected into the magnet accommodating hole 13 becomes less likely to decrease.
[0059] In the heating step, the mold body 61 does not have to be heated. In this case, since the gate plate 65 is not heated, the resin 31 remaining in the flow path P after the injection step is solidified quickly. Therefore, the gate plate 65 can be separated from the rotor 10 quickly after the solidification step.
[0060] The manufacturing apparatus 40 may include a first die 50 which is a movable die, and a second die 60 which is a fixed die. In this case, the first die 50 approaches the rotor core 11 placed on the second die 60, thereby performing die clamping.
[0061] The gate plate 65 may be connected to the second die 60 so as to be capable of moving relatively thereto. In the injection process, the resin 31 may be injected immediately after stopping the heating of the first die 50 and the die body 61. In other words, as long as the rotor core 11 is heated to a desired temperature range immediately before the injection of the resin 31, the heating of the first die 50 and the die body 61 may be stopped when the resin 31 is injected.
[0062] The gate plate 65 may be omitted from the second die 60. In this case, it is sufficient that a flow path P corresponding to the runner 67 and the gate 68 is formed inside the second die 60. The first die 50 may have a side wall that protrudes from the first contact surface 51 and surrounds the outer peripheral surface of the rotor core 11. The side wall may be in contact with the outer peripheral surface of the rotor core 11, or may have a gap between it and the outer peripheral surface of the rotor core 11. By using such a first die 50, heat radiation from the outer peripheral surface of the rotor core 11 is suppressed, so that the efficiency of heating the rotor core 11 by the first die 50 can be improved.
[0063] Prior to the injection process, the rotor core 11 may be preheated. In the solidification step, the rotor 10 may be cooled using a first die 50 and a second die 60 each having a cooling passage.
[0064] The resin 31 is not limited to a liquid crystal polymer, but may be, for example, PPS (polyphenylene sulfide), PEEK (polyether ether ketone), PA (polyamide), or the like.
[0065] The above embodiment includes the configurations described in the following supplementary notes. [Appendix 1] A manufacturing method for a rotor including a rotor core having magnet accommodating holes that open to a first end face and a second end face opposite the first end face, and magnets that are accommodated in the magnet accommodating holes and fixed to the rotor core via a thermoplastic resin, the manufacturing method comprising an injection step of contacting a first mold with the first end face of the rotor core with the magnets accommodated in the magnet accommodating holes, and injecting the resin into the magnet accommodating holes via the flow path while contacting a second mold having a flow path through which the resin flows with the second end face, wherein the injection step involves injecting the resin into the magnet accommodating holes while the first mold is heated.
[0066] [Appendix 2] The method for manufacturing a rotor according to [Appendix 1], wherein in the injection step, the resin is injected in a heated state of the second mold. [Appendix 3] The rotor core is formed by stacking a plurality of iron core pieces, and a pressing step is provided prior to the injection step in which the second end face is pressed by the second mold, thereby pressing the first end face against the first mold, and in the injection step, the resin is injected in a state in which the first end face is pressed against the first mold. [Appendix 1] or [Appendix 2]
[0067] [Appendix 4] A manufacturing method for a rotor as described in [Appendix 3], in which when the height from the first end face to the second end face of the rotor core is defined as a stacking height, the length of the magnet in the stacking direction of the multiple core pieces is shorter than the stacking height, and in the pressing process, the stacking height is reduced by closely contacting the multiple core pieces in the stacking direction, while the second end face is pressed so as to create a flow space through which the resin can flow between the second die and the magnet in the stacking direction.
[0068] [Appendix 5] The rotor core is formed by stacking a plurality of iron core pieces, the plurality of iron core pieces having a dowel that bulges to one side in the stacking direction of the plurality of iron core pieces, and includes a plurality of first core pieces stacked with the dowels connected to each other, and a second core piece having a through hole into which the dowel is inserted and constituting the first end face or the second end face, and the method for manufacturing a rotor described in any one of [Appendix 1] to [Appendix 4] includes a crushing process that, prior to the injection process, presses the tip of the dowel protruding from the through hole, thereby crushing the dowel so that the tip is positioned inside the through hole.
[0069] [Appendix 6] The rotor core is formed by stacking a plurality of iron core pieces, the plurality of iron core pieces having a dowel that bulges to one side in the stacking direction of the plurality of iron core pieces and including a plurality of first core pieces stacked in a state in which the dowels are connected to each other, and a second core piece having a through hole into which the dowel is inserted and constituting the first end face, and in the injection process, the resin is injected in a state in which the tip of the dowel protruding from the through hole is accommodated in an accommodating recess formed in the first mold. A manufacturing method for a rotor described in any one of [Appendix 1] to [Appendix 5]. [Explanation of symbols]
[0070] P…Flow path S…Distribution space 10...Rotor 11...Rotor core 11a...first end surface 11b…Second end surface 12...Center hole 13...Magnet receiving hole 20…Iron core piece 21…First core piece 21a…Dabo 22…Second core piece 22a...Through hole 30…Magnet 31...Resin 40...Manufacturing equipment 50...Type 1 51...1st contact surface 51a...accommodating recess 52…First heater 60...2nd type 61…Mold body 62…Sprue 63…Second heater 65…Gate plate 66…Second contact surface 67…Runner 68…Gate 70...Pressing tool 100...Injection device
Claims
1. A manufacturing method of a rotor including a rotor core having magnet accommodating holes that open to a first end face and a second end face located opposite to the first end face, and magnets that are accommodated in the magnet accommodating holes and fixed to the rotor core via a thermoplastic resin, an injection step of bringing a first die into contact with the first end surface of the rotor core in a state in which the magnets are accommodated in the magnet accommodating holes, and bringing a second die having a flow path through which the resin flows into contact with the second end surface, and injecting the resin into the magnet accommodating holes through the flow path, In the injection step, the resin is injected into the first mold in a heated state. A method for manufacturing a rotor.
2. In the injection step, the resin is injected into the second mold in a heated state. A method for manufacturing the rotor according to claim 1 .
3. The rotor core is formed by stacking a plurality of iron core pieces, a pressing step of pressing the second end surface with the second mold, thereby pressing the first end surface against the first mold, before the injection step; In the injecting step, the resin is injected in a state in which the first end surface is pressed against the first die. A method for manufacturing a rotor according to claim 1 or 2.
4. When a height from the first end surface to the second end surface of the rotor core is defined as a stacking height, a length of the magnet in a lamination direction of the plurality of iron core pieces is shorter than the lamination height, In the pressing step, the stacking height is reduced by bringing the plurality of iron core pieces into close contact with each other in the stacking direction, and the second end surface is pressed so as to generate a flow space through which the resin flows between the second die and the magnet in the stacking direction. A method for manufacturing the rotor according to claim 3.
5. The rotor core is formed by stacking a plurality of iron core pieces, the plurality of core pieces include a plurality of first core pieces having a dowel that bulges out to one side in a stacking direction of the plurality of core pieces and stacked in a state in which the dowels are connected to each other, and a second core piece having a through hole into which the dowel is inserted and constituting the first end surface or the second end surface, A crushing step is provided before the injection step, in which the tip of the dowel protruding from the through hole is pressed to crush the dowel so that the tip is positioned inside the through hole. A method for manufacturing the rotor according to claim 1 .
6. The rotor core is formed by stacking a plurality of iron core pieces, the plurality of core pieces include a plurality of first core pieces having a dowel that bulges out to one side in a stacking direction of the plurality of core pieces and stacked in a state in which the dowels are connected to each other, and a second core piece having a through hole into which the dowel is inserted and constituting the first end surface, In the injection step, the resin is injected while the tip of the dowel protruding from the through hole is accommodated in an accommodating recess formed in the first mold. A method for manufacturing the rotor according to claim 1 .
Citation Information
Patent Citations
Method for manufacturing rotor for motor
JP2006035831A
Method of manufacturing laminated iron core
JP2014113027A
Method of manufacturing laminated iron core
JP2019161699A
Rotor manufacturing method
JP2015192575A