Method for grinding workpiece

By forming an annular groove on the substrate and adjusting the grinding trajectory, the method stabilizes the grinding process for wafers with thin films, effectively addressing the challenge of grinding hard materials like gallium nitride without damaging the wheel.

JP2024168968APending Publication Date: 2024-12-05DISCO CORP
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
JP2023086065
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-05-25
Publication Date
2024-12-05

AI Technical Summary

Technical Problem

The challenge of stably grinding a wafer with a thin film formed on its surface, particularly when the thin film is a hard material like gallium nitride, which can cause damage to the grinding wheel.

Method used

A method involving forming an annular groove on the substrate surface, using a rotating grinding wheel to grind the substrate while maintaining the wheel's condition by dressing it with the groove, and adjusting the grinding trajectory to prevent wheel deterioration.

Benefits of technology

The method allows for stable grinding of wafers with thin films by preventing wheel damage and ensuring consistent quality, even when grinding hard materials like gallium nitride.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024168968000001_ABST
    Figure 2024168968000001_ABST
Patent Text Reader

Abstract

To grind a wafer provided with a thin film stably.SOLUTION: An annular groove 120 is formed on a rear surface 103 in a semiconductor substrate 101 of a wafer 100 and then the rear surface 103 is ground. Thus, during griding, a lower surface of a grinding wheel 28 is dressed by the annular groove 120. Hence, the structure can inhibit deterioration of conditions of the grinding wheel 28 effectively when the rear surface 103 and a thin film 105 of an outer peripheral end of the semiconductor substrate 101 are ground. Therefore, the wafer 100 provided with the thin film 105 can be ground stably.SELECTED DRAWING: Figure 5
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a method for grinding a workpiece. [Background technology]

[0002] In the manufacturing process of semiconductor devices, streets are formed in a grid pattern on the surface of a wafer, and devices such as ICs and LSIs are formed in the areas partitioned by the streets. After the backside of these wafers is ground to thin them to a specified thickness, they are divided along the streets by a cutting device or the like. In this way, individual semiconductor device chips are manufactured. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] JP 2014-124690 A Summary of the Invention [Problem to be solved by the invention]

[0004] Incidentally, a thin film of a crystal different from that of the wafer may be formed on the surface of the wafer to be ground by epitaxial growth. In epitaxial growth, the thin film is formed not only on the surface of the wafer but also around the outer peripheral edge of the wafer. Therefore, when the back surface of the wafer is ground, the thin film formed on the outer peripheral edge of the wafer is also ground at the same time.

[0005] This type of grinding is more difficult because it involves grinding workpieces that contain two different materials: wafers and thin films. For example, when a thin film of gallium nitride is formed on a silicon wafer, the grinding wheel may become dull or chipped because gallium nitride is a hard material.

[0006] Therefore, an object of the present invention is to establish a method for stably grinding a wafer on which a thin film has been formed by epitaxial growth up to the outer peripheral edge of the wafer. [Means for solving the problem]

[0007] The grinding method for a workpiece of the present invention (the grinding method) is a method for grinding a second surface of a substrate of a workpiece having a substrate and a thin film of a material different from the substrate formed on a first surface of the substrate by epitaxial growth, and is characterized by comprising a groove forming step including forming an annular groove on the second surface of the substrate of the workpiece, and a grinding step including bringing the rotating grinding wheel and the second surface of the substrate of the rotating workpiece relatively close to each other while positioning the rotational trajectory of the grinding wheel at a position overlapping with the rotational axis of the workpiece, and grinding the second surface of the substrate by the grinding wheel at least to the depth of the groove, thereby grinding the workpiece to a desired finishing thickness.

[0008] In addition, the grinding method may further include a first holding step, which is performed before the groove forming step, in which the first surface side of the substrate in the workpiece is held by a first holding surface of a first chuck table, and a second holding step, which is performed after the groove forming step and before the grinding step, in which the first surface side of the substrate in the workpiece is held by a second holding surface of a second chuck table, and the groove forming step may be performed on the workpiece held on the first holding surface of the first chuck table, and the grinding step may be performed on the workpiece held on the second holding surface of the second chuck table.

[0009] In the present grinding method, the substrate may be made of silicon, and the thin film may be made of gallium nitride.

[0010] In addition, in this grinding method, the grinding step may include contacting a portion of the rotating grinding wheel that moves from the center toward the outer peripheral end of the workpiece with the second surface of the substrate of the workpiece.

[0011] In addition, in this grinding method, the grinding step may include contacting a portion of the rotating grinding wheel that moves from the outer peripheral end of the workpiece toward the center with the second surface of the substrate of the workpiece. Effect of the Invention

[0012] In this grinding method, after forming an annular groove on the second surface of the substrate of the workpiece in the groove forming step, the second surface on which the annular groove is formed is ground by a grinding wheel in the grinding step. Therefore, the lower surface of the grinding wheel can be dressed by the annular groove during grinding. Therefore, it is possible to effectively prevent the condition of the grinding wheel from deteriorating when grinding the second surface of the substrate and the thin film. Therefore, it is possible to stably grind the workpiece on which the thin film is formed. [Brief description of the drawings]

[0013] [Figure 1] FIG. 2 is a cross-sectional view showing a structure of a wafer. [Diagram 2] FIG. 2(a) is a cross-sectional view showing the first holding step, and FIG. 2(b) is a perspective view showing the first holding step. [Diagram 3] FIG. 3(a) is an explanatory diagram showing the groove forming step, and FIG. 3(b) is a perspective view showing the groove forming step. [Figure 4] FIG. 4(a) is a cross-sectional view showing the second holding step, and FIG. 4(b) is a perspective view showing the second holding step. [Diagram 5] FIG. 5(a) is an explanatory diagram showing the grinding step, and FIG. 5(b) is a perspective view showing the grinding step. [Figure 6] FIG. [Figure 7] FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0014] The method for grinding a workpiece according to this embodiment is a method for stably grinding a workpiece having a thin film formed by epitaxial growth. As shown in FIG. 1, a wafer 100, which is an example of a workpiece, has a disk-shaped semiconductor substrate 101 and a thin film 105 formed on the semiconductor substrate 101. The semiconductor substrate 101 is a semiconductor substrate made of silicon, and has a front surface 102 which is a first surface, and a back surface 103 which is a second surface.

[0015] A thin film 105 is formed on a surface 102 of the semiconductor substrate 101. The thin film 105 is a thin film formed on the surface 102 by epitaxial growth and made of a material (crystals of this material) different from the material of the semiconductor substrate 101. In this embodiment, the material of the thin film 105 is gallium nitride. Since the thin film 105 is formed on the surface 102 by epitaxial growth, it protrudes from the surface 102 and reaches the outer periphery (side surface) of the semiconductor substrate 101.

[0016] The back surface 103 of the semiconductor substrate 101 is the surface to be ground. That is, the grinding method of the present embodiment is a method for grinding the back surface 103 of the semiconductor substrate 101.

[0017] The steps of the grinding method of this embodiment will be described below.

[0018] [First holding step] In this step, as shown in FIGS. 2(a) and 2(b), the front surface 102 side of the semiconductor substrate 101 of the wafer 100 is held by the first holding surface 12 of the first chuck table 10 which is the chuck table of the cutting device 1.

[0019] The first chuck table 10 includes a porous member 11 and a frame 13 that houses the porous member 11 so that the upper surface of the porous member 11 is exposed. The upper surface of the porous member 11 is a first holding surface 12 that is a holding surface that suction-holds the wafer 100. The first holding surface 12 is connected to a suction source (not shown) to suction-hold the wafer 100. The first chuck table 10 is rotatable about a rotation axis 301 extending in the Z-axis direction (vertical direction).

[0020] In the first holding step, an operator or a transfer device (not shown) places the front surface 102 side of the semiconductor substrate 101 of the wafer 100 on the first holding surface 12 of the first chuck table 10 so that the center of the first holding surface 12 and the center of the wafer 100 overlap. Then, the first holding surface 12 is connected to a suction source, so that the front surface 102 of the semiconductor substrate 101 of the wafer 100 is suction-held by the first holding surface 12 of the first chuck table 10 via the thin film 105.

[0021] [Groove Forming Step] The groove forming step, which is performed after the first holding step, is performed on the wafer 100 held on the first holding surface 12 of the first chuck table 10. In this groove forming step, an annular groove is formed on the back surface 103 of the semiconductor substrate 101 of the wafer 100. That is, an annular groove is formed on the front surface 102 of the first chuck table 10 of the wafer 100 held on the first holding surface 12 of the first chuck table 10 of the cutting device 1.

[0022] 3(a) and 3(b), the cutting device 1 has a cutting mechanism 15 that cuts the wafer 100 held on the first chuck table 10. The cutting mechanism 15 has a cutting blade 17 and a blade rotation mechanism 16 that rotates the cutting blade 17 about a horizontal rotation axis 302. The cutting device 1 also has a first position adjustment mechanism (not shown) that can adjust the relative position between the cutting blade 17 of the cutting mechanism 15 and the first chuck table 10.

[0023] In the groove forming step, the first position adjustment mechanism positions the cutting blade 17 of the cutting mechanism 15 at a groove forming position on the back surface 103 of the semiconductor substrate 101 of the wafer 100. In this embodiment, this groove forming position is a portion of the back surface 103 of the semiconductor substrate 101 that is a predetermined distance inward from the outer circumferential end (outer periphery).

[0024] Then, the first chuck table 10 is rotated as shown by an arrow 401, and the cutting blade 17 is rotated by the blade rotation mechanism 16 as shown by an arrow 402. In this state, the cutting blade 17 is lowered by the first position adjustment mechanism so that the cutting blade 17 cuts into the rear surface 103 of the semiconductor substrate 101 at a groove formation position.

[0025] 3(a) and 3(b), an annular groove 120 is formed at the groove formation position on the back surface 103 of the semiconductor substrate 101 in the wafer 100. The cutting depth of the cutting blade 17, i.e., the depth of the annular groove 120, is set to be equal to or less than the amount by which the wafer 100 is ground in a grinding step described later (the amount by which the wafer 100 is ground). After such annular groove 120 is formed on the rear surface 103, the wafer 100 is removed from the first chuck table 10 by an operator or a transfer device (not shown).

[0026] [Second holding step] The second holding step is performed after the groove forming step and before the grinding step. In this step, as shown in Figures 4(a) and 4(b), the front surface 102 side of the semiconductor substrate 101 of the wafer 100 is held by the second holding surface 22 of the second chuck table 20, which is a chuck table of the grinding device 2.

[0027] The second chuck table 20 includes a porous member 21 and a frame 23 that houses the porous member 21 so that the upper surface of the porous member 21 is exposed. The upper surface of the porous member 21 is a second holding surface 22 that is a holding surface that suction-holds the wafer 100. The second holding surface 22 is connected to a suction source (not shown) to suction-hold the wafer 100. In addition, the second chuck table 20 is rotatable about a rotation axis 303 extending in the Z-axis direction (vertical direction).

[0028] In the second holding step, an operator or a transfer device (not shown) places the front surface 102 of the semiconductor substrate 101 of the wafer 100 on the second holding surface 22 of the second chuck table 20 so that the center of the second holding surface 22 and the center of the wafer 100 overlap. Then, the second holding surface 22 is connected to a suction source, so that the front surface 102 of the semiconductor substrate 101 of the wafer 100 is suction-held by the second holding surface 22 of the second chuck table 20 via the thin film 105.

[0029] [Grinding step] The grinding step performed after the second holding step is performed on the wafer 100 held on the second holding surface 22 of the second chuck table 20. In this grinding step, the back surface 103 of the semiconductor substrate 101 of the wafer 100 is ground by a predetermined grinding amount by the grinding mechanism of the cutting device 1.

[0030] As shown in Figures 5(a) and 5(b), the cutting device 1 has a grinding mechanism 25 equipped with a grinding wheel 28. The grinding mechanism 25 includes a spindle 26 rotated by a motor (not shown) about a rotation axis 304 extending in the Z-axis direction, a mount 27 disposed at the lower end of the spindle 26, and the grinding wheel 28 attached to the mount 27. The grinding wheel 28 includes a wheel base 281 and a plurality of grinding stones 282, each of which has a substantially rectangular parallelepiped shape and is arranged in a ring shape on the lower surface of the wheel base 281.

[0031] The grinding device 2 also has a second position adjustment mechanism (not shown) capable of adjusting the relative position between the grinding mechanism 25 and the second chuck table 20. This second position adjustment mechanism makes it possible to move the grinding wheel 28 of the grinding mechanism 25 relatively close to or away from the second chuck table 20, and to adjust the position of the grinding trajectory of the grinding wheel 28 with respect to the wafer 100.

[0032] In the grinding step using such a grinding mechanism 25, the rotational trajectory of the grinding wheel 28 is positioned at a position overlapping with the rotation axis 303 which is the rotation axis of the wafer 100, and the rotating grinding wheel 28 and the back surface 103 of the semiconductor substrate 101 of the rotating wafer 100 are brought relatively close to each other, and the grinding wheel 28 grinds the back surface 103 of the semiconductor substrate 101 to at least the depth of the annular groove 120 or more, thereby grinding the wafer 100 to the desired finishing thickness.

[0033] Specifically, in the grinding step, first, the second position adjustment mechanism is used to adjust the positions of the grinding mechanism 25 and the second chuck table 20 in the horizontal directions (XY directions) to position the rotation trajectory of the grinding wheel 28 in the grinding mechanism 25 at a position overlapping with the rotation axis 303 that is the rotation axis of the wafer 100. In other words, the relative positions of the grinding mechanism 25 and the second chuck table 20 are adjusted so that the grinding stone 282 of the grinding wheel 28 in the grinding mechanism 25 passes through the center of the wafer 100 held on the second chuck table 20.

[0034] Next, by rotating the second chuck table 20, the wafer 100 held on the second holding surface 22 is rotated about the rotation axis 303 as shown by the arrow 403. Furthermore, by rotating the spindle 26, the grinding wheel 28 is rotated about the rotation axis 304 as shown by the arrow 404. In this state, the grinding mechanism 25 is lowered in the -Z direction using the second position adjustment mechanism. As a result, the rotating grinding wheel 28 and the back surface 103 of the semiconductor substrate 101 of the rotating wafer 100 are relatively close to each other, and the grinding stone 282 of the grinding wheel 28 comes into contact with the back surface 103 of the semiconductor substrate 101 of the wafer 100 to grind the back surface 103.

[0035] In this grinding step, the back surface 103 of the semiconductor substrate 101 is ground by the grinding wheel 28 by a predetermined grinding amount that is at least equal to or greater than the depth of the annular groove 120, thereby grinding the wafer 100 to a desired finishing thickness. During this grinding, the grinding wheel 28 grinds not only the back surface 103 of the semiconductor substrate 101, but also the thin film 105 formed on the outer circumferential edge of the semiconductor substrate 101, as shown in FIG.

[0036] In this grinding step, grinding is performed from the center of the semiconductor substrate 101 of the wafer 100 toward the outer periphery (inner and outer grinding). That is, in this grinding step, a portion of the rotating grinding wheel 28 (grinding stone 282) moving from the center of the wafer 100 toward the outer periphery is brought into contact with the back surface 103 of the semiconductor substrate 101 of the wafer 100.

[0037] 5(a), the second holding surface 22 of the second chuck table 20 is formed into a conical surface with the apex at the center. The second chuck table 20 is tilted so that a radius portion of the back surface 103 of the semiconductor substrate 101 of the wafer 100 held on the second holding surface 22 is parallel to the lower surface of the grinding wheel 28 (grinding stone 282). Here, the radius portion of the back surface 103 of the semiconductor substrate 101 is a portion of the back surface 103 that contacts the lower surface of the grinding wheel 28 (grinding stone 282).

[0038] In this embodiment, the inclination of the second chuck table 20, the rotation direction of the second chuck table 20, and the rotation direction of the grinding wheel 28 are set so that the portion of the grinding wheel 28 in contact with the radial portion of the back surface 103 moves from the center of the wafer 100 toward the outer circumferential edge while grinding the back surface 103, as shown in FIG. 6.

[0039] As described above, in this embodiment, the annular groove 120 is formed on the back surface 103 of the semiconductor substrate 101 of the wafer 100 in the groove forming step, and then the back surface 103 with the annular groove 120 formed therein is ground in the grinding step. Therefore, during grinding, the lower surface of the grinding wheel 28 (the lower surface of the grinding stone 282) can be dressed by the annular groove 120 (for example, to regenerate the cutting edge of abrasive grains that have become dull).

[0040] Therefore, it is possible to effectively prevent the condition of the grinding wheel 28 from deteriorating (for example, the occurrence of blemishes or chipping) when grinding the back surface 103 and the thin film 105 on the outer peripheral edge of the semiconductor substrate 101. That is, the back surface 103 and the thin film 105 can be effectively ground while preventing the condition of the grinding wheel 28 from deteriorating. Therefore, it is possible to stably grind the wafer 100 on which the thin film 105 is formed.

[0041] 6, in the grinding step of this embodiment, a portion of the grinding wheel 28 (grinding stone 282) moving from the center of the wafer 100 toward the outer peripheral edge is brought into contact with the back surface 103 of the semiconductor substrate 101 (inner and outer grinding). In this case, the grinding wheel 28 that has ground the back surface 103 is dressed at the outer corner 121 of the annular groove 120, and then grinds the thin film 105.

[0042] Therefore, the grinding wheel 28 is dressed (sharpened) by the surface 102 immediately before grinding the thin film 105 of gallium nitride, which is difficult to grind, and therefore the thin film 105 can be ground well.

[0043] Furthermore, in the internal and external grinding, it is easy to discharge the grinding debris made of gallium nitride of the thin film 105 to the outside of the wafer 100. For this reason, it is preferable that the annular groove 120 is formed in a position close to the outer circumferential edge of the semiconductor substrate 101.

[0044] In the grinding step, outer and inner grinding may be performed to grind the back surface 103 of the semiconductor substrate 101 of the wafer 100 from the outer circumferential edge toward the center. That is, in the grinding step, a portion of the rotating grinding wheel 28 (grinding stone 282) moving from the outer circumferential edge toward the center of the wafer 100 may be brought into contact with the back surface 103 of the semiconductor substrate 101 of the wafer 100.

[0045] In this case, the inclination of the second chuck table 20, the rotation direction of the second chuck table 20 and the rotation direction of the grinding wheel 28 are set so that the portion of the grinding wheel 28 (grinding stone 282) in contact with the radial portion of the back surface 103 of the semiconductor substrate 101 of the wafer 100 held on the second holding surface 22 moves from the outer peripheral end toward the center of the wafer 100 while grinding the back surface 103, as shown in FIG. 7.

[0046] In this configuration, the grinding wheel 28, which has ground the thin film 105, is dressed by the inner corner 122 of the annular groove 120, and then grinds the back surface 103 of the semiconductor substrate 101. Therefore, immediately after the grinding wheel 28 has been ground and its condition has deteriorated due to grinding the gallium nitride thin film 105, the grinding wheel 28 is dressed by the annular groove 120, and its condition is restored. Therefore, the back surface 103 of the semiconductor substrate 101 can be satisfactorily ground by the grinding wheel 28 in a restored condition.

[0047] In the grinding method of this embodiment, in the groove forming step, after the wafer 100 is held by the first chuck table 10 of the cutting device 1 (first holding step), an annular groove 120 is formed in the back surface 103 of the semiconductor substrate 101 of the wafer 100 (groove forming step). Furthermore, thereafter, the wafer 100 is removed from the first chuck table 10 and held by the second chuck table 20 of the grinding device 2 (second holding step), and the back surface 103 and thin film 105 of the semiconductor substrate 101 of the wafer 100 are ground (grinding step).

[0048] In this regard, the grinding method of the present embodiment may be performed using one processing apparatus having a holding mechanism for holding the wafer 100, a groove forming mechanism capable of forming annular grooves 120 on the back surface 103 of the semiconductor substrate 101 of the wafer 100, and a grinding mechanism capable of grinding the back surface 103. As the holding mechanism and the groove forming mechanism, for example, the first chuck table 10 and the cutting mechanism 15 shown in Fig. 3(a) can be used. Also, as the grinding mechanism, for example, the grinding mechanism 25 shown in Fig. 5(a) can be used.

[0049] In this case, after the wafer 100 is held by a chuck table of a processing device (holding step), an annular groove 120 is formed in the back surface 103 of the semiconductor substrate 101 of the wafer 100 by a groove forming mechanism (groove forming step). Furthermore, thereafter, the back surface 103 and the thin film 105 of the semiconductor substrate 101 of the wafer 100 held on the chuck table are ground by a grinding mechanism (grinding step).

[0050] Even with this configuration, the annular groove 120 prevents the condition of the grinding wheel 28 from deteriorating, while the back surface 103 and the thin film 105 can be ground satisfactorily. Furthermore, in this configuration, the number of chuck tables that hold the wafer 100 can be reduced to one, making it possible to simplify the structure of the apparatus.

[0051] In the present embodiment, in the groove forming step, the cutting blade 17 of the cutting device 1 forms the annular groove 120 on the back surface 103 of the semiconductor substrate 101 of the wafer 100. In this regard, in the groove forming step, the annular groove 120 may be formed on the back surface 103 using laser light. [Explanation of symbols]

[0052] 1: Cutting device, 2: Grinding device, 10: first chuck table, 11: porous member, 12: first holding surface, 13: frame body, 15: cutting mechanism, 16: blade rotation mechanism, 17: cutting blade, 20: second chuck table, 21: porous member, 22: second holding surface, 23: frame body, 25: grinding mechanism, 26: spindle, 27: mount, 28: grinding wheel, 100: wafer, 101: semiconductor substrate, 102: front surface, 103: back surface, 105: thin film, 120: groove, 121: outer corner, 122: inner corner, 281: Wheel base, 282: Grinding wheel

Claims

1. A method for grinding a workpiece, the method comprising the steps of: grinding a second surface of a substrate of a workpiece having a substrate and a thin film formed on a first surface of the substrate by epitaxial growth and made of a material different from that of the substrate, the method comprising the steps of: a groove forming step including forming an annular groove in the second surface of the substrate of the workpiece; a grinding step including bringing the rotating grinding wheel and the second surface of the substrate of the rotating workpiece relatively close to each other in a state where the rotation locus of the grinding wheel is positioned at a position overlapping with the rotation axis of the workpiece, and grinding the second surface of the substrate by the grinding wheel at least to a depth equal to or greater than the depth of the groove, thereby grinding the workpiece to a desired finishing thickness. A method for grinding a workpiece.

2. a first holding step, which is performed before the groove forming step, of holding the first surface side of the substrate of the workpiece by a first holding surface of a first chuck table; and a second holding step, which is performed after the groove forming step and before the grinding step, of holding the first surface side of the substrate of the workpiece by a second holding surface of a second chuck table; The groove forming step is performed on the workpiece held on the first holding surface of the first chuck table, The grinding step is performed on the workpiece held on the second holding surface of the second chuck table.

2. The method for grinding a workpiece according to claim 1.

3. the substrate is formed of silicon and the thin film is formed of gallium nitride; 2. The method for grinding a workpiece according to claim 1.

4. The grinding step includes contacting a portion of the rotating grinding wheel moving from the center toward the outer peripheral edge of the workpiece with the second surface of the substrate of the workpiece. The method for grinding a workpiece according to any one of claims 1 to 3.

5. The grinding step includes contacting a portion of the rotating grinding wheel, the portion moving from the outer circumferential edge of the workpiece toward the center, with the second surface of the substrate of the workpiece. The method for grinding a workpiece according to any one of claims 1 to 3.

Citation Information

Patent Citations

  • Grinding method and grinding device

    JP2014124690A