Pellicle membrane for lithography equipment

A pellicle film with metal silicide crystals in a silicon-based matrix addresses the challenges of high power and temperature in EUV lithography by maintaining high EUV transmission and lower operating temperatures, enhancing emissivity and mechanical strength through controlled manufacturing processes.

JP2024536499APending Publication Date: 2024-10-04ASML NETHERLANDS BV
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
JP2024522232
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2021-10-22
Filing Date
2022-10-07
Publication Date
2024-10-04

AI Technical Summary

Technical Problem

Existing pellicles in EUV lithographic apparatuses face challenges in withstanding high power and maintaining low operating temperatures due to high EUV radiation absorption, leading to potential delamination and degradation, while also allowing undesired out-of-band radiation to degrade image quality and cause heating effects.

Method used

A pellicle film composed of metal silicide crystals in a silicon-based matrix with high emissivity and controlled crystal structure, allowing for high EUV transmission and lower operating temperatures, achieved through controlled annealing, ion bombardment, and doping to enhance mechanical strength.

Benefits of technology

The pellicle film maintains high EUV transmission and lower operating temperatures, enabling higher source power usage with reduced degradation and improved image quality by minimizing crystal size and enhancing emissivity without altering chemical composition.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024536499000001_ABST
    Figure 2024536499000001_ABST
Patent Text Reader

Abstract

A pellicle membrane comprising a population of metal silicide crystals in a silicon-based matrix, the pellicle membrane having an emissivity of 0.3 or greater, a method of manufacturing the pellicle membrane, a pellicle assembly, and a lithographic apparatus comprising such a pellicle membrane or pellicle assembly, and the use of such a pellicle membrane, pellicle assembly, or lithographic apparatus in a lithographic apparatus or method are also described.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] [CROSS REFERENCE TO RELATED APPLICATIONS]

[0001] This application claims priority to European Patent Application No. 21204216.2, filed October 22, 2021, the entire contents of which are incorporated by reference into this specification.

[0002] The present invention relates to a pellicle membrane for a lithographic apparatus, an assembly for a lithographic apparatus, a method for manufacturing a pellicle membrane, and the use of a pellicle membrane in a lithographic apparatus or method. [Background technology]

[0003] A lithographic apparatus is a machine constructed to apply a desired pattern onto a substrate. Lithographic apparatus can be used, for example, in the manufacture of integrated circuits (ICs). A lithographic apparatus can project a pattern from a patterning device (e.g. mask) onto a layer of radiation-sensitive material (resist) provided on the substrate.

[0004]

[0003] The wavelength of radiation used by a lithographic apparatus to project a pattern onto a substrate determines the minimum size of features that can be formed on the substrate. Lithographic apparatus using EUV radiation, which is electromagnetic radiation having a wavelength in the range of 4-20 nm, can be used to form smaller features on a substrate compared to conventional lithographic apparatus (which may use electromagnetic radiation having a wavelength of 193 nm, for example).

[0005]

[0004] A lithographic apparatus includes a patterning device (e.g. a mask or reticle). Radiation is provided through or reflected from the patterning device to form an image on a substrate. To protect the patterning device from airborne particles and other forms of contamination, a membrane assembly, also called a pellicle, may be provided. Contaminants on the surface of the patterning device may cause manufacturing defects on the substrate.

[0006]

[0005] Pellicles may also be provided to protect optical components other than the patterning device. Pellicles may also be used to provide a passageway for lithographic radiation between areas of the lithographic apparatus that are sealed from one another. Pellicles may also be used as filters, such as spectral purity filters, or as part of a dynamic gas lock in the lithographic apparatus.

[0007]

[0006] The mask assembly may include a pellicle that protects the patterning device (e.g., mask) from particle contaminants. The pellicle may be supported by a pellicle frame to form a pellicle assembly. The pellicle may be attached to the frame, for example, by gluing or otherwise attaching an edge region of the pellicle to the frame. The frame may be permanently or removably attached to the patterning device.

[0008]

[0007] The presence of a pellicle in the path of the EUV radiation beam requires that the pellicle have a high EUV transmittance. A high EUV transmittance results in a greater proportion of the incident radiation passing through the pellicle. Furthermore, a reduced amount of EUV radiation absorbed by the pellicle may reduce the operating temperature of the pellicle. Since the transmittance depends at least in part on the thickness of the pellicle, it is desirable to provide a pellicle that is as thin as possible while still maintaining sufficient strength to withstand the sometimes harsh environment within a lithographic apparatus.

[0009]

[0008] It would therefore be desirable to provide a pellicle that can withstand the harsh environment of a lithographic apparatus, particularly an EUV lithographic apparatus, and in particular, a pellicle that can withstand higher powers than have been available hitherto available.

[0010]

[0009] Although this application refers generally to pellicles in the context of lithographic apparatus, and in particular EUV lithographic apparatus, it should be understood that the present invention is not limited to only pellicles and lithographic apparatus and that the subject matter of the present invention can be used in any other suitable apparatus or context.

[0011]

[0010] For example, the method of the present invention may be similarly applied to spectral purity filters. Some EUV radiation sources, such as those that use plasma to generate EUV radiation, emit not only the desired "in-band" EUV radiation, but also undesired (out-of-band) radiation. This out-of-band radiation is most prominent in the deep UV (DUV) radiation range (100-400 nm). Furthermore, for some EUV radiation sources, such as laser-produced plasma EUV radiation sources, the radiation from the laser, typically at 10.6 microns, causes significant out-of-band radiation.

[0012]

[0011] Spectral purity is required in lithographic apparatus for several reasons. One reason is that resist is sensitive to out-of-band wavelengths of radiation and therefore the quality of the pattern applied to the resist may be degraded if the resist is exposed to such out-of-band radiation. Furthermore, out-of-band infrared radiation, for example the 10.6 micron radiation in some laser-produced plasma radiation sources, can result in undesirable and unnecessary heating of the patterning device, substrate and optical components in the lithographic apparatus. Such heating can lead to damage to the above elements, reduced lifetimes, and / or defects or distortions in the pattern projected and applied onto the resist-coated substrate.

[0013]

[0012] A typical spectral purity filter may be formed from a silicon base structure (e.g. a silicon grating or other member with openings) coated with a reflective metal such as molybdenum. In use, a typical spectral purity filter may be subjected to high heat loads, e.g. from incident infrared and EUV radiation. This heat load may cause the temperature of the spectral purity filter to exceed 800°C. Under this high heat load, the coating may spall due to differences in the linear expansion coefficient between the reflective molybdenum coating and the underlying silicon support structure. The spalling and degradation of the silicon base structure is accelerated by the presence of hydrogen, which is often used as a gas in the environment in which the spectral purity filter is used to suppress debris (e.g. debris such as particles) from entering or leaving certain parts of the lithographic apparatus. In this way, a spectral purity filter may be used as a pellicle and vice versa. Thus, any reference in this application to a "pellicle" is also a reference to a "spectral purity filter". Although reference is made primarily to a pellicle in this application, all features apply equally to a spectral purity filter.

[0014]

[0013] The present invention has been devised in an attempt to address at least some of the problems identified above. Summary of the Invention

[0015]

[0014] According to a first aspect of the present invention, there is provided a pellicle film including a population of metal silicide crystals in a silicon-based matrix, the pellicle film having an emissivity of 0.3 or greater. The silicon-based matrix may include silicon crystals.

[0016]

[0015] The emissivity of the pellicle film is related to the temperature at which the pellicle film operates in the lithographic apparatus. It is desirable for the pellicle film to operate at a lower temperature, and therefore a higher emissivity is required. Alternatively, or in addition, a higher emissivity also allows the lithographic apparatus to operate at a higher source power, because the pellicle film can still operate at a suitable temperature despite the increase in source power due to the increased emissivity of the pellicle film.

[0017]

[0016] The emissivity may be 0.33 or greater, 0.35 or greater, 0.37 or greater, or 0.4 or greater.

[0018]

[0017] The pellicle film may have a transmittance of 90% or more, 91% or more, 92% or more, 93% or more, 94% or more, or 95% or more. The transmittance of the pellicle film can be high because it does not contain atoms that absorb EUV radiation, or contains only low levels of atoms that absorb EUV radiation. Due to the emissivity of the pellicle film, the operating temperature of the film can be lowered and / or the pellicle can be used with higher source power. In general, an increase in transmittance leads to a decrease in emissivity and vice versa. The present invention provides good transmittance together with good emissivity.

[0019]

[0018] The pellicle membrane may include nitrogen in an amount of up to about 5 atomic %. Nitrogen may be present in an amount of up to about 4 atomic %, up to about 3 atomic %, up to about 2 atomic %, or up to about 1 atomic %.

[0020]

[0019] Even low nitrogen concentrations, such as 5 atomic % or less, have been found to lead to lower resistivity (higher emissivity), which in turn leads to lower operating temperatures in the lithographic apparatus for the same source power, or allows the use of higher source powers.

[0021] The metal suicide crystals and / or silicon crystals may have a diameter of 30 nm or less.

[0022]

[0021] The diameter of the crystals can be determined through scanning electron microscope images. The diameter can be measured as the maximum dimension of an individual crystal. The metal silicide crystals can have a diameter of 28 nm or less or 25 nm or less. It is preferred that more than 90%, more than 95%, more than 98%, or more than 99% of the metal silicide crystals and / or silicon crystals have a diameter of 30 nm or less, 28 nm or less, or 25 nm or less.

[0023]

[0022] The pellicle film that includes metal silicide crystals in a silicon-based matrix usually has a lower emissivity than the pellicle film that includes molybdenum silicide nitride. Although the pellicle film that includes metal silicide crystals in a silicon-based matrix usually has a higher transmittance than the pellicle film that includes molybdenum silicide nitride, this higher transmittance does not compensate for the lower emissivity with respect to the operating temperature. Therefore, at the same radiation source power, the pellicle film that includes metal silicide crystals in a silicon-based matrix has a higher operating temperature. This is disadvantageous in that higher temperatures are associated with faster chemical reactions and therefore faster degradation. This is believed to be due to low emissivity silicon crystals or amorphous silicon, which are distinguished from metal silicide crystals with high emissivity. In addition, compared to a molybdenum silicide nitride composite pellicle, where the distance between the molybdenum silicide crystals in the molybdenum silicide nitride composite is less than 10 nm, the distance between the molybdenum silicide crystals in the pellicle film containing metal silicide crystals in a silicon matrix is ​​longer, and in addition, the metal silicide crystals themselves are larger. Therefore, it has been found that reducing the crystal size provides improved emissivity without the need to change the chemical composition of the pellicle film. Therefore, the present invention provides a pellicle film with improved emissivity without necessarily changing the chemical composition of the pellicle film. This is achieved by affecting the crystal structure of the pellicle film so that smaller and more mixed grains are formed in the final pellicle, which in turn provides improved emissivity.

[0024]

[0023] The metal silicide crystals and / or silicon crystals may be aligned substantially perpendicular to the surface of the pellicle membrane.

[0025]

[0024] The crystal size in the film is important with respect to emissivity. Therefore, the dimensionality of the film can be exploited to form smaller crystals. Pellicle films are thin, for example 40 nm or less, 30 nm or less, 20 nm or less, 15 nm or less, or 12 nm or less. Therefore, by placing the crystals perpendicular to the surface, it is possible to limit the crystal size and place multiple parallel crystal "pillars". This serves to improve the emissivity of the film.

[0026] At least a portion of the population of metal suicide crystals and / or silicon crystals may be present across the thickness of the film, such that the length of the crystals may be the same as the thickness of the pellicle film.

[0027]

[0026] The pellicle film can be a multilayer film. A multilayer film is a film in which there are stacked layers with different chemical or physical properties. The pellicle film can include a layer that includes a population of metal silicide crystals in a silicon-based matrix, which optionally includes silicon crystals disposed between one or more layers that include silicon-molybdenum alloy.

[0028]

[0027] The metal silicide crystals may be molybdenum silicide crystals, which are suitable for use in lithographic apparatus and have high emissivity leading to lower operating temperatures for a given source power and / or the ability to withstand higher source powers.

[0029]

[0028] The silicon matrix may comprise p-Si or SiN. p-Si, as is well understood, is used in pellicle membranes for lithographic apparatus and has a high emissivity to EUV radiation.

[0030]

[0029] The silicon-based matrix may be doped. Since the silicon-based matrix has a low emissivity, it may be doped to increase the emissivity. The silicon-based matrix may be doped with one or more of boron, phosphorus, and yttrium. The metal silicide crystals, preferably molybdenum silicide crystals, are separated from each other by non-conductive silicon crystals that limit the emissivity of the entire pellicle film. Doping increases the conductivity of the silicon crystals, thus increasing the emissivity. In addition, it has been found that pellicle films that include a silicon-based matrix rather than a silicon nitride matrix have lower strength. Without wishing to be bound by scientific theories, one reason for the above is believed to be due to the higher resistance of the silicon nitride matrix to HF etching. Doping increases the etching resistance of the film, thereby limiting the adverse effect of inadvertent overetching on the film's strength.

[0031]

[0030] The dopants boron, phosphorus, and / or yttrium are 10 15 cm -3 ~10 21 cm -3 A pure p-Si film contains silicon at approximately 10 21 cm -3 By doping with boron at a concentration of 1000 MPa, the strength can be increased from 2.7 GPa to 3.7 GPa, thus increasing the mechanical strength of the pellicle membrane. Similarly, doping with boron increases the emissivity of pure p-Si from 0.02 to 0.06, thus increasing the overall emissivity of the membrane.

[0032] The pellicle membrane can include about 10 atomic % to about 30 atomic % molybdenum, optionally about 15 atomic % to about 25 atomic % molybdenum, or optionally about 20 atomic % molybdenum.

[0033]

[0032] The pellicle membrane may contain about 90 atomic % to about 70 atomic % silicon, optionally about 90 atomic % to about 65 atomic % silicon, optionally about 85 atomic % to about 70 atomic % silicon, or optionally about 75 atomic % silicon.

[0034]

[0033] Thus, the pellicle film may comprise about 10 atomic % to about 30 atomic % molybdenum, about 90 atomic % to about 65 atomic % silicon, and about 0 atomic % to about 5 atomic % nitrogen. It is clear that small amounts of non-functional impurities may be present. In addition, dopants may be provided in the concentrations mentioned herein.

[0035]

[0034] The thickness of the film may be about 10 nm to about 100 nm. The thickness of the film may be about 12 nm, about 15 nm, about 20 nm, about 25 nm, about 30 nm, about 40 nm, about 50 nm, about 60 nm, about 70 nm, about 80 nm, or about 90 nm.

[0036] According to the second aspect of the present invention, there is provided a method for manufacturing a pellicle film.The method may include at least one step selected from: a) removing the film from an annealing furnace operating at an annealing temperature, exposing the film to ambient temperature and rapidly cooling the film; b) annealing the film for a period of less than one hour; c) bombarding the film with ions during film deposition; d) providing a capping layer on the film before annealing; e) placing the film at a temperature of about 500°C or more on a surface at a temperature of about 100°C or less to induce crystallization; or f) heating one side of an amorphous film to above glass transition temperature to induce crystallization from the other side of the amorphous film.

[0037]

[0036] The film may comprise a population of metal silicide crystals in a silicon matrix, optionally including silicon crystals. The film may be a film according to the first aspect of the invention. Thus, the method may include providing a film comprising a population of metal silicide crystals in a silicon matrix, optionally including silicon crystals. Alternatively, the method may include providing a film comprising amorphous metal silicide regions in an amorphous silicon material. It should be understood that reference to a pellicle in the context of the second aspect of the invention also includes reference to a film that is at least partially amorphous and that is converted into a crystalline or semi-crystalline film suitable for use in a lithographic apparatus. Thus, a film in the context of the second aspect of the invention may be a precursor film of a final pellicle film. The film referred to in the second aspect of the invention is converted into a final pellicle film by the method described herein. Once the film has been treated according to the method of the second aspect of the invention, the film is suitable for use in a lithographic apparatus. As the chemical composition of the film is not, or effectively is not, changed during processing according to the method of the second aspect of the invention, the composition of the film can be any of those as described in relation to the first aspect of the invention.

[0038]

[0037] The method of the second aspect of the present invention provides a pellicle membrane having a desirable emissivity of 0.3 or greater. This can be achieved in a number of ways.

[0039]

[0038] Previously, annealing was performed at a temperature of approximately 900°C for 8 hours, after which the furnace was switched off and the wafers remained in the furnace for 1.5-2 hours. This long annealing process is intended to prevent changes to the pellicle membrane during operation, which would result in the formation of large grains in the membrane. It has been found that by rapidly cooling the membrane by removing it from the furnace and allowing it to reach room temperature, the membrane is able to retain the microstructure present at 900°C, avoiding the increase in crystal size. This in turn leads to a good emissivity of the membrane without changing its chemical composition.

[0040]

[0039] It has also been found that extensive grain growth can be prevented by heating the film to an annealing temperature, e.g., approximately 90°C, quickly, particularly for 30 seconds or less, 25 seconds or less, 20 seconds or less, 15 seconds or less, 10 seconds or less, or 5 seconds or less, annealing for a period of 1 minute to 10 minutes, and then allowing the film to cool.

[0041]

[0040] By bombarding the substrate on which the pellicle film is formed during deposition, for example with high energy ions of Kr or Ar, the nucleation mechanism and the final microstructure of the film can be altered, making it possible to control the directionality of crystal growth.

[0042]

[0041] The microstructure of the film can also be influenced by providing a capping layer on the film prior to annealing, for example, covering the film with a TEOS layer prior to annealing provides more heterogeneous nucleation sites for grains to begin growing.

[0043]

[0042] The microstructure can also be controlled by controlling the directional growth of the crystals within it. Crystallization can be induced by placing a heated film on a cooler surface. Similarly, crystallization can be initiated from the cooler bottom surface by heating an amorphous sample above the glass transition temperature, for example, about 5°C, about 10°C, about 15°C, or about 20°C above the glass transition temperature, for a period of time.

[0044]

[0043] Except where these methods are incompatible with each other or exclude each other, each of the methods can be combined as necessary to provide a pellicle membrane having the desired microstructure that achieves a membrane with the desired emissivity of 0.3 or greater.

[0045]

[0044] Annealing can be carried out for about 30 minutes or less, about 20 minutes or less, about 15 minutes or less, about 10 minutes or less, or about 5 minutes or less.

[0046]

[0045] Annealing may be performed at an annealing temperature of about 600° C. to about 900° C., optionally about 600° C. to about 800° C., or optionally about 650° C. to about 700° C. Annealing is performed at a temperature of about 750° C. or less, optionally about 700° C. or less, optionally about 650° C. or less, or optionally about 600° C. or less.

[0047]

[0046] Annealing may be carried out for a period of up to 10 hours, up to 9 hours, up to 8 hours, or from about 1 hour to about 8 hours.

[0048]

[0047] The method may include doping the pellicle membrane, and optionally the dopant is one or more of boron, phosphorus, and yttrium. 15 cm -3 ~10 21 cm -3 It may be present in concentrations of about

[0049] According to a third aspect of the present invention there is provided a pellicle assembly comprising a pellicle membrane according to the first aspect of the present invention or manufactured by the method of the second aspect of the present invention.

[0050] According to a fourth aspect of the present invention, there is provided a lithographic apparatus comprising a pellicle membrane according to the first aspect of the present invention or a pellicle assembly according to the third aspect of the present invention.

[0051]

[0050] According to a fifth aspect of the present invention there is provided the use of a pellicle membrane, a pellicle assembly, a lithographic apparatus or a method according to any of the first to fourth aspects of the present invention in a lithographic apparatus or method.

[0052]

[0051] It is apparent that any feature described with respect to one embodiment may be combined with any feature described with respect to another embodiment, and that all such combinations are expressly contemplated and disclosed in this document. [Brief description of the drawings]

[0053]

[0052] Some embodiments of the invention will now be described, by way of example only, with reference to the accompanying schematic drawings in which like reference symbols indicate corresponding parts, in which:

[0054] [Figure 1] FIG. 1 depicts a lithographic apparatus according to an embodiment of the invention. [Diagram 2] FIG. 2 is an SEM image of a damaged film according to the first embodiment of the invention, showing phase separation between silicon crystals and molybdenum silicide crystals. [Diagram 3]

[0055] FIG. 3 is an array of SEM images showing the microstructure of films having different thicknesses and made at different annealing temperatures. [Figure 4]

[0056] FIG. 4 is a graph comparing operating temperature with EUV transmittance operating at 600 W.

[0055]

[0057] The features and advantages of the present invention will become more apparent from the following detailed description taken in conjunction with the drawings, in which like reference characters identify corresponding elements throughout and in which like reference numbers generally indicate identical, functionally similar, and / or structurally similar elements. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0056]

[0058] Figure 1 shows a lithographic system including a pellicle 15 (also called a membrane assembly) according to the present invention. The lithographic system comprises a radiation source SO and a lithographic apparatus LA. The radiation source SO is configured to generate an extreme ultraviolet (EUV) radiation beam B. The lithographic apparatus LA comprises an illumination system IL, a support structure MT configured to support a patterning device MA (e.g. a mask), a projection system PS, and a substrate table WT configured to support a substrate W. The illumination system IL is configured to condition the radiation beam B before it is incident on the patterning device MA. The projection system is configured to project the radiation beam B (currently patterned by the mask MA) onto the substrate W. The substrate W may contain an already formed pattern. In this case, the lithographic apparatus aligns the patterned radiation beam B with the pattern already formed on the substrate W. In this embodiment, a pellicle 15 is shown in the path of the radiation to protect the patterning device MA. It will be apparent that the pellicle 15 may be placed in any desired location and may be used to protect any of the mirrors within the lithographic apparatus.

[0057]

[0059] The source SO, illumination system IL, and projection system PS may all be constructed and arranged such that they can be isolated from the external environment. A gas at a pressure below atmospheric pressure (e.g. hydrogen) may be provided in the source SO. A vacuum may be provided in the illumination system IL and / or projection system PS. A small amount of gas at a pressure well below atmospheric pressure (e.g. hydrogen) may be provided in the illumination system IL and / or projection system PS.

[0058]

[0060] The radiation source SO shown in Figure 1 is of a type that may be called a laser-produced plasma (LPP) source. 2A laser (which may be a laser) is arranged to deposit energy via a laser beam into a fuel, such as tin (Sn), provided from a fuel emitter. Although tin is referred to in the following description, any suitable fuel may be used. The fuel may be in the form of, for example, a liquid and may be, for example, a metal or an alloy. The fuel emitter may comprise a nozzle configured to direct the tin, for example in the form of droplets, along a trajectory towards the plasma formation region. The laser beam is incident on the tin in the plasma formation region. A plasma is created in the plasma formation region by the deposition of the laser energy in the tin. Radiation, including EUV radiation, is emitted from the plasma during de-excitation and recombination of the ions of this plasma.

[0059]

[0061] The EUV radiation is collected and focused by a near-normal incidence radiation collector (sometimes more commonly referred to as a normal incidence radiation collector). The collector may have a multi-layer structure arranged to reflect EUV radiation (e.g., EUV radiation having a desired wavelength, such as 13.5 nm). The collector may have an elliptical configuration with two elliptical foci. The first focus may be located at the plasma formation region and the second focus may be at an intermediate focus, as described below.

[0060]

[0062] The laser may be separate from the radiation source SO. In this case, the laser beam may be delivered from the laser to the radiation source SO using, for example, a beam delivery system (not shown) including appropriate directing mirrors and / or beam expanders, and / or other optics. The laser and radiation source SO may be collectively referred to as a radiation system.

[0061]

[0063] Radiation reflected by the collector forms a radiation beam B. The radiation beam B focuses to a point forming an image of the plasma formation region, which acts as a virtual radiation source for the illumination system IL. The point at which the radiation beam B focuses may be referred to as an intermediate focus. The radiation source SO is arranged such that the intermediate focus is located at or near an opening of a source closure structure.

[0062]

[0064] A radiation beam B travels from a radiation source SO into an illumination system IL, which is configured to condition the radiation beam. The illumination system IL may include a facetted field mirror device 10 and a facetted pupil mirror device 11. Together the facetted field mirror device 10 and the facetted pupil mirror device 11 impart a desired cross-sectional shape and a desired angular distribution to the radiation beam B. The radiation beam B travels from the illumination system IL and is incident on a patterning device MA, which is held by a support structure MT. The patterning device MA reflects and patterns the radiation beam B. The illumination system IL may include other mirrors or devices in addition to or instead of the facetted field mirror device 10 and the facetted pupil mirror device 11.

[0063]

[0065] Following reflection from the patterning device MA, the patterned radiation beam B enters a projection system PS. The projection system comprises a number of mirrors 13, 14 configured to project the radiation beam B onto a substrate W held by a substrate table WT. The projection system PS may apply a demagnification factor to the radiation beam, thereby forming an image having smaller features than corresponding features on the patterning device MA. For example a demagnification factor of four may be applied. Although the projection system PS has two mirrors 13, 14 in Figure 1, the projection system may include any number of mirrors (for example six mirrors).

[0064]

[0066] The radiation source SO shown in Figure 1 may include components not shown. For example, a spectral filter may be provided within the radiation source. The spectral filter may be substantially transmissive to EUV radiation, while being substantially blocking radiation of other wavelengths, such as infrared radiation.

[0065]

[0067] In one embodiment, the membrane assembly 15 is a pellicle for a patterning device MA for EUV lithography. The membrane assembly 15 of the present invention can be used as a dynamic gas lock, or a pellicle, or for another purpose. In one embodiment, the membrane assembly 15 includes a membrane formed from at least one membrane layer having an emissivity of 0.3 or greater. To ensure maximum EUV transmission and minimal impact on imaging performance, the membrane is preferably supported only at its edges.

[0066]

[0068] If the patterning device MA is left unprotected, contaminants may necessitate cleaning or discarding the patterning device MA. Cleaning the patterning device MA interrupts valuable production time, discarding the patterning device MA is costly, and replacing the patterning device MA also interrupts valuable production time.

[0067]

[0069] FIG. 2 shows a scanning electron microscope (SEM) image of a broken pellicle film according to the first embodiment of the present invention. Silicon crystals and molybdenum silicide crystals can be seen. According to the present invention, by controlling the microstructure of the pellicle film, a pellicle film with good emissivity and high EUV transmittance can be obtained. For example, the emissivity can be 0.3 or more. The transmittance can be 90% or more, or 92% or more. When used in an EUV lithography apparatus, a combination of high emissivity and high EUV transmittance is desirable.

[0068]

[0070] Figure 3 includes various SEM images of different pellicle films annealed at different temperatures and with different thicknesses. The crystal size increases with annealing temperature. Therefore, if smaller crystals are desired, a lower annealing temperature can be employed. All other conditions were kept constant, and only the thickness and annealing time were changed.

[0069]

[0071] Figure 4 compares the operating temperature and EUV transmittance of three films according to the invention (so-called MoSiSi, because it contains molybdenum silicide in a silicon matrix) against a pellicle film of a molybdenum nitride silicide composite, which contains much more nitrogen (up to approximately 20 atomic %) than the film of the invention, which contains nitrogen (up to approximately 5 atomic %). It can be seen that the film of the invention operates at a similar temperature while having a higher EUV transmittance. The references to 17.5%, 20%, and 22.5% refer to the atomic percentage of molybdenum in the various samples.

[0070]

[0072] Thus, the present invention provides a pellicle membrane that has an emissivity of at least 0.3 that allows it to operate in a lithographic tool, particularly an EUV tool, while having comparable or higher transmittance compared to other pellicle membranes. The methods described herein provide multiple ways in which such a membrane can be formed.

[0071]

[0073] Whilst specific embodiments of the invention have been described above, it will be apparent that the invention can be practiced otherwise than as described above.

[0072]

[0074] The above description is intended to be illustrative rather than limiting. Thus, it will be apparent to one skilled in the art that modifications may be made to the invention as described without departing from the scope of the appended claims.

Claims

1. A pellicle film comprising a population of metal silicide crystals in a silicon-based matrix, the pellicle film having an emissivity of 0.3 or greater.

2. 2. The pellicle membrane of claim 1, having a transmittance of 90% or more, 91% or more, 92% or more, 93% or more, 94% or more, or 95% or more.

3. 3. The pellicle membrane of claim 1 or claim 2, comprising nitrogen in an amount up to approximately 5 atomic percent.

4. The pellicle film according to any one of claims 1 to 3, wherein the metal silicide crystals have a diameter of 30 nm or less, and / or the silicon-based matrix contains silicon crystals having a diameter of 30 nm or less.

5. The pellicle film of any one of claims 1 to 4, wherein the metal silicide crystals are aligned substantially perpendicular to a surface of the pellicle film, and / or the silicon-based matrix comprises silicon crystals aligned substantially perpendicular to a surface of the pellicle film.

6. The pellicle film of any one of claims 1 to 5, wherein at least a portion of the population of metal silicide crystals spans the thickness of the pellicle film and / or the silicon-based matrix comprises silicon crystals spanning the thickness of the pellicle film.

7. The pellicle membrane according to any one of claims 1 to 6, which is a multilayer membrane.

8. 8. The pellicle membrane of claim 7, wherein the pellicle membrane includes a layer including the population of the metal silicide crystals in a silicon-based matrix between one or more layers including a silicon-molybdenum alloy.

9. The pellicle film according to any one of claims 1 to 8, wherein the metal silicide crystal is a molybdenum silicide crystal.

10. The pellicle membrane of any one of claims 1 to 9, wherein the silicon-based matrix comprises p-Si, poly-Si, or SiN, and / or the silicon-based matrix comprises silicon crystals.

11. The pellicle membrane of any one of claims 1 to 10, wherein the silicon-based matrix is ​​doped, and optionally the silicon-based matrix is ​​doped with one or more of boron, phosphorus, and yttrium.

12. The one or more of boron, phosphorus, and yttrium is 10 15 cm -3 ~10 21 cm -3 The pellicle membrane of claim 11 , wherein the pellicle membrane is present in a concentration of about 100%.

13. 13. The pellicle membrane of any one of claims 1 to 12, wherein the pellicle membrane comprises from about 10 atomic % to about 30 atomic % molybdenum, optionally from about 15 atomic % to about 25 atomic % molybdenum, optionally about 20 atomic % molybdenum.

14. 14. The pellicle membrane of any one of claims 1 to 13, wherein the pellicle membrane comprises between about 90 atomic % and about 65 atomic % silicon, optionally between about 85 atomic % and about 70 atomic % silicon, optionally about 75 atomic % silicon.

15. The pellicle membrane of any one of claims 1 to 14, wherein the thickness of the pellicle membrane is from about 10 nm to about 100 nm.

16. 1. A method for manufacturing a pellicle membrane, comprising: a) quenching the film by removing the film from an annealing furnace operating at an annealing temperature and exposing the film to ambient temperature to rapidly cool the film; b) heating the film to an annealing temperature for a period of 30 seconds or less; c) bombarding the film with ions while depositing the film; d) providing a capping layer over the film prior to annealing; e) placing a film at a temperature of about 500° C. or higher onto a surface at a temperature of about 100° C. or lower to induce crystallization; or f) heating one side of the amorphous film above the glass transition temperature to induce crystallization from the opposite side of the amorphous film; The method includes at least one step selected from the following:

17. 17. The method of claim 16, wherein annealing is performed for about 30 minutes or less, about 20 minutes or less, about 15 minutes or less, about 10 minutes or less, or about 5 minutes or less.

18. The method of claim 16 or claim 17, wherein annealing is performed at an annealing temperature of from about 600°C to about 900°C, optionally from about 600°C to about 800°C, or optionally from about 650°C to about 700°C.

19. 18. The method of claim 16 or claim 17, wherein the annealing is performed at a temperature of about 750°C or less, optionally about 700°C or less, optionally about 650°C or less, or optionally about 600°C or less.

20. 20. The method of claim 16, a) and c) to f), claim 18, or claim 19, wherein the annealing is carried out for a period of up to 10 hours, up to 9 hours, up to 8 hours, or from about 1 hour to about 8 hours.

21. 21. The method of any one of claims 16 to 20, comprising doping the pellicle membrane, optionally wherein the dopant is one or more of boron, phosphorus, and yttrium.

22. The dopant is 10 15 cm -3 ~10 21 cm -3 The method of claim 21 , wherein the compound is present in a concentration of about

23. A pellicle assembly comprising a pellicle membrane according to any one of claims 1 to 15, or a pellicle assembly manufactured by the method according to any one of claims 16 to 22.

24. A lithographic apparatus comprising a pellicle membrane according to any one of claims 1 to 15 or a pellicle assembly according to claim 23.

25. Use of a pellicle membrane, a pellicle assembly, a lithographic apparatus or a method according to any one of claims 1 to 24 in a lithographic apparatus or method.

Citation Information

Patent Citations

  • Films used in lithographic apparatus and lithographic apparatus containing such films

    JP2017522590A

  • Mask assembly

    JP2017534077A

  • Metal silicide nitridation for stress reduction

    JP2021501909A

  • Pellicle membrane for a lithographic apparatus

    WO2021144097A1