Nuclear fuel rod cladding tube and method for manufacturing nuclear fuel rod cladding tube
The chromium-niobium nitride coating on nuclear fuel rod claddings addresses stability and debris fretting issues by stabilizing oxidation and enhancing protection, achieving improved performance and cost-effectiveness.
Patent Information
- Application Number
- JP2024532509
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2021-12-09
- Filing Date
- 2022-12-08
- Publication Date
- 2024-12-09
AI Technical Summary
Existing nuclear fuel rod claddings face issues with stability and protection from debris fretting under boiling water reactor (BWR) conditions, particularly due to the instability of hard contact coatings.
A chromium-niobium nitride (Cr-Nb-N) oxidation-resistant coating is applied to the fuel rod cladding, which stabilizes oxidation and enhances debris protection by incorporating niobium, reducing neutron absorption and allowing for thicker coatings if needed, optionally as a single layer, multilayer, or nanoscale superlattice structure.
The Cr-Nb-N coating provides improved oxidation resistance and debris protection, maintaining consistent performance and potentially reducing manufacturing costs, while also offering enhanced adhesion, wear performance, and fatigue strength.
Smart Images

Figure 2024545490000001_ABST
Abstract
Description
[Technical field]
[0001] The present disclosure relates to nuclear fuel rod cladding and, more particularly, to a nuclear fuel rod cladding having an outer coating. The present disclosure also relates to a method for manufacturing a nuclear fuel rod cladding. [Background technology]
[0002] In a typical nuclear reactor, the reactor core contains a number of fuel assemblies, each of which is made up of a number of elongated fuel rods. Each fuel rod contains fissile nuclear material, usually in the form of a stack of fuel pellets surrounded by a gas such as He. The fuel rods have cladding that acts as a containment for the fissile material.
[0003] Light water reactors (LWRs) use water as a coolant and neutron moderator. There are two basic types of LWRs: pressurized water reactors (PWRs) and boiling water reactors (BWRs). The water-water energy reactor (VVER) can be considered a type of PWR. Small modular reactors (SMRs) can also be a type of LWR. In LWRs, the fuel rod cladding is typically made of a zirconium-based alloy.
[0004] WO2021 / 112938 describes a nuclear fuel rod cladding tube having an outer coating that includes an intermediate layer of Nb.
[0005] WO2018 / 067425 describes forming a double-stranded layer on a nuclear fuel rod cladding tube, the double layer including an inner intermediate layer and an outer corrosion-resistant layer.
[0006] WO2020 / 018361 describes a nuclear fuel rod cladding tube in which ceramic yarn is wrapped around the tube and bonded with a coating.
[0007] One issue with hard contact coatings on fuel cladding materials that have been developed to counteract fuel damage due to debris fretting is the stability of these coatings under conditions prevalent, for example, within the core of a BWR.
[0008] Thus, there is a need for improved coatings for nuclear fuel rod cladding.
[0009] It is therefore an object of the present invention to provide an improved nuclear fuel rod cladding, in particular with regard to stability and protection against debris fretting. It is a further object of the present invention to achieve a method for manufacturing the improved nuclear fuel rod cladding. Summary of the Invention
[0010] The above mentioned objects are achieved according to the present invention according to the independent claims.
[0011] Preferred embodiments are defined in the dependent claims.
[0012] According to one aspect, the present invention relates to a nuclear fuel rod cladding having an oxidation resistant coating of chromium-niobium nitride (Cr-Nb-N). The oxidation resistant coating comprises Cr-Nb-N.
[0013] Niobium (Nb) is present in the coating together with chromium nitride (Cr-N) and can therefore stabilize the oxidation of Cr-N, making the coating more protective (by forming stabilized Cr2O3), as opposed to the non-protective oxidation of pure Cr systems with the formation of CrOx, for example, under BWR conditions. Thus, nuclear fuel rod cladding with improved oxidation resistance is achieved, as compared to fuel rod cladding known in the art.
[0014] Furthermore, the Cr-Nb-N oxidation resistant coating provides a surface with higher hardness compared to uncoated or Cr coated fuel cladding, and therefore demonstrates adequate debris protection in, for example, a BWR environment.
[0015] The addition of Nb to Cr not only increases the oxidation resistance but also reduces the overall neutron cross section, the benefits of which can be obtained either as lower neutron absorption or allowing for thicker coatings where the additional protection is deemed advantageous.
[0016] As a result, a nuclear fuel rod cladding is provided that has improved oxidation resistance and improved debris protection compared to rod cladding known in the art. Thus, the above-mentioned objectives are achieved.
[0017] Optionally, the oxidation resistant coating is configured as a single layer. Having a single layer ensures consistent performance across the layer against corrosion and may be the simplest, and therefore the cheapest, coating to manufacture.
[0018] Optionally, the oxidation-resistant coating is configured as a multi-layer coating. The multiple layers can combine the advantageous properties of both layer components. Furthermore, the interfaces between the layers can act to deflect cracks. The interfaces between the layers can also allow some degree of sliding against each other, keeping the layers intact from a larger perspective. The multiple layer coating can be referred to as a multi-layer coating.
[0019] Optionally, the oxidation-resistant coating is configured as a nanoscale multi-layer coating, such as a chromium-niobium nitride / chromium-niobium nitride (Cr-Nb-N / Cr-Nb-N)-superlattice. Superlattice structures can often have improved properties that are not achievable by single-layer thin films, or even some multi-layer coatings, such as bi-layer coatings. The layers in the superlattice contribute further improved properties in terms of oxidation resistance and mechanical properties, including enhanced debris protection of fuel rod cladding.
[0020] Optionally, every second Cr-Nb-N layer of the superlattice has a different Cr to Nb ratio compared to the remaining layers of the superlattice. The synergistic effect of the superlattice structure and the combination of two Cr-Nb-N variants with different Cr to Nb ratios may provide further enhanced properties such as improved adhesion, wear performance, and fatigue strength, as well as improved corrosion resistance.
[0021] Optionally, the content of niobium in Cr—Nb—N is between 5 at% and 90 at%, preferably between 5 at% and 50 at%, and most preferably between 5 at% and 35 at%.
[0022] Optionally, the niobium content of each second Cr-Nb-N layer of the superlattice is in the range of 1 at% to 45 at%, preferably 1 at% to 35 at%, and most preferably 2 at% to 20 at%, and the niobium content of the remaining layers of the superlattice is in the range of 55 at% to 99 at%, preferably 65 at% to 99 at%, and most preferably 80 at% to 98 at%.
[0023] Optionally, the oxidation resistant coating has a thickness between 1 μm and 30 μm, preferably between 2 μm and 15 μm, most preferably between 4 μm and 12 μm. Thus, in case of an oxidation resistant coating configured as a multi-layer coating, the thickness refers to the total thickness of the coating.
[0024] Optionally, the nuclear fuel rod cladding is adapted for use in a boiling water reactor (BWR). Alternatively, the nuclear fuel rod cladding can be used in other types of light water reactors (LWRs), such as pressurized water reactors (PWRs), water-water energy reactors (VVERs), and small modular reactors (SMRs).
[0025] According to a further aspect, the present invention relates to a method for manufacturing nuclear fuel rod cladding, the method comprising the steps of: Providing a nuclear fuel rod cladding base; and providing an oxidation resistant coating of chromium-niobium nitride (Cr-Nb-N) on said tubular base, said oxidation resistant coating consisting of Cr-Nb-N.
[0026] Niobium (Nb) is present in the coating together with chromium nitride (Cr-N) and can therefore stabilize the oxidation of Cr-N, making the coating more protective (by forming stabilized Cr2O3), as opposed to the non-protective oxidation of pure Cr systems with the formation of CrOx, for example, under BWR conditions. Thus, nuclear fuel rod cladding with improved oxidation resistance is achieved, compared to rod cladding known in the art.
[0027] Furthermore, the Cr-Nb-N oxidation resistant coating provides a surface with higher hardness compared to uncoated or Cr coated fuel cladding, and therefore demonstrates adequate debris protection in, for example, a BWR environment.
[0028] The addition of Nb to Cr not only increases the oxidation resistance but also reduces the overall neutron cross section, the benefits of which can be obtained either as lower neutron absorption or allowing for thicker coatings where the additional protection is deemed advantageous.
[0029] As a result, a method is provided for manufacturing an improved nuclear fuel rod cladding that provides a nuclear fuel rod cladding having improved oxidation resistance and improved debris protection compared to fuel rod cladding known in the art. Thus, the above-mentioned objectives are achieved.
[0030] Optionally, the oxidation resistant coating is configured as a single layer. Having a single layer ensures consistent performance across the layer against corrosion and may be the simplest, and therefore the cheapest, coating to manufacture.
[0031] Optionally, the oxidation-resistant coating is configured as a multi-layer coating. A multi-layer coating can combine the advantageous properties of both layer components. Furthermore, the interface between the layers can act to deflect cracks. The interface between the layers can also allow some sliding against each other, keeping the layers intact from a larger perspective. The multiple layer coating can be referred to as a multi-layer coating.
[0032] Optionally, the oxidation-resistant coating is configured as a nanoscale multi-layer coating, such as a chromium-niobium nitride / chromium-niobium nitride (Cr-Nb-N / Cr-Nb-N)-superlattice. Superlattice structures can often have improved properties that are not achievable by single-layer thin films, or even some multi-layer coatings, such as bi-layer coatings. The layers in the superlattice contribute further improved properties in terms of oxidation resistance and mechanical properties, including enhanced debris protection of fuel rod cladding.
[0033] Optionally, every second Cr-Nb-N layer of the superlattice has a different Cr to Nb ratio compared to the remaining layers of the superlattice. The synergistic effect of the superlattice structure and the combination of two Cr-Nb-N variants with different Cr to Nb ratios may provide further enhanced properties such as improved adhesion, wear performance, and fatigue strength, as well as improved corrosion resistance.
[0034] Optionally, the chromium-niobium nitride (Cr—Nb—N) coating is achieved by a physical vapor deposition (PVD) process, so that the coating can be achieved in an effective and reliable manner.
[0035] Optionally, the content of niobium in Cr—Nb—N is between 5 at% and 90 at%, preferably between 5 at% and 50 at%, and most preferably between 5 at% and 35 at%.
[0036] Optionally, the niobium content of each second Cr—Nb—N layer of the superlattice is in the range of 1 at% to 45 at%, preferably 1 at% to 35 at%, and most preferably 2 at% to 20 at%, and the niobium content of the remaining layers of the superlattice is in the range of 55 at% to 99 at%, preferably 65 at% to 99 at%, and most preferably 80 at% to 98 at%.
[0037] Optionally, the oxidation resistant coating has a thickness between 1 μm and 30 μm, preferably between 2 μm and 15 μm, most preferably between 4 μm and 12 μm. Thus, in case of an oxidation resistant coating configured as a multi-layer coating, the thickness refers to the overall thickness of the coating. [Brief description of the drawings]
[0038] [Figure 1] The results of simulating the surface appearance of Cr-Nb-N and Cr-N coatings are shown. [Diagram 2] 1 is a cross-sectional view through a schematic example nuclear fuel rod cladding having an oxidation resistant coating configured as a single layer. [Diagram 3] 1 is a cross-sectional view through a schematic example nuclear fuel rod cladding with an oxidation resistant coating configured as a multi-layer coating; [Figure 4] 1 is a cutaway view of a schematic fuel assembly for a BWR nuclear reactor including nuclear fuel rod cladding, according to an embodiment. [Diagram 5] FIG. 1 is a cutaway view of a schematic fuel assembly for a PWR nuclear reactor including nuclear fuel rod cladding, according to an embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0039] The present invention will now be described in detail with reference to the accompanying drawings, in which the same or similar items have the same reference numerals throughout the drawings, and in which: Further, the items and drawings are not necessarily to scale, emphasis instead being placed upon illustrating the principles of the invention.
[0040] Niobium, also known as colobium, is a chemical element with the symbol Nb (formerly Cb) and atomic number 41. Niobium is a light gray, crystalline, ductile transition metal. Pure niobium has a Mohs hardness rating similar to pure titanium and a ductility similar to iron. Niobium oxidizes very slowly in the Earth's atmosphere.
[0041] According to one aspect, the invention relates to a nuclear fuel rod cladding 1, 1' having an oxidation resistant coating 5, 5' of chromium-niobium nitride (Cr-Nb-N).
[0042] Niobium (Nb) is present in the coating together with chromium nitride (Cr-N) and therefore can stabilize and be more protective against oxidation of Cr-N (by forming stabilized Cr2O3) as opposed to the non-protective oxidation of pure Cr systems with the formation of CrOx, for example, under BWR conditions. Several simulations have been performed and attached FIG. 1 shows the results of a simulation of the surface appearance of Cr-Nb-N and Cr-N coatings after 60 days of exposure in an autoclave simulating BWR conditions. As can be seen, the Cr-Nb-N coating has a smooth and stable surface, which provides both improved corrosion resistance and improved protection against debris.
[0043] Cr-Nb-N coatings can be achieved by a physical vapor deposition (PVD) process using multiple targets of Cr and Nb, or by prefabrication of a Cr-Nb alloy target with the selected composition followed by deposition in either case under a N2 atmosphere.
[0044] The attached drawings, Figs. 2 to 5, are now described. Fig. 2 is a cross-sectional view through a schematic example nuclear fuel rod cladding 1 with an oxidation-resistant coating 5 configured as a single layer. The nuclear fuel rod cladding 1 comprises a nuclear fuel cladding base 7 and an oxidation-resistant coating 5, the coating 5 consisting of chromium-niobium nitride (Cr-Nb-N). The thickness of the nuclear fuel cladding base 7 is typically about 0.5 to 0.8 mm (500 to 800 μm). The nuclear fuel cladding base 7 is preferably made of a zirconium-based alloy. The coating 5 consists of Cr-Nb-N. The oxidation-resistant coating 5 has a thickness between 1 μm and 30 μm, preferably between 2 μm and 15 μm, most preferably between 4 μm and 12 μm. The oxidation-resistant coating 5 is therefore much thinner than the nuclear fuel cladding base 7. The niobium content of Cr-Nb-N is 5 at%-90 at%, preferably 5 at%-50 at%, and most preferably 5 at%-35 at%. The nuclear fuel cladding base 7 can be coated with an oxidation-resistant coating 5 using a physical vapor deposition (PVD) process. The principles of the PVD process are common knowledge and therefore will not be described in detail herein.
[0045] FIG. 3 is a cross-sectional view through a schematic example nuclear fuel rod cladding tube 1' with an oxidation-resistant coating 5' configured as a multi-layer coating. A multi-layer coating can be called a multi-layer coating. According to the embodiment shown in FIG. 3, the oxidation-resistant coating 5' comprises two layers. However, the oxidation-resistant coating 5' can comprise not only two layers but also many very thin layers. The nuclear fuel rod cladding tube 1' comprises a nuclear fuel cladding tube base 7 and an oxidation-resistant coating 5' having a plurality of layers, each layer of the plurality of layers being made of chromium-niobium nitride (Cr-Nb-N). According to the embodiment shown in FIG. 3, the nuclear fuel cladding tube base 7 is similar to the nuclear fuel cladding tube base 7 according to the embodiment shown in FIG. 2. Thus, the thickness of the nuclear fuel cladding tube base 7 is typically about 0.5-0.8 mm (500-800 μm). The nuclear fuel cladding tube base 7 is preferably made of a zirconium-based alloy. Each layer of the coating 5' is made of Cr-Nb-N. The coating 5' has a thickness t' between 1 μm and 30 μm, preferably between 2 μm and 15 μm, most preferably between 4 μm and 12 μm. The oxidation-resistant coating 5' configured as a multi-layer coating therefore has a total thickness t' between 1 μm and 30 μm, preferably between 2 μm and 15 μm, most preferably between 4 μm and 12 μm. The oxidation-resistant coating 5' is therefore much thinner than the nuclear fuel cladding base 7. The thickness of each layer of the coating 5' may be the same or the thickness of each layer of the coating 5' may be different. The content of niobium in the Cr-Nb-N of each layer is between 5 at% and 90 at%, preferably between 5 at% and 50 at%, most preferably between 5 at% and 35 at%. The nuclear fuel cladding base 7 may be coated with the oxidation-resistant coating 5' using a physical vapor deposition (PVD) process, i.e. each layer of the coating 5' may be realized by a PVD process. The principles of the PVD process are common knowledge and therefore will not be described in detail herein.
[0046] Optionally, the oxidation resistant coating 5' may be configured as a nanoscale multilayer coating such as a chromium-niobium nitride / chromium-niobium nitride (Cr-Nb-N / Cr-Nb-N)-superlattice (not shown).
[0047] As a further option, each second Cr-Nb-N layer of the superlattice may have a different Cr to Nb ratio compared to the remaining layers of the superlattice: the niobium content of each second Cr-Nb-N layer may range from 1 at% to 45 at%, preferably from 1 at% to 35 at%, and most preferably from 2 at% to 20 at%, and the niobium content of the remaining layers may range from 55 at% to 99 at%, preferably from 65 at% to 99 at%, and most preferably from 80 at% to 98 at%.
[0048] FIG. 4 is a cutaway view of a schematic fuel assembly for a BWR reactor 2 including nuclear fuel cladding rod tubes 1, 1' according to embodiments of the invention described herein.
[0049] FIG. 5 is a cutaway view of a schematic fuel assembly for a PWR reactor 3 including nuclear fuel cladding rod tubes 1, 1' according to embodiments of the invention described herein.
[0050] The nuclear fuel rod cladding 1, 1' according to the invention can also be arranged in a light water reactor (LWR), a water-water energy reactor (VVER) or a small modular reactor (SMR).
[0051] The present invention is not limited to the above preferred embodiments. Various alternatives, modifications, and equivalents may be used. Therefore, the above embodiments should not be construed as limiting the scope of the present invention, which is defined by the appended claims.
Claims
1. A nuclear fuel rod cladding tube (1, 1') characterized in that it has an oxidation resistant coating (5, 5') of chromium-niobium nitride (Cr-Nb-N).
2. 2. Nuclear fuel rod cladding tube (1) according to claim 1, characterized in that the oxidation resistant coating (5) is constructed as a single layer.
3. 2. Nuclear fuel rod cladding tube (1') according to claim 1, wherein said oxidation resistant coating (5') is configured as a multi-layer coating.
4. The nuclear fuel rod cladding tube (1') according to claim 3, wherein said oxidation resistant coating (5') is configured as a nanoscale multi-layer coating such as a chromium nitride-niobium / chromium nitride-niobium (Cr-Nb-N / Cr-Nb-N)-superlattice.
5. The nuclear fuel rod cladding tube (1') of claim 4, wherein every second Cr-Nb-N layer of the superlattice has a different Cr to Nb ratio compared to the remaining layers of the superlattice.
6. The nuclear fuel rod cladding tube (1, 1') according to any one of claims 1 to 4, wherein the niobium content of the Cr-Nb-N is between 5 at% and 90 at%, preferably between 5 at% and 50 at%, most preferably between 5 at% and 35 at%.
7. 6. The nuclear fuel rod cladding tube (1') according to claim 5, wherein for each second Cr-Nb-N layer, the niobium content is in the range of 1 at% to 45 at%, preferably 1 at% to 35 at%, most preferably 2 at% to 20 at%, and the niobium content of the remaining layers is in the range of 55 at% to 99 at%, preferably 65 at% to 99 at%, most preferably 80 at% to 98 at%.
8. The nuclear fuel rod cladding tube (1, 1') according to any of the preceding claims, wherein said oxidation resistant coating (5, 5') has a thickness (t, t') between 1 μm and 30 μm, preferably between 2 μm and 15 μm, most preferably between 4 μm and 12 μm.
9. A method for manufacturing a nuclear fuel rod cladding tube (1, 1') comprising the following steps: - Providing a nuclear fuel cladding base (7), and providing said nuclear fuel cladding tube base with an oxidation resistant coating (5, 5') of chromium-niobium nitride (Cr-Nb-N).
10. The method according to claim 9, wherein the oxidation resistant coating (5) is configured as a single layer.
11. The method according to claim 9, wherein the oxidation resistant coating (5') is configured as a multi-layer coating.
12. The method according to claim 11, wherein the oxidation resistant coating (5') is configured as a nanoscale multilayer coating, such as a chromium-niobium nitride / chromium-niobium nitride (Cr-Nb-N / Cr-Nb-N)-superlattice.
13. The method of claim 12, wherein every second Cr-Nb-N layer of the superlattice has a different Cr to Nb ratio as compared to the remaining layers of the superlattice.
14. The method according to any of claims 9 to 13, wherein said oxidation resistant coating (5, 5') of Cr-Nb-N is achieved by a physical vapor deposition (PVD) process.
15. 15. The method according to any of claims 9 to 11 or 14, wherein the niobium content of the Cr-Nb-N is between 5 at% and 90 at%, preferably between 5 at% and 50 at%, most preferably between 5 at% and 35 at%.
16. 14. The method of claim 13, wherein the niobium content of each second Cr—Nb—N layer is in the range of 1 at% to 45 at%, preferably 1 at% to 35 at%, most preferably 2 at% to 20 at%, and the niobium content of the remaining layers is in the range of 55 at% to 99 at%, preferably 65 at% to 99 at%, most preferably 80 at% to 98 at%.
17. The method according to any of claims 9 to 16, wherein said oxidation resistant coating (5, 5') has a thickness (t, t') between 1 μm and 30 μm, preferably between 2 μm and 15 μm, most preferably between 4 μm and 12 μm.