Electrode Assembly

The electrode assembly's innovative design with controlled slitting and sliding portions ensures an N/P ratio greater than 1, enhancing energy density by optimizing the cathode and anode arrangement.

KR103045157B1Active Publication Date: 2026-11-06LG ENERGY SOLUTION LTD
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
KR1020220086635
Authority / Receiving Office
KR · KR
Patent Type
Patents
Current Assignee / Owner
Filing Date
2022-07-14
Publication Date
2026-11-06
Estimated Expiration
2042-07-14

AI Technical Summary

Technical Problem

Existing electrode assemblies struggle to maintain an N/P ratio greater than 1 across the entire region where the cathode and anode face each other, leading to inefficiencies in energy density due to excess space and material usage.

Method used

The electrode assembly design includes specific arrangements of slitting and sliding portions in the active material layers of the cathode and anode, with controlled gaps and angles to ensure an N/P ratio greater than 1, maximizing the capacity of the anode relative to the cathode.

Benefits of technology

This design effectively achieves an N/P ratio greater than 1, maximizing energy density per unit volume and weight, while preventing the N/P inversion phenomenon.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 112022073277914-PAT00012_ABST
    Figure 112022073277914-PAT00012_ABST
Patent Text Reader

Abstract

The present application may provide an electrode assembly and its uses. The present application may provide a structure of an electrode assembly capable of maximizing the capacity per unit area of ​​the anode relative to the cathode while effectively achieving an N / P ratio greater than 1 across the entire region where the anode and cathode face each other. Accordingly, the present application may provide an electrode assembly capable of maximizing energy density per unit volume and unit weight even under an N / P ratio greater than 1. The present application may also provide a method for manufacturing such an electrode assembly and its uses.
Need to check novelty before this filing date? Find Prior Art

Description

Technology Field

[0001] This application relates to an electrode assembly. Background Technology

[0002] The application areas of energy storage technology are expanding to include mobile phones, camcorders, laptop PCs, and even electric vehicles.

[0003] One of the research fields of energy storage technology is rechargeable secondary batteries, and research and development are underway to improve the capacity density and specific energy of these secondary batteries.

[0004] A secondary battery includes an electrode assembly having a structure in which a positive electrode and a negative electrode are stacked with a separator in between. When designing the electrode assembly, the negative electrode is made to have a higher loading and wider width than the positive electrode, which is a design intended to make the so-called N / P ratio greater than 1.

[0005] The above N / P ratio is the ratio of the capacity per unit area of ​​the cathode and the anode, and is the value obtained by dividing the capacity per unit area of ​​the cathode by the capacity per unit area of ​​the anode.

[0006] The reason for designing the N / P ratio to be greater than 1 is that problems such as lithium electroplating occur when the negative electrode is not positioned opposite the positive electrode during the charging process, or when the loading of the negative electrode is low and the amount of lithium that can be accommodated by the negative electrode is smaller than the amount of lithium generated by the positive electrode.

[0007] When the N / P ratio is less than 1, a short circuit may occur in the battery due to lithium precipitated in the form of needles, and since the lithium generated at the positive electrode is not fully utilized during discharge, a decrease in efficiency and a degradation of capacity may occur, and the electrolyte may decompose on the surface of the precipitated lithium and a film may grow, which may result in a decrease in efficiency and an increase in resistance.

[0008] Typically, a cathode or an anode is manufactured by coating a slurry containing an electrode active material onto the surface of a current collector and undergoing drying and rolling processes, and the coated slurry forms an active material layer of the electrode.

[0009] However, as exemplarily shown in FIG. 1, in the process of forming an active material layer (101) by coating the slurry onto the current collector (100) due to the characteristics of the slurry, a sliding portion (S in FIG. 1) is generated at the beginning and end portions of the coating, which is a portion where the thickness increases or decreases along the direction of the coating (direction of the arrow in FIG. 1).

[0010] The inclination or width of the sliding portion is determined according to the composition of the slurry. When forming an electrode assembly by bringing the anode and cathode into contact, an N / P ratio exceeding 1 must be achieved even in the area where the sliding portions of the anode and cathode exist; however, since it is not easy to control the inclination or width of the sliding portion, controlling the N / P ratio is also a difficult task.

[0011] Accordingly, it is a difficult problem to manufacture an electrode assembly such that the N / P ratio is greater than 1 across the entire region where the cathode and the anode face each other.

[0012] Typically, since achieving an N / P ratio greater than 1 is important, the capacity per unit area of ​​the cathode is applied in excess of what is required when designing electrodes.

[0013] In the above case, the N / P ratio can be achieved as desired, but there is excess space at the negative electrode that is not utilized during the actual charging and discharging of the secondary battery, which unnecessarily increases the volume or weight of the electrode assembly or the secondary battery, and results in inefficient outcomes in terms of energy density. The problem to be solved

[0014] The present application relates to an electrode assembly and its uses. One objective of the present application is to provide a structure of an electrode assembly that can effectively achieve an N / P ratio greater than 1 across the entire area where the anode and cathode face each other, while maximizing the capacity of the anode per unit area relative to the cathode. Accordingly, the present application aims to provide an electrode assembly that can maximize energy density per unit volume and per unit weight even under an N / P ratio greater than 1.

[0015] The present application also aims to provide a method for manufacturing an electrode assembly as described above.

[0016] The present application also has one objective of providing a use for the electrode assembly. means of solving the problem

[0017] This application relates to an electrode assembly.

[0018] The electrode assembly of the present application comprises a cathode; an anode and a separator, and

[0019] The above cathode and anode are stacked with the above separator in between,

[0020] The above-mentioned cathode and anode each comprise a current collector layer and an active material layer existing at least between the current collector layer and the separator, and

[0021] Each of the above-mentioned cathode and anode has a first end portion having a tab portion formed therein and a second end portion on the opposite side of the first end portion, and

[0022] The above-mentioned cathode and anode are stacked such that their first ends face each other, or one first end and another second end face each other, and

[0023] A slitting portion is formed in one of the first and second end portions of the active material layer of the above-mentioned cathode, and a sliding portion is formed in the other active material layer.

[0024] The active material layers at both ends of the anode are located inwardly compared to the active material layers at both ends of the cathode facing each other.

[0025] The ratio I2 / I1 of the gap (I1) between the positive active material layer and the negative active material layer at the end of the negative electrode where the slitting portion is formed and the gap (I2) between the positive active material layer and the negative active material layer at the end of the negative electrode where the sliding portion is formed may be within the range of 0.5 to 10.

[0026] In the above electrode assembly, the active material layer of the negative electrode may be thicker than the active material layer of the positive electrode.

[0027] In the electrode assembly above, a sliding portion may be formed in the active material layer of the end portion facing the end portion of the positive electrode where the slitting portion of the negative electrode is formed.

[0028] In the above electrode assembly, the surface of the sliding portion of the active material layer of the anode may be a cut surface.

[0029] In the above electrode assembly, a slitting portion may be formed in the active material layer of the positive electrode at the opposite end of the end where the sliding portion of the active material layer of the positive electrode is formed.

[0030] In the above electrode assembly, the slitting portion of the active material layer of the positive electrode may be located on the inner side relative to the sliding portion of the active material layer of the negative electrode.

[0031] The above electrode assembly can be designed to satisfy the following Equation 1.

[0032] [Equation 1]

[0033] TN / tanθ1≤ I2

[0034] T in Equation 1 N I is the thickness of the active material layer of the cathode, θ1 is the angle of inclination of the sliding portion of the cathode, and I2 is the gap between the active material layer of the anode and the active material layer of the cathode at the end of the cathode where the sliding portion is formed.

[0035] In the above, tanθ1 may be within the range of 0.001 to 10.

[0036] The above electrode assembly can be designed to additionally satisfy Equation 2 below.

[0037] [Equation 2]

[0038] I2≤ T N / sinθ1

[0039] T in Equation 2 N I is the thickness of the active material layer of the cathode, θ1 is the angle of inclination of the sliding portion of the cathode, and I2 is the gap between the active material layer of the anode and the active material layer of the cathode at the end of the cathode where the sliding portion is formed.

[0040] In the electrode assembly above, a second sliding portion may be formed in the active material layer of the positive electrode at the opposite end of the end where the sliding portion of the active material layer of the positive electrode is formed.

[0041] In the above, the surface of the second sliding portion of the active material layer of the anode may be a cut surface.

[0042] The above electrode assembly can be designed to satisfy Equation 3 below.

[0043] [Equation 3]

[0044] T N / tanθ1≤ I2+ T P / tanθ2

[0045] T in Equation 3 N ε is the thickness of the active material layer of the cathode, θ1 is the inclination angle of the sliding portion of the cathode, I2 is the gap between the active material layer of the anode and the active material layer of the cathode at the end of the cathode where the sliding portion is formed, and T P is the thickness of the active material layer of the anode, and θ2 is the angle of inclination of the second sliding part of the anode.

[0046] The above electrode assembly can be designed to additionally satisfy the following Equation 4.

[0047] [Equation 4]

[0048] I2+ TP / tanθ2≤ T N / sinθ1

[0049] T in Equation 4 N ε is the thickness of the active material layer of the cathode, θ1 is the inclination angle of the sliding portion of the cathode, I2 is the gap between the active material layer of the anode and the active material layer of the cathode at the end of the cathode where the sliding portion is formed, and T P is the thickness of the active material layer of the anode, and θ2 is the angle of inclination of the second sliding part of the anode.

[0050] The above electrode assembly can be designed to additionally satisfy the following Equation 5.

[0051] [Equation 5]

[0052] θ2 / θ1> 1

[0053] In Equation 5, θ1 is the angle of inclination of the sliding part of the cathode, and θ2 is the angle of inclination of the second sliding part of the anode.

[0054] In the above electrode assembly, the cathode may additionally include an active material layer formed on a side opposite to the surface of the current collector layer facing the separator, and in this case, the active material layer formed on the side opposite to the surface of the current collector layer of the cathode facing the separator and the active material layer existing between the current collector layer and the separator may have a symmetrical structure.

[0055] In the above electrode assembly, the anode may additionally include an active material layer formed on a side opposite to the surface of the current collector layer facing the separator, and in this case, the active material layer formed on the side opposite to the surface of the current collector layer of the anode facing the separator and the active material layer existing between the current collector layer and the separator may have a symmetrical structure.

[0056] The present application also relates to a secondary battery comprising the electrode assembly and the electrolyte. Effects of the invention

[0057] The present application may provide an electrode assembly and its uses. The present application may provide a structure of an electrode assembly capable of maximizing the capacity per unit area of ​​the anode relative to the cathode while effectively achieving an N / P ratio greater than 1 across the entire region where the anode and cathode face each other. Accordingly, the present application may provide an electrode assembly capable of maximizing energy density per unit volume and unit weight even under an N / P ratio greater than 1. The present application may also provide a method for manufacturing such an electrode assembly and its uses. Brief explanation of the drawing

[0058] Figures 1 to 3, 6 and 8 are drawings for explaining the structure of an electrode. Figures 4, 5, and 7 are drawings illustrating the structure of an electrode assembly. Figure 9 is a diagram illustrating the process of forming a slitting portion on an electrode. FIG. 10 is a drawing for explaining an exemplary structure of a cathode included in the electrode assembly of the present application. FIGS. 11 and 12 are exemplary drawings for explaining the structure of the electrode assembly of the present application. Specific details for implementing the invention

[0059] In this specification, the term "sliding portion" refers to a region of an active material layer in a cross-section of an electrode comprising a current collector layer and an active material layer formed on at least one surface of the current collector layer, wherein the thickness of the active material layer substantially increases or decreases along the longitudinal direction of the current collector layer. The increase or decrease in thickness may occur at a constant rate or at a non-constant rate.

[0060] In this specification, the term "normal thickness region" refers to a region in the cross-section of the electrode where the thickness of the active material layer is maintained substantially constant along the longitudinal direction of the current collector layer.

[0061] The above electrode refers to the positive or negative electrode.

[0062] The cross-section of the electrode refers to the cut surface obtained when the electrode is cut in a direction parallel to the direction connecting the end where the unseen portion of the electrode exists and the end opposite to the end where the unseen portion exists, when the electrode is observed from the front, and parallel to the normal of the surface of the current collector layer. This cut surface may be a virtual cut surface or an actual cut surface.

[0063] In the following description of the electrode assembly, the positional relationship of the active material layers of the anode and cathode may be a relationship based on the cross-section of the electrode.

[0064] FIG. 2 is a drawing that exemplarily shows a cross-section of the electrode. As shown in FIG. 2, the electrode of the present application may include a current collector layer (100) and active material layers (101, 102) formed on one or both sides thereof. At this time, the active material layers (101, 102) are formed such that at least one of the two ends of the current collector layer (100) has a portion (so-called un-active portion) where the active material layers (101, 102) are not formed. This un-active portion may form a tab portion as described later. The un-active portion may be formed at both ends of the electrode as shown in the drawing, or it may be formed at only one end of the electrode. If un-active portions exist at both ends of the electrode, the cutting may be performed parallel to the direction connecting the two ends where the un-active portions exist.

[0065] FIG. 3 is an example of the electrode of FIG. 2 observed from the front (the surface on which the active material layer (101) is formed), and the dotted line in FIG. 3 is a cutting line for observing the cross-section of the electrode. As shown by the dotted line in FIG. 3, the cutting may be made in a direction parallel to the direction connecting the end where the unsold portion of the electrode exists and the end opposite to the end where the unsold portion exists (or the direction connecting both ends where the unsold portion of the electrode exists) when the electrode is observed from the front, parallel to any one side of the electrode, and parallel to the normal of the surface of the current collector layer.

[0066] The longitudinal direction of the current collector layer may mean a direction parallel to the current collector layer in the cross-section of the electrode (e.g., the direction of the arrow in FIG. 2).

[0067] Generally, an electrode such as a cathode or an anode is manufactured by coating a slurry containing an electrode active material on one or both sides of a current collector layer and performing drying and rolling processes, and the coated slurry forms an active material layer of the electrode.

[0068] As shown in FIG. 2, in such electrodes, due to the characteristics of the slurry, a region (e.g., the part indicated by S in FIG. 2) is formed in which the thickness of the active material layer (101, 102) substantially increases or decreases along the longitudinal direction (direction of the arrow in FIG. 2) of the current collector layer (100).

[0069] In this specification, a portion of the active material layer in which the thickness substantially increases or decreases as described above may be designated as a sliding portion. The sliding portion does not necessarily occur only during the coating process of the slurry, and may also be formed by etching, cutting, or non-contact cutting as described later.

[0070] In addition, the statement that the thickness substantially increases or decreases as described above means that when a graph is drawn with the origin at the point where the active material layer (101, 102) begins in the cross-section of the electrode (e.g., 10 in FIG. 2), the distance from the origin to any point of the active material layer (101, 102) measured along the length direction of the current collector layer as the x-axis value, and the thickness of the active material layer (101, 102) at that point as the y-axis value, the absolute value of the slope of the graph is 0.001 or greater. The length on the x-axis and the thickness on the y-axis have the same unit. In the case where the graph is not a straight line, the slope may be the derivative value at that point. The absolute value of the slope in the sliding part above is, in other examples, 0.002 or more, 0.004 or more, 0.006 or more, 0.008 or more, 0.01 or more, 0.02 or more, 0.04 or more, 0.06 or more, 0.08 or more, 0.1 or more, 0.12 or more, 0.14 or more, 0.16 or more, 0.18 or more, or 0.2 or more, or 10 or less, 9 or less, 8 or less, 7 or less, 6 or less, 5 or less, 4 or less, 3 or less, 2 or less, 1 or less, 0.8 or less, 0.6 or less, 0.4 or less, 0.2 or less, 0.1 or less, 0.08 or less, 0.06 or less, 0.04 or less, 0.02 or less, 0.01 or less, 0.008 or less, 0.006 or less, It may be 0.004 or less, or about 0.002 or less.

[0071] Meanwhile, when observing the active material layer (101, 102) of the electrode cross-section of FIG. 2 along the longitudinal direction of the current collector (arrow direction of FIG. 2) starting from the origin (10), there exists a region where the thickness of the active material layer (101, 102) is substantially maintained constant from the point where the sliding part ends until the sliding part at the other end begins; this region becomes the normal thickness region. In the normal thickness region, the absolute value of the slope may be in the range of approximately 0 or greater and less than 0.001. In other examples, the upper limit of the absolute value of the slope may be approximately 0.0008 or less, 0.0006 or less, 0.0004 or less, or 0.0002 or less.

[0072] The electrode assembly of the present application comprises at least a cathode; an anode and a separator, and the cathode and the anode may be included in the electrode assembly in a stacked state with the separator in between. FIG. 4 is a drawing showing a configuration in which a cathode (300) and an anode (400) are stacked with the separator (200) in between.

[0073] As shown in FIG. 4, the electrode assembly may each include one separator (200), one cathode (300), and one anode (400), or it may include two or more of any one of the above. For example, as illustrated in FIG. 5, the electrode assembly may include two or more unit structures stacked in the order of the cathode (300), the separator (200), and the anode (400).

[0074] The negative electrode of the above electrode assembly may include a current collector layer and an active material layer formed on at least one surface of the current collector layer, and the positive electrode may also include a current collector layer and an active material layer formed on at least one surface of the current collector layer.

[0075] FIG. 6 exemplarily shows the structure of a cathode in which the active material layers (301, 302) are formed on both sides of a current collector layer (103). Although FIG. 6 shows a structure in which the active material layers (301, 302) are formed on both sides of the current collector layer (103), the active material layers may be formed on only one side of the current collector layer.

[0076] The positive electrode can also be formed in the same shape as the above-mentioned negative electrode.

[0077] A structure in which a cathode and an anode of the same type as shown in FIG. 6 are stacked with a separator in between is exemplarily shown in FIG. 7, and such a structure may sequentially include a cathode active material layer (302), a cathode current collector layer (103), a cathode active material layer (301), a separator (200), an anode active material layer (401), an anode current collector layer (104), and an anode active material layer (402).

[0078] In the electrode assembly above, the cathode and the anode may each include a current collector layer (103, 104 in FIG. 7) and an active material layer (301, 401 in FIG. 5) existing between at least the current collector layer (103, 104 in FIG. 7) and the separator (200 in FIG. 7).

[0079] The above-mentioned cathode and anode may each have a first end portion having a tab portion formed therein and a second end portion on the opposite side of the first end portion.

[0080] The above tab portion may refer to the aforementioned non-existent portion (an area of ​​the current collector layer where the active material layer is not formed), and this area may be a region where a tab is attached during a tab welding process, etc. In another example, the above tab portion may refer to a region where the electrode is electrically connected to the outside. Such non-existent portions may be formed at both ends of the electrode, or may be formed at only one end of the electrode. FIG. 8 shows a case where non-existent portions (NC) are formed at both ends of an electrode in which active material layers (101, 102) are formed on both sides of the current collector layer (100). In the case where non-existent portions are formed at both ends of the electrode as in FIG. 8, one of the two non-existent portions may be designated as the first end portion, and the opposite side may be designated as the second end portion. In one example, a region where a tab is attached or electrically connected to the outside through tab welding, etc., may be designated as the first end portion.

[0081] In the electrode assembly, the cathode and the anode may be stacked so that their first ends face each other. In another example, they may be stacked so that the first end of one of the cathode and the anode faces the other second end. In the above, the fact that two parts face each other means that when observing the electrode along the normal direction of the surface of the separator (200) in the structure of FIGS. 4, 5 and 7, the parts overlap and at least a portion overlaps.

[0082] In the electrode assembly of the present application having the above structure, a slitting portion may be formed in one of the first and second end portions of the cathode active material layer, and a sliding portion may be formed in the other active material layer. A normal thickness region may be formed between the slitting portion and the sliding portion in the cathode.

[0083] The above-mentioned slitting portion refers to a portion formed such that the extension direction of the side of the end portion of the active material layer in the cross-section of the electrode forms an angle of ±5 degrees, ±4 degrees, ±3 degrees, ±2 degrees, or ±1 degree with the normal of the surface of the current collector layer, or substantially parallel to the normal of the surface of the current collector layer.

[0084] Such slitting portions can be formed by a cutting process such as a slitting or notching process. At this time, the cross-section of the electrode is the same as the cross-section of the electrode in the process of describing the sliding portion and the normal thickness region.

[0085] As described above, the electrode, which has undergone coating, drying, and rolling of the slurry, typically has sliding portions formed at both ends, and its cross-section appears in the form shown in FIG. 9. That is, as exemplarily shown in FIG. 9, due to the characteristics of the slurry, in the process of forming an active material layer (101, 102) by coating the slurry onto a current collector (100), a sliding portion (S in FIG. 9) is formed at the beginning and end portions of the coating, which is a portion where the thickness increases or decreases along the direction of the coating or the length direction of the current collector layer (100) (direction of the two arrows in FIG. 9).

[0086] By cutting one of the two ends in which the sliding portion is formed in this way through a cutting process such as slitting or notching, an electrode can be formed in which one end is the sliding portion and the other end is the slitting portion.

[0087] For example, if cutting is performed in the direction of the dotted line following the direction of the unidirectional arrow in Fig. 9, an electrode is formed in which one end is a sliding part and the other end is a slitting part, as shown in Fig. 10.

[0088] In the electrode of Fig. 10, the extension direction (1011) of the side of the active material layer at the end portion, which is the slitting portion, is substantially parallel to the normal of the surface of the current collector layer (direction of the one-way arrow).

[0089] In the electrode assembly of the present application, the active material layers at both ends of the positive electrode may be located inwardly from the active material layers at both ends of the negative electrode facing each other.

[0090] In the above, the statement that the active material layers at both ends of the positive electrode are located inwardly compared to the active material layers at both ends of the negative electrode facing each other means that when the electrode assembly is observed in the direction normal to the surface of the separator, the active material layer of the negative electrode is formed such that its ends are extended further than the active material layer of the positive electrode.

[0091] That is, as exemplarily shown in FIG. 11 or FIG. 12, when observing the electrode assembly along the normal direction of the surface of the separator (200), the active material layer (301) of the negative electrode is formed to be extended further along the length direction of the current collector layer (103, 104) than the active material layer (401) of the positive electrode. Accordingly, in FIG. 11 and 12, I1 and I2 each exceed 0. With such an arrangement, the phenomenon in which the N / P ratio becomes less than 1 (hereinafter referred to as the N / P inversion phenomenon) can be efficiently prevented.

[0092] In one example, the active material layer (301) of the cathode can be formed with a larger area than the active material layer (401) of the anode.

[0093] In one example, the ratio I2 / I1 of the gap between the positive active material layer (401) and the negative active material layer (301) at the end of the negative electrode where the slitting portion is formed in the cross-section of the electrode (I1 in FIG. 11 and 12) and the gap between the positive active material layer (401) and the negative active material layer (301) at the end of the negative electrode where the sliding portion is formed (I2 in FIG. 11 and 12) may be within the range of 0.5 to 10.

[0094] The above ratio I2 / I1 may be 1 or more, 1.5 or more, 2 or more, 2.5 or more, 3 or more, 4 or more, 5 or more, 6 or more, or 7 or more, or 9 or less, 8 or less, 7 or less, 6 or less, 5 or less, 4 or less, 3 or less, 2.5 or less, 2 or less, 1.5 or less, or 1 or less. Under such a ratio, an electrode assembly that secures high energy density while effectively preventing the N / P reversal phenomenon can be provided.

[0095] In the above electrode assembly, the active material layer of the negative electrode may also be formed to be thicker than the active material layer of the positive electrode, thereby providing an electrode assembly that secures high energy density while effectively preventing the N / P inversion phenomenon. In the above, the thickness of each active material layer is the thickness in the normal thickness region. If the thickness of the normal thickness region is somewhat inconsistent, the thickness refers to the average thickness of the corresponding normal thickness region. Although not specifically limited, the ratio (TN / TP) of the thickness of the active material layer of the negative electrode (TN) and the thickness of the active material layer of the positive electrode (TP) may be greater than 1 and less than or equal to 5. In other examples, the ratio (TN / TP) may be less than or equal to 4.5, less than or equal to 4, less than or equal to 3.5, less than or equal to 3, less than or equal to 2.5, less than or equal to 2, or less than or equal to 1.5.

[0096] In the electrode assembly above, a sliding portion may be formed in the active material layer of the end portion facing the end portion of the anode where the slitting portion of the cathode is formed. By adopting this shape, an electrode assembly that secures high energy density while effectively preventing the N / P reversal phenomenon can be provided.

[0097] FIGS. 11 and 12 illustrate an electrode assembly of this type as an example. Although the drawings show a case where an active material layer (301, 401) is formed only between the current collector (103, 104) and the separator (200), the active material layer (301, 401) may also be formed on the opposite side of each current collector layer (103, 104).

[0098] In addition, in FIGS. 11 and 12, the inclined surface of the sliding part (e.g., S N , S P Although the inclined surface is indicated as being in a straight line shape, this is for the convenience of explaining the electrode assembly of the present application, and the inclined surface may be in a curved shape (e.g., a convex curve or a concave curve shape, etc.) or other shapes other than a straight line shape.

[0099] As shown in FIGS. 11 and 12, a slitting portion is formed at the right end of the negative electrode active material layer (301) and a sliding portion is formed at the left end, and a sliding portion is formed at the right end of the positive electrode active material layer (401) facing the end where the slitting portion is formed.

[0100] FIG. 11 is an embodiment of the electrode assembly of the present application, in which a slitting portion is formed on the active material layer (401) of the positive electrode at the opposite end of the end (right end of FIG. 11) where the sliding portion of the active material layer (401) of the positive electrode is formed in the above state.

[0101] In this structure, the slitting portion of the active material layer (401) of the positive electrode may be located on the inner side relative to the sliding portion of the active material layer (301) of the negative electrode.

[0102] Referring to the structure of FIG. 11, the fact that the slitting portion of the active material layer (401) of the positive electrode is located on the inner side relative to the sliding portion of the active material layer (301) of the negative electrode means that the following Equation 1 is satisfied.

[0103] [Equation 1]

[0104] T N / tanθ1≤ I2

[0105] T in Equation 1 N I is the thickness of the active material layer of the negative electrode, which is the thickness of the normal thickness region of the negative electrode active material layer, θ1 is the angle of inclination of the sliding portion of the negative electrode active material layer, and I2 is the gap between the active material layer of the positive electrode and the active material layer of the negative electrode at the end of the negative electrode where the sliding portion is formed.

[0106] The above T N , θ1 and I2 are shown in Fig. 11.

[0107] The inclined surface (S) of the negative active material layer (also 301 of 11) for determining θ1 above N ) is the angle formed by the straight line connecting the point where the sliding part starts and the point where the sliding part ends, as shown in the drawing, and the length direction of the collector layer (103). The inclined surface of the actual sliding part may be in the form of a straight line as shown in FIG. 11, or it may not be. Even if it is not in the form of a straight line, when calculating θ1, it is calculated based on a virtual straight line.

[0108] In Equation 1 above, T N / tanθ1 is W in Fig. 11 N This is the width of the sliding portion of the active material layer (301) of the negative electrode indicated by .

[0109] By forming an active material layer (301, 401) such that Equation 1 is satisfied, the electrode assembly can be designed to exhibit high energy density while stably preventing the N / P reversal phenomenon.

[0110] In the above, tanθ1 can have a value within the range of 0.001 to 10. tanθ1 is, in other examples, 0.002 or more, 0.004 or more, 0.006 or more, 0.008 or more, 0.01 or more, 0.02 or more, 0.04 or more, 0.06 or more, 0.08 or more, 0.1 or more, 0.12 or more, 0.14 or more, 0.16 or more, 0.18 or more, or 0.2 or more, or 9 or less, 8 or less, 7 or less, 6 or less, 5 or less, 4 or less, 3 or less, 2 or less, 1 or less, 0.8 or less, 0.6 or less, 0.4 or less, 0.2 or less, 0.1 or less, 0.08 or less, 0.06 or less, 0.04 or less, 0.02 or less, 0.01 or less, 0.008 or less, 0.006 or less, 0.004 or less, or It could be about 0.002 or less.

[0111] The sun in Fig. 11 may additionally satisfy Equation 2 below.

[0112] [Equation 2]

[0113] I2≤ T N / sinθ1

[0114] T in Equation 2 N The meanings of , θ1 and I2 are the same as in the case of Equation 1.

[0115] The effect intended in the present application can be further improved by additionally satisfying Equation 2.

[0116] In another aspect of the present application, as shown in FIG. 12, a second sliding portion may be formed on the active material layer (401) of the positive electrode at the opposite end (left end of FIG. 12) of the end (right end of FIG. 12) where the sliding portion of the active material layer (401) of the positive electrode is formed.

[0117] In such cases, the electrode assembly can be designed to satisfy Equation 3 below.

[0118] [Equation 3]

[0119] T N / tanθ1≤ I2+ TP / tanθ2

[0120] T in Equation 3 N , θ1 and I2 are as defined in Equations 1 and 2, and T P is the thickness of the active material layer of the positive electrode, and θ2 is the angle of inclination of the second sliding portion of the positive electrode active material layer.

[0121] In the above, the meaning of the thickness TP of the positive active material layer is the thickness of the normal thickness region of the positive active material layer, just like the thickness TN of the negative active material layer in Equations 1 and 2. In addition, the inclination angle θ2 of the second sliding portion of the positive active material layer can also be calculated in accordance with the method of calculating θ1 in Equations 1 and 2.

[0122] The relationship in Equation 3 is between I2 and W in Fig. 12. P The sum of is W N It means something equal to or greater than. Such a relationship is necessary for the achievement of the purpose of the present application.

[0123] The structure of Fig. 12 can be designed to additionally satisfy Equation 4 below.

[0124] [Equation 4]

[0125] I2+ T P / tanθ2≤ T N / sinθ1

[0126] T in Equation 4 N , θ1, I2, T P and θ2 have the same meaning as in Equation 3.

[0127] The structure of Fig. 12 can also be designed to additionally satisfy Equation 5 below.

[0128] [Equation 5]

[0129] θ2 / θ1> 1

[0130] In Equation 5, θ1 and θ2 have the same meaning as in Equations 3 and 4.

[0131] The upper limit of θ2 / θ1 in the above Equation 5 can be formed at an appropriate ratio. For example, θ2 / θ1 may be 5 or less, 4.5 or less, 4 or less, 3.5 or less, 3 or less, 2.5 or less, 2 or less, or 1.5 or less.

[0132] With the above design, the capacitance per unit area of ​​the anode can be maximized while securing a capacitance relationship between the cathode and anode where N / P inversion does not occur.

[0133] As described above, in the structure of the electrode assembly of FIGS. 11 and 12, the active material layer (301, 401) is shown as being formed only between the current collector (103, 104) and the separator (200), but the active material layer (301, 401) may also be formed on the opposite side of each current collector layer (103, 104).

[0134] For example, in the above structure, the cathode may additionally include an active material layer formed on a side opposite to the side facing the separator (200) of the current collector layer (103 in FIG. 11 and 12).

[0135] In this case, the additionally included active material layer may have a symmetrical structure with respect to the active material layer (301 in FIG. 11 and 12) existing between the current collector layer (103 in FIG. 11 and 12) and the separator (200 in FIG. 11 and 12).

[0136] That is, for example, as shown in FIG. 10, when active material layers (101, 102) are formed on both sides of the current collector layer (100), the active material layers (101, 102) may have a symmetrical structure. In this case, the symmetrical structure refers to a substantial symmetrical structure.

[0137] Accordingly, in the above-mentioned symmetrical structure, the inclination angle of the sliding part (e.g., θ1 in FIG. 11 and 12) or the thickness of the active material layer (T in FIG. 11 and 12) N) does not have to have completely identical values. For example, if the absolute value of the error in the inclination angle or thickness is 10% or less, 9% or less, 8% or less, 7% or less, 6% or less, 5% or less, 4% or less, 3% or less, 2% or less, or 1% or less in both active material layers, both active material layers may be considered to have a symmetrical structure. In the above, the error refers, for example, in the case of thickness, to the thickness of one active material layer T N1 It is called, and the thickness of the other active material layer is T N2 In the case of saying that, 100Х(T N1 - T N2 ) / T N2 It is calculated as such, and the same applies to the angle of inclination.

[0138] In the above structure, the positive electrode may also additionally include an active material layer formed on the side opposite to the side facing the separator (200) of the current collector layer (104 in FIG. 11 and 12).

[0139] In this case, the additionally included active material layer may have a symmetrical structure with respect to the active material layer (401 in FIG. 11 and 12) existing between the current collector layer (104 in FIG. 11 and 12) and the separator (200 in FIG. 11 and 12), as in the case of the cathode, and the meaning of the symmetrical structure is the same as in the case of the cathode.

[0140] In the present application, the surface of the sliding portion of the active material layer of the cathode or anode (i.e., the surface of the inclined portion) may be a cut surface, i.e., a cut surface. That is, the sliding portion may be a sliding portion that occurs naturally during the slurry coating process, or it may be artificially formed by cutting. The angle of inclination or width of the naturally occurring sliding portion (W in FIG. 11 and 12) N , W PIf the gap between the negative active material layer and the positive active material layer (I1 and I2 in FIG. 11 and 12, etc.) or the gap between the negative active material layer and the positive active material layer does not satisfy Equations 1 to 5 above, the sliding portion can be artificially formed by a known cutting method.

[0141] There are no specific restrictions on the method of artificially forming such sliding parts, and known etching, cutting, or non-contact cutting methods (e.g., laser cutting methods) may be applied.

[0142] In addition, there are no special limitations on the materials forming the current collector, active material layer, etc., in the electrode assembly of the present application, and the structure can be formed using known materials.

[0143] In addition, there are no restrictions on the manufacturing method, and the electrode assembly can be constructed by manufacturing the electrode using a known manufacturing method. If necessary, the aforementioned etching, cutting, or non-contact cutting processes may be performed on the electrode formed by the known manufacturing method.

[0144] The present application also relates to a secondary battery or electrochemical device comprising the electrode assembly and the electrolyte.

[0145] As long as the electrode assembly of the present application is applied, there are no special restrictions on the materials constituting the secondary battery or electrochemical element, and known materials may be used. Explanation of the symbols

[0146] 200: Separator 300: Cathode 400: Anode 100, 103, 104: Entire floor of the house 101, 102, 301, 302, 401, 402: Active material layer S: Sliding part 10: Starting point of the active material layer NC: Uninformed 1011: Side of the slitting section

Claims

Claim 1 cathode; The cathode and the anode are stacked with the separator in between, and the cathode and the anode each include a current collector layer and an active material layer existing between at least the current collector layer and the separator, and each of the cathode and the anode has a first end portion having a tab portion formed therein and a second end portion opposite to the first end portion, and the cathode and the anode are stacked such that their first end portions face each other or one first end portion faces the other second end portion, and a slitting portion is formed in the active material layer of one of the first and second end portions of the cathode, and a sliding portion is formed in the other active material layer, and the active material layers of both end portions of the anode are located inwardly than the active material layers of both end portions of the cathode that they face each, and the gap (I1) between the anode active material layer and the cathode active material layer at the end of the cathode where the slitting portion is formed and the cathode where the sliding portion is formed An electrode assembly in which the ratio I2 / I1 of the gap (I2) between the active material layer of the positive electrode and the active material layer of the negative electrode at the end is within the range of 0.5 to 10, and the active material layer of the negative electrode is thicker than the active material layer of the positive electrode. Claim 2 delete Claim 3 An electrode assembly according to claim 1, wherein a sliding portion is formed in the active material layer of the end portion facing the end portion of the positive electrode where the slitting portion of the negative electrode is formed. Claim 4 In claim 3, the surface of the sliding portion of the active material layer of the positive electrode is a cut surface, in an electrode assembly. Claim 5 In claim 3, an electrode assembly having a slitting portion formed on the active material layer of the positive electrode at the opposite end of the end where the sliding portion of the active material layer of the positive electrode is formed. Claim 6 An electrode assembly according to claim 5, wherein the slitting portion of the active material layer of the positive electrode is located on the inner side relative to the sliding portion of the active material layer of the negative electrode. Claim 7 In claim 5, an electrode assembly satisfying the following Equation 1: [Equation 1]T N / tanθ1≤I2 From Equation 1 T N I is the thickness of the active material layer of the cathode, θ1 is the angle of inclination of the sliding portion of the cathode, and I2 is the gap between the active material layer of the anode and the active material layer of the cathode at the end of the cathode where the sliding portion is formed. Claim 8 An electrode assembly according to claim 7, wherein tanθ1 is within the range of 0.001 to 10. Claim 9 In claim 7, an electrode assembly further satisfying the following Equation 2: [Equation 2] I2 ≤ T N / sinθ1 in Equation 2 T N I is the thickness of the active material layer of the cathode, θ1 is the angle of inclination of the sliding portion of the cathode, and I2 is the gap between the active material layer of the anode and the active material layer of the cathode at the end of the cathode where the sliding portion is formed. Claim 10 In claim 3, an electrode assembly having a second sliding portion formed on the active material layer of the positive electrode at the opposite end of the end where the sliding portion of the active material layer of the positive electrode is formed. Claim 11 In claim 10, the surface of the second sliding portion of the active material layer of the positive electrode is a cutting surface, in an electrode assembly. Claim 12 In claim 10, an electrode assembly satisfying the following Equation 3: [Equation 3]T N / tanθ1≤ I2+ T P / tanθ2 in Equation 3 T N ε is the thickness of the active material layer of the cathode, θ1 is the inclination angle of the sliding portion of the cathode, I2 is the gap between the active material layer of the anode and the active material layer of the cathode at the end of the cathode where the sliding portion is formed, and T P is the thickness of the active material layer of the anode, and θ2 is the angle of inclination of the second sliding part of the anode. Claim 13 In claim 12, an electrode assembly further satisfying the following Equation 4: [Equation 4] I2 + T P / tanθ2≤ T N / sinθ1 in Equation 4 T N ε is the thickness of the active material layer of the cathode, θ1 is the inclination angle of the sliding portion of the cathode, I2 is the gap between the active material layer of the anode and the active material layer of the cathode at the end of the cathode where the sliding portion is formed, and T P is the thickness of the active material layer of the anode, and θ2 is the angle of inclination of the second sliding part of the anode. Claim 14 In claim 10, an electrode assembly satisfying the following Equation 5: [Equation 5] θ2 / θ1 > 1. In Equation 5, θ1 is the angle of inclination of the sliding part of the cathode, and θ2 is the angle of inclination of the second sliding part of the anode. Claim 15 In claim 1, the negative electrode further comprises an active material layer formed on a side opposite to the side facing the separator of the current collector layer, forming an electrode assembly. Claim 16 In claim 15, the electrode assembly has a symmetric structure in which an active material layer formed on a side opposite to the side of the current collector layer facing the separator and an active material layer existing between the current collector layer and the separator. Claim 17 In claim 1, the positive electrode assembly further comprises an active material layer formed on a side opposite to the side facing the separator of the current collector layer. Claim 18 In claim 17, the electrode assembly has a symmetric structure in which an active material layer formed on a side opposite to the side of the current collector layer facing the separator and an active material layer existing between the current collector layer and the separator. Claim 19 A secondary battery comprising an electrode assembly and an electrolyte according to any one of claims 1 and 3 to 18.

Citation Information

Patent Citations

  • Electrode plate and secondary battery

    US20180006322A1

  • Electrode plate and secondary battery

    WO2014034708A1