Graphene based additive for cement and concrete, compositions and methods of preparation

By dispersing high purity graphene in a pre-blend mixture with an activator, the method enhances the structural strength of cement and concrete products, overcoming dispersion issues and cost limitations, and enables the creation of high-performing concretes with reduced cement usage.

WO2024197394A1PCT designated stage expired Publication Date: 2024-10-03BARCLIFF ENERGY SERVICES LTD
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
PCT/CA2024/050371
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-03-29
Filing Date
2024-03-26
Publication Date
2024-10-03

AI Technical Summary

Technical Problem

The incorporation of graphene into cement and concrete compositions is hindered by its high cost and limited dispersion in water, which restricts its wide-scale adoption for enhancing structural properties.

Method used

A pre-blend mixture is prepared by dissolving an activator in water under low shear conditions and dispersing high purity graphene, such as reduced graphene oxide or pristine graphene, to enhance its dispersion in cement and concrete slurries, allowing for improved interaction with calcium binding sites and increased structural strength.

Benefits of technology

The method achieves substantial improvements in the strength of cement and concrete products, reducing the amount of cement required and lowering production costs, while enabling the use of additives like flyash to create high-performing concretes that meet infrastructure specifications.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CA2024050371_03102024_PF_FP_ABST
    Figure CA2024050371_03102024_PF_FP_ABST
Patent Text Reader

Abstract

Compositions and processes related to the preparation of concrete and cement slurries having enhanced properties are described. The compositions and processes enhance the incorporation of graphene into concrete and cement slurries that ultimately improves the dispersion of graphene within these slurries. The resulting products can have substantially improved strength properties.
Need to check novelty before this filing date? Find Prior Art

Description

GRAPHENE BASED ADDITIVE FOR CEMENT AND CONCRETE, COMPOSITIONS AND METHODS OF PREPARATIONFIELD

[0001] Compositions and processes related to the preparation of concrete and cement slurries having enhanced properties are described. The compositions and processes enhance the incorporation of graphene into concrete and cement slurries that ultimately improves the dispersion of graphene within these slurries. The resulting products can have substantially improved strength properties.BACKGROUND

[0002] The production of Portland cement is an energy-intensive process that can contribute to greenhouse gas (GHG) emissions. As such, Portland Cement producers are being encouraged, and in various jurisdictions, mandated to reduce GHG emissions if the production energy source is carbon derived.

[0003] The production of concrete from cement is a well-known and complex process where final concrete products can be engineered to have a wide-range of structural properties. Desired structural properties can be controlled / developed by adjustment / manipulation of any number of variables throughout the production cycle including for example, the processes by which cement is manufactured, the formulations of cement prior to mixing concrete, the processes of mixing and curing the concrete as well as other variables.SUMMARY

[0004] In accordance with the disclosure, methods of preparing a pre-blend (PB) mixture for addition to cement and concrete slurries are described. The methods include the steps of: dissolving an activator in a sufficient volume of pre-blend water under low shear conditions to form an aqueous mixture; and, dispersing a graphene in the aqueous mixture under low shear conditions to effect dispersion of the graphene in the aqueous mixture wherein the graphene is characterized as having greater than 90 mol% carbon.

[0005] In various embodiments:• the graphene is a reduced graphene oxide (rGO) characterized as having greater than 92 mol% carbon.• the graphene is a pristine graphene (PG) characterized as having greater than 94 mol% carbon.• the concrete or cement slurry is a blend of cement water, cement and / or additives and wherein the activator is added to the pre-blend water at 0.05-0.25% by weight of cement (BWOC).• the activator is 0.1 % BWOC.• the cement slurry or concrete comprises a blend of cement water, cement and additives and wherein the graphene is added to the pre-blend water at 0.002% to 0.02% by weight of cement (BWOC).• the graphene is 0.008% BWOC.

[0006] In another aspect a cement slurry is described, the cement slurry comprising a slurried mixture of: cement and cement water; and, a pre-blend mixture of pre-blend water, activator and graphene wherein the activator is dissolved in the pre-blend water prior to mixing with the cement and the graphene is dispersed in the pre-blend mixture, wherein the graphene is characterized as having greater than 90 mol% carbon.

[0007] In various embodiments:• the graphene is 0.002% to 0.02% by weight of cement (BWOC).• the graphene is a reduced graphene oxide (rGO) characterized as having greater than 92 mol% carbon.• the graphene is a pristine graphene (PG) characterized as having greater than 94 mol% carbon.• the activator is 0.05-0.25% by weight of cement (BWOC).• the cement slurry includes one or more aggregates.• the cement slurry includes one or more additives.• the additives include flyash.BRIEF DESCRIPTION OF THE DRAWINGS

[0008] Various objects, features and advantages of the disclosure will be apparent from the following description of particular embodiments of the disclosure, as illustrated in the accompanying drawings.Figure 1 is a schematic diagram showing typical structures of graphite, pristine graphene, graphene oxide (GO) and reduced graphene oxide (rGO).Figure 2 is a schematic diagram of a polycarboxylate activator.DETAILED DESCRIPTION

[0009] The inventors, who have experience in the manufacture and formulation of cement and concrete products, have determined the use of additives to cement can be used to produce cement and concrete products having superior and / or desirable structural properties.

[0010] Various aspects of the disclosure will be described with reference to the figures. For the purposes of illustration, components depicted in the figures are not necessarily drawn to scale. Instead, emphasis is placed on highlighting the various contributions of the components to the functionality of various aspects of the disclosure. A number of possible alternative features are introduced during the course of this disclosure. It is to be understood that, according to the knowledge and judgment of persons skilled in the art, such alternative features may be substituted in various combinations to arrive at different embodiments of the disclosure.

[0011] Graphene generally refers to a class of compositions characterized as oxidized layers of crystalline graphite (Figure 1). As shown in Figure 1, each of graphite, pristine graphene, graphene oxide and reduced graphene oxide are comprised of 2D layers of hexagonal carbon rings.

[0012] Graphite is composed of 2D layers of carbon atoms that are arranged in sheets of 6- membered hexagonal rings. Generally, graphene can be produced via various processes by oxidizing graphite carbon atoms. These layers are attached to one another on their edges and generally be considered as an infinite series of fused benzene rings without hydrogen atoms. The graphene structure conserves the integrity of the 2D layer structure of graphitebut introduces oxygen-containing functional groups attached to both sides of the carbon plane and to the edges. rGO is characterized by a higher proportion of carbon in the 2D structure as compared to GO. Pristine graphene (PG) is a purer form of rGO and is typically characterized by a carbon content greater than 96% by wt.

[0013] Graphene structures can be obtained using other techniques including hydrothermal treatment of glucose and by chemical vapor deposition (OVD) techniques. Thus, a more general definition of graphene is a single atom carbon layer with both surfaces modified by oxygen containing functional groups.

[0014] Without being bound to any particular theory, the disclosure references various chemical properties and morphological structures of forms of graphene including PG and rGO. That is, like any 2D carbon layer, graphene can be single layer or multilayer structures of different sizes and shapes and have varying levels of purity and / or variations in functional groups. The relative purity of graphene is determined by the functional groups that may be interspersed across the 2D layer that affect the localized and macroscopic properties of the graphene.

[0015] Typically, the carbon layers in a multilayer graphene are separated by hydroxyl and / or carboxy functional groups of the planar carbon atoms.

[0016] As noted above, higher carbon purity graphene oxides are generally referred to reduced graphene oxide (rGO) and pristine graphene (PG). Each are characterized by a reduced number of carboxy groups and a greater proportion of hydroxy groups. For the purposes of definition rGO has carbon content by weight greater than 94% and PG has carbon content by weight greater than 96%.

[0017] Generally, rGO and PG have higher chemical activity.

[0018] Further, lower purity GO is typically hydrophilic due to the presence of hydroxy / carboxy groups to the hexagonal carbon rings within the two-dimensional carbon layers that project into the interplanar space.

[0019] Generally, as the carbon purity of the graphene increases, the number of inter-ring and inter-planar oxygens decreases, the graphene becomes increasingly hydrophobic. As the graphene purity increases and the hydrophobicity increases, this decreases the ability ofgraphene to disperse in water. Generally, GO will be hydrophilic whereas rGO may be amphipathic and PG is generally hydrophobic.

[0020] In the past, the use of graphene in cement and / or concrete compositions has been known to enhance various structural properties of concrete when GO is blended within the concrete. However, while GO is known to provide benefits, its wide-scale and / or commercial adoption is limited by the high cost of GO and the concentrations required in the concrete to impart improved properties.

[0021] Accordingly, there has been a need for compositions and processes that improve the incorporation of the GO into cement and / or concrete compositions.Pre-blend Suspension of GO

[0022] In accordance with one aspect of the disclosure, processes for preparing a pre-blend suspension of high purity graphene as an additive to disperse in cement (e.g. Portland cement) and / or a concrete slurry are described. The pre-blend suspension is prepared as follows:

[0023] Step 1-An activator (e.g. a polycarboxylate) powder is added to water and mixed. The activator is mixed under low shear conditions to effect dispersion of the activator in the water. The O' groups of the activator and water form an ionic mixture (Figure 2).

[0024] Step 2- High purity GO, preferably rGO or PG, is added to the activator / water mix. The O' groups of the activator enables the hydrophobic rGO / PG to fully disperse in the water / activator mix. The rGO / PG is added under low shear conditions to preserve the integrity of the 2D carbon layers of the rGO / PG.

[0025] As explained in greater detail below, the process to prepare the pre-blend suspension will typically consider the desired batch volume of concrete, and the desired rGO / PG mass in the concrete to determine the volume of pre-blend suspension that will be added to the concrete mixture.

[0026] Generally, in accordance with the disclosure, rGO / PG in the final concrete product will be in the range of 0.002% to 0.02% by weight of cement (termed herein as “by weight of cement” or BWOC) in concrete product. Hence, the amount of rGO / PG added to the preblend mixture will typically be based on the desired total mass rGO / PG in the concrete batch.

[0027] For example, if the total volume of a concrete batch is 1 m3, the total weight of cement in a 1 m3batch of concrete may be 350 kg. The total water volume / mass in the mixture may be about 150 liters (kg). Accordingly, based on 0.008 wt% rGO / PG BWOC, the total mass of rGO / PG in the concrete would be 0.008% x 350 kg or 0.028 kg or 28 g.

[0028] Accordingly, a pre-blend suspension is prepared in which at least 28 g of rGO / PG is prepared within a known volume of water. A relatively small volume of PB mixture is required to suspend 28 g of rGO / PG. For example, 28 g of rGO / PG can be suspended in about 1 liter of water together with 350 g of activator (0.1% BWOC).

[0029] The volume of water used to suspend the rGO / PG is arbitrary, provided the volume is sufficient to fully dissolve the activator. For example, and for convenience, batches of preblend in fixed volumes amounts of 1, 10, 100 liters, etc. may be prepared with a known mass of rGO / PG in each batch.

[0030] Thus, in our example of preparing a l m3batch of concrete with 0.008% BWOC rGO / PG with 150 liters of water being added, a 1 -liter PB mixture (with 28 g of rGO / PG) may be mixed with 149 liters of water and then blended with the cement, aggregates and other solid ingredients.

[0031] The mass of activator is preferably 0.05-0.25 % BWOC, and more preferably about 0.1% relative to BWOC to rGO / PG.

[0032] Other additives to PB mixture may include an antisettling agent or activator aid and should be used if the water concentration is greater than 50%. The activator aid may be added at various concentrations to satisfy the required results, with typical concentrations ranging from 0.05-3.5%.

[0033] An optional freeze protection agent, such as methanol, may also be added to the PB mixture. Freeze protection concentrations can be varied depending on the temperatures the mixtures may be exposed to. Possible concentrations range from 5-40% by weight of water (BWOW)

[0034] The PB mixture is stable and will not settle out over a number of days.

[0035] As introduced above, the PB mixture is used as an additive during slurry / concrete mixing processes to fully disperse rGO / PG within the concrete / cement slurry mixture. It istheorized that the improved dispersion of rGO / PG within the PB mixture also enhances the dispersion of rGO / PB within a cement / concrete slurry which in turn increases the number of interactions between rGO / PG and calcium binding sites within concrete and the calcium silica hydration (C-S-H) process.

[0036] It is generally understood that the rGO / PG concrete interaction is a cross- linking / mechanical interaction that promote the growth of C-S-H by creating nucleation sites.PB Example

[0037] An example of the preparation of a PB mixture is as follows:

[0038] All components are referenced as by weight of cement (BWOC).

[0039] 0.1% BWOC polycarboxylate activator was added to 1 liter of room temperature water and blended under low shear conditions within a low shear blender (about 0.5-1.5 minutes). 0.008% BWOC rGO was added and blended under low shear conditions to fully disperse the rGO within the mixture (about 0.5-1.5 minutes). 0.25-2.25% of a suspension / activator aid (e.g., a natural clay, synthetic polymer based, or any other viscosifying additive) was added and blended under low shear conditions (about 1-2 minutes) until homogeneity was reached. The resulting mixture had suspension stability.Process for Mixing PB Mixture within a Cement or Concrete Slurry

[0040] The PB mixture may be added to a cement / concrete mixture in an amount such that the concentration of rGO / PG within a cement or concrete slurry is about 0.008% BWOC. Substantial improvements in various cement / concrete products when cured are observed when prepared with the PB mixture when 0.002%-0.016%; preferably 0.006-0.01% and more preferably 0.008% rGO / PG BWOC are incorporated into the slurry.

[0041] The following examples are provided of various concretes with and without flyash as an additive:Examples and Testing ResultsSample 1-ControlSample 2- Control plus 0.008% BWOC PG and longer mix time

[0042] A “long time” mix is batch where mixing is continued over a period of time to replicate the concrete being in a mixing truck for a period of time as it is being transported to a job site.

[0043] Sample 2 testing shows that the 3-, 7- and 28-day crush tests showed significant strength increase.Sample 3- Control plus 0.008% BWOC PG (Higher Slump)

[0044] Sample 3 testing shows that the 3, 7 and 28 day crush tests showed modest strength increase for a higher slump.Sample 4-Control plus 0.008% BWOC

[0045] Sample 4 testing shows that the 3-, 7- and 28-day crush tests showed substantial strength increase for a reduced water.Sample 5-Control plus Flyash (Control 2)Sample 6-Control plus Flyash plus 0.22 g PG

[0046] Sample 6 testing shows that the 3-, 7- and 28-day crush tests showed substantial strength increase for a concrete with PG, flyash and comparable slump.Sample 7-Control plus Flyash plus 0.008% BWOC PG

[0047] Sample 7 testing shows that the 3-, 7- and 28-day crush tests showed substantial strength increase for a concrete with PG, flyash and low slump.Sample 8-Control plus Flyash plus 0.008% BWOC rGO

[0048] Sample 8 testing shows that the 3-, 7- and 28-day crush tests showed substantial strength increase for a concrete with PG, flyash and comparable slump.Advantages

[0049] As illustrated by the foregoing examples, the addition of high purity graphene oxide to cement and concrete slurries enables the creation of high-performing cement / concretes when cured. Thus, products can be produced that reduce the amount of cement required for the product to meet infrastructure specifications with reduced costs.

[0050] The examples further illustrate that the addition of flyash together with high purity graphene can also enable the creation of high-performing concretes.

[0051] The technology is applicable to a wide range of cement and concrete formulations and products. It could possibly be used to enhance the “non-Portland cement” products (e.g. Mag Phos products).

[0052] Although the present disclosure has been described and illustrated with respect to preferred embodiments and preferred uses thereof, it is not to be so limited since modifications and changes can be made therein which are within the full, intended scope of the disclosure as understood by those skilled in the art.

Claims

CLAIMS1. A method of preparing a pre-blend (PB) mixture for addition to a cement slurry, the method comprising the steps of: a) dissolving an activator in a sufficient volume of pre-blend water under low shear conditions to form an aqueous mixture; and, b) dispersing a graphene in the aqueous mixture under low shear conditions to effect dispersion of the graphene in the aqueous mixture wherein the graphene is characterized as having greater than 90 mol% carbon.

2. The method as in claim 1 wherein the graphene is a reduced graphene oxide (rGO) characterized as having greater than 92 mol% carbon.

3. The method as in claim 1 wherein the graphene is a pristine graphene (PG) characterized as having greater than 94 mol% carbon.

4. The method as in any one of claims 1-4 wherein the cement slurry comprises a blend of cement water, cement and additives and wherein the activator is added to the pre-blend water at 0.05-0.25% by weight of cement (BWOC).

5. The method as in claim 4 wherein the activator is 0.1 % BWOC.

6. The method as in any one of claims 1-5 wherein the cement slurry comprises a blend of cement water, cement and additives and wherein the graphene is added to the pre-blend water at 0.002% to 0.02% by weight of cement (BWOC).

7. The method as in claim 6 wherein the graphene is 0.008% BWOC.

8. A cement slurry comprising a slurried mixture of: cement and cement water; and, a pre-blend mixture of pre-blend water, activator and graphene wherein the activator is dissolved in the pre-blend water prior to mixing with thecement and the graphene is dispersed in the pre-blend mixture, wherein the graphene is characterized as having greater than 90 mol% carbon.

9. The cement slurry of claim 8 wherein the graphene is 0.002% to 0.02% by weight of cement (BWOC).

10. The cement slurry of claim 8 or claim 9 wherein the graphene is a reduced graphene oxide (rGO) characterized as having greater than 92 mol% carbon.

11. The cement slurry of claim 8 or claim 9 wherein the graphene is a pristine graphene (PG) characterized as having greater than 94 mol% carbon.

12. The cement slurry of any one of claims 8-11 wherein the activator is 0.05-0.25% by weight of cement (BWOC).

13. The cement slurry of any one of claims 8-12 further comprising one or more aggregates.

14. The cement slurry of any one of claims 8-13 further comprising one or more additives.

15. The cement slurry of claim 14 where the additive is flyash.

Citation Information

Patent Citations

  • Active carbon cement composite material and preparation method thereof

    CN101941821A

  • Low-carbon easy-to-mix concrete admixture as well as preparation method and application thereof

    CN116332552A

  • Quick-setting environment-friendly alkali-activated cement-based low-carbon concrete and preparation method thereof

    CN116621511A

  • Carbon storage using ash, seawater, and alkali activator as a non-cement-based building materials

    US11174201B1