A vessel with a joule heating element and methods of using the same

The Joule heating element system in a vessel efficiently depolymerizes high-viscosity plastic waste by direct heating, addressing the inefficiencies of current reactor systems and producing a usable product stream with improved viscosity and molecular weight.

WO2024200203A1PCT designated stage expired Publication Date: 2024-10-03SABIC GLOBAL TECHNOLOGIES BV
View PDF 8 Cites 0 Cited by

Patent Information

Application Number
PCT/EP2024/057600
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-03-24
Filing Date
2024-03-21
Publication Date
2024-10-03

AI Technical Summary

Technical Problem

Current reactor systems for converting high-viscosity plastic waste to usable liquids and gases face inefficiencies due to poor mixing, heat transfer, and mass transfer issues, making them unsuitable for commercial use, especially when processing feed streams with viscosities exceeding 200,000 centipoise.

Method used

A vessel equipped with a Joule heating element featuring a bundle of electrically-resistive wires, which provides a high surface area to void volume ratio, allowing for direct heating of high-viscosity polymeric feed streams to achieve efficient depolymerization, reducing residence time and minimizing the production of undesirable by-products.

Benefits of technology

The Joule heating element system enables effective depolymerization of high-viscosity plastic waste, producing a product stream with lower viscosity and molecular weight, suitable for further processing, while maintaining high heat and mass transfer characteristics, thus overcoming the inefficiencies of existing reactor systems.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure EP2024057600_03102024_PF_FP_ABST
    Figure EP2024057600_03102024_PF_FP_ABST
Patent Text Reader

Abstract

This disclosure includes vessels having Joule heating elements and methods of using the same. In some vessels, the Joule heating element has electrically-resistive elements in the form of wires extending from a first end of the heating element to a second end of the heating element. The electrically-resistive elements define a void volume between the electrically-resistive elements and between the electrically-resistive elements and the vessel, the void volume is configured to permit liquid to flow therethrough from the first end of the heating element to the second end of the heating element. In some methods, a polymeric feed stream is passed through the vessel and heat is transferred from the electrically-resistive heating elements to the polymeric feed stream to produce a product stream that includes depolymerized polymers. The feed stream includes plastic waste, and the product stream includes depolymerized plastic waste.
Need to check novelty before this filing date? Find Prior Art

Description

A VESSEL WITH A JOULE HEATING ELEMENT AND METHODS OF USING THE SAME

[0001] This application claims the benefit of European Patent Application No. EP23164111 filed March 24, 2023. The entire contents of the above-referenced disclosure is specifically incorporated herein by reference.Technical Field

[0002] The invention generally concerns a vessel that includes a Joule heating element and methods of using the vessel to depolymerize polymers, preferably plastic waste.Background Art

[0003] Refinery integration involves using existing refinery equipment such as delayed cokers and fluid catalytic crackers to convert waste feed streams (e.g., plastic waste, high-boiling-point petrochemical streams) to usable liquids (e.g., pyrolysis oils) and gases (e.g., ethylene and propylene). Conversion of high-molecular- weight feed streams to usable lower-molecular-weight feed streams can require temperatures in the range 350 °C to 500 °C for reaction times of 30 to 120 minutes.

[0004] However, conversion of viscous polymers to oligomers and liquids and gases has been a challenge. Many reactor systems that process waste plastic to liquids (e.g., pyrolysis oil, also referred to as “pyoil”) are batch or semi-batch processes that are inefficient and capital intensive. Viscosities of feed systems can exceed 200,000 centipoise (cP), making it difficult for reactor stirrers to work well. Feasible residence times in some reactors are too short and the typical operating temperatures of less than 300 °C are too low to achieve the required conversion. Other reactors require an external heat supply and exhibit poorer than desired mass and heat transfer characteristics. The lower surface area afforded by the heating elements of some reactors significantly reduces the rate of heat transfer, and these reactors also have concentration and temperature gradients that adversely affect their performance.

[0005] Several reactors exist for conversion of waste feed streams to usable liquids and gases. U.S. Patent No. 6,216,343 to Leland et al. describes a microchannel heat pipe that includes a tubular housing split longitudinally into two halves. U.S. Patent No. 11,261,140 to Sangar et al.describes applying an electrical current to an electrically-conductive reaction zone that can be a monolith made from a ceramic material or metallic material (e.g., silicon carbide, aluminum nitride, boron nitride, tungsten carbide, a MAX phase alloy, a ferrochrome alloy, and combinations thereof). International Patent Application Publication No. WO 2022 / 180470 to Fioravante describes a plastic pyrolysis plant that includes an electric heat exchanger as the pyrolysis reactor. International Patent Application Publication No. WO 2022 / 219053 to Ratnakar et al. describes a modular reactor for carrying out endothermic reactions that includes a series of resistive heating elements placed inside the reactor.

[0006] However, all of these processes suffer from poor mixing, which in turn affects heat transfer and mass transfer, and the types of reactors that they use can be inefficient and cost- ineffective for commercial use. Further, such reactors may be unsuitable for processing higher- viscosity (e.g., 200,000 cP or greater) feed streams.

[0007] While methods for heating reaction feed streams exist, the need for improvements in this field persists.SUMMARY OF THE INVENTION

[0008] A solution to at least one of the problems associated with heating chemical feed streams has been discovered. In one aspect of the present invention, methods for depolymerization of high viscosity polymeric compositions comprising plastic waste are described. A method includes passing (e.g., flowing) a polymeric feed stream through a vessel of a reactor having a Joule heating element disposed within the vessel. The Joule heating element has electrically-resistive elements (a bundle of wires) extending from a first end of the heating element to a second end of the heating element, and at least the electrically-resistive elements and the vessel cooperate to define a void volume. The polymeric feed stream flows through the void volume of the vessel between the first end of the heating element and the second end of the heating element. For clarification, the void volume in this regard should be understood to mean, in a reactor free of any feed stream the volume not occupied by the electrically-resistive elements and any other volume displacing material in the reactor. The void volume permits viscous material (e.g., a high viscosity polymeric stream) to flow therethrough from the first end of the heating element to the second end of the heating element. A ratio of the surface area to void volume can be greater than 1.3 square millimeters per cubicmillimeter (mm2 / mm3). The electrically-resistive elements can include iron (Fe), chromium (Cr), aluminum (Al), yttrium (Y), or a combination thereof, or an alloy thereof. In a preferred aspect, each of the electrically-resistive elements are an FeCrAl alloy or a nickel / chromium alloy. Each of the electrically-resistive elements have a resistivity at 20 °C that is greater than about 1 microohm meter (pQ*m). In a preferred aspect, the electrically-resistive elements are wires. The heating element can take on the shape of the vessel. An interior surface of the vessel that surrounds the electrically-resistive elements can be electrically-insulative. In other aspects, an electrically- insulative layer can be disposed within the vessel and around the electrically-resistive elements (e.g., a sleeve). In a preferred aspect, the electrically-insulative layer is not disposed around the electrically-resistive elements. In some aspects, the electrically-resistive elements are not coated with a catalyst. Such a vessel provides the advantage of a smaller-sized vessel with high heat and mass transfer characteristics. It also facilitates the processing of relatively high-viscosity (e.g., 200,000 cP or greater) feed streams.

[0009] The polymeric feed stream can include a high-molecular-weight polymer having a zero-shear viscosity of at least 100,000 centipoise (cP), preferably 200,000 cP to 500,000 cP or 100,000 cP to 1,000,000 cP at 150 °C to 300 °C, a weight average molecular weight (Mw) of 30,000 Dalton (Da) to 250,000 Da, or a combination thereof. In some aspects, the polymeric feed stream is a plastic waste feed stream, preferably a plastic waste feed stream, containing primarily polyolefins. The polymeric feed stream has a temperature of 150 °C to 300 °C at the inlet of the reactor. The flowable polymeric feed stream can be heated by passing an electric current through the electrically-resistive elements such that heat is transferred (e.g., directly transferred or directly heated) from the electrically-resistive elements to produce a product stream that includes depolymerized polymers. In some aspects, the polymeric feed stream is heated to a temperature from 375 °C to 500 °C over a residence time of 10 minutes to 60 minutes. Direct heating in combination with minimal residence time provides the advantage of depolymerizing polymers without production of undesirable by products. In addition, the process advantageously produces a product stream (e.g., a depolymerized product stream containing plastic waste) suitable to be used in other processing units, sold, or transported. Notably, the product stream temperature exiting the reactor is greater than the temperature of the feed stream entering the reactor. In a preferred aspect, the polymer feed stream is heated to temperature (e.g., 150 °C to 300 °C) suitableto produce a flowable material (e.g., molten and / or liquid phase) prior to entering the reactor. The polymer feed stream can include plastic waste. In some aspects, a diluent is added to the feed stream prior to entering the vessel. In preferred embodiments, no solvent or diluent is added to the feed stream and in such cases the feed stream is a molten polymeric feed stream. The diluent can be an inert solvent that can withstand temperatures of 375 °C to 500 °C. The product stream includes a depolymerized polymer composition having a kinematic viscosity of less than 1,000 cP, preferably less than 500 cP, more preferably less than 100 cP, a weight average molecular weight of 1,000 Da to 20,000 Da, or a combination thereof. The product stream is a depolymerized plastic waste stream. In some aspects, the product stream includes depolymerized polyolefins. In certain aspects, a diluent can be added to the product stream as the product stream exits the vessel.

[0010] In some aspects of the present invention, a reactor can include 1, 2, 3, 4, 5, 6, 7, 8, 9, 10, or more Joule heating elements. In certain aspects where 2 or more Joule heating elements are used, the Joule heating elements can be positioned in parallel or in series to one another. The use of multiple Joule heating elements in a reactor can be used to help control the temperature and / or flow of the polymer feed stream. In some aspects, a reactor can have a temperature profile such that the temperature of the reactor and / or of the polymer feed stream remains substantially constant from the inlet to the outlet of the reactor. In other aspects, a reactor can have a varying temperature profile such that the temperature of the reactor and / or the polymer feed stream is different in different portions or zones of the reactor. For instance, and in one aspect, a reactor can have 1, 2, 3, 4, 5, 6, 7, 8, 9, 10, or more zones. In one example, a reactor can have a first zone at around the inlet of the reactor, a second zone at around the midpoint of the reactor, and / or a third zone at around the outlet of the reactor. The temperatures of the zones and / or the product stream can vary in each zone (e.g., the temperature of the product stream can increase from zone 1 to zone 2 to zone 3, can decrease from zone 1, to zone 2, to zone 3, etc.) or remain substantially the same in each of zone 1, zone 2, and / or zone 3.

[0011] In yet another aspect of the present invention, a plurality of reactors (e.g., 1, 2, 3, 4, 5, 6, 7, 8, 9, 10, or more) can be used. The reactors can be positioned in parallel or in series relative to one another.

[0012] In other aspects of the present invention, the product stream can be a crude product stream that includes solid material (e.g., solid non-hydrocarbon material). In some aspects, the solid material is separated from the crude product stream to produce a refined product stream. The refined product stream can have a total solids content less than the original feed stream and / or the crude product stream. In some aspects, a diluent is added to the crude product stream prior to separation and / or transfer to another processing unit.

[0013] In the context of the present invention, the Joule heating element includes a wire, preferably a bundle of electrically-resistive wires, each extending between and in electrical communication with the first and second electrical conductors. Each of the wires of the bundle is non-linear and, preferably, is crimped along a length of the wire. A diameter of each of the wires in the bundle is between 0.1 millimeter (mm) and 1.3 mm. Notably, the wires of the bundle are not interwoven or bonded to one another, except at the ends for electrical connectivity.

[0014] The reactor can allow liquid flow from an inlet to an outlet of the vessel. In some aspects, the vessel is a reactor. Non-limiting examples of reactors can include a depolymerization reactor. In such a reactor, the inlet can receive a feed stream (e.g., a polymeric feed stream) and the outlet can receive a product stream (e.g., a partially depolymerized polymeric stream).

[0015] In another aspect of the invention, systems that include the present reactors are described. A system can include one of the present reactors, an optional extruder or stirring tank, and / or an optional separation / purification unit. The reactor can be coupled to the optional extruder or stirring tank and / or the optional separation unit. In some aspects, the extruder or stirring tank is positioned upstream of the reactor. The separation / purification unit can be positioned downstream of the reactor.

[0016] In another aspect of the invention, a reactor includes a vessel, a Joule heating element disposed within the vessel, the heating element having a bundle of electrically-resistive wires. Each of the wires extends between a first end of the heating element and a second end of the heating element, and at least the wires and the vessel cooperate to define a void volume through which fluid is permitted to flow through the vessel between the first end of the heating element and the second end of the heating element, a first electrical conductor coupled to the wires at thefirst end of the heating element, and a second electrical conductor coupled to the wires at the second end of the heating element.

[0017] In some aspects, each of the wires is non-linear and, preferably, is crimped along a length of the wire. In some aspects, each of the wires has a resistivity at 20 °C that is greater than about 1 pQ*m. In some aspects, the wires are not interwoven or bonded to one another. In some aspects, each of the wires comprises iron (Fe), chromium (Cr), aluminum (Al), yttrium (Y), or a combination thereof, or an alloy thereof, preferably a FeCrAl alloy or a nickel-chromium alloy. In some aspects, each of the wires has a diameter that is between 0.10 and 1.30 mm. In some aspects, the wires are electrically-insulated from the vessel, optionally, by an electrically-insulative layer of the vessel that surrounds the wires.

[0018] In some aspects, the electrically-resistive elements the ratio of the surface area of the electrically-resistive elements to the void volume is greater than 1.3 mm2 / mm3. In preferred aspects, the electrically-resistive elements are not coated with a catalyst and / or insulated. In some aspects, each of the electrically-resistive elements has a resistivity at 20 °C that is greater than about 1 pQ*m. First and second electrical conductors can be coupled to the electrically-resistive elements at the first end of the heating element and the second end of the heating element, respectively. An electrical power source can be coupled to the first and second electrical conductors. The electrical power source can be configured to pass a current through and thereby heat the electrically-resistive elements.

[0019] Other embodiments of the invention are discussed throughout this application. Any embodiment discussed with respect to one aspect of the invention can apply to other aspects of the invention as well and vice versa. It is contemplated that any embodiment or aspect discussed herein can be combined with other embodiments or aspects discussed herein and / or implemented with respect to any method or composition of the invention, and vice versa. Furthermore, compositions of the invention can be used to achieve methods of the invention.

[0020] The following includes definitions of various terms and phrases used throughout this specification.

[0021] The term “zero shear viscosity” refers to a viscosity of a material having non-Newtonian viscosity flow properties. Zero shear viscosities are measured at a shear rate of between 0.1 and 1 hertz using a shear rheometer. A non-limiting method to measure low shear and zero shear viscosities can include using an Ares G2 (TA® Instruments, USA) parallel plate rheometer having a plate diameter of 25 mm. Samples are dried for four hours prior to testing; and viscosity is measured at temperatures between 200 °C and 350 °C. The Carreau- Yasuda Model can be used to extrapolate to zero-shear viscosity (See, Casteran, et. al., Data-Driven Modelling of Polyethylene Recycling under High-Temperature Extrusion. Polymers 2022, 14 (4), 800).

[0022] The term “kinematic viscosity” refers to a viscosity of a flowable material. Kinematic viscosities can be measured using ASTM D445 or ASTM D446.

[0023] The phrase “direct heating” refers to the heating of a material with heat generated in situ in the reactor with the material to be heated and transferred to the material. For example, a composition (example, a feed stream) contacts the Joule heating element and is heated. This is distinguished from, for example, heating through the use of a working fluid that is heated externally and introduced into the reactor to heat the material.

[0024] The term “depolymerization” as used in the specification and / or claims, means partial depolymerization of the original polymer to a product having a weight average molecular weight (Mw) of 1,000 Da to 20,000 Da as measured by gel permeation chromatography. As used herein, “depolymerization” does not include complete depolymerization such as in the production of pyrolysis oil or in the production of significant quantities of product having a weight average molecular weight of less than 1,000 Da.

[0025] The terms “about” or “approximately” are defined as being close to as understood by one of ordinary skill in the art. In one non-limiting embodiment, the terms are defined to be within 10%, preferably within 5%, more preferably within 1%, and most preferably within 0.5%.

[0026] The terms “inhibiting” or “reducing” or “preventing” or “avoiding” or any variation of these terms, when used in the claims and / or the specification, includes any measurable decrease or complete inhibition to achieve a desired result.

[0027] The term “effective,” as that term is used in the specification and / or claims, means adequate to accomplish a desired, expected, or intended result.

[0028] The use of the word “a” or “an” when used in conjunction with any of the terms “comprising,” “including,” “containing,” or “having” in the claims, or the specification, may mean “one,” but it is also consistent with the meaning of “one or more,” “at least one,” and “one or more than one.”

[0029] The words “comprising” (and any form of comprising, such as “comprise” and “comprises”), “having” (and any form of having, such as “have” and “has”), “including” (and any form of including, such as “includes” and “include”) or “containing” (and any form of containing, such as “contains” and “contain”) are inclusive or open-ended and do not exclude additional, unrecited elements or method steps.

[0030] The present methods can “comprise,” “consist essentially of,” or “consist of’ particular ingredients, components, compositions, etc. disclosed throughout the specification. With respect to the transitional phrase “consisting essentially of,” in one non-limiting aspect, a basic and novel characteristic of the present methods are their ability to convert a high-molecular-weight polymeric feed stream (e.g., a plastic waste stream) to usable lower-molecular weight depolymerized polymer product streams (e.g., depolymerized plastic waste stream).

[0031] Other objects, features, and advantages of the present invention will become apparent from the following figures, detailed description, and examples. It should be understood, however, that the figures, detailed description, and examples, while indicating specific embodiments of the invention, are given by way of illustration only and are not meant to be limiting. Additionally, it is contemplated that changes and modifications within the spirit and scope of the invention will become apparent to those skilled in the art from this detailed description. In further embodiments, features from specific embodiments may be combined with features from other embodiments. For example, features from one embodiment may be combined with features from any of the other embodiments. In further embodiments, additional features may be added to the specific embodiments described herein.BRIEF DESCRIPTION OF THE DRAWINGS

[0032] Advantages of the present invention may become apparent to those skilled in the art with the benefit of the following detailed description and upon reference to the accompanying drawings.

[0033] FIG. 1 is a cross-sectional, schematic side view of one of the present reactors having a vessel, a Joule heating element disposed within the vessel comprising electrically-resistive elements, and electrical conductors coupled to the electrically-resistive elements.

[0034] FIG. 2 is a cross-sectional side view of an example of a reactor of the present invention, which can include the Joule heating element of a bundle of wires.

[0035] FIG. 3 is a schematic view of the bundle of wires of FIG. 2 outside of the reactor.

[0036] FIG. 4A is a schematic view of a first non-linear configuration of a wire that can be included in the bundle of wires of FIG. 3.

[0037] FIG. 4B is a schematic view of a second non-linear configuration of a wire that can be included in the bundle of wires of FIG. 3.

[0038] FIG. 5A is a cross-sectional, schematic side view of a comparative reactor including a Joule heating element having electrically-resistive elements including a stack of sheets showing a side view of the sheets.

[0039] FIG. 5B is a cross-sectional, schematic front view of the comparative reactor of FIG. 5 A, taken along plane 5B-5B of FIG. 5 A showing the end view of the comparative sheets.

[0040] FIG. 6 is a schematic front view of a comparative corrugated stack of sheets as the Joule heating element for use in a comparative reactor.

[0041] FIG. 7 is a schematic view of a system for the conversion of a high-molecular-weight polymeric feed stream to usable lower-molecular-weight depolymerized polymer product streams, where that system includes the reactor of the present invention having electrically-resistive elements a pretreatment unit.

[0042] FIG. 8 is a schematic view of a system for the conversion of a high-molecular-weight polymeric feed stream to usable lower-molecular weight depolymerized polymer product streams, where that system includes one of the reactors of the present invention having electrically-resi stive elements, a pretreatment unit, and a purification system.

[0043] While the invention is susceptible to various modifications and alternative forms, specific embodiments thereof are shown by way of example in the drawings.DETAILED DESCRIPTION

[0044] A solution to at least one of the problems associated with heating feed streams in a cost- effective manner has been discovered. Notably, embodiments of the invention provide a metal packing made of electrically-resistive heating elements (a bundle of conductive wires) that provide channels that can be heated resistively using a commercial A / C power supply and that can be used up to temperatures of 1,450 °C. The temperature of the heating elements can be controlled by the current passing through them, and mass and heat transfer can be enhanced by providing a high surface area for contact of the feed stream with the heating elements. At the same time, the present packings are suitable for use even with high-molecular-weight feed streams (e.g., polymeric plastic waste) that might otherwise exclude traditional packings. And because the heat is supplied electrically, there is a positive effect on greenhouse gas emissions (particularly if the electricity is generated by wind or solar).

[0045] Ranges are provided for the various parameters discussed herein, along with specific discrete values within the ranges. It should be understood that the values are not limited to the specific discrete values recited and may be any other values within the ranges.

[0046] These and other non-limiting aspects of the present invention are discussed in further detail in the following sections.A. Vessel with a Joule Heating Element

[0047] Referring now to the drawings, FIG. 1 depicts a first embodiment of the present reactors for heating high-molecular-weight feed streams for conversion to usable lower-molecular-weight liquid and gas feed streams. As shown in FIG. 1, reactor 100 can include a vessel 14 and a Jouleheating element 18 disposed within the vessel 14. Vessel 14 can be formed of a metal, e.g., a steel and / or a steel alloy, and the metal may be resistant to high temperatures to facilitate reactions at temperatures required for conversion of high-molecular-weight feed streams to lower-molecular- weight liquid and gas feed streams (e.g., 350-500 °C). Although not shown in FIG. 1, the reactor 100 can include a second, third, fourth, fifth, sixth, seventh, eighth, ninth, or tenth, or more Joule heating elements 18 disposed within the vessel 14. The additional heating elements 18 can be positioned in parallel and / or in series relative to one another. When positioned in series relative to one another, the high-molecular- weight feed stream can be subjected to a first Joule heating elements 18 and then subsequently subjected to a second Joule heating element 18.

[0048] An interior surface of vessel 14 that surrounds Joule heating element 18 can be electrically-insulative. Alternatively, an electrically-insulative layer can be disposed within vessel 14 and around heating element 18. Suitable electrically-insulative materials that may be included in the electrically-insulative interior surface of vessel 14 and / or the electrically-insulative layer disposed within the vessel include, but are not limited to, inorganic solid materials (e.g., alumina (AI2O3) and / or silica (SiC>2)).

[0049] Primary reactants such as waste feed streams (e.g., plastic waste, high-boiling-point petrochemical streams), and / or other reagents may be fed into vessel 14 through one or more inlets 22 in fluid communication with vessel 14. Once inside vessel 14 of reactor 100, chemical reactions (e.g., depolymerization reactions) can be initiated by heat generated by heating element 18. Reaction products can be recovered from vessel 14 of reactor 100 by outlet 26.

[0050] Joule heating element 18 can include electrically-resistive elements 30 (a bundle of wires) that extend from a first end 34 of heating element 18 to a second end 38 of heating element 18, and an electrical power source 42 can be configured to pass a current through the electrically- resistive elements to generate heat. For example, as shown in FIG. 3, electrically-resistive elements 30, shown as non-linear wires, can be coupled to a first electrical conductor 46 at first end 34 of heating element 18 and a second electrical conductor 50 at second end 38 of heating element 18. First electrical conductor 46 and second electrical conductor 50 can be coupled to electrical power source 42, and the electrical power source can pass a current through the first electrical conductor, the second electrical conductor, and the electrically-resistive elements.

[0051] Reactor 100 has a void volume 54 through which liquid or molten compositions are permitted to flow through vessel 14 and between first end 34 of heating element 18 and second end 38 of the heating element. Void volume 54 can be defined at least by electrically-resistive elements 30 and vessel 14. To illustrate, vessel 14 can have an interior volume that is occupied by electrically-resistive elements 30, and the void volume can be the interior volume of vessel minus the volume of the electrically-resistive elements. Of course, other structure(s) can occupy other portion(s) of the interior volume of vessel 14 such that liquid is not permitted to flow through those other portion(s), and in such instances, the void volume can be the interior volume of the vessel minus the volume of electrically-resistive elements 30 and minus the volume of the other structure(s). Electrically-resistive elements 30 have a surface area. In some aspects, a ratio of surface area to a void volume 54 of electrically-resistive elements 30 can be greater than or equal to any one of, or between any two of: 0.10, 0.20, 0.30, 0.40, 0.50, 0.60, 0.70, 0.80, 0.90, 1.0, 1.1, 1.2, 1.3, 1.4, 1.5, 1.6, 1.7, 1.8, 1.9, 2.0, 2.1, 2.2, 2.3, 2.4, 2.5, 2.6, 2.7, 2.8, 2.9, or 3.0 mm2 / mm3. In reactors for processing relatively viscous feed streams, such as those having a low or zero-shear viscosity between 200,000 cP and 500,000 cP at 150 °C to 300 °C, this ratio can be on the higher end of this range, e.g., at least 1.3 mm2 / mm3, to facilitate the flow of such feed streams through the vessel and past the heating element.

[0052] In some aspects, a ratio of surface area to a void volume 54 of electrically-resistive elements 30 that is greater than 1.3 mm2 / mm3can enhance mass and heat transfer in reactor 100, which can allow the reactor to have a smaller size and can therefore reduce costs, particularly for high-molecular-weight feed streams that might otherwise occlude the reactor. Enhanced mass and heat transfer in reactor 100 can also improve use of the reactor for conversion of viscous, high- molecular-weight polymers to lower molecular weight oligomers and lighter liquids through process intensification.

[0053] Electrically-resistive elements 30 can include iron (Fe), chromium (Cr), aluminum (Al), yttrium (Y), a combination thereof, or an alloy thereof. In some aspects, electrically-resistive elements 30 include NiCr, NiCu, NiCrFe, MnNiCu, CrAlSiCFe, NiCoMnSiFe, NiAlTi, SiC, MoSri, or FeCrAl alloys. In some aspects, electrically-resistive elements 30 include an FeCrAl alloy. FeCrAl alloys can provide robust heating due to the resistivity of the alloy. Additionally, FeCrAl alloys have favorable lifetime and performance properties. In some aspects, FeCrAl alloys are capable of operating at relatively high temperature (e.g., up to 1300 °C) and have a good surfaceload (e.g., about 50 kW / m2). In some aspects, electrically-resistive elements 30 include a nickel / chromium alloy. Nickel-chromium alloys are used in many industrial furnaces and electric household appliances. The material is robust and repairable (e.g., weldable) and is available at medium costs and in various grades. Additional materials may be used to construct electrically- resistive elements 30 for heating elements (e.g., 18) of the present reactors (e.g., 100) based on the needs and parameters of the specific embodiment.

[0054] Electrically-resistive elements 30 have a resistivity at about 20 °C (e.g., at or between any two of: 18, 19, 20, 21, or 22 °C) that is at least 1 pQ m (e.g., 1, 2, 3, 4, 5, or more pQ m). In some aspects, electrically-resistive elements 30 are not coated with a catalyst and / or an insulating material.

[0055] Referring additionally to FIGs. 2 and 3, embodiments of depolymerization reactor 200 useful in the method described herein are shown. As shown in FIGs. 2 and 3 the electrically- resistive elements are non-linear wires. FIG. 3 shows the assembly of the bundle of wires 58 outside of the reactor, while FIG. 2 shows the bundle of wires inside of reactor 200. Each of the wires in bundle of wires 58 of electrically-resistive elements 30 can have different appearances and forms, e.g., round wires or flat wires. Notably, the bundle of wires 58 can be assembled outside of the reactor and provided to the reactor. This provides an advantage of being able to customize the bundle of wires for different reactor configurations (e.g., lengths and / or shapes). Although the wires shown in FIGs. 2 and 3 are non-linear (e.g., twisted, or crimped), in other embodiments the wires can be linear. In specific aspects, each of the wires of the bundle of wires 58 is crimped along a length of the wire. The person of ordinary skill in the art will readily understand that the crimp profile of the wires is not particularly limited and may be, e.g., pyramidal, hexagonal, trapezoidal, square, oval, indent, etc., or a combination thereof. For example, as shown in FIG. 4A, in some aspects, each of the wires of bundle of wires 58 is pyramidally crimped along a length of the wire. As shown in FIG. 4B, in other aspects, each of the wires of bundle of wires 58 is hexagonally crimped along a length of the wire.

[0056] In some aspects, each of the wires of bundle of wires 58 of electrically-resistive elements 30 may have a length of at least, at most, exactly, or between any two of: 0.1, 0.2, 0.3, 0.4, 0.5, 0.6, 0.7, 0.8, 0.9, 1, 1.1, 1.2, 1.3, 1.4, 1.5, 1.6, 1.7, 1.8, 1.9, 2, 2.1, 2.2, 2.3, 2.4, 2.5, 2.6, 2.7, 2.8, 2.9, 3, 3.1, 3.2, 3.3, 3.4, 3.5, 3.6, 3.7, 3.8, 3.9, 4, 4.1, 4.2, 4.3, 4.4, 4.5, 4.6, 4.7, 4.8, 4.9,5, 5.1, 5.2, 5.3, 5.4, 5.5, 5.6, 5.7, 5.8, 5.9, 6, 6.1, 6.2, 6.3, 6.4, 6.5, 6.6, 6.7, 6.8, 6.9, 7, 7.1, 7.2, 7.3,7.4, 7.5, 7.6, 7.7, 7.8, 7.9, 8, 8.1, 8.2, 8.3, 8.4, 8.5, 8.6, 8.7, 8.8, 8.9, 9, 9.1, 9.2, 9.3, 9.4, 9.5, 9.6, 9.7, 9.8, 9.9, or 10 m. Additionally, each of the wires of bundle of wires 58 of electrically-resistive elements 30 may have a diameter of at least, at most, exactly, or between any two of: 0.2, 0.225, 0.25, 0.275, 0.3, 0.325, 0.35, 0.375, 0.4, 0.425, 0.45, 0.475, 0.5, 0.525, 0.55, 0.575, 0.6, 0.625, 0.65, 0.675, 0.7, 0.725, 0.75, 0.775, 0.8, 0.825, 0.85, 0.875, 0.9, 0.925, 0.95, 0.975, 1, 5, 1.5, 1.75, 2, 2.25, 2.5, 2.75, 3, 3.25, 3.5, 3.75, 4, 4.25, 4.5, 4.75, 5, 5.25, 5.5, 5.75, 6, 6.25, 6.5, 6.75, 7, 7.25,7.5, 7.75, or 8 mm. In specific aspects, each of the wires of bundle of wires 58 of electrically- resistive elements 30 has a diameter that is between 0.20 and 1.30 mm.

[0057] Each wire in bundle of wires 58 of electrically-resistive elements 30 can extend between first end 34 of heating element 18 and second end 38 of heating element 18. Each wire in bundle of wires 58 of electrically-resistive elements 30 can extend between first electrical conductor 46 and second electrical conductor 50. Additionally, each wire in bundle of wires 58 of electrically-resistive elements 30 can be in electrical communication with first electrical conductor 46 and second electrical conductor 50. The wires may be configured as a single electrical circuit across all wires; alternatively, the wires may be configured such that one or more wires operate as a standalone circuit. The wires may be bundled as a single layer of parallel wires or as multiple layers of parallel wires. In some aspects, the wires of bundle of wires 58 of electrically-resistive elements 30 are not interwoven. In some aspects, the wires of bundle of wires 58 of electrically- resistive elements 30 are not bonded to one another. These aspects can enhance the ability of wires 58 to permit flow (e.g., viscous, high-molecular-weight polymer flow) therethrough. As high- molecular-weight polymer flows through wires 58, the viscosity of the high-molecular-weight polymer can decrease along a gradient from about 100,000 cP or greater at first end 34 of heating element 18 to about 1,000 cP or less at second end 38 of heating element 18.

[0058] FIGs. 5A, 5B, and 6 illustrates comparative examples of a Joule heating element outside of the scope of that used in the present invention. These examples illustrate the use of electrically-resistive elements 30 in reactor 300, which comprise a monolith in the form of a stack of sheets 62. Each of the sheets in stack of sheets 62 of electrically-resistive elements 30 can have different appearances and forms, e.g., flat, smooth, corrugated, pleated, creased, etc. In specific aspects, at least some of the sheets of electrically-resistive elements 30 are flat. In specific aspects, at least some of the sheets of electrically-resistive elements 30 are corrugated, for example, asshown in FIG. 6. Devices of this kind in FIGs. 5A, 5B, and 6 have found particular use in gas phase reactions where that resistance to flow of a viscous feed stream is not expected to pose problems. With feed streams of significant viscosity, such as molten polymers such as molten plastic waste, the flow of a viscous stream through wire bundles rather than rigid structures such as sheets and other monoliths is problematic as further discussed herein.

[0059] Joule heating element reactors having resistive heating elements in the form of 3D monoliths comprising either corrugated sheets structures or foams are known in the prior art, examples of which are provided in the discussion above under Background Art. However, these reactors have numerous significant disadvantages (in terms of both cost and performance) in comparison to the Joule heating element reactors having electrically-resistive elements in the form of wires, particularly in the context of use in a thermally -based polymer depolymerization reactor.

[0060] Wires are sold on spools and can be used to form very long bundles for large reactors. For example, crimping of the wire can be easily carried out by passing the wires through a set of gears at > 1 m / sec resulting in a large production rate of non-linear wires. Bundles of wires are easily welded to form electrodes that can be connected to power sources. Overall, the cost of wire bundles is considerably less than the alternatives. In addition, flow of viscous polymers through the wire bundles shows a lower pressure drop because the wires are not in a rigid structure and depending on the conformation and configuration, may yield mechanically, as needed to accommodate flow, particularly flow of viscous fluids.

[0061] In comparison, corrugated sheet structures are formed from sheets of the resistive elements by alternating flat sheets with crimped sheets as shown in FIG 6. Unfortunately sheets of these resistive elements are not available in the very large sizes required for commercial operation, meaning that smaller sections would have to be welded together to achieve the desired length. This has two disadvantages: (1) flow of current through the welds is non-uniform resulting in hot spots and (2) it costs more to create the welded reactor inserts. Resistance to flow along the sheets is higher when using a viscous feed resulting a larger pressure drop and the potential for plugging is also higher. The same applies to resistive element monoliths and / or foams which are typically more expensive than corrugated sheet structures. Monoliths and / or foams made as smaller pieces would also need to be welded together to achieve a commercial size and would have similar current mal-distribution as the sheets. It is expected that pressure drop of a viscous liquid throughmonoliths and / or foams would also be high as would be the potential for plugging. In addition, there is the potential for “dead zones” (zones of no or low flow) in monoliths and / or foams resulting in an increase in residence time for some molecules and overreaction.

[0062] These disadvantages of Joule heating element reactors having electrically-resistive elements in the form of rigid sheets, monoliths or foams, or combinations thereof may be less important in the context of other reactors such as those involving gas phase reactions, but the disadvantages discussed above are significant in the context of use in a thermally-based polymer depolymerization reactor.B. Systems and Methods for Heating Feed Streams

[0063] Certain aspects are directed to systems and methods for heating feed streams, preferably high-molecular weight streams. Referring to FIG. 7, a system and method of using a reactor of the present invention are described. System 400 can include any reactor comprising the Joule heating element of the present invention (e.g., bundle of wires shown in FIGs. 1, 2, 3, 4 A, and 4B). As shown in FIG. 7, reactor 100 is shown. Feed stream 72 can enter vessel 14 of reactor 100. Feed stream 72 can be a polymeric composition that includes plastic waste. Non-limiting examples of plastic waste include consumer products (e.g., plastic waste). Non-limiting examples of consumer goods can include a packaging product, a pharmaceutical container, a bottle, a cap, a closure, a liner, a trash bag, a food packaging film, a lamination, a pipe, a hose, a fitting, or a combination thereof. In some aspects, the polymeric composition can contain a blend of polymers of varying molecular weight. The polymeric composition can include monomers, processing aids, and / or additives (e.g., plasticizers, impact modifiers, lubricants, fillers, extenders, antioxidants, stabilizers, rheology modifiers, tackifiers, etc.) In some instances, feed stream 72 can include plastic waste or be a mixture of plastic waste and one or more diluents that are stable to reaction conditions. In some embodiments, feed stream 72 is plastic waste containing predominately polyolefins. In some aspects, feed stream 72 consists essentially of a polyolefin plastic waste composition. Feed stream 72 can enter inlet 22 at a temperature approximate the melting point of the polymeric composition. For example, feed stream 72 can be at a temperature of 150 °C to 300 °C (for example, at least, at most, exactly, or between any two of 150, 155, 160, 165, 170, 175, 180, 185, 190, 195, 200, 205, 210, 215, 220, 225, 230, 235, 240, 245, 250, 255, 260, 275, 280, 285, 290, 295, 300 °C) when entering inlet 22. Feed stream 72 can have a zero-shear viscosityof greater than 100,000 cP at 150 °C to 300 °C, or a low shear or zero shear viscosity at least, at most, exactly, or between any two of 100,000 cP, 150,000 cP, 200,000 cP, 250,000 cP, 300,000 cP, 350,000 cP, 400,000 cP, 450,000 cP, 500,000, cP, 550,000 cP, 600,000 cP, 650,000 cP, 700,000 cP, 750,000 cP, 800,000 cP, 850,000 cP, 900,000 cP, 950,000 cP and 1,000,000 cP at 150 °C to 300 °C. Feed stream 72 can have a weight average molecular weight at least, at most, exactly, or between any two of 30,000 Da, 50,000 Da, 75,000 Da, 100,000 Da, 125,000 Da, 150,000 Da, 175,000 Da, 200,000 Da, 225,000 Da to 250,000 Da. In some aspects, feed stream 72 can have a low shear or zero shear viscosity of 100,000 Cp to 1,000,000 cP at 150 °C to 300 °C and a weight average molecular weight of 30,000 Da to 250,000 Da.

[0064] As polymeric feed stream 72 flows (shown by arrows) through void volumes 54, it can contact Joule heating system 18 and be heated. For example, activating electrical power source 42 can pass a current through electrically resistive elements 30 of the present invention (See, FIGS. 1-6) to generate heat. As the polymeric feed stream 72 flows through void volumes 54 and contacts electrically resistive elements 30, the generated heat can be transferred, preferably directly transferred, from the electrically resistive elements to the polymeric feed stream to vis- break / depolymerize the polymers in the polymeric feed stream and produce product stream 74, which includes the vis-broken / depolymerized polymer compositions. The feed stream is not heated via indirect heating or heat generated outside the vessel and provided to the polymeric feed stream. For example, the feed stream is not heated through heat exchange with a heat transfer medium. Conditions in vessel 14 can be any temperature, pressure, and residence time to perform the necessary reaction to produce heated / reaction product stream 74. Vis-breaking / depolymerization temperatures can be from 350 °C to 550 °C, or 350 °C, 375 °C, 400 °C, 425 °C, 450 °C, 575 °C, 500 °C, 525 °C, 550 °C, or any range or value there between. A pressure in vessel 14 can range from 0.1 megapascals (MPa) to 4.5 MPa, or 0.1 MPa, 0.15 MPA, 1 MPa, 1.5 MPa, 2 MPa, 2.5 MPa, 3 MPa, 3.5 MPa, 4.0 MPa, 4.5 MPa, 5.0 MPa, 5.5 MPa, 6.0 MPa, 6.5 MPa, 7 MPa, or any range or value there between. A residence time in vessel 14 can be 10 minutes to 60 minutes, or 10, 15, 20, 25, 30, 35, 40, 45, 50, 55, 60 minutes, or any range or value there between. In some aspects, the depolymerization / vis-breaking can be performed in an inert atmosphere. At these conditions, the polymer depolymerizes and forms a vis-broken polymer having a lower viscosity than the polymeric feed stream 72 entering vessel 14. The product stream 74 containing vis- broken / depolymerized polymers can have a kinematic viscosity of less than 1,000 cP, or less than500 cP, or less than 100 cP, or 1,000 cP to 50 cP, or less than 1000, cP, 500 cP, 250 cP, 100 cP, or any value or range there between. The product stream 74 containing vis-broken / depolymerized polymers have a weight average Mw of 1,000 Da to 20,000 Da, or 1,000 Da, 2,000 Da, 3,000 Da, 4,000 Da, 5,000 Da, 6,000 Da, 7,000 Da, 8,000 Da, 9,000 Da, 10,000 Da, 11,000 Da, 12,000 Da, 13,000 Da, 14,000 Da, 15,000 Da or any value or range there between. In some aspects, product stream 74 has a kinematic viscosity of 50 cP to 1000, cP and a weight average Mw of 1,000 Da to 20,000 Da.

[0065] Product stream 74 (e.g., depolymerized / vis-broken polymer product stream) can exit vessel 14 via outlet 26 and be sold, transported, or further processed. For example, product stream 74 can be provided to a FCC unit to be further processed into hydrocarbon materials (e.g., ethylene, propylene, diesel, gasoline, aromatics, and the like).

[0066] Referring to FIG. 8, System 500 can include pretreatment unit 76 and purification unit 78 coupled to reactor 100. In some embodiments, System 500 only includes pretreatment unit 76. In other embodiments, System 500 only includes separation / purification unit 78. Pretreatment unit 76 can be positioned upstream of reactor 100 and be used to pretreat feed stream 72 prior to entering reactor 100. Pretreatment unit 76 can be an extruder, stirred tank, and / or a combination thereof capable of heating a solid, semi-solid, or viscous polymeric composition 80 to produce a stream (e.g., feed stream 72) having sufficient viscosity so that it can be moved using mechanical means (e.g., pumped) to reactor 100. Polymeric composition 80 can be a solid or a viscous liquid. In preferred aspects, polymeric composition 80 is solid plastic waste (e.g., waste consumer products). In some aspects, polymeric composition 80 can be cleaned of contaminants and shredded into smaller pieces prior to being fed to pretreatment unit 76. Polymeric composition 80 can include polymers and other materials such as monomers, processing aids, and / or additives (e.g., plasticizers, impact modifiers, lubricants, fillers, extenders, antioxidants, stabilizers, rheology modifiers, tackifiers, etc.). In pretreatment unit 76, polymeric composition 80 can be heated to 120 °C to 300 °C (e.g., at least, at most, exactly, or between any two of 120, 125, 130, 135, 140, 145, 150, 155, 160, 165, 170, 175, 180, 185, 190, 195, 200, 205, 210, 215, 220, 225, 230, 235, 240, 245, 250, 255, 260, 265, 270, 275, 280, 285, 290, 295, 300 °C) to produce flowable polymeric feed stream 72. Neither polymeric stream 80 nor feed stream 72 have been depolymerized. In some embodiments, a diluent can be added to polymeric feed stream 80 or feed stream 72 to aid in the flow properties of the feed stream. For example, diluent can be added awaste plastic stream to lower the viscosity of the stream for processing purpose. Feed stream 72 can exit pretreatment unit 76 and enter one of the present reactors 100, 200, or 300 and be processed as previously described in FIG. 7 to produce product stream 74.

[0067] In some aspects, a portion or all of product stream 74 (e.g., depolymerized / vis-broken polymer stream) exits vessel 14 via outlet 26 and enter separation / purification unit 78. Separation / purification unit 78 can separate various components from product stream 74 (e.g., lighter boiling or lower viscosity compounds can be separated from higher boiling or higher viscosity compounds) to produce purified stream 82. Examples of separation techniques can include distillation, filtration, centrifugation, precipitation, solid / liquid separation, or other known separation techniques. In some embodiments, a diluent can be added to product stream 74 to aid in separation of desired components from the stream. For example, diluent can be an added a visbroken polymer stream to lower the viscosity of the stream for processing purposes. Diluents can include hydrocarbons, alcohols, esters, acetates, and the like. Hydrocarbons can include vacuum gas oil. Purified stream 82 can exit separation unit 78 and be sold, transported, or further processed. For example, purified product stream 82 can be provided to a FCC unit to be further processed into hydrocarbon materials (e.g., ethylene, propylene, diesel, gasoline, aromatics, and the like).

[0068] In some embodiments, the above-described method can be used to heat and / or react non-polymeric viscous streams.

[0069] Although embodiments of the present application and their advantages have been described in detail, it should be understood that various changes, substitutions, and alterations can be made herein without departing from the spirit and scope of the embodiments as defined by the appended claims. Moreover, the scope of the present application is not intended to be limited to the particular embodiments of the processes, machines, manufactures, compositions of matter, means, methods, and steps described in the specification. As one of ordinary skill in the art will readily appreciate from the above disclosure, processes, machines, manufactures, compositions of matter, means, methods, or steps that perform substantially the same function or achieve substantially the same result as the corresponding embodiments described herein can be utilized. Accordingly, the appended claims are intended to include within their scope such processes, machines, manufactures, compositions of matter, means, methods, or steps.EXAMPLES

[0070] The present invention will be described in greater detail by way of specific examples. The following examples are offered for illustrative purposes only and are not intended to limit the invention in any manner. Those of skill in the art will readily recognize a variety of noncritical parameters, which can be changed or modified to yield essentially the same results.Example 1 (simulated data)

[0071] A simulated process for depolymerizing a polymeric feed stream with a Joule heating element of the present invention was modelled based on Heat Transfer Research, Inc. (HTRI) software. The HTRI software was Xchanger Suite® version 9.2 The parameters in the following Table 1 were used in this simulation:Table 1

[0072] For the simulation, a unit that included a Joule heating element of the present invention was disposed inside a vessel (shell), and the polymeric stream was passed through the vessel while heat was transferred from the electrically-resistive elements to the polymeric stream. The Joule heating element used in the simulations were resistive wires surrounded by insulating material, which were enclosed by a metal sheath. The so-formed element was bendable and shapable within certain limits.

[0073] As a first step, the unit was modelled as an electric heater with no baffles (shell type “E”), meaning that the shell side stream (modelled as LDPE melt) flowed parallel to the heating elements. The selected dimensions of the shell were 20” (500 mm) nominal diameter and 16 mlength. The heating element had an outside diameter of 1 ” (12.7 mm) and was disposed in a triangular layout fashion with a pitch (e.g., center-to-center distance) of 1” (25.4 mm). A total of 291 heating elements were able to be hosted within the given shell diameter. The resulting heat transfer surface area, based on the outside diameter of the elements, was about 186 m2. The duty that was necessary to heat the LDPE melt from 200 °C to 400 °C, at a flow rate of 6000 kg / h, was 833.8 kW. This meant that the heat flux of the heating elements was around 4.5 kW / m2. The ratio between the surface area and the volume was 0.08 mm2 / mm3.

[0074] Under these conditions, the calculated “can” velocity (i.e., the one based on the internal cross-sectional area minus the cumulative cross-sectional area of the heating elements) was 0.0147 m / s. The residence time was 18 minutes. The HTRI software predicted an average shell side heat transfer coefficient of 103 W / m2-K and a total pressure drop of around 4 bar. The maximum calculated sheath temperature is 439 °C.

[0075] As a second step, the polymeric stream was modeled flowing in a cross-flow with respect to the heating elements. The module included an electric heater with shell type “X”, having a nominal size of 20” and a length equal to the diameter, e.g., 500 mm. This simulated the flow of the melt through the vessel having 19 heating elements along the horizontal axis disposed vertically, i.e., perpendicular to the axis of the vessel.

[0076] Three zones were considered: 1) one at the inlet of the melt into the vessel (local temperature: 200 °C), 2) one at midpoint through the vessel (local temperature: 300 °C), and 3) one at the outlet of the melt from the vessel (local temperature: 400 °C). In all the three cases a portion of the vessel having a length of 1 m was simulated; this meant that two of the abovedescribed modules (each having a length of 0.5 m) were considered at each location. In order to have the same heat flux under point 3 (4.5 kW / m2), the temperature increase within each zone was set to be 13 °C. Under these conditions, considering that the effective heat transfer surface area of each zone is 11.670 m2, the duty was 54.2 kW.

[0077] At a bulk temperature of 200 °C (melt inlet) the viscosity was 1,500,000 cP. Conversely, at a bulk temperature of 400 °C (melt outlet) the viscosity was 7,500 cP. Using the HTRI software, it was determined that an average shell side heat transfer coefficient was lower at the melt inlet (around 27 W / m2-K), higher at the melt outlet (around 176 W / m2-K), and the midpoint regionwas at an intermediate average value of around 82 W / m2-K. Modeling the flow of the melt perpendicular to the elements as shell type “X” was an approximation.

[0078] As stated above, the duty within each zone was 54.2 kW. The surface of the heating elements therefore reached a temperature that, depending on the local heat transfer coefficient, allowed to exchange the set duty in view of the local bulk temperature of the melt. In the inlet region, the maximum sheath temperature was 421 °C, in the midpoint region the maximum sheath temperature was 374 °C, and in the outlet region the maximum sheath temperature was 426 °C. As the heat transfer coefficient increased, and as the melt temperature increased, it was determined that the maximum sheath temperature did not overshoot. A sensitivity analysis performed in the hot (exit) zone showed that the heat transfer coefficient was as low as about 93 W / m2-K before the sheath temperature exceeded 450 °C.

[0079] The configuration described above was used to approximate the performance of heating elements having bends or serrations (similar to those described in FIG. 4A and FIG. 4B) such that the sheath was substantially perpendicular to the flow direction. Thus, it was assumed that the heat transfer coefficients and the maximum sheath temperatures were similar to those reported above. The maximum sheath temperatures were lower than the one reported above for the longitudinal flow configuration. If portions of the heating elements were disposed perpendicular the flow, it was reasonable to expect that the pressure drop would increase with respect to the value of 4 bar that was calculated for the longitudinal flow configuration. The HTRI software did not produce useful results for pressure drops in cross flow conditions.

[0080] Based on the simulated data, it was determined that the structure of heating elements of the present invention promoted an effective mixing with no dead zones present. Thus, the advantage of the sheath metal temperature exceeding the prescribed limits was avoided.

Claims

CLAIMS1. A method of depolymerizing a polymer, the method comprising: passing a polymeric feed stream through a vessel of a reactor, the reactor having a Joule heating element disposed within the vessel, wherein: the Joule heating element has electrically-resistive elements extending from a first end of the heating element to a second end of the heating element; and at least the electrically-resistive elements and the vessel cooperate to define a void volume, wherein the electrically-resistive elements are wires; flowing the polymeric feed stream through the void volume of the vessel between the first end of the Joule heating element and the second end of the Joule heating element; and heating the polymeric feed stream by passing an electric current through the electrically- resistive elements such that heat is directly transferred from the electrically-resistive elements to the polymeric feed stream to produce a product stream comprising depolymerized polymers.

2. The method of claim 1, wherein the wires comprise non-linear wires.

3. The method of any one of claims 1 to 2, wherein the wires have a ratio of the surface area to the void volume of greater than 1.3 square millimeter per cubic millimeter (mm2 / mm3).

4. The method of any one of claims 1 to 3, wherein the wires are not coated with a catalyst.

5. The method of any one of claims 1 to 4, wherein each of the wires has a resistivity at 20°C that is greater than about 1 pQ*m.

6. The method of any one of claims 1 to 5, wherein the wires are not interwoven or bonded to one another.

7. The method of any one of claims 1 to 6, wherein each of the wires comprises iron (Fe), chromium (Cr), aluminum (Al), yttrium (Y), or a combination thereof, or an alloy thereof, preferably an FeCrAl alloy or a nickel / chromium alloy.

8. The method of any one of claims 1 to 7, wherein each of the wires has a diameter that is between 0.10 and 1.30 millimeters (mm).

9. The method of any one of one of claims 1 to 8, wherein the wires are electrically-insulated from the vessel, optionally, by an electrically-insulative layer of the vessel that surrounds the wires.

10. The method of any one of claims 1 to 9, wherein the product stream has a kinematic viscosity of less than 1,000 cP, preferably less than 100 cP, a weight average molecular weight (Mw) of 1,000 Da to 20,000 Da, or a combination thereof.

11. The method of any of claims 1 to 10, wherein the polymeric feed stream is heated to a temperature of 375 °C to 500 °C over a residence time of 10 minutes to 60 minutes and / or wherein the polymeric feed stream has a temperature of 150 °C to 300 °C at the inlet of the reactor.

12. The method of any one of claims 1 to 11, wherein the polymeric feed stream has a zeroshear viscosity of 100,000 cP to 1,000,000 cP at 150 °C to 300 °C, a weight average molecular weight of 30,000 Da to 250,000 Da, or a combination thereof.

13. The method of any one of claims 1 to 12, wherein the polymeric feed stream further comprises one or more solvents, the product stream comprises one or more solvents, or a combination thereof.

14. The method of any one of claims 1 to 13, wherein the polymeric feed stream is plastic waste comprising polyolefins.

15. The method of any one of claims 1 to 14, wherein the reactor comprises a second Joule heating element disposed in the vessel, and optionally wherein the Joule heating element and the second Joule heating element are positioned in series with one another such that the polymeric feed stream first contacts the Joule heating element and then contacts the second Joule heating element.

Citation Information

Patent Citations

  • Grade-dependent depolymerization process and its use for recycling plastics

    EP4155341A1

  • Processes and systems for the conversion of acyclic hydrocarbons to cyclopentadiene

    US11261140B2

  • Nanoparticles and systems and methods for synthesizing nanoparticles through thermal shock

    US20180369771A1

  • Tunable molten oxide pool assisted plasma-melter vitrification systems

    US6160238A

  • Method of making micro channel heat pipe having corrugated fin elements

    US6216343B1