Etching method and plasma processing apparatus

The etching method and plasma processing apparatus address the issue of etching uniformity and shape abnormalities by using a protective layer and controlled power supply to achieve consistent etching depths across different trench sizes, effectively mitigating microloading effects and bowing.

WO2024203479A1PCT designated stage expired Publication Date: 2024-10-03TOKYO ELECTRON LTD
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
PCT/JP2024/010318
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-03-27
Filing Date
2024-03-15
Publication Date
2024-10-03

AI Technical Summary

Technical Problem

Existing etching methods face challenges in maintaining uniformity and preventing shape abnormalities, such as bowing and variations in etching depth, particularly when etching trenches of different sizes, due to microloading effects.

Method used

An etching method and plasma processing apparatus that form a recess in a substrate using a first plasma, followed by forming a protective layer on the sidewalls and etching the bottom using a second plasma, with non-overlapping periods of high-frequency power and bias power supply to control the etching process.

Benefits of technology

This approach effectively suppresses bowing and etching variations across different opening sizes, ensuring high aspect ratio etching with minimal microloading effects, achieving consistent etching depths across varying trench sizes.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure JP2024010318_03102024_PF_FP_ABST
    Figure JP2024010318_03102024_PF_FP_ABST
Patent Text Reader

Abstract

An etching method according to one exemplary embodiment comprises: a step for forming a recess which overlaps with an opening of a mask by etching a silicon layer; a step for forming a protective layer on at least a side wall of the recess; and a step for etching the bottom of the recess. The step for forming a protective layer comprises: a layer formation step for forming a precursor layer on at least the side wall of the recess; and a modification step for modifying the precursor layer into a protective layer. The step for etching the bottom of the recess comprises: a first step for supplying a pulse of source high-frequency power from a high-frequency power supply; and a second step for supplying a pulse of bias power from a bias power supply to a support part that supports a substrate. The period during which the first step is executed and the period during which the second step is executed do not overlap with each other.
Need to check novelty before this filing date? Find Prior Art

Description

Etching method and plasma processing apparatus

[0001] SUMMARY OF THE INVENTION Exemplary embodiments of the present disclosure relate to an etching method and a plasma processing apparatus.

[0002] U.S. Patent No. 6,277,633 relates to a method and apparatus for reducing roughness using an integrated atomic layer deposition and etching process, and discloses a technique for depositing a conformal layer on a pattern mask layer of a substrate by ALD, followed by etching a first material layer of the substrate.

[0003] Special Publication No. 2021-504974

[0004] For example, a mask placed on an etching target may have a pattern (a dense and sparse pattern) including openings of various sizes. In this case, the deeper the trench (groove) formed in the etching target, the more likely the trench depth will vary (i.e., the more likely the etching amount will vary). In addition, trenches formed through smaller openings tend to be more susceptible to shape abnormalities such as bowing. Therefore, the present disclosure provides an etching method and a plasma processing apparatus that can suppress both the occurrence of bowing and the variation in the etching amount depending on the size of the opening.

[0005] In one exemplary embodiment, an etching method includes the steps of: preparing a substrate including a mask having a sparse / dense pattern and a silicon layer located below the mask; etching the silicon layer using a first plasma generated from a first process gas to form a recess overlapping an opening in the mask; forming a protective layer on at least a side wall of the recess; and etching a bottom of the recess using a second plasma generated from a second process gas, wherein the step of forming the protective layer includes: a layer formation step of forming a precursor layer on at least the side wall of the recess; and a modification step of modifying the precursor layer into the protective layer using a third process gas, and the step of etching the bottom of the recess includes: a first step of supplying pulses of source radio frequency power from a radio frequency power source; and a second step of supplying pulses of bias power from a bias power source to a support portion supporting the substrate, wherein a period during which the first step and a period during which the second step are performed do not overlap with each other.

[0006] According to one exemplary embodiment, an etching method and a plasma processing apparatus are provided that can suppress both the occurrence of bowing and variations in the amount of etching depending on the size of the opening.

[0007] FIG. 1 is a diagram illustrating an example of the configuration of a plasma processing system according to an exemplary embodiment. FIG. 2 is a diagram illustrating an example of the configuration of an inductively coupled plasma processing apparatus according to an exemplary embodiment. FIG. 3 is a flowchart of an etching method according to an exemplary embodiment. FIG. 4 is a cross-sectional view of an example substrate to which the method of FIG. 3 can be applied. FIG. 5 is a cross-sectional view illustrating a step of the etching method according to an exemplary embodiment. FIG. 6 is a cross-sectional view illustrating a step of the etching method according to an exemplary embodiment. FIG. 7 is a cross-sectional view illustrating a step of the etching method according to an exemplary embodiment. FIG. 8 is a cross-sectional view illustrating a step of the etching method according to an exemplary embodiment. FIG. 9 is a cross-sectional view illustrating a step of the etching method according to an exemplary embodiment. FIG. 10 is a cross-sectional view illustrating a step of the etching method according to an exemplary embodiment. FIG. 11 is a cross-sectional view illustrating a step of the etching method according to an exemplary embodiment.

[0008] Various exemplary embodiments will be described in detail below with reference to the drawings, in which the same or equivalent parts are designated by the same reference numerals.

[0009] FIG. 1 is a diagram illustrating an exemplary configuration of a plasma processing system. In one embodiment, the plasma processing system includes a plasma processing apparatus 1 and a control unit 2. The plasma processing system is an example of a substrate processing system, and the plasma processing apparatus 1 is an example of a substrate processing apparatus. The plasma processing apparatus 1 includes a plasma processing chamber 10, a substrate support 11, and a plasma generation unit 12. The plasma processing chamber 10 has a plasma processing space. The plasma processing chamber 10 also has at least one gas supply port for supplying at least one processing gas to the plasma processing space and at least one gas exhaust port for exhausting gas from the plasma processing space. The gas supply port is connected to a gas supply unit 20 (described later), and the gas exhaust port is connected to an exhaust system 40 (described later). The substrate support 11 is disposed in the plasma processing space and has a substrate support surface for supporting a substrate.

[0010] The plasma generating unit 12 is configured to generate plasma from at least one processing gas supplied into the plasma processing space. The plasma generated in the plasma processing space may be capacitively coupled plasma (CCP), inductively coupled plasma (ICP), electron-cyclotron-resonance plasma (ECR plasma), helicon wave plasma (HWP), surface wave plasma (SWP), or the like. Various types of plasma generators may be used, including alternating current (AC) plasma generators and direct current (DC) plasma generators. In one embodiment, the AC signal (AC power) used in the AC plasma generator has a frequency in the range of 100 kHz to 10 GHz. Thus, AC signals include radio frequency (RF) signals and microwave signals. In one embodiment, the RF signal has a frequency in the range of 100 kHz to 150 MHz.

[0011] The control unit 2 processes computer-executable instructions that cause the plasma processing apparatus 1 to perform various processes described in this disclosure. The control unit 2 may be configured to control each element of the plasma processing apparatus 1 to perform various processes described herein. In one embodiment, part or all of the control unit 2 may be included in the plasma processing apparatus 1. The control unit 2 may include a processing unit 2a1, a storage unit 2a2, and a communication interface 2a3. The control unit 2 may be implemented by, for example, a computer 2a. The processing unit 2a1 may be configured to read a program from the storage unit 2a2 and execute the read program to perform various control operations. This program may be stored in the storage unit 2a2 in advance or may be acquired via a medium when needed. The acquired program is stored in the storage unit 2a2 and read from the storage unit 2a2 by the processing unit 2a1 for execution. The medium may be various storage media readable by the computer 2a or a communication line connected to the communication interface 2a3. The processing unit 2a1 may be a CPU (Central Processing Unit). The storage unit 2a2 may include a random access memory (RAM), a read-only memory (ROM), a hard disk drive (HDD), a solid state drive (SSD), or a combination thereof. The communication interface 2a3 may communicate with the plasma processing apparatus 1 via a communication line such as a local area network (LAN).

[0012] The following describes a configuration example of an inductively coupled plasma processing apparatus as an example of the plasma processing apparatus 1. Fig. 2 is a diagram for explaining a configuration example of an inductively coupled plasma processing apparatus.

[0013] The inductively coupled plasma processing apparatus 1 includes a plasma processing chamber 10, a gas supply unit 20, a power supply 30, and an exhaust system 40. The plasma processing chamber 10 includes a dielectric window 101. The plasma processing apparatus 1 also includes a substrate support 11, a gas inlet, and an antenna 14. The substrate support 11 is disposed within the plasma processing chamber 10. The antenna 14 is disposed on or above the plasma processing chamber 10 (i.e., on or above the dielectric window 101). The plasma processing chamber 10 has a plasma processing space 10s defined by the dielectric window 101, a sidewall 102 of the plasma processing chamber 10, and the substrate support 11. The plasma processing chamber 10 is grounded.

[0014] The substrate support 11 includes a main body 111 and a ring assembly 112. The main body 111 has a central region 111a for supporting a substrate W and an annular region 111b for supporting the ring assembly 112. A wafer is an example of a substrate W. The annular region 111b of the main body 111 surrounds the central region 111a of the main body 111 in a plan view. The substrate W is disposed on the central region 111a of the main body 111, and the ring assembly 112 is disposed on the annular region 111b of the main body 111 so as to surround the substrate W on the central region 111a of the main body 111. Therefore, the central region 111a is also called a substrate support surface for supporting the substrate W, and the annular region 111b is also called a ring support surface for supporting the ring assembly 112.

[0015] In one embodiment, the main body 111 includes a base 1110 and an electrostatic chuck 1111. The base 1110 includes a conductive member. The conductive member of the base 1110 can function as a bias electrode. The electrostatic chuck 1111 is disposed on the base 1110. The electrostatic chuck 1111 includes a ceramic member 1111a and an electrostatic electrode 1111b disposed within the ceramic member 1111a. The ceramic member 1111a has a central region 111a. In one embodiment, the ceramic member 1111a also has an annular region 111b. Note that the annular region 111b may also be provided by another member surrounding the electrostatic chuck 1111, such as an annular electrostatic chuck, an annular insulating member, or the like. In this case, the ring assembly 112 may be disposed on the annular electrostatic chuck or the annular insulating member, or may be disposed on both the electrostatic chuck 1111 and the annular insulating member. Furthermore, at least one RF / DC electrode coupled to an RF power supply 31 and / or a DC power supply 32, which will be described later, may be disposed within the ceramic member 1111a. In this case, the at least one RF / DC electrode functions as a bias electrode. Note that the conductive member of the base 1110 and the at least one RF / DC electrode may function as multiple bias electrodes. Alternatively, the electrostatic electrode 1111b may function as a bias electrode. Therefore, the substrate support 11 includes at least one bias electrode.

[0016] The ring assembly 112 includes one or more annular members. In one embodiment, the one or more annular members include one or more edge rings and at least one cover ring. The edge rings are formed of a conductive or insulating material, and the cover rings are formed of an insulating material.

[0017] The substrate support 11 may also include a temperature adjustment module configured to adjust at least one of the electrostatic chuck 1111, the ring assembly 112, and the substrate to a target temperature. The temperature adjustment module may include a heater, a heat transfer medium, a flow passage 1110a, or a combination thereof. A heat transfer fluid such as brine or a gas flows through the flow passage 1110a. In one embodiment, the flow passage 1110a is formed in the base 1110, and one or more heaters are disposed in the ceramic member 1111a of the electrostatic chuck 1111. The substrate support 11 may also include a heat transfer gas supply configured to supply a heat transfer gas to a gap between the backside of the substrate W and the central region 111a.

[0018] The gas inlet is configured to introduce at least one process gas from the gas supply unit 20 into the plasma processing space 10s. In one embodiment, the gas inlet includes a center gas injector (CGI) 13. The center gas injector 13 is disposed above the substrate support 11 and attached to a central opening formed in the dielectric window 101. The center gas injector 13 has at least one gas supply port 13a, at least one gas flow path 13b, and at least one gas inlet port 13c. The process gas supplied to the gas supply port 13a passes through the gas flow path 13b and is introduced into the plasma processing space 10s from the gas inlet port 13c. Note that the gas inlet may include one or more side gas injectors (SGIs) attached to one or more openings formed in the sidewall 102 in addition to or instead of the center gas injector 13.

[0019] The gas supply unit 20 may include at least one gas source 21 and at least one flow controller 22. In one embodiment, the gas supply unit 20 is configured to supply at least one process gas from a corresponding gas source 21 to the gas inlet through a corresponding flow controller 22. Each flow controller 22 may include, for example, a mass flow controller or a pressure-controlled flow controller. Additionally, the gas supply unit 20 may include at least one flow modulation device that modulates or pulses the flow rate of the at least one process gas.

[0020] The power supply 30 includes an RF power supply 31 coupled to the plasma processing chamber 10 via at least one impedance matching circuit. The RF power supply 31 is a high-frequency power supply configured to supply at least one RF signal (also referred to as RF power or high-frequency power) to at least one bias electrode and the antenna 14. This causes plasma to be formed from at least one processing gas supplied to the plasma processing space 10s. Therefore, the RF power supply 31 can function as at least a part of the plasma generation unit 12. Furthermore, by supplying a bias RF signal to the at least one bias electrode, a bias potential is generated on the substrate W, thereby attracting ions in the formed plasma to the substrate W.

[0021] In one embodiment, the RF power supply 31 includes a first RF generating unit 31a and a second RF generating unit 31b. The first RF generating unit 31a is a high-frequency power supply coupled to the antenna 14 via at least one impedance matching circuit and configured to generate a source RF signal (also referred to as source RF power or source high-frequency power) for plasma generation. In one embodiment, the source RF signal has a frequency within a range of 0.1 kHz to 150 MHz. In one embodiment, the first RF generating unit 31a may be configured to generate multiple source RF signals having different frequencies. The generated one or more source RF signals are supplied to the antenna 14.

[0022] The second RF generator 31b is a bias power supply coupled to at least one bias electrode via at least one impedance matching circuit and configured to generate a bias RF signal (also referred to as bias RF power). The frequency of the bias RF signal may be the same as or different from the frequency of the source RF signal. In one embodiment, the bias RF signal has a frequency lower than the frequency of the source RF signal. In one embodiment, the bias RF signal has a frequency in the range of 0.1 kHz to 60 MHz. In one embodiment, the second RF generator 31b may be configured to generate multiple bias RF signals having different frequencies. The generated one or more bias RF signals are supplied to at least one bias electrode. In various embodiments, at least one of the source RF signal and the bias RF signal may be pulsed. In this case, the first RF generator 31a supplies pulses of source RF power to the antenna 14, and the second RF generator 31b supplies pulses of bias power to the substrate support 11.

[0023] The power supply 30 may also include a DC power supply 32 coupled to the plasma processing chamber 10. The DC power supply 32 includes a bias DC generator 32a. In one embodiment, the bias DC generator 32a is connected to at least one bias electrode and configured to generate a bias DC signal. The generated bias DC signal is applied to the at least one bias electrode.

[0024] In various embodiments, the bias DC signal may be pulsed. In this case, a sequence of voltage pulses is applied to at least one bias electrode. The voltage pulses may have a rectangular, trapezoidal, triangular, or combination thereof. In one embodiment, a waveform generator for generating the sequence of voltage pulses from the DC signal is connected between the bias DC generator 32a and at least one bias electrode. Thus, the bias DC generator 32a and the waveform generator constitute a voltage pulse generator. The voltage pulses may have positive or negative polarity. Furthermore, the sequence of voltage pulses may include one or more positive voltage pulses and one or more negative voltage pulses within one cycle. Note that the bias DC generator 32a may be provided in addition to the RF power supply 31 or may be provided instead of the second RF generator 31b.

[0025] The antenna 14 includes one or more coils. In one embodiment, the antenna 14 may include an outer coil and an inner coil arranged coaxially. In this case, the RF power supply 31 and the DC power supply 32 may be connected to both the outer coil and the inner coil, or to either the outer coil or the inner coil, respectively. In the former case, the same RF generator may be connected to both the outer coil and the inner coil, or separate RF generators may be connected to the outer coil and the inner coil separately.

[0026] The exhaust system 40 may be connected to, for example, a gas exhaust port 10e provided at the bottom of the plasma processing chamber 10. The exhaust system 40 may include a pressure regulating valve and a vacuum pump. The pressure in the plasma processing space 10s is regulated by the pressure regulating valve. The vacuum pump may include a turbomolecular pump, a dry pump, or a combination thereof.

[0027] 3 is a flowchart of an etching method according to one exemplary embodiment. The etching method MT1 shown in FIG. 3 (hereinafter referred to as "method MT1") can be performed by the plasma processing apparatus 1 of the above embodiment. The method MT1 can be applied to a substrate W. Therefore, the method MT1 is at least a part of a method for processing the substrate W.

[0028] Figure 4 is a cross-sectional view of an example substrate to which the method of Figure 3 can be applied. As shown in Figure 4, in one embodiment, the substrate W has a mask M, a silicon layer F1 located below the mask M, and a base region UR located below the silicon layer F1.

[0029] The mask M has at least one opening OP. The at least one opening OP may be a hole or a slit. The at least one opening OP may be formed by development. The development may be performed by the plasma processing apparatus 1 or by a developing apparatus different from the plasma processing apparatus 1. The openings OP include a first opening OP1 and a second opening OP2. The width D1 of the first opening OP1 is smaller than the width D2 of the second opening OP2. Each of the widths D1 and D2 narrows toward the silicon layer F1, but is not limited to this. The minimum width of the width D1 is, for example, 5 nm or more and 20 nm or less. The minimum width of the width D2 is, for example, 10 nm or more and 30 nm or less. In one embodiment, the portion where the first opening OP1 is provided may be referred to as a dense pattern, and the portion where the second opening OP2 is provided may be referred to as a sparse pattern. For this reason, the mask M can also be called a mask having a sparsely and densely patterned pattern.

[0030] In one embodiment, the mask M has a first region R1 located on the silicon layer F1 and a second region R2 located on the first region R1. The first region R1 includes, for example, an oxide material. The oxide material may be a metal oxide or a silicon oxide (SiO X ) where x is a positive real number. The thickness of the first region R1 is not particularly limited, but is, for example, 30 nm or more and 100 nm or less. The first region R1 may contain nitrogen or the like. The second region R2 contains, for example, silicon. The silicon may be amorphous silicon or polysilicon. The thickness of the second region R2 is not particularly limited, but is, for example, 30 nm or more and 100 nm or less.

[0031] The silicon layer F1 is an etching target in the etching method MT1 and contains silicon. The silicon of the silicon layer F1 may be amorphous silicon, polysilicon, or single-crystal silicon. The thickness of the silicon layer F1 is, for example, 200 nm to 500 nm, but is not limited thereto.

[0032] Method MT1 will be described below with reference to FIGS. 5 to 11 in addition to FIG. 4 , taking as an example a case where method MT1 is applied to a substrate W using the plasma processing apparatus 1 of the above embodiment. Each of FIGS. 5 to 11 is a cross-sectional view showing a step of an etching method according to one exemplary embodiment. When the plasma processing apparatus 1 is used, method MT1 can be performed in the plasma processing apparatus 1 by controlling each part of the plasma processing apparatus 1 with the control unit 2. In method MT1, a substrate W on a substrate support 11 arranged in a plasma processing chamber 10 is processed, as shown in FIG. 2 .

[0033] 3, the method MT1 may include steps ST1 to ST8, which may be performed in sequence within the same plasma processing chamber 10.

[0034] (Process ST1) In process ST1, the substrate W shown in FIG. 4 is prepared. The substrate W may be supported by a substrate support 11 in the plasma processing chamber 10. The opening OP may be formed in process ST1, or may be formed in advance prior to process ST1. A native oxide film NO may be formed on the surface of the silicon layer F1 in the substrate W. The native oxide film NO is a surface oxide film of the silicon layer F1, and is formed, for example, when the opening OP is formed, when the substrate W is transported into the plasma processing chamber 10, or the like.

[0035] (Step ST2) In step ST2, as shown in FIG. 5, the native oxide film NO is removed. In step ST2, the native oxide film NO is etched by plasma generated from, for example, a fluorine-containing gas. The fluorine-containing gas is, for example, hydrogen fluoride gas (HF gas), a fluorocarbon gas, or a hydrofluorocarbon gas. The fluorocarbon gas is, for example, C4 F 6 Gas, C 4 F 8 Gas, C 3 F 8 gas, and CF 4 Hydrofluorocarbon gases include, for example, CHF 3 Gas, CH 2 F 2 For example, a fluorine-containing gas is first supplied from the gas supply unit 20 into the plasma processing space 10s. Next, a pulse of source high-frequency power is supplied from the first RF generating unit 31a to the antenna 14, and a pulse of bias power is supplied from the second RF generating unit 31b to the substrate support 11. As a result, accelerated electrons collide with the fluorine-containing gas in the plasma processing space 10s, generating plasma from the fluorine-containing gas. The native oxide film NO is then etched using the plasma. The supply of the fluorine-containing gas can be stopped at the end of step ST2.

[0036] (Step ST3) In step ST3, as shown in FIG. 6, the silicon layer F1 is etched (first etching) using a first plasma generated from a processing gas (first processing gas) to form a recess Re overlapping the opening OP of the mask M. In step ST3, partial etching of the silicon layer F1 is performed. The etching of the silicon layer F1 is anisotropic etching using the mask M, but is not limited to this. The first processing gas is Cl 2The first process gas may further include a halogen-containing gas such as argon gas or nitrogen gas. The first process gas may further include an inert gas such as argon gas or nitrogen gas, or may further include an oxygen-containing gas. The first plasma may be, for example, an inductively coupled plasma, but is not limited thereto. In one example, the first process gas is first supplied from the gas supply unit 20 into the plasma processing space 10s. Next, a step (first step) of supplying a pulse of source high-frequency power from the first RF generator 31a to the antenna 14 and a step (second step) of supplying a pulse of bias power from the second RF generator 31b to the substrate support 11 are performed. By performing the first and second steps, a first plasma is generated. As a result, accelerated electrons collide with the first process gas in the plasma processing space 10s, generating a first plasma from the first process gas. The silicon layer F1 is then etched using the first plasma. The supply of the first process gas may be stopped at the end of step ST3.

[0037] In step ST3, the first step and the second step do not have to be performed simultaneously. In other words, the period (first period) in which the first RF generator 31a supplies pulses of source high-frequency power to the antenna 14 and the period (second period) in which the second RF generator 31b supplies pulses of bias power to the substrate support 11 do not have to overlap. In one example, the first step and the second step are performed consecutively in order. In this case, the first period and the second period are consecutive to each other. In step ST3, the lengths of the first period and the second period may be the same or different from each other. In one example, the first period may be 1.5 times or more, 2 times or more, 3 times or less, or 2.5 times or less than the second period. The first step and the second step may be performed consecutively without a gap, but this is not limited to this. For example, there may be a gap (interval) between the first step and the second step. In other words, there may be a short blank period between the first period and the second period.

[0038] In step ST3, the first step and the second step may be performed alternately and consecutively, but this is not limited thereto. For example, after the second step is completed, the first step may be performed again after a predetermined interval. In this case, step ST3 includes a step (third step) in which neither the source high-frequency power pulse nor the bias power pulse is supplied. In one example, the first step, the second step, and the third step are performed consecutively in a unit period (one cycle). In other words, in one example, the unit period is composed of a first period, a second period, and a period in which the third step is performed (a third period, also referred to as an offset period) that are consecutive to each other. The third period may be longer than at least one of the first period and the second period, shorter than at least one of the first period and the second period, or the same as at least one of the first period and the second period. In one example, the third period is approximately the same as the first period.

[0039] The recess Re has a first recess Re1 overlapping the first opening OP1 and a second recess Re2 overlapping the second opening OP2. The width w1 of the first recess Re1 corresponds to the minimum value of the width D1 of the first opening OP1, and the width w2 of the second recess Re2 corresponds to the minimum value of the width D2 of the second opening OP2. The depths of the first recess Re1 and the second recess Re2 are, for example, 30% to 60% of the thickness of the silicon layer F1. In one example, due to a change in etching depth depending on the width of the opening OP of the mask M (microloading effect), the depth of the second recess Re2 is greater than the depth of the first recess Re1, but this is not limited to this. The depths of the first recess Re1 and the second recess Re2 may be the same.

[0040] (Steps ST4 to ST6) In steps ST4 to ST6, as shown in FIGS. 8 and 9, a protective layer PL is formed at least on the sidewall SW of the recess Re. First, as shown in FIG. 7, in step ST4, a precursor layer PCL is formed at least on the sidewall SW of the recess Re (layer formation step). In step ST4, the precursor layer PCL is formed using plasma generated from a processing gas supplied into the plasma processing chamber 10. The precursor layer PCL may cover the entire sidewall SW or may cover only a portion of the sidewall SW. The precursor layer PCL may be formed not only on the sidewall SW of the recess Re but also on the bottom BT of the recess Re, on the side surface of the mask M, or on the upper surface of the mask M. In one example, the precursor layer PCL is formed by chemical vapor deposition (CVD), but is not limited to this. The CVD may be thermal CVD or plasma CVD. By using the CVD method, it is easier to form the precursor layer PCL in the desired region (i.e., on the sidewall SW of the recess Re). In other words, compared to the atomic layer deposition (ALD) method, it is more difficult to form the precursor layer PCL on the bottom BT of the recess Re (particularly, on the bottom BT of the first recess Re1).

[0041] The processing gas used in step ST4 is SiH 4 , SiCl 4 The process gas may include at least one of a silicon-containing gas such as SiO 2 , a diluent gas such as argon, helium, or nitrogen, and a halogen-containing gas such as HBr. The silicon-containing gas may correspond to a source gas for the precursor layer PCL. Therefore, the precursor layer PCL is a layer whose main component is silicon. If the process gas includes a halogen-containing gas, the precursor layer PCL may contain halogen. For example, if the process gas includes HBr, the precursor layer PCL may contain Br. The supply of the process gas may be stopped at the end of step ST4.

[0042] Next, in step ST5, as shown in FIG. 8 , the precursor layer PCL is modified into the protective layer PL using an oxygen-containing gas, which is a processing gas (third processing gas) (modification step). In step ST5, the oxygen-containing gas is supplied from the gas supply unit 20 into the plasma processing space 10s. This oxidizes (ashes) the precursor layer PCL, forming the protective layer PL, which is a silicon oxide film. Ashing of the precursor layer PCL may be performed simply by supplying the oxygen-containing gas into the plasma processing space 10s, or may be performed using plasma generated from the oxygen-containing gas. The oxygen-containing gas contains, for example, at least one of oxygen, carbon dioxide, carbon monoxide, and carbonyl sulfide.

[0043] If steps ST4 and ST5 have not been performed the predetermined number of times (step ST6: NO), steps ST4 and ST5 are performed again in sequence. As a result, a precursor layer PCL is deposited on the protective layer PL, and then the precursor layer PCL is ashed. Then, as shown in FIG. 9 , a thickened protective layer PL is formed. In one example, steps ST4 and ST5 are alternately repeated until each of steps ST4 and ST5 has been performed two to ten times (e.g., three, five, seven, or ten times). In other words, in one example, a cycle of steps ST4 and ST5 is performed two to ten times. If steps ST4 and ST5 have been performed the predetermined number of times (step ST6: YES), step ST7, described below, is performed.

[0044] (Process ST7) In process ST7, as shown in FIG. 10, a portion of the protective layer PL is removed. This may expose the bottom BT of the recess Re. In process ST7, another portion of the protective layer PL may be thinned. In process ST7, for example, using a method similar to process ST2, plasma generated from a fluorine-containing gas is used to remove the portion of the protective layer PL located on the bottom BT of the recess Re. The fluorine-containing gas used in process ST7 may be, for example, the same as the fluorine-containing gas used in process ST2, but is not limited to this. The supply of the fluorine-containing gas may be stopped at the end of process ST7.

[0045] (Step ST8) In step ST8, as shown in FIG. 11 , the bottom BT of the recess Re is etched (second etching) using a second plasma generated from a processing gas (second processing gas). In step ST8, the silicon layer F1 is etched using the second plasma to etch the bottom BT of the recess Re. This allows the bottom BT of the recess Re to reach the underlying region UR or its vicinity. The etching of the bottom BT is anisotropic etching using a mask M, but is not limited to this. In step ST8, the sidewall SW of the recess Re is covered with the protective layer PL. Therefore, the aspect ratio of the etching amount of the bottom BT to the sidewall SW can be extremely high. Therefore, not only the bottom BT of the second recess Re2 but also the bottom BT of the first recess Re1 can reach the underlying region UR or its vicinity. In other words, the microloading effect is less likely to occur. For example, the total etching amount of the first recess Re1 is 96.5% or more, 97% or more, 98% or more, or 99% or more of the total etching amount of the second recess Re2.

[0046] The second process gas may be the same as or different from the first process gas. When the second process gas is different from the first process gas, for example, the first process gas may contain Cl as a halogen-containing gas. 2 The second process gas contains Cl as a halogen-containing gas. 2 In this case, the second process gas contains Cl gas and HBr gas. 2 The flow rate of the gas is, for example, at least two, three, or four times, but not more than five times, the flow rate of HBr gas. The second process gas may further contain an inert gas such as argon gas or nitrogen gas, or may further contain an oxygen-containing gas. The second plasma may be, for example, an inductively coupled plasma, but is not limited thereto.

[0047] In one example, first, a second processing gas is supplied from the gas supply unit 20 into the plasma processing space 10s. Next, the first and second steps are performed to generate a second plasma. As a result, accelerated electrons collide with the second processing gas in the plasma processing space 10s, generating a second plasma from the second processing gas. Then, the silicon layer F1 is etched using the second plasma.

[0048] The duration of the first step in process ST8 may be the same as or different from the duration of the first step in process ST3. Similarly, the duration of the second step in process ST8 may be the same as or different from the duration of the second step in process ST3. In one example, the duration of the first step in process ST8 is longer than the duration of the first step in process ST3, and the duration of the second step in process ST8 is shorter than the duration of the second step in process ST3. The total duration of the first and second steps in process ST8 may be the same as or different from the total duration of the first and second steps in process ST3. In one example, the total duration of the first and second steps in process ST8 may be longer than the total duration of the first and second steps in process ST3. Furthermore, in process ST8, in addition to the first and second steps, the third step may be performed, as in process ST3. In this case, the duration of the third step in step ST8 may be the same as or different from the duration of the third step in step ST3. The supply of the second process gas may be stopped at the end of step ST8.

[0049] In step ST3, while the substrate W is supported on the substrate support 11, the control unit 2 controls the gas supply unit 20 and the plasma generation unit 12 to etch the silicon layer F1 using a first plasma generated from a first process gas, thereby forming a recess Re. In steps ST4 to ST6, the control unit 2 controls at least one of the gas supply unit 20 and the plasma generation unit 12 to form a protective layer PL at least on the sidewall SW of the recess Re. At this time, the control unit 2 controls the gas supply unit 20 and the plasma generation unit 12 to form a precursor layer PCL at least on the sidewall SW of the recess Re, and then to modify the precursor layer PCL into a protective layer PL using the third process gas. In step ST8, the bottom BT of the recess Re is etched using a second plasma generated from a second process gas. At this time, the control unit 2 controls the high-frequency power supply and the bias power supply to supply a pulse of source high-frequency power during a first period and to supply a pulse of bias power to the substrate support 11 during a second period that does not overlap with the first period.

[0050] Next, an example of the effects of the exemplary embodiment will be described with reference to the following reference examples. In Reference Example 1, the silicon layer F1 is etched only once. That is, steps ST4 to ST8 are not performed in Reference Example 1. In Reference Example 1, the total etching amount of the first recess Re1 is approximately 90% of the total etching amount of the second recess Re2. Therefore, when the thickness of the silicon layer F1 is approximately 200 nm, the difference between the total etching amount of the first recess Re1 and the total etching amount of the second recess Re2 in Reference Example 1 can be 20 nm or more. Furthermore, in Reference Example 2, steps ST4 to ST7 are not performed, and instead, oxygen ashing is performed between steps ST3 and ST8. In Reference Example 2, the total etching amount of the first recess Re1 is approximately 95% of the total etching amount of the second recess Re2. Therefore, when the thickness of the silicon layer F1 is about 200 nm, in Reference Example 2, the difference between the total etching amount of the first recess Re1 and the total etching amount of the second recess Re2 can be 10 nm or more.

[0051] In contrast, Example 1, which performs steps ST1 to ST8 of the method MT1 described above, can suppress both the occurrence of bowing and variations in the etching amount depending on the size of the opening. Specifically, in Example 1, after partially etching the silicon layer F1 in step ST3, a protective layer PL is formed on at least the sidewall SW of the recess Re in steps ST4 to ST6. Then, in step ST8, the silicon layer F1 is etched again to etch the bottom BT of the recess Re. This allows not only the bottom BT of the second recess Re2 but also the bottom BT of the first recess Re1 to reach or be close to the underlying region UR. In other words, the microloading effect is less likely to occur. Therefore, in Example 1, the total etching amount of the first recess Re1 can exceed 99% of the total etching amount of the second recess Re2. In other words, even when the thickness of the silicon layer F1 is approximately 200 nm, the difference between the total etching amount of the first recess Re1 and the total etching amount of the second recess Re2 can be suppressed to within a few nanometers. Additionally, in the step ST8, the protective layer PL makes it difficult for the sidewall SW of the recess Re to be etched, so that bowing is unlikely to occur in the first embodiment.

[0052] In one embodiment, the precursor layer PCL may be formed by a CVD method in step ST4. In this case, the precursor layer PCL can be favorably formed at least on the sidewall SW of the recess Re.

[0053] In one embodiment, the precursor layer PCL may be formed using a process gas including a silicon-containing gas and a halogen-containing gas.

[0054] In one embodiment, in the step of forming the protective layer PL, step ST4 and step ST5 may be alternately repeated, which can effectively suppress the occurrence of bowing.

[0055] In one embodiment, the method MT1 may include a step ST7 of removing the protective layer PL located on the bottom BT before the step ST8. In this case, the occurrence of bowing can be effectively suppressed.

[0056] Although various exemplary embodiments have been described above, the present invention is not limited to the above-described exemplary embodiments, and various additions, omissions, substitutions, and modifications may be made. Furthermore, elements in different embodiments may be combined to form other embodiments.

[0057] Various exemplary embodiments included in the present disclosure are now described in [E1] to [E10] below.

[0058] [E1] An etching method, comprising: preparing a substrate including a mask having a sparse / dense pattern and a silicon layer located below the mask; etching the silicon layer using a first plasma generated from a first process gas to form recesses overlapping with openings in the mask; forming a protective layer on at least side walls of the recesses; and etching a bottom of the recesses using a second plasma generated from a second process gas, wherein the step of forming the protective layer includes: a layer formation step of forming a precursor layer on at least the side walls of the recesses; and a modification step of modifying the precursor layer into the protective layer using a third process gas, and the step of etching the bottom of the recesses includes: a first step of supplying pulses of source radio frequency power from a radio frequency power supply; and a second step of supplying pulses of bias power from a bias power supply to a support portion that supports the substrate, wherein a period during which the first step and a period during which the second step are performed do not overlap with each other.

[0059] [E2] The etching method according to [E1], wherein the precursor layer is formed by a CVD method in the layer forming step.

[0060] [E3] The etching method according to [E1] or [E2], wherein the precursor layer is formed using a process gas containing a silicon-containing gas and a halogen-containing gas.

[0061] [E4] The etching method according to any one of [E1] to [E3], wherein in the step of forming the protective layer, the layer forming step and the modifying step are repeated alternately.

[0062] [E5] The etching method according to any one of [E1] to [E4], wherein the step of etching the bottom of the recess includes a third step in which neither the source high frequency power pulse nor the bias power pulse is supplied.

[0063] [E6] The etching method according to any one of [E1] to [E5], wherein each of the first plasma and the second plasma is an inductively coupled plasma.

[0064] [E7] The etching method according to any one of [E1] to [E6], wherein the second process gas is different from the first process gas.

[0065] [E8] The etching method according to any one of [E1] to [E7], wherein the third process gas is an oxygen-containing gas.

[0066] [E9] The etching method according to any one of [E1] to [E8], further comprising, before the step of etching the bottom of the recess, a step of removing the protective layer located on the bottom.

[0067] [E10] A semiconductor device comprising: a chamber; a substrate support provided in the chamber; a gas supply unit configured to supply a process gas into the chamber; a plasma generation unit configured to generate plasma from the process gas in the chamber; and a control unit, wherein the plasma generation unit has a high frequency power supply that supplies pulses of source high frequency power and a bias power supply that supplies pulses of bias power to the substrate support unit, and the control unit controls the gas supply unit and the plasma generation unit, with a mask having a sparse / dense pattern and a substrate including a silicon layer located under the mask, supported on the substrate support unit, to: form a recess overlapping an opening in the mask by etching the silicon layer using a first plasma generated from a first process gas; form a protective layer at least on a side wall of the recess; etch a bottom of the recess using a second plasma generated from a second process gas; and when forming the protective layer, the control unit controls the gas supply unit and the plasma generation unit to form a precursor layer at least on the side wall of the recess, and then modify the precursor layer into the protective layer using a third process gas. When etching the bottom of the recess, the control unit controls the high frequency power supply and the bias power supply so as to supply a pulse of the source high frequency power in a first period and to supply a pulse of the bias power to the substrate support unit in a second period that does not overlap with the first period.

[0068] From the foregoing, it will be understood that various embodiments of the present disclosure have been described herein for purposes of illustration, and that various modifications may be made without departing from the scope and spirit of the present disclosure. Accordingly, the various embodiments disclosed herein are not intended to be limiting, with the true scope and spirit being indicated by the appended claims.

[0069] 1...plasma processing apparatus, 2...control unit, 10...plasma processing chamber, 11...substrate support unit, 12...plasma generation unit, 20...gas supply unit, F1...silicon layer, M...mask, NO...native oxide film, OP...opening, OP1...first opening, OP2...second opening, PCL...precursor layer, PL...protective layer, Re...recess, Re1...first recess, Re2...second recess, SW...side wall, W...substrate.

Claims

1. An etching method comprising the steps of: preparing a substrate including a mask having a sparse / dense pattern and a silicon layer located below the mask; etching the silicon layer with a first plasma generated from a first process gas to form a recess overlapping an opening in the mask; forming a protective layer on at least a side wall of the recess; and etching a bottom of the recess with a second plasma generated from a second process gas, wherein the step of forming the protective layer includes a layer formation step of forming a precursor layer on at least the side wall of the recess; and a modification step of modifying the precursor layer into the protective layer using a third process gas, and wherein the step of etching the bottom of the recess includes a first step of supplying a pulse of source high frequency power from a high frequency power supply; and a second step of supplying a pulse of bias power from a bias power supply to a support portion supporting the substrate, wherein a period during which the first step is performed and a period during which the second step is performed do not overlap each other.

2. The etching method according to claim 1, wherein in the layer forming step, the precursor layer is formed by a CVD method.

3. The etching method according to claim 1 or 2, wherein the precursor layer is formed using a process gas containing a silicon-containing gas and a halogen-containing gas.

4. The etching method according to claim 1 or 2, wherein in the step of forming the protective layer, the layer forming step and the modifying step are repeated alternately.

5. An etching method according to claim 1 or 2, wherein the step of etching the bottom of the recess includes a third step in which neither the pulse of source high frequency power nor the pulse of bias power is supplied.

6. The etching method according to claim 1 or 2, wherein each of the first plasma and the second plasma is an inductively coupled plasma.

7. The etching method of claim 1 or 2, wherein the second process gas is different from the first process gas.

8. The etching method according to claim 1 or 2, wherein the third process gas is an oxygen-containing gas.

9. The etching method according to claim 1 or 2, further comprising the step of removing the protective layer located on the bottom of the recess before the step of etching the bottom of the recess.

10. A method for manufacturing a semiconductor device comprising: a chamber; a substrate support provided within the chamber; a gas supply unit configured to supply a process gas into the chamber; a plasma generation unit configured to generate plasma from the process gas in the chamber; and a control unit, wherein the plasma generation unit has a high frequency power supply that supplies pulses of source high frequency power and a bias power supply that supplies pulses of bias power to the substrate support unit, and the control unit, while a mask having a sparse / dense pattern and a substrate including a silicon layer located under the mask are supported by the substrate support unit, controls the gas supply unit and the plasma generation unit to: form a recess overlapping an opening of the mask by etching the silicon layer using a first plasma generated from a first process gas; form a protective layer at least on a side wall of the recess; etch a bottom of the recess using a second plasma generated from a second process gas; and, when forming the protective layer, the control unit controls the gas supply unit and the plasma generation unit to form a precursor layer at least on the side wall of the recess, and then modify the precursor layer into the protective layer using a third process gas, the control unit controls the high frequency power supply and the bias power supply so as to supply a pulse of the source high frequency power in a first period and to supply a pulse of the bias power to the substrate support unit in a second period that does not overlap with the first period when etching the bottom of the recess.

Citation Information

Patent Citations

  • Method for processing workpiece

    JP2017183689A

  • Etching method and plasma processing device

    JP2019220508A

  • High Energy Atomic Layer Etching

    JP2020536393A

  • Atomic layer deposition and etching for fin field effect transistor formation in a single plasma chamber

    JP2021504973A