Methods for producing a nanocrystal

The method of optimizing hold time and temperature in the production of nanocrystals with elemental chalcogen and aliphatic amine solutions addresses inefficiencies in existing methods, producing high-quality, monodisperse nanocrystals with narrow excitonic absorption widths for advanced applications.

WO2024217792A1PCT designated stage expired Publication Date: 2024-10-24AMS OSRAM INT GMBH
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
PCT/EP2024/056964
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-04-19
Filing Date
2024-03-15
Publication Date
2024-10-24

AI Technical Summary

Technical Problem

Current methods for producing nanocrystals are inefficient and lack control over size dispersity and excitonic absorption width, leading to polydisperse and low-quality nanocrystals.

Method used

A method involving a first solution of elemental chalcogen and aliphatic amine, heated to form a reactive species, then added to a second solution with a heavy metal halide and alkene, optimizing hold time and temperature to control nucleation and precursor ratios, resulting in monodisperse nanocrystals with narrow excitonic absorption widths.

Benefits of technology

This method enables the production of large, monodisperse nanocrystals with narrow excitonic absorption widths, improving reaction control and reducing material waste, suitable for applications like photovoltaics and infrared light absorption.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure EP2024056964_24102024_PF_FP_ABST
    Figure EP2024056964_24102024_PF_FP_ABST
Patent Text Reader

Abstract

A method for producing a nanocrystal comprises - providing a first solution comprising an elemental chalcogen and a first aliphatic amine, - holding the first solution at a hold temperature of at least 50 °C for a hold time of at least 10 minutes, - adding the first solution to a second solution comprising a heavy metal halide, a second aliphatic amine, and an alkene.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] Description

[0002] METHODS FOR PRODUCING A NANOCRYSTAL

[0003] Methods for producing a nanocrystal , in particular for producing a plurality of nanocrystals , are speci fied .

[0004] It is an obj ect to provide simple and ef ficient methods for producing a nanocrystal .

[0005] According to at least one embodiment , a method for producing a nanocrystal , in particular for producing a plurality of nanocrystals , is provided . A nanocrystal is a small obj ect with dimensions in the nanometer range that can have di f ferent properties than bulk material of the same composition . In particular, the nanocrystal has at least one dimension smaller than 100 nm . The nanocrystal is a nanoparticle with a mostly crystalline structure , for example , a semiconductor nanoparticle or a quantum dot . In particular, the nanocrystal is composed of atoms in a single- or polycrystalline arrangement .

[0006] For instance , the nanocrystal is a heavy metal chalcogenide nanocrystal . A heavy metal chalcogenide is a binary chemical compound consisting of at least one chalcogen anion of the group 16 elements of the periodic table and at least one or more heavy metal cation . Here and in the following, a heavy metal is in particular a metal element having a density of more than 5 g / cm3. For example , the nanocrystal is a lead sul fide ( PbS ) nanocrystal .

[0007] In particular, the nanocrystal is a radiation-converting nanocrystal . A radiation-converting nanocrystal may be used as a conversion material for converting primary radiation of a first wavelength range in secondary radiation of a second wavelength range which comprises , for example , longer wavelengths than the primary radiation .

[0008] According to at least one embodiment of the method, a first solution comprising an elemental chalcogen and a first aliphatic amine is provided . In particular, the elemental chalcogen is one of the precursors for producing the nanocrystal . For example , the first solution is produced by combining the elemental chalcogen and the first aliphatic amine while bubbling a gas such as argon through the first solution and stirring .

[0009] Chalcogens are the chemical elements in group 16 of the periodic table . In particular, the elemental chalcogen is at least one of the elements sul fur, selenium, and tellurium .

[0010] Aliphatic amines are amine compounds having only non-aromatic hydrocarbon substituents on nitrogen . In other words , aliphatic amines are ammonia derivatives with one or more hydrogen atoms substituted by aliphatic hydrocarbon substituents . Aliphatic amines can be primary amines having one aliphatic hydrocarbon substituent and two hydrogen atoms , secondary amines having two aliphatic hydrocarbon substituents and one hydrogen atom, or tertiary amines having three aliphatic hydrocarbon substituents as substituents on the nitrogen . In particular, the first aliphatic amine is a primary amine .

[0011] Each aliphatic hydrocarbon substituent can be saturated or unsaturated and / or linear or branched and / or open-chained or cyclic . Saturated aliphatic hydrocarbon substituents such as alkyl groups contain only single bonds . An unsaturated aliphatic hydrocarbon substituent contains one or more double bonds such as alkenyl groups and / or one or more triple bonds such as alkynyl groups . A linear aliphatic hydrocarbon substituent comprises a linear backbone with each carbon atom of the molecular skeleton bonded to at most two other carbon atoms . A branched aliphatic hydrocarbon substituent has a nonlinear backbone with at least one carbon atom of the molecular skeleton bonded to at least three other carbon atoms . An open-chain aliphatic hydrocarbon substituent contains no ring of any type . A cyclic aliphatic hydrocarbon substituent contains a ring that is not aromatic . Each aliphatic hydrocarbon substituent can comprise between and including 1 and 20 carbon atoms .

[0012] According to at least one embodiment of the method, the first solution is held at a hold temperature of at least 50 ° C for a hold time of at least 10 minutes . In particular, the elemental chalcogen and the first aliphatic amine in the first solution react during the hold time to form a reactive chalcogen species . After the hold time at the hold temperature is completed, the first solution may be cooled back to room temperature . In this context , room temperature may be a temperature between and including 15 ° C and 30 ° C . For instance , the first solution is held at a hold temperature of at least 50 ° C for a hold time of less than 100 minutes .

[0013] According to at least one embodiment of the method, the first solution is added to a second solution comprising a heavy metal halide , a second aliphatic amine , and an alkene . In particular, the heavy metal halide is one of the precursors for producing the nanocrystal . For instance , the first solution is added to the second solution to initiate the growth of nanocrystals . In other words , a nucleation event or a nucleation reaction takes place when the first solution is added to the second solution . For example , the first solution is inj ected into the second solution .

[0014] A heavy metal halide or heavy metal halogenide is a binary chemical compound consisting of at least one halogen anion of the group 17 elements of the periodic table and at least one or more heavy metal cations . In particular, the halogen for the halogen anion is at least one of fluorine , chlorine , bromine , and iodine . In particular, the heavy metal for the heavy metal cation is lead .

[0015] In particular, the second aliphatic amine is a primary amine .

[0016] An alkene is a hydrocarbon containing at least one carboncarbon double bond . A hydrocarbon containing at least one carbon-carbon double bond is also called olefin . The double bond can be a terminal double bond located at one end of the hydrocarbon or an internal double bond located on a carbon somewhere in the center of the hydrocarbon chain . Hydrocarbons with a terminal double bond are called alphaolefin . The alkene can comprise between and including 2 and 20 carbon atoms , in particular between and including 2 and 10 carbon atoms . In particular, the alkene has a boiling point above 120 ° C . For example , the alkene is an alpha-olefin .

[0017] According to at least one embodiment , the method for producing a nanocrystal is provided comprises :

[0018] - providing a first solution comprising an elemental chalcogen and a first aliphatic amine , - holding the first solution at a hold temperature of at least 50 ° C for a hold time of at least 10 minutes , and

[0019] - adding the first solution to a second solution comprising a heavy metal halide , a second aliphatic amine , and an alkene .

[0020] The method steps for producing a nanocrystal described here are not restricted to this order . According to one embodiment , however, they are carried out in this order .

[0021] In the method described herein, the hold time is , in particular, a parameter for tuning the color of the nanocrystal and / or the dispersity of a plurality of nanocrystals . A shorter hold time results in a faster nucleation reaction in the second solution such that producing bigger nanocrystals and thus accessing di f ferent colors is possible . In other words , when the hold time is less , poorer nucleation results in fewer nuclei that then grow fast resulting in bigger and more polydisperse nanocrystals . A longer hold time results in a slower nucleation reaction in the second solution such that the yield increases for nanocrystals of a similar si ze . In other words , increasing the hold time results in more nuclei formed and fewer resources for the nuclei to grow fast resulting in more monodisperse nanocrystals . In particular, there is a near-linear correlation between the hold time and the rate at which the nucleation reaction in the second solution proceeds to a given color point , when the hold time is set between more than 20 minutes and 80 minutes .

[0022] Such a method allows for the synthesis of large , monodispersed nanocrystals having a narrow first excitonic absorption hal f width at hal f maximum (HWHM) by lengthening the hold time of the first solution prior to adding the first solution to the second solution . By optimi zing the time that the first solution is held at the hold temperature , the amount of elemental chalcogen that is converted to the reactive sul fur species is increased . Therefore , the number of nuclei is increased that can be generated upon adding the first solution to the heavy metal precursor-containing second solution . The reaction is further promoted by the combination of an alkene in the second solution and the first and the second aliphatic amines in the reaction . With increasing the hold time and the addition of the alkene , the nucleation event is signi ficantly improved while the reaction control , even at scaled-up reaction si zes , is maintained and a heavy metal-to-chalcogen precursor molar ratio can be reduced .

[0023] According to at least one embodiment , the hold time is more than 20 minutes . The near-linear correlation between the hold time and the rate at which the nucleation reaction in the second solution proceeds to a given color point , when the hold time is set between more than 20 minutes and 80 minutes is advantageous for controlling the nucleation reaction .

[0024] According to at least one embodiment , the hold time is between and including 40 minutes and 80 minutes . The near- linear correlation between hold time and the rate at which the nucleation reaction in the second solution proceeds to a given color point , when the hold time is set between and including 40 minutes and 80 minutes is advantageous for controlling the nucleation reaction .

[0025] According to at least one embodiment , the hold temperature is at least 90 ° C, for example 100 ° C or 120 ° C . In particular, the maximum hold temperature is selected in such a way that the maximum hold temperature is below the boiling point of any solvents in the first solution such as the aliphatic amine .

[0026] It should be noted that a lower hold temperature results in a longer reaction time for forming the reactive chalcogen species. In particular, the hold temperature and the hold time are related in such a way that increasing either the hold temperature or the hold time may result in the possibility of decreasing the hold time or the hold temperature, respectively, without affecting the result of the nucleation reaction when the first solution is added to the second solution. In other words, there may be a tradeoff between the hold temperature and the hold time. For example, a hold time of 40 minutes at a hold temperature of 120 °C could have the same effect on the nucleation reaction as a hold time of 80 minutes at a hold temperature of 100 °C.

[0027] According to at least one embodiment, a precursor molar ratio of the heavy metal to the elemental chalcogen is less than 24:1. In other words, the heavy metal-to-chalcogen precursor molar ratio is less than 24:1. In particular, the heavy metal-to-chalcogen precursor molar ratio is at most 20:1 or at most 15:1 or at most 10:1, for instance at most 5:1, for example 4:1, 2:1, 1.5:1, or 1:1. For instance, the minimum metal-to-chalcogen precursor molar ratio is 1:1. An excess of the heavy metal precursor or an equal amount of heavy metal precursor and elemental chalcogen precursor is advantageous for driving the nucleation reaction due to kinetic reasons. With a precursor molar ratio of less than 24:1, less material is needed and subsequently goes to waste. This also makes purification much more straightforward. Further, as the reaction is scaled, decreasing the precursor molar ratio allows for much greater control of the nucleation event, therefore leading to the formation of higher-quality nanocrystals .

[0028] According to at least one embodiment , a first excitonic absorption hal f width at hal f maximum of the nanocrystal is less than 30 meV . In particular, the first excitonic absorption hal f width at hal f maximum of the nanocrystal is at most 25 meV, for example 23 meV or 22 meV . The first excitonic absorption hal f width at hal f maximum of the nanocrystal is the hal f width at hal f maximum of the first absorption peak . The first excitonic absorption hal f width at hal f maximum can be a metric for the si ze dispersity of a plurality nanocrystals with a small hal f width at hal f maximum value signaling a monodisperse batch of nanocrystals . Thus , a plurality of monodisperse nanocrystals can advantageously be produced by the method for producing a nanocrystal .

[0029] According to at least one embodiment , the nanocrystal has a peak absorption wavelength of between and including 1100 nm and 1500 nm, in particular between and including 1300 nm and 1500 nm, for example of 1450 nm . With the method disclosed herein, a large heavy metal chalcogenide nanocrystal can be produced that advantageously absorbs between and including 1100 nm and 1500 nm .

[0030] According to at least one embodiment , the elemental chalcogen is one of sul fur, selenium, or tellurium . In particular, the elemental chalcogen is sul fur . In this instance , the sul fur forms a reactive sul fur species by reacting with the first aliphatic amine in the first solution . Such elemental chalcogens are advantageously suited for producing heavy metal sul fide nanocrystals , heavy metal selenide nanocrystals , or heavy metal telluride nanocrystals .

[0031] According to at least one embodiment , the first aliphatic amine and / or the second aliphatic amine comprises a double bond . In other words , the first aliphatic amine and / or the second aliphatic amine is an unsaturated amine comprising at least one unsaturated hydrocarbon substituent . For example , the first aliphatic amine and / or the second aliphatic amine is an unsaturated fatty amine . An unsaturated fatty amine is an amine with an unsaturated hydrocarbon substituent having a chain of eight or more carbon atoms . A first aliphatic amine and / or a second aliphatic amine with a double bond advantageously increase the reactivity of the first solution and / or the second solution, respectively .

[0032] According to at least one embodiment , the first aliphatic amine and / or the second aliphatic amine is oleylamine . Oleylamine or 9-octadecenylamine is an organic compound with a molecular formula Ci8H35NH2. The IUPAC name of oleylamine is ( 9Z ) -octadec- 9-en- l-amine . Oleylamine is an unsaturated fatty amine related to the fatty acid oleic acid . For instance , both the first aliphatic amine and the second aliphatic amine are oleylamine . In the first solution, oleylamine is advantageously suited to react with the elemental chalcogen to form the reactive chalcogen species . In the second solution, the combination of oleylamine and the alkene advantageously promote the nucleation reaction .

[0033] According to at least one embodiment , the first aliphatic amine and / or the second aliphatic amine comprises only single bonds . In other words , the first aliphatic amine and / or the second aliphatic amine is a saturated amine comprising only saturated hydrocarbon substituent. For example, the first aliphatic amine and / or the second aliphatic amine are one of dodecylamine, octadecylamine, and hexylamine.

[0034] According to at least one embodiment, the first aliphatic amine and the second aliphatic amine are identical. In other words, the aliphatic amine in the first solution and the aliphatic amine in the second solution are the same aliphatic amine. In particular, the first aliphatic amine and the second aliphatic amine are both the same aliphatic amine comprising a double bond. For example, the first aliphatic amine and the second aliphatic amine are both oleylamine. For identical first and second aliphatic amines, the first solution and the second solution can advantageously form a homogeneous phase upon mixing and thereby improving the nucleation event.

[0035] According to at least one embodiment, the first aliphatic amine and the second aliphatic amine are different. In particular, the first aliphatic amine is oleylamine, whereas the second aliphatic amine is an unsaturated aliphatic amine different from oleylamine. Alternatively, the first aliphatic amine is oleylamine, whereas the second aliphatic amine is a saturated amine such as dodecylamine, octadecylamine, or hexylamine. For different first and second aliphatic amines, the first solution and the second solution may not be homogeneous upon mixing, which may advantageously increase the reactivity.

[0036] According to at least one embodiment, the heavy metal halide is PbF2, PbC12, PbBr2, or Pbl2. For example, the heavy metal halide is PbCl2. Such heavy metal halides are advantageously suited for producing lead chalcogenide nanocrystals. According to at least one embodiment , the alkene and the second aliphatic amine have an equal volume ratio in the second solution . Having an equal volume ratio of the alkene and the second aliphatic amine advantageously allows for a greater control of the nucleation event when the first solution is added to the second solution .

[0037] According to at least one embodiment , the alkene is octadecene . Octadecene is an unsaturated hydrocarbon with the molecular formula Ci8H36. In particular, the alkene is 1- octadecene . 1-Octadecene contains one double bond as a terminal double bond . In other words , 1-octadecene is an alpha-olefin . The introduction of octadecene into the second solution advantageously results in a narrower first excitonic absorption hal f width at hal f maximum, a greater peak-to- valley ratio in an absorption curve , and, in the case that a plurality of nanocrystals is produced, an improved monodispersity of the nanocrystals .

[0038] According to at least one embodiment , the first solution is added to the second solution at an adding temperature of less than 120 ° C, in particular of less than or equal to 110 ° C . In this context , the adding temperature is the temperature of the second solution to which the first solution is added . For example , the first solution is added to the second solution at an adding temperature of 110 ° C . In particular, the first solution is added to the second solution at an adding temperature of 110 ° C after the first solution was held at a hold temperature for a hold time of 80 minutes . A hold time of at least 10 minutes , in particular of more than 20 minutes for the first solution advantageously enables the ability to synthesi ze nanocrystals at lower adding temperatures as an added route to controlling the reaction rate .

[0039] According to at least one embodiment , the method is a method for producing a plurality of nanocrystals , wherein the plurality of nanocrystals is monodisperse . In particular, a plurality of nanocrystals comprises at least two nanocrystals for example , 1027nanocrystals . In other words , a plurality of nanocrystals comprises at least 1 nanomole of nanocrystals , for example 5 moles of nanocrystals . Here and in the following, monodisperse means that the nanocrystals of the plurality of nanocrystals have a si ze dispersity of less than 5% . In other words , monodisperse nanocrystals are nanocrystals of nearly all the same si ze . For example , a plurality of monodisperse nanocrystals creates a flat energy landscape and provides a narrow and well-controlled absorption and emission . Thus , monodisperse nanocrystals are advantageously suited for applications such as photovoltaics , photodetectors , and infrared light absorption and emission .

[0040] Another aspect relates to a method for producing a nanocrystal , in particular for producing a plurality of nanocrystals . Features and embodiments of the method described above are therefore also disclosed for the method as follows and vice versa .

[0041] According to at least one embodiment , a method for producing a nanocrystal , in particular for producing a plurality of nanocrystals , is provided . The method comprises

[0042] - providing a first solution comprising an elemental chalcogen and a first aliphatic amine ,

[0043] - heating the first solution to a temperature above 50 ° C, - adding the first solution to a second solution comprising a heavy metal halide and a second aliphatic amine, wherein a precursor molar ratio of the heavy metal to the elemental chalcogen is less than 24:1, and a first excitonic absorption half width at half maximum of the nanocrystal is less than 30 meV.

[0044] The method steps for producing a nanocrystal described here are not restricted to this order. According to one embodiment, however, they are carried out in this order.

[0045] In the method, a reactive chalcogen species is, in particular, produced from the elemental chalcogen in the first solution by heating the first solution to a temperature above 50 °C, in particular above 90 °C, for example 100 °C or 120 °C. By adding the first solution with the reactive chalcogen species to the second solution, a nucleation reaction is initiated in the second solution and the nuclei then grow to form heavy metal chalcogenide nanocrystals. The precursor molar ratio of the heavy metal to the elemental chalcogen is, in particular, less than 20:1 or less than 15:1, for instance less than 10:1 or less than 5:1, for example 4:1, 2:1, 1.5:1, 1:1. The first excitonic absorption half width at half maximum of the nanocrystal is, in particular, less than 25 meV, for example 23.5 meV, 23 meV, or 22 meV.

[0046] Such a method allows for producing heavy metal chalcogenide nanocrystals having a peak absorption wavelength between and including 1100 nm and 1500 nm, in particular between and including 1300 nm and 1500 nm, and a narrow first excitonic absorption half width at half maximum by using a precursor molar ratio of heavy metal to elemental chalcogen of less than 24 : 1 . Such a reduced precursor molar ratio is advantageous as less material is needed and subsequently goes to waste which also makes puri fication much more straightforward . Further, as the reaction is scaled, the method allows for much greater control of the nucleation event , and therefore , enables the formation of nanocrystals having a narrow first excitonic absorption hal f width at hal f maximum of less than 30 meV .

[0047] According to at least one embodiment , the method further comprises holding the first solution at a hold temperature of at least 50 ° C for a hold time of at least 10 minutes , in particular of more than 20 minutes . In particular, the first solution is held at a hold temperature of at least 90 ° C . For example , the first solution is held at the hold temperature for a hold time of between and including 40 and 80 minutes . By optimi zing the hold time , the amount of elemental chalcogen converted to the reactive chalcogen species is advantageously increased, therefore increasing the number of nuclei that can be generated upon adding the first solution to the second solution .

[0048] According to at least one embodiment , the second solution further comprises an alkene , for example 1-octadecene . Advantageously, the combination of the second aliphatic amine and the alkene in the second solution promotes the nucleation reaction .

[0049] Advantageous embodiments and developments of the methods for producing a nanocrystal will become apparent from the exemplary embodiments described below in conj unction with the figures . In the figures:

[0050] FIG. 1 shows a schematic illustration of a nanocrystal according to an exemplary embodiment,

[0051] FIG. 2 and FIG. 3 each show three absorption curves of a plurality of nanocrystals according to different exemplary embodiments ,

[0052] FIG. 4 shows two absorption curves of a plurality of nanocrystals according to different exemplary embodiments, and

[0053] FIG. 5 and FIG. 6 each show a transmission electron microscopy (TEM) image of a plurality of nanocrystals according to different exemplary embodiments.

[0054] In the exemplary embodiments and figures, similar or similarly acting constituent parts are provided with the same reference symbols. The elements illustrated in the figures and their size relationships among one another should not be regarded as being true to scale. Rather, individual elements may be represented with an exaggerated size for the sake of better representability and / or for the sake of better understanding .

[0055] FIG. 1 shows a schematic illustration of a nanocrystal 1. In particular, the nanocrystal 1 is a heavy metal chalcogenide nanocrystal 1, for example, a lead sulfide (PbS) nanocrystal 1.

[0056] A PbS nanocrystal 1 or a plurality of PbS nanocrystals 1 is produced as follows: A first solution is provided by combining elemental sulfur and oleylamine in a three neck flask while bubbling argon through the solution and stirring. For making the reactive sulfur species, the first solution is heated to a hold temperature of 120 °C. The first solution is held at the hold temperature for a hold time of at least 10 minutes, in particular of more than 20 minutes, for example, between and including 40 minutes and 80 minutes, wherein the timing of the hold time is started once the temperature reaches T = 100 °C. Then, the first solution is cooled back to room temperature. The first solution comprising the reactive sulfur species is then added to a second solution by swiftly injecting the first solution into a flask comprising the second solution. The second solution comprises PbC12, oleylamine, and 1-octadecene with an equal volume ratio of oleylamine and 1-octadecene. The first solution is added to the second solution at an adding temperature of 120 °C to initiate the growth of PbS nanocrystals 1. The precursor molar ratio of lead to elemental sulfur is 4:1. The resulting plurality of PbS nanocrystals 1 have a peak absorption wavelength between and including 1100 nm and 1300 nm, in particular between and including 1300 nm and 1500 nm, such as 1450 nm with a first excitonic absorption half width at half maximum of less than 30 meV such as 23.5 meV, 23 meV, or 22 meV. In other words, the plurality of PbS nanocrystals 1 is monodisperse. For example, the plurality of PbS nanocrystals 1 has a first excitonic absorption half width at half maximum of 23.5 meV at a peak absorption wavelength of 1500 nm.

[0057] By optimizing the time that the first solution is held at the hold temperature, the amount of elemental sulfur is increased that is converted to the reactive sulfur species. Therefore, the number of nuclei is increased that can be generated upon injection the first solution into the lead precursorcontaining second solution. This can be done without having to alter the Pb : S precursor ratio, yet still allowing for the potential to attain a wide range of PbS nanocrystal sizes and thus colors.

[0058] It was further recognized that there is a near-linear correlation between hold time and the rate at which the PbS nucleation reaction proceeds to a given color point, when the hold time is set between more than 20 minutes and 80 minutes, in particular between and including 40 minutes and 80 minutes (FIG. 2 and FIG. 3) .

[0059] FIG. 2 and FIG. 3 each shows three absorption curves of PbS nanocrystals 1. The normalized absorbance is plotted as a function of the wavelength X in nm.

[0060] FIG. 2 shows three absorption curves of PbS nanocrystals 1 grown after a hold time of 40 minutes. The PbS nanocrystals 1 are grown for 2:00 minutes (curve 2-1) , 7:00 minutes (curve 2-2) or 8:40 minutes (curve 2-3) after adding the first solution to the second solution.

[0061] FIG. 3 shows three absorption curves of PbS nanocrystals 1 grown after a hold time of 80 minutes. The PbS nanocrystals 1 are grown for 2:00 minutes (curve 3-1) , 7:00 minutes (curve 3-2) or 17:00 minutes (curve 3-3) after adding the first solution to the second solution.

[0062] When the hold time is 40 minutes, poorer nucleation results in fewer nuclei that grow fast with a high amount of unreacted precursors at the end (FIG. 2) . Increasing the hold time to 80 minutes results in more nuclei formed, fewer resources for the nuclei to grow very fast , and yields a more controllable reaction especially at larger scales ( FIG . 3 ) .

[0063] The vertical dashed lines are located at the same wavelengths in both FIG . 2 and FIG . 3 for indicating the growth speed of the PbS nanocrystals 1 with di f ferent hold times . It becomes apparent from both FIG . 2 and FIG . 3 that a longer reaction time after adding the first solution to the second solution leads to bigger nanocrystals and thus longer wavelengths of the resulting PbS nanocrystals 1 . Further, FIG . 3 shows in comparison to FIG . 2 that increasing the hold time from 40 minutes to 80 minutes decreases the growth rate of the PbS nanocrystals 1 and increases the monodispersity of the PbS nanocrystals 1 .

[0064] Additionally, introduction of 1-octadecene into the second solution results in narrower first excitonic absorption hal f width at hal f maximum and greater peak-to-valley ratios in corresponding absorption curves ( FIG . 4 ) .

[0065] FIG . 4 shows two absorption curves of PbS nanocrystals 1 . The normali zed absorbance is plotted as a function of the wavelength X in nm . Curve 4- 1 shows the absorption curve of PbS nanocrystals 1 grown without 1-octadecene present in the second solution . Curve 4-2 shows the absorption curve of PbS nanocrystals 1 grown with 1-octadecene present in the second solution . Curve 4-2 illustrates the narrower first excitonic absorption hal f width at hal f maximum values that can be attained when 1-octadecene is added to the second solution . Curve 4- 1 shows the wider first excitonic absorption hal f width at hal f maximum when 1-octadecene is not added to the second solution . In addition, curve 4-2 shows a peak-to- valley ratio of approximately 7, whereas curve 4-1 merely shows a peak-to-valley ratio of 5.8.

[0066] FIG. 5 and FIG. 6 each show shows a TEM image of PbS nanocrystals 1. FIG. 5 shows the TEM image of the PbS nanocrystals 1 that produced the absorption curve 4-1 in FIG. 4. FIG. 6 shows the TEM image of the PbS nanocrystals 1 that produced the absorption curve 4-2 in FIG. 4. FIG. 5 highlights the polydispersity in nanocrystal sizes when 1- octadecene is not added to the second solution, while FIG. 6 shows a higher degree of size homogeneity that correlates with the higher-quality optical data of curve 4-2 in FIG. 4.

[0067] Alternatively, a PbS nanocrystal 1 or a plurality of PbS nanocrystals 1 can be produced as follows:

[0068] A first solution is provided by combining elemental sulfur and oleylamine in a three neck flask while bubbling argon through the solution and stirring. For making the reactive sulfur species, the first solution is heated to a hold temperature of 120 °C. The first solution is held at the hold temperature for a hold time of 80 minutes, wherein the timing of the hold time is started once the temperature reaches T = 100 °C. Then, the first solution is cooled back to room temperature. The first solution comprising the reactive sulfur species is then added to a second solution by swiftly injecting the first solution into a flask comprising the second solution. The second solution comprises PbC12, oleylamine, and 1-octadecene with an equal volume ratio of oleylamine and 1-octadecene. The first solution is added to the second solution at an adding temperature of less than or equal to 110 °C, in particular of 110 °C, to initiate the growth of PbS nanocrystals 1. The precursor molar ratio of lead to elemental sul fur is 4 : 1 . The resulting plurality of PbS nanocrystals 1 is monodisperse .

[0069] In this method, an 80 minute hold time for the first solution enables the ability to synthesi ze PbS nanocrystals 1 at lower adding temperatures of less than or equal to 110 ° C .

[0070] The features and exemplary embodiments described in connection with the figures can be combined with each other according to further exemplary embodiments , even i f not all combinations are explicitly described . Furthermore , the exemplary embodiments described in connection with the figures may have alternative or additional features as described in the general part .

[0071] The invention is not restricted to the exemplary embodiments by the description on the basis of said exemplary embodiments . Rather, the invention encompasses any new feature and also any combination of features , which in particular comprises any combination of features in the patent claims and any combination of features in the exemplary embodiments , even i f this feature or this combination itsel f is not explicitly speci fied in the patent claims or exemplary embodiments .

[0072] This patent application claims the priority of US patent application 63 / 496 , 964 , the disclosure content of which is hereby incorporated by reference . References

[0073] 1 nanocrystal

[0074] 2-1, 2-2, 2-3 curve 3-1, 3-2, 3-3 curve

[0075] 4-1, 4-2 curve

Claims

Claims1. A method for producing a nanocrystal (1) , the method comprising- providing a first solution comprising an elemental chalcogen and a first aliphatic amine,- holding the first solution at a hold temperature of at least 50 °C for a hold time of at least 10 minutes, and- adding the first solution to a second solution comprising a heavy metal halide, a second aliphatic amine, and an alkene.

2. The method according to the preceding claim, wherein the hold time is more than 20 minutes.

3. The method according to one of the preceding claims, wherein the hold time is between and including 40 minutes and 80 minutes.

4. The method according to one of the preceding claims, wherein the hold temperature is at least 90 °C.

5. The method according to one of the preceding claims, wherein a precursor molar ratio of the heavy metal to the elemental chalcogen is less than 24:1.

6. The method according to one of the preceding claims, wherein a first excitonic absorption half width at half maximum of the nanocrystal is less than 30 meV.

7. The method according to one of the preceding claims, wherein the nanocrystal has a peak absorption wavelength of between and including 1100 nm and 1500 nm.

8. The method according to one of the preceding claims, wherein the elemental chalcogen is one of sulfur, selenium, or tellurium.

9. The method according to one of the preceding claims, wherein the first aliphatic amine and / or the second aliphatic amine comprises a double bond.

10. The method according to one of the preceding claims, wherein the first aliphatic amine and / or the second aliphatic amine is oleylamine.

11. The method according to one of the preceding claims, wherein the heavy metal halide is PbF2, PbC12, PbBr2, or Pbl2.

12. The method according to one of the preceding claims, wherein the alkene and the second aliphatic amine have an equal volume ratio in the second solution.

13. The method according to one of the preceding claims, wherein the alkene is octadecene.

14. The method according to one of the preceding claims, wherein the first solution is added to the second solution at an adding temperature of less than 120 °C.

15. The method according to one of the preceding claims, wherein the method is a method for producing a plurality of nanocrystals, wherein the plurality of nanocrystals is monodisperse .

16. A method for producing a nanocrystal (1) , the method comprising- providing a first solution comprising an elemental chalcogen and a first aliphatic amine ,- heating the first solution to a temperature above 50 ° C,- adding the first solution to a second solution comprising a heavy metal halide and a second aliphatic amine , wherein a precursor molar ratio of the heavy metal to the elemental chalcogen is less than 24 : 1 , and a first excitonic absorption hal f width at hal f maximum of the nanocrystal is less than 30 meV .17 . The method according to claim 16 , further comprising holding the first solution at a hold temperature of at least 50 ° C for a hold time of at least 10 minutes .18 . The method according to one of the claims 16 or 17 , wherein the second solution further comprises an alkene .

Citation Information

Patent Citations

  • Blends of polyesters and polysaccharides

    US62634969P0