Semiconductor apparatus and electronic device

By using vertical projection structures and Schottky contact electrodes in semiconductor devices, the electric field is used to increase carrier collision ionization, solving the problem of high sub-threshold swing and achieving low power consumption and high conduction effects.

WO2024222037A1PCT designated stage expired Publication Date: 2024-10-31HUAWEI TECH CO LTD
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
PCT/CN2024/070423
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-04-25
Filing Date
2024-01-03
Publication Date
2024-10-31

AI Technical Summary

Technical Problem

The sub-threshold swing (SS) of existing semiconductor devices is too high, resulting in high operating voltage and power consumption, making it difficult to effectively reduce leakage current.

Method used

Design a semiconductor device that adopts a vertically projected gate and active layer overlapping structure to form a Schottky junction through the first Schottky contact electrode and the active layer. The synergistic effect of the external electric field and the built-in electric field is used to increase the load capacity. The probability of flow collision and ionization achieves avalanche breakdown, thereby lowering the potential barrier of the channel and increasing the current flux.

Benefits of technology

It achieves rapid turning on of semiconductor devices at smaller voltages, reduces sub-threshold swing, reduces dynamic and static power consumption, and improves the conduction capability of the device.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN2024070423_31102024_PF_FP_ABST
    Figure CN2024070423_31102024_PF_FP_ABST
Patent Text Reader

Abstract

Disclosed in the embodiments of the present application are a semiconductor apparatus and an electronic device. The present application relates to the technical field of semiconductors, and is used for solving the technical problem of an excessively high SS of existing transistors. The semiconductor apparatus comprises a substrate, a gate electrode, an active layer and a first Schottky contact electrode, wherein the gate electrode, the active layer and the first Schottky contact electrode are all arranged on the substrate. The active layer comprises a channel portion, the vertical projection of the gate electrode on the substrate overlapping with the vertical projection of the channel portion on the substrate. The first Schottky contact electrode is in contact with the active layer, a first Schottky junction being formed therebetween. The portion of the active layer in contact with the first Schottky contact electrode has the same doping type as the channel portion. The semiconductor apparatus has a lower SS, so that the apparatus can be turned on simply by applying a very small voltage to the gate electrode.
Need to check novelty before this filing date? Find Prior Art

Description

Semiconductor device and electronic equipment

[0001] This application claims priority to the Chinese patent application filed with the State Intellectual Property Office on April 25, 2023, with application number 202310475059.5 and application name “A Semiconductor Device and Electronic Device”, the entire contents of which are incorporated by reference into this application. Technical Field

[0002] The present application relates to the field of semiconductor technology, and in particular to a semiconductor device and an electronic device. Background Art

[0003] As the feature size of semiconductor devices continues to shrink, the integration density of transistors increases, significantly improving performance and accelerating device operation. However, this is also accompanied by issues such as limited device operating voltage reduction and increased leakage current, leading to a serious power consumption problem for semiconductor devices.

[0004] Reducing the subthreshold swing (SS) of transistors helps lower the operating voltage of semiconductor devices while also maintaining or even reducing leakage current, effectively reducing both dynamic and static power consumption. However, SS currently cannot be lower than 60mV / dec at room temperature, resulting in high operating voltages and power consumption for semiconductor devices.

[0005] Summary of the Invention

[0006] The embodiments of the present application provide a semiconductor device and an electronic device for solving the technical problem of excessively high SS of existing transistors.

[0007] To achieve the above objectives, this application adopts the following technical solutions:

[0008] According to a first aspect of an embodiment of the present application, a semiconductor device is provided, comprising a substrate, a gate, an active layer, and a first Schottky contact electrode, wherein the gate, the active layer, and the first Schottky contact electrode are all disposed on the substrate. The active layer includes a channel portion, and a vertical projection of the gate on the substrate overlaps a vertical projection of the channel portion on the substrate. The first Schottky contact electrode contacts the active layer and forms a first Schottky junction with the active layer. The portion of the active layer in contact with the first Schottky contact electrode has the same doping type as the channel portion.

[0009] Thus, when a voltage is applied to the first Schottky contact electrode on one side of the channel portion and the active layer on the other side of the channel portion, an external electric field is applied to both ends of the channel portion. Since the metal and the semiconductor come into contact, the carriers within the metal and the semiconductor diffuse, forming a built-in electric field between the first Schottky contact electrode and the active layer. At this time, a first Schottky junction is formed at the interface between the first Schottky contact electrode and the active layer. Based on this, when the external electric field and the built-in electric field are in the same direction, the carriers within the first Schottky contact electrode and the active layer undergo collision ionization within the first Schottky junction, generating new carriers. At the same time, under the action of the electric field, the range of the first Schottky junction at the interface between the first Schottky contact electrode and the active layer continues to expand, thereby increasing the probability of collision ionization of carriers and ultimately causing avalanche breakdown.

[0010] Because the portion of the active layer in contact with the first Schottky contact electrode shares the same doping type as the channel, after the first Schottky junction undergoes avalanche breakdown, some carriers can enter the channel, raising its potential and lowering its potential barrier, allowing more carriers to flow through it. These carriers flowing through the channel then collide and ionize within the first Schottky junction, generating more carriers that raise the channel potential and lower its potential barrier. This creates a positive feedback mechanism within the semiconductor device, enabling it to turn on quickly with only a small voltage applied to the gate, resulting in a lower SS.

[0011] In some embodiments, the active layer is one or more of silicon, germanium, silicon germanium, gallium nitride, or indium gallium arsenide, with a thickness of 5-500 nm. The first Schottky contact electrode is one or more of silver, aluminum, magnesium, erbium, platinum, titanium, nickel, or cobalt. Thus, different metals have different work functions and can form Schottky junctions with different barrier heights when in contact with semiconductors of different materials. This allows the barrier height of the Schottky junction, and thus the degree of collisional ionization of carriers within the Schottky junction, to be regulated by the selection of metals and semiconductors.

[0012] In some embodiments, the active layer further includes a first semiconductor portion, which contacts the channel portion and has the same doping type as the channel portion. A first Schottky contact electrode is stacked with the active layer and located on a side of the active layer away from the substrate. The vertical projection of the first Schottky contact electrode on the substrate overlaps with the vertical projection of the first semiconductor portion on the substrate. Thus, the first semiconductor portion can be used to store new carriers generated by impact ionization within the first Schottky junction, thereby increasing the number of carriers entering the channel portion.

[0013] In some embodiments, the active layer further includes a first semiconductor portion, which contacts the channel portion and has the same doping type as the channel portion. A first Schottky contact electrode is disposed on the same surface of the substrate as the first semiconductor portion and contacts the substrate; the first Schottky contact electrode contacts a side surface of the first semiconductor portion. This allows the formation of a fin field-effect transistor (FinFET), further reducing leakage current and shortening the transistor's gate length.

[0014] In some embodiments, a semiconductor device includes at least two stacked active layers, two of which are a first active layer and a second active layer, respectively. The first active layer is disposed on and in contact with a substrate. The first active layer has a first channel portion, and the second active layer has a second channel portion. The first channel portion and the second channel portion are made of different semiconductor materials. Thus, by making the channel portion of the fin field-effect transistor of semiconductor materials with different band gaps, the voltage applied to the semiconductor device can be further reduced.

[0015] In some embodiments, the first Schottky contact electrode and the active layer are disposed on the same surface of the substrate and are in contact with the substrate. The first Schottky contact electrode is in contact with the channel portion. Thus, the first Schottky contact electrode can also be disposed directly on the substrate and in contact with the channel portion, thereby eliminating the first semiconductor portion.

[0016] In some embodiments, the active layer further includes a second semiconductor portion, which contacts the channel portion and has a different doping type than the channel portion. The first Schottky contact electrode and the second semiconductor portion are located on either side of the channel portion. Thus, a PN junction can be formed between the second semiconductor portion and the channel portion. Under the action of an electric field, the semiconductor device can thermally emit electrons through the PN junction toward the first Schottky junction.

[0017] In some embodiments, the active layer further includes a second semiconductor portion, which is in contact with the channel portion and has a different doping type from that of the channel portion. The first semiconductor portion and the second semiconductor portion are respectively located on either side of the channel portion, and are disposed on the same surface of the substrate and in contact with the substrate; the first Schottky contact electrode is coated on the top and both sides of the first semiconductor portion. At least one channel portion is connected between the first semiconductor portion and the second semiconductor portion, each channel portion is suspended above the substrate, and adjacent channel portions are spaced apart. In this way, a gate-all-around field-effect transistor (GAAFET) can be formed, further enhancing the gate's control capability over the channel portion and shortening the transistor's gate length.

[0018] In some embodiments, the semiconductor device further includes a first electrode and a second electrode. The first electrode is disposed on and in contact with the first Schottky contact electrode. The second electrode is coated on the top and both sides of the second semiconductor portion. Thus, a voltage can be applied to the semiconductor device via the first electrode and the second electrode.

[0019] In some embodiments, the first electrode and the second electrode are one or more of bismuth, aluminum, nickel, titanium, chromium, gold, silver, or metal silicide. Thus, different electrode metal materials can be selected according to the different polarities of the first electrode and the second electrode.

[0020] In some embodiments, the active layer further includes a second semiconductor portion, the second semiconductor portion being in contact with the channel portion and having the same doping type as the channel portion. The semiconductor device further includes a second Schottky contact electrode, which is stacked with the active layer and located on a side of the active layer away from the substrate, with the vertical projection of the second Schottky contact electrode on the substrate overlapping the vertical projection of the second semiconductor portion on the substrate. Thus, a second Schottky junction can be formed between the second semiconductor portion and the second Schottky contact electrode, and the semiconductor device can also thermally emit electrons through the second Schottky junction to the first Schottky junction.

[0021] In some embodiments, the semiconductor device further includes a second Schottky contact electrode. The second Schottky contact electrode is disposed on the same surface of the substrate as the active layer and is in contact with the substrate. The second Schottky contact electrode is in contact with the channel portion, and the first and second Schottky contact electrodes are located on either side of the channel portion. Thus, the second Schottky contact electrode can be disposed directly on the substrate and in contact with the channel portion, thereby eliminating the need for the second semiconductor portion.

[0022] In some embodiments, the active layer further includes a second semiconductor portion, the second semiconductor portion is in contact with the channel portion, and has a different doping type from the channel portion. The first Schottky contact electrode is a metal with a work function WF < 4.5 eV, and the second semiconductor portion is a metal with a doping concentration of 10 19 -10 21 cm -3 N-type semiconductor, the channel part is an intrinsic semiconductor or the doping concentration is 10 15 -10 17 cm -3 Thus, an N-type semiconductor device can be formed.

[0023] In some embodiments, the active layer further includes a second semiconductor portion, the second semiconductor portion is in contact with the channel portion, and has a different doping type from the channel portion. The first Schottky contact electrode is a metal with a work function WF ≥ 4.5 eV, and the second semiconductor portion is a metal with a doping concentration of 10 19 -1021 cm -3 P-type semiconductor, the channel part is an intrinsic semiconductor or the doping concentration is 10 15 -10 17 cm -3 Thus, a P-type semiconductor device can be formed.

[0024] In some embodiments, the semiconductor device further includes a gate oxide layer. The gate oxide layer is stacked between the active layer and the gate, with the vertical projection of the gate oxide layer on the substrate overlapping the vertical projection of the channel portion on the substrate. Thus, the gate oxide layer can effectively control current flow, preventing excessive current from causing overheating or short circuiting of the device.

[0025] In some embodiments, the gate is made of one or more of polysilicon, metal, or a composite structure of polysilicon and metal, and has a thickness of 10-500 nm. The gate oxide is made of one or more of silicon dioxide, aluminum oxide, or hafnium oxide, and has a thickness of 1-30 nm. Therefore, to effectively suppress short channel effects, different gate and gate oxide materials and thicknesses can be selected based on different feature sizes.

[0026] In some embodiments, the substrate is a bulk substrate, with the active layer disposed on top of the bulk substrate and integrally formed with the bulk substrate. Alternatively, the substrate includes a top semiconductor, a buried oxide layer, and a back substrate, with the buried oxide layer disposed between the top semiconductor and the back substrate, and the active layer disposed within the top semiconductor. Thus, depending on the processing technology of the semiconductor device, a bulk substrate or a substrate-on-insulator structure can be selected.

[0027] In some embodiments, the substrate is one or more of silicon, germanium, silicon germanium, gallium nitride, or indium gallium arsenide. The buried oxide layer is one or more of silicon dioxide, aluminum oxide, or hafnium oxide, and has a thickness of 10-1000 nm. Thus, substrates of different materials and thicknesses can be selected based on the different electrical properties of the device.

[0028] In some embodiments, the semiconductor device further includes two sidewall spacers disposed on either side of the gate. One sidewall spacer is proximal to the first Schottky contact electrode, while the other sidewall spacer is distal to the first Schottky contact electrode. Thus, the provision of the sidewall spacers can prevent short circuits between the gate and the first Schottky contact electrode, the first electrode, and the second electrode.

[0029] In some embodiments, the sidewall spacers are made of one or more of silicon dioxide, silicon nitride, silicon oxycarbon nitride (SiOCN), and silicon boron carbon nitride (SiBCN), and have a thickness of 10-1000 nm. Therefore, different sidewall spacer materials can be used corresponding to the materials of the first Schottky contact electrode, the first electrode, and the second electrode.

[0030] A second aspect of the present application provides an electronic device comprising a circuit board and a semiconductor device according to any one of the first aspects, wherein the semiconductor device is electrically connected to the circuit board. Thus, the semiconductor device has the same technical effects as the semiconductor device according to the first aspect, and will not be further described here.

[0031] A third aspect of the embodiments of the present application provides a method for fabricating a semiconductor device, comprising: forming a channel portion of an active layer on a substrate; forming a first Schottky contact electrode on the substrate, the first Schottky contact electrode in contact with the active layer, and the portion of the active layer in contact with the first Schottky contact electrode having the same doping type as the channel portion; and forming a first Schottky junction between the first Schottky contact electrode and the active layer. Forming a gate on the active layer, the vertical projection of the gate on the substrate overlapping the vertical projection of the channel portion on the substrate. Thus, using the fabrication method provided in the third aspect, a transistor with low SS can be fabricated. BRIEF DESCRIPTION OF THE DRAWINGS

[0032] FIG1 is a schematic structural diagram of an electronic device provided in an embodiment of the present application;

[0033] FIG2 is a schematic cross-sectional view of a semiconductor device according to an embodiment of the present application;

[0034] FIG3 is a schematic diagram of the cross-sectional structure of FIG2 when the active layer is not etched;

[0035] FIG4 is a diagram showing the working principle of the semiconductor device in FIG2 when it is an N-type semiconductor;

[0036] FIG5 is an energy band diagram of the semiconductor device in FIG4 ;

[0037] FIG6 is a schematic diagram of the positive feedback mechanism of the semiconductor device in FIG4 ;

[0038] FIG7A is a schematic diagram showing a comparison between a semiconductor device provided by an embodiment of the present application and the prior art;

[0039] FIG7B is a schematic diagram of a SS of a semiconductor device provided in an embodiment of the present application;

[0040] FIG7C is a schematic diagram of SS of a semiconductor device with different channel materials provided by an embodiment of the present application;

[0041] FIG8 is a diagram showing the working principle of the semiconductor device in FIG2 when it is a P-type semiconductor;

[0042] FIG9 is a schematic cross-sectional view of a semiconductor device according to another embodiment of the present application;

[0043] FIG10 is a schematic cross-sectional view of a semiconductor device according to another embodiment of the present application;

[0044] FIG11 is a schematic cross-sectional view of a semiconductor device according to another embodiment of the present application;

[0045] FIG12A is a top view of the semiconductor device in FIG2;

[0046] FIG12B is a first cross-sectional view taken along line AA of the semiconductor device in FIG12A;

[0047] FIG12C is a BB cross-sectional view 1 of the semiconductor device in FIG12A;

[0048] FIG13A is a second top view of the semiconductor device in FIG2;

[0049] FIG13B is a second AA cross-sectional view of the semiconductor device in FIG13A;

[0050] FIG13C is a second BB cross-sectional view of the semiconductor device in FIG13A;

[0051] FIG14A is a third top view of the semiconductor device in FIG2;

[0052] FIG14B is a third AA cross-sectional view of the semiconductor device in FIG14A;

[0053] FIG14C is a third BB cross-sectional view of the semiconductor device in FIG14A;

[0054] FIG15A is a top view 4 of the semiconductor device in FIG2;

[0055] FIG15B is a fourth AA cross-sectional view of the semiconductor device in FIG15A;

[0056] FIG15C is a CC cross-sectional view 4 of the semiconductor device in FIG15A;

[0057] FIG16A is a top view 5 of the semiconductor device in FIG2;

[0058] FIG16B is a fifth AA cross-sectional view of the semiconductor device in FIG16A;

[0059] FIG16C is a CC cross-sectional view 5 of the semiconductor device in FIG16A;

[0060] FIG17A is a top view of the semiconductor device in FIG2;

[0061] FIG17B is a sixth AA cross-sectional view of the semiconductor device in FIG17A;

[0062] FIG18A is a top view of the semiconductor device in FIG2;

[0063] FIG18B is a seventh AA cross-sectional view of the semiconductor device in FIG18A;

[0064] FIG18C is a CC cross-sectional view VII of the semiconductor device in FIG18A;

[0065] FIG19A is a top view of the semiconductor device in FIG2;

[0066] FIG19B is a cross-sectional view taken along line AA of the semiconductor device in FIG19A;

[0067] FIG19C is a BB cross-sectional view 8 of the semiconductor device in FIG19A;

[0068] FIG20A is a top view of another semiconductor device being prepared;

[0069] FIG20B is a cross-sectional view taken along line AA of the semiconductor device in FIG20A;

[0070] FIG20C is a BB cross-sectional view of the semiconductor device in FIG20A;

[0071] FIG21 is a perspective view of a FinFET provided in an embodiment of the present application;

[0072] FIG22A is a schematic structural diagram of an embodiment of the active layer in FIG21 ;

[0073] FIG22B is a second schematic structural diagram of an embodiment of the active layer in FIG21 ;

[0074] FIG22C is a third structural diagram of an embodiment of the active layer in FIG21;

[0075] FIG22D is a fourth structural diagram of an embodiment of the active layer in FIG21;

[0076] FIG22E is a fifth structural diagram of an embodiment of the active layer in FIG21 ;

[0077] FIG22F is a sixth structural diagram of an embodiment of the active layer in FIG21;

[0078] FIG22G is a seventh structural diagram of an embodiment of the active layer in FIG21;

[0079] FIG22H is a schematic structural diagram of an embodiment of the active layer in FIG21 8;

[0080] FIG23 is a schematic diagram of SS of different channel widths of the semiconductor device in FIG21;

[0081] FIG24 is a perspective view of a gate-all-around field-effect transistor provided in an embodiment of the present application;

[0082] FIG25 is a perspective view of the first step of preparing the semiconductor device in FIG24;

[0083] FIG26 is a second perspective view of the preparation of the semiconductor device in FIG24;

[0084] FIG27 is a third perspective view of the preparation of the semiconductor device in FIG24;

[0085] FIG28 is a perspective view of a fourth step in preparing the semiconductor device shown in FIG24;

[0086] FIG29 is a perspective view of a fifth step in preparing the semiconductor device in FIG24;

[0087] FIG30 is a perspective view of the sixth step of preparing the semiconductor device in FIG24;

[0088] FIG31 is a perspective view showing the seventh step of preparing the semiconductor device in FIG24;

[0089] FIG32 is a perspective view of the semiconductor device of FIG24;

[0090] FIG33 is a perspective view of the semiconductor device of FIG24;

[0091] FIG34 is a perspective view of the semiconductor device of FIG24;

[0092] FIG35 is a perspective view 11 of the preparation of the semiconductor device in FIG24;

[0093] FIG36 is a perspective view 12 of the preparation of the semiconductor device in FIG24;

[0094] FIG37 is a perspective view 13 of the preparation of the semiconductor device in FIG24;

[0095] FIG38 is a fourteenth perspective view of the semiconductor device in FIG24. DETAILED DESCRIPTION

[0096] In order to make the purpose, technical solutions and advantages of this application clearer, this application will be further described in detail below with reference to the accompanying drawings.

[0097] Hereinafter, the terms "first," "second," etc., are used for descriptive purposes only and should not be construed as indicating or implying relative importance or implicitly specifying the number of the technical features being referred to. Thus, a feature identified with "first," "second," etc., may explicitly or implicitly include one or more of the features. In the description of this application, unless otherwise specified, "plurality" means two or more.

[0098] In addition, in this application, directional terms such as "upper" and "lower" are defined relative to the orientation of the components in the drawings. It should be understood that these directional terms are relative concepts. They are used for relative description and clarification, and they can change accordingly according to changes in the orientation of the components in the drawings.

[0099] The present application provides an electronic device. The electronic device may be a tablet computer, a mobile phone, an e-reader, a remote control, a personal computer (PC), a laptop computer, a personal digital assistant (PDA), an in-vehicle device, an Internet-connected television, a wearable device, a television, or other products with a display interface, as well as smart display wearable products such as smart watches and smart bracelets.

[0100] As shown in FIG1 , the electronic device 01 may include a semiconductor device 100 and a printed circuit board (PCB) 300. The semiconductor device 100 may be electrically connected to the PCB 300 via a connection structure 200. For example, the connection structure 200 may be a ball grid array (BGA) or a copper pillar bump. Furthermore, the semiconductor device 100 may be a chip package structure, which may include a package substrate and at least one bare chip (die) disposed on the package substrate. The bare chip may be electrically connected to the PCB 300 via the package substrate and the connection structure 200.

[0101] Based on this, the semiconductor device 100 may include at least one of a central processing unit (CPU), a graphics processing unit (GPU), a field programmable gate array (FPGA), or a microcontroller unit (MCU). The embodiment of the present application does not impose any special restrictions on the specific type of the semiconductor device 100. The above-mentioned bare chip in the semiconductor device 100 may include a plurality of transistors, such as field effect transistors. The above-mentioned plurality of transistors may be connected to form a corresponding functional circuit so that the semiconductor device 100 can realize its corresponding function. The specific structure of the semiconductor device 100 having the above-mentioned field effect transistor is illustrated below.

[0102] As shown in FIG2 , an embodiment of the present application provides a semiconductor device 100. Semiconductor device 100 may include a substrate 110, a gate 120, an active layer 130, and a first Schottky contact electrode 140. Active layer 130 may include a first semiconductor portion 131, a second semiconductor portion 132, and a channel portion 133. Gate 120, active layer 130, and first Schottky contact electrode 140 may all be disposed on substrate 110.

[0103] As shown in Figure 2, the first semiconductor portion 131 is in contact with the substrate 110, and the first Schottky contact electrode 140 is stacked on the surface of the first semiconductor portion 131 away from the substrate 110. At this time, the energy band of the semiconductor is bent at the interface between the first semiconductor portion 131 and the first Schottky contact electrode 140, forming a Schottky barrier. The interface between metal and semiconductor is called a Schottky junction. Therefore, when the first Schottky contact electrode 140 contacts the first semiconductor portion 131, a first Schottky junction 141 can be formed.

[0104] In some embodiments, the active layer 130 can be made of one or more semiconductor materials such as silicon (Si), germanium (Ge), silicon germanium (SiGe), gallium nitride (GaN), or indium gallium arsenide (InGaAs). The thickness of the active layer 130 can be set to 5-500 nm. This can prevent low switching current while ensuring carrier mobility within the active layer 130. The first Schottky contact electrode 140 can be made of one or more metals such as silver (Ag), aluminum (Al), magnesium (Mg), erbium (Er), platinum (Pt), titanium (Ti), nickel (Ni), or cobalt (Co).

[0105] In addition, platinum (Pt), erbium (Er), titanium (Ti), nickel (Ni), or cobalt (Co) can be annealed with silicon to form a silicide, which can also be used as the first Schottky contact electrode 140. The embodiment of the present application does not impose any particular restrictions on the specific materials and thicknesses of the active layer 130 and the first Schottky contact electrode 140.

[0106] On this basis, as shown in FIG2 , the first semiconductor portion 131, the second semiconductor portion 132, and the channel portion 133 can be provided on the same side surface of the substrate 110 and all contact the surface of the substrate 110. The gate 120 can be provided on a surface of the channel portion 133 away from the substrate 110 and contact the channel portion 133. At the same time, the vertical projection of the gate 120 on the substrate 110 overlaps with the vertical projection of the channel portion 133 on the substrate 110.

[0107] The first semiconductor portion 131 can have the same doping type as the channel portion 133, and the doping concentrations of the first semiconductor portion 131 and the channel portion 133 can be the same or different. The second semiconductor portion 132 can have a different doping type than the channel portion 133, thereby forming a PN junction 134 between the second semiconductor portion 132 and the channel portion 133. The embodiments of the present application do not impose any particular restrictions on the doping concentrations of the first semiconductor portion 131, the second semiconductor portion 132, and the channel portion 133.

[0108] 2 , the semiconductor device 100 may further include a gate oxide layer 150 . The gate oxide layer 150 may be stacked between the active layer 130 and the gate 120 . A vertical projection of the gate oxide layer 150 on the substrate 110 may overlap with a vertical projection of the channel portion 133 on the substrate 110 .

[0109] Among them, the gate 120 can be made of one or more of polysilicon, metal or a composite structure of polysilicon and metal, and the thickness of the gate 120 can be set to 10-500nm to ensure that the gate 120 can provide sufficient electric field strength when the device is turned on. The gate oxide layer 150 can be made of one or more insulating materials such as silicon dioxide (SiO2), aluminum oxide (Al2O3) or hafnium oxide (HfO2), and the thickness of the gate oxide layer 150 can be set to 1-30nm. The use of materials with high dielectric constants can effectively reduce the thickness of the gate oxide layer 150, but it is also necessary to avoid the tunneling effect of carriers. The embodiment of the present application does not impose any special restrictions on the specific materials and thicknesses of the gate 120 and the gate oxide layer 150.

[0110] Before the active layer 130 is photolithographically or etched, as shown in FIG3 , the substrate 110 may include a top semiconductor layer 111, a buried oxide layer 112, and a back substrate 113. The buried oxide layer 112 may be disposed between the top semiconductor layer 111 and the back substrate 113, and the top semiconductor layer 111 may be photolithographically or etched to form the active layer 130.

[0111] Among them, the top semiconductor 111 and the back substrate 113 can be made of one or more semiconductor materials such as silicon (Si), germanium (Ge), silicon germanium (SiGe), gallium nitride (GaN) or indium gallium arsenide (InGaAs). The materials of the top semiconductor 111 and the back substrate 113 can be the same or different. The buried oxide layer 112 can be made of one or more insulating materials such as silicon dioxide (SiO2), aluminum oxide (Al2O3) or hafnium oxide (HfO2). The thickness of the buried oxide layer 112 can be set to 10-1000nm to ensure good deformation resistance of the device and to provide good support for the active layer. The embodiment of the present application does not impose any special restrictions on the specific materials and thicknesses of the top semiconductor 111, the buried oxide layer 112 and the back substrate 113.

[0112] On this basis, as shown in FIG3 , the semiconductor device 100 may further include a first electrode 171, a second electrode 172, a third electrode 173, and a fourth electrode 174. The first electrode 171 is provided on the first Schottky contact electrode 140 (shown in FIG2 ) and contacts the surface of the first Schottky contact electrode 140 away from the substrate 110. The second electrode 172 is provided on the second semiconductor portion 132 (shown in FIG2 ) and contacts the surface of the second semiconductor portion 132 away from the buried oxide layer 112. The third electrode 173 is provided on the gate 120 (shown in FIG2 ) and contacts the surface of the gate 120 away from the substrate 110. The fourth electrode 174 is provided on the back substrate 113 and contacts the surface of the back substrate 113 away from the buried oxide layer 112.

[0113] In addition, the first electrode 171, the second electrode 172, the third electrode 173, and the fourth electrode 174 can be made of one or more of bismuth (Bi), aluminum (Al), nickel (Ni), titanium (Ti), chromium (Cr), gold (Au), silver (Ag), or metal silicide. The embodiments of the present application do not impose any particular restrictions on the specific materials and thicknesses of the first electrode 171, the second electrode 172, the third electrode 173, and the fourth electrode 174.

[0114] On this basis, as shown in FIG3 , the semiconductor device 100 may further include two sidewall spacers 160 , which may be disposed on either side of the third electrode 173 and the gate 120 (shown in FIG2 ). One of the sidewall spacers 160 is located between the first Schottky contact electrode 140 (shown in FIG2 ) and the gate 120 , and also between the first electrode 171 and the third electrode 173 , thereby preventing a short circuit between the first Schottky contact electrode 140 and the gate 120 , and also between the first electrode 171 and the third electrode 173 . The other sidewall spacer 160 is located between the second electrode 172 and the gate 120 , thereby preventing a short circuit between the second electrode 172 and the gate 120 .

[0115] The sidewall spacer 160 can be made of one or more insulating materials such as silicon dioxide (SiO2), silicon nitride (Si3N4), silicon oxycarbon nitride (SiOCN), and silicon boron carbon nitride (SiBCN). The thickness of the sidewall spacer 160 can be set to 10-1000 nm, which can effectively protect the gate 120 and the gate oxide layer 150. The specific material and thickness of the sidewall spacer 160 are not particularly limited in this embodiment of the application.

[0116] The above is a detailed description of the specific structure of the semiconductor device 100 provided in the embodiment of the present application. In order to better understand how to reduce the SS of the semiconductor device 100, the working principle of the semiconductor device 100 provided in the embodiment of the present application will be described in detail below.

[0117] As a specific embodiment, the first Schottky contact electrode 140 may be made of a metal with a work function WF < 4.5 eV. The second semiconductor portion 132 may be made of a metal with a doping concentration of 10 19 -10 21 cm -3 The first semiconductor portion 131 and the channel portion 133 can be made of an intrinsic semiconductor or a heavily doped N-type semiconductor. 15 -10 17 cm -3 At this time, the semiconductor device 100 can form an N-type semiconductor device.

[0118] When the semiconductor device 100 is an N-type semiconductor device, in the first aspect, as shown in FIG4 , the first Schottky contact electrode 140 can be connected to the positive electrode of the power supply via the first electrode 171 (shown in FIG3 ), that is, the first electrode 171 serves as the drain of the device; and the second semiconductor portion 132 can be connected to the negative electrode of the power supply via the second electrode 172 (shown in FIG3 ), that is, the second electrode 172 serves as the source of the device. In this case, the direction of the external electric field is shown by the solid arrow in the figure, that is, a positive voltage is applied to the first Schottky contact electrode 140, and a negative voltage is applied to the second semiconductor portion 132.

[0119] As shown in FIG4 , when the first semiconductor portion 131 is a weakly P-type doped semiconductor and the second semiconductor portion 132 is a heavily N-type doped semiconductor, the free electrons in the PN junction 134 flow from the second semiconductor portion 132 to the first semiconductor portion 131, causing the built-in electric field of the PN junction 134 to be directed from the second semiconductor portion 132 to the first semiconductor portion 131 (in the direction of the dotted arrow of the PN junction 134 in the figure). Therefore, the direction of the built-in electric field of the PN junction 134 is opposite to the direction of the external electric field. Under the action of the external electric field, the PN junction 134 becomes narrower in the direction of the dotted arrow, allowing the free electrons in the second semiconductor portion 132 to be thermally emitted toward the first semiconductor portion 131.

[0120] Secondly, as shown in FIG4 , when the work function of the first Schottky contact electrode 140 is low (for example, when the first semiconductor portion 131 is a weakly doped P-type semiconductor and the first Schottky contact electrode 140 is aluminum (Al) with a temperature of 4.28 eV), free electrons within the first Schottky junction 141 flow from the first Schottky contact electrode 140 to the first semiconductor portion 131, causing the direction of the built-in electric field of the first Schottky junction 141 to be from the first Schottky contact electrode 140 to the first semiconductor portion 131 (in the direction of the dotted arrow of the first Schottky junction 141 in the figure). Therefore, the direction of the external electric field is the same as the direction of the built-in electric field of the first Schottky junction 141, allowing impact ionization of carriers within the first Schottky junction 141.

[0121] Under the action of the external electric field, the length of the first Schottky junction 141 increases in the direction of the dotted arrow in Figure 4, thereby increasing the range of the first Schottky junction 141. This increases the probability of collision ionization of carriers within the first Schottky junction 141, ultimately leading to avalanche breakdown. As shown in Figure 5, after avalanche breakdown, the free electrons ionized by collision within the first Schottky junction 141 are collected in the first Schottky contact electrode 140, while the holes enter the channel portion 133, raising the potential of the channel portion 133 and lowering the potential barrier of the channel portion 133.

[0122] As shown in the right figure of Figure 6, when holes enter the channel portion 133, the potential barrier of the channel portion 133 is lowered from the dotted line position to the solid line position. As a result, when the potential barrier of the channel portion 133 is lowered, more carriers will flow from the channel portion 133 to the first Schottky junction 141 in the second semiconductor portion 132 (indicated by the thick arrow in the figure). These carriers flowing through the channel portion 133 continue to collide and ionize within the first Schottky junction 141, generating more holes, which increase the potential of the channel portion 133 and lower the potential barrier of the channel portion 133 (indicated by the short arrow in the figure).

[0123] In this way, as shown in FIG6 , a positive feedback mechanism is formed: carriers collide and ionize in the first Schottky junction 141 → the generated holes flow into the channel portion 133 → the holes reduce the potential barrier of the channel portion 133 → the carriers in the second semiconductor portion 132 flow into the first Schottky junction 141. At this time, the semiconductor device 100 can be quickly turned on by applying a very small voltage to the gate 120 through the third electrode 173. This achieves the function of causing the current between the source and the drain to change by an order of magnitude with only a very small change in the gate voltage. In this way, the semiconductor device 100 has better gate control capability and can reduce the SS of the semiconductor device 100 to below 60mV / dec.

[0124] If the horizontal axis represents the voltage applied to the gate (i.e., the operating voltage), and the vertical axis represents the current detected by the drain. As shown in Figure 7A, when the vertical axis reaches the maximum current, the device turns on. The current at this time is the on-state current of the device, and the voltage at this time is the threshold voltage. As can be seen from the figure, the Metal Oxide Semiconductor Field Effect Transistor (MOSFET) (curve ① in the figure) requires a larger threshold voltage to turn on the device, that is, the volt-ampere curve of the MOSFET is not steep enough. In addition, it can be seen from the intercept of the vertical axis that the leakage current of the MOSFET is large.

[0125] As shown in Figure 7A, the tunneling field effect transistor (TFET) (curve ② in the figure) has a steep volt-ampere curve (i.e., a small threshold voltage) and a small intercept on the vertical axis (i.e., a small leakage current), but due to the low probability of electron tunneling, the on-state current after the device is turned on is difficult to meet actual needs, that is, the on-state current of the TFET is not as large as the on-state current of the MOSFET.

[0126] As shown in FIG7A , a negative-capacitance Field Effect Transistor (NC-FET) (curve ③ in the figure) and a zero subthreshold swing and zero impact ionization Field Effect Transistor (Z 2 -FET) (curve ④ in the figure) has a large hysteresis effect (the rectangular area between curves ③ and ④ in the figure), which is not conducive to the timely transmission of signals.

[0127] As shown in FIG7A , the impact ionization metal oxide semiconductor field effect transistor (I-MOSFET) (curve ⑤ in the figure) requires a very high operating voltage to reach the on-state current, and the strong electric field may also cause hot electron injection and lead to degradation of the gate dielectric.

[0128] As shown in FIG7A , the field-effect transistor provided in the embodiment of the present application has a first Schottky contact electrode 140 comprising a metal or metal silicide disposed between the first electrode 171 (drain) and the first semiconductor portion 131. Therefore, the field-effect transistor provided in the embodiment of the present application is referred to as a field-effect transistor with a metal drain region (MD-MOSFET) (curve 6 in the figure). MD-MOSFETs can be applied to planar field-effect transistors (PFETs).

[0129] As shown in Figure 7A, when the operating voltage is zero, the potential barrier of the first Schottky junction 141 blocks carriers, resulting in very low drain leakage current. This means the MD-MOSFET has a small intercept on the vertical axis. When a very low voltage is applied to the gate 120, the semiconductor device 100 can undergo thermal emission of free electrons at the source and collisional ionization of carriers at the drain, allowing it to turn on quickly. This results in a steep volt-ampere curve for the MD-MOSFET. Furthermore, the on-state current after turn-on is relatively high, improving the conduction capability of the semiconductor device 100.

[0130] Combined with the data, as shown in FIG7B , the semiconductor device 100 provided in the embodiment of the present application can cause the drain current to jump from 1e-10 to 1e-6 at a voltage of less than 0.3 V. This enables the semiconductor device 100 to achieve an ultra-steep current jump of 3-4 orders of magnitude under very low operating voltage conditions, achieving an ultra-steep SS of the semiconductor device 100 and reducing the SS of the semiconductor device 100.

[0131] Furthermore, the channel of semiconductor device 100 can be made of different materials. As shown in FIG7C , curve 7 represents a semiconductor channel material composed of 85% silicon and 15% germanium, curve 8 represents a semiconductor channel material composed of 90% silicon and 10% germanium, and curve 9 represents an intrinsic semiconductor channel material. The energy gaps of the three channel materials are: curve 7 < curve 8 < curve 9. Therefore, as can be seen from the figure, as the energy gap of the channel material decreases, the operating voltage of the gate (i.e., the horizontal axis where the curve begins to enter the ultra-steep state) also gradually decreases.

[0132] As another specific embodiment, in contrast to the N-type semiconductor device, the first Schottky contact electrode 140 may be made of a metal with a work function WF ≥ 4.5 eV. The second semiconductor portion 132 may be made of a metal with a doping concentration of 10 19 -10 21 cm -3 The first semiconductor portion 131 and the channel portion 133 can be made of an intrinsic semiconductor or a P-type heavily doped semiconductor with a doping concentration of 10 15 -10 17 cm -3 At this time, the semiconductor device 100 can form a P-type semiconductor device.

[0133] When semiconductor device 100 is a P-type semiconductor device, in a first aspect, as shown in FIG8 , first Schottky contact electrode 140 can be connected to the negative pole of a power source via first electrode 171, i.e., first electrode 171 serves as the drain of the device; and second semiconductor portion 132 can be connected to the positive pole of a power source via second electrode 172, i.e., second electrode 172 serves as the source of the device. In this case, the direction of the external electric field is indicated by the solid arrow in the figure, i.e., a negative voltage is applied to first Schottky contact electrode 140, and a positive voltage is applied to second semiconductor portion 132.

[0134] As shown in FIG8 , when the first semiconductor portion 131 is a weakly N-type doped semiconductor and the second semiconductor portion 132 is a heavily P-type doped semiconductor, the free electrons in the PN junction 134 flow from the first semiconductor portion 131 to the second semiconductor portion 132, causing the built-in electric field of the PN junction 134 to be directed from the first semiconductor portion 131 to the second semiconductor portion 132 (in the direction of the dotted arrow of the PN junction 134 in the figure). Therefore, the direction of the built-in electric field of the PN junction 134 is still opposite to the direction of the external electric field. Under the action of the external electric field, the PN junction 134 continues to narrow in the direction of the dotted arrow, allowing the holes in the second semiconductor portion 132 to be thermally emitted toward the first semiconductor portion 131.

[0135] Secondly, as shown in FIG8 , when the work function of the first Schottky contact electrode 140 is high (for example, when the first semiconductor portion 131 is a weakly N-type doped semiconductor and the first Schottky contact electrode 140 is platinum (Pt) with a temperature of 5.65 eV), free electrons within the first Schottky junction 141 flow from the first semiconductor portion 131 toward the first Schottky contact electrode 140, causing the direction of the built-in electric field of the first Schottky junction 141 to be from the first semiconductor portion 131 to the first Schottky contact electrode 140 (in the direction of the dotted arrow of the first Schottky junction 141 in the figure). Therefore, the direction of the external electric field is the same as the direction of the built-in electric field of the first Schottky junction 141, allowing impact ionization of carriers within the first Schottky junction 141.

[0136] Under the influence of an external electric field, the length of the first Schottky junction 141 increases in the direction of the dashed arrow in FIG8 , thereby increasing the area of ​​the first Schottky junction 141 and thereby increasing the probability of collisional ionization of carriers within the first Schottky junction 141 , ultimately leading to avalanche breakdown. Similar to the aforementioned N-type semiconductor device, after avalanche breakdown, the holes ionized by collision within the first Schottky junction 141 are collected within the first Schottky contact electrode 140 , while free electrons enter the channel portion 133 , raising the potential of the channel portion 133 and lowering the potential barrier of the channel portion 133 . Similarly, carriers flowing through the channel portion 133 continue to undergo collisional ionization within the first Schottky junction 141 , generating more free electrons that raise the potential of the channel portion 133 and lower the potential barrier of the channel portion 133 . This creates a positive feedback mechanism within the semiconductor device 100 , thereby reducing the SS of the semiconductor device 100 .

[0137] The above is the specific structure of the N-type semiconductor device and the P-type semiconductor device provided in the embodiments of the present application. On this basis, other improvements can be made to the semiconductor device 100. For example, in some embodiments, the drain side of the semiconductor device 100 can be entirely set to metal. Specifically, as shown in Figure 9, the first Schottky contact electrode 140, the second semiconductor portion 132 and the channel portion 133 can be set on the same surface of the substrate 110, and all are in contact with the substrate 110. Among them, the first Schottky contact electrode 140 is in contact with the channel portion 133. As a result, the setting of the first semiconductor portion 131 can be cancelled.

[0138] Based on the operating principle of the semiconductor device 100 described above, the provision of the first semiconductor portion 131 has two benefits. First, during the fabrication of the semiconductor device 100, the first semiconductor portion 131 can be eliminated by photolithography, thereby simplifying the fabrication process. Second, the provision of the first semiconductor portion 131 facilitates the storage of impact-ionized carriers, allowing more carriers to enter the channel portion 133, thereby increasing the potential of the channel portion 133 and lowering the potential barrier of the channel portion 133. However, eliminating the first semiconductor portion 131 can also reduce the SS of the semiconductor device 100.

[0139] In other embodiments, as shown in FIG10 , the source side of the semiconductor device 100 may also be configured as a structure in which metal and semiconductor are in contact. In this case, the doping type of the second semiconductor portion 132 needs to be set to be the same as the doping type of the channel portion 133, that is, the doping type of the first semiconductor portion 131, the second semiconductor portion 132, and the channel portion 133 are all the same.

[0140] In addition, as shown in FIG10 , a second Schottky contact electrode 180 is stacked on the surface of the second semiconductor portion 132 away from the substrate 110. The vertical projection of the second Schottky contact electrode 180 on the substrate 110 overlaps with the vertical projection of the second semiconductor portion 132 on the substrate 110. When the semiconductor device 100 is an N-type device, the second Schottky contact electrode 180 may be made of a metal with a work function WF < 4.5 eV. When the semiconductor device 100 is a P-type device, the second Schottky contact electrode 180 may be made of a metal with a work function WF ≥ 4.5 eV. Of course, the first Schottky contact electrode 140 and the second Schottky contact electrode 180 may be made of the same metal material.

[0141] In this way, because the polarity of the power supply connected to the drain and source is different, when a voltage is applied to the semiconductor device 100, thermal emission of source carriers and impact ionization of drain carriers can also be achieved. At the same time, the entire active layer 130 is composed of a single type of lightly doped semiconductor material, eliminating the need for ion implantation in the active layer 130, further simplifying the manufacturing process of the semiconductor device 100.

[0142] In some other embodiments, the entire source side of the semiconductor device 100 can be set to metal. Specifically, as shown in Figure 11, the first Schottky contact electrode 140, the channel portion 133, and the second Schottky contact electrode 180 can be set on the same surface of the substrate 110 and all contact the substrate 110. Among them, the second Schottky contact electrode 180 contacts the channel portion 133, and the first Schottky contact electrode 140 and the second Schottky contact electrode 180 are respectively located on both sides of the channel portion 133. As a result, the second semiconductor portion 132 can be eliminated.

[0143] To obtain the semiconductor device 100 in the above embodiment, the present application also provides a manufacturing method. The following detailed description will be given using the manufacturing of an N-type semiconductor device as an example. As shown in FIG12A , a substrate 110 is selected. The substrate 110 may have a length direction and a width direction as shown in the figure. The length direction described below is the same as the length direction of the substrate 110, and the width direction described below is the same as the width direction of the substrate 110. AA is a cross-sectional view along the length direction, and BB is a cross-sectional view along the width direction.

[0144] As shown in FIG12B , the substrate 110 may include a stacked top semiconductor layer 111, a buried oxide layer 112, and a back substrate 113. The buried oxide layer 112 is located on and in contact with the back substrate 113. The top semiconductor layer 111 is located on and in contact with the buried oxide layer 112.

[0145] As shown in FIG. 12C , the top semiconductor layer 111 , the buried oxide layer 112 and the back substrate 113 of the substrate 110 are all planar layered structures.

[0146] After the material selection is completed, as shown in FIG13A , a window of the top semiconductor 111 (shown in FIG12A ) can be opened by photolithography. Then, the top semiconductor 111 is etched using a photoresist as a mask to form an active layer 130. Etching can be performed using either a dry or wet method. Dry etching can use fluorine-based or halogen-based gases, such as sulfur hexafluoride (SF6), trifluoromethane (CHF3), hydrogen bromide (HBr), or chlorine (Cl2). Wet etching can use solutions such as tetramethylammonium hydroxide (TMAH) or potassium hydroxide (KOH).

[0147] 13B , the length of the active layer 130 after etching may be smaller than the length of the buried oxide layer 112. As shown in FIG13C , the width of the active layer 130 after etching may be smaller than the width of the buried oxide layer 112.

[0148] After the active layer 130 is formed, as shown in FIG14A , a gate electrode 120 can be deposited on the active layer 130 (shown in FIG13C ) by atomic layer deposition, thermal oxidation, or chemical vapor deposition. The vertical projection of the gate electrode 120 on the buried oxide layer 112 can be larger than the vertical projection of the active layer 130 on the buried oxide layer 112.

[0149] As shown in FIG14B , before depositing the gate 120, a gate oxide layer 150 may be deposited on the active layer 130 by methods such as atomic layer deposition, thermal oxidation, or chemical vapor deposition. The gate oxide layer 150 is located on and in contact with the active layer 130. The gate 120 is located on and in contact with the gate oxide layer 150. The gate 120, the active layer 130, and the gate oxide layer 150 have the same length.

[0150] As shown in FIG14C , the gate oxide layer 150 covers both sides and the top of the active layer 130 in the width direction of the active layer 130, and the gate oxide layer 150 also extends along the width direction of the active layer 130 to contact the buried oxide layer 112. The width of the gate 120 is the same as the width of the gate oxide layer 150.

[0151] After the gate 120 is deposited, as shown in FIG15A , the gate 120 and the gate oxide layer 150 can be etched so that the vertical projections of the gate 120 and the gate oxide layer 150 on the buried oxide layer 112 overlap with the vertical projections of the channel portion 133 (shown in FIG2 ) to be fabricated on the buried oxide layer 112. That is, the widths of the gate 120 and the gate oxide layer 150 are the same as the width of the channel portion 133.

[0152] 15B , the channel portion 133 is located below the gate 120 and the gate oxide layer 150, and the first semiconductor portion 131 and the second semiconductor portion 132 are located on either side of the channel portion 133. The BB cross-sectional view in FIG15A is the same as the BB cross-sectional view in FIG14C and will not be repeated here.

[0153] As shown in FIG. 15C , which is a CC cross-sectional view in FIG. 15A , at this time, the gate 120 and the gate oxide layer 150 still cover both sides and the top of the active layer 130 .

[0154] After the gate 120 is formed, as shown in FIG16A , a sidewall spacer 160 can be deposited on the gate 120 by chemical vapor deposition or atomic layer deposition. After the sidewall spacer 160 is deposited, etching can be performed to form the sidewall spacer 160 on both sides of the gate 120 and the gate oxide layer 150. The etching can be performed using an anisotropic dry etching process, and a fluorine-based gas such as sulfur hexafluoride (SF6) or trifluoromethane (CHF3) can be used for the dry etching.

[0155] 16B , on the active layer 130 , the bottom of the spacer 160 contacts the active layer 130 , and the top of the spacer 160 is flush with the top of the gate 120 . The BB cross-sectional view in FIG16A is the same as the BB cross-sectional view in FIG14C , and will not be repeated here.

[0156] As shown in FIG. 16C , which is a CC cross-sectional view in FIG. 16A , in the width direction of the spacer 160 of the active layer 130 , the spacer 160 is also in contact with the surface of the buried oxide layer 112 .

[0157] After the sidewall spacers 160 are formed, as shown in FIG17A , a window for ion implantation in the second semiconductor portion 132 region can be opened by photolithography. Ions are implanted into the window to form the heavily N-type doped second semiconductor portion 132. The remaining active layer 130 not implanted with ions becomes the first semiconductor portion 131 and the channel portion 133.

[0158] Among them, arsenic or phosphorus can be used for ion implantation, and the dosage can be 10 13 -10 16 cm -2 After the ion implantation, the ions can be activated by annealing. The annealing temperature can be between 900° C. and 1200° C., and the time can be between 1 microsecond and 10 seconds.

[0159] As shown in FIG17B , the first semiconductor portion 131 and the channel portion 133 are intrinsic semiconductors or weakly doped P-type semiconductors, and the second semiconductor portion 132 is a heavily doped N-type semiconductor. The BB cross-sectional view in FIG17A is the same as the BB cross-sectional view in FIG14C and will not be repeated here.

[0160] After the second semiconductor portion 132 is formed, as shown in FIG18A , a window in the first semiconductor portion 131 (shown in FIG17B ) can be opened by photolithography. Metal is deposited on top of the first semiconductor portion 131 within the window and annealed to form a first Schottky contact electrode 140. The vertical projection of the first Schottky contact electrode 140 on the buried oxide layer 112 overlaps with the vertical projection of the first semiconductor portion 131 on the buried oxide layer 112. Metal deposition can be performed using processes such as evaporation or physical vapor deposition, and the annealing temperature can be between 300°C and 900°C.

[0161] As shown in FIG18B , the first Schottky contact electrode 140 is arranged flat above the first semiconductor portion 131 and contacts the first semiconductor portion 131. Furthermore, the first Schottky contact electrode 140 is located on one side of the spacer 160, while the gate 120 and the gate oxide layer 150 are located on the other side of the spacer 160. The BB cross-sectional view in FIG18A is the same as the BB cross-sectional view in FIG14C and will not be described again here.

[0162] As shown in FIG. 18C , which is a CC cross-sectional view in FIG. 18A , the width of the first Schottky contact electrode 140 is the same as the width of the active layer 130 .

[0163] After the first Schottky contact electrode 140 is formed, as shown in FIG19A , metals can be deposited on the source, drain, and gate of the device and annealed to form a first electrode 171, a second electrode 172, and a third electrode 173. The metal deposition can be performed using processes such as evaporation or physical vapor deposition, and the annealing temperature can be between 300° C. and 900° C.

[0164] As shown in FIG19B , windows can be opened in the first Schottky contact electrode 140, the second semiconductor portion 132, the gate 120, and the back substrate 113 by photolithography. A first electrode 171 is deposited on the surface of the first Schottky contact electrode 140 away from the back substrate 113, a second electrode 172 is deposited on the surface of the second semiconductor portion 132 away from the back substrate 113, a third electrode 173 is deposited on the surface of the gate 120 away from the back substrate 113, and a fourth electrode 174 is deposited on the surface of the back substrate 113 away from the second semiconductor portion 132.

[0165] 19B , the vertical projection of the first electrode 171 on the back substrate 113 may overlap with the vertical projection of the first Schottky contact electrode 140 on the back substrate 113. Of course, the length of the first electrode 171 may also be shorter than the length of the first Schottky contact electrode 140. The vertical projection of the second electrode 172 on the back substrate 113 may overlap with the vertical projection of the second semiconductor portion 132 on the back substrate 113.

[0166] 19C , a vertical projection of the third electrode 173 on the back substrate 113 may overlap with a vertical projection of the gate 120 on the back substrate 113 . A vertical projection of the fourth electrode 174 on the back substrate 113 may overlap with the back substrate 113 .

[0167] Based on this, in metal-semiconductor structures, the metal and semiconductor are usually in horizontal contact, which greatly increases the process difficulty and is incompatible with complementary metal oxide semiconductor (CMOS) processes. The preparation method provided in the embodiments of the present application deposits metal on the semiconductor, thereby forming a vertical contact between the metal and semiconductor materials. This not only reduces the process difficulty but also is compatible with CMOS processes.

[0168] The above description is based on the preparation of an N-type semiconductor device as an example. The preparation method provided in the embodiment of the present application is also applicable to the preparation of a P-type semiconductor device. When preparing a P-type semiconductor device, the top semiconductor 111 and the back substrate 113 can be weakly N-type doped, the second semiconductor portion 132 can be ion-implanted with a heavily P-type doping, and the first Schottky contact electrode 140 can be a metal with a work function WF ≥ 4.5 eV, and the first Schottky contact electrode 140 is still configured as a metal drain region structure. The rest of the preparation method is the same as the above-mentioned method for preparing an N-type semiconductor device and will not be repeated here.

[0169] In some embodiments, as shown in FIG20A , when fabricating semiconductor device 100, substrate 110 may be a bulk substrate made entirely of semiconductor material. Specifically, windows for first isolation trench 114 and second isolation trench 115 may be opened in substrate 110 through photolithography. Then, first isolation trench 114 and second isolation trench 115 are etched using photoresist as a mask. Finally, silicon dioxide is filled into first isolation trench 114 and second isolation trench 115 using chemical vapor deposition, followed by chemical mechanical polishing to form first isolation trench 114 and second isolation trench 115.

[0170] Etching can be done using either dry or wet methods. Dry etching can use fluorine-based or halogen-based gases, such as sulfur hexafluoride (SF6), trifluoromethane (CHF3), hydrogen bromide (HBr), or chlorine (Cl2). Wet etching can use solutions such as tetramethylammonium hydroxide (TMAH) or potassium hydroxide (KOH).

[0171] Furthermore, since the bulk substrate is made of semiconductor material, there is no need to deposit the fourth electrode 174 on the bottom of the substrate 110. When fabricating an N-type semiconductor device, the bulk substrate can be an intrinsic semiconductor or a weakly P-type doped material. When fabricating a P-type semiconductor device, the bulk substrate can be an intrinsic semiconductor or a weakly N-type doped material.

[0172] After the substrate 110 is prepared, the top of the bulk substrate can be used as the active layer 130. As shown in FIG20B , when performing ion implantation on the second semiconductor portion 132, ions can be directly implanted into the bulk substrate in the region of the second semiconductor portion 132, so that this portion of the bulk substrate is heavily doped, thereby forming the second semiconductor portion 132. The remaining fabrication method is the same as that of the aforementioned semiconductor device 100 and will not be further described here.

[0173] As shown in FIG. 20C , the vertical projection of the gate 120 on the substrate 110 is located within the second isolation trench 115 , which can effectively isolate adjacent semiconductor devices 100 on the wafer.

[0174] The above is a detailed description of the specific structure and preparation method of the PFET. In addition, in some other embodiments of the present application, the above-mentioned MD-MOSFET can also be applied to fin field-effect transistors (FinFETs). The structure of the FinFET will be described in detail below.

[0175] 21 , the first semiconductor portion 131, the second semiconductor portion 132, the first Schottky contact electrode 140, the first electrode 171, and the second electrode 172 are all disposed on the same surface of the substrate 110 and are in contact with the substrate 110. The first Schottky contact electrode 140 is in contact with a side surface of the first semiconductor portion 131, and the second electrode 172 is in contact with a side surface of the second semiconductor portion 132.

[0176] As a result, the first semiconductor portion 131, the second semiconductor portion 132, and the channel portion 133 protrude away from the substrate 110, forming the fin portion of the FinFET. The gate 120 covers the channel portion 133 on three sides (shielded by the gate 120), increasing the contact area between the gate 120 and the channel portion 133 and enhancing the control effect of the gate 120 on the channel portion 133, thereby enabling the feature size of the semiconductor device 100 to be smaller.

[0177] Similar to the operating principle of a PFET, a FinFET can also form a first Schottky junction 141 between the first Schottky contact electrode 140 and the first semiconductor portion 131. This can also be combined with metal work function control to achieve impact ionization of carriers within the first Schottky junction 141, utilizing the FinFET channel to achieve a floating body effect, ultimately achieving an ultra-steep SS of the semiconductor device 100 and helping to reduce the SS of the transistor.

[0178] In addition, the FinFET channel can be made of the same material, such as silicon, silicon germanium, germanium, or other semiconductor materials from the III-V group. Alternatively, the FinFET channel can be made of different materials, such as SiGe / Si heterojunction materials. When the FinFET channel is made of different materials, the channel bandgap can be reduced, thereby helping to reduce the operating voltage of the FinFET. The following will provide a detailed description of the specific channel structures of different FinFET materials.

[0179] For example, as shown in FIG22A , the active layer of the FinFET may include a first active layer 1301 and a second active layer 1302 that are stacked. The first active layer 1301 is disposed on the substrate 110 and in contact with the substrate 110. The second active layer 1302 is stacked on the first active layer 1301 and in contact with the first active layer 1301. The first active layer 1301 may be made of silicon germanium, and the second active layer 1302 may be made of silicon. Of course, the first active layer 1301 and the second active layer 1302 may also be made of other different semiconductor materials. This application does not impose any particular restrictions on the specific materials of the first active layer 1301 and the second active layer 1302.

[0180] In some embodiments, as shown in FIG22B , the first active layer 1301 may include a first drain portion 1311, a first source portion 1321, and a first channel portion 1331. The second active layer 1302 may include a second drain portion 1312, a second source portion 1322, and a second channel portion 1332. The second source portion 1322 and the second channel portion 1332 may be made of silicon. The second drain portion 1312, the first drain portion 1311, the first source portion 1321, and the first channel portion 1331 may be made of silicon germanium. Alternatively, as shown in FIG22C , the first source portion 1321 and the first channel portion 1331 may be made of silicon. The first drain portion 1311, the second drain portion 1312, the second source portion 1322, and the second channel portion 1332 may be made of silicon germanium. In other words, different portions of the first active layer 1301 and the second active layer 1302 may be made of two different semiconductor materials. This application does not impose any particular restrictions on specific materials.

[0181] Alternatively, as shown in FIG22D , the first source electrode 1321 and the first channel portion 1331 can be made of silicon. The second source electrode 1322 and the second channel portion 1332 can be made of silicon germanium. The first drain electrode 1311 and the second drain electrode 1312 can be made of indium gallium arsenide. That is, different portions of the first active layer 1301 and the second active layer 1302 can be made of three different semiconductor materials. This application also imposes no particular limitation on the specific materials.

[0182] In other embodiments, as shown in FIG22D , regardless of the different materials used for the active layer of the FinFET, the first drain portion 1311, the second drain portion 1312, the first channel portion 1331, the second channel portion 1332, and the first source portion 1321 can be weakly doped to form a weakly doped region 191 (shown in FIG22E ). The second source portion 1322 can be heavily doped to form a heavily doped region 192 (shown in FIG22E ). Of course, the weakly doped region 191 can also be made of an intrinsic semiconductor. The embodiments of the present application do not impose any special restrictions on the specific doping type of the active layer of the FinFET.

[0183] Alternatively, as shown in Figure 22D, the first drain portion 1311 and the second drain portion 1312 may be subjected to a first weak doping to form a first weak doping region 191 (shown in Figure 22F). The first channel portion 1331, the second channel portion 1332 and the first source portion 1321 may be subjected to a second weak doping to form a second weak doping region 192 (shown in Figure 22F). The doping concentrations of the first weak doping region 191 and the second weak doping region 192 may be different. The second source portion 1322 may be heavily doped to form a heavily doped region 193 (shown in Figure 22F). Of course, the first weak doping region 191 and the second weak doping region 192 may also be made of intrinsic semiconductors. The embodiment of the present application does not impose any special restrictions on the specific doping concentration of the active layer of the FinFET.

[0184] On this basis, as shown in FIG22G , the active layer of the FinFET may further include a stacked third active layer 1303. The third active layer 1303 is disposed on the second active layer 1302 and is in contact with the second active layer 1302. The third active layer 1303 may include a third drain portion 1313, a third source portion 1323, and a third channel portion 1333. Of course, the active layer of the FinFET may further include more layers, and this application does not impose any particular limitation on the number of layers of the active layer of the FinFET.

[0185] As shown in FIG22G , the first drain portion 1311, the second active layer 1302, and the third drain portion 1313 can be made of silicon germanium, and the first source portion 1321, the first channel portion 1331, the third source portion 1323, and the third channel portion 1333 can be made of silicon. Of course, the first active layer 1301, the second active layer 1302, and the third drain portion 1313 can also be made of other different semiconductor materials. This application does not impose any particular limitation on the specific materials of the first active layer 1301, the second active layer 1302, and the third drain portion 1313.

[0186] Similarly, as shown in FIG22G , no matter what different materials are used for the active layer of the FinFET, the third source portion 1323 can be heavily doped to form a heavily doped region 192 (shown in FIG22H ). Other parts of the active layer of the FinFET are weakly doped to form a weakly doped region 191 (shown in FIG22H ). Of course, the weakly doped region 191 can also be made of intrinsic semiconductors. Alternatively, the doping concentration of the weakly doped region 191 can also be different. In addition, the width of the FinFET fin (the length shown in the W direction in FIG22H ) also has a certain influence on the SS of the semiconductor device 100. For example, as shown in FIG23 , the length L and height H of the FinFET fin are both 30 nm, and curve ⑩ indicates that the width of the FinFET fin is 70 nm, and curve ⑩ indicates that the width of the FinFET fin is 70 nm. Indicates that the width of the FinFET fin is 50nm, and the curve The width of the FinFET fin is 30nm. Indicates that the FinFET fin width is 10nm.

[0187] As can be seen from the figure, the operating voltage of the semiconductor device 100 (i.e., the horizontal axis where the curve begins to enter the super-steep state) decreases as the width of the FinFET fin decreases. Therefore, it is once again proved that the semiconductor device 100 provided by the embodiment of the present application is suitable for transistors with small feature sizes and has the characteristics of low power consumption and high performance.

[0188] In some other embodiments of the present application, the above-mentioned MD-MOSFET can also be applied to a gate-all-around field-effect transistor (GAAFET). The structure of the GAAFET will be described in detail below.

[0189] For example, as shown in FIG24 , the active layer of the GAAFET may include a first semiconductor portion 131 and a second semiconductor portion 132 spaced apart on the same surface of a substrate 110, and both the first semiconductor portion 131 and the second semiconductor portion 132 are in contact with the substrate 110. The first semiconductor portion 131 and the second semiconductor portion 132 extend in a direction away from the substrate 110, respectively, and a plurality of channels suspended above the substrate 110 are disposed between the first semiconductor portion 131 and the second semiconductor portion 132, with adjacent channels spaced apart.

[0190] In some embodiments, as shown in FIG24 , each channel may include a first channel segment 1310 and a second channel segment 1320 that are in contact with each other. The other end of the first channel segment 1310 contacts a side surface of the first semiconductor portion 131, and the first channel segment 1310 and the first semiconductor portion 131 may be made of the same semiconductor material. The other end of the second channel segment 1320 contacts a side surface of the second semiconductor portion 132, and the second channel segment 1320 and the second semiconductor portion 132 may be made of the same semiconductor material.

[0191] The materials of the first semiconductor portion 131 and the second semiconductor portion 132 may be the same or different. Consequently, the materials of the first channel segment 1310 and the second channel segment 1320 may be the same or different. The different materials of the first channel segment 1310 and the second channel segment 1320 help reduce the energy gap of the channel.

[0192] Furthermore, the first Schottky contact electrode 140 can be coated on the top and both sides of the first semiconductor portion 131, thereby increasing the contact area between the first Schottky contact electrode 140 and the first semiconductor portion 131, thereby increasing the probability of collisional ionization of carriers within the first Schottky junction 141. The first semiconductor portion 131, the first channel segment 1310, and the second channel segment 1320 can be made of intrinsic semiconductors or weakly doped semiconductors. The second semiconductor portion 132 can be heavily doped.

[0193] Compared with FinFET, the gate 120 (not shown in the figure) of GAAFET can cover the channel on all sides, further increasing the contact area between the gate 120 and the channel, and expanding the control effect of the gate 120 on the channel, thereby enabling the characteristic size of the semiconductor device 100 to be further reduced.

[0194] At the same time, similar to the working principle of PFET and FinFET, the first Schottky contact electrode 140 of GAAFET covers the first semiconductor part 131 on three sides, and a first Schottky junction 141 can also be formed between the first Schottky contact electrode 140 and the first semiconductor part 131. The work function of the metal can also be combined with the control to achieve collision ionization of carriers in the first Schottky junction 141, thereby achieving an ultra-steep SS of the semiconductor device 100 and reducing the SS of the transistor.

[0195] In order to obtain the above-mentioned GAAFET, the embodiment of the present application also provides a method for preparing a GAAFET. For example, taking the preparation of an N-type GAAFET as an example, as shown in FIG25 , a silicon wafer can be selected as a substrate 511, and then the substrate 511 is subjected to epitaxial growth. Specifically, a P-type layer 512 can be epitaxially grown on the substrate 511, and then a germanium silicon layer 513 can be epitaxially grown on the P-type layer 512, thereby forming a substrate 510.

[0196] Fin etching, as shown in FIG26 , can be performed by photolithography to form two spaced fins 520 from the substrate 510. The two fins 520 are parallel to each other and perpendicular to the substrate 511. The bottoms of the two fins 520 are in contact with the substrate 511.

[0197] Shallow trench isolation, as shown in Figure 27, can deposit an isolation layer 530 on the substrate 511 (shown in Figure 26) to prevent direct current conduction between the two fins 520, which could cause device failure. The isolation layer 530 can be made of materials such as silicon nitride or silicon oxide. The specific material of the isolation layer 530 is not particularly limited in this embodiment of the present application. The isolation layer 530 and the substrate 511 have the same coverage area.

[0198] As shown in FIG28 , a dummy gate layer 540 can be deposited on the isolation layer 530. The dummy gate layer 540 has the same coverage area as the isolation layer 530, and the top of the dummy gate layer 540 exceeds the top of the fin 520 (shown in FIG26 ). In this way, the dummy gate layer 540 can cover both side surfaces and the top surface of the fin 520. The dummy gate layer 540 can be made of amorphous silicon material, and the embodiment of the present application does not impose any special restrictions on the specific material of the dummy gate layer 540.

[0199] As shown in FIG29 , the dummy gate layer 540 can be etched by photolithography to form the dummy gate 541 of the device. The length of the dummy gate 541 is perpendicular to the length of the fin 520 (shown in FIG26 ). In this way, the dummy gate 541 can divide the fin 520 into alternating drain regions 521 and source regions 522.

[0200] Metal deposition and ion implantation, as shown in FIG30 , can be performed on the silicon-germanium layer 513 in the drain region 521 to form a Schottky contact. Ion implantation can be performed on the silicon-germanium layer 513 in the source region 522 to form a PN junction. This results in a field-effect transistor structure with a Schottky junction at the drain end and a PN junction at the source end.

[0201] As shown in FIG31 , spacers 550 may be deposited on both sides of the dummy gate 541 along the length direction of the fin 520 (shown in FIG26 ).

[0202] As shown in FIG32 , thin film deposition can be performed to isolate adjacent semiconductor devices and prevent device contamination by depositing a thin film 560 between the sidewalls 550 of adjacent dummy gates 541 to protect the devices. The material of the thin film 560 can be tetraethyl orthosilicate (TEOS), and the specific material of the thin film 560 is not particularly limited in this embodiment of the present application.

[0203] The thin film is opened, as shown in FIG33 , by etching the fin 520 in the portion enclosed by the dummy gate 541 and the thin film 560 to deposit electrodes for the drain and source regions.

[0204] Electrode deposition, as shown in FIG34 , is performed within the thin film opening to form an electrode layer 570. The material of the electrode layer 570 can be a metal or silicide that matches a P-type semiconductor or an N-type semiconductor. The present embodiment does not impose any particular limitation on the specific material of the electrode layer 570.

[0205] Tungsten filling, as shown in FIG35 , in order to ensure the continuity of electrical performance between multilayer devices, a tungsten layer 580 may be filled on the electrode layer 570 (shown in FIG34 ).

[0206] As shown in FIG36 , the dummy gate 541 (shown in FIG33 ) between adjacent sidewall spacers 550 may be removed by photolithography to expose the P-type layer 512 and the silicon germanium layer 513 between adjacent sidewall spacers 550 .

[0207] As shown in FIG37 , the P-type layer 512 between adjacent sidewall spacers 550 can be removed by selective etching, leaving the SiGe layer 513 between adjacent sidewall spacers 550. In this way, all four sides of the SiGe layer 513 are exposed, forming the GAAFET channel.

[0208] 38 , a high-k material may be deposited between adjacent sidewall spacers 550 as a gate oxide layer, and then a metal gate 590 may be deposited on the gate oxide layer to form a GAAFET semiconductor device 100 .

[0209] The above is only a specific embodiment of the present application, but the scope of protection of this application is not limited to this. Any changes or substitutions within the technical scope disclosed in this application should be included in the scope of protection of this application. Therefore, the scope of protection of this application should be based on the scope of protection of the claims.

Claims

1. A semiconductor device, characterized in that: include: substrate; A gate is disposed on the substrate; an active layer disposed on the substrate, the active layer comprising a channel portion; wherein a vertical projection of the gate on the substrate overlaps a vertical projection of the channel portion on the substrate; and A first Schottky contact electrode is disposed on the substrate and in contact with the active layer; a first Schottky junction is formed between the first Schottky contact electrode and the active layer; Wherein, a portion of the active layer in contact with the first Schottky contact electrode has the same doping type as that of the channel portion.

2. The semiconductor device according to claim 1, wherein: The active layer further includes a first semiconductor portion, the first semiconductor portion is in contact with the channel portion and has the same doping type as the channel portion; The first Schottky contact electrode is stacked with the active layer and located on a side of the active layer away from the substrate. A vertical projection of the first Schottky contact electrode on the substrate overlaps with a vertical projection of the first semiconductor portion on the substrate.

3. The semiconductor device according to claim 1, wherein: The active layer further includes a first semiconductor portion, the first semiconductor portion is in contact with the channel portion and has the same doping type as the channel portion; The first Schottky contact electrode and the first semiconductor portion are disposed on the same surface of the substrate and are in contact with the substrate; the first Schottky contact electrode is in contact with a side surface of the first semiconductor portion.

4. The semiconductor device according to claim 3, characterized in that The semiconductor device comprises at least two stacked active layers, two of which are a first active layer and a second active layer, respectively, and the first active layer is disposed on the substrate and in contact with the substrate; The first active layer has a first channel portion, and the second active layer has a second channel portion; The first channel portion and the second channel portion are made of different semiconductor materials.

5. The semiconductor device according to claim 1, wherein: The first Schottky contact electrode and the active layer are disposed on the same surface of the substrate and are in contact with the substrate; The first Schottky contact electrode is in contact with the channel portion.

6. The semiconductor device according to any one of claims 1 to 5, characterized in that: The active layer further includes a second semiconductor portion, the second semiconductor portion is in contact with the channel portion and has a doping type different from that of the channel portion; The first Schottky contact electrode and the second semiconductor portion are respectively located on both sides of the channel portion.

7. The semiconductor device according to claim 2, characterized in that The active layer further includes a second semiconductor portion, the second semiconductor portion is in contact with the channel portion and has a doping type different from that of the channel portion; The first semiconductor portion and the second semiconductor portion are respectively located on both sides of the channel portion, and are disposed on the same surface of the substrate and in contact with the substrate; the first Schottky contact electrode covers the top and both sides of the first semiconductor portion; At least one channel portion is connected between the first semiconductor portion and the second semiconductor portion. Each channel portion is suspended above the substrate, and adjacent channel portions are spaced apart.

8. The semiconductor device according to claim 7, characterized in that The semiconductor device further includes a first electrode and a second electrode; The first electrode is disposed on the first Schottky contact electrode and is in contact with the first Schottky contact electrode; The second electrode covers the top and both sides of the second semiconductor portion.

9. The semiconductor device according to any one of claims 1 to 5, characterized in that: The active layer further includes a second semiconductor portion, the second semiconductor portion is in contact with the channel portion and has the same doping type as the channel portion; The semiconductor device further includes a second Schottky contact electrode; The second Schottky contact electrode is stacked with the active layer and located on a side of the active layer away from the substrate. The vertical projection of the second Schottky contact electrode on the substrate overlaps with the vertical projection of the second semiconductor portion on the substrate.

10. The semiconductor device according to any one of claims 1 to 5, characterized in that: The semiconductor device further includes a second Schottky contact electrode; The second Schottky contact electrode and the active layer are arranged on the same surface of the substrate and are in contact with the substrate; the second Schottky contact electrode is in contact with the channel portion, and the first Schottky contact electrode and the second Schottky contact electrode are respectively located on both sides of the channel portion.

11. The semiconductor device according to any one of claims 1 to 10, characterized in that: The active layer further includes a second semiconductor portion, the second semiconductor portion is in contact with the channel portion and has a doping type different from that of the channel portion; The first Schottky contact electrode is a metal with a work function WF < 4.5 eV; The second semiconductor portion has a doping concentration of 10 19 -10 21 cm -3 N-type semiconductor; The channel portion is an intrinsic semiconductor or a semiconductor with a doping concentration of 10 15 -10 17 cm -3 P-type semiconductor.

12. The semiconductor device according to any one of claims 1 to 10, characterized in that: The active layer further includes a second semiconductor portion, the second semiconductor portion is in contact with the channel portion and has a doping type different from that of the channel portion; The first Schottky contact electrode is a metal with a work function WF≥4.5eV; The second semiconductor portion has a doping concentration of 10 19 -10 21 cm -3 P-type semiconductor; The channel portion is an intrinsic semiconductor or a semiconductor with a doping concentration of 10 15 -10 17 cm -3 N-type semiconductor.

13. An electronic device, characterized in that: include: Circuit boards; as well as, The semiconductor device according to any one of claims 1 to 12, wherein the semiconductor device is electrically connected to the circuit board.

Citation Information

Patent Citations

  • Double-layer schottky barrier MOS transistor and manufacturing method thereof

    CN104241397A

  • Short-channel schottky-barrier MOSFET device and manufacturing method

    US20060244052A1

  • Low schottky barrier semiconductor structure and method for forming the same

    US20120025279A1