Experimental system for researching corrosion behavior of steel in high-temperature flowing lead-bismuth eutectic

By designing an experimental system to study the interaction of multiple corrosion behaviors in high-temperature flowing lead-bismuth alloys, the research difficulties in the existing technology were solved, and the effective corrosion behavior of steel materials for lead-bismuth alloy cooling fast neutron reactors was achieved. Research has promoted industrial applications in this field.

WO2024234599A1PCT designated stage expired Publication Date: 2024-11-21ROCKET FORCE UNIV OF ENG

Patent Information

Application Number
PCT/CN2023/132519
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-05-12
Filing Date
2023-11-20
Publication Date
2024-11-21

AI Technical Summary

Technical Problem

The existing technology is difficult to effectively study the interaction between steel materials in erosion, oxidation and dissolution in high-temperature flowing lead-bismuth alloys, and dynamic corrosion experiments are mainly limited to laminar flow environments. Research under extreme erosion conditions is relatively rare, which affects Selection and corrosion protection of lead-bismuth alloy cooled fast neutron reactor steel materials.

Method used

An experimental system including lead-bismuth alloy storage and supply system, lead-bismuth alloy dissolved oxygen pretreatment system and experimental main loop system was designed, and the argon cylinder, thermocouple thermometer, electric heating system, solid-phase oxygen control device and impurities were used. Filters realize precise control of the temperature, oxygen content and flow rate of high-temperature flowing lead-bismuth alloys, provide circular pipes of different diameters and removable sample placement boxes, and conduct corrosion experiments of steel materials under different oxygen content, flow rate and angle of attack. .

Benefits of technology

This system can study the interaction of steel materials in various corrosion behaviors in high-temperature flowing lead-bismuth alloys, expanding the research scope, providing an important reference for the selection and corrosion protection of steel materials for lead-bismuth alloy cooling fast neutron reactors, and promoting Industrial applications in this field.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN2023132519_21112024_PF_FP_ABST
    Figure CN2023132519_21112024_PF_FP_ABST
Patent Text Reader

Abstract

An experimental system for researching a corrosion behavior of steel in a high-temperature flowing lead-bismuth eutectic, relating to a lead-bismuth cooled fast neutron reactor. The experimental system comprises a lead-bismuth eutectic storage and supply system (1), a lead-bismuth eutectic dissolved oxygen pretreatment system (2), a lead-bismuth eutectic purification system (3), an experiment main loop system (4); the experiment main loop system (4) comprises an electromagnetic pump (403), a flow meter (404), a solid-phase oxygen control device (405), sample placement boxes (407-1, 407-2, 407-3), an impurity filter (401), three sections of pipelines (408-1, 408-2, 408-3) having different diameters, a gas supply system, and a heating and heat preservation system; the experiment main loop system (4) can control the temperature and the oxygen content of a fluid in a loop in real time, and can simultaneously carry out corrosion experiments of the steel under different attack angles and different lead-bismuth eutectic flow rates; after an experiment is finished, a lead-bismuth eutectic is purified and reset, and after the samples in the sample placement boxes (407-1, 407-2, 407-3) are treated, the corrosion behavior characteristics of the steel under different attack angles and different lead-bismuth eutectic flow rates are represented by using multiple means. The present invention provides an important experimental apparatus for researching the corrosion behavior of the lead-bismuth cooled fast neutron reactor steel in the lead-bismuth eutectic.
Need to check novelty before this filing date? Find Prior Art

Description

An experimental system for studying the corrosion behavior of steel in high-temperature flowing lead-bismuth alloy Technical Field

[0001] The present invention relates to the technical field of research on the corrosion behavior characteristics of lead-bismuth alloy-cooled fast neutron reactor steel materials in a lead-bismuth alloy coolant, and in particular to an experimental system for studying the corrosion behavior of steel in a high-temperature flowing lead-bismuth alloy. Background Art

[0002] Lead-bismuth alloy is a candidate coolant for fourth-generation fast neutron reactors. Due to its excellent physical and chemical properties, it is expected to significantly improve the operational safety of nuclear reactors. However, the compatibility of this coolant with the structural steel within nuclear reactors still restricts its large-scale industrial application in the nuclear energy sector. Oxidation and dissolution are two material corrosion failure mechanisms in static lead-bismuth alloys with different dissolved oxygen concentrations. Although numerous studies have been conducted domestically and internationally on the corrosion behavior of structural steel in flowing lead-bismuth, due to the difficulty in setting up and maintaining dynamic corrosion experimental equipment, dynamic corrosion experiments on lead-bismuth are still mainly limited to laminar flow environments. Research on the erosion behavior of materials under extreme erosion conditions is extremely rare. Even fewer reports have explored the interaction between multiple traditional corrosion failure modes, such as erosion, oxidation, and dissolution.

[0003] Generally speaking, in static liquid lead-bismuth alloy, steel materials have two corrosion failure modes: oxidation and dissolution. These two corrosion behaviors are closely related to the dissolved oxygen content in the liquid lead-bismuth alloy. In order to avoid dissolution corrosion after the steel material substrate comes into direct contact with the lead-bismuth alloy, the most common way is to generate a continuous outer oxide layer on the surface of the steel material, which can be achieved by appropriately increasing the concentration of dissolved oxygen in the lead-bismuth alloy. However, it should be noted that excessively high oxygen concentration will cause the oxide layer on the surface of the steel material to grow too fast, and may even cause the liquid lead-bismuth alloy itself to be oxidized. An excessively thick oxide layer will not only affect surface heat transfer, but may also pose a risk of clogging the pipeline after partial shedding of the oxide layer. Once the oxide particles in the lead-bismuth alloy are transported with the liquid lead When bismuth alloys flow together, the solid-liquid two-phase flow intensifies the wear on the surfaces of components such as impellers, pipes, and valves. Therefore, researchers are hoping to control the dissolved oxygen concentration in the lead-bismuth alloy within a range that ensures continuous and slow growth of the oxide layer on the surface of structural steel. Currently, the Karlsruhe Institute of Technology in Germany has achieved precise control of oxygen concentration throughout the dynamic corrosion process of lead-bismuth in the CORRIDA lead-bismuth circuit using gas-phase oxygen control and oxygen pump technology. Professor Niu Fenglei's team at the School of Nuclear Science and Engineering at North China Electric Power University, the Anhui Institute of Optics and Fine Mechanics of the Chinese Academy of Sciences, the Institute of Nuclear Safety of the Chinese Academy of Sciences, and the China General Nuclear Power Research Institute have all reported independently developed technologies for real-time online monitoring or control of oxygen content in static or dynamic lead-bismuth corrosion devices.

[0004] In actual equipment operation, the dissolution and oxidation corrosion behaviors of steel in lead-bismuth alloys are related not only to oxygen concentration but also to corrosion time, temperature, the specific composition of the material, heat treatment, and machining processes. At temperatures above 500°C to 550°C, or for extended periods (over 10,000 hours), even in static lead-bismuth alloys above the critical oxygen partial pressure for oxidation, there have been reports of steel elements being dissolved and corroded after the local oxide film loses its protective effect.

[0005] The study of the corrosion behavior mechanism of lead-bismuth alloy fast neutron reactor steel materials in high-temperature flowing lead-bismuth alloy is very important and necessary. It helps to clarify the corrosion behavior of steel surfaces at different erosion angles or steel surfaces that have undergone corrosion protection treatment under the interaction of various corrosion behaviors such as erosion, oxidation, and dissolution. It has important reference value for the selection and corrosion protection of various steel materials that serve in lead-bismuth alloy-cooled fast neutron reactors under extreme lead-bismuth flow conditions for a long time.

[0006] Summary of the Invention

[0007] The purpose of the present invention is to overcome the shortcomings of the existing technology and provide an experimental system for studying the corrosion behavior of steel in high-temperature flowing lead-bismuth alloy. The system can study the corrosion mechanism of steel materials under the interaction of various corrosion behaviors such as scouring, oxidation and dissolution in high-temperature flowing lead-bismuth alloy and reveal its laws.

[0008] In order to achieve the above object, the present invention adopts the following technical solutions:

[0009] An experimental system for studying the corrosion behavior of steel in high-temperature flowing lead-bismuth alloy comprises a lead-bismuth alloy storage and supply system, a lead-bismuth alloy dissolved oxygen pretreatment system, and an experimental main loop system. The lead-bismuth alloy storage and supply system comprises a first argon gas cylinder, a first valve, a lead-bismuth alloy storage and heating tank, a second valve, a first thermocouple thermometer, and a third valve. The first argon gas cylinder is connected to the lead-bismuth alloy storage and heating tank via the first valve to provide air pressure. The first thermocouple thermometer is connected to the lead-bismuth alloy storage and heating tank to detect the temperature of the lead-bismuth alloy therein. The third valve serves as an air inlet valve for the lead-bismuth alloy storage and heating tank.

[0010] The lead-bismuth alloy dissolved oxygen pretreatment system includes a second argon gas cylinder, a fourth valve, a lead-bismuth alloy dissolved oxygen pretreatment tank, a fifth valve, a second thermocouple thermometer, a sixth valve, a mixed gas cylinder for providing argon and oxygen, and a seventh valve. The lead-bismuth alloy storage and supply system is connected to the lead-bismuth alloy dissolved oxygen pretreatment tank via the third valve. The second argon gas cylinder is connected to the lead-bismuth alloy dissolved oxygen pretreatment tank via the fourth valve to provide air pressure. The second thermocouple thermometer is connected to the lead-bismuth alloy dissolved oxygen pretreatment tank to detect the temperature of the lead-bismuth alloy therein. The seventh valve is connected to the main experimental loop system.

[0011] The experimental main loop system includes three sections of circular pipes of different diameters, namely, first, second, and third sections. The first, second, and third sections respectively house first, second, and third sample storage boxes. The first, second, and third sections are interconnected via first, second, and third section connectors. Third, fourth, and fifth thermocouple thermocouples are respectively located on the first, second, and third sections to monitor the temperature of the lead-bismuth alloy therein. The system also includes an electric heating system with PID control. The third argon gas cylinder is connected to an electromagnetic pump via an eighth valve to provide air pressure.

[0012] Among them, the preferred scheme also includes a lead-bismuth alloy purification system, which includes a ninth valve, a lead-bismuth alloy purification device, and a tenth valve connected in series in sequence, one end of the ninth valve is connected to the lead-bismuth alloy storage and heating tank, and one end of the tenth valve is connected to the lead-bismuth alloy dissolved oxygen pretreatment tank.

[0013] Among them, the preferred solution is: the volume fractions of argon and oxygen in the mixed gas bottle are 95% and 5% respectively.

[0014] Among them, the preferred solution is: the lead-bismuth alloy storage and supply system is set separately from the lead-bismuth alloy dissolved oxygen pretreatment system, and a lead-bismuth alloy purification system is set in the two systems to ensure the purity of the lead-bismuth alloy returned to the lead-bismuth alloy storage and heating tank after each experiment.

[0015] Among them, the preferred solution is: the first, second and third circular pipes of different diameters in the experimental main loop system, the entire system can provide three lead-bismuth alloy flow environments with different flow rates under a constant liquid lead-bismuth alloy flow rate.

[0016] Among them, the preferred solution is: the experimental main loop system also includes an electromagnetic pump, an electromagnetic flowmeter and a solid-phase oxygen control device, and the electromagnetic pump, electromagnetic flowmeter and solid-phase oxygen control device are placed in series between the eleventh valve and the first circular pipe. By adjusting the power of the electromagnetic pump, the reading of the electromagnetic flowmeter reaches the value required for the experiment, and the solid-phase oxygen control device adjusts the oxygen content of the lead-bismuth alloy in the loop in real time.

[0017] Among them, the preferred solution is: the first, second and third sample placement boxes in the experimental main loop system are respectively placed with processed steel sheet samples, and multiple steel sheet samples can be placed in each sample placement box. When placing the samples, the angle between the surface of the steel sheet sample and the direction of the lead-bismuth alloy flow velocity can be placed and fixed according to experimental requirements. After each experiment, the sample placement box can be disassembled and the steel sheet sample can be taken out for analysis.

[0018] Among them, the preferred solution is: the first, second and third circular pipes where the first, second and third sample placement boxes in the experimental main loop system are located should have sufficient straight pipe length to ensure the stability of the flow field of the liquid lead-bismuth alloy initially entering the sample placement box.

[0019] Among them, the preferred solution is: the impurity filter in the experimental main loop system can be selectively opened. When opened, it can prevent the impurities in the liquid lead-bismuth alloy from causing scouring and wear of the steel sheet samples in the first, second, and third sample placement boxes. When the impurity filter is not opened, the wear effect of impurities in the liquid lead-bismuth alloy on the steel sheet samples can be studied.

[0020] The experimental system of the present invention relates to a lead-bismuth alloy-cooled fast neutron reactor, including a lead-bismuth alloy storage and supply system, a lead-bismuth alloy dissolved oxygen pretreatment system, a lead-bismuth alloy purification system, and an experimental main loop system; the experimental main loop system includes an electromagnetic pump, a flow meter, a solid-phase oxygen control device, a sample placement box, an impurity filter, three sections of pipes with different diameters, an air supply system, and a heating and insulation system; the experimental main loop system can control the temperature and oxygen content of the fluid in the loop in real time, and can simultaneously carry out corrosion experiments on steel at different attack angles and different lead-bismuth alloy flow rates; after the experiment is completed, the lead-bismuth alloy purification is reset, and the sample in the sample placement box is processed and then characterized by multiple means for the corrosion behavior characteristics of the steel at different attack angles and different lead-bismuth alloy flow rates; the present invention provides an important experimental device for studying the corrosion behavior of lead-bismuth-cooled fast neutron reactor steel in lead-bismuth alloy. Compared with the existing technology, the present invention has the following advantages:

[0021] 1. The experimental system of the present invention comprises three circular tubes of varying diameters. A considerable length of straight tube section is provided before and after the sample placement box to ensure adequate development of the flow field within the tubes. At a fixed liquid lead-bismuth alloy flow rate, the lead-bismuth alloy flow rates within the three circular tubes are all different, enabling simultaneous steel corrosion experiments at three different lead-bismuth alloy flow rates. Furthermore, the simplified flow field can reduce the impact of a complex lead-bismuth alloy flow field on steel corrosion.

[0022] 2. The experimental system of the present invention is equipped with a detachable sample placement box. The steel samples used in the experiment are fixed at a certain angle in the sample placement box by welding, so that the high-temperature flowing lead-bismuth alloy erodes them at a certain angle of attack. Each sample placement box can be welded with multiple steel samples. The sample placement box is replaceable, allowing for corrosion experiments on steel under the erosion of lead-bismuth alloy flowing at different angles of attack.

[0023] 3. The experimental system of the present invention is equipped with a solid-phase oxygen control device and an impurity filter. The solid-phase oxygen control system can adjust the oxygen concentration in the liquid lead-bismuth alloy in real time. The optional opening and closing of the impurity filter enables the experimental main loop system to analyze the difference in the corrosion behavior of steel sheet samples with and without impurity particles in the liquid lead-bismuth alloy.

[0024] The present invention can study the corrosion mechanism of steel materials under the interaction of various corrosion behaviors such as scouring, oxidation and dissolution in high-temperature flowing lead-bismuth alloy, including the oxidation corrosion behavior of steel materials in lead-bismuth alloy environments with different oxygen contents, the scouring corrosion behavior under scouring of lead-bismuth alloys with different flow rates and different attack angles, and the influence of impurities on the corrosion of steel materials in lead-bismuth alloys. It greatly expands the research and discussion on the corrosion behavior of steel materials in high-temperature flowing lead-bismuth alloys, and fills the research gap on the corrosion mechanism of steel in high-temperature flowing lead-bismuth alloys under the interaction of multiple corrosion forms. The research results have important reference value for the selection and corrosion protection of steel structural materials that serve for a long time in various lead-bismuth flow states in lead-bismuth alloy-cooled fast neutron reactors, help accelerate the industrial application of lead-bismuth alloy-cooled fast neutron reactors, and have broad application prospects. BRIEF DESCRIPTION OF THE DRAWINGS

[0025] FIG1 is a schematic diagram of the overall structure of an experimental system for studying the corrosion behavior of steel in a high-temperature flowing lead-bismuth alloy according to the present invention;

[0026] FIG2 is a schematic diagram of the lead-bismuth alloy storage and supply system (1) of the present invention;

[0027] FIG3 is a schematic diagram of the lead-bismuth alloy dissolved oxygen pretreatment system (2) of the present invention;

[0028] FIG4 is a schematic diagram of the lead-bismuth alloy purification system (3) of the present invention;

[0029] FIG5 is a schematic diagram of the experimental main loop system (4) of the present invention;

[0030] FIG6 is a three-view diagram of the sample placement box ( 407 - 1 ) in the experimental main loop system ( 4 ) of the present invention.

[0031] Icon Description:

[0032] 1. Lead-bismuth alloy storage and supply system;

[0033] 101 first argon gas cylinder, 102 first barometer, 103-1 first valve, 104 lead-bismuth alloy storage and heating tank, 103-2 second valve, 105 first thermocouple thermometer, 103-3 third valve;

[0034] 2. Lead-bismuth alloy dissolved oxygen pretreatment system;

[0035] 201 Second argon cylinder, 202-1 Second barometer, 203-1 Fourth valve, 204 Lead-bismuth alloy dissolved oxygen pretreatment tank, 203-2 Fifth valve, 205 Second thermocouple thermometer, 203-3 Sixth valve, 202-2 Third barometer, 206 Mixed gas cylinder, 203-4 Seventh valve;

[0036] 3. Lead-bismuth alloy purification system;

[0037] 301-1 eighth valve, 302 lead-bismuth alloy purification device, 301-2 ninth valve;

[0038] 4 Experimental main circuit system;

[0039] 401 impurity filter, 402-1 tenth valve, 402-2 eleventh valve, 403 electromagnetic pump, 404 electromagnetic flowmeter, 405 solid-phase oxygen control device, 406-1 third thermocouple thermometer, 407-1 first sample placement box, 408-1 first circular pipe, 409-1 first circular pipe connector, 408-2 second circular pipe, 406-2 fourth thermocouple thermometer, 407-2 second sample placement box, 409-2 second circular pipe connector, 408-3 third circular pipe, 406-3 fifth thermocouple thermometer, 407-3 third sample placement box, 410 electric heating system with PID control, 402-3 twelfth valve, 411 third barometer, 412 third argon gas cylinder. DETAILED DESCRIPTION

[0040] The present invention will be described in detail below with reference to the accompanying drawings and specific embodiments:

[0041] As shown in Figures 1, 2, 3, 4 and 5, an experimental system for studying the corrosion behavior of steel in high-temperature flowing lead-bismuth alloy of the present invention includes a lead-bismuth alloy storage and supply system 1, a lead-bismuth alloy dissolved oxygen pretreatment system 2, a lead-bismuth alloy purification system 3, and an experimental main loop system 4; the lead-bismuth alloy storage and supply system 1 includes a first argon gas cylinder 101, a first barometer 102, a first valve 103-1, a lead-bismuth alloy storage and heating tank 104, a second valve 103-2, a first thermocouple thermometer 105 and a third valve 103-3; the lead-bismuth alloy dissolved oxygen pretreatment system 2 includes a second argon gas cylinder 201, a second barometer 202-1, a fourth valve 203 -1, lead-bismuth alloy dissolved oxygen pretreatment tank 204, fifth valve 203-2, second thermocouple thermometer 205, sixth valve 203-3, third barometer 202-2, mixed gas bottle 206 providing 95% by volume argon and 5% by volume oxygen, seventh valve 203-4; the lead-bismuth alloy purification system 3 includes an eighth valve 301-1, a lead-bismuth alloy purification device 302, and a ninth valve 301-2; the experimental main loop system 4 includes an impurity filter 401, a tenth valve 402-1, an eleventh valve 402-2, an electromagnetic pump 403, an electromagnetic flowmeter 404, a solid-phase oxygen control device 405, a third thermocouple thermometer 406-1, The first sample placement box 407-1, the first circular pipe 408-1, the first circular pipe connector 409-1, the second circular pipe 408-2, the fourth thermocouple thermometer 406-2, the second sample placement box 407-2, the second circular pipe connector 409-2, the third circular pipe 408-3, the fifth thermocouple thermometer 406-3, the third sample placement box 407-3, the electric heating system with PID control 410, the twelfth valve 402-3, the third barometer 411, and the third argon gas cylinder 412; the lead-bismuth alloy storage and supply system 1 and the lead-bismuth alloy dissolved oxygen pretreatment system 2 are separately arranged, and the lead-bismuth alloy purification system 3 is arranged in the two systems to ensure that each time After the experiment, the purity of the lead-bismuth alloy in the lead-bismuth alloy storage and heating tank 104 is returned. The experimental main loop system 4 includes three sections of first, second, and third circular pipes 408-1, 408-2, and 408-3 with different diameters. The entire system can provide three lead-bismuth alloy flow environments with different flow rates under a constant liquid lead-bismuth alloy flow rate. The first, second, and third sample placement boxes 407-1, 407-2, and 407-3 in the experimental main loop system 4 respectively place processed steel sheet samples. When placing the samples, the angle between the surface of the steel sheet sample and the direction of the lead-bismuth alloy flow rate can be fixed according to experimental requirements. After each experiment, the sample placement box can be disassembled and the steel sheet sample can be removed for analysis.The first, second, and third circular pipes 408-1, 408-2, and 408-3 within the first, second, and third sample storage boxes 407-1, 407-2, and 407-3 of the experimental main loop system 4 should have sufficient straight length to ensure the stability of the flow field of the liquid lead-bismuth alloy initially entering the sample storage boxes. The impurity filter 401 in the experimental main loop system 4 can be selectively activated. When activated, it can prevent impurities in the liquid lead-bismuth alloy from eroding and abrading the steel samples within the first, second, and third sample storage boxes 407-1, 407-2, and 407-3. When the impurity filter 401 is not activated, the abrasive effects of impurities in the liquid lead-bismuth alloy on the steel samples can be studied.

[0042] First, the steel sheet samples are welded at a certain angle in the first, second and third sample placement boxes 407-1, 407-2 and 407-3. Figure 6 is a three-view diagram of the sample placement box 407-1. The first steel sheet sample 407-1-1 and the second steel sheet sample 407-1-2 are two steel sheet samples to be tested welded in the first sample placement box 407-1. α is the angle between the surface of the steel sheet sample to be corroded and the incoming flow velocity of the high-temperature flowing lead-bismuth alloy. The placement of the steel sheet samples in the second and third sample placement boxes 407-2 and 407-3 is similar to that of the first sample placement box 407-1. After the steel sheet samples in the three sample placement boxes are welded, they are installed in the experimental main loop system 4 to prepare for the experiment. Before the experiment is carried out, all valves are in the closed state. At this time, the tenth valve 402-1 and the eleventh valve 402-3 are opened, and the argon gas provided by the third argon gas cylinder 412 is used to flush the pipeline of the experimental main loop system 4. The argon gas enters the pipeline of the experimental main loop system from the eleventh valve 402-3 and flows out from the tenth valve 402-1. The purpose is to remove the residual oxygen in the pipeline and prevent the high-temperature lead-bismuth alloy from being oxidized when entering the experimental main loop system 4. After completing this step, the eleventh valve 402-3 and the tenth valve 402-1 are closed; the lead-bismuth alloy in the lead-bismuth alloy storage and supply system 1 is flushed. The lead-bismuth alloy in the storage and heating tank 104 is heated and melted, and the lead-bismuth alloy dissolved oxygen pretreatment system 2 and the pipes connected to the lead-bismuth alloy storage and supply system 1 are preheated and kept warm to prevent the lead-bismuth alloy from solidifying during the flow process; the temperature of the lead-bismuth alloy in the lead-bismuth alloy storage and heating tank 104 is determined by the first thermocouple thermometer 105. After the lead-bismuth alloy is heated to the required temperature for the experiment, the third valve 103-3 and the first valve 103-1 are opened in sequence, and the lead-bismuth alloy storage and heating tank 104 is heated by the air pressure provided by the first argon gas cylinder 101. 04 is pressed into the lead-bismuth alloy dissolved oxygen pretreatment tank 204. After completion, the third valve 103-3 and the first valve 103-1 in the lead-bismuth alloy storage and supply system 1 are closed; the sixth valve 203-3 is opened, and the mixed gas containing argon and oxygen in the mixed gas bottle 206 is supplied to the lead-bismuth alloy dissolved oxygen pretreatment tank 204. After the dissolved oxygen content of the lead-bismuth alloy reaches the value required for the experiment, the sixth valve 203-3 is closed; the electric heating system 410 is turned on to heat and keep the experimental main loop system 4 warm; then Then, the seventh valve 203-4, the eighth valve 402-1, the eleventh valve 402-2, and the seventh valve 203-1 are opened in sequence. The second argon cylinder 201 provides air pressure to pressurize the lead-bismuth alloy with a certain oxygen content in the lead-bismuth alloy dissolved oxygen pretreatment tank 204 into the experimental main loop system 4. The gas in the experimental main loop system 4 can be discharged by controlling the tenth valve 402-1. After the experimental main loop system 4 is filled with high-temperature liquid lead-bismuth alloy, the fourth valve 203-1, the seventh valve 203-4, and the tenth valve 402-1 are closed.The electromagnetic pump 403 is turned on, and the power of the electromagnetic pump 403 is adjusted so that the actual value of the electromagnetic flowmeter 404 reaches the value required for the experiment. The solid-phase oxygen control device 405 can adjust the oxygen content of the lead-bismuth alloy in the loop in real time. The impurity filter 401 can be selectively turned on if it is necessary to prevent the precipitation of oxides generated by oxidation of the lead-bismuth alloy or the impact of the steel sheet sample with the flow of the fluid from the fallen materials after corrosion. The impurity filter 401 can be turned on. The temperature of the lead-bismuth alloy in the experimental main loop system 4 can be measured by the third, fourth, and fifth thermocouple thermometers 406-1, 406-2, and 406-3. Based on the change in the temperature reading, the electric heating system 410, with its own PID control system, automatically adjusts the power output to maintain a constant temperature of the lead-bismuth alloy in the loop. After the experiment, the electromagnetic pump 403 is turned off, the eleventh valve 402-2 is closed, the seventh valve 203-4, the twelfth valve 402-3, and the fifth valve 203-2 are opened, and the third argon cylinder 4 is used to generate a argon gas. The gas pressure provided by the second argon cylinder 201 is used to press the liquid lead-bismuth alloy in the experimental main loop system 4 back into the lead-bismuth alloy dissolved oxygen pretreatment tank 204. After completion, the seventh valve 203-4 and the twelfth valve 402-3 are closed, and the electric heating system 410 is turned off. The eighth valve 301-1, the ninth valve 301-2, the fourth valve 203-1, and the second valve 103-2 are opened, and the lead-bismuth alloy in the lead-bismuth alloy dissolved oxygen pretreatment tank 204 is pressed back into the lead-bismuth alloy storage and heating tank 104 using the gas pressure provided by the second argon cylinder 201. Oxygen and solid impurities in the lead-bismuth alloy are removed through the lead-bismuth alloy purification device 302. After completion, all valves are closed, and the experiment is terminated after the lead-bismuth alloy storage and heating tank 104 cools to room temperature. The first, second, and third sample storage boxes 407-1, 407-2, and 407-3 are disassembled, and the steel sheet samples that have undergone the corrosion experiment are removed for analysis. The corrosion mechanism of steel materials under the interaction of multiple corrosion behaviors such as scouring, oxidation, and dissolution in the high-temperature flowing lead-bismuth alloy is studied, and the underlying corrosion laws are revealed. ;

Claims

1. An experimental system for studying the corrosion behavior of steel in high temperature flowing lead-bismuth alloy, characterized in that: The experimental system includes a lead-bismuth alloy storage and supply system (1), a lead-bismuth alloy dissolved oxygen pretreatment system (2), and an experimental main loop system (4); The lead-bismuth alloy storage and supply system (1) comprises a first argon gas cylinder (101), a first valve (103-1), a lead-bismuth alloy storage and heating tank (104), a second valve (103-2), a first thermocouple thermometer (105) and a third valve (103-3); the first argon gas cylinder (101) is connected to the lead-bismuth alloy storage and heating tank (104) through the first valve (103-1) to provide gas pressure; the first thermocouple thermometer (105) is connected to the lead-bismuth alloy storage and heating tank (104) to detect the temperature of the lead-bismuth alloy therein, and the third valve (103-3) is an air inlet valve of the lead-bismuth alloy storage and heating tank (104); The lead-bismuth alloy dissolved oxygen pretreatment system (2) comprises a second argon gas cylinder (201), a fourth valve (203-1), a lead-bismuth alloy dissolved oxygen pretreatment tank (204), a fifth valve (203-2), a second thermocouple thermometer (205), a sixth valve (203-3), a mixed gas cylinder (206) for providing argon and oxygen, and a seventh valve (203-4); the lead-bismuth alloy storage and supply system (1) is connected to the lead-bismuth alloy dissolved oxygen pretreatment tank (204) through the third valve (103-3); the second argon gas cylinder (201) is connected to the lead-bismuth alloy dissolved oxygen pretreatment tank (204) through the fourth valve (203-1) to provide gas pressure; the second thermocouple thermometer (205) is connected to the lead-bismuth alloy dissolved oxygen pretreatment tank (204) to detect the temperature of the lead-bismuth alloy therein; and the seventh valve (203-4) is connected to the experimental main loop system (4); The experimental main loop system (4) includes a first, a second, and a third circular pipe (408-1, 408-2, 408-3) having three sections of different diameters. The first, the second, and the third circular pipe (408-1, The first, second and third sample placement boxes (407-1, 407-2 and 407-3) are respectively placed in the first, second and third round pipes (408-1, 408-2 and 408-3); the first, second and third round pipes (408-1, 408-2 and 408-3) are connected to each other through the first, second and third round pipe connectors (409-1, 409-2 and 409-2); the third thermocouple thermometer (406-1), the fourth thermocouple thermometer (406-2) and the fifth thermocouple thermometer (406-3) are respectively arranged on the first, second and third round pipes (408-1, 408-2 and 408-3) to monitor the temperature of the lead-bismuth alloy therein; an electric heating system (410) with PID control is also included; the third argon gas bottle (412) is connected to the electromagnetic pump (403) through the eighth valve (402-3) to provide gas pressure.

2. An experimental system for studying the corrosion behavior of steel in high temperature flowing lead-bismuth alloy according to claim 1, characterized in that: The invention also comprises a lead-bismuth alloy purification system (3), wherein the lead-bismuth alloy purification system (3) comprises a ninth valve (301-1), a lead-bismuth alloy purification device (302), and a tenth valve (301-2) which are connected in series in sequence, one end of the ninth valve (301-1) is connected to a lead-bismuth alloy storage and heating tank (104), and one end of the tenth valve (301-2) is connected to a lead-bismuth alloy dissolved oxygen pretreatment tank (204).

3. The experimental system for studying the corrosion behavior of steel in high temperature flowing lead-bismuth alloy according to claim 1, characterized in that: The volume fractions of argon and oxygen in the mixed gas bottle (206) are 95% and 5% respectively.

4. The experimental system for studying the corrosion behavior of steel in high temperature flowing lead-bismuth alloy according to claim 1, characterized in that: The lead-bismuth alloy storage and supply system (1) is separately arranged from the lead-bismuth alloy dissolved oxygen pretreatment system (2), and a lead-bismuth alloy purification system (3) is arranged in the two systems to ensure the purity of the lead-bismuth alloy returned to the lead-bismuth alloy storage and heating tank (104) after each experiment.

5. An experimental system for studying the corrosion behavior of steel in high temperature flowing lead-bismuth alloy according to claim 1, characterized in that: The first, second and third circular pipes (408-1, 408-2, 408-3) of different diameters of the experimental main loop system (4) can provide three lead-bismuth alloy flow environments with different flow rates under a constant liquid lead-bismuth alloy flow rate.

6. The experimental system for studying the corrosion behavior of steel in high temperature flowing lead-bismuth alloy according to claim 1, characterized in that: The first, second and third sample placement boxes (407-1, 407-2, 407-3) in the experimental main loop system (4) are respectively used to place processed steel sheet samples. Multiple steel sheet samples can be placed in each sample placement box. When placing the samples, the angle between the surface of the steel sheet sample and the direction of the flow velocity of the lead-bismuth alloy can be placed and fixed according to experimental requirements. After each experiment, the sample placement box can be disassembled and the steel sheet samples can be taken out for analysis.

7. An experimental system for studying the corrosion behavior of steel in high temperature flowing lead-bismuth alloy according to claim 1, 5 or 6, characterized in that: The experimental main loop system (4) further comprises an electromagnetic pump (403), an electromagnetic flowmeter (404) and a solid-phase oxygen control device (405). The electromagnetic pump (403), the electromagnetic flowmeter (404) and the solid-phase oxygen control device (405) are arranged in series between the eleventh valve (402-2) and the first circular pipe (408-1). By adjusting the power of the electromagnetic pump (403) so that the reading of the electromagnetic flowmeter (404) reaches the value required for conducting the experiment, the solid-phase oxygen control device (405) adjusts the oxygen content of the lead-bismuth alloy in the loop in real time.

8. An experimental system for studying the corrosion behavior of steel in high temperature flowing lead-bismuth alloy according to claim 1, characterized in that: The first, second and third circular pipes (408-1, 408-2, 408-3) in which the first, second and third sample placement boxes (407-1, 407-2, 407-3) in the experimental main loop system (4) are located should have sufficient straight pipe length to ensure the stability of the flow field of the liquid lead-bismuth alloy initially entering the sample placement boxes.

9. The experimental system for studying the corrosion behavior of steel in high temperature flowing lead-bismuth alloy according to claim 1, characterized in that: The impurity filter (401) in the experimental main loop system (4) can be selectively opened. When opened, it can prevent the impurities in the liquid lead-bismuth alloy from causing scouring and wear effects on the steel sheet samples in the first, second and third sample placement boxes (407-1, 407-2, 407-3). When the impurity filter (401) is not opened, the wear effects of the impurities in the liquid lead-bismuth alloy on the steel sheet samples can be studied.

Citation Information

Patent Citations

  • Experimental system for thermal-hydraulic characteristics and corrosive properties of liquid lead-bismuth alloy

    CN108761022A

  • Experimental system and method for measuring thermal-hydraulic performance and corrosion rate of high-temperature lead-bismuth pump

    CN112096622A

  • Fatigue test device in high-temperature liquid lead-bismuth environment and use method

    CN113203644A

  • Experimental system and method for researching flow heat transfer characteristics of lead-bismuth alloy under marine condition

    CN113670979A

  • Experimental system and method for measuring diving depth of water vapor in lead-bismuth alloy

    CN114974627A

Cited By

  • Liquid lead bismuth comprehensive experiment system

    CN117969589A

  • In-reactor water chemical environment material corrosion test system and test method thereof

    CN119845835A

  • A test system and method for corrosion of materials in an in-pile water chemical environment

    CN119845835B

  • Punching-sliding composite fretting corrosion testing machine suitable for high-temperature lead-bismuth environment

    CN119915661A

  • Experimental device for deposition of corrosion products of lead-bismuth fast reactor fuel assembly

    CN119959088A