Electronic device comprising cover member and method for forming same

A method for forming a cover member with a glass layer and layered reflectance on electronic devices addresses durability and productivity issues, achieving enhanced aesthetics and functionality by using a layered reflectance structure on the glass layer.

WO2026235250A1PCT designated stage Publication Date: 2026-11-12SAMSUNG ELECTRONICS CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
PCT/KR2025/023176
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2025-07-03
Filing Date
2025-12-30
Publication Date
2026-11-12

AI Technical Summary

Technical Problem

Existing methods for forming cover members on electronic devices, such as press thermoforming, suction thermoforming, etching, and partial reflective deposition, face challenges including high equipment costs, limited production volume, reduced durability, and prolonged process times due to issues with etching depth and peeling processes.

Method used

A method involving the formation of a cover member with a glass layer having peaks and valleys, where a first member with a higher reflectance is deposited on the peaks and a second member with lower reflectance is applied to the glass layer and peaks, enhancing durability and aesthetics while reducing process time and defects.

Benefits of technology

The method improves durability and productivity by providing a three-dimensional effect without deep etching, reducing defects, and shortening process time, thus enhancing the external aesthetics and functional performance of electronic devices.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure KR2025023176_12112026_PF_FP_ABST
    Figure KR2025023176_12112026_PF_FP_ABST
Patent Text Reader

Abstract

According to various embodiments, an electronic device comprises a display and a cover member defining at least a portion of the exterior of the electronic device at a position opposite the display, wherein the cover member may comprise: a glass layer comprising a plurality of peaks formed on a first surface and a plurality of valleys formed between adjacent peaks; a first member deposited on the plurality of peaks and having a first reflectance; and a second member deposited on the first surface of the glass layer and the first member and having a second reflectance lower than the first reflectance. In addition, various other embodiments are possible.
Need to check novelty before this filing date? Find Prior Art

Description

Electronic device including a cover member and method of forming the same

[0001] The various embodiments disclosed in this document relate to an electronic device including a cover member and a method for forming the same.

[0002] Electronic devices can be applied to various fields closely integrated into our daily lives. These devices are released in various sizes depending on their functions and user preferences, and external aesthetics, as well as diverse functions and slimness, can be important design elements. For example, even if devices generally possess the same functions, electronic devices with superior and aesthetic designs are more preferred by users.

[0003] The information described above may be provided as related art for the purpose of aiding understanding of the present disclosure. No claim or determination is made as to whether any of the foregoing may be applied as prior art related to the present disclosure.

[0004] The electronic device may include a housing that forms at least a part of the exterior, and at least a part of the housing may include a cover member (e.g., a rear cover, a cover plate, a patterned glass, or a glass plate). For example, a pattern may be formed on the surface of the cover member, and the electronic device may exhibit a three-dimensional effect through the cover member.

[0005] Methods for forming a pattern on the surface of a cover member may include press thermoforming, suction thermoforming, etching (e.g., etching method), or partial reflective and non-reflective deposition methods.

[0006] However, press thermoforming methods using molds and suction thermoforming methods using suction thermoforming machines have high equipment costs and limited production volume, and process costs may increase due to issues with the lifespan of manufacturing machinery. Additionally, while the etching method offers excellent productivity, increasing the etching time to enhance the three-dimensional effect may result in damage to the surface of the cover member or reduced wear resistance, thereby limiting the achievable etching depth. For example, increasing the etching depth improves the three-dimensional effect of the pattern but may reduce the durability of the cover member (e.g., surface durability); conversely, if the etching depth is limited to account for durability, the three-dimensional effect of the pattern may be significantly reduced.

[0007] In the partial reflection and non-reflection deposition method, after the glass layer of the cover member is etched, a printed layer is laminated on a part of the etched glass layer, a reflective layer is laminated on the printed layer, and then the printed layer is peeled off, so that a layer having reflectivity is formed only in a part of the etched glass layer. The partial reflection and non-reflection deposition method requires the process of forming and peeling the printed layer, which may prolong the process time, and productivity may be reduced due to defects caused by the failure to peel off the printed layer.

[0008] Various embodiments of the present disclosure may provide a cover member, a method for forming a cover member, and an electronic device including a cover member, which can contribute to external aesthetics while improving the durability of an electronic device.

[0009] Various embodiments of the present disclosure can provide a cover member with excellent productivity and reduced process time, a method for forming a cover member, and an electronic device including a cover member.

[0010] However, the problems intended to be solved in this disclosure are not limited to those mentioned above, and may be expanded in various ways without departing from the spirit and scope of this disclosure.

[0011] According to various embodiments, an electronic device comprises a display and a cover member forming at least a portion of the exterior of the electronic device at a position facing the display, wherein the cover member may comprise a glass layer comprising a plurality of peaks formed on a first surface and a plurality of valleys formed between adjacent peaks, a first member deposited on the plurality of peaks and having a first reflectance, and a second member deposited on the first surface of the glass layer and the first member and having a second reflectance lower than the first reflectance.

[0012] According to various embodiments, a method for forming a cover member may include the steps of: forming a first layer by depositing a first layer having a first reflectance on a first surface of a substrate of a glass layer; placing a masking member in a first portion of the first layer; etching the first layer and the substrate of the glass layer to form a plurality of valleys formed between a plurality of peaks and adjacent peaks on the first surface of the glass layer, and placing the first member on the plurality of peaks; and forming a second layer by depositing a second member having a second reflectance lower than the first reflectance on the first surface of the glass layer and the first member.

[0013] According to various embodiments, a method for forming a cover member may include the steps of: forming a first layer by depositing a first member having a first reflectance on at least a portion of a first surface of a glass layer base material; placing a masking member on the first layer; etching the glass layer base material to form a plurality of valleys formed between a plurality of peaks and adjacent peaks on the first surface of the glass layer, and placing the first member on the plurality of peaks; and forming a second layer by depositing a second member having a second reflectance lower than the first reflectance on the first surface of the glass layer and the first member.

[0014] An electronic device according to exemplary embodiments of the present disclosure may include a cover member comprising a glass layer having a pattern structure in which a plurality of peaks and a plurality of valleys disposed between adjacent peaks are formed. The cover member may have a laminated structure comprising a first member deposited on the plurality of peaks, a glass layer, and a second member deposited on the first member. Such a laminated structure can improve the durability of the electronic device through the second member deposited to cover the glass layer, and contribute to the external aesthetics of the electronic device by expressing a three-dimensional effect on the cover member through the difference in reflectance between the plurality of peaks on which the first member and the second member are deposited and the plurality of valleys on which only the second member is deposited.

[0015] In addition, since the electronic device according to the exemplary embodiments of the present disclosure does not include a process of forming and peeling off a printed layer, the process time can be shortened and the number of defects caused by unintended non-peeling of the printed layer can be reduced, thereby improving productivity.

[0016] In addition, various effects identified directly or indirectly through this document may be provided.

[0017] The effects obtainable from the present disclosure are not limited to those mentioned above, and other unmentioned effects will be clearly understood by those skilled in the art to which the present disclosure belongs from the description below.

[0018] In relation to the description of the drawings, the same or similar reference numerals may be used for identical or similar components.

[0019] FIG. 1a is a front perspective view of an electronic device according to various embodiments of the present disclosure.

[0020] FIG. 1b is a perspective view of the rear of the electronic device of FIG. 1a according to various embodiments of the present disclosure.

[0021] FIG. 2 is a partial cross-sectional view of a cover member shown along line 2a-2a of FIG. 1b according to various embodiments of the present disclosure.

[0022] FIG. 3 is a process flow diagram illustrating a method for forming a cover member according to various embodiments of the present disclosure.

[0023] FIG. 4 is a drawing illustrating a method for forming a cover member according to various embodiments of the present disclosure.

[0024] FIG. 5 is a drawing illustrating a method for forming a cover member comprising a first member including an organic material according to various embodiments of the present disclosure.

[0025] FIG. 6 is a drawing illustrating a method for forming a cover member including a first member and a second member that induce reflection according to various embodiments of the present disclosure.

[0026] FIG. 7a is a partial cross-sectional view of a cover member including a color layer according to various embodiments of the present disclosure.

[0027] FIG. 7b is a partial cross-sectional view of a cover member comprising a color layer, a reflective layer, and a plurality of adhesive layers according to various embodiments of the present disclosure.

[0028] FIG. 7c is a partial cross-sectional view of a cover member including a color layer, a reflective layer, and a reinforcing layer according to various embodiments of the present disclosure.

[0029] FIG. 7d is a partial cross-sectional view of a cover member comprising a color layer, a reflective layer, a pattern layer, and a plurality of adhesive layers according to various embodiments of the present disclosure.

[0030] Hereinafter, embodiments of the present disclosure are described in detail with reference to the drawings so that those skilled in the art can easily practice them. However, the present disclosure may be embodied in various different forms and is not limited to the embodiments described herein. In relation to the description of the drawings, the same or similar reference numerals may be used for identical or similar components. Furthermore, in the drawings and related descriptions, descriptions of well-known functions and configurations may be omitted for clarity and brevity.

[0031] FIG. 1a is a front perspective view of an electronic device according to various embodiments of the present disclosure. FIG. 1b is a rear perspective view of the electronic device of FIG. 1a according to various embodiments of the present disclosure.

[0032] Referring to FIGS. 1a and 1b, an electronic device (200) according to one embodiment may include a housing (210) comprising a front (210A), a rear (210B), and a side (210C) surrounding the space between the front (210A) and the rear (210B). In other embodiments (not shown), the housing (210) may refer to a structure forming some of the front (210A), the rear (210B), and the side (210C). According to one embodiment, the housing (210) may include a front cover (202) and / or a cover member (300) (e.g., a rear cover, a cover plate, a patterned glass, or a glass plate) coupled to the housing (210). According to one embodiment, the front (210A) may be formed by a front cover (202) in which at least a portion is substantially transparent. The rear surface (210B) may be formed by a cover member (300) in which at least a portion is substantially transparent or translucent. For example, the second surface (210B) may be formed by the cover member (300) in the remaining area, excluding the area that is combined with another electronic device (e.g., a stylus pen or a cover of the electronic device (200)). The side surface (210C) may be formed by a side member (or "side bezel structure") (218) comprising a metal and / or polymer, which is combined with the front cover (202) and the cover member (300). In some embodiments, the cover member (300) and the side member (218) may be formed integrally and may comprise the same material (e.g., a metallic material such as aluminum).

[0033] In one embodiment, the front cover (202) may include a first region (210D) that is curved and seamlessly extended from the front (210A) toward the cover member at both ends of the long edge of the front cover. In one embodiment, the cover member (300) may include a second region (210E) that is curved and seamlessly extended from the rear (210B) toward the front cover at both ends of the long edge. In some embodiments, the front cover (202) or the cover member (300) may include only one of the first region (210D) or the second region (210E). In some embodiments, the front cover (202) and the cover member (300) may not include the first region and the second region, but may include only a flat plane positioned parallel to the rear (210B). In the above embodiments, when viewed from the side of the electronic device, the side member (218) may have a first thickness (or width) on the side side that does not include the first region (210D) or the second region (210E) as above, and may have a second thickness that is thinner than the first thickness on the side side that includes the first region or the second region.

[0034] According to one embodiment, the electronic device (200) may include at least one of a display (201), an input device (203), an audio output device (207, 214), a sensor module (204, 219), a camera module (205, 212, 213), a key input device (217), an indicator (not shown), and a connector (208). In some embodiments, the electronic device (200) may omit at least one of the components (e.g., a key input device (217), or an indicator) or additionally include other components.

[0035] The display (201) may be exposed, for example, through a substantial portion of the front cover (202). In some embodiments, at least a portion of the display (201) may be exposed through the front cover (202) forming the first area (210D) of the front (210A) and the side (210C). The display (201) may be combined with or placed adjacent to a touch sensing circuit, a pressure sensor capable of measuring the intensity (pressure) of the touch, and / or a digitizer that detects a magnetic field-type stylus pen. In some embodiments, at least a portion of the sensor module (204, 219) and / or at least a portion of the key input device (217) may be placed in the first area (210D) and / or the second area (210E).

[0036] The cover member (300) may form at least a portion of the exterior of the electronic device (200) in a position facing, for example, the display (201). With respect to the housing (210) (e.g., side member (218)), the display may be located in a first direction (e.g., +z-axis direction), and the cover member (300) may be located in a second direction (e.g., -z-axis direction).

[0037] The input device (203) may include a microphone. In some embodiments, the input device (203) may include a plurality of microphones positioned to detect the direction of sound. The sound output device (207, 214) may include speakers. The speakers may include an external speaker (207) and a call receiver (214). In some embodiments, the microphone, speakers, and connector (208) may be positioned in the space of the electronic device (200) and may be exposed to the external environment through at least one hole formed in the housing (210). In some embodiments, the hole formed in the housing (210) may be used for both the microphone and the speakers. In some embodiments, the sound output device (207, 214) may include a speaker (e.g., a piezo speaker) that operates with the hole formed in the housing (210) excluded. In some embodiments, the electronic device (200) may include a tray member positioned through at least a portion of the side member (218).

[0038] The sensor module (204, 219) can generate an electrical signal or data value corresponding to an internal operating state of the electronic device (200) or an external environmental state. The sensor module (204, 219) may include, for example, a first sensor module (204) (e.g., proximity sensor) and / or a second sensor module (not shown) (e.g., fingerprint sensor) disposed on the front (210A) of the housing (210), and / or a third sensor module (219) (e.g., HRM sensor) disposed on the rear (210B) of the housing (210). The fingerprint sensor may be disposed on the front (210A) of the housing (210). The fingerprint sensor (e.g., ultrasonic or optical fingerprint sensor) may be disposed below the display (201) on the front (210A). The electronic device (200) may further include at least one of an unillustrated sensor module, for example, a gesture sensor, a gyroscope sensor, a barometric pressure sensor, a magnetic sensor, an accelerometer sensor, a grip sensor, a color sensor, an IR (infrared) sensor, a biosensor, a temperature sensor, a humidity sensor, or an illuminance sensor (204).

[0039] The camera module (205, 212, 213) may include a first camera device (205) positioned on the front (210A) of the electronic device (200), a second camera device (212) positioned on the rear (210B), and / or a flash (213). The camera modules (205, 212) may include one or more lenses, an image sensor, and / or an image signal processor. The flash (213) may include, for example, a light-emitting diode or a xenon lamp. In some embodiments, two or more lenses (wide-angle and telephoto lenses) and image sensors may be positioned on one side of the electronic device (200). In some embodiments, the second camera device (212) may be configured to detect the external environment through a camera window (not shown). The camera window may be formed by a cover member (300) in which at least a portion is substantially transparent or translucent.

[0040] A key input device (217) may be placed on the side (210C) of the housing (210). In another embodiment, the electronic device (200) may not include some or all of the aforementioned key input devices (217), and the key input device (217) not included may be implemented in other forms, such as soft keys, on the display (201). In another embodiment, the key input device (217) may be implemented using a pressure sensor included in the display (201).

[0041] The indicator may be placed, for example, on the front (210A) of the housing (210). The indicator may, for example, provide status information of the electronic device (200) in the form of light. In another embodiment, the light-emitting element may, for example, provide a light source that is coupled with the operation of the camera module (205). The indicator may include, for example, an LED, an IR LED, and a xenon lamp.

[0042] The connector hole (208) may include a first connector hole (208) capable of accommodating a connector (e.g., a USB connector or an IF module (interface connector port module)) for transmitting and receiving power and / or data with an external electronic device, and / or a second connector hole (or earphone jack) capable of accommodating a connector for transmitting and receiving audio signals with an external electronic device.

[0043] Some of the camera modules (205, 212), some of the sensor modules (204, 219), or indicators may be positioned to be exposed through the display (201). For example, the camera module (205), sensor module (204), or indicator may be positioned to come into contact with the external environment through an opening or a transparent area perforated to the front cover (202) of the display (201) within the internal space of the electronic device (200). In one embodiment, the area where the display (201) and the camera module (205) face each other may be formed as a transparent area having a certain transmittance as part of the area for displaying content. In one embodiment, the transparent area may be formed to have a transmittance in the range of about 5% to about 20%. This transparent area may include an area that overlaps with the effective area (e.g., field of view area) of the camera module (205) through which light passes to form an image and generate an image by being formed by an image sensor. For example, the transparent area of ​​the display (201) may include an area with a lower pixel density than the surrounding area. For example, the transparent area may replace the opening. For example, the camera module (205) may include an under-display camera (UDC). In another embodiment, some sensor modules (204) may be positioned to perform their functions without being visually exposed through the front cover (202) within the internal space of the electronic device. For example, in this case, the perforated opening may be unnecessary for the area of ​​the display (201) facing the sensor modules.

[0044] According to various embodiments, the cover member (300) may be formed in a structure in which a plurality of layers (e.g., the glass layer (310) of FIG. 2b, the first member (320), the second member (340), and the third member (350)) are stacked. This stacked structure can improve the durability of the electronic device (200) and contribute to the external aesthetics of the electronic device (200) by expressing a three-dimensional effect through the difference in reflectance between a portion in which at least some of the plurality of layers are stacked and a portion in which all of the plurality of layers are stacked. For example, when light is incident on the cover member (300) from the outside of the electronic device (200), at least some area of ​​the cover member (300) may express a three-dimensional effect due to the difference in reflectance between a portion in which at least some of the plurality of layers are stacked and a portion in which all of the plurality of layers are stacked.

[0045] Furthermore, even if the etching depth (e.g., etching depth) of the glass layer (e.g., glass layer (310) in FIG. 2b) is not set relatively deep, this stacked structure can help improve the durability (e.g., surface durability) of the cover member (300) by providing an improved three-dimensional effect due to the difference in reflectance between the glass layer portion where the first member (e.g., first member (320) in FIG. 2) and the second member (e.g., second member (340) in FIG. 2) are stacked and the glass layer portion where only the second member is stacked. Additionally, the second member can help improve the durability (e.g., surface durability) of the cover member (300) by being stacked to cover the first surface (e.g., first surface (310a) in FIG. 2).

[0046] FIG. 2 is a partial cross-sectional view of a cover member shown along line 2a-2a of FIG. 1b according to various embodiments of the present disclosure.

[0047] Referring to FIG. 2, the cover member (300) may include a glass layer (310), a first member (320) (e.g., a first optical member or a first layer), a second member (340) (e.g., a second optical member or a second layer), and / or a third member (350) (e.g., a third optical member or a third layer). The third member (350) may include a color layer (351) and / or a plurality of adhesive layers (355, 356). In some embodiments, the cover member (300) may omit at least one of the components (e.g., a plurality of adhesive layers (355, 356))) or additionally include other components.

[0048] According to various embodiments, the glass layer (310) may include a first surface (310a) facing outward from the electronic device (e.g., the electronic device (200) of FIG. 1b) and a second surface (310b) facing in the opposite direction to the first surface (310a). The glass layer (310) may be formed of a transparent inorganic material. For example, the glass layer (310) may be formed of at least one of silicon dioxide (SiO2) or other inorganic materials. According to some embodiments, the glass layer (310) may be formed of ceramic, glass fiber reinforced plastic (GFRP), or other composite materials. The glass layer (310) may include a pattern formed on the first surface (310a). The pattern may include a plurality of peaks (311) (e.g., a plurality of peaks) formed on a first surface (310a) and a plurality of valleys (312) (e.g., a plurality of valleys) disposed between the plurality of peaks (311). The plurality of peaks (311) may be at least part of the first surface (310a), and the plurality of valleys (312) may be formed lower than the first surface (310a) by a certain depth. In some embodiments, the plurality of peaks may be formed higher than the first surface. In such cases, the plurality of valleys may be the first surface or may be formed lower than the first surface. In some embodiments, each of the plurality of peaks may include at least a plane. In some embodiments, each of the plurality of valleys may include at least a plane.

[0049] According to various embodiments, the first member (320) (e.g., an AR (anti-reflection) blocking layer or a first reflective layer) may be deposited on a plurality of peaks (311) of the glass layer (310). In one embodiment, the first member (320) may be formed of a transparent inorganic material or of a transparent or translucent organic material.

[0050] According to various embodiments, a second member (340) (e.g., an AR (anti-reflection) layer or a second reflective layer) may be deposited on a first surface (310a) of the glass layer (310) and on a first member (320). For example, the second member (340) may be deposited to cover the first surface (310a) of the glass layer (310) and may be deposited on the first member (320) at a plurality of peaks (311). The second member (340) may be formed of a transparent inorganic material.

[0051] According to various embodiments, a third member (350) (e.g., a deco film layer) may be disposed on a second surface (310b) of the glass layer (310). The third member (350) may block light incident from the outside from entering the interior of the electronic device (e.g., the electronic device (200) of FIG. 1b).

[0052] According to various embodiments, the first member (320) may be deposited on a plurality of peaks (311) of the glass layer (310), and the second member (340) may be deposited on the remaining portion of the glass layer (310) excluding the plurality of peaks (111) of the glass layer (310) (e.g., a plurality of valleys (312)) and the first member (320). The second member (340) may be formed on a portion exposed to the outside of the electronic device (e.g., the electronic device (200) of FIG. 1b) to protect the electronic device from chemical and / or physical shocks applied from the outside of the electronic device, thereby improving the durability of the electronic device.

[0053] According to various embodiments, each of the plurality of peaks (311) may extend from each of the plurality of valleys (312) and be formed alternately with each of the plurality of valleys (312). Although the plurality of peaks (311) and the plurality of valleys (312) have been described separately, the plurality of peaks (311) and the plurality of valleys (312) may not be physically separated. The plurality of peaks (311) and the plurality of valleys (312) may be conceptually separated for convenience of description regarding the glass layer (310). In some embodiments, some of the plurality of peaks may have a different height from the remaining peaks. In some embodiments, some of the plurality of valleys may have a different depth from the remaining valleys. Redundant descriptions are omitted below.

[0054] FIG. 3 is a process flow diagram illustrating a method for forming a cover member according to various embodiments of the present disclosure.

[0055] Referring to FIG. 3, the cover member (300) does not include a separate process for forming and peeling off the printed layer, so the process time can be shortened and the number of defects caused by unintended non-peeling of the printed layer can be reduced, thereby improving productivity.

[0056] According to various embodiments, a cover member (e.g., the cover member (300) of FIG. 4) comprises the operation of forming a first layer (e.g., the first layer (320') of FIG. 4) by depositing a first member (e.g., the first layer (320') of FIG. 4) having a first reflectance on a first surface (e.g., the first surface (310'a) of FIG. 4) of a substrate of a glass layer (e.g., the substrate of a glass layer (310') of FIG. 4), the operation of placing a masking member (e.g., the masking member (330) of FIG. 4) on at least a portion of the first layer, and etching the first layer and the substrate of the glass layer to form a plurality of valleys (e.g., the plurality of peaks (311) of FIG. 4) and adjacent peaks on a first surface (e.g., the first surface (310a) of FIG. 4) of a glass layer (e.g., the glass layer (310) of FIG. 4). It can be formed by the operation of forming a plurality of valleys (312)) of 4 and placing a first member on a plurality of peaks, and by depositing a second member (e.g., the second member (340) of FIG. 4) having a second reflectance lower than the first reflectance on the first surface of the glass layer and the first member to form a second layer (e.g., the second layer (340) of FIG. 4). In one example, the cover member may be formed by further placing a third member (e.g., the third member (350) of FIG. 4) on the second surface of the glass layer (e.g., the second surface (310b) of FIG. 4). In some embodiments, the cover member may be formed by attaching a third member (e.g., the third member (350) of FIG. 4) to the second surface of the glass layer.In some embodiments, the cover member may be formed by the operation of placing a substrate of a glass layer on a third member, the operation of forming a first layer by depositing a first member having a first reflectance on a first surface of the substrate of the glass layer, the operation of placing a masking member on at least a portion of the first layer, the operation of etching the substrate of the first layer and the glass layer to form a plurality of peaks and a plurality of valleys formed between adjacent peaks on the glass layer, and the operation of placing the first member on the plurality of peaks, and the operation of forming a second layer by depositing a second member having a second reflectance lower than the first reflectance on the first surface of the glass layer and the first member. In one embodiment, the etching of the substrate of the first layer and the glass layer is performed using an acid, and the etching operation may further include the operation of removing the masking member placed on the first member. In one embodiment, a plurality of valleys are the remaining portions of a second region of the substrate of the glass layer etched by acid (e.g., the second region (3102) in FIG. 4), and a plurality of peaks may be formed as the portions of the substrate of the glass layer (e.g., the first region (3101) in FIG. 4) that remain unetched, such that a masking member is positioned to cover a first portion of the first layer (e.g., the first portion (321) in FIG. 4). In one embodiment, the first member may refer to a material forming the first layer or may constitute at least a part of the first layer. The second member may refer to a material forming the second layer or may refer to the second layer itself. Although the second member and the second layer have been described separately, this distinction may be conceptual for the convenience of describing the second member and the second layer. Redundant descriptions are omitted below.

[0057] According to various embodiments, a cover member (e.g., cover member (300-1) of FIG. 5) comprises the operation of forming a first layer (e.g., first layer (320-1) of FIG. 5) by depositing a first member (e.g., first member (320-1) of FIG. 5) having a first reflectance on a first surface (e.g., first surface (310'a) of FIG. 5) of a substrate of a glass layer (e.g., substrate of a glass layer (310'-1) of FIG. 5), the operation of placing a masking member (e.g., masking member (330) of FIG. 5) on the first layer, and etching the substrate of the glass layer to form a plurality of valleys (e.g., a plurality of peaks (311) of FIG. 5) and adjacent peaks on a first surface (e.g., first surface (310a) of FIG. 5) of a glass layer (e.g., glass layer (310) of FIG. 5). It can be formed by the operation of forming a plurality of valleys (312)) of 5 and placing a first member on a plurality of peaks, and by depositing a second member (e.g., the second member (340) of FIG. 5) having a second reflectance lower than the first reflectance on the first surface of the glass layer and the first member to form a second layer (e.g., the second layer of FIG. 5). In one embodiment, the cover member can be formed by further placing a third member (e.g., the third member (350) of FIG. 5) on the second surface of the glass layer (e.g., the second surface (310b) of FIG. 5). In some embodiments, the cover member can be formed by combining the third member (e.g., the third member (350) of FIG. 5) with the second surface of the glass layer. In some embodiments, the cover member may be formed by the operation of placing a base material of a glass layer on a third member, the operation of depositing a first member having a first reflectance on the base material of the glass layer to form a first layer, the operation of placing a masking member on the first layer, the operation of etching the base material of the glass layer to form a plurality of peaks and a plurality of valleys formed between adjacent peaks on the glass layer, and the operation of placing the first member on the plurality of peaks, and the operation of depositing a second member having a second reflectance lower than the first reflectance on the first surface of the glass layer and the first member.In one embodiment, the etching of the substrate of the glass layer is performed using acid, and the etching operation may further include the operation of removing a masking member disposed on the first member. In one embodiment, a plurality of valleys are the remaining portions of the second region of the substrate of the glass layer etched by acid (e.g., the second region (3102) in FIG. 5), and a plurality of peaks may be formed as the portions where the first region of the substrate of the glass layer (e.g., the first region (3101) in FIG. 5) is not etched and remains, such that the masking member is disposed to cover the first layer. In one embodiment, the first member may refer to a material forming the first layer or the first layer itself. Although the first member and the first layer have been described separately, this distinction may be conceptual for the convenience of describing the first member and the first layer.

[0058] FIG. 4 is a drawing illustrating a method for forming a cover member according to various embodiments of the present disclosure.

[0059] The cover member (300) of FIG. 4 may be at least partially similar to the cover member (300) of FIG. 1b and the cover member (300) of FIG. 2, or may include other embodiments of the cover member. Redundant descriptions are omitted below.

[0060] Referring to FIG. 4(a), a first layer (320') can be formed by depositing a first member (320) having a first reflectance on a first surface (310'a) of a glass layer substrate (310'). In one embodiment, the first member (320) can be deposited on the first surface (310'a) with a thickness of about 500 nm or less by an electron beam mechanism to form a first layer (320'). The glass layer substrate (310') may include a first region (3101) and a second region (3202). The first layer (320') may include a first portion (321) and a second portion (322) extending from the first portion (321). A first part (321) may be placed in a first area (3101), and a second part (322) may be placed in a second area (3202). A masking member (330) (e.g., a masking layer) may be placed in the first part (321) of the first layer (320').

[0061] According to various embodiments, the masking member (330) may be formed as a single layer through which a portion corresponding to a second region (3102) of the base material (310') of the glass layer and a second portion (322) of the first layer (320') is penetrated. The masking member (330) may be formed from an acid-resistant material (e.g., acid-resistant ink). In one embodiment, the masking member (330) may be formed by applying a photosensitive material, such as a resist (e.g., dry film resist (DFR) or photoresist (PR)), to the first layer (320'), then irradiating light (e.g., ultraviolet (UV)) onto the resist through a mask, and removing the portion of the resist irradiated with ultraviolet light through a development process. In one embodiment, the masking member (330) may be formed by selectively printing acid-resistant ink onto the first layer (320') through a screen mesh with a pattern formed thereon.

[0062] Referring to FIG. 4(b), at least a portion of the base material (310') of the glass layer and the first layer (320') can be etched (e.g., etched) through an acid. For example, a second region (3102) of the base material (310') of the glass layer and a second portion (322) of the first layer (320') can be etched through an acid. Through this, the first member (320) and the glass layer (310) can be formed. A plurality of peaks (311) of the glass layer (310) can be formed such that a masking member (330) is positioned to cover a first portion (321) of the first layer (320'), so that the first region (3101) of the base material (310') of the glass layer remains unetched. A plurality of valleys (312) of the glass layer (310) may be formed from the remaining portion of the second region (3202) of the base material (310') of the glass layer etched by acid.

[0063] According to various embodiments, the base material (310') of the glass layer and the first layer (320') may be formed of a transparent inorganic material. For example, the base material (310') of the glass layer may be formed of at least one of silicon dioxide (SiO2) or other inorganic materials. According to some embodiments, the base material (310') of the glass layer may be formed of ceramic, GFRP (glass fiber reinforced plastic), or other composite materials.

[0064] According to various embodiments, a second portion (322) of the first layer (320') and a second region (3102) of the substrate (310') of the glass layer may be etched to a specific depth from the first surface (310'a) through acid. The substrate (310') of the glass layer and the first layer (320') may each have an etching rate (e.g., etching rate) of about 1 µm / min (micrometer per minute). When the acid is applied, the masking member (330) is formed of an acid-resistant material, so the masking member (330), the first portion (321) of the first layer (320') where the masking member (330) is placed, and the first region (3101) of the substrate (310') of the glass layer where the first portion (321) is placed may not be etched by the acid. A first region (3101) of the substrate (310') of the glass layer under the first member (320) that is not etched through the masking member (330) may form a plurality of peaks (311). In a region other than the masking member (330), an etched second region (3202) of the substrate (310') of the glass layer, together with a second portion (322) of the first layer (320'), may form a plurality of valleys (312). Thus, the first member (320) may be deposited only on the plurality of peaks (311) (e.g., planar regions of the plurality of peaks (311)) of the finally provided glass layer (310). In one embodiment, after forming a glass layer (310) comprising a plurality of peaks (311) and a plurality of valleys (312) and a first member (320) deposited on the plurality of peaks (311), the masking member (330) can be removed from the first member (320).

[0065] According to various embodiments, chemical etching (e.g., wet etching) may be carried out chemically using hydrofluoric acid (HF), ammonium fluoride (NH4F), or other acids. Etching may proceed at the same speed in the vertical and horizontal directions by an isotropic etching mechanism. As a result, the first surface (310a) of the substrate (310') of the glass layer may be formed with an undercut shape that is wider at the top and narrower at the bottom. In some embodiments, if the substrate (310') of the glass layer comprises ceramic or GFRP (glass fiber reinforced plastic), mechanical etching (e.g., mechanical etching) may be carried out by a CNC (computer numerical control) mechanism.

[0066] Referring to FIG. 4(c), a second member (340) can be formed by depositing a second member (340) on a first surface (310a) of a glass layer (310) and a first member (320). For example, the second member (340) can be deposited to cover the first surface (310a) of the glass layer (310) and deposited on the first member (320) at a plurality of peaks (311) to form the second layer (340). In one embodiment, the first member (320) and the second member (340) can be deposited at a plurality of peaks (311), and the second member (340) can be deposited at a plurality of valleys (312). In one embodiment, the second member (340) may be deposited on the first surface (310a) of the glass layer (310) and the first member (320) with a thickness of about 1.5 to 2.5 μm (micrometer) by an inductively coupled plasma (ICP) sputtering mechanism to form a second layer (2340). In one embodiment, the second member (340) may be formed to have a second reflectance lower than the first reflectance of the first member (320). In one embodiment, the second member (340) may be formed thicker than the first member (320).

[0067] According to various embodiments, the second member (340) may be formed from a transparent inorganic material. For example, the second member (340) may be formed from at least one of silicon dioxide (SiO2), silicon nitride (Si3N4), silicon oxynitride (SiON), or other inorganic materials. In one embodiment, the second member (340) may be formed by stacking a plurality of layers, approximately 10 to 20 layers. For example, the second member (340) may be formed by sequentially stacking silicon nitride (Si3N4) 10 nm, silicon dioxide (SiO2) 90 nm, silicon nitride 40 nm, silicon dioxide 100 nm, silicon nitride 65 nm, silicon dioxide 50 nm, silicon nitride 15 nm, silicon dioxide 70 nm, and silicon nitride 85 nm. In one embodiment, when light is incident on the cover member (300) from the outside of an electronic device (e.g., electronic device (200) of FIG. 1b), the second member (340) may have a reflectance of less than 4%.

[0068] According to various embodiments, the second member (340) may be formed with an indentation hardness of about 10 GPa or more. Even if the etching depth of the base material (310') of the glass layer is increased by increasing the etching time with acid, or even if the pattern of the glass layer (310) (e.g., a plurality of peaks (311) and a plurality of valleys (312)) is implemented more finely, the durability of the electronic device (e.g., the electronic device (200) of FIG. 1B) can be secured by the second member (340) deposited to cover the first surface (310a) of the glass layer (310). As the durability of the portion exposed to the outside of the electronic device is improved by the second member (340), various patterns can be implemented on the glass layer (310).

[0069] Referring to FIG. 4(d), a third member (350) may be disposed on a second surface (310b) of the glass layer (310). The third member (350) may include a color layer (351) (e.g., a shielding printing layer) and a plurality of adhesive layers (355, 356) disposed between the second surface (310b) of the glass layer (310) and the color layer (351). The color layer (351) may include black or other colors.

[0070] According to various embodiments, the color layer (351) can block external light from entering the interior of the electronic device. A plurality of adhesive layers may include a first adhesive layer (355) and a second adhesive layer (356). The first adhesive layer (355) may include, for example, an optically clear adhesive (OCA). The second adhesive layer (356) may include, for example, a polyethylene terephthalate (PET) material. The first adhesive layer (355) and the second adhesive layer (356) are disposed between the color layer (351) and the glass layer (310) to adhere the color layer (351) to the glass layer (310).

[0071] According to various embodiments, the glass layer (310), the first member (320), the second member (340), and the plurality of adhesive layers (355, 356) are formed of a substantially transparent material, so that when light is incident on the cover member (300) from outside the electronic device (e.g., the electronic device (200) of FIG. 1b), the color observed on the cover member (300) may refer to the color of the color layer (351).

[0072] According to various embodiments, the second member (340) may refer to a layer that suppresses reflection of the cover member (300) when light is incident on the cover member (300) from outside the electronic device (e.g., the electronic device (200) of FIG. 1b). The first member (320) may refer to a layer formed such that the reflection suppression function of the second member (340) is at least partially limited by depositing the second member (340) on the first member (320). The first member (320) may be formed of at least one of silicon dioxide (SiO2) or other inorganic materials. A three-dimensional effect may be formed on the cover member (300) through the difference in reflectance between the plurality of peaks (311) on which the first member (320) and the second member (340) are deposited and the plurality of valleys (312) on which the second member (340) is deposited. For example, when light is incident on a cover member (300) from the outside of an electronic device, the brightness of the color layer (351) observed in a plurality of peaks (311) where the first member (320) and the second member (340) are deposited can be formed to be higher than the brightness of the color layer (351) observed in a plurality of valleys (312) where the second member (340) is deposited.

[0073] According to various embodiments, the second member (340) may refer to a layer that suppresses reflection of the cover member (300) when light is incident on the cover member (300) from outside the electronic device (e.g., the electronic device (200) of FIG. 1b). The first member (320) may refer to a layer that induces reflection of the cover member (300) by depositing the second member (340) on the first member (320). The first member (320) may be formed of at least one of silicon dioxide (SiO2), titanium dioxide (TiO2), aluminum oxide (Al2O3), niobium pentoxide (Nb2O3), or other inorganic materials.

[0074] According to various embodiments, the first member (320) may be formed by stacking a plurality of layers. For example, the first member (320) may be formed by sequentially stacking silicon dioxide (SiO2) 35 nm, titanium dioxide (TiO2) 15 nm, and silicon dioxide 40 nm. In one embodiment, when light of a wavelength of 450 nm is incident on the cover member (300) from the outside of the electronic device, the first member (320) may have a reflectance of 20%.

[0075] According to various embodiments, a first member (320) and a second member (340) may be deposited on a plurality of peaks (311) of the glass layer (310), and a second member (340) may be deposited on a plurality of valleys (312) of the glass layer (310). In one embodiment, on a plurality of peaks (311) of the glass layer (310), a first member (320) in which silicon dioxide 35 nm, titanium dioxide 15 nm, and silicon dioxide 40 nm are sequentially stacked, and a second member (340) in which silicon nitride 10 nm, silicon dioxide 90 nm, silicon nitride 40 nm, silicon dioxide 100 nm, silicon nitride 65 nm, silicon dioxide 50 nm, silicon nitride 15 nm, silicon dioxide 70 nm, and silicon nitride 85 nm are sequentially stacked may be deposited. In one embodiment, when light is incident on the cover member (300) from the outside of the electronic device, the first member (320) and the second member (340) may have a reflectance of 70%. In one embodiment, a second member (340) may be deposited in a plurality of valleys (312) of the glass layer (310), wherein silicon nitride 10 nm, silicon dioxide 90 nm, silicon nitride 40 nm, silicon dioxide 100 nm, silicon nitride 65 nm, silicon dioxide 50 nm, silicon nitride 15 nm, silicon dioxide 70 nm, and silicon nitride 85 nm are sequentially stacked. In one embodiment, when light is incident on the cover member (300) from the outside of the electronic device, the second member (340) may have a reflectance of less than 4%. A three-dimensional effect can be formed in the cover member (300) through the difference in reflectance between the plurality of peaks (311) on which the first member (320) and the second member (340) are deposited and the plurality of valleys (312) on which the second member (340) is deposited. In one embodiment, when light is incident on the cover member (300) from outside the electronic device, the brightness of the color layer (351) can be formed high due to the optical interference effect between the first member (320) and / or the second member (340) at the plurality of peaks (311) of the glass layer (310).For example, when light is incident on a cover member (300) from the outside of an electronic device, the brightness of the color layer (351) observed in a plurality of peaks (311) where the first member (320) and the second member (340) are deposited can be formed to be higher than the brightness of the color layer (351) observed in a plurality of valleys (312) where the second member (340) is deposited.

[0076] In various embodiments, the brightness of the color layer (351) observed at a plurality of peaks (311) due to the optical interference effect between the first member (320) and the second member (340) can be predicted by simulation, and the range of brightness achievable can be varied depending on the combination of various inorganic materials. As a result, various color patterns can be implemented on the cover member (300).

[0077] FIG. 5 is a drawing illustrating a cover member including a first member including an organic material according to various embodiments of the present disclosure and a method for forming a cover member.

[0078] The cover member (300-1) of FIG. 5 may be at least partially similar to the cover member (300) of FIG. 1b, the cover member (300) of FIG. 2, and the cover member (300) of FIG. 4, or may include other embodiments of the cover member. The first member (320-1) of FIG. 5 may be at least partially similar to the first member (320) of FIG. 2 and the first member (320) of FIG. 4, or may include other embodiments of the first member. Redundant descriptions are omitted below.

[0079] Referring to FIG. 5(a), a first layer (320-1) may be formed by depositing a first member (320-1) having a first reflectance on at least a portion of the first surface (310'a) of the substrate (310') of the glass layer. In one embodiment, the first member (320-1) may be deposited on at least a portion of the first surface (310'a) with a thickness of about 1 nm or more and 10 nm or less by a screen printing mechanism, a gravure printing mechanism, a reverse offset printing mechanism, or a pad printing mechanism to form the first layer (320-1). The substrate (310') of the glass layer may include a first region (3101) and a second region (3202). The first member (320-1) may be deposited on the first region (3101). A masking member (330) (e.g., a masking layer) may be placed on the first member (320-1).

[0080] According to various embodiments, the masking member (330) may be formed as a single layer through which a portion corresponding to a second region (3102) of the base material (310') of the glass layer is penetrated. In one embodiment, the masking member (330) may be formed by applying a photosensitive material, such as a resist (e.g., dry film resist (DFR) or photoresist (PR)), to the first member (320-1), then irradiating light (e.g., ultraviolet (UV)) onto the resist through a mask, and removing the portion of the resist irradiated with ultraviolet light through a development process. In one embodiment, the masking member (330) may be formed by selectively printing acid-resistant ink onto the first member (320-1) through a patterned screen mesh.

[0081] Referring to FIG. 5(b), at least a portion of the base material (310') of the glass layer can be etched (e.g., etched) through an acid. For example, a second region (3102) of the base material (310') of the glass layer can be etched through an acid. Through this, the glass layer (310) can be formed. A plurality of peaks (311) of the glass layer (310) can be formed as a portion where the first region (3101) of the base material (310') of the glass layer remains unetched, by positioning a masking member (330) to cover the first member (320-1). A plurality of valleys (312) of the glass layer (310) can be formed as a portion of the second region (3202) of the base material (310') of the glass layer that was etched by the acid.

[0082] According to various embodiments, the base material (310') of the glass layer may be formed from a transparent inorganic material. For example, the base material (310') of the glass layer may be formed from at least one of silicon dioxide (SiO2) or other inorganic materials. According to some embodiments, the base material (310') of the glass layer may be formed from ceramic, GFRP (glass fiber reinforced plastic), or other composite materials. The first member (320-1) may be formed from a transparent or translucent organic material. For example, the first member (320-1) may be formed from at least one of an acrylic-based polymer, an epoxy-based polymer, a polyester-based polymer, a siloxane-based polymer, a silsesquioxane-based polymer, or other organic materials. The first component (320-1) may include a dye or pigment.

[0083] According to various embodiments, a second region (3102) of the base material (310') of the glass layer can be etched to a specific depth from the first surface (310'a) through an acid. When the acid is applied, the masking member (330) is formed of an acid-resistant material, so the masking member (330), the first member (320-1) on which the masking member (330) is disposed, and the first region (3101) of the base material (310') of the glass layer on which the first member (320-1) is deposited may not be etched by the acid. The first region (3101) of the base material (310') of the glass layer below the first member (320-1) that is not etched through the masking member (330) may form a plurality of peaks (311). In an area other than the masking member (330), the etched second region (3202) of the base material (310') of the glass layer may form a plurality of valleys (312). Accordingly, the first member (320-1) may be deposited only on the plurality of peaks (311) of the finally formed glass layer (310) (e.g., planar regions of the plurality of peaks (311)). In one embodiment, after forming the glass layer (310) including the plurality of peaks (311) and the plurality of valleys (312), the masking member (330) may be removed from the first member (320-1).

[0084] According to various embodiments, the second member (340) may refer to a layer that suppresses reflection of the cover member (300-1) when light is incident on the cover member (300-1) from outside of an electronic device (e.g., electronic device (200) of FIG. 1b). The first member (320-1) may refer to a layer formed such that the reflection suppression function of the second member (340) is at least partially limited by depositing the second member (340) on the first member (320-1). A three-dimensional effect may be formed on the cover member (300) through the difference in reflectance between the plurality of peaks (311) on which the first member (320-1) and the second member (340) are deposited and the plurality of valleys (312) on which the second member (340) is deposited. In one embodiment, when light is incident on a cover member (300-1) from outside the electronic device, the brightness of the color layer (351) can be formed high due to the optical interference effect between the first member (320-1) and / or the second member (340) at a plurality of peaks (311) of the glass layer (310). For example, when light is incident on a cover member (300-1) from outside the electronic device, the brightness of the color layer (351) observed at a plurality of peaks (311) where the first member (320-1) and the second member (340) are deposited can be formed to be higher than the brightness of the color layer (351) observed at a plurality of valleys (312) where the second member (340) is deposited.

[0085] FIG. 6 is a drawing illustrating the manufacturing process of a cover member including a first member and a second member that induce reflection according to various embodiments of the present disclosure.

[0086] The cover member (300-2) of FIG. 6 may be at least partially similar to the cover member (300) of FIG. 1b, the cover member (300) of FIG. 2, the cover member (300) of FIG. 4, and the cover member (300-1) of FIG. 5, or may include other embodiments of the cover member. The first member (320-2) of FIG. 6 may be at least partially similar to the first member (320) of FIG. 2, the first member (320) of FIG. 4, and the first member (320-1) of FIG. 5, or may include other embodiments of the first member. The second member (340-1) of FIG. 6 may be at least partially similar to the second member (340) of FIG. 2, the second member (340) of FIG. 4, and the second member (340) of FIG. 5, or may include other embodiments of the second member. The third member (350-1) of FIG. 6 may be at least partially similar to the third member (350) of FIG. 2, the third member (350) of FIG. 4, and the third member (350) of FIG. 5, or may include other embodiments of the third member. The color layer (351-1) of FIG. 6 may be at least partially similar to the color layer (351) of FIG. 2, the color layer (351) of FIG. 4, and the color layer (351) of FIG. 5, or may include other embodiments of the color layer. Redundant descriptions are omitted below.

[0087] Referring to FIG. 6(d), a third member (350-1) may be disposed on a second surface (310b) of a base material (310') of a glass layer. The third member (350-1) may include a color layer (351-1) and a plurality of adhesive layers (355, 356) laminated on the color layer (351-1). The color layer (351-1) may include white or other colors.

[0088] According to various embodiments, the second member (340-1) may refer to a layer that induces reflection of the cover member (300-2) when light is incident on the cover member (300-2) from outside the electronic device (e.g., the electronic device (200) of FIG. 1b). The first member (320-2) may refer to a layer that induces reflection of the cover member (300-2) by depositing the second member (340-1) on the first member (320-2). The first member (320-2) may be formed of at least one of silicon dioxide (SiO2), titanium dioxide (TiO2), aluminum oxide (Al2O3), niobium pentoxide (Nb2O3), or other inorganic materials. The second member (340-1) may include at least one of silicon dioxide (SiO2), titanium dioxide (TiO2), aluminum oxide (Al2O3), niobium pentoxide (Nb2O3), silicon nitride (Si3N4), silicon oxynitride (SiON), or other inorganic materials. A three-dimensional effect may be formed on the cover member (300-2) through the difference in reflectance between the plurality of peaks (311) on which the first member (320-2) and the second member (340-1) are deposited and the plurality of valleys (312) on which the second member (340) is deposited. In one embodiment, when light is incident on the cover member (300-2) from the outside of the electronic device, the brightness of the color layer (351-1) can be formed high due to the optical interference effect between the first member (320-2) and the second member (340-1) at a plurality of peaks (311) of the glass layer (310).For example, when light is incident on a cover member (300-2) from the outside of an electronic device, the brightness of the color layer (351-1) observed in a plurality of peaks (311) where the first member (320-2) and the second member (340-1) are deposited can be formed to be higher than the brightness of the color layer (351-1) observed in a plurality of valleys (312) where the second member (340-1) is deposited.

[0089] According to various embodiments, when light is incident from outside the electronic device (e.g., the electronic device (200) of FIG. 1b), the brightness of the color layer (351-1) observed in a plurality of peaks (311) where the first member (320-2) and the second member (340-1) are deposited can be formed to be similar to the brightness of the color layer (351-1) observed in a plurality of valleys (312) where the second member (340-1) is deposited. For example, the brightness of the color layer (351-1) in the plurality of peaks (311) where the first member (320-2) and the second member (340-1) are deposited includes a brightness of the same series according to the Munsell color system as the brightness of the color layer (351-1) in the plurality of valleys (312) where the second member (340-1) is deposited, and can be observed as a higher brightness than the brightness of the color layer (351-1) in the plurality of valleys (312) where the second member (340-1) is deposited.

[0090] FIG. 7a is a drawing illustrating a cover member including a color layer according to various embodiments of the present disclosure. FIG. 7b is a drawing illustrating a cover member including a color layer, a reflective layer, and a plurality of adhesive layers according to various embodiments of the present disclosure. FIG. 7c is a drawing illustrating a cover member including a color layer, a reflective layer, and a reinforcing layer according to various embodiments of the present disclosure. FIG. 7d is a drawing illustrating a cover member including a color layer, a reflective layer, a pattern layer, and a plurality of adhesive layers according to various embodiments of the present disclosure.

[0091] The cover member (300-3) of FIG. 7a, the cover member (300-4) of FIG. 7b, the cover member (300-5) of FIG. 7c, and the cover member (300-6) of FIG. 7d may be at least partially similar to the cover member (300) of FIG. 1b, the cover member (300) of FIG. 2, the cover member (300) of FIG. 4, the cover member (300-1) of FIG. 5, and the cover member (300-2) of FIG. 6, or may include other embodiments of the cover member. The third member (350-2) of FIG. 7a, the third member (350-3) of FIG. 7b, the third member (350-4) of FIG. 7c, and the third member (350-5) of FIG. 7d may be at least partially similar to the third member (350) of FIG. 2, the third member (350) of FIG. 4, the third member (350) of FIG. 5, and the third member (350-1) of FIG. 6, or may include other embodiments of the third member. The color layer (351) of FIG. 7a may be at least partially similar to the color layer (351) of FIG. 2, the color layer (351) of FIG. 4, the color layer (351) of FIG. 5, and the color layer (351-1) of FIG. 6, or may include other embodiments of the color layer. Redundant descriptions are omitted below.

[0092] Referring to FIG. 7a, a third member (350-2) may be laminated on the second surface (310b) of the glass layer (310). The third member (350-2) may include a color layer (351).

[0093] According to various embodiments, the color layer (351) may include black, white, or other colors.

[0094] Referring to FIG. 7b, a third member (350-3) may be laminated on a second surface (310b) of a glass layer (310). The third member (350-3) may include a color layer (351), a reflective layer (352), and a plurality of adhesive layers (355, 356). The plurality of adhesive layers (355, 356) may be laminated on the second surface (310b) of the glass layer (310). The reflective layer (352) may be laminated on the plurality of adhesive layers (355, 356). The color layer (351) may be laminated on the reflective layer (352).

[0095] According to various embodiments, the reflective layer (352) may comprise a metal (e.g., aluminum (Al), silver (Ag), or chromium (Cr)), an inorganic material (titanium dioxide (TiO2), niobium pentoxide (Nb2O5), silicon dioxide (SiO2), aluminum oxide (Al2O3)), or other reflective deposition materials. In one embodiment, the reflective layer (352) may reflect light reaching the color layer (351) when light is incident on the cover member (300-4) from the outside of the electronic device (e.g., the electronic device (200) of FIG. 1b), thereby increasing the brightness and / or lightness of the color of the color layer (351). In one embodiment, the glass layer (310) is formed of a substantially transparent material, so that when light is incident on the cover member (300-4) from the outside of the electronic device, the color observed through the plurality of peaks (311) and plurality of valleys (312) of the glass layer (310) may refer to the color of the color layer (351) reflected by the reflective layer (352).

[0096] Referring to FIG. 7c, a third member (350-4) may be laminated on a second surface (310b) of a glass layer (310). The third member (350-4) may include a color layer (351), a reflective layer (352), and a reinforcing layer (354) (e.g., a buffer layer). The reinforcing layer (354) may be laminated on the second surface (310b) of the glass layer (310). The reflective layer (352) may be laminated on the reinforcing layer (354). The color layer (351) may be laminated on the reflective layer (352).

[0097] According to various embodiments, the reinforcing layer (354) is positioned between the glass layer (310) and the color layer (351) to reduce the phenomenon of reduced impact strength of the glass layer (310) that may occur when the color layer (351) is directly laminated to the second surface (310b) of the glass layer (310). The reinforcing layer (354) is positioned between the glass layer (310) and the reflective layer (352) to prevent the phenomenon of the reflective deposition material of the reflective layer (352) diffusing into the glass layer (310). The reinforcing layer (354) may include a silicone-based polymer (e.g., polydimethylsiloxane (PDMS), silicone rubber, siloxane-based resin). The reinforcing layer (354) may be formed with a thickness of about 1 μm (micrometer).

[0098] Referring to FIG. 7d, a third member (350-5) may be laminated on a second surface (310b) of a glass layer (310). The third member (350-5) may include a color layer (351), a reflective layer (352), a pattern layer (353), and a plurality of adhesive layers (355, 356). The plurality of adhesive layers (355, 356) may be laminated on the second surface (310b) of the glass layer (310). The pattern layer (353) may be laminated on the plurality of adhesive layers (355, 356). The reflective layer (352) may be laminated on the pattern layer (353). The color layer (351) may be laminated on the reflective layer (352).

[0099] According to various embodiments, the pattern layer (353) may include a resin (e.g., acrylic, urethane, or epoxy resin) that hardens when irradiated with ultraviolet (UV) light. The pattern layer (353) may be formed, for example, as a prism pattern, which is a three-dimensional structure with an uneven shape (e.g., triangle or sawtooth shape), a lenticular pattern, which is a repeating arc shape, a Fresnel pattern, which includes a plurality of stepped surfaces arranged in a concentric direction, or a hologram pattern, which is a diffraction grating structure with a period in the nanometer range (e.g., nm). In one embodiment, the pattern layer (353) may provide a three-dimensional effect, texture, and / or pattern (e.g., interference pattern) to an electronic device (e.g., electronic device (200) of FIG. 1b). A pattern layer reflective layer (352) may be laminated onto the pattern layer (353) in correspondence with the pattern shape of the pattern layer (353). In one embodiment, when light is incident on a cover member (300-6) from the outside of an electronic device, the light reaching the color layer (351) may be refracted or scattered by the pattern shape of the pattern layer (353), then reflected by the reflection layer (352) and pass through the color layer (351) again or be reflected from the color layer (351). As a result, the brightness and / or lightness of the color of the color layer (351) can be increased.

[0100] According to various embodiments, an electronic device (e.g., the electronic device (200) of FIG. 1b) comprises a display (e.g., the display (201) of FIG. 1a), and a cover member (e.g., the cover member (300) of FIG. 1b, the cover member (300-1) of FIG. 5, the cover member (300-2) of FIG. 6, the cover member (300-3) of FIG. 7a, the cover member (300-4) of FIG. 7b, the cover member (300-5) of FIG. 7c, or the cover member (300-6) of FIG. 7d) forming at least a portion of the exterior of the electronic device at a position facing the display, wherein the cover member comprises a glass layer (e.g., FIG. 2a) comprising a plurality of peaks (e.g., the plurality of peaks (311) of FIG. 2a) formed on a first surface (e.g., the first surface (310a) of FIG. 2a)) and a plurality of valleys (e.g., the plurality of valleys (312) of FIG. 2a) formed between adjacent peaks (e.g., FIG. 2a It may include a glass layer (310) of 2a), a first member (e.g., the first member (320) of FIG. 2, the first member (320-1) of FIG. 5, or the first member (320-2) of FIG. 6) that is deposited on the plurality of peaks and has a first reflectance, and a second member (e.g., the second member (340) of FIG. 2) that is deposited on the first surface of the glass layer and the first member and has a second reflectance lower than the first reflectance.

[0101] According to various embodiments, the cover member may include a third member (e.g., the third member (350) of FIG. 2, the third member (350-1) of FIG. 6, the third member (350-2) of FIG. 7a, the third member (350-3) of FIG. 7b, the third member (350-4) of FIG. 7c, and the third member (350-5) of FIG. 7d) laminated on a second surface (e.g., the second surface (310b) of FIG. 2) or the third member (350-5) of FIG. 7d) of FIG. 7d, and the third member may include a color layer (e.g., the color layer (351) of FIG. 2 or the color layer (351-1) of FIG. 6) disposed on the second surface of the glass layer.

[0102] According to various embodiments, the third member may include a plurality of adhesive layers (e.g., a plurality of adhesive layers (355, 356) of FIG. 2) disposed between the second surface of the glass layer and the color layer.

[0103] According to various embodiments, the third member may include a reflective layer (e.g., the reflective layer (352) of FIG. 7b) disposed between the color layer and the plurality of adhesive layers.

[0104] According to various embodiments, the third member may include a reflective layer disposed on the color layer (e.g., the reflective layer (352) of FIG. 7c), and a reinforcing layer (e.g., the reinforcing layer (354) of FIG. 7c) laminated between the second surface of the glass layer and the reflective layer to prevent the reflective material of the reflective layer from diffusing into the glass layer.

[0105] According to various embodiments, the third member comprises a reflective layer disposed on the color layer (e.g., the reflective layer (352) of FIG. 7d), and a pattern layer disposed between the plurality of adhesive layers and the reflective layer (e.g., the pattern layer (353) of FIG. 7d), and the pattern layer may form a three-dimensional effect, texture, and / or pattern on the cover member.

[0106] According to various embodiments, the pattern layer may be formed as a prism pattern, a lenticular pattern, a Fresnel pattern, or a holographic pattern.

[0107] According to various embodiments, when light is incident from outside the electronic device, the luminance or brightness of the color layer observed at the plurality of peaks where the first member and the second member are deposited can be formed to be higher than the luminance or brightness of the color layer observed at the plurality of valleys where the second member is stacked.

[0108] According to various embodiments, when light is incident from outside the electronic device, the brightness of the color layer observed at the plurality of peaks where the first member and the second member are deposited can be formed to be similar to the brightness of the color layer observed at the plurality of valleys where the second member is deposited.

[0109] According to various embodiments, in a method for forming a cover member (e.g., cover member (300) of FIG. 1b, cover member (300-2) of FIG. 6, cover member (300-3) of FIG. 7a, cover member (300-4) of FIG. 7b, cover member (300-5) of FIG. 7c, or cover member (300-6) of FIG. 7d), the method comprises the step of depositing a first member (e.g., first member (320) of FIG. 4 or first member (320-2) of FIG. 6) having a first reflectance on a first surface (e.g., first surface (310'a) of FIG. 4) of a substrate of a glass layer (e.g., substrate (310') of FIG. 4) to form a first layer (e.g., first layer (320') of FIG. 4 or first layer (320'-2) of FIG. 6), and a masking member (e.g., FIG. 1) on at least a portion of the first layer. The method may include the operation of placing a masking member (330) of 4, etching the base material of the first layer and the glass layer to form a plurality of peaks (e.g., a plurality of peaks (311) of Fig. 4) and a plurality of valleys (e.g., a plurality of valleys (312) of Fig. 4) formed between adjacent peaks on a first surface (e.g., a first surface (310a) of Fig. 4) of the glass layer (e.g., a glass layer (310) of Fig. 4), and placing the first member on the plurality of peaks, and depositing a second member (e.g., a second member (340) of Fig. 4 or a second member (340-1) of Fig. 6) having a second reflectance lower than the first reflectance on the first surface of the glass layer and the first member to form a second layer (e.g., a second member (340) of Fig. 4 or a second member (340-1) of Fig. 6).

[0110] According to various embodiments, the operation further includes placing a third member (e.g., the third member (350) of FIG. 4, the third member (350-1) of FIG. 6, the third member (350-2) of FIG. 7a, the third member (350-3) of FIG. 7b, the third member (350-4) of FIG. 7c, or the third member (350-5) of FIG. 7d) on a second surface (e.g., the second surface (310b) of FIG. 4) facing the first surface of the glass layer, and the third member may include a color layer (e.g., the color layer (351) of FIG. 4 or the color layer (351-1) of FIG. 6) placed on the second surface of the glass layer.

[0111] According to various embodiments, the glass layer, the first member, and / or the second member may be formed of a transparent inorganic material.

[0112] According to various embodiments, the etching of the substrate of the first layer and the glass layer is performed using acid, and the operation may further include the operation of removing the masking member disposed on the first member.

[0113] According to various embodiments, in a method for forming a cover member (e.g., cover member (300) of FIG. 1b, cover member (300-1) of FIG. 5, cover member (300-3) of FIG. 7a, cover member (300-4) of FIG. 7b, cover member (300-5) of FIG. 7c, or cover member (300-6) of FIG. 7d), the method comprises the steps of: forming a first layer (e.g., first layer (320-1) of FIG. 5) by depositing a first member (e.g., first member (320-1) of FIG. 5) having a first reflectance on at least a portion of a first surface (e.g., first surface (310'a) of FIG. 5) of a base material of a glass layer (e.g., base material of FIG. 5 (310')); placing a masking member (e.g., masking member (330) of FIG. 5) on the first layer; and etching the base material of the glass layer. The method may include forming a plurality of peaks (e.g., a plurality of peaks (311) of FIG. 5) and a plurality of valleys (e.g., a plurality of valleys (312) of FIG. 5) formed between adjacent peaks on a first surface (e.g., a glass layer (310) of FIG. 5) of a glass layer (e.g., a glass layer (310) of FIG. 5), and placing the first member on the plurality of peaks, and depositing a second member (e.g., a second member (340) of FIG. 5) having a second reflectance lower than the first reflectance on the first surface of the glass layer and the first member to form a second layer (e.g., a second layer (340) of FIG. 5).

[0114] According to various embodiments, the operation of laminating a third member (e.g., third member (350) of FIG. 5, third member (350-2) of FIG. 7a, third member (350-3) of FIG. 7b, third member (350-4) of FIG. 7c, or third member (350-5) of FIG. 7d) on a second surface (e.g., (310b) of FIG. 5) facing a direction opposite to the first surface of the glass layer is further included, and the third member may include a color layer (e.g., color layer (351) of FIG. 5) disposed on the second surface of the glass layer.

[0115] According to various embodiments, the glass layer and the second member may be formed of a transparent inorganic material, and the first member may be formed of a transparent or translucent organic material.

[0116] According to various embodiments, the etching of the substrate of the glass layer is performed using acid, and the operation may further include the operation of removing the masking member disposed on the first member.

[0117] Furthermore, the embodiments of the present disclosure disclosed in this specification and drawings are merely specific examples provided to facilitate the explanation of the technical content according to the embodiments of the present disclosure and to aid in understanding the embodiments of the present disclosure, and are not intended to limit the scope of the embodiments of the present disclosure. Accordingly, the scope of the various embodiments of the present disclosure should be interpreted to include all modifications or variations derived based on the technical concept of the various embodiments of the present disclosure, in addition to the embodiments disclosed herein.

Claims

1. In an electronic device (200), Display (201); and It includes a cover member (300, 300-1, 300-2, 300-3, 300-4, 300-5, 300-6) that forms at least a part of the exterior of the electronic device at a position facing the display, The above cover member is, A glass layer (310) comprising a plurality of peaks (311) formed on a first surface (310a) and a plurality of valleys (312) formed between adjacent peaks; A first member (320, 320-1, 320-2) deposited on the plurality of peaks and having a first reflectance; and An electronic device comprising a second member (340, 340-1) deposited on the first surface of the glass layer and the first member, and having a second reflectance lower than the first reflectance.

2. In Paragraph 1, The above cover member is, It includes a third member (350, 350-1, 350-2, 350-3, 350-4, 350-5) disposed on a second surface (310b) facing a direction opposite to the first surface of the glass layer, and The above third member is, An electronic device comprising a color layer (351, 351-1) disposed on the second surface of the glass layer.

3. In Paragraph 2, The third absence is, An electronic device comprising a plurality of adhesive layers (355, 356) disposed between the second surface of the glass layer and the color layer.

4. In Paragraph 3, The above third member is, An electronic device comprising a reflective layer (352) disposed between the color layer and the plurality of adhesive layers.

5. In Paragraph 2, The above third member is, A reflective layer (352) disposed on the color layer above, and An electronic device comprising a reinforcing layer (354) disposed between the second surface of the glass layer and the reflective layer, which prevents the reflective material of the reflective layer from diffusing into the glass layer.

6. In Paragraph 3, The above third member is, A reflective layer (352) disposed on the color layer above, and It includes a pattern layer (353) disposed between the plurality of adhesive layers and the reflective layer, The above pattern layer is, An electronic device that forms a three-dimensional effect, texture, and / or pattern on the above-mentioned cover member.

7. In Paragraph 6, The above pattern layer is, An electronic device formed with a prism pattern, lenticular pattern, Fresnel pattern, or holographic pattern.

8. In Paragraph 2, When light is incident from outside the above electronic device, An electronic device in which the brightness or lightness of the color layer observed in the plurality of peaks where the first member and the second member are deposited is higher than the brightness or lightness of the color layer observed in the plurality of valleys where the second member is deposited.

9. In Paragraph 2, When light is incident from outside the above electronic device, An electronic device in which the brightness of the color layer observed in the plurality of peaks where the first member and the second member are deposited is similar to the brightness of the color layer observed in the plurality of valleys where the second member is deposited.

10. A method for forming cover members (300, 300-1, 300-2, 300-3, 300-4, 300-5, 300-6), The operation of forming a first layer (320', 320-1, 320-2) by depositing a first member (320, 320-1, 320'-2) having a first reflectance on at least a portion of the first surface (310'a) of the base material (310') of the glass layer; The operation of placing a masking member (330) on at least a portion of the first layer; The operation of etching the base material of the glass layer to form a plurality of valleys (312) formed between a plurality of peaks (311) and adjacent peaks on a first surface (310a) of the glass layer (310), and placing the first member on the plurality of peaks; and A method for forming a cover member, comprising the operation of forming a second layer (340, 340-1) by depositing a second member (340, 340-1) having a second reflectance lower than the first reflectance on the first surface of the glass layer and the first member.

11. In Paragraph 10, The method further includes the operation of placing a third member (350, 350-1, 350-2, 350-3, 350-4, 350-5) on a second surface (310b) facing a direction opposite to the first surface of the glass layer, and The above third member is, A method for forming a cover member comprising a color layer (351, 351-1) disposed on the second surface of the glass layer.

12. In Paragraph 10, The glass layer, the first member, and / or the second member are, Method for forming a cover member formed from a transparent inorganic material.

13. In Paragraph 12, The operation of forming the first layer above is, The first member is formed by depositing the first member on the first surface of the base material of the glass layer, and The operation of placing the first member on the plurality of peaks is, The base material of the first layer and the glass layer is etched to form the plurality of peaks and the plurality of valleys, and the first member is placed on the plurality of peaks. The etching of the substrate of the first layer and the glass layer is performed using acid, and A method for forming a cover member, the above operation further comprising the operation of removing the masking member disposed on the first member.

14. In Paragraph 10, The glass layer and the second member are, Formed of a transparent inorganic material, The above-mentioned first member is, Method for forming a cover member formed from a transparent or translucent organic material.

15. In Paragraph 14, The etching of the substrate of the above glass layer is performed using acid, and A method for forming a cover member, the above operation further comprising the operation of removing the masking member disposed on the first member.