An anti-wrinkle finishing agent and a technology for its application are applied in the field of anti-wrinkle finishing and its preparation, which can solve the problems of high cost of the finishing agent and complicated finishing methods, and achieve the effects of improving the anti-wrinkle effect, the anti-wrinkle effect and the large recovery angle.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0017] Take the following ingredients by weight:
[0018]
[0019] The above-mentioned components were heated at a heating temperature of 60° C., stirred after heating at a stirring speed of 500 rpm, and stirred for 30 minutes, and cooled after stirring to prepare an anti-wrinkle finishing agent.
Embodiment 2
[0021] Take the following ingredients by weight:
[0022]
[0023] The above-mentioned components were heated at a heating temperature of 40° C., stirred after heating at a stirring speed of 200 rpm, and stirred for 90 minutes, and cooled after stirring to prepare an anti-wrinkle finishing agent.
Embodiment 3
[0025] Take the following ingredients by weight:
[0026]
[0027] The above-mentioned components were heated at a heating temperature of 40° C., stirred after heating at a stirring speed of 200 rpm, and stirred for 90 minutes, and cooled after stirring to prepare an anti-wrinkle finishing agent.