Preparation technology of jelly-feel three-layer mesh fabric and weaving method of grey fabric
Through the jelly-feel three-layer mesh fabric technology woven with seven combs, the problem of single pattern and lack of transparency of the three-layer structure in the existing technology has been solved, and the thickness, elasticity and visual effect have been improved, and the Physical properties and service life of fabrics.
Patent Information
- Application Number
- CN202410604320.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-05-15
- Publication Date
- 2024-10-15
- Estimated Expiration
- 2044-05-15
AI Technical Summary
The existing three-layer structure warp knitted fabric has a single pattern effect, poor visual experience, and the material lacks transparency, resulting in small differentiation.
It adopts a jelly-like three-layer mesh fabric process woven with seven combs. Through a specific weaving organization and hierarchical structure, a geometric mesh bottom layer and a transparent surface layer are formed. Combined with the support layer, a three-layer mesh fabric with thickness and elasticity is achieved. fabric.
It achieves a visually looming effect, improves the physical properties and service life of the fabric, and improves color fastness and texture.
Smart Images

Figure CN118186676B_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the field of preparation of three-layer mesh fabrics, and particularly relates to a preparation process of a three-layer mesh fabric with a jelly feel and a weaving method of the grey fabric. Background Art
[0002] The existing three-layer warp knitted fabric, including the surface layer, the support layer and the base layer, has the following disadvantages: 1. The pattern effect of the three-layer structure is relatively simple, and the visual experience is poor, resulting in little differentiation of the three-layer warp knitted mesh; 2. The surface layer and the bottom layer of the three-layer warp knitted fabric are both filament fibers, and the material has no sense of transparency; therefore, it is necessary to further improve the existing three-layer fabric structure. Summary of the invention
[0003] The purpose of the present invention is to overcome the shortcomings of the prior art and provide a preparation process of a jelly-feel three-layer mesh fabric and a weaving method of the grey fabric.
[0004] The present invention adopts the following technical solution:
[0005] A weaving method for a grey cloth with a jelly-feel three-layer mesh fabric, the grey cloth comprising a bottom layer, a support layer and a surface layer, the weaving method is woven by seven combs, the seven combs are sequentially arranged as GB1, GB2, GB3, GB4, GB5, GB6, GB7; the surface layer is woven by two combs, GB6 and GB7, the bottom layer is woven by four combs, GB1, GB2, GB3 and GB4, and the support layer is woven by one comb, GB5; wherein,
[0006] The weaving structure of the ground comb GB1 is: (1-0 / 2-3)×2 / (3-2 / 2-3)×2 / (4-5 / 3-2)×2 / (2-3 / 3-2)×2 / / , and it adopts a combination of threading and empty threading;
[0007] The weaving structure of the ground comb GB2 is: (4-5 / 3-2)×2 / (2-3 / 3-2)×2 / (1-0 / 2-3)×2 / (3-2 / 2-3)×2 / / , and it adopts a combination of threading and empty threading;
[0008] The weaving structure of the ground comb GB3 is: 1-0 / 4-5 / (1-0 / 1-2)×3 / / , and it adopts a combination of threading and empty threading;
[0009] The weaving structure of the ground comb GB4 is: 4-5 / 1-0 / (4-5 / 4-3)×3 / / , and it adopts a combination of threading and empty threading;
[0010] The weaving structure of the ground comb GB5 is: 2-3-1-2 / 1-0-2-1 / / ;
[0011] The weaving structure of the ground comb GB6 is: 1-1-1-0 / 2-2-2-3 / / ;
[0012] The weaving structure of the ground comb GB7 is: 2-2-2-3 / 1-1-1-0 / / ;
[0013] The ground combs GB1, GB2, GB3, and GB4 are matched with each other to form meshes of geometric shapes as the bottom layer.
[0014] Preferably, the bottom layer is woven from polyester FDY, the support layer is woven from polyester semi-gloss monofilament, and the surface layer is woven from transparent polyester monofilament.
[0015] Preferably, the bottom layer is woven with two materials, 100D / 48F polyester FDY filament and 75D / 36F polyester FDY filament, to form a geometric mesh, wherein the ground combs GB1 and GB2 are woven with 75D / 36F polyester FDY filament, and the ground combs GB3 and GB4 are woven with 100D / 48F polyester FDY filament.
[0016] Preferably, the polyester semi-gloss monofilament is 30D polyester semi-gloss monofilament, and the transparent polyester monofilament is 0.09mm / 1F transparent polyester monofilament.
[0017] Preferably, the layers of the grey cloth include, by weight percentage: 45% of the surface layer, 25% of the support layer and 30% of the bottom layer.
[0018] A preparation process of a jelly-feel three-layer mesh fabric, specifically comprising the following steps:
[0019] Step 1, preparing and warping the raw materials required for each layer, and then weaving the grey cloth by any of the weaving methods described above;
[0020] Step 2: Put the woven grey cloth into the warehouse, drop the cloth, and then send it into the pretreatment tank for pretreatment;
[0021] Step 3, sending the grey cloth processed in step 2 into a dyeing tank for dyeing;
[0022] Step 4, soaping, color fixing and finalizing the dyed grey cloth to obtain the jelly-feel three-layer mesh fabric;
[0023] The pretreatment includes: sending the grey cloth into a pretreatment tank, and immersing it in a pretreatment liquid at a temperature of 80-90°C for 30-40 minutes, drying it, and then immersing it again, followed by multiple washing with clean water, drying it, and sending it to a pre-setting machine for setting treatment; wherein the pretreatment liquid includes 0.5-0.7g / L of low-temperature scouring agent TF-189, 4-5g / L of sodium hydroxide, 1-2g / L of penetrant, and 1-2g / L of neutralizing acid.
[0024] Preferably, the dyeing comprises: placing the grey cloth in water at a bath ratio of 1:12, adding a neutralizing acid, a disperse dye, a penetrant, a dye accelerator and a leveling agent in sequence, stirring evenly, and heat-treating at 60-70°C for 20-30 minutes; wherein the amount of the neutralizing acid added is 2% of the weight of the grey cloth, the amount of the disperse dye added is 5% of the weight of the grey cloth, the amount of the penetrant added is 0.7% of the weight of the grey cloth, the amount of the dye accelerator added is 0.8% of the weight of the grey cloth, and the amount of the leveling agent added is 1.5% of the weight of the grey cloth.
[0025] Preferably, the soap washing comprises: placing the dyed blank in a treatment solution containing 2 g / L soaping agent and 0.5 g / L acetic acid, and treating at a temperature of 90-100° C. for 15-25 min.
[0026] Preferably, the color fixing comprises: steaming the soap-washed grey cloth with a color fixing solution for 1-2 hours, and then cooling to room temperature; wherein the color fixing solution comprises 1.5-2.5 g / L of soda ash and 3-5 g / L of color fixing base XH-01.
[0027] Preferably, the finished product shaping includes: placing the color-fixed blank in a treatment liquid containing 2g / L softener for shaping treatment, with a shaping temperature of 120-140°C and a vehicle speed of 14-16m / min.
[0028] It can be seen from the above description of the present invention that, compared with the prior art, the present invention has the following beneficial effects:
[0029] First, the weaving method of the grey cloth of the present application is to weave it by seven combs according to the set weaving organization, so that the bottom layer obtained is used as a jacquard layer, which is composed of geometric meshes of equal spacing, shape and size; the surface layer is a plane with a semi-transparent texture of jelly, through which the geometric meshes on the bottom layer can be seen, giving a visually looming effect, and a support layer is set between the surface layer and the bottom layer, so that the obtained three-layer mesh fabric has thickness and elasticity, ensuring that the fabric has good physical properties, which can bring consumers a different visual experience;
[0030] Second, the preparation process of the three-layer mesh fabric of the present invention is to clean the grey cloth by setting a pretreatment step to ensure the cleanliness of the grey cloth and the colorability of the subsequent dyeing, and then perform a shaping treatment on the grey cloth after cleaning and drying to ensure the stability of the shape and structure of the grey cloth, thereby improving the service life of the prepared three-layer mesh fabric;
[0031] Third, the present invention limits the specific operations of the dyeing and fixing steps, and adds a specific amount of leveling agent, dyeing accelerator and penetrant during the dyeing process to increase the dispersibility and colorability of the disperse dye in the fabric, ensure dyeing uniformity, and improve color fastness and dyeing efficiency; hot steaming and fixing after dyeing can further improve the color fastness of the fabric and enhance the texture of the prepared three-layer mesh fabric. BRIEF DESCRIPTION OF THE DRAWINGS
[0032] Figure 1 It is a schematic diagram of the structure of the surface layer;
[0033] Figure 2 It is a schematic diagram of the underlying structure;
[0034] Figure 3 is a schematic diagram of the structure of the support layer;
[0035] Figure 4 It is a schematic diagram of the structure after the surface layer is combined with the bottom layer and part of the surface layer is cut away;
[0036] Figure 5 This is a schematic diagram of the structure after the bottom layer is combined with the surface layer and part of the bottom layer is cut away. DETAILED DESCRIPTION
[0037] The present invention is further described below through specific implementation modes.
[0038] A preparation process of a jelly-feel three-layer mesh fabric, specifically comprising the following steps:
[0039] Step 1: preparing and warping the raw materials required for each layer, and then weaving to obtain the grey cloth, wherein the grey cloth includes a bottom layer, a support layer and a surface layer, and each layer includes, by weight percentage, 45% of the surface layer, 25% of the support layer and 30% of the bottom layer;
[0040] Step 2: Put the woven grey cloth into the warehouse, drop the cloth, and then send it into the pretreatment tank. After being immersed in the pretreatment liquid at a temperature of 80-90°C for 30-40 minutes, it is dried and immersed again. Then, it is washed with clean water for many times, dried and sent to the pre-setting machine for setting treatment; wherein the pretreatment liquid includes 0.5-0.7g / L low-temperature scouring agent TF-189, 4-5g / L sodium hydroxide, 1-2g / L penetrant JFC, and 1-2g / L neutralizing acid NA;
[0041] Step 3, sending the grey cloth treated in step 2 into a dyeing tank, putting the grey cloth into water according to a bath ratio of 1:12, adding neutralizing acid NA, disperse dye, penetrant JFC, accelerator B-604 and leveling agent AT-2110 in sequence, stirring evenly, and heat-treating at 60-70°C for 20-30 minutes; wherein, the amount of neutralizing acid NA added is 2% of the weight of the grey cloth, the amount of disperse dye added is 5% of the weight of the grey cloth, the amount of penetrant JFC added is 0.7% of the weight of the grey cloth, the amount of accelerator B-604 added is 0.8% of the weight of the grey cloth, and the amount of leveling agent AT-2110 added is 1.5% of the weight of the grey cloth;
[0042] Step 4: Place the dyed blank in a treatment solution containing 2 g / L soaping agent AT-1508 and 0.5 g / L acetic acid, and treat at a temperature of 90-100° C. for 15-25 min;
[0043] Step 5, steaming the soap-washed grey cloth with a color fixing solution for 1-2 hours, and then cooling it to room temperature; wherein the color fixing solution includes 1.5-2.5 g / L of soda ash and 3-5 g / L of color fixing base XH-01;
[0044] Step six, placing the fixed color blank in a treatment solution containing 2g / L softener for setting treatment to obtain the jelly-feel three-layer mesh fabric, wherein the setting temperature is 120-140°C, the vehicle speed is 14-16m / min, and the softener is hydrophilic silicone oil T718.
[0045] Specifically, the grey cloth is woven with seven combs, which are arranged in sequence as GB1, GB2, GB3, GB4, GB5, GB6, and GB7; the surface layer is woven with two combs, GB6 and GB7, the bottom layer is woven with four combs, GB1, GB2, GB3, and GB4, and the supporting layer is woven with one comb, GB5; wherein,
[0046] The weaving structure of the ground comb GB1 is: (1-0 / 2-3)×2 / (3-2 / 2-3)×2 / (4-5 / 3-2)×2 / (2-3 / 3-2)×2 / / , and it adopts a combination of threading and empty threading;
[0047] The weaving structure of the ground comb GB2 is: (4-5 / 3-2)×2 / (2-3 / 3-2)×2 / (1-0 / 2-3)×2 / (3-2 / 2-3)×2 / / , and it adopts a combination of threading and empty threading;
[0048] The weaving structure of the ground comb GB3 is: 1-0 / 4-5 / (1-0 / 1-2)×3 / / , and it adopts a combination of threading and empty threading;
[0049] The weaving structure of the ground comb GB4 is: 4-5 / 1-0 / (4-5 / 4-3)×3 / / , and it adopts a combination of threading and empty threading;
[0050] The weaving structure of the ground comb GB5 is: 2-3-1-2 / 1-0-2-1 / / ;
[0051] The weaving structure of the ground comb GB6 is: 1-1-1-0 / 2-2-2-3 / / ;
[0052] The weaving structure of the ground comb GB7 is: 2-2-2-3 / 1-1-1-0 / / ;
[0053] The bottom layer is made of 100D / 48F polyester FDY filament and 75D / 36F polyester FDY filament to weave geometric meshes, among which, the ground combs GB1 and GB2 are woven with 75D / 36F polyester FDY filaments, and the ground combs GB3 and GB4 are woven with 100D / 48F polyester FDY filaments; the ground combs GB1, GB2, GB3, and GB4 are matched with each other to form geometric meshes as the bottom layer; the supporting layer is woven with 30D polyester semi-gloss monofilament; the surface layer is woven with 0.09mm / 1F transparent polyester monofilament.
[0054] The present application specifically defines a weaving method for the grey cloth, which is woven by seven combs according to a set weaving structure, so that the obtained bottom layer is used as a jacquard layer, and is composed of geometric meshes of equal spacing, shape, and size; the surface layer is a plane with a semi-transparent jelly texture, through which the geometric meshes on the bottom layer can be seen, giving a visually looming effect, and a supporting layer is arranged between the surface layer and the bottom layer, so that the obtained three-layer mesh fabric has thickness and elasticity, ensuring that the fabric has good physical properties, can bring consumers a different visual experience, and is loved by consumers.
[0055] Example 1
[0056] A preparation process of a jelly-feel three-layer mesh fabric, specifically comprising the following steps:
[0057] Step 1: preparing and warping the raw materials required for each layer, and then weaving to obtain the grey cloth, wherein the grey cloth includes a bottom layer, a support layer and a surface layer, and each layer includes, by weight percentage, 45% of the surface layer, 25% of the support layer and 30% of the bottom layer;
[0058] Step 2: Put the woven grey cloth into the warehouse, drop the cloth, feed the cloth, and then send it into the pretreatment tank. After being immersed in the pretreatment liquid at a temperature of 80°C for 40 minutes, it is dried and immersed again. Then, it is washed with clean water for many times, dried and sent to the pre-setting machine for setting treatment; wherein the pretreatment liquid includes 0.5g / L low-temperature scouring agent TF-189, 5g / L sodium hydroxide, 1g / L penetrant JFC, and 2g / L neutralizing acid NA;
[0059] Step 3, sending the grey cloth treated in step 2 into the dyeing tank, putting the grey cloth into water according to the bath ratio of 1:12, adding neutralizing acid NA, disperse dye, penetrant JFC, accelerator and B-604 leveling agent AT-2110 in sequence, stirring evenly, and heat-treating at 60°C for 30 minutes; wherein, the addition amount of neutralizing acid NA is 2% of the weight of the grey cloth, the addition amount of disperse dye is 5% of the weight of the grey cloth, the addition amount of penetrant JFC is 0.7% of the weight of the grey cloth, the addition amount of accelerator B-604 is 0.8% of the weight of the grey cloth, and the addition amount of leveling agent AT-2110 is 1.5% of the weight of the grey cloth;
[0060] Step 4: Place the dyed blank in a treatment solution containing 2 g / L soaping agent AT-1508 and 0.5 g / L acetic acid, and treat at 90° C. for 25 min;
[0061] Step 5, steaming the soap-washed grey cloth with a color fixing solution for 1 hour, and then cooling it to room temperature; wherein the color fixing solution includes 1.5 g / L of soda ash and 5 g / L of color fixing base XH-01;
[0062] Step six, placing the fixed color blank in a treatment liquid containing 2g / L softener for setting treatment to obtain the jelly-feel three-layer mesh fabric, wherein the setting temperature is 120°C, the vehicle speed is 14m / min, and the softener is hydrophilic silicone oil T718.
[0063] Example 2
[0064] A preparation process of a jelly-feel three-layer mesh fabric, specifically comprising the following steps:
[0065] Step 1: preparing and warping the raw materials required for each layer, and then weaving to obtain the grey cloth, wherein the grey cloth includes a bottom layer, a support layer and a surface layer, and each layer includes, by weight percentage, 45% of the surface layer, 25% of the support layer and 30% of the bottom layer;
[0066] Step 2: Put the woven grey cloth into the warehouse, drop the cloth, feed the cloth, and then send it into the pretreatment tank. After being immersed in the pretreatment liquid at a temperature of 90°C for 30 minutes, it is dried and immersed again. Then, it is washed with clean water for many times, dried and sent to the pre-setting machine for setting treatment; wherein the pretreatment liquid includes 0.7g / L low-temperature scouring agent TF-189, 4g / L sodium hydroxide, 2g / L penetrant JFC, and 1g / L neutralizing acid NA;
[0067] Step 3, sending the grey cloth treated in step 2 into the dyeing tank, putting the grey cloth into water according to the bath ratio of 1:12, adding neutralizing acid NA, disperse dye, penetrant JFC, accelerator B-604 and leveling agent AT-2110 in sequence, stirring evenly, and heat-treating at 70°C for 20 minutes; wherein, the addition amount of neutralizing acid NA is 2% of the weight of the grey cloth, the addition amount of disperse dye is 5% of the weight of the grey cloth, the addition amount of penetrant JFC is 0.7% of the weight of the grey cloth, the addition amount of accelerator B-604 is 0.8% of the weight of the grey cloth, and the addition amount of leveling agent AT-2110 is 1.5% of the weight of the grey cloth;
[0068] Step 4: Place the dyed blank in a treatment solution containing 2 g / L soaping agent AT-1508 and 0.5 g / L acetic acid, and treat at a temperature of 100° C. for 15 minutes;
[0069] Step 5, steaming the soap-washed grey cloth with a color fixing solution for 2 hours, and then cooling it to room temperature; wherein the color fixing solution includes 2.5 g / L of soda ash and 3 g / L of color fixing base XH-01;
[0070] Step six, placing the fixed color blank in a treatment solution containing 2g / L softener for setting treatment to obtain the jelly-feel three-layer mesh fabric, wherein the setting temperature is 140°C, the vehicle speed is 16m / min, and the softener is hydrophilic silicone oil T718.
[0071] Example 3
[0072] A preparation process of a jelly-feel three-layer mesh fabric, specifically comprising the following steps:
[0073] Step 1: preparing and warping the raw materials required for each layer, and then weaving to obtain the grey cloth, wherein the grey cloth includes a bottom layer, a support layer and a surface layer, and each layer includes, by weight percentage, 45% of the surface layer, 25% of the support layer and 30% of the bottom layer;
[0074] Step 2: Put the woven grey cloth into the warehouse, drop the cloth, feed the cloth, and then send it into the pretreatment tank. After being immersed in the pretreatment liquid at a temperature of 85°C for 35 minutes, it is dried and immersed again. Then, it is washed with clean water for many times, dried and sent to the pre-setting machine for setting treatment; wherein the pretreatment liquid includes 0.6g / L low-temperature scouring agent TF-189, 4.5g / L sodium hydroxide, 1.5g / L penetrant JFC, and 1.5g / L neutralizing acid NA;
[0075] Step 3, sending the grey cloth treated in step 2 into the dyeing tank, putting the grey cloth into water according to the bath ratio of 1:12, adding neutralizing acid NA, disperse dye, penetrant JFC, accelerator B-604 and leveling agent AT-2110 in sequence, stirring evenly, and heat-treating at 65°C for 25 minutes; wherein, the addition amount of neutralizing acid NA is 2% of the weight of the grey cloth, the addition amount of disperse dye is 5% of the weight of the grey cloth, the addition amount of penetrant JFC is 0.7% of the weight of the grey cloth, the addition amount of accelerator B-604 is 0.8% of the weight of the grey cloth, and the addition amount of leveling agent AT-2110 is 1.5% of the weight of the grey cloth;
[0076] Step 4: Place the dyed blank in a treatment solution containing 2 g / L soaping agent AT-1508 and 0.5 g / L acetic acid, and treat at a temperature of 95° C. for 20 min;
[0077] Step 5, steaming the soap-washed grey cloth with a color fixing solution for 1.5 hours, and then cooling it to room temperature; wherein the color fixing solution includes 2g / L soda ash and 4g / L color fixing base XH-01;
[0078] Step six, placing the fixed color blank in a treatment liquid containing 2g / L softener for setting treatment to obtain the jelly-feel three-layer mesh fabric, wherein the setting temperature is 130°C, the vehicle speed is 15m / min, and the softener is hydrophilic silicone oil T718.
[0079] The present application specifically defines the preparation process of the three-layer mesh fabric, and by setting a pretreatment step, the grey cloth is cleaned to ensure the cleanliness of the grey cloth and the colorability of the subsequent dyeing, and then the grey cloth after cleaning and drying is subjected to a shaping treatment to ensure the stability of the shape and structure of the grey cloth, thereby improving the service life and use value of the prepared three-layer mesh fabric; at the same time, the specific operations of the dyeing and fixing processes are defined, and a specific amount of leveling agent, dyeing accelerator and penetrant are added during the dyeing process to increase the dispersibility and colorability of the disperse dye in the fabric, ensure dyeing uniformity, and improve color fastness and dyeing efficiency; hot steaming and fixing after dyeing can further improve the color fastness of the fabric and enhance the texture of the prepared three-layer mesh fabric.
[0080] The above description is only a preferred embodiment of the present invention, and therefore cannot be used to limit the scope of implementation of the present invention. That is, equivalent changes and modifications made according to the scope of the patent application of the present invention and the contents of the specification should still fall within the scope covered by the patent of the present invention.
Claims
1. A method for weaving a grey cloth for a three-layer mesh fabric with a jelly feel, wherein the grey cloth comprises a bottom layer, a support layer and a surface layer, characterized in that: It is woven by seven combs, which are arranged in sequence as GB1, GB2, GB3, GB4, GB5, GB6, and GB7; the surface layer is woven by two combs, GB6 and GB7, the bottom layer is woven by four combs, GB1, GB2, GB3, and GB4, and the supporting layer is woven by one comb, GB5; wherein, The weaving structure of the ground comb GB1 is: (1-0 / 2-3)×2 / (3-2 / 2-3)×2 / (4-5 / 3-2)×2 / (2-3 / 3-2)×2 / / , and it adopts a combination of threading and empty threading; The weaving structure of the ground comb GB2 is: (4-5 / 3-2)×2 / (2-3 / 3-2)×2 / (1-0 / 2-3)×2 / (3-2 / 2-3)×2 / / , and it adopts a combination of threading and empty threading; The weaving structure of the ground comb GB3 is: 1-0 / 4-5 / (1-0 / 1-2)×3 / / , and it adopts a combination of threading and empty threading; The weaving structure of the ground comb GB4 is: 4-5 / 1-0 / (4-5 / 4-3)×3 / / , and it adopts a combination of threading and empty threading; The weaving structure of the ground comb GB5 is: 2-3-1-2 / 1-0-2-1 / / ; The weaving structure of the ground comb GB6 is: 1-1-1-0 / 2-2-2-3 / / ; The weaving structure of the ground comb GB7 is: 2-2-2-3 / 1-1-1-0 / / ; The ground comb GB1, GB2, GB3, GB4 match each other to form a geometric mesh, as the bottom layer; The bottom layer is woven from polyester FDY, the supporting layer is woven from polyester semi-bright monofilament, and the surface layer is woven from transparent polyester monofilament.
2. A method for weaving grey cloth for three-layer mesh fabric with jelly feel according to claim 1, characterized in that: The bottom layer is woven with 100D / 48F polyester FDY filament and 75D / 36F polyester FDY filament to form geometric meshes, wherein the ground combs GB1 and GB2 are woven with 75D / 36F polyester FDY filament, and the ground combs GB3 and GB4 are woven with 100D / 48F polyester FDY filament.
3. The weaving method of a grey cloth for a jelly-feel three-layer mesh fabric according to claim 1, characterized in that: The polyester semi-gloss monofilament is 30D polyester semi-gloss monofilament, and the transparent polyester monofilament is 0.09mm / 1F transparent polyester monofilament.
4. The weaving method of a grey cloth for a jelly-feel three-layer mesh fabric according to claim 1, characterized in that: The layers of the grey cloth include, by weight percentage, 45% of a surface layer, 25% of a support layer and 30% of a bottom layer.
5. A preparation process of a jelly-feel three-layer mesh fabric, characterized in that: The specific steps include: Step 1, preparing and warping the raw materials required for each layer, and then weaving the grey cloth according to the weaving method according to any one of claims 1 to 4; Step 2: Put the woven grey cloth into the warehouse, drop the cloth, and then send it into the pretreatment tank for pretreatment; Step 3, sending the grey cloth processed in step 2 into a dyeing tank for dyeing; Step 4, soaping, color fixing and finalizing the dyed grey cloth to obtain the jelly-feel three-layer mesh fabric; The pretreatment includes: sending the grey cloth into a pretreatment tank, and immersing it in a pretreatment liquid at a temperature of 80-90°C for 30-40 minutes, drying it, and then immersing it again, followed by multiple washing with clean water, drying it, and sending it to a pre-setting machine for setting treatment; wherein the pretreatment liquid includes 0.5-0.7g / L of low-temperature scouring agent TF-189, 4-5g / L of sodium hydroxide, 1-2g / L of penetrant, and 1-2g / L of neutralizing acid.
6. The preparation process of the three-layer mesh fabric with jelly feeling according to claim 5, characterized in that: The dyeing process comprises: placing the grey cloth in water at a bath ratio of 1:12, sequentially adding a neutralizing acid, a disperse dye, a penetrant, a dye accelerator and a leveling agent, stirring evenly, and heat-treating at 60-70°C for 20-30 minutes; wherein the amount of the neutralizing acid added is 2% of the weight of the grey cloth, the amount of the disperse dye added is 5% of the weight of the grey cloth, the amount of the penetrant added is 0.7% of the weight of the grey cloth, the amount of the dye accelerator added is 0.8% of the weight of the grey cloth, and the amount of the leveling agent added is 1.5% of the weight of the grey cloth.
7. The preparation process of the three-layer mesh fabric with jelly feeling according to claim 5, characterized in that: The soap washing comprises: placing the dyed blank in a treatment solution containing 2g / L soaping agent and 0.5g / L acetic acid, and treating at a temperature of 90-100°C for 15-25min.
8. The preparation process of the three-layer mesh fabric with jelly feeling according to claim 5, characterized in that: The color fixing method comprises: steaming the soap-washed grey cloth with a color fixing solution for 1-2 hours, and then cooling it to room temperature; wherein the color fixing solution comprises 1.5-2.5 g / L of soda ash and 3-5 g / L of color fixing base XH-01.
9. The preparation process of the three-layer mesh fabric with jelly feeling according to claim 5, characterized in that: The finished product shaping comprises: placing the color-fixed blank in a treatment liquid containing 2g / L softener for shaping treatment, with a shaping temperature of 120-140°C and a vehicle speed of 14-16m / min.
Citation Information
Patent Citations
Method for dyeing multicomponent intrinsic flame-retardant fiber textile
CN104278547A
Water drop-shaped mesh cloth and manufacturing method thereof
CN108790332A
Method for manufacturing stereoscopic suspension mesh cloth
CN108998883A
Polyester sunshade fabric dyeing and finishing process
CN109440502A
In-hole velvet lifting process screen cloth as well as manufacturing method and application thereof
CN112030344A
Cited By
Screen cloth fabric with suspension-sense polygonal meshes and preparation process of screen cloth fabric
CN119020912A
Mesh fabric with suspended polygonal mesh and preparation process thereof
CN119020912B