Prediction method of creep fatigue life of SOFC bipolar plates during thermal cycling
Through numerical simulation and multi-software joint simulation, the creep fatigue life of SOFC bipolar plates under hot and cold cycles is accurately predicted, which solves the problem of inaccurate simulation in the existing technology and improves the accuracy of prediction and calculation efficiency.
Patent Information
- Application Number
- CN202411126090.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-16
- Publication Date
- 2024-10-29
- Estimated Expiration
- 2044-08-16
AI Technical Summary
It is difficult to accurately simulate and predict the creep fatigue life of SOFC bipolar plates during hot and cold cycles with existing technology, making it difficult to solve the problem of structural failure.
A numerical simulation method was used to establish a three-dimensional geometric model of a single cell. Finite element simulation was performed using Fluent and ANSYS Workbench software to obtain the temperature and stress field distribution. The creep fatigue parameters were fitted through the Larson-Miller equation and CAE technology was used to predict the bipolar plate. creep fatigue life.
It achieves accurate life prediction of SOFC bipolar plates under hot and cold cycle conditions, reduces simulation complexity and calculation efficiency, and improves the accuracy of prediction.
Smart Images

Figure CN118655011B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of creep fatigue life numerical simulation, and in particular to a method for predicting the creep fatigue life of a SOFC bipolar plate during a hot-cold cycle. Background Art
[0002] Fuel cells, as an efficient and clean energy conversion device, have received widespread attention. Solid oxide fuel cells (SOFCs) are power generation devices that directly convert the chemical energy of fuel and oxidant into electrical energy at medium and high temperatures. They have the advantages of high efficiency, cleanliness, high power generation efficiency, and good fuel flexibility, and are considered to be an important development direction in the future energy field. However, there are still many problems in the actual application of solid oxide fuel cells. One of the key problems is that the metal bipolar plates in SOFCs are affected by cyclic thermal stress during the periodic startup, stable operation, and shutdown stages. In addition, the number of startup cycles of some SOFC systems in actual applications is far higher than 100 times. The impact of this cyclic thermal stress on the metal bipolar plates may cause the overall structure to fail.
[0003] During the hot and cold cycle stage of solid oxide fuel cells, the temperature of the bipolar plate is expected to rise from room temperature to 800°C. Under the cyclic mechanical and thermal loads, the bipolar plate structure is susceptible to thermomechanical fatigue damage. It is necessary to study the creep fatigue life of SOFC bipolar plates to understand the structural failure state of SOFC. At present, most researchers use creep fatigue test methods to obtain the creep fatigue life of bipolar plates, but this test method is difficult to simulate the actual working conditions of SOFC, and the creep fatigue life obtained is inaccurate. Therefore, in order to accurately predict the creep fatigue life of SOFC bipolar plates, a method for predicting the creep fatigue life of SOFC bipolar plates during hot and cold cycles is proposed. Summary of the invention
[0004] In order to solve the above technical problems, the present invention provides a method for predicting the creep fatigue life of SOFC bipolar plates during hot and cold cycles, and uses a numerical simulation method to accurately predict the creep fatigue life of SOFC bipolar plates during hot and cold cycles.
[0005] The technical solution adopted by the present invention is:
[0006] The present invention provides a method for predicting creep fatigue life of a SOFC bipolar plate during a hot and cold cycle, comprising the steps of:
[0007] (1) Based on the structure of a single cell of a solid oxide fuel cell, a three-dimensional geometric model of the single cell is established;
[0008] (2) Importing the single-cell three-dimensional model established in step (1) into the Fluent finite element analysis software, setting the physical parameters, boundary conditions, and assumptions required for the finite element simulation according to the actual working conditions, setting the control equations for gas flow and heat transfer according to the assumptions, establishing a single-cell multi-physics field coupling model based on the coupling of flow and heat transfer, performing finite element simulation calculations in the Fluent software, and obtaining the temperature field distribution of the single-cell under the cold and hot cycles;
[0009] (3) Based on the temperature field distribution obtained in step (2), a solid mechanics analysis is performed on the single cell to obtain the stress field distribution of the single cell under the thermal cycle;
[0010] (4) Using the same material as the bipolar plate of the single cell, several creep fatigue specimens were prepared and subjected to high temperature creep fatigue tests to obtain the parameters related to the Larson-Miller creep model and obtain the Larson-Miller equation for the bipolar plate material;
[0011] (5) Based on the Larson-Miller equation of the bipolar plate material obtained in step (4), a creep fatigue simulation is performed using fatigue analysis software to predict the creep fatigue life of the solid oxide fuel cell bipolar plate during the hot and cold cycle process.
[0012] Furthermore, in step (1), the single cell structure comprises a bipolar plate consisting of an anode plate and a cathode plate, a PEN unit consisting of an anode electrode layer, an electrolyte layer, and a cathode electrode layer is arranged between the anode plate and the cathode plate, and an anode flow channel is arranged on the side of the anode plate close to the anode electrode layer, and a cathode flow channel is arranged on the side of the cathode plate close to the cathode electrode layer.
[0013] Furthermore, the physical parameters in step (2) include:
[0014] Density, thermal conductivity, thermal expansion coefficient, Poisson’s ratio and elastic modulus of each structural material of a single cell;
[0015] Reverse absolute permeability and porosity of anode electrode layer and cathode electrode layer of porous materials;
[0016] Gas materials Dynamic viscosity, molar mass, specific heat capacity and thermal conductivity of anode gas and cathode gas.
[0017] Furthermore, the boundary conditions in step (2) include: gas inlet temperature, gas inlet flow rate, gas outlet pressure, solid thermal boundary conditions and solid mechanical boundary conditions.
[0018] Furthermore, the assumptions of the single-cell multi-physics field model in step (2) include:
[0019] The gas is an ideal gas and the flow state of the gas is laminar flow;
[0020] The influence of thermal radiation during the hot and cold cycle is negligible;
[0021] The properties of each structural material of a single cell are isotropic;
[0022] The contact thermal resistance between the cathode, anode electrodes and the bipolar plate is negligible;
[0023] Electrochemical reactions are not considered during the hot and cold cycle, and no mass transfer process is involved.
[0024] Furthermore, the step (3) is specifically as follows:
[0025] (31) Importing the temperature field of the flow channel surface in the temperature field result obtained in step (2) into the transient temperature module in the ANSYS Workbench simulation software, applying solid thermal boundary conditions in the transient temperature module, and recalculating the body temperature field of the single battery during the hot and cold cycle;
[0026] (32) The body temperature field result recalculated in step (31) is imported into the transient dynamics module in the ANSYS Workbench simulation software, and solid mechanics boundary conditions are applied to calculate the stress field of the single battery during the hot and cold cycle.
[0027] Furthermore, the step (4) is specifically as follows:
[0028] (41) Prepare several creep fatigue specimens using the same material as the bipolar plate of the single cell, conduct high temperature creep fatigue tests, and obtain several sets of stress, temperature and cracking time data;
[0029] (42) Based on the Larson-Miller equation, the stress, temperature, and cracking time data obtained from the high-temperature creep test were fitted using MATLAB software to obtain the parameters of the Larson-Miller equation and the Larson-Miller equation for the bipolar plate material.
[0030] Furthermore, the step (5) is specifically as follows:
[0031] The stress field of the single cell under the hot and cold cycle obtained in step (3), the body temperature field recalculated in step (3), and the Larson-Miller equation of the bipolar plate material obtained in step (4) are imported into the fatigue analysis software, and the CAE technology is used to perform creep fatigue simulation to predict the creep life of the solid oxide fuel cell bipolar plate during the hot and cold cycle.
[0032] The beneficial effects of the present invention are:
[0033] (1) The present invention proposes a method for predicting the creep fatigue life of a SOFC bipolar plate during a hot and cold cycle, and uses a numerical simulation method to predict the creep fatigue life of a SOFC bipolar plate during a hot and cold cycle. Compared with conventional test methods, the present invention can accurately simulate the hot and cold cycle service conditions of SOFC, and combine the stress field and temperature field of the hot and cold cycle service conditions with the creep fatigue characteristics of the bipolar plate material itself, so as to accurately calculate the creep fatigue life of the bipolar plate under the hot and cold cycle service conditions of SOFC;
[0034] (2) The present invention uses a method of joint simulation of multiple software to simulate the temperature distribution, stress distribution and creep fatigue life of the solid oxide fuel cell bipolar plate during the hot and cold cycle in steps, thereby reducing the complexity of multi-physics field simulation and improving the computational efficiency of the simulation. BRIEF DESCRIPTION OF THE DRAWINGS
[0035] In order to clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0036] Figure 1 is a flow chart of the present invention;
[0037] Figure 2 It is a schematic diagram of the structure of a single SOFC cell;
[0038] Figure 3 This is a graph showing the change in inlet gas temperature in step (2) of an embodiment of the present invention;
[0039] Figure 4 The temperature distribution of the single battery at a certain moment in the heating process obtained by recalculating in step (3) of the embodiment of the present invention;
[0040] Figure 5 The stress distribution of the single cell at a certain moment during the heat preservation process calculated in step (3) of the embodiment of the present invention;
[0041] Figure 6 The Larson-Miller equation curve diagram of the bipolar plate material obtained in step (4) of the embodiment of the present invention;
[0042] Figure 7 This is a creep fatigue life distribution diagram of the cathode plate of a single SOFC cell obtained in step (5) of the embodiment of the present invention during the hot and cold cycle process.
[0043] Labels in the figure: 1. anode plate; 2. cathode plate; 3. anode electrode layer; 4. electrolyte layer; 5. cathode electrode layer; 6. anode flow channel; 7. cathode flow channel. DETAILED DESCRIPTION
[0044] The present invention provides a method for predicting creep fatigue life of SOFC bipolar plates during hot and cold cycles. To make the purpose, technical solution and effect of the present invention clearer and more specific, the present invention is further described in detail below. It should be understood that the specific embodiments described herein are only used to explain the present invention and are not intended to limit the present invention.
[0045] The present invention is described in detail below with reference to the accompanying drawings.
[0046] Reference Figure 1 This embodiment provides a method for predicting creep fatigue life of a SOFC bipolar plate during a hot-cold cycle, comprising the steps of:
[0047] (1) Based on the single cell structure of solid oxide fuel cell, a three-dimensional geometric model of the single cell is established.
[0048] like Figure 2 As shown, the three-dimensional models of the single battery established in this step include a bipolar plate composed of an anode plate and a cathode plate, and a PEN unit composed of an anode electrode layer, an electrolyte layer, and a cathode electrode layer is arranged between the anode plate and the cathode plate, and an anode flow channel is arranged on the side of the anode plate close to the anode electrode layer, and a cathode flow channel is arranged on the side of the cathode plate close to the cathode electrode layer. In this embodiment, in order to improve the calculation efficiency, only one anode flow channel and one cathode flow channel are arranged. Among them, the overall length of the single battery is 100mm, the width of the anode flow channel and the cathode flow channel is 2mm and the height is 1mm, the width of the anode electrode layer is 3mm and the height is 0.5mm, the width of the electrolyte layer and the cathode electrode layer is 3mm and the height is 0.1mm, and the width of the anode plate and the cathode plate is 3mm and the height is 3mm.
[0049] (2) Import the single-cell three-dimensional model established in step (1) into the Fluent finite element analysis software, set the physical parameters, boundary conditions, and assumptions required for the finite element simulation according to the actual working conditions, set the control equations for gas flow and heat transfer according to the assumptions, establish a single-cell multi-physics field coupling model based on the coupling of flow and heat transfer, perform finite element simulation calculations in the Fluent software, and obtain the temperature field distribution of the single cell under the hot and cold cycles.
[0050] Specifically, in this step, the required physical parameters include:
[0051] Density, thermal conductivity, thermal expansion coefficient, Poisson's ratio and elastic modulus of each structural material of a single cell (anode electrode layer, cathode electrode layer, electrolyte layer, bipolar plate);
[0052] Reverse absolute permeability and porosity of anode electrode layer and cathode electrode layer of porous materials;
[0053] Gas materials Dynamic viscosity, molar mass, specific heat capacity and thermal conductivity of anode gas and cathode gas.
[0054] In this step, the boundary conditions include: gas inlet temperature, gas inlet velocity, gas outlet pressure, solid thermal boundary conditions and solid mechanical boundary conditions. Figure 3 As shown in the figure, the temperature is raised from 298.15K to 1098.15K, then kept warm for a period of time and cooled down. The heating-keeping-cooling period is 48000s each, i.e., one hot and cold cycle. The inlet flow rate of the anode gas and the cathode gas is 0.45m / s. The outlet pressure of the anode gas and the cathode gas is 1.013×10 5 Pa; the solid thermal boundary condition is assumed to be an adiabatic boundary; the solid mechanical boundary condition is that the geometric lower surface, front surface and left side roller support of the single cell are supported, and a uniform pressure of 0.2 MPa is applied to other surfaces.
[0055] In this step, the assumptions of the single-cell multiphysics model include:
[0056] The gas is an ideal gas and the flow state of the gas is laminar flow;
[0057] The influence of thermal radiation during the hot and cold cycle is negligible;
[0058] The properties of each structural material of a single cell are isotropic;
[0059] The contact thermal resistance between the cathode and anode electrode layers and the bipolar plates is negligible;
[0060] Electrochemical reactions are not considered during the hot and cold cycle, and no mass transfer process is involved.
[0061] Since it is assumed that no chemical reaction occurs in the hot and cold cycle, the electrochemical reaction rate is 0, and there is no current transmission and component transmission in the battery, the SOFC heating and cooling process only involves gas flow and heat transfer.
[0062] The control equations for gas flow include mass conservation model and momentum conservation model, where the mass conservation model includes mass conservation control equation, and the momentum conservation model includes Reynolds number equation, Navier-Stokes equation, and Brinkman equation, as follows:
[0063] Solid oxide fuel cells obey the law of conservation of mass, and their governing equation is:
[0064] (1)
[0065] in, is the velocity vector; is the density of the gas; For the quality source; For porous media porosity.
[0066] The flow of gas inside a solid oxide fuel cell follows the law of conservation of momentum. By calculating the Reynolds number, the Reynolds number of gas inside a SOFC is less than 2300, which is laminar flow. Its governing equation is:
[0067] (2)
[0068] in, is the density of the gas; is the flow rate; is the characteristic length; is the dynamic viscosity of the fluid; is the Reynolds number.
[0069] The Navier-Stokes equation is used as the control equation during the flow of gas in the cathode and anode channels:
[0070] (3)
[0071] in, is the pressure of the gas; is the velocity vector; is the unit tensor; is the viscous stress tensor; is the volume force tensor of the gas.
[0072] When the gas enters the porous PEN unit, the Brinkman equation is selected as the control equation considering the loss of mechanical energy due to viscous shear:
[0073] (4)
[0074] in, is the density of the gas; For porous media Porosity; For porous media The penetration rate; is the pressure of the gas; is the velocity vector; For the quality source; is the dynamic viscosity of the fluid; is the unit tensor; is the volume force tensor of the gas.
[0075] The governing equation for heat transfer is the heat transfer equation. The SOFC heat transfer model includes heat conduction and heat convection, and the energy equation is:
[0076] (5)
[0077] (6)
[0078] in, is the density of the gas; is the velocity vector; is the heat capacity at constant pressure; is the conductive heat flux, is the effective thermal conductivity; is temperature; As heat source.
[0079] (3) Based on the temperature field distribution obtained in step (2), a solid mechanics analysis is performed on the single cell to obtain the stress field distribution of the single cell under the thermal cycle.
[0080] The steps are as follows:
[0081] (31) The temperature field of the flow channel surface in the temperature field result obtained in step (2) is imported into the Transient Temperature module (i.e., transient thermal module) in the ANSYS Workbench simulation software, and solid thermal boundary conditions are applied in the Transient Temperature module to recalculate the body temperature field of the single battery during the hot and cold cycle process; Figure 4 The figure shows the recalculated temperature distribution of the single cell at a certain moment during the heating process;
[0082] (32) The body temperature field result recalculated in step (31) is imported into the Transient Structure module (i.e., transient structure module) in the ANSYS Workbench simulation software, and solid mechanics boundary conditions are applied to calculate the stress field of the single cell during the hot and cold cycle process; Figure 5 The figure shows the stress distribution of a single cell at a certain moment during the heat preservation process.
[0083] The solid thermal boundary conditions and solid mechanical boundary conditions applied in the above steps (31) and (32) are the same as those in step 2.
[0084] (4) Several creep fatigue specimens were prepared using the same material as the bipolar plate of the single cell, and high-temperature creep fatigue tests were performed to obtain the parameters related to the Larson-Miller creep model and the Larson-Miller equation for the bipolar plate material.
[0085] The specific steps of step (4) are:
[0086] (41) Several creep fatigue standard specimens were prepared using the same material as the bipolar plate material of the single cell (Crofer22 H). High-temperature creep fatigue tests were performed to obtain several sets of stress, temperature, and cracking time data, as shown in Tables 1 to 4.
[0087] Table 1 Creep cracking time of Crofer22H at 650℃
[0088]
[0089] Table 2 Creep cracking time of Crofer22H at 700℃
[0090]
[0091] Table 3 Creep cracking time of Crofer22H at 750℃
[0092]
[0093] Table 4 Creep cracking time of Crofer22H at 800℃
[0094]
[0095] (42) Based on the Larson-Miller equation, the stress, temperature, and cracking time data obtained from the high-temperature creep test in Tables 1 to 4 were fitted using Matlab software to obtain the parameters of the Larson-Miller equation and the Larson-Miller equation for the bipolar plate material.
[0096] Specifically, in this step, the high temperature creep fatigue test is carried out according to the "Metal Tensile Creep and Endurance Test Method", and the stress, temperature, and cracking time data obtained from the high temperature creep test are fitted using MATLAB software to obtain the parameters of the Larson-Miller equation. The parameter derivation process of the Larson-Miller equation is as follows:
[0097] The Larson-Miller equation can be expressed as:
[0098] (7)
[0099] in, is the temperature, is the constant in the Larson-Miller equation, is the total creep cracking time.
[0100] The constants in the above Larson-Miller equation are The size of is only related to the material, the parameters of the Larson-Miller equation It is related to the material's temperature and creep cracking time. When conducting creep tensile tests on materials, if the temperature and stress of the same material are determined, its cracking time must be determined.
[0101] Parameters of the Larson-Miller Equation Is with stress A parameter related to the parameter can be approximated by a polynomial. It can be expressed as the following polynomial:
[0102] (8)
[0103] in, , , , , are the fitting parameters of the polynomial.
[0104] After multiple curve fitting calculations by MATLAB, when the first 4 items on the right side of the equal sign of formula (8) are taken, the curve fitting degree is better and the error in creep life prediction of experimental data is smaller. By taking 4 items on the right side of the equal sign of formula (8), the simplified formula (9) can be obtained, namely:
[0105] (9)
[0106] in, is the total creep cracking time.
[0107] In order to facilitate the fitting of Matlab and obtain the unknown quantity, the formula can be sorted out to obtain formula (10), that is:
[0108] (10)
[0109] Assume that , , , and we get the following formula:
[0110] (11)
[0111] Based on formula (11) and the high temperature tensile creep test data of the bipolar plate material Crofer22 H, the surface fitting tool in Matlab software is used to fit formula (11) to obtain the unknown parameters in formula (11): , , , and , substituting into formula (9) we can obtain the Larson-Miller equation of material Crofer22 H, as Figure 6 The Larson-Miller equation curve of the fitted material Crofer22 H is used. The creep life of the SOFC bipolar plate under hot and cold cycles can be evaluated based on the obtained equation.
[0112] The Larson-Miller equation for the above bipolar plate material Crofer22 H is:
[0113] (12)
[0114] (5) The stress field distribution of the single cell under the hot and cold cycle obtained in step (3), the recalculated body temperature field, and the Larson-Miller equation curve or equation of the bipolar plate material obtained in step (4) are imported into nCode software (i.e., fatigue analysis software), and a CAE Creep Analysis module is used to perform creep fatigue simulation to predict the creep fatigue life of the solid oxide fuel cell bipolar plate during the hot and cold cycle process.
[0115] like Figure 7 The figure shows the creep fatigue life distribution of the cathode plate of a single SOFC cell. When the cathode plate uses Crofer22 H material, the minimum number of hot and cold cycles is 386 times, and the maximum damage is located at the gas inlet where the cathode plate contacts the cathode.
[0116] It should be noted that some parts not described in the present invention can be implemented by adopting or drawing on existing technologies.
[0117] Of course, the above description is not a limitation of the present invention, and the present invention is not limited to the above examples. Changes, modifications, additions or substitutions made by technicians in this technical field within the essential scope of the present invention should also fall within the protection scope of the present invention.
Claims
1. A method for predicting creep fatigue life of SOFC bipolar plates during hot and cold cycles. It is characterized in that Includes steps: (1) Based on the structure of a single cell of a solid oxide fuel cell, a three-dimensional geometric model of the single cell is established; (2) Importing the single-cell three-dimensional model established in step (1) into the Fluent finite element analysis software, setting the physical parameters, boundary conditions, and assumptions required for the finite element simulation according to the actual working conditions, setting the control equations for gas flow and heat transfer according to the assumptions, establishing a single-cell multi-physics field model based on the coupling of flow and heat transfer, performing finite element simulation calculations in the Fluent software, and obtaining the temperature field distribution of the single-cell under the cold and hot cycles; (3) Based on the temperature field distribution obtained in step (2), a solid mechanics analysis is performed on the single cell to obtain the stress field distribution of the single cell under the thermal cycle; (4) Using the same material as the bipolar plate of the single cell, several creep fatigue specimens were prepared and subjected to high temperature creep fatigue tests to obtain the parameters related to the Larson-Miller creep model and obtain the Larson-Miller equation for the bipolar plate material; (5) Based on the Larson-Miller equation of the bipolar plate material obtained in step (4), a creep fatigue simulation is performed using fatigue analysis software to predict the creep fatigue life of the solid oxide fuel cell bipolar plate during the hot and cold cycle process; The step (3) is specifically as follows: (31) Importing the temperature field of the flow channel surface in the temperature field result obtained in step (2) into the transient temperature module in the ANSYS Workbench simulation software, applying solid thermal boundary conditions in the transient temperature module, and recalculating the body temperature field of the single battery during the hot and cold cycle; (32) Importing the body temperature field result recalculated in step (31) into the transient dynamics module in the ANSYS Workbench simulation software, applying solid mechanics boundary conditions, and calculating the stress field of the single cell during the hot and cold cycle; The step (5) is specifically as follows: The stress field of the single cell under the hot and cold cycle obtained in step (3), the body temperature field recalculated in step (3), and the Larson-Miller equation of the bipolar plate material obtained in step (4) are imported into the fatigue analysis software, and the CAE technology is used to perform creep fatigue simulation to predict the creep life of the solid oxide fuel cell bipolar plate during the hot and cold cycle.
2. The method for predicting creep fatigue life of SOFC bipolar plates during hot and cold cycles according to claim 1, It is characterized in that The single cell structure in step (1) comprises a bipolar plate consisting of an anode plate and a cathode plate, a PEN unit consisting of an anode electrode layer, an electrolyte layer and a cathode electrode layer is arranged between the anode plate and the cathode plate, and an anode flow channel is arranged on the side of the anode plate close to the anode electrode layer, and a cathode flow channel is arranged on the side of the cathode plate close to the cathode electrode layer.
3. The method for predicting creep fatigue life of SOFC bipolar plates during hot and cold cycles according to claim 1, It is characterized in that The physical parameters in step (2) include: Density, thermal conductivity, thermal expansion coefficient, Poisson’s ratio and elastic modulus of each structural material of a single cell; Reverse absolute permeability and porosity of the anode electrode layer and cathode electrode layer of the porous material; Gas materials Dynamic viscosity, molar mass, specific heat capacity and thermal conductivity of anode gas and cathode gas.
4. The method for predicting creep fatigue life of SOFC bipolar plates during hot and cold cycles according to claim 1, It is characterized in that The boundary conditions in step (2) include: gas inlet temperature, gas inlet flow rate, gas outlet pressure, solid thermal boundary conditions and solid mechanical boundary conditions.
5. The method for predicting creep fatigue life of SOFC bipolar plates during hot and cold cycles according to claim 1, It is characterized in that The assumptions of the single-cell multi-physics model in step (2) include: The gas is an ideal gas and the flow state of the gas is laminar flow; The influence of thermal radiation during the hot and cold cycle is negligible; The properties of each structural material of a single cell are isotropic; The contact thermal resistance between the cathode, anode electrodes and the bipolar plate is negligible; Electrochemical reactions are not considered during the hot and cold cycle, and no mass transfer process is involved.
6. The method for predicting creep fatigue life of SOFC bipolar plates during hot and cold cycles according to claim 1, It is characterized in that The step (4) is specifically as follows: (41) Prepare several creep fatigue specimens using the same material as the bipolar plate of the single cell, conduct high temperature creep fatigue tests, and obtain several sets of stress, temperature and cracking time data; (42) Based on the Larson-Miller equation, the stress, temperature, and cracking time data obtained from the high-temperature creep test were fitted using Matlab software to obtain the parameters of the Larson-Miller equation and the Larson-Miller equation for the bipolar plate material.
Citation Information
Patent Citations
A prediction method for thermodynamic responses and fatigue-creep damage of a high-chrome steel material
CN108931448A
Method for predicting creep life of solid oxide fuel cell stack
CN116879782A
Solid oxide fuel cell flexible bipolar plate structure optimization design method
CN117592224A
Method for shutting down a solid oxide fuel cell at least for a short time
DE102006031717A1
Ferritic stainless steel having excellent thermal fatigue property
JP2009197305A