CMOS device and method for forming the same

By forming grooves in CMOS devices and performing in-situ epitaxial growth within them, combined with in-situ pre-baking treatment, the problems of uneven silicon channel thickness and the influence of pollutants are solved, and the uniformity of the channel layer is improved and quality.

CN118676063BActive Publication Date: 2024-11-29HANGZHOU HFC SEMICONDUCTOR CO
View PDF 8 Cites 0 Cited by

Patent Information

Application Number
CN202411095538.5
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-08-12
Publication Date
2024-11-29
Estimated Expiration
2044-08-12

AI Technical Summary

Technical Problem

During the epitaxial growth process of traditional silicon channels, the thickness is uneven due to different crystal epitaxial rates, and the carbon pollutants and oxygen pollutants on the surface of the PFET region affect the quality of the channel layer.

Method used

In the formation method of CMOS device, by forming grooves in the PFET region and exposing the side walls of shallow trench isolation structures, a channel layer is formed in the grooves by in-situ epitaxial growth process, and the original operation is performed before forming the channel layer. Pre-bake treatment to remove water vapor and contaminants.

Benefits of technology

The thickness uniformity of the channel layer is improved, the content of carbon pollutants and oxygen pollutants is reduced, and the quality of the channel layer is improved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118676063B_ABST
    Figure CN118676063B_ABST
Patent Text Reader

Abstract

The present invention provides a CMOS device and a method for forming the same. In the method for forming the CMOS device, a groove is formed by in-situ etching back a PFET region, the groove penetrates a portion of the thickness of the PFET region, and the groove exposes a portion of the sidewall of a shallow trench isolation structure. When a channel layer is subsequently formed in the groove by an in-situ epitaxial growth process, the shallow trench isolation structure on the sidewall of the groove can block the lateral growth of the channel layer, thereby avoiding the problem that the thickness of the channel layer at the edge of the PFET region is thinner than that of the channel layer at the center of the PFET region, thereby improving the thickness uniformity of the channel layer. In addition, before forming the channel layer, an in-situ pre-baking treatment is performed on the substrate to remove water vapor and pollutants in the groove, and the processes of in-situ etching back the PFET region, in-situ pre-baking treatment, and in-situ epitaxial growth process are all performed in-situ, thereby reducing the content of carbon pollutants and oxygen pollutants in the groove, thereby improving the quality of the channel layer.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of semiconductor technology, and in particular to a CMOS device and a method for forming the same. Background Art

[0002] As device size decreases, the carrier mobility of traditional silicon channels is low. In order to better improve device performance, such as Figure 1 As shown, an epitaxial channel layer 12 is usually introduced into the PFET region 11 of the substrate 10, and the material of the channel layer 12 is, for example, germanium silicon. However, during the epitaxial growth process of the channel layer 12, due to the different epitaxial growth rates in each crystal direction, the channel layer will undergo lateral epitaxial growth, resulting in the thickness of the channel layer 12 in the edge region being thinner than that in the central region, and even the problem of different thicknesses of the channel layer 12 in the device sparse region II and the device dense region I, resulting in different thicknesses of the channel layer 12 on the PFET regions with different channel widths, that is, the thickness of the channel layer 12 is uneven, and this thickness unevenness not only reduces the quality of the channel layer, but also affects the reliability and performance of subsequent devices. In addition, there are carbon pollutants and oxygen pollutants on the surface of the PFET region 11, which will affect the growth of the channel layer 12 and thus form defects. Summary of the invention

[0003] The object of the present invention is to provide a CMOS device and a method for forming the same, so as to improve the thickness uniformity of the channel layer and reduce or avoid carbon pollutants and oxygen pollutants.

[0004] To achieve the above-mentioned purpose, the present invention provides a method for forming a CMOS device, comprising: providing a substrate, the substrate comprising adjacent PFET regions and NFET regions, a shallow trench isolation structure being formed between the PFET regions and the NFET regions; forming a patterned mask layer on the substrate, the patterned mask layer covering the NFET region and exposing the PFET region; using the patterned mask layer as a mask, in-situ etching back the PFET region to form a groove, the groove penetrating a portion of the thickness of the PFET region, and the groove exposing a portion of the sidewall of the shallow trench isolation structure; performing an in-situ pre-baking treatment on the substrate; forming a channel layer in the groove using an in-situ epitaxial growth process, the top surface of the channel layer being flush with the top surface of the shallow trench isolation structure; and removing the patterned mask layer.

[0005] Optionally, in the method for forming the CMOS device, when the PFET region is etched back in situ, the etching gas used includes hydrogen chloride.

[0006] Optionally, in the method for forming the CMOS device, the gas used for the in-situ pre-bake includes hydrogen, and the temperature of the in-situ pre-bake is 750°C to 850°C.

[0007] Optionally, in the method for forming the CMOS device, the depth of the groove is 5 nm to 15 nm.

[0008] Optionally, in the method for forming the CMOS device, after forming the patterned mask layer and before in-situ back-etching the PFET region, a natural oxide layer is also formed on the surface of the patterned mask layer and the surface of the PFET region; before in-situ back-etching the PFET region, the method for forming the CMOS device also includes: performing an in-situ plasma cleaning process to remove the natural oxide layer.

[0009] Optionally, in the method for forming the CMOS device, when performing the in-situ plasma cleaning process, the cleaning gas used includes nitrogen trifluoride and ammonia.

[0010] Optionally, in the method for forming the CMOS device, the in-situ plasma cleaning process, the in-situ etching back of the PFET region, the in-situ pre-bake process and the in-situ epitaxial growth process are completed in the same reaction chamber.

[0011] Optionally, in the method for forming a CMOS device, the material of the channel layer is silicon germanium.

[0012] Optionally, in the method for forming the CMOS device, the substrate has a device-dense area and a device-sparse area, the substrate in the device-dense area and the substrate in the device-sparse area both include a plurality of the PFET areas and a plurality of the NFET areas, at least two of the PFET areas in all the PFET areas in the device-dense area have different channel widths, at least two of the PFET areas in all the PFET areas in the device-sparse area have different channel widths, and the thickness of the channel layer on all the PFET areas in the device-dense area is the same as the thickness of the channel layer on all the PFET areas in the device-sparse area.

[0013] Based on the same inventive concept, the present invention also provides a CMOS device, comprising: a substrate, the substrate comprising adjacent PFET regions and NFET regions, a shallow trench isolation structure being formed between the PFET region and the NFET region, a groove being formed in the PFET region, the groove penetrating a portion of the thickness of the PFET region, and the groove exposing a portion of the sidewall of the shallow trench isolation structure; a channel layer, the channel layer being formed in the groove, and the top surface of the channel layer being flush with the top surface of the shallow trench isolation structure.

[0014] In the CMOS device and its formation method provided by the present invention, a groove is formed by in-situ etching back the PFET region, the groove penetrates the PFET region of a part of the thickness, and the groove exposes the side wall of a part of the shallow trench isolation structure. When the channel layer is subsequently formed in the groove by an in-situ epitaxial growth process, the shallow trench isolation structure on the side wall of the groove can block the lateral growth of the channel layer, thereby avoiding the problem that the thickness of the channel layer at the edge of the PFET region is thinner than the thickness of the channel layer in the center of the PFET region, thereby improving the thickness uniformity of the channel layer. Furthermore, before forming the channel layer, the substrate is subjected to an in-situ pre-baking treatment, so that the water vapor and pollutants in the groove can be removed. And the processes of in-situ etching back the PFET region, in-situ pre-baking treatment and in-situ epitaxial growth process are all carried out in-situ, thereby reducing the content of carbon pollutants and oxygen pollutants in the groove, so that the content of carbon pollutants and oxygen pollutants in the groove is maintained at a low level, thereby improving the quality of the channel layer. BRIEF DESCRIPTION OF THE DRAWINGS

[0015] Figure 1 Schematic diagram of SEM of the channel layer in the prior art.

[0016] Figure 2 It is a schematic flow chart of a method for forming a CMOS device provided by an embodiment of the present invention.

[0017] Figure 3 It is a schematic diagram of the structure after the PFET region and the NFET region are formed in the method for forming a CMOS device provided by an embodiment of the present invention.

[0018] Figure 4 It is a schematic diagram of the structure after a mask layer is formed in the method for forming a CMOS device provided by an embodiment of the present invention.

[0019] Figure 5 It is a schematic diagram of the structure after a patterned mask layer is formed in the method for forming a CMOS device provided by an embodiment of the present invention.

[0020] Figure 6 It is a schematic diagram of the structure after a natural oxide layer is formed in the method for forming a CMOS device provided in an embodiment of the present invention.

[0021] Figure 7 It is a schematic diagram of the structure after a groove is formed in the method for forming a CMOS device provided by an embodiment of the present invention.

[0022] Figure 8 It is a schematic diagram of the structure after a channel layer is formed in the method for forming a CMOS device provided by an embodiment of the present invention.

[0023] Fig. 9 It is a schematic diagram of the structure after removing the patterned mask layer in the method for forming a CMOS device provided by an embodiment of the present invention.

[0024] Fig.10 It is a schematic diagram of the structure after a gate dielectric layer is formed in the method for forming a CMOS device provided by an embodiment of the present invention.

[0025] Fig.11 is a SEM schematic diagram of a CMOS device provided in an embodiment of the present invention.

[0026] Among them, the figure numbers are explained as follows: 10-substrate; 11-PFET region; 12-channel layer; 100-substrate; 100A-PFET region; 100B-NFET region; 101-bottom silicon layer; 102-insulating layer; 103-top silicon layer; 110-shallow trench isolation structure; 120-mask layer; 120A-patterned mask layer; 130-natural oxide layer; 140-groove; 140A-corner; 150-channel layer; 160-gate dielectric layer. DETAILED DESCRIPTION

[0027] The CMOS device and the method for forming the same proposed by the present invention are further described in detail below in conjunction with the accompanying drawings and specific embodiments. The advantages and features of the present invention will become more apparent from the following description. It should be noted that the accompanying drawings are all in a very simplified form and are not in precise proportions, and are only used to conveniently and clearly assist in explaining the purpose of the embodiments of the present invention.

[0028] As used in the present invention, the singular forms "one", "an", and "the" include plural objects, the term "or" is generally used to include the meaning of "and / or", the term "several" is generally used to include the meaning of "at least one", and the term "at least two" is generally used to include the meaning of "two or more". In addition, the terms "first", "second", and "third" are used only for descriptive purposes and cannot be understood as indicating or implying relative importance or implicitly indicating the number of indicated technical features. Therefore, the features defined as "first", "second", and "third" may explicitly or implicitly include one or at least two of the features.

[0029] Figure 2 FIG. 1 is a flow chart of a method for forming a CMOS device provided by an embodiment of the present invention. Figure 2 As shown, the method for forming the CMOS device includes: step S1: providing a substrate, the substrate including adjacent PFET regions and NFET regions, a shallow trench isolation structure being formed between the PFET region and the NFET region; step S2: forming a patterned mask layer on the substrate, the patterned mask layer covering the NFET region and exposing the PFET region; step S3: using the patterned mask layer as a mask, in-situ etching back the PFET region to form a groove, the groove penetrating a portion of the thickness of the PFET region, and the groove exposing a portion of the sidewall of the shallow trench isolation structure; step S4: performing an in-situ pre-bake treatment on the substrate; step S5: forming a channel layer in the groove by an in-situ epitaxial growth process, the top surface of the channel layer being flush with the top surface of the shallow trench isolation structure; step S6: removing the patterned mask layer.

[0030] The following will be combined with the attached Figure 3~Figure 10 The method for forming the CMOS device provided in this embodiment is described in more detail.

[0031] Figure 3 FIG. 1 is a schematic diagram of a structure after forming a PFET region and an NFET region in a method for forming a CMOS device provided by an embodiment of the present invention. First, referring to FIG. Figure 3 As shown, step S1 is performed to provide a substrate 100, wherein the substrate 100 includes adjacent PFET regions 100A and NFET regions 100B, and a shallow trench isolation structure (STI) 110 is formed between the PFET region 100A and the NFET region 100B. The PFET region 100A is used to form a P-type field effect transistor (PFET), and the NFET region 100B is used to form an N-type field effect transistor (NFET). Further, both the PFET region 100A and the NFET region 100B have a well region. In order to better illustrate the invention, the description and illustration of the well region are omitted.

[0032] In this embodiment, the material of the substrate 100 may be silicon on insulator (SOI), that is, the substrate 100 is composed of a bottom silicon layer 101, an insulating layer 102, and a top silicon layer 103 stacked in sequence from bottom to top, wherein the shallow trench isolation structure 110 is formed in the top silicon layer 103, and the shallow trench isolation structure 110 may penetrate the top silicon layer 103 and isolate the top silicon layer 103 into a PFET region 100A and an NFET region 100B. Further, the top surface of the shallow trench isolation structure 110, the top surface of the PFET region 100A, and the top surface of the NFET region 100B are flush. The cross-sectional shape of the shallow trench isolation structure 110 may be a rectangle or an inverted trapezoid. In this embodiment, the cross-sectional shape of the shallow trench isolation structure 110 is an inverted trapezoid as an example for description.

[0033] Further, such as Figure 3 As shown, the substrate 100 has a device dense area I and a device sparse area II, wherein the device sparse area II refers to an area with a lower device density, and the device dense area I refers to an area with a higher device density.

[0034] Furthermore, the substrate 100 of the device dense area I and the substrate 100 of the device sparse area II both include multiple (more than three) PFET regions 100A and multiple (more than three) NFET regions 100B, and among all the PFET regions 100A in the device sparse area II, at least two of the PFET regions 100A have different channel widths. For example, the channel width of one PFET region 100A in the device sparse area II may be a short width, and the channel width of another PFET region 100A may be a long width, and the long width is greater than the short width.

[0035] Among all the PFET regions 100A in the device dense area I, at least two PFET regions have different channel widths. Figure 3 As shown, the channel width of one PFET region 100A in the device dense area I is a short width W1, and the channel width of another PFET region 100A is a long width W2, and the long width W2 is greater than the short width W1.

[0036] The density of the PFET region 100A in the device dense area I is greater than the density of the PFET region 100A in the device sparse area II, and the density of the NFET region 100B in the device dense area I is greater than the density of the NFET region 100B in the device sparse area II.

[0037] Figure 4It is a schematic diagram of the structure after a mask layer is formed in the method for forming a CMOS device provided by an embodiment of the present invention. Figure 5 FIG. 1 is a schematic diagram of a structure after a patterned mask layer is formed in the method for forming a CMOS device provided in an embodiment of the present invention. Figure 5 As shown, step S2 is performed to form a patterned mask layer 120A on the substrate 100, wherein the patterned mask layer 120A covers the NFET region 100B and exposes the PFET region 100A. In a further solution, the patterned mask layer 120A may also expose a portion of the shallow trench isolation structure 110 close to the PFET region 100A and cover a portion of the shallow trench isolation structure 110 close to the NFET region 100B.

[0038] Specifically, the method of forming the patterned mask layer 120A on the substrate 100 includes: Figure 4 As shown, a mask layer 120 covering the substrate 100 is formed, wherein the material of the mask layer 120 may be silicon oxide, and the method for forming the mask layer 120 may adopt any existing technology familiar to those skilled in the art, such as a wet oxygen oxidation process; a patterned photoresist layer (not shown) is formed on the mask layer 120, and the patterned photoresist layer exposes the PFET region 100A; as shown Figure 5 As shown, the mask layer 120 is etched using the patterned photoresist layer as a mask to remove the mask layer 120 in the PFET region 100A, thereby forming a patterned mask layer 120A; thereafter, the patterned photoresist layer is removed.

[0039] Figure 6 FIG. 1 is a schematic diagram of a structure after a natural oxide layer is formed in the method for forming a CMOS device provided in an embodiment of the present invention. Figure 6 As shown, since the patterned mask layer 120A and the PFET region 100A are exposed, a natural oxide layer 130 will be formed on their surfaces in an environment containing oxygen and water. Therefore, a natural oxide layer 130 will be formed on the surface of the patterned mask layer 120A and the surface of the PFET region 100A.

[0040] Afterwards, an in-situ plasma cleaning process is performed to remove the natural oxide layer 130, as well as carbon pollutants (derived from the atmosphere and organic volatilization in the photoresist layer, etc.) and oxygen pollutants on the surface of the patterned mask layer 120A, and carbon pollutants and oxygen pollutants on the surface of the PFET region 100A. Further, when performing the in-situ plasma cleaning process, the cleaning gas used includes nitrogen trifluoride (NF3) and ammonia (NH3).

[0041] Specifically, the process of in-situ plasma cleaning treatment includes: placing the substrate 100 in a reaction chamber, and exciting the cleaning gas (NF3 and NH3) in the reaction chamber by means of a high-frequency electric field or microwave to generate plasma. After the cleaning gas (NF3 and NH3) is introduced into the plasma region, it decomposes in the plasma environment to generate active free radicals. These free radicals react chemically with the natural oxide layer 130, thereby converting the natural oxide layer 130 into a volatile gas or solid product, and at the same time, the carbon pollutants and oxygen pollutants on the surface of the patterned mask layer 120A, and the carbon pollutants and oxygen pollutants on the surface of the PFET region 100A are discharged from the reaction chamber.

[0042] Figure 7 FIG. 1 is a schematic diagram of a structure after a groove is formed in the method for forming a CMOS device provided by an embodiment of the present invention. Figure 7 As shown, step S3 is performed, using the patterned mask layer 120A as a mask, in-situ etching back the PFET region 100A to form a groove 140, wherein the groove 140 penetrates a portion of the thickness of the PFET region 100A, and the groove 140 exposes a portion of the sidewall of the shallow trench isolation structure 110. Specifically, during the in-situ etching back of the PFET region 100A, the etching gas used includes hydrogen chloride (HCl), so that the PFET region 100A has a higher etching selectivity with the shallow trench isolation structure 110, thereby reducing or avoiding damage to the shallow trench isolation structure 110.

[0043] Preferably, during the in-situ etching back of the PFET region 100A, the PFET region 100A is etched along the sidewall of the shallow trench isolation structure 110 to form a groove 140 , and the groove 140 is used as a growth window for a channel layer 150 to be formed subsequently.

[0044] Preferably, the cross-sectional shape of the groove 140 may be a rectangle, which is helpful to reduce the lateral growth of the subsequent channel layer 150. Alternatively, the cross-sectional shape of the groove 140 may also be a trapezoid.

[0045] It should be noted that in-situ etching back the PFET region 100A means that all PFET regions 100A in the device dense region I and the device sparse region II are etched back in-situ, so as to form a groove 140 in each PFET region 100A, and the depth of the groove 140 in each PFET region 100A is the same. Further, the depth of the groove 140 can be 5nm to 15nm. In addition, since there are PFET regions 100A with different channel widths in both the device dense region I and the device sparse region II, the widths of the grooves 140 in the PFET regions 100A with different channel widths are also different.

[0046] The in-situ etching back of the PFET region 100A and the in-situ plasma cleaning process are performed in the same reaction chamber.

[0047] Next, step S4 is performed to perform an in-situ pre-baking treatment on the substrate 100, wherein the gas used in the in-situ pre-baking treatment includes hydrogen. By performing the in-situ pre-baking treatment on the substrate 100, water vapor and impurities on the substrate 100 can be removed, especially water vapor in the groove 140 and impurities (carbon pollutants and oxygen pollutants) remaining in the groove 140 can be removed.

[0048] It should be noted that the temperature during the in-situ pre-baking process should not be too high or too low. If the temperature during the in-situ pre-baking process is too high, it is easy to cause heat diffusion inside the substrate 100 and cause uncontrolled reflow of silicon atoms in the groove 140, thereby destroying the structural contour of the groove 140, thereby causing the corner 140A of the groove 140 to be rounded, that is, causing damage to the silicon in the substrate 100 at the corner 140A of the groove 140, and then causing the edge area of ​​the channel layer 150 subsequently formed in the groove 140 to become thinner. In addition, if the temperature during the in-situ pre-baking process is too high, it will also cause lattice disturbance in the groove 140, affecting the quality of the channel layer 150 subsequently formed in the groove 140. If the temperature during the in-situ pre-baking process is too low, it is easy to cause water vapor or impurities in the groove 140 to be difficult to remove. For this reason, in this embodiment, the temperature of the in-situ pre-baking process is 750°C~850°C, for example, 800°C.

[0049] Furthermore, since in-situ plasma cleaning is performed in the aforementioned steps and the groove 140 is formed by in-situ back etching, the impurity content in the groove 140 during the etching process can be further reduced, so a low temperature in-situ pre-baking process can be used, that is, the temperature of the in-situ pre-baking process can be set to 750°C~850°C. In this way, while ensuring that water vapor or impurities in the groove 140 can be removed, the backflow of silicon atoms in the groove 140 can be avoided and the rounding of the corner 140A of the groove 140 can be avoided, thereby avoiding damage to the silicon in the substrate 100 at the corner 140A of the groove 140, which is beneficial to avoid thinning of the edge area of ​​the subsequently formed channel layer 150.

[0050] Figure 8 FIG. 1 is a schematic diagram of a structure after a channel layer is formed in the method for forming a CMOS device provided by an embodiment of the present invention. Figure 8As shown, step S5 is performed to form a channel layer 150 in the groove 140 by an in-situ epitaxial growth process, and the top surface of the channel layer 150 is flush with the top surface of the shallow trench isolation structure 110. The thickness of the channel layer 150 can be 5nm~15nm, that is, the thickness of the channel layer 150 is the same as the depth of the groove 140.

[0051] Specifically, the in-situ epitaxial growth process may be a selective epitaxial growth process, such as a molecular beam epitaxy (MBE) process or a reduced pressure chemical vapor deposition (RPCVD) process, so that the channel layer 150 may be formed only on the surface of the PFET region 100A. The material of the channel layer 150 may be germanium silicon.

[0052] In this embodiment, in the process of forming the channel layer 150 by the in-situ epitaxial growth process, the process temperature can be 600°C to 700°C. The process gas includes a silicon source gas, a germanium source gas, an etching gas and a doping source gas, wherein the doping source gas is used to provide doping ions, for example, borane (BH3), diborane (B2H6) or boron trichloride (BCl3); the silicon source gas can be silane (SiH4), disilane (Si2H6), trisilane (Si3H8) or dichlorosilane (SiH2Cl2), and the germanium source gas can be germanium (GeH4); the etching gas can be hydrogen chloride (HCl), which is used to increase the selectivity of deposition to form the channel layer 150 in the groove 140. Further, the process gas for forming the channel layer 150 also includes hydrogen, which is used as a carrier gas for the etching gas.

[0053] Preferably, the in-situ plasma cleaning treatment, the in-situ back-etching of the PFET region 100A, the in-situ pre-baking treatment and the in-situ epitaxial growth process are completed in the same reaction chamber, that is, the in-situ plasma cleaning treatment, the in-situ back-etching of the PFET region 100A, the in-situ pre-baking treatment and the in-situ epitaxial growth process are completed by the same equipment, for example, molecular beam epitaxy (MBE) process equipment or reduced pressure chemical vapor deposition (RPCVD) equipment, thereby reducing the content of carbon pollutants and oxygen pollutants in the groove 140, so that the content of carbon pollutants and oxygen pollutants in the groove 140 is maintained at a low level, thereby improving the quality of the channel layer 150.

[0054] In this embodiment, the <110> The crystal direction is used as the channel direction of the PFET region 100A to accelerate the hole mobility in the channel of the PFET region 100A. In the process of forming the channel layer 150, due to the epitaxial anisotropy of the in-situ epitaxial growth process, the channel layer 150 is <100> The growth rate in the width direction (or lateral direction, i.e., toward <110> The growth rate of the channel layer 150 is fast. And because the channel layer 150 is formed in the groove 140, and the sidewall of the groove 140 is the shallow trench isolation structure 110, the shallow trench isolation structure 110 can block the lateral growth of the channel layer 150 during the epitaxial growth of the channel layer 150, thereby avoiding the problem that the thickness of the channel layer 150 at the edge of the PFET region 100A (close to the shallow trench isolation structure) is thinner than the thickness of the channel layer 150 at the center of the PFET region 100A, thereby improving the thickness uniformity of the channel layer 150, and making the thickness of the channel layer 150 on the PFET regions 100A with different channel widths and different densities the same. That is, since the PFET regions 100A with different channel widths exist in both the device dense area I and the device sparse area II, the widths of the channel layers 150 formed on the PFET regions 100A with different channel widths are also different, and the concentration (density) of the channel layer 150 on the PFET region 100A in the device dense area I and the channel layer 150 on the PFET region 100A in the device sparse area II are different, but the thickness of the channel layer 150 on all the PFET regions 100A in the device dense area I is the same as the thickness of the channel layer 150 on all the PFET regions 100A in the device sparse area II, thereby avoiding the thickness difference between the channel layers 150 on the PFET regions 100A with different channel widths and different densities, and further avoiding the thickness loading effect.

[0055] Fig. 9 FIG. 1 is a schematic diagram of a structure after removing the patterned mask layer in the method for forming a CMOS device provided by an embodiment of the present invention. Fig. 9 As shown, step S6 is performed to remove the patterned mask layer 120A. Preferably, the patterned mask layer 120A is removed by a wet etching process, and the solution used in the wet etching process includes hydrofluoric acid, so that the patterned mask layer 120A has a high etching selectivity with the channel layer 150, thereby avoiding damage to the channel layer 150.

[0056] Fig.10 FIG. 1 is a schematic diagram of a structure after a gate dielectric layer is formed in a method for forming a CMOS device according to an embodiment of the present invention. Fig.10As shown, a gate dielectric layer 160 is formed, and the gate dielectric layer 160 covers the channel layer 150, the shallow trench isolation structure 110, the PFET region 100A and the NFET region 100B. The material of the gate dielectric layer 160 can be silicon oxide. Preferably, the gate dielectric layer 160 is formed by a thermal oxidation process. Compared with other methods, the interface compatibility between the gate dielectric layer 160 formed by the thermal oxidation process and the channel layer 150 is good.

[0057] This embodiment also provides a CMOS (Complementary Metal Oxide Semiconductor) device, such as Fig.10 As shown, it includes: a substrate 100, the substrate 100 includes adjacent PFET regions 100A and NFET regions 100B, a shallow trench isolation structure 110 is formed between the PFET region 100A and the NFET region 100B, a groove 140 is formed in the PFET region 100A, the groove 140 penetrates a portion of the thickness of the PFET region 100A, and the groove 140 exposes a portion of the sidewall of the shallow trench isolation structure 110; a channel layer 150, the channel layer 150 is formed in the groove 140, and the top surface of the channel layer 150 is flush with the top surface of the shallow trench isolation structure 110.

[0058] Specifically, Fig.10 As shown, the substrate 100 has a device dense area I and a device sparse area II. The substrate 100 in the device dense area I and the substrate 100 in the device sparse area II both include a plurality of (more than three) PFET regions 100A and a plurality of (more than three) NFET regions 100B. The density of the PFET regions 100A in the device dense area I is greater than the density of the PFET regions 100A in the device sparse area II, and the density of the NFET regions 100B in the device dense area I is greater than the density of the NFET regions 100B in the device sparse area II. Among all the PFET regions 100A in the device dense area I, at least two of the PFET regions have different channel widths. For example, the channel width of one PFET region 100A in the device dense area I is a short width, and the channel width of another PFET region 100A is a long width, and the long width is greater than the short width.

[0059] Among all the PFET regions 100A in the device sparse region II, at least two of the PFET regions 100A have different channel widths. For example, the channel width of one PFET region 100A in the device sparse region II may be a short width, and the channel width of another PFET region 100A may be a long width, and the long width is greater than the short width.

[0060] Fig.11 is a SEM schematic diagram of a CMOS device provided by an embodiment of the present invention. Fig.11 As shown, the thickness of the channel layer 150 at the edge of the PFET region 100A is substantially the same as the thickness of the channel layer 150 at the center of the PFET region 100A, and the thickness of the channel layer 150 on the PFET region 100A in the device dense region I is the same as the thickness of the channel layer 150 on the PFET region 100A in the device sparse region II, that is, the thickness of the channel layer 150 on the PFET regions 100A with different densities and different channel widths is the same, thereby improving the thickness uniformity of the channel layer 150.

[0061] Further, such as Fig.10 As shown, the CMOS device further includes a gate dielectric layer 160 , and the gate dielectric layer 160 covers the channel layer 150 , the shallow trench isolation structure 110 , the PFET region 100A and the NFET region 100B.

[0062] In summary, in the CMOS device and the method for forming the same provided by the embodiment of the present invention, the PFET region is etched back in situ to form a groove, the groove penetrates the PFET region of a part of the thickness, and the groove exposes the sidewall of a part of the shallow trench isolation structure. When the channel layer is subsequently formed in the groove by an in-situ epitaxial growth process, the shallow trench isolation structure on the sidewall of the groove can block the lateral growth of the channel layer, thereby avoiding the problem that the thickness of the channel layer at the edge of the PFET region is thinner than the thickness of the channel layer at the center of the PFET region, thereby improving the thickness uniformity of the channel layer. Furthermore, before forming the channel layer, the substrate is subjected to an in-situ pre-baking treatment, so that the water vapor and pollutants in the groove can be removed. And the processes of in-situ etching back the PFET region, in-situ pre-baking treatment and in-situ epitaxial growth process are all carried out in situ, thereby reducing the content of carbon pollutants and oxygen pollutants in the groove, so that the content of carbon pollutants and oxygen pollutants in the groove is maintained at a low level, thereby improving the quality of the channel layer.

[0063] The above description is only a description of the preferred embodiment of the present invention, and is not any limitation on the scope of the present invention. Any changes and modifications made by ordinary technicians in the field of the present invention based on the above disclosure are within the scope of protection of the claims. In addition, it should be recognized that although the present invention has been disclosed as above with preferred embodiments, the above embodiments are not used to limit the present invention. For any technician familiar with the art, without departing from the scope of the technical solution of the present invention, the technical content disclosed above can be used to make many possible changes and modifications to the technical solution of the present invention, or modified into equivalent embodiments of equivalent changes. Therefore, any simple modifications, equivalent changes and modifications made to the above embodiments based on the technical essence of the present invention without departing from the content of the technical solution of the present invention are still within the scope of protection of the technical solution of the present invention.

Claims

1. A method for forming a CMOS device, It is characterized in that include: Providing a substrate, the substrate comprising a PFET region and an NFET region adjacent to each other, wherein a shallow trench isolation structure is formed between the PFET region and the NFET region; forming a patterned mask layer on the substrate, wherein the patterned mask layer covers the NFET region and exposes the PFET region; Using the patterned mask layer as a mask, in-situ etching back the PFET region to form a groove, wherein the groove penetrates a portion of the thickness of the PFET region and the groove exposes a portion of the sidewall of the shallow trench isolation structure; performing an in-situ pre-baking process on the substrate; Forming a channel layer in the groove by an in-situ epitaxial growth process, wherein the top surface of the channel layer is flush with the top surface of the shallow trench isolation structure; The patterned mask layer is removed.

2. The method for forming a CMOS device according to claim 1, It is characterized in that When the PFET region is etched back in situ, the etching gas used includes hydrogen chloride.

3. The method for forming a CMOS device according to claim 1, It is characterized in that The gas used in the in-situ pre-bake treatment includes hydrogen, and the temperature of the in-situ pre-bake treatment is 750° C. to 850° C.

4. The method for forming a CMOS device according to claim 1, It is characterized in that The depth of the groove is 5nm~15nm.

5. The method for forming a CMOS device according to claim 1, It is characterized in that After forming the patterned mask layer and before in-situ etching back the PFET region, a natural oxide layer is also formed on the surface of the patterned mask layer and the surface of the PFET region; Before in-situ etching back the PFET region, the method for forming the CMOS device further includes: performing an in-situ plasma cleaning process to remove the natural oxide layer.

6. The method for forming a CMOS device according to claim 5, It is characterized in that When performing the in-situ plasma cleaning process, the cleaning gas used includes nitrogen trifluoride and ammonia.

7. The method for forming a CMOS device according to claim 5, It is characterized in that The in-situ plasma cleaning process, the in-situ etching back of the PFET region, the in-situ pre-baking process and the in-situ epitaxial growth process are completed in the same reaction chamber.

8. The method for forming a CMOS device according to claim 1, It is characterized in that The material of the channel layer is germanium silicon.

9. The method for forming a CMOS device according to claim 1, It is characterized in that The substrate has a device-dense area and a device-sparse area, and both the substrate of the device-dense area and the substrate of the device-sparse area include multiple PFET areas and multiple NFET areas. Among all the PFET areas in the device-dense area, at least two of the PFET areas have different channel widths, and among all the PFET areas in the device-sparse area, at least two of the PFET areas have different channel widths, and the thickness of the channel layer on all the PFET areas in the device-dense area is the same as the thickness of the channel layer on all the PFET areas in the device-sparse area.

10. A CMOS device, It is characterized in that Prepared by the method for forming a CMOS device according to any one of claims 1 to 9, comprising: A substrate, the substrate comprising adjacent PFET regions and NFET regions, a shallow trench isolation structure is formed between the PFET region and the NFET region, a groove is formed in the PFET region, the groove penetrates a portion of the thickness of the PFET region, and the groove exposes a portion of the sidewall of the shallow trench isolation structure; A channel layer is formed in the groove, and a top surface of the channel layer is flush with a top surface of the shallow trench isolation structure.

Citation Information

Patent Citations

  • Semiconductor device and manufacturing method thereof

    CN104934324A

  • Semiconductor device and manufacturing method thereof

    CN109427676A

  • Using a metal-containing layer as an etching stop layer and to pattern source / drain regions of a finfet

    CN109427872A

  • Methods for protecting film layers while removing hardmasks during fabrication of semiconductor devices

    US20110086495A1

  • Integrated circuit structure having substantially planar n-p step height and methods of forming

    US20120256268A1