Rumen protection L-carnitine and preparation method thereof

By using a combination of silicon-based L-carnitine and multi-component protective agents, combined with twin-screw extrusion granulation and coating technology, the degradation of L-carnitine in the rumen of ruminants and the problem of moisture absorption and adhesion during the granulation process have been solved, and the problem has been improved. Its bioavailability and stability achieve efficient rumen protection and release effects.

CN118766010APending Publication Date: 2024-10-15SHANGHAI MEINONG FEED CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410999587.5
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-24
Publication Date
2024-10-15

AI Technical Summary

Technical Problem

In the prior art, L-carnitine is degraded in the rumen of ruminants, resulting in low utilization of effective substances, and there are problems such as moisture adhesion and low primary yield during the granulation process.

Method used

Silicone L-carnitine is used as the core material. The internal protective agent is composed of fillers, adhesives and wetting agents. The outer coating agent is composed of main coating materials and controlled release agents. It is granulated and coated through twin-screw extrusion. technology to prepare highly bioavailable rumen-protecting L-carnitine.

Benefits of technology

It improves the bioavailability and stability of L-carnitine, solves the problems of moisture absorption and low primary yield during the granulation process, ensures the effective release and absorption of L-carnitine in ruminants, and enhances its biological effects.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118766010A_ABST
    Figure CN118766010A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of feed additive processing, in particular to rumen protection L-carnitine and a preparation method thereof. The composite material comprises the following components in percentage by weight: 60-75% of a core material, 5-10% of an inner protective agent and 20-30% of an outer coating agent, the core material is silicon-type L-carnitine, the protective agent is composed of a filler, an adhesive and a wetting agent, and the outer coating agent is composed of a main coating material and a controlled release agent. The preparation method comprises the following steps: uniformly mixing a core material with a filler and a dry powder adhesive, mixing with spray water, granulating, and coating with a suspension coating agent prepared from a main coating material and a controlled release agent to obtain the rumen protection L-carnitine product. Results of the embodiment show that the L-carnitine product prepared by the invention is high in bioavailability, and can smoothly pass through the rumen of a ruminant to reach a capsid in the abomasum to be damaged, so that the L-carnitine is quickly released to reach the small intestine to play the effects of converting fat into energy, reducing fat accumulation and the like.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of feed additive processing, and particularly relates to rumen-protected L-carnitine and a preparation method thereof. Background Art

[0002] L-Carnitine, also known as L-carnitine, can be synthesized in animals from lysine and methionine. It is a vitamin-like or amino acid-like substance that promotes the conversion of fat into energy. The pure product is white crystal or white transparent fine powder with a slightly special fishy smell. It is very soluble in water and absorbs moisture. It will deliquesce or even liquefy when exposed to air.

[0003] There are two main sources of L-carnitine in animals, namely, self-synthesis and feed supply. About 75% of the source comes from feed supply, and about 25% comes from biosynthesis in the body. As a feed additive, L-carnitine can accelerate the transport and oxidation of fatty acids, promote fat metabolism, help reduce fat accumulation, and increase the growth rate and weight gain of animals. In addition, L-carnitine also has the functions of reducing the incidence of metabolic diseases such as fatty liver and ammonia poisoning in animals, enhancing antioxidant capacity, improving immunity, and promoting muscle development. Studies have shown that adding L-carnitine to ruminant feed will increase the carnitine content in ruminants, and has a significant effect on inhibiting fat deposition, preventing and treating hyperammonemia. However, due to the special digestive physiology of ruminants, unprotected L-carnitine will be degraded by rumen vitamins after passing through the rumen of ruminants, thereby reducing the content of effective substances reaching the small intestine, resulting in a lower utilization rate of the final effective substances. Therefore, it is necessary to protect L-carnitine through the rumen to stabilize it in the rumen of ruminants, and slowly release it after reaching the true stomach to play a role in the small intestine.

[0004] The patent application with patent number CN 111227117 B mentioned that L-carnitine powder was used as raw material, water was used as a binder to granulate L-carnitine, and then a coating agent composed of ethyl cellulose, tributyl citrate, and talcum powder was used for double coating to prepare rumen-protected L-carnitine. Although the technology in this application has a certain rumen-protective effect, the yield of qualified products in the granulation process is only 77%, and the sample after two layers of coating has a rumen-passing rate of only about 47% in simulated rumen fluid for 12 hours, and a small intestinal release rate of only about 71% in simulated intestinal fluid for 12 hours, and its bioavailability is 33.3%. Therefore, it is necessary to provide a rumen-protected L-carnitine with good bioavailability, high yield, and no moisture absorption and adhesion during the preparation process and a preparation method thereof. Summary of the invention

[0005] The purpose of the present invention is to provide a rumen-protected L-carnitine with good biological utilization effect and a preparation method thereof, so as to solve the problems of moisture absorption and adhesion and low primary yield in the L-carnitine granulation process.

[0006] In order to achieve the above-mentioned invention object, the present invention adopts the following technical solutions:

[0007] On one hand, the present invention provides a rumen-protected L-carnitine, which is composed of a core material, an internal protective agent and an external coating agent, which, by mass fraction, is composed of 60-75% of the core material, 5-10% of the internal protective agent and 20-30% of the external coating agent; the core material is silicon-type L-carnitine; the internal protective agent is composed of a filler, a binder and a wetting agent; and the external coating agent is composed of a main coating material and a controlled release agent.

[0008] Preferably, in the above scheme, the internal protective agent is composed of 40-48% filler, 10-12% binder and 40-50% wetting agent by mass.

[0009] Preferably, in the above scheme, the outer coating agent is composed of 80-90% of the main coating material and 10-20% of the controlled release agent by mass.

[0010] Preferably, the content of silicon-type L-carnitine in the core material is 51%, and the remaining 49% is silicon dioxide.

[0011] Preferably, the primary coating material has an initial melting point between 60-80°C.

[0012] More preferably, the filler in the inner protective agent is sodium stearate fumarate; the binder is one or more of calcium carboxymethyl cellulose, cross-linked polyvinylpyrrolidone, sodium alginate and alginic acid; the wetting agent is water; the main coating material in the outer coating agent is one or more of hydrogenated rapeseed oil, hydrogenated soybean oil, and carnauba wax; the controlled release agent is one or more of light calcium carbonate, magnesium carbonate, and calcium sulfate.

[0013] Another aspect of the present invention provides a method for preparing rumen-protected L-carnitine, which specifically comprises the following steps:

[0014] (1) mixing silicon-based L-carnitine, a filler, and a dry powder binder to obtain a dry powder material; spraying a wetting agent onto the surface of the dry powder material while stirring and mixing, and mixing while spraying to obtain a wet powder material;

[0015] (2) granulating, shaping, drying and sieving the wet powder material through twin-screw extrusion to obtain L-carnitine internal protection particles;

[0016] (3) The main coating material is first heated and melted, and then a controlled release agent is added and mixed to obtain a suspension outer coating agent; the outer coating agent is sprayed on the surface of the L-carnitine inner protection particles for coating, and then sieved after coating to obtain a rumen-protected L-carnitine finished product.

[0017] Preferably, in step (1), the spraying speed is 30-40 L / min, and the atomization pressure is 0.2-0.3 MPa.

[0018] Preferably, in step (2), the speed of the twin-screw extruder granulator is 500-600 r / min, the feed speed is 15-20 Hz, and the cutter speed is 10-20 Hz;

[0019] The shaping time is 2-3 minutes. The drying temperature is 90-100°C and the drying time is 0.5-1h;

[0020] The mesh number of the sieving is a double-layer vibrating sieve of 10 mesh and 14 mesh, and the components in the collection sieve are L-carnitine internal protection particles.

[0021] Preferably, in step (3), the melting temperature of the coating material is 110-120°C, the coating air inlet temperature is 65-70°C, the atomization temperature is 110-120°C, the atomization pressure is 0.2-0.3Mpa, and the spraying speed is 2.0-2.5L / min;

[0022] The sieving screen has 8 mesh and 14 mesh double-layer vibrating screen, and the components in the sieve are collected to obtain the rumen-protected L-carnitine product.

[0023] The beneficial effects of the present invention are as follows:

[0024] (1) The present invention uses silicon-type L-carnitine as a raw material, and the added filler is a hydrophilic lubricant sodium stearate fumarate. The hydrophilic lubricant sodium stearate fumarate not only plays a lubricating role, but also reduces the friction and viscosity between the material and the granulator. At the same time, it can be well contacted with the wetting agent water, avoiding the phenomenon of rough surface of the particles after drying. The surface of the prepared particles becomes smooth and suitable for subsequent coating. Moreover, sodium stearate fumarate can be hydrolyzed to produce stearyl alcohol and stearic acid after entering the small intestine of ruminants, thereby being absorbed by ruminants.

[0025] (2) The adhesive of the present invention is added in the form of dry powder, mixed with the core material and the filler, and then sprayed with a wetting agent water to mix to obtain a wet powder material. The adhesive of the present invention selects one or more of calcium carboxymethyl cellulose, cross-linked polyvinylpyrrolidone, sodium alginate and algae powder that have both adhesive and disintegrating effects. It plays a bonding role in the granulation stage, and after reaching the abomasum of ruminants and the outer coating agent being acted upon by the acidic conditions in the abomasum, these substances encounter the water environment in the abomasum, absorb water and swell, and play a disintegrating role. In addition, the problem of adhesion during wet powder granulation is solved.

[0026] (3) The present invention selects a twin-screw extrusion granulation process with a cutter function for granulation. The prepared granules are cut by the cutter. By adjusting the cutter speed, the cut granules are uniform in size. After shaping, drying and screening, the finished product yield is high, reaching more than 95%.

[0027] (4) The present invention selects hydrogenated rapeseed oil, hydrogenated soybean oil and carnauba wax as the main coating materials. On the one hand, these substances can be directly melted as coating agents, and the operation is simple and fast; on the other hand, these substances have a high initial melting point, between 60-80°C, and the samples coated with these substances will not agglomerate during storage and transportation in a normal high temperature environment, and their stability is better than that of low-melting-point oil coating materials. In addition, the present invention selects acid-soluble powder auxiliary materials light calcium carbonate, magnesium carbonate, and calcium sulfate as controlled release agents. The controlled release agents are added to the melted main coating materials for mixing, and are in a suspended state to obtain a suspension coating agent, i.e., an outer coating agent. After the L-carnitine inner protection particles are coated with the outer coating agent, rumen-protected L-carnitine is obtained, which will not be destroyed in the rumen of ruminants and can pass through the rumen smoothly. When reaching the true stomach, the controlled-release agent begins to react in an acidic environment to slowly destroy the outer coating agent, and the disintegrant in the inner protection particles quickly absorbs water and swells when it meets water, thereby releasing L-carnitine, so that the L-carnitine reaches the small intestine of ruminants and exerts its effects of promoting the conversion of fat into energy and reducing fat accumulation.

[0028] (5) The present invention prepares rumen-protected L-carnitine, solves the adhesion problem caused by moisture absorption of L-carnitine raw materials during the granulation process, and solves the problem of low one-time forming rate and poor bioavailability of L-carnitine in the patent application with patent number CN 111227117 B. In addition, the rumen-protected L-carnitine prepared by the present invention has good stability. After being placed at 50° C. for 2 months under simulated 1t pressure, the L-carnitine content of the sample remains unchanged and no lumps are formed. BRIEF DESCRIPTION OF THE DRAWINGS

[0029] In order to more clearly illustrate the technical solutions in the embodiments of the present invention, the drawings required for use in the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without creative work.

[0030] Figure 1 The following is a picture of the state of the samples prepared in Example 1-3 after being placed at 50°C for 0.5 months;

[0031] Figure 2 The following are pictures of the samples prepared in Example 1-3 after being placed at 50°C for one month;

[0032] Figure 3The following is a picture of the state of the samples prepared in Examples 1-3 after being placed at 50° C. for 2 months. DETAILED DESCRIPTION

[0033] The invention provides a rumen-protected L-carnitine, which is composed of 60-75% of core material, 5-10% of internal protective agent and 20-30% of external coating agent.

[0034] The core material is 51% silicon-type L-carnitine, and the other 49% is silicon dioxide; the inner protective agent is composed of 40-48% filler, 10-12% adhesive and 40-50% wetting agent; the outer coating agent is composed of 80-90% main coating material and 10-20% controlled release agent.

[0035] The filler in the preferred internal protective agent of the present invention is sodium stearate fumarate, and sodium stearate fumarate is a hydrophilic lubricant stearic acid. The hydrophilic lubricant sodium stearate fumarate is selected to play a lubricating role, reduce the friction and viscosity between the material and the granulator, and can be well in contact with the wetting agent water, avoiding the problem that the hydrophobic lubricants calcium stearate and magnesium stearate as fillers cannot be well in contact with the wetting agent water, and are exposed to the surface of the particles after drying, and the surface of the particles prepared is rough. The surface of the particles prepared by the hydrophilic lubricant sodium stearate fumarate is smooth and more suitable for subsequent coating; in addition, sodium stearate fumarate can be hydrolyzed to produce stearyl alcohol and stearic acid after entering the small intestine of ruminants, so as to be absorbed by ruminants.

[0036] The adhesive of the present invention is added in the form of dry powder, mixed with the core material and the filler, and then sprayed with wetting agent water to mix to obtain a wet powder material. The adhesive of the present invention is preferably one or more of carboxymethylcellulose calcium, cross-linked polyvinylpyrrolidone, sodium alginate and algae powder, which have both adhesive and disintegrating effects. The adhesive plays a bonding role in the granulation stage, avoiding the problem that the adhesive is first added with water to form an adhesive aqueous solution, and then added to the granulation formula, and the mixed wet powder material becomes sticky after granulation, and the prepared granules are clumped and not formed. And when it reaches the abomasum of ruminants, after the outer coating agent is acted on by the acidic conditions in the abomasum, these substances encounter the water environment in the abomasum, absorb water and swell, and play a disintegrating role.

[0037] The preferred main coating material in the outer coating agent of the present invention is one or more of hydrogenated rapeseed oil, hydrogenated soybean oil, and carnauba wax. On the one hand, these substances can be directly melted and used as coating agents, and the operation is simple and fast; on the other hand, these substances have a high initial melting point, between 60-80°C, and the samples coated with these substances will not agglomerate during storage and transportation in a normal high temperature environment, and their stability is better than that of low melting point fat coating materials.

[0038] The present invention preferably uses acid-soluble powder auxiliary materials such as light calcium carbonate, magnesium carbonate and calcium sulfate as controlled release agents, and the controlled release agents are added into the melted main coating material for mixing, and are in a suspended state to obtain a suspension coating agent, i.e., an outer coating agent. After the L-carnitine inner protection particles are coated with the outer coating agent, rumen-protected L-carnitine is obtained, which will not be destroyed when passing through the rumen of ruminants, and can pass through the rumen smoothly. When reaching the true stomach, the controlled release agent starts to react in an acidic environment, thereby slowly destroying the outer coating agent, and the disintegrant in the inner protection particles rapidly absorbs water and swells when encountering water, thereby releasing L-carnitine, so that the L-carnitine reaches the small intestine of ruminants to play its effects of promoting fat conversion into energy and reducing fat accumulation.

[0039] The present invention preferably uses a twin-screw extrusion granulation process with a cutter function for granulation. The prepared particles are cut by the cutter. By adjusting the cutter speed, the cut particles are uniform in size. After shaping, drying and screening, the finished product yield is high, reaching more than 95%.

[0040] The preparation method of rumen protection L-carnitine of the present invention comprises the following steps: firstly mixing silicon-type L-carnitine with a filler and a dry powder adhesive, spraying water into the mixture, and then granulating the mixture using a twin-screw extruder granulator, and finally coating the mixture with a suspension coating agent formed by a main coating material and a controlled release agent.

[0041] In order to further illustrate the present invention, the technical solutions provided by the present invention are described in detail below in conjunction with embodiments, but they should not be construed as limiting the protection scope of the present invention.

[0042] The production processes, experimental methods or detection methods involved in the embodiments of the present invention, unless otherwise specified, are all conventional methods in the prior art, and their names and / or abbreviations are all conventional names in the field, and are very clear and unambiguous in the relevant application fields. Technical personnel in the field can understand the conventional process steps based on the names and apply the corresponding equipment, and implement them according to conventional conditions or the conditions recommended by the manufacturer.

[0043] The various instruments, equipment, raw materials or reagents used in the embodiments of the present invention are not particularly limited in terms of their sources, and are all conventional products that can be purchased through regular commercial channels, or can be prepared according to conventional methods well known to those skilled in the art.

[0044] Example 1

[0045] A rumen-protected L-carnitine is composed of 75% internal protection particles and 25% external coating agent. The internal protection particles are composed of 90% silicon-type L-carnitine, 8% sodium stearate fumarate and 2% carboxymethylcellulose calcium. The external coating agent is composed of 86% hydrogenated rapeseed oil and 14% light calcium carbonate. The specific preparation steps are as follows:

[0046] Weigh 450kg of silicon-type L-carnitine, 40kg of sodium stearate fumarate, and 10kg of carboxymethyl cellulose calcium and put them into a mixer for mixing. After mixing for 3 minutes, a dry powder material is obtained, and then 250kg of water is sprayed while mixing, wherein the spraying speed is 35L / min, and the atomization pressure is 0.25Mpa. After spraying, mix for 5 minutes to obtain a wet powder material. The wet mixed material enters a twin-screw extrusion granulator for granulation, and its feed rate is 18Hz, the main engine speed is 550r / min, and the cutter speed is 15Hz. After granulation, it enters a shaping machine for shaping for 2 minutes, and then enters a dryer for drying for 0.8h, wherein the drying temperature is 95°C. The dried particles are sieved through a 10-mesh and 14-mesh double-layer vibrating screen, and the components in the screen are the L-carnitine internal protection particles.

[0047] Weigh 107.5kg hydrogenated rapeseed oil and melt it in a spray tank, wherein the melting temperature is 115°C. After the hydrogenated rapeseed oil is melted, add 17.5kg light calcium carbonate and stir to obtain a suspension outer coating agent. Then weigh 375kg of the inner protection particles obtained in the above steps and place them in a fluidized bed coater for fluidization. After the state is stable, start spraying the suspension outer coating agent for coating. During the entire coating process, the inlet air temperature is 68°C, the spray speed is 2.3L / min, the atomization temperature is 115°C, and the atomization pressure is 0.25Mpa. The sample after coating is passed through an 8-mesh and 14-mesh double-layer vibrating sieve, and the components in the sieve are collected to obtain the rumen protection L-carnitine finished product.

[0048] Example 2

[0049] A rumen-protected L-carnitine is composed of 75% inner protection particles and 25% outer coating agent. The inner protection particles are composed of 90% silicon-type L-carnitine, 8% sodium stearate fumarate and 2% cross-linked polyvinylpyrrolidone. The outer coating agent is composed of 86% hydrogenated soybean oil and 14% magnesium carbonate. The specific preparation steps are as follows:

[0050] Weigh 450kg of silicon-type L-carnitine, 40kg of sodium stearate fumarate, and 10kg of cross-linked polyvinylpyrrolidone and put them into a mixer for mixing. After mixing for 3 minutes, a dry powder material is obtained, and then 250kg of water is sprayed while mixing, wherein the spraying speed is 35L / min, and the atomization pressure is 0.25Mpa. After spraying, mix for 5 minutes to obtain a wet powder material. The wet mixed material enters a twin-screw extrusion granulator for granulation, and its feed rate is 18Hz, the main engine speed is 550r / min, and the cutter speed is 15Hz. After granulation, it enters a shaping machine for shaping for 2 minutes, and then enters a dryer for drying for 0.8h, wherein the drying temperature is 95°C. The dried particles are sieved through a 10-mesh and 14-mesh double-layer vibrating screen, and the components in the screen are the L-carnitine internal protection particles.

[0051] Weigh 107.5kg of hydrogenated soybean oil and melt it in a spray tank, wherein the melting temperature is 115°C. After the hydrogenated soybean oil is melted, add 17.5kg of magnesium carbonate and stir to obtain a suspension coating agent. Then weigh 375kg of the inner protection particles obtained in the above steps and place them in a fluidized bed coater for fluidization. After the state is stable, start spraying the suspension coating agent for coating. During the entire coating process, the inlet air temperature is 68°C, the spray speed is 2.3L / min, the atomization temperature is 115°C, and the atomization pressure is 0.25Mpa. After the coating is completed, the sample is passed through an 8-mesh and 14-mesh double-layer vibrating sieve, and the components in the sieve are collected to obtain the rumen-protected L-carnitine finished product.

[0052] Example 3

[0053] A rumen-protected L-carnitine is composed of 75% inner protection particles and 25% outer coating agent. The inner protection particles are composed of 90% silicon-type L-carnitine, 8% sodium stearate fumarate, 1% sodium alginate and 1% alginic acid. The outer coating agent is composed of 86% carnauba wax and 14% calcium sulfate. The specific preparation steps are as follows:

[0054] Weigh 450kg of silicon-type L-carnitine, 40kg of sodium stearate fumarate, 5kg of sodium alginate and 5kg of alginic acid and put them into a mixer for mixing. After mixing for 3 minutes, a dry powder material is obtained, and then 250kg of water is sprayed while mixing, wherein the spraying speed is 35L / min, and the atomization pressure is 0.25Mpa. After spraying, mix for 5 minutes to obtain a wet powder material. The wet mixed material enters a twin-screw extrusion granulator for granulation, and its feed rate is 18Hz, the main engine speed is 550r / min, and the cutter speed is 15Hz. After granulation, it enters a shaping machine for shaping for 2 minutes, and then enters a dryer for drying for 0.8h, wherein the drying temperature is 95°C. The dried particles are sieved through a 10-mesh and 14-mesh double-layer vibrating screen, and the components in the screen are the L-carnitine internal protection particles.

[0055] Weigh 107.5kg of carnauba wax and melt it in a spray tank, wherein the melting temperature is 120°C. After the carnauba wax is melted, add 17.5kg of calcium sulfate and stir to obtain a suspension coating agent. Then weigh 375kg of the inner protection particles obtained in the above steps and place them in a fluidized bed coater for fluidization. After the state is stable, start spraying the suspension coating agent for coating. During the entire coating process, the inlet air temperature is 70°C, the spray rate is 2.3L / min, the atomization temperature is 120°C, and the atomization pressure is 0.25Mpa. After the coating is completed, the sample is passed through a double-layer vibrating sieve of 8 mesh and 14 mesh, and the components in the sieve are collected to obtain the rumen-protected L-carnitine finished product.

[0056] Comparative Example 1

[0057] A rumen-protected L-carnitine is composed of 75% internal protection particles and 25% external coating agent. The internal protection particles are composed of 90% silicon-type L-carnitine, 8% sodium stearate fumarate and 2% sodium carboxymethyl cellulose. The external coating agent is composed of 86% hydrogenated rapeseed oil and 14% light calcium carbonate. The specific preparation steps are as follows:

[0058] Weigh 450kg of silicon-type L-carnitine, 40kg of sodium stearate fumarate, and 10kg of sodium carboxymethyl cellulose and put them into a mixer for mixing. After mixing for 3 minutes, a dry powder material is obtained, and then 250kg of water is sprayed while mixing, wherein the spraying speed is 35L / min, and the atomization pressure is 0.25Mpa. After spraying, mix for 5 minutes to obtain a wet powder material. The wet mixed material enters a twin-screw extrusion granulator for granulation, and its feed rate is 18Hz, the main engine speed is 550r / min, and the cutter speed is 15Hz. After granulation, it enters a shaping machine for shaping for 2 minutes, and then enters a dryer for drying for 0.8h, wherein the drying temperature is 95°C. The dried particles are sieved through a 10-mesh and 14-mesh double-layer vibrating screen, and the components in the screen are the L-carnitine internal protection particles.

[0059] Weigh 107.5kg hydrogenated rapeseed oil and melt it in a spray tank, wherein the melting temperature is 115°C. After the hydrogenated rapeseed oil is melted, add 17.5kg light calcium carbonate and stir to obtain a suspension outer coating agent. Then weigh 375kg of the inner protection particles obtained in the above steps and place them in a fluidized bed coater for fluidization. After the state is stable, start spraying the suspension outer coating agent for coating. During the entire coating process, the inlet air temperature is 68°C, the spray speed is 2.3L / min, the atomization temperature is 115°C, and the atomization pressure is 0.25Mpa. The sample after coating is passed through an 8-mesh and 14-mesh double-layer vibrating sieve, and the components in the sieve are collected to obtain the rumen protection L-carnitine finished product.

[0060] Comparative Example 2

[0061] A rumen-protected L-carnitine, composed of 75% inner protection particles and 25% outer coating agent. The inner protection particles are composed of 90% silicon-type L-carnitine, 8% sodium stearate fumarate and 2% calcium carboxymethylcellulose. The outer coating agent is all hydrogenated rapeseed oil. The specific preparation steps are as follows:

[0062] Weigh 450kg of silicon-type L-carnitine, 40kg of sodium stearate fumarate, and 10kg of carboxymethyl cellulose calcium and put them into a mixer for mixing. After mixing for 3 minutes, a dry powder material is obtained, and then 250kg of water is sprayed while mixing, wherein the spraying speed is 35L / min, and the atomization pressure is 0.25Mpa. After spraying, mix for 5 minutes to obtain a wet powder material. The wet mixed material enters a twin-screw extrusion granulator for granulation, and its feed rate is 18Hz, the main engine speed is 550r / min, and the cutter speed is 15Hz. After granulation, it enters a shaping machine for shaping for 2 minutes, and then enters a dryer for drying for 0.8h, wherein the drying temperature is 95°C. The dried particles are sieved through a 10-mesh and 14-mesh double-layer vibrating screen, and the components in the screen are the L-carnitine internal protection particles.

[0063] Weigh 125kg of hydrogenated rapeseed oil and melt it in a spray tank, wherein the melting temperature is 115°C, and the hydrogenated rapeseed oil is completely melted to obtain an outer coating agent. Then weigh 375kg of the inner protection particles obtained in the above steps and place them in a fluidized bed coater for fluidization. After the state is stable, start spraying the outer coating agent for coating. During the entire coating process, the inlet air temperature is 68°C, the spray rate is 2.3L / min, the atomization temperature is 115°C, and the atomization pressure is 0.25Mpa. After the coating is completed, the sample is passed through an 8-mesh and 14-mesh double-layer vibrating sieve, and the components in the sieve are collected to obtain the rumen-protected L-carnitine finished product.

[0064] Experimental Example 1

[0065] The rumen bypass rates of Examples 1 to 3 and Comparative Examples 1 and 2 were compared using an in vitro simulated rumen environment experiment and a fistula cow experiment; the small intestinal release rates of Examples 1 to 3 and Comparative Examples 1 and 2 were compared using an in vitro simulated small intestinal environment experiment.

[0066] 1. In vitro simulated rumen environment experiment

[0067] Accurately measure 700 mL of ruminant rumen fluid in the dissolution tank of the dissolution instrument, set the temperature to 39°C and the speed to 75 r / min to simulate the rumen peristalsis environment conditions; then weigh 5.00 g of each sample of Examples 1 to 3 and Comparative Examples 1 and 2 in the dissolution tank, repeat 3 times for each sample (take the average value for calculation), collect the samples into nylon bags after 2, 4, 6, 8, 10, and 12 hours of reaction, rinse with clean water, place in a 65°C oven to dry to constant weight, weigh again, and then use high performance liquid chromatography to detect the L-carnitine content in the sample, and at the same time detect the L-carnitine content in the sample before passing the rumen, so as to calculate its rumen passing rate.

[0068] Calculation method of rumen passing rate of each sample:

[0069] X1(%)=(A2×B2 / A1×B1)×100%

[0070] Where: X1—sample rumen passing rate

[0071] A1—Weight of sample taken before passing through the rumen

[0072] B1—L-carnitine content before rumen

[0073] A2—Sample weight after rumen drying

[0074] B2—L-carnitine content after rumen

[0075] 2. Fistula Cow Experiment

[0076] Three Chinese Holstein cows equipped with permanent rumen fistulas were selected (parallel samples were used, and the average value was taken when calculating), and 300 mesh nylon cloth was used to make 8cm×16cm nylon bags. Before use, they were balanced in the rumen of the three cows for 24 hours, then taken out and cleaned, and dried in a 65°C oven to constant weight, and the weight was recorded. Then, 5.00g of each sample of Examples 1 to 3, Comparative Examples 1 and 2 was weighed at the bottom of a nylon bag of known weight (repeatedly weighed 3 times, and placed in three fistula cows respectively), and the L-carnitine content in the original particles was detected at the same time. Five nylon bags containing samples of Examples 1 to 3, Comparative Examples 1 and 2 were fixed on each plastic hose, and sent into the rumen abdominal sac chyme 2 hours after morning feeding. The plastic hose was fixed to the rumen fistula cover with a nylon line, and taken out and rinsed with tap water after 2, 4, 6, 8, 10, and 12 hours, respectively. During the rinsing process, the bag can be gently stroked by hand, and do not rub it until the water is clear. The rinsed nylon bag was placed in an oven at 65°C and dried to constant weight, then weighed and the L-carnitine content was tested.

[0077] Calculation method of rumen passing rate of each sample:

[0078] X2(%)=(A4×B4 / A3×B3)×100%

[0079] Where: X2—sample rumen passing rate

[0080] A3—Weight of sample taken before passing through the rumen

[0081] B3—L-carnitine content before rumen

[0082] A4—Sample weight after rumen drying

[0083] B4—L-carnitine content after rumen

[0084] 3. In vitro simulation of small intestine environment experiment

[0085] Take 0.500g of the samples after the rumen in the above simulated in vitro rumen environment experiment and the fistula cow experiment respectively in a 50ml culture tube, and repeat 3 times for each sample (take the average value for calculation). Add 10ml of pepsin solution (pH=2) and shake in a 38℃ shaker for 1h. Then add 14ml of trypsin solution (PH=7.8), shake in a 38℃ shaker for 2, 4, 6, 8, 10, and 12h respectively, then take it out, and then immediately add 3ml of 100% (w / v) trichloroacetic acid solution, shake and mix, let it stand for 15min, collect the sample into a nylon bag, put it in a 65℃ oven to dry to constant weight, weigh it again, and then use high performance liquid chromatography to detect the L-carnitine content, and calculate the small intestine release rate.

[0086] Y(%)=(1-C2×D2 / C1×D1)×100%

[0087] Where: Y—sample small intestine release rate

[0088] C1—sample weight before small intestine release

[0089] D1—L-carnitine content before small intestine release

[0090] C2—Weight of dried sample after small intestine release

[0091] D2—L-carnitine content after small intestine release

[0092] 3.1 The test results of rumen passage rate and small intestine release rate in simulated in vitro rumen environment are shown in the following table:

[0093]

[0094] From the experimental results, the samples of Examples 1-3 have good rumen-passing effect and high small intestinal release rate. After 12 hours of treatment in the simulated rumen environment and small intestinal environment, the rumen-passing rate is between 94-97%, the small intestinal release rate is between 92-97%, and the bioavailability is between 88-91%. It can be seen that the rumen-protected L-carnitine samples prepared by the present invention have high bioavailability.

[0095] Comparative Example 1 is based on Example 1, but the binder is changed to sodium carboxymethyl cellulose without disintegration performance. It can be seen that the small intestinal release rate of Comparative Example 1 is significantly reduced. After 12 hours of treatment, the small intestinal release rate is 78%, which is 19% points lower than that of Example 1, indicating that the binder selected by the present invention having both bonding and disintegration effects has the effect of improving the small intestinal release rate.

[0096] Comparative Example 2 is based on Example 1, but the acid-soluble excipients in the outer coating agent are removed, and hydrogenated rapeseed oil is directly used for coating. The sample of Comparative Example 2 is treated in simulated small intestinal fluid for 12 hours, and the small intestine release rate is only 58%, which is 39% lower than that of Example 1, indicating that when only the main materials are used for coating, L-carnitine will be over-protected, resulting in failure to be released in the small intestine. After adding acid-soluble excipients to the outer coating agent of the present invention, the coating agent can be reacted when the sample enters the acidic condition of the true stomach of ruminants, thereby releasing L-carnitine to exert its effect.

[0097] 3.2 The test results of rumen passing rate and small intestine release rate of fistula cattle are shown in the following table:

[0098]

[0099] From the experimental results, after the fistula cattle rumen treatment for 12 hours, the rumen passing rate of Examples 1-3 was between 90-92%, and after the simulated small intestinal fluid treatment for 12 hours, the small intestinal release rate was between 91-99%, and the overall bioavailability was between 86-90%, and the results were not much different from the simulated in vitro rumen fluid experiment, proving that the method of the present invention of treating in the laboratory simulated in vitro rumen fluid and then detecting its rumen passing rate is reliable. In addition, the results of Comparative Examples 1 and 2 are also consistent with the above.

[0100] 4. Stability experimental observation

[0101] 4.1 Experimental methods:

[0102] Simulate the stacking method of mass production products: The packaging specification of this product is 25kg / bag, the stacking height is 8 layers, 5 bags per layer, and the pressure on the bottom layer of materials is: P = F / S = mg / S = 1000×10 / 0.928 = 10776Pa. This verification is based on the same pressure on the materials. Taking 8cm×5cm partition as the force area, the required increase is F = P×S = 10776×(0.08×0.05) = 43N. One lead plate is 1.07kg, and 4 lead plates are required.

[0103] Use small ziplock bags to put 9 bags of samples from Examples 1-3 (including 3 parallel samples), put them in a 50°C oven, and place 4 lead plates on them. After 0.5 month, 1 month and 2 months, observe whether they are agglomerated and test their content.

[0104] 4.2 The experimental results are as follows:

[0105]

[0106] Note: The initial L-carnitine content in the samples of Examples 1-3 was 34.5±0.6%.

[0107] like Figure 1-3As shown, the results show that the rumen-protected L-carnitine sample prepared by the present invention has good stability: after being placed in a 50° C. oven for 2 months under simulated 1 t pressure, the content is basically unchanged and the sample does not agglomerate.

[0108] The present invention solves the adhesion problem caused by moisture absorption of L-carnitine raw materials during granulation by changing the adding mode of the binder and adding it in the form of dry powder. Carboxymethylcellulose calcium, cross-linked polyvinylpyrrolidone, sodium alginate and alginic acid having both bonding and disintegrating effects are used as binders, a twin-screw extrusion granulator is used for granulation, and light calcium carbonate, magnesium carbonate and calcium sulfate dissolved in acid as the main coating material with an initial melting point between 60 and 80° C. are used as a suspension coating agent of a controlled release agent for coating, thereby solving the problems of low one-time forming rate and low bioavailability of L-carnitine granulation in the patent application with patent number CN 111227117B. In addition, the rumen-protected L-carnitine prepared by the present invention has good stability, and the L-carnitine content of the sample remains unchanged after being placed at 50° C. for 2 months under a simulated 1t pressure, and no caking occurs.

[0109] The foregoing description of the specific exemplary embodiments of the present invention is for the purpose of explanation and illustration. Without departing from the scope of the technical solution of the present invention, the technical content disclosed above can be used to make many possible changes and modifications to the technical solution of the present invention, or modified into equivalent embodiments of equivalent changes. Therefore, any simple modification, equivalent change and modification made to the above embodiments according to the technical essence of the present invention without departing from the content of the technical solution of the present invention should still fall within the scope of protection of the technical solution of the present invention.

Claims

1. A rumen-protected L-carnitine, comprising a core material, an inner protective agent and an outer coating agent, characterized in that: According to the mass fraction, it is composed of 60-75% core material, 5-10% internal protective agent and 20-30% external coating agent; the core material is silicon-type L-carnitine; the internal protective agent is composed of filler, adhesive and wetting agent; the external coating agent is composed of main coating material and controlled release agent.

2. The rumen-protected L-carnitine according to claim 1, characterized in that: Calculated by mass, the internal protective agent consists of 40-48% filler, 10-12% binder and 40-50% wetting agent.

3. The rumen-protected L-carnitine according to claim 1, characterized in that: By mass fraction, the outer coating agent consists of 80-90% of a main coating material and 10-20% of a controlled release agent.

4. The rumen-protected L-carnitine according to claim 1, characterized in that: The content of silicon-type L-carnitine in the core material is 51%, and the other 49% is silicon dioxide.

5. The rumen-protected L-carnitine according to claim 1, characterized in that: The initial melting point of the main coating material is between 60-80°C.

6. The rumen-protected L-carnitine according to claim 1, characterized in that: The filler in the inner protective agent is sodium stearate fumarate; the binder is one or more of calcium carboxymethyl cellulose, cross-linked polyvinylpyrrolidone, sodium alginate and alginic acid; the wetting agent is water; the main coating material in the outer coating agent is one or more of hydrogenated rapeseed oil, hydrogenated soybean oil and carnauba wax; the controlled release agent is one or more of light calcium carbonate, magnesium carbonate and calcium sulfate.

7. A method for preparing rumen-protected L-carnitine, characterized in that: The specific steps include: (1) mixing silicon-based L-carnitine, a filler, and a dry powder binder to obtain a dry powder material; spraying a wetting agent onto the surface of the dry powder material while stirring and mixing, and mixing while spraying to obtain a wet powder material; (2) granulating, shaping, drying and sieving the wet powder material through twin-screw extrusion to obtain L-carnitine internal protection particles; (3) The main coating material is first heated and melted, and then a controlled release agent is added and mixed to obtain a suspension outer coating agent; the outer coating agent is sprayed on the surface of the L-carnitine inner protection particles for coating, and then sieved after coating to obtain a rumen-protected L-carnitine finished product.

8. The method for preparing rumen-protected L-carnitine according to claim 7, characterized in that: The spraying speed of the spray in the step (1) is 30-40 L / min, and the atomization pressure is 0.2-0.3 MPa.

9. The method for preparing rumen-protected L-carnitine according to claim 7, characterized in that: In the step (2), the main engine speed of the twin-screw extruder is 500-600r / min, the feed speed is 15-20Hz, and the cutter speed is 10-20Hz; the shaping time is 2-3min. The drying temperature is 90-100°C, and the drying time is 0.5-1h; the sieving mesh is a double-layer vibrating screen with 10 mesh and 14 mesh, and the components in the collection screen are L-carnitine internal protection particles.

10. The method for preparing rumen-protected L-carnitine according to claim 7, characterized in that: In the step (3), the melting temperature of the coating material is 110-120° C., the coating air inlet temperature is 65-70° C., the atomization temperature is 110-120° C., the atomization pressure is 0.2-0.3 MPa, and the spraying speed is 2.0-2.5 L / min; the sieve mesh number is 8 mesh and 14 mesh double-layer vibrating sieve, and the components in the sieve are collected to obtain the rumen-protected L-carnitine finished product.