Manufacturing method of paper food container and manufacturing mold of paper food container

By using hot pressing to form an airtight film layer in part of the paper food container, the airtightness and environmental protection problems of traditional disposable food containers are solved, and a low-cost and efficient production process is achieved.

CN118927711AActive Publication Date: 2024-11-12SABERT ZHONGSHAN LTD

Patent Information

Application Number
CN202411382864.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-30
Publication Date
2024-11-12
Estimated Expiration
2044-09-30

AI Technical Summary

Technical Problem

Traditional disposable food containers have poor airtightness and high production costs due to the airtight film made of plastic, and do not meet environmental protection requirements.

Method used

The hot pressing method is used to form an airtight film layer in part of the paper food container, reducing the weight and area of ​​the airtight film layer, and avoiding the use of vacuum equipment and heating processes through mold design.

Benefits of technology

It improves the airtightness of food containers, reduces production costs and energy consumption, meets environmental protection requirements, and simplifies the production process.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118927711A_ABST
    Figure CN118927711A_ABST
Patent Text Reader

Abstract

The invention provides a manufacturing method of a paper food container and a manufacturing mould of the paper food container, the method comprises the steps that paper is folded to form a container body of the food container, the upper end of the container body is open, the container body is provided with a bottom wall and a peripheral wall adjacent to the bottom wall, and at least one seam line is formed on the bottom wall or the peripheral wall; the seam line is positioned at a seam formed by overlapping at least two layers of sheet-shaped paper materials; then, the container body is placed on a lower die, an airtight film is placed above the lower die, and the airtight film is located above a part of the area of the container body; the upper die is driven to move downwards, so that the airtight film is clamped between the upper die and the container body, and the upper die is heated, so that the airtight film is tightly attached to a part of area of the bottom wall and / or the peripheral wall of the container body, and an airtight film layer is formed. The mold is applied to the manufacturing method for manufacturing the paper food container. The paper food container manufactured through the method is low in plastic content, air tightness is guaranteed, and meanwhile the requirement for environmental protection is met.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of disposable tableware manufacturing, in particular to a method for manufacturing a paper food container made of paper and a mold used in the method. Background Art

[0002] Traditional disposable food containers are mostly made of plastic. Since plastic food containers are not easy to degrade and cause plastic pollution, disposable food containers made of environmentally friendly materials such as paper are becoming more and more popular.

[0003] Usually, disposable food containers made of paper are made by folding a flat piece of kraft paper or cardboard, where a seam line is formed and an airflow channel is formed. The gas inside the food container can leak to the outside through the seam, and the external gas can also flow into the inside of the food container through the seam, which results in poor airtightness of the food container.

[0004] In order to solve the airtightness problem of food containers, it is usually necessary to cover the surface of the food container with an airtight film layer. A multi-layer composite film is used. A film layer with a very small thickness is made of PP, PE, PET, PA, EVOH and other materials. The airtight film layer is attached to the inner surface of the food container by traditional vacuum forming, especially at the seams. The seams are sealed by the airtight film layer to reduce the gas flow inside and outside the food container.

[0005] However, since the airtight film layer is made of materials such as PP, PE, PET, PA, EVOH, etc., and not made of environmentally friendly materials such as paper, if the thickness of the airtight film layer is large, the plastic content of the food container will be high. For example, the weight of the airtight film layer accounts for more than 20% of the total weight of the food container, which does not meet the requirements of environmental protection. For example, according to EU legal requirements, if the proportion of plastic in a food container exceeds 10%, the user needs to tear off the airtight film layer made of plastic from the food container when discarding the food container, and the airtight film layer and the container body made of paper need to be recycled separately. Obviously, if the weight of the airtight film layer is large, it will not only fail to meet the requirements of environmental protection, but will also bring great inconvenience to the user.

[0006] In addition, before the airtight film layer is attached to the inner surface of the food container by the traditional vacuum forming method, a whole piece of plastic film with a large area, a large thickness (usually more than 0.02 mm) and a certain hardness needs to be heated and softened, and then the softened plastic film is spread on the food container, and finally the softened plastic film is attached to the food container by vacuum forming. However, the above process consumes more energy and takes a long time to heat the plastic film, which increases the production time of the food container and leads to a higher production cost of the food container.

[0007] In addition, when using the traditional blister method to form a plastic film on a food container, a blister equipment is required. The blister equipment usually includes a lower mold and an upper mold. The food container to be coated is placed on the lower mold. During blister forming, the plastic film needs to be adsorbed onto the food container by vacuuming the lower mold, and the softened plastic film is attached to the inner wall of the food container by heating. Therefore, this blister production equipment needs to be equipped with a vacuum device, and the blister production equipment has many parts and components, and the production cost of the blister production equipment is high. Summary of the invention

[0008] The first object of the present invention is to provide a method for making a paper food container with low production cost, low energy consumption and short production time.

[0009] A second object of the present invention is to provide a mold for producing a food container having good sealing performance and low specific gravity of plastic.

[0010] To achieve the first objective of the present invention, the present invention provides a method for making a paper food container, comprising folding a paper to form a container body of the food container, wherein the upper end of the container body is open, and the container body has a bottom wall and a peripheral wall adjacent to the bottom wall, and at least one seam line is formed on the bottom wall or the peripheral wall, and the seam line is located at the seam formed by overlapping at least two layers of sheet paper, and the outer end of the seam line forms an edge seam position; then, the container body is placed on a lower mold, and an airtight film is placed above the lower mold, and the airtight film is located above a portion of the container body; the upper mold is driven to move downward so that the airtight film is clamped between the upper mold and the container body, and the upper mold is heated so that the airtight film is tightly attached to a portion of the bottom wall and / or the peripheral wall of the container body and forms an airtight film layer, and all edge seams are covered with the airtight film layer, and at least a portion of the bottom wall and / or the peripheral wall is not covered with the airtight film layer.

[0011] As can be seen from the above scheme, when making a food container, the container body is placed behind the lower mold and covered with an airtight film, and the upper mold adheres the airtight film to a part of the inner wall of the container body by hot pressing. Since the airtight film layer is not formed by blistering, it is not necessary to heat the airtight film, and the airtight film with a softer texture can be directly laid on the container body. The production time of the food container is short and the energy consumption is also low.

[0012] The food container made by the above method can prevent air leakage at the edge seams of the food container because the edge seams are sealed by the airtight film layer, thereby effectively improving the airtightness of the food container. In addition, since the bottom wall and / or the peripheral wall of the food container are not covered with the airtight film layer in all areas, that is, the airtight film layer only covers a part of the bottom wall and / or the peripheral wall, and covers all the edge seams, the coverage area of ​​the airtight film layer on the food container is small, especially for the case where the bottom wall is relatively flat, the area of ​​the bottom wall covered by the airtight film layer is small, thereby reducing the weight of the airtight film layer, so that the weight of the airtight film layer accounts for a smaller proportion of the total weight of the entire food container, meeting the requirements of environmental protection performance, and the user does not need to tear off the airtight film layer after use, which is convenient for the user.

[0013] A preferred solution is that the number of airtight films placed above the lower mold is more than two, and each airtight film covers a portion of the edge seam.

[0014] It can be seen that the airtight film layer formed on the food container is not formed by a whole piece of airtight film, but is formed by multiple pieces of airtight film respectively covering a part of the area of ​​the food container. In this way, the inner wall of the food container is not entirely covered with the airtight film layer, thereby ensuring that a part of the area is not necessarily covered by the airtight film layer, thereby reducing the proportion of plastic in the food container.

[0015] A further solution is that the airtight film has a fitting portion and a clamping portion, a fracture portion is formed between the fitting portion and the clamping portion, and the fracture portion has discontinuously distributed fracture through holes.

[0016] It can be seen that a breaking portion is provided on the airtight film, and when the upper mold moves downward, the airtight film will be broken along the breaking portion and adhered to the inner wall of the food container under the action of the upper mold, making the processing of the food container very convenient.

[0017] A further solution is that when the airtight film is placed above the lower mold, a tensioning member is used to tension the two ends of the clamping portion so that the fitting portion is located above the container body.

[0018] It can be seen that by tensioning the airtight film through the tensioning member, it can be ensured that the airtight film is located at a specified position during the production process, thereby achieving positioning between the airtight film and the food container and improving the qualified rate of the food container.

[0019] A further solution is that the tensioning member includes a winding device for winding the airtight film; or the tensioning member includes a clamping member for clamping the airtight film.

[0020] It can be seen that the winding device can realize the discharge and collection of the airtight film and realize automated production.

[0021] To achieve the second purpose of the present invention, the present invention provides a mold for making a paper food container, comprising a lower mold, the upper end of which is open, the lower mold forming a mold cavity, and the container body formed by folding paper to form the food container can be placed in the mold cavity; an upper mold is arranged above the lower mold, and the upper mold moves in a direction toward or away from the lower mold; and the upper mold is provided with a substrate, the substrate is formed with at least one protrusion toward the lower mold, the protrusion extends into the mold cavity of the lower mold, and an airtight film is clamped between the protrusion and the container body, and after the upper mold is heated, the airtight film is tightly attached to a part of the bottom wall and / or the peripheral wall of the container body and forms an airtight film layer, and at least a part of the bottom wall and / or the peripheral wall is not covered with the airtight film layer.

[0022] It can be seen from the above scheme that when the above mold is used to make a food container, the airtight film layer of the food container is formed on the inner wall of the container body by hot pressing. Since there is no need for blister processing, the production equipment does not need to be equipped with a vacuum device, and there is no need to heat and soften the airtight film before blister processing. Therefore, the production time of the food container is short and the energy consumption is low. Since the entire bottom wall and the surrounding wall of the produced food container are not covered with an airtight film layer, the proportion of plastic is low, and the food container does not need to tear off the airtight film layer and then discard it after use.

[0023] A preferred solution is that the number of the bumps is more than two, and there is a gap between two adjacent bumps.

[0024] It can be seen that the food container does not form an airtight film layer in the gap between two adjacent protrusions. On the one hand, it can reduce the volume of the protrusion, reduce the material used in the lower mold, and reduce the production cost of the mold. On the other hand, the area of ​​the airtight film layer of the manufactured food container is small, and the proportion of plastic is low, which meets the requirements of environmental protection.

[0025] A further solution is that a step portion is provided at the lower end of the bump, and in the normal direction of the substrate, an upper end surface of the step portion is higher than a lower end surface of the bump.

[0026] It can be seen that the shape of the protrusion can be flexibly set according to the shape of the food container, which can ensure that the airtight film layer can fit tightly to the inner wall of the food container.

[0027] A further solution is that the lower mold has a flange support portion located at the periphery of the mold cavity, and the base plate of the upper mold can press the flange portion of the container body onto the flange support portion.

[0028] In this way, the airtight film is placed on the flanged portion of the food container, and after hot pressing, the flanged portion of the food container is also covered with the airtight film layer, which can improve the deformation resistance of the food container.

[0029] A further solution is that a heating device is provided in the upper mold and / or the lower mold. Since the upper mold and / or the lower mold need to be heated when the airtight film layer is hot-pressed on the container body, the heating device is directly provided in the upper mold and / or the lower mold. On the one hand, the heating efficiency of the upper mold and / or the lower mold can be improved, so that the upper mold can be heated quickly. On the other hand, it avoids providing a heating device outside the mold and occupying a large volume, which is conducive to the miniaturization of the production equipment. BRIEF DESCRIPTION OF THE DRAWINGS

[0030] Figure 1 It is a structural diagram of a food container manufactured by applying the manufacturing method of a paper food container of the present invention from a first perspective.

[0031] Figure 2 It is a structural diagram of a food container manufactured by applying the manufacturing method embodiment of a paper food container of the present invention from a second viewing angle.

[0032] Figure 3 The invention is a structural diagram of the unfolded kraft paper in an embodiment of a method for making a paper food container.

[0033] Figure 4 yes Figure 3 A partial enlarged view of .

[0034] Figure 5 It is a structural diagram of a food container manufactured by applying the manufacturing method of a paper food container of the present invention from a third perspective.

[0035] Figure 6 It is a structural diagram of a food container manufactured by applying the manufacturing method of a paper food container of the present invention at a fourth viewing angle.

[0036] Figure 7 It is a cross-sectional view of a food container manufactured by applying the manufacturing method of a paper food container of the present invention.

[0037] Figure 8 It is a structural diagram of a manufacturing mold embodiment of a paper food container of the present invention and an airtight film from a first perspective.

[0038] Fig. 9 It is a structural diagram of a second viewing angle of a mold embodiment of a paper food container of the present invention and an airtight film.

[0039] Fig.10 It is a structural diagram of a lower mold in an embodiment of a mold for making a paper food container of the present invention.

[0040] Fig.11 It is a structural diagram of the upper mold from the first perspective in an embodiment of a mold for making a paper food container of the present invention.

[0041] Fig.12 It is a structural diagram of the upper mold from a second viewing angle in an embodiment of a mold for making a paper food container of the present invention.

[0042] The present invention is further described below in conjunction with the accompanying drawings and embodiments. DETAILED DESCRIPTION

[0043] The method for making a paper food container of the present invention first uses environmentally friendly materials such as paper to make a container body of the food container, and then forms an airtight film layer on the container body by heat pressing. The airtight film layer does not cover the entire inner wall of the food container, but only covers a part of the area, thereby reducing the weight of the airtight film layer in the total weight of the entire food container.

[0044] See also Figure 1 and Figure 2 The food container 10 manufactured by the method for manufacturing a paper food container of the present invention comprises a container body 11. The container body 11 is formed by folding a piece of kraft paper. The shape of the kraft paper before folding is as follows: Figure 3 The container body 11 has a flat bottom wall 12, and a peripheral wall is formed on the bottom wall 12. In this embodiment, the container body 11 has eight peripheral walls, such as Figure 1 As shown in the clockwise direction, the peripheral walls 21, 22, 23, 24, 25, 26, 27, 28 are included in sequence, wherein the peripheral wall 21 is adjacent to the peripheral walls 22 and 28, the peripheral wall 22 is adjacent to the peripheral walls 21 and 23, and so on. Moreover, the lower edge of each peripheral wall 21, 22, 23, 24, 25, 26, 27, 28 is adjacent to the bottom wall 12.

[0045] The container body 11 is a container with an open top, that is, the end of the container body 11 away from the bottom wall 12 is open, and no sealing component is provided. When in use, the user puts food into the container body, and then uses a sealing film or the like to seal the open end of the container body 11. When the user needs to take out the food, the sealing film or the like needs to be torn off from the open end of the container body 11 first.

[0046] See also Figure 3The container body 11 is formed by folding a whole piece of kraft paper. Preferably, a layer of waterproof coating is coated on the surface of the kraft paper itself, for example, a plant fiber waterproof coating is coated on one surface of the kraft paper. These waterproof coatings make the kraft paper itself have certain waterproof properties.

[0047] A plurality of folding marks are arranged on the kraft paper, for example, a folding mark 401 is arranged, and the folding mark 401 is located between the bottom wall 12 and the peripheral wall 21. After the kraft paper is folded along the folding mark 401, the bottom wall 12 and the peripheral wall 21 of the container body 11 are formed. Similarly, the peripheral wall 22 of the container body can be formed by folding along the folding mark 402, and the peripheral wall 23 of the container body 11 can be formed by folding along the folding mark 403. It can be seen that since the bottom wall 12 of the container body 11 and each peripheral wall 21, 22, 23, 24, 25, 26, 27, 28 are formed by folding, no seam line is formed between the bottom wall 12 and each peripheral wall 21, 22, 23, 24, 25, 26, 27, 28, and no seam line is formed on the bottom wall 12 itself, so the bottom wall 12 itself has good sealing performance.

[0048] A folding portion is formed at one corner of the kraft paper 40, and the folding portion includes a sheet 41. The sheet 41 forms the peripheral wall 26 of the container body 11 after being folded. In addition, folding pieces 42 and 44 are respectively provided on both sides of the sheet 41, and a sheet 43 is further provided on one side of the folding piece 42. The sheet 43 forms the peripheral wall 27 after being folded. When the kraft paper 40 is folded, the folding piece 42 will be folded between the sheet 41 and the sheet 43, that is, on the container body 11 after being folded, and the folding piece 42 will be clamped between the sheet 41 and the sheet 43, as shown in FIG. Figure 5 shown.

[0049] In this way, a seam is formed at the connection between the sheet body 41 and the folded sheet 42, such as Figure 6 As shown, a seam line 31 is formed between the peripheral wall 26 and the peripheral wall 27. The seam line 31 is a gap formed by folding the sheet body 41 and the folding sheet 42, that is, a seam line is formed where two or more sheets of paper material overlap. The seam line 31 extends from the bottom wall 12 to the upper edge of the peripheral wall 27, see Figure 4, an opening 49 is formed between the sheet 43 and the adjacent sheet 48. Therefore, the position of the seam line 31 close to the opening 49 is a position that is prone to air leakage. This position is the outer edge end of the seam line 31, that is, the position close to the edge of the sheet paper material, which is called the edge seam position. Due to the existence of the edge seam position, the air inside the container body 11 can pass through the edge seam position and communicate with the outside air. Correspondingly, a seam line 32 is also formed between the peripheral wall 25 and the peripheral wall 26. In this embodiment, all seams are formed on the peripheral wall, no seams are formed on the bottom wall 12, and no seams are formed between each peripheral wall and the bottom wall.

[0050] Since air flow will be formed inside and outside the container body 11 at the edge seams, for this reason, the present embodiment needs to cover the container body 11 with an airtight film layer, and all edge seams are covered by the airtight film layer to ensure the sealing of the food container 10. In the present embodiment, the airtight film layer is a thin film covering a local area on the bottom wall 12 and / or the peripheral wall, for example, the film is a plastic film or a degradable film made of materials such as PP, PE, PET, PA or EVOH, wherein the degradable film can be PLA, PBS, PVOH or PCL, etc., and the airtight film layer should use a food-grade film to meet the requirements of food safety.

[0051] like Figure 2 As shown, the airtight film layers 60 and 62 are only adsorbed on a part of the bottom wall 12, such as the two ends along the length direction of the bottom wall 12. Therefore, one end of the airtight film layer 60 extends to the fold mark between the bottom wall 12 and the peripheral wall 27, and the other end of the airtight film layer 60 forms an edge 61 on the bottom wall 12. Correspondingly, one end of the airtight film layer 62 extends to the fold mark between the bottom wall 12 and the peripheral wall 23, and the other end of the airtight film layer 62 forms an edge 63 on the bottom wall 12. The area between the edge 61 and the edge 63 is not covered by the airtight film layer, that is, the area between the edge 61 and the edge 63 of the bottom wall 12 is not covered by the airtight film layer.

[0052] In this way, the airtight film layer does not cover the entire bottom wall 12, but only covers a part of the area. Preferably, the area of ​​the bottom wall 12 covered with the airtight film layer does not exceed 50% of the area of ​​the bottom wall 12, and further, the area of ​​the bottom wall 12 covered with the airtight film layer does not exceed 10% of the area of ​​the bottom wall 12. Since there is no seam line or edge seam on the bottom wall 12, and the kraft paper 40 itself has good airtightness, even if there is a large area on the bottom wall 12 that is not covered by the airtight film layer, it will not affect the overall sealing performance of the food container 10.

[0053] Since all edge seams are formed on the peripheral wall, in this embodiment, the airtight film layer will cover all the peripheral walls, thereby ensuring that all edge seams will be covered by the airtight film layer, and utilizing the good sealing performance of the airtight film layer to avoid air leakage inside and outside the food container 10, thereby ensuring the sealing performance of the food container 10. Preferably, the weight of the airtight film layer accounts for less than 12% of the total weight of the food container 10, and further, the weight of the airtight film layer accounts for less than 5% of the total weight of the food container 10. In this way, the weight of the airtight film layer is very small, which can meet the requirements of environmental protection on the one hand, and on the other hand, after the food container 10 is used, the user does not need to tear off the airtight film layer and then discard the food container 10, which can facilitate the use of the user.

[0054] In other embodiments, the airtight film layer may only cover a portion of the peripheral wall, rather than covering all of the peripheral wall, which can further reduce the area of ​​the airtight film layer and reduce the weight of the airtight film layer. Of course, in order to ensure that the airtight film layer can effectively seal all edge seams, a certain distance needs to be maintained between the edge of the airtight film layer and the edge seam, for example, the distance between the edge of the airtight film layer and the edge seam is not less than 5 mm.

[0055] During the use of the food container 10, the user often holds the peripheral wall. Since the peripheral wall made of paper is soft in texture, it is easy for the peripheral wall to be severely deformed when the user holds the peripheral wall. If the user holds with great force, the peripheral wall may be damaged and the entire food container 10 may be damaged, affecting the use of the food container 10.

[0056] In order to improve the strength of the peripheral wall, a flange portion 51 is provided on the upper edge of the peripheral wall. Figure 7 The flange portion 51 is formed at a position of the peripheral wall 27 close to the open end, that is, at the upper edge of the peripheral wall 27 away from the bottom wall 12. The flange portion 51 extends from the upper edge of the peripheral wall 27 in a radially outward direction of the food container 10, that is, it is flanged outward. Figure 3 A flange piece 46 is provided at one end of the sheet body 43 away from the bottom wall 12 , and a folding mark 406 is provided between the flange piece 46 and the sheet body 43 . After the flange piece 46 and the sheet body 43 are folded along the folding mark 406 , the flange piece 46 will form a flange portion 51 .

[0057] In this embodiment, the upper edge of each peripheral wall is connected with a flange portion, so the flange portion surrounds the upper edge of the entire peripheral wall, that is, the flange portion is arranged around the open end of the food container 10. Further, the flange portion is also covered with an airtight film layer, preferably, the airtight film layer is formed on the flange portion by hot pressing, so that the hardness of the flange portion is enhanced by the hot pressed airtight film layer, thereby enhancing the strength of the peripheral wall, and the peripheral wall is not easily collapsed or damaged when the user holds the peripheral wall.

[0058] In addition, a folding portion 52 is also provided at the free end of the flange portion 51. Figure 7 As shown, one end of the folded edge portion 52 is connected to the flange portion 51, and the free end of the folded edge portion 52 extends toward the bottom wall 12. In this embodiment, the folded edge portion 52 extends in a direction substantially perpendicular to the bottom wall 12. Figure 3 An overhanging piece 47 is provided at one end of the flange piece 46 away from the sheet body 43 , and a folding mark 407 is provided between the flange piece 46 and the overhanging piece 47 . After the overhanging piece 47 and the flange piece 46 are folded along the folding mark 407 , the overhanging piece 47 will form a folded edge portion 52 .

[0059] In addition, the folded edge portion 52 may also be covered with an airtight film layer. Preferably, the airtight film layer is formed on the folded edge portion 52 by hot pressing. The method of forming the airtight film layer by hot pressing can improve the strength of the folded edge portion 52, and then increase the ability of the flange portion 52 to resist deformation. Since the flange portion 52 is connected to the upper edge of the peripheral wall 27, this design can further improve the strength of the peripheral wall 27. Even if the user holds the peripheral wall 27, it is not easy to cause the peripheral wall to collapse, so that the food container 10 can maintain its original shape.

[0060] When making a food container, firstly, the container body 11 of the food container needs to be made. First, a whole sheet of kraft paper is folded, for example, cut into Figure 3 The kraft paper shown in the figure may be coated with a waterproof coating on its surface. Then, the container body 11 is folded to form the container body 11. It should be noted that the folded container body 11 does not have a flange and a folded edge. The flange and the folded edge are folded after the airtight film layer is hot-pressed. Next, the container body 11 is placed in a mold, and an airtight film layer is formed on the container body 11 by hot pressing through the mold.

[0061] See also Figure 8 and Fig. 9 The mold includes an upper mold 60 and a lower mold 80. The upper mold 60 can move up and down relative to the lower mold 80, that is, the upper mold 60 can be close to the lower mold 80 or away from the lower mold 80. When the upper mold 60 moves upward, a gap is formed between the upper mold 60 and the lower mold 80 to facilitate the placement of the container body 11 into the lower mold 80, or to take the food container with the airtight film layer hot-pressed from the lower mold 80. In addition, airtight films 91 and 92 are also placed between the upper mold 60 and the lower mold 80.

[0062] See also Fig.10The lower mold 80 has a mold cavity 81, and the shape of the mold cavity 81 is the same as the outer contour of the container body 11. Therefore, when the container body 11 is placed in the mold cavity 81, the outer surface of the container body 11 can be attached to the inner surface of the mold cavity 81. In addition, the lower mold 80 is also provided with a flange support portion 83, which surrounds the mold cavity 81. When the container body 11 is placed in the mold cavity 81, the flange portion 52 of the food container is located on the flange support portion 83.

[0063] See also Fig.11 and Fig.12 The upper mold 60 has a base plate 61, and two protrusions 62 and 63 are arranged at the lower end of the base plate 61, that is, in the direction toward the lower mold 80, and there is a gap 84 between the two protrusions 62 and 63. When the upper mold 60 moves downward, the two protrusions 62 and 63 can extend into the mold cavity 81 of the lower mold 80. In addition, the shape of each protrusion 62 and 63 at both ends of the length direction and the width direction of the upper mold 60 matches the shape of the mold cavity 81, but a small gap is formed between each protrusion 62 and 63 and the mold cavity 81, and the gap is used to accommodate the container body 11 and the airtight films 91 and 92.

[0064] According to the shape of the food container to be manufactured, a step portion 71 is provided at the lower end of each protrusion 62, 63, and in the normal direction of the substrate 61, the upper end surface 72 of the step portion 71 is higher than the lower end surface 70 of the protrusions 62, 63, wherein the lower end surface 70 of the protrusions 62, 63 is the end surface of the protrusions 62, 63 closest to the bottom wall of the mold cavity 81. Preferably, the shape of the step portion 71 is completely matched with the shape of the bottom wall of the container body 11, and the provision of the step portion 71 enables the airtight films 91, 92 to be pressed by the step portion 71 and closely fit to the bottom wall of the container body 11, thereby avoiding the formation of a gap between the airtight film layer and the bottom wall of the container body 11.

[0065] After the container body 11 is placed in the mold cavity 81 of the lower mold 80, the peripheral wall and the bottom wall of the container body 11 are attached to the inner surface of the mold cavity 81, and then two airtight films 91 and 92 are placed above the lower mold 81. Figure 8 As shown. Since the container body 11 has also been placed in the mold cavity 81, the two airtight films 91, 92 are also located above the container body 11. Preferably, there is a gap between the two airtight films 91, 92, so the two airtight films 91, 92 do not completely cover the entire container body 11. Since the airtight films 91, 92 are formed on the peripheral wall and bottom wall of the container body 11 by heat pressing and form an airtight film layer, each airtight film needs to cover a portion of the edge seam positions on a portion of the container body 11. In addition, the two airtight films 91, 92 need to cover all edge seams on the container body 11 to ensure that the formed airtight film layer can cover all edge seams of the food container.

[0066] Taking the airtight film 91 as an example, the airtight film 91 has a fitting portion 94 and a clamping portion 93, and a breaking portion 95 is formed between the fitting portion 94 and the clamping portion 93. The breaking portion 95 has discontinuously distributed breaking through holes, for example, the breaking portion 95 includes a plurality of strip-shaped through holes, which can be circular through holes or long strip-shaped through holes. The two ends of the clamping portion 93 are tensioned by tensioning members, so that before the upper mold 60 moves downward, the airtight film 91 always maintains a tensioned state, that is, maintains a state as shown in FIG. Figure 8 The position of the airtight film 91 can be adjusted by the tensioning member, so that the airtight film 91 can be accurately located above the container body 11, thereby ensuring that the airtight film layer after hot pressing is just attached to the specified position of the container body 11.

[0067] Preferably, the tensioning member includes a winding device, and the two ends of the airtight film 91 are wound by the winding device. For example, the airtight film 91 is a long strip of film, and the film is wound by the winding device. When in use, the winding device is used to discharge and reel in the material, thereby realizing automated production. In other embodiments, the tensioning member may also include a clamping member, which is clamped at both ends of the length direction of the airtight film 91. The shape of the airtight film 92 is the same as that of the airtight film 91, and will not be repeated.

[0068] After the airtight films 91 and 92 are placed above the container body 11, the upper mold 60 is driven to move downward. Preferably, the upper mold 60 is driven by a driving mechanism such as a cylinder or a motor. When the protrusions 62 and 63 of the upper mold 60 abut against the airtight films 91 and 92, under the pressure of the upper 62 and 63, the airtight films 91 and 92 will be broken along the breaking portion 95, so that the fitting portion 94 is clamped between the protrusions 62 and 63 and the inner wall of the container body 11, and the clamping portion 93 is still tensioned by the tensioning member.

[0069] Preferably, the airtight films 91 and 92 should cover the flange and folded edge of the container body 11 in addition to the peripheral wall and the bottom wall of the container body 11, so that both the flange and the folded edge are covered with an airtight film layer. To this end, when the upper mold 60 moves downward, the base plate 61 of the upper mold 60 needs to press the flange of the container body 11 onto the flange support portion 83, so that the fitting portion 94 also covers the corresponding area of ​​the flange and the folded edge.

[0070] Then, the upper mold 60 starts to heat. Preferably, a heating device is provided in at least one of the upper mold 60 or the lower mold 80. Furthermore, heating wires are provided in the two protrusions 62 and 63, respectively. The heating temperature and heating time of the upper mold 60 can be determined according to factors such as the material of the container body 11, the material of the airtight films 91 and 92, the thickness of the airtight films 91 and 92, and the area of ​​the fitting portion 94. After being heated by the upper mold 60, the fitting portion 94 will be tightly fitted on the peripheral wall, bottom wall, flanged portion and folded edge portion of the container body 11, thereby forming an airtight film layer on the peripheral wall, bottom wall, flanged portion and folded edge portion of the container body 11. After being heated for a period of time, the upper mold 60 will move upward so as to remove the semi-finished food container covered with the airtight film layer from the lower mold 80.

[0071] Then, the semi-finished food container covered with the airtight film layer is moved to the next station, and the semi-finished food container covered with the airtight film layer is pressed using a mold for making the flanged portion and the folded edge portion, so as to form the flanged portion and the folded edge portion at the upper edge of the peripheral wall. At this point, the food container is completed. Since the airtight film layer has a certain toughness, the airtight film layer will not be damaged when the flanged portion and the folded edge portion are made. In addition, since the airtight film layer is covered in advance in the areas corresponding to the flanged portion and the folded edge portion, the produced flanged portion and the folded edge portion are both covered with the airtight film layer.

[0072] The food container manufactured by the method of the present invention forms an airtight film layer on a local area of ​​the bottom wall and / or the peripheral wall, rather than forming the airtight film layer on the entire bottom wall and / or the peripheral wall, thereby reducing the area of ​​the airtight film layer and thereby reducing the weight of the airtight film layer relative to the weight of the entire food container. On the one hand, the amount of the airtight film layer can be reduced, making the food container more environmentally friendly. On the other hand, while meeting the requirements of environmental protection performance and recycling and reuse, it avoids the inconvenience caused to users by the need to tear off the airtight film layer after using the food container.

[0073] In addition, the manufacturing process of the food container is not achieved by the blister forming method, but by the hot pressing process, which does not require the use of vacuum equipment, thereby reducing the production equipment. Moreover, since the airtight film is attached to the container body by the hot pressing process, this process does not require the thickness of the airtight film, and will not cause the airtight film to be damaged during vacuuming due to the thickness of the airtight film being too small. Therefore, an airtight film with a very small thickness can be used to form an airtight film layer, which can effectively reduce the proportion of plastic in the food container. In addition, in the process of making the food container, the airtight film should not be heated to soften it, and there is no waiting time for heating and softening the airtight film, which can improve the production efficiency of the food container and reduce the energy consumed in the production process of the food container.

[0074] Finally, it should be emphasized that the above are only preferred embodiments of the present invention and are not intended to limit the present invention. For those skilled in the art, the present invention may have various changes and modifications. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention should be included in the scope of protection of the present invention.

Claims

1. A method for making a paper food container, comprising: A container body of a food container is formed by folding paper, wherein the upper end of the container body is open, and the container body has a bottom wall and a peripheral wall adjacent to the bottom wall, at least one seam line is formed on the bottom wall or the peripheral wall, the seam line is located at a seam formed by overlapping at least two layers of sheet paper, and the outer end of the seam line forms an edge seam position; Features: Placing the container body on a lower mold, placing an airtight film on the lower mold, wherein the airtight film is located above a portion of the container body; The upper mold is driven to move downward so that the airtight film is clamped between the upper mold and the container body, and the upper mold is heated so that the airtight film is tightly attached to a part of the bottom wall and / or the peripheral wall of the container body and forms an airtight film layer, and all the edge seams are covered with the airtight film layer, and at least a part of the bottom wall and / or the peripheral wall is not covered with the airtight film layer.

2. The method for making a paper food container according to claim 1, characterized in that: The number of the airtight films placed above the lower mold is more than two, and each of the airtight films covers a portion of the edge seam.

3. The method for making a paper food container according to claim 1 or 2, characterized in that: The airtight film comprises a bonding portion and a clamping portion, a fracture portion is formed between the bonding portion and the clamping portion, and the fracture portion comprises fracture through holes which are distributed discontinuously.

4. The method for making a paper food container according to claim 3, characterized in that: When the airtight film is placed above the lower mold, two ends of the clamping portion are tensioned using a tensioning member so that the fitting portion is located above the container body.

5. The method for making a paper food container according to claim 4, characterized in that: The tensioning member includes a winding device for winding the airtight film; or The tensioning member includes a clamping member for clamping the airtight film.

6. A mold for making paper food containers, including: A lower mold, the upper end of which is open, and the lower mold forms a mold cavity, and a container body formed by folding paper to form a food container can be placed in the mold cavity; An upper die is disposed above the lower die, and the upper die moves in a direction toward or away from the lower die; Features: The upper mold is provided with a substrate, and the substrate has at least one protrusion formed in the direction of the lower mold. The protrusion extends into the mold cavity of the lower mold, and the airtight film is clamped between the protrusion and the container body. After the upper mold is heated, the airtight film is tightly attached to a part of the bottom wall and / or the surrounding wall of the container body and forms an airtight film layer, and at least a part of the bottom wall and / or the surrounding wall is not covered with the airtight film layer.

7. The mold for making a paper food container according to claim 6, characterized in that: The number of the bumps is more than two, and there is a gap between two adjacent bumps.

8. The mold for making a paper food container according to claim 7, characterized in that: A step portion is provided at the lower end of the bump, and in the normal direction of the substrate, an upper end surface of the step portion is higher than a lower end surface of the bump.

9. The mold for making a paper food container according to any one of claims 6 to 8, characterized in that: The lower mold has a flange support portion located at the periphery of the mold cavity, and the base plate of the upper mold can press the flange portion of the container body onto the flange support portion.

10. The mold for making a paper food container according to any one of claims 6 to 8, characterized in that: A heating device is arranged in the upper mold and / or the lower mold.

Citation Information

Patent Citations

  • Paper box for fresh keeping

    CN111000347A

  • Production process of opening folding edge flattening paper container

    CN116215004A

  • Packaging container for printing ink, etc.

    JP1999079158A

Cited By

  • High-airtightness food container

    CN119142632A

  • Manufacturing method for paper food container, and manufacturing mold for paper food container

    WO2026065971A1

  • High-airtightness food container

    WO2026065972A1