Process for efficiently producing water-soluble flaky magnesium nitrate

Through the coordination of the material control plate and the drive plate, intermittent feeding and precise control of magnesium oxide powder are achieved, which solves the problem of powder in magnesium nitrate synthesis, and improves the reaction efficiency and product purity.

CN118954553APending Publication Date: 2024-11-15SHANDONG HUAYANG DIER CHEM CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411431246.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-10-14
Publication Date
2024-11-15

AI Technical Summary

Technical Problem

During the synthesis of magnesium nitrate, it is difficult for magnesium oxide powder to dissolve quickly in the reaction liquid during secondary feeding, affecting the reaction efficiency and product purity.

Method used

The material control plate and the drive plate are used to cooperate with each other to achieve batch feeding and precise control of magnesium oxide powder. The powder is directly put into the reaction liquid, and combined with the design of stirring spiral blades and frame stirrer to ensure that the powder is completely dissolved.

Benefits of technology

It saves reaction time, improves the water solubility and product purity of magnesium nitrate, realizes precise control of the secondary feed quantity, and improves process efficiency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118954553A_ABST
    Figure CN118954553A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of magnesium nitrate production, in particular to a process for efficiently producing water-soluble flaky magnesium nitrate, which comprises the following steps: adding magnesium oxide and nitric acid into a reaction kettle through a feed port and a liquid inlet respectively, stirring and reacting to obtain a magnesium nitrate solution, and judging whether raw materials need to be supplemented or not according to the pH value; pumping the reaction solution into a filter press, and filtering out insoluble impurities to obtain a filtered magnesium nitrate solution; the filtered magnesium nitrate solution enters a crystallization kettle through a magnesium nitrate intermediate tank, centrifugation is performed after crystallization, the obtained mother liquor returns to the reaction kettle, and the obtained solid is directly packaged or enters a magnesium nitrate heat preservation tank; and tabletting the magnesium nitrate crystals entering the magnesium nitrate thermal insulation tank in a tablet press to obtain flaky magnesium nitrate, and packaging and delivering the flaky magnesium nitrate. By adopting the steps, the magnesium oxide powder is directly put into the reaction liquid during secondary feeding, the reaction time is saved, the material control disc and the driving disc are matched with each other, intermittent feeding of secondary feeding is completed, and the feeding amount is accurately controlled.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of magnesium nitrate production, and in particular to a process for efficiently producing water-soluble flaky magnesium nitrate. Background Art

[0002] Nitric acid and magnesium oxide react to form magnesium nitrate, which is an important inorganic salt. Due to its high water solubility and value as a magnesium source, it plays an important role in agricultural fertilizers, fireworks, catalysts, ceramics and various industrial applications. During the reaction process in the synthesis reactor, in order to more finely control the reaction process and improve the purity and yield of the product after the first feeding, a secondary feeding will be carried out according to the progress of the reaction. The powdered raw material magnesium oxide needs to be accurately fed in the secondary feeding. The reactor is a comprehensive reaction vessel. The design of the reactor structure function and configuration accessories is based on the reaction conditions. Its structure is generally composed of a reactor body, a transmission device, a stirring device, a heating device, a cooling device, a sealing device, and corresponding auxiliary equipment: a fractionation column, a condenser, a water separator, a collection tank, a filter, etc. However, during the secondary feeding process, directly feeding into the reactor will cause the magnesium oxide powder to float on the surface of the reaction liquid, which is not conducive to rapid dissolution in the reaction liquid. Summary of the invention

[0003] The invention aims to provide a process for efficiently producing water-soluble flaky magnesium nitrate. During secondary feeding, magnesium oxide powder is directly fed into a reaction solution, thereby saving reaction time. A control disc and a drive disc cooperate with each other to complete intermittent feeding of the secondary feeding, and the feeding amount is precisely controlled.

[0004] To achieve the above object, the present invention provides a process for efficiently producing water-soluble flaky magnesium nitrate, comprising the following steps: S1, adding magnesium oxide and nitric acid into the reactor through the feed inlet and the liquid inlet respectively, stirring the reaction to obtain a magnesium nitrate solution, and judging whether it is necessary to supplement raw materials according to the pH value; S2, pumping the reaction solution obtained in S1 into a filter press to filter out insoluble impurities to obtain a filtered magnesium nitrate solution; S3, the magnesium nitrate solution filtered in S2 enters the crystallization kettle through the magnesium nitrate intermediate tank, centrifuges after crystallization, returns the obtained mother liquor to the reactor, and the obtained solid is directly packaged or enters the magnesium nitrate insulation tank; S4. The magnesium nitrate crystals entering the magnesium nitrate insulation tank in S3 are tableted in a tablet press to obtain flaky magnesium nitrate, which are packaged and shipped out of the warehouse.

[0005] Preferably, in S1, the reactor includes a liquid inlet mechanism, a feeding mechanism, a stirring mechanism and a cooling mechanism, the liquid inlet mechanism and the feeding mechanism are respectively located on both sides of the stirring mechanism, the interlayer of the side wall of the reactor is connected with the cooling mechanism, a material control chamber is provided below the storage chamber of the feeding mechanism, the first discharge port and the first feeding port of the storage chamber are respectively connected with the second discharge port and the second feeding port of the control chamber, the upper and middle part of the stirring shaft of the stirring mechanism is connected with the stirring spiral blade, and the lower part is connected with the frame agitator.

[0006] Preferably, the stirring spiral blade is composed of a first spiral portion and a second spiral portion which are arranged alternately, a feed channel is provided in the first spiral portion, a feed inlet is protruding from the top end of the first spiral portion, a feed outlet is provided at the bottom end of the first spiral portion, and the first spiral portion and the second spiral portion are connected to the stirring shaft through a fixed rod.

[0007] Preferably, in S1, the molar ratio of magnesium oxide to nitric acid in the reactor is 1:2.

[0008] Preferably, in S3, the temperature in the crystallization kettle is cooled to 20-25° C., and the pH is adjusted to 3-4.

[0009] Preferably, in S4, the heating temperature in the magnesium nitrate insulation tank is 25-90°C.

[0010] Preferably, the first feeding port is connected to the first feeding pipe inside the feed control chamber, the second feeding pipe is slidably connected to the second feeding port, a third feeding pipe is provided below the first feeding pipe, the second feeding pipe is sleeved outside the third feeding pipe, the limit block on the top of the second feeding pipe is slidably connected to the limit frame on the side wall of the third feeding pipe, the rack on the side wall of the second feeding pipe is connected to the driving gear, and the taking-over motor connected to the driving gear is located on one side of the feed control chamber.

[0011] Preferably, the first feeding pipe and the third feeding pipe are in contact with a material control disk, and a plurality of driving channels are evenly arranged on the material control disk. The driving channels are slidingly connected to the first driving rod or the second driving rod, and the first driving rod and the second driving rod are respectively connected to the driving disk.

[0012] Preferably, the driving disk is connected to the driving motor through a driving shaft, and a first driving rod, a first intermittent fan-shaped disk, a second driving rod and a second intermittent fan-shaped disk are evenly arranged on the driving disk in sequence, and the central angle of the second intermittent fan-shaped disk is smaller than the central angle of the first intermittent fan-shaped disk.

[0013] Preferably, there is a material control plate between adjacent driving channels, and two discharge ports are symmetrically arranged on the material control plate, the discharge ports are located in the center of the material control plate, the center of the material control plate is connected to the material control shaft, and the material control shaft is hinged to the side wall of the material control cavity.

[0014] Preferably, the feed port of the feed mechanism is connected to the storage chamber, a weighing sensor is provided at the bottom of the storage chamber, a distance sensor is provided at the bottom of the second feeding pipe, and the third feeding pipe is connected to the top of the control chamber through a feeding fixing frame.

[0015] Therefore, the present invention adopts the above-mentioned process for efficiently producing water-soluble flaky magnesium nitrate. During the secondary feeding, magnesium oxide powder is directly added to the reaction solution to save reaction time. The control disk and the drive disk cooperate with each other to complete the intermittent feeding of the secondary feeding and accurately control the feeding amount.

[0016] The technical solution of the present invention is further described in detail below through the accompanying drawings and embodiments. BRIEF DESCRIPTION OF THE DRAWINGS

[0017] Figure 1 This is a flow chart of a process for efficiently producing water-soluble flaky magnesium nitrate according to the present invention; Figure 2 It is a cross-sectional schematic diagram of the reaction kettle in the present invention (the material control plate and the driving plate are not shown); Figure 3 yes Figure 2 A in the enlarged view; Figure 4 It is a schematic diagram of the connection between the material control disk and the driving disk in the present invention.

[0018] Reference numerals: 1. Liquid inlet mechanism; 11. Upper liquid inlet nozzle; 12. Middle liquid inlet nozzle; 13. Lower liquid inlet nozzle; 14. Liquid inlet port; 15. Liquid inlet pipe; 2. Feeding mechanism; 21. Material storage chamber; 211. Weighing sensor; 22. Material control chamber; 23. Material control plate; 231. Driving channel; 232. Third material outlet; 233. Material control plate; 234. Material control shaft; 24. Driving plate; 241. Driving shaft; 242. First driving rod; 243. First intermittent sector disc; 244. Second driving rod; 245. Second intermittent sector disc Sector-shaped disc; 25. First feeding pipe; 26. Second feeding pipe; 261. Limit block; 262. Take-over motor; 263. Driving gear; 264. Rack; 265. Distance sensor; 27. Third feeding pipe; 271. Limit frame; 272. Feed fixing frame; 28. First discharge port; 3. Stirring mechanism; 31. First spiral portion; 311. Feed inlet; 312. Feed outlet; 32. Second spiral portion; 33. Frame agitator; 34. Fixed rod; 35. Stirring shaft; 4. Cooling mechanism; 5. Reactor. DETAILED DESCRIPTION

[0019] The present invention is further described below in conjunction with the accompanying drawings and embodiments. Unless otherwise defined, the technical terms or scientific terms used in the present invention should be the common meanings understood by people with ordinary skills in the field to which the present invention belongs. The above-mentioned features or features mentioned in the specific examples mentioned in the present invention can be combined arbitrarily, and these specific embodiments are only used to illustrate the present invention and are not used to limit the scope of the present invention.

[0020] Example 1 like Figure 1 As shown, the present invention provides a process for efficiently producing water-soluble flaky magnesium nitrate, comprising the following steps: S1, adding magnesium oxide and nitric acid into the reactor through the feed inlet and the liquid inlet respectively, stirring the reaction to obtain a magnesium nitrate solution, and judging whether it is necessary to supplement raw materials according to the pH value; In S1, the molar ratio of magnesium oxide to nitric acid in the reactor is 1:2.

[0021] S2. Pump the reaction solution obtained in S1 into a filter press to filter out insoluble impurities to obtain a filtered magnesium nitrate solution.

[0022] S3, the magnesium nitrate solution filtered in S2 enters the crystallization kettle through the magnesium nitrate intermediate tank, centrifuges after crystallization, returns the obtained mother liquor to the reactor, and the obtained solid is directly packaged or enters the magnesium nitrate insulation tank; In S3, the temperature in the crystallization kettle is cooled to 25°C and the pH is adjusted to 3-4.

[0023] S4. The magnesium nitrate crystals entering the magnesium nitrate insulation tank in S3 are tableted in a tablet press to obtain flaky magnesium nitrate, which are packaged and shipped out of the warehouse.

[0024] In S4, the heating temperature in the magnesium nitrate insulation tank is 25-90°C.

[0025] Example 2 like Figure 2-Figure 4 As shown, the reactor 5 used in S1 of Example 1 includes a liquid inlet mechanism 1, a feeding mechanism 2, a stirring mechanism 3 and a cooling mechanism 4. The liquid inlet mechanism 1 and the feeding mechanism 2 are respectively located on both sides of the stirring mechanism 3, and the interlayer of the side wall of the reactor 5 is connected to the cooling mechanism 4. A material control chamber 22 is provided below the storage chamber 21 of the feeding mechanism 2, and the first discharge port 28 and the first feeding port of the storage chamber 21 are respectively connected to the second discharge port and the second feeding port of the control chamber 22. The upper and middle parts of the stirring shaft 35 of the stirring mechanism 3 are connected to the stirring spiral blade, and the lower part thereof is connected to the frame stirrer 33.

[0026] Nitric acid enters the reactor 5 through the liquid feeding mechanism 1, and magnesium oxide enters the reactor 5 through the feeding mechanism 2. After the feeding is completed, the stirring mechanism 3 is started to fully react to obtain magnesium nitrate. The cooling mechanism 4 controls the temperature in the reactor 5 to ensure that the reaction is fully carried out. The feeding mechanism 2 can perform two processes of primary feeding and secondary feeding. In the primary feeding process, the feeding is carried out through the connected first discharge port 28 and the second discharge port according to the molar ratio with nitric acid. The secondary feeding adds magnesium oxide through the first feeding port to fully react or adjust the pH. The stirring mechanism 3 stirs the upper and lower parts of the reactor 5 respectively through the stirring spiral blades and the frame stirrer 33 to ensure that the reaction liquid in each place is fully reacted.

[0027] The stirring spiral blade is composed of a staggered first spiral portion 31 and a second spiral portion 32, and a material feeding channel is provided in the first spiral portion 31. A material feeding inlet 311 is protruding from the top of the first spiral portion 31, and a material feeding outlet 312 is provided at the bottom of the first spiral portion 31. The first spiral portion 31 and the second spiral portion 32 are connected to the stirring shaft 35 through a fixing rod 34.

[0028] The stirring spiral blade stirs the reaction liquid in the reactor 5 through the first spiral portion 31 and the second spiral portion 32, and the magnesium oxide powder of the secondary feed is directly put into the reaction liquid through the feeding channel of the first spiral portion 31, so that the magnesium oxide powder is completely dissolved in the reaction liquid. The diameter of the feeding inlet 311 is slightly larger than the diameter of the second feeding pipe 26. When the feeding inlet 311 is located below the second feeding pipe 26, it moves downward until the second feeding pipe 26 is connected to the feeding inlet 311, and intermittent feeding is performed to control the feeding amount. The fed magnesium oxide powder slides down to the feeding outlet 312 in the spiral descending feeding channel, and the magnesium oxide is further driven to leave the feeding channel during the rotation of the stirring spiral blade.

[0029] The first feeding port is connected to the first feeding pipe 25 inside the control chamber 22, and the second feeding port is slidably connected with the second feeding pipe 26, and the third feeding pipe 27 is provided below the first feeding pipe 25. The second feeding pipe 26 is sleeved outside the third feeding pipe 27, and the limit block 261 at the top of the second feeding pipe 26 is slidably connected with the limit frame 271 on the side wall of the third feeding pipe 27. The rack 264 on the side wall of the second feeding pipe 26 is connected to the driving gear 263, and the connecting motor 262 connected to the driving gear 263 is located on one side of the control chamber 22. The distance between the bottom of the first feeding pipe 25 and the top of the third feeding pipe 27 is the same as the thickness of the control plate 23. When the third discharge port 232 of the control plate 23 is located between the first feeding pipe 25 and the third feeding pipe 27, the magnesium oxide powder in the storage chamber 21 enters the feeding channel. The amount of magnesium oxide powder added can be precisely controlled through the connection area between the third discharge port 232 and the first feeding pipe 25 and the third feeding pipe 27 .

[0030] Start the take-over motor 262, drive the gear 263 to drive the second feeding pipe 26 to move up and down through the rack 264, and the setting of the limit block 261 and the limit frame 271 limits the movement range of the second feeding pipe 26. The second feeding pipe 26 moves relative to the bottom of the control chamber 22. When the second feeding pipe 26 is retracted, it does not affect the operation of the stirring mechanism 3.

[0031] The first feeding tube 25 and the third feeding tube 27 are in contact with the material control disk 23, and a plurality of driving channels 231 are evenly arranged on the material control disk 23. The driving channels 231 are slidably connected with the first driving rod 242 or the second driving rod 244, and the first driving rod 242 and the second driving rod 244 are respectively connected with the driving disk 24. When the first driving rod 242 or the second driving rod 244 contacts the driving channel 231, the material control disk 23 is driven to rotate, and then the third material outlet 232 is driven to intermittently connect the first feeding tube 25 and the third feeding tube 27.

[0032] The driving disk 24 is connected to the driving motor through the driving shaft 241. The driving disk 24 is evenly provided with a first driving rod 242, a first intermittent sector disk 243, a second driving rod 244 and a second intermittent sector disk 245 in sequence. The center angle of the second intermittent sector disk 245 is smaller than the center angle of the first intermittent sector disk 243. The driving motor is started to drive the driving disk 24 to rotate. When the first driving rod 242 and the second driving rod 244 enter the driving channel 231 in the material control disk 23, the material control disk 23 rotates with the driving disk 24. When the first intermittent sector disk 243 and the second intermittent sector disk 245 contact the side wall of the material control plate 233 of the material control disk 23, the material control disk 23 does not rotate with the driving disk 24.

[0033] Between the adjacent driving channels 231 is a material control plate 233, and two third material discharge ports 232 are symmetrically arranged on the material control plate 23, and the third material discharge port 232 is located in the center of the material control plate 233. The center of the material control plate 23 is connected to the material control shaft 234, and the material control shaft 234 is hinged to the side wall of the material control chamber 22. The material control shaft 234 is located on one side of the first material discharge port 28 and the first feeding port, and does not affect the smooth discharge of the two. The rotation of the material control plate 23 drives the third material discharge port 232 to change its position. When the third material discharge port 232 is located between the first feeding pipe 25 and the third feeding pipe 27, the magnesium oxide powder in the storage chamber 21 enters the feeding channel; when the third material discharge port 232 is not located between the first feeding pipe 25 and the third feeding pipe 27, the material control plate 233 separates the first feeding pipe 25 and the third feeding pipe 27, and the magnesium oxide powder cannot enter the feeding channel.

[0034] The liquid inlet 14 of the liquid inlet mechanism 1 is connected to the liquid inlet pipe 15 in the reactor 5. The liquid inlet pipe 15 is provided with a lower liquid inlet nozzle 13, a middle liquid inlet nozzle 12 and an upper liquid inlet nozzle 11 from top to bottom, and the liquid inlet pipe 15 is connected to the side wall of the reactor 5 through a liquid inlet fixing frame. Liquid is fed at different positions in the reactor 5 through the lower liquid inlet nozzle 13, the middle liquid inlet nozzle 12 and the upper liquid inlet nozzle 11, and different positions can be selected for liquid feeding according to the amount of liquid fed.

[0035] The feed port of the feed mechanism 2 is connected to the storage chamber 21. A weighing sensor 211 is provided at the bottom of the storage chamber 21. The weighing sensor 211 is used to control the amount of magnesium oxide powder added to the reactor 5. A distance sensor 265 is provided at the bottom of the second feed pipe 26. Since the feed inlet 311 is protruding, when it is detected that the feed inlet 311 is located below the second feed pipe 26, the second feed pipe 26 is moved down to communicate with the feed inlet 311. The third feed pipe 27 is connected to the top of the control chamber 22 through a feed fixing frame 272. The feed fixing frame 272 is located on the side of the third feed pipe 27 away from the control plate 23, and the third feed pipe 27 is fixed below the control plate 23. The limit frame 271 is located below the feed fixing frame 272. The feed fixing frame 272 does not affect the normal operation of the control plate 23 and the second feed pipe 26.

[0036] Therefore, the present invention adopts the above-mentioned process for efficiently producing water-soluble flaky magnesium nitrate. During the secondary feeding, magnesium oxide powder is directly added to the reaction solution to save reaction time. The control disk and the drive disk cooperate with each other to complete the intermittent feeding of the secondary feeding and accurately control the feeding amount.

[0037] Finally, it should be noted that the above embodiments are only used to illustrate the technical solution of the present invention rather than to limit it. Although the present invention has been described in detail with reference to the preferred embodiments, those skilled in the art should understand that they can still modify or replace the technical solution of the present invention with equivalents, and these modifications or equivalent replacements cannot cause the modified technical solution to deviate from the spirit and scope of the technical solution of the present invention.

Claims

1. A process for efficiently producing water-soluble flaky magnesium nitrate, characterized in that: The following steps are included: S1, adding magnesium oxide and nitric acid into the reactor through the feed inlet and the liquid inlet respectively, stirring the reaction to obtain a magnesium nitrate solution, and judging whether it is necessary to supplement raw materials according to the pH value; S2, pumping the reaction solution obtained in S1 into a filter press to filter out insoluble impurities to obtain a filtered magnesium nitrate solution; S3, the magnesium nitrate solution filtered in S2 enters the crystallization kettle through the magnesium nitrate intermediate tank, centrifuges after crystallization, returns the obtained mother liquor to the reactor, and the obtained solid is directly packaged or enters the magnesium nitrate insulation tank; S4. The magnesium nitrate crystals entering the magnesium nitrate insulation tank in S3 are tableted in a tablet press to obtain flaky magnesium nitrate, which are packaged and shipped out of the warehouse.

2. A process for efficiently producing water-soluble flaky magnesium nitrate according to claim 1, characterized in that: In S1, the reactor includes a liquid inlet mechanism, a feeding mechanism, a stirring mechanism and a cooling mechanism. The liquid inlet mechanism and the feeding mechanism are respectively located on both sides of the stirring mechanism. The interlayer of the side wall of the reactor is connected with the cooling mechanism. A material control chamber is provided below the storage chamber of the feeding mechanism. The first discharge port and the first feeding port of the storage chamber are respectively connected with the second discharge port and the second feeding port of the control chamber. The upper and middle part of the stirring shaft of the stirring mechanism is connected with the stirring spiral blade, and the lower part is connected with the frame agitator.

3. A process for efficiently producing water-soluble flaky magnesium nitrate according to claim 2, characterized in that: The stirring spiral blade is composed of a first spiral portion and a second spiral portion which are arranged alternately. A feeding channel is arranged in the first spiral portion. A feeding inlet is protruding from the top of the first spiral portion. A feeding outlet is arranged at the bottom of the first spiral portion. Both the first spiral portion and the second spiral portion are connected to the stirring shaft through a fixing rod.

4. A process for efficiently producing water-soluble flaky magnesium nitrate according to claim 1, characterized in that: In S1, the molar ratio of magnesium oxide to nitric acid in the reactor is 1:

2.

5. A process for efficiently producing water-soluble flaky magnesium nitrate according to claim 1, characterized in that: In S3, the temperature in the crystallization kettle is cooled to 20-25°C and the pH is adjusted to 3-4.

6. A process for efficiently producing water-soluble flaky magnesium nitrate according to claim 1, characterized in that: In S4, the heating temperature in the magnesium nitrate insulation tank is 25-90°C.

7. A process for efficiently producing water-soluble flaky magnesium nitrate according to claim 2, characterized in that: The first feeding port is connected to the first feeding pipe inside the feeding control chamber, the second feeding port is slidably connected with the second feeding pipe, a third feeding pipe is arranged below the first feeding pipe, the second feeding pipe is sleeved outside the third feeding pipe, a limiting block on the top of the second feeding pipe is slidably connected to the limiting frame on the side wall of the third feeding pipe, the rack on the side wall of the second feeding pipe is connected to the driving gear, and the taking-over motor connected to the driving gear is located on one side of the feeding control chamber.

8. A process for efficiently producing water-soluble flaky magnesium nitrate according to claim 7, characterized in that: The first feeding pipe and the third feeding pipe are in contact with the material control disk, and a plurality of driving channels are evenly arranged on the material control disk. The driving channels are slidably connected to the first driving rod or the second driving rod, and the first driving rod and the second driving rod are respectively connected to the driving disk.

9. A process for efficiently producing water-soluble flaky magnesium nitrate according to claim 8, characterized in that: The driving disk is connected to the driving motor through a driving shaft. The driving disk is evenly provided with a first driving rod, a first intermittent sector disk, a second driving rod and a second intermittent sector disk in sequence. The central angle of the second intermittent sector disk is smaller than the central angle of the first intermittent sector disk.

10. A process for efficiently producing water-soluble flaky magnesium nitrate according to claim 8, characterized in that: A material control plate is disposed between adjacent driving channels, and two discharge ports are symmetrically arranged on the material control plate. The discharge ports are located in the center of the material control plate. The center of the material control plate is connected to the material control shaft, and the material control shaft is hinged to the side wall of the material control cavity.