Porous aromatic skeleton energetic material based on tetrazine ring and guanidine salt as well as preparation method and application of porous aromatic skeleton energetic material
Through the synthesis of tetrazine ring and guanidine salt, porous aromatic framework energy-containing materials EPAF-8 and EPAF-9 were prepared, solving the problems of existing high-energy explosive sensitivity and complex preparation process, and achieving high energy density and low sensitivity Porous aromatic skeleton energy-containing material has significant detonation performance and industrial application potential.
Patent Information
- Application Number
- CN202410953086.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-16
- Publication Date
- 2024-11-15
- Estimated Expiration
- 2044-07-16
AI Technical Summary
The existing high-energy explosives are sensitive to external stimuli, have low safety, and there is room for improvement in the detonation performance and preparation process of porous aromatic skeleton energy-containing materials, which affects their energy density and industrial development in actual applications.
Using tetrazine ring and guanidine salt as raw materials, the porous aromatic skeleton energy-containing materials EPAF-8 and EPAF-9 are synthesized through ultrasonic treatment and oil bath reaction under nitrogen protection, and the preparation process is optimized to improve the energy density and thermal stability of the product. , while reducing the sensitivity.
The preparation of porous aromatic skeleton energy-containing materials with high energy and low sense has high energy density, low sensitivity and good thermal stability, simplifies the preparation process, and enhances its safety and industrialization potential in practical applications.
Smart Images

Figure CN118955897A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of energetic materials, and relates to a porous aromatic skeleton energetic material based on tetrazine rings and guanidine salts, and a preparation method and application thereof. Background Art
[0002] As a typical energetic material, explosives are widely used in military and civilian fields. However, high-energy explosives are often very sensitive to external stimuli, and safety issues seriously restrict their practical application. In response to the above problems, researchers have made great efforts to try to make high energy and low sensitivity compatible in energetic materials, including: (1) molecular level design, including the introduction of functional groups (such as nitro, amino, etc.), the merging of various types of nitrogen heterocycles, the formation of salts, the stereochemical effects of molecular structures, hydrogen bonding strategies, etc.; (2) eutectic design of energetic material molecules; (3) preparation of energetic composite materials based on polymer or other material coating; (4) development of new energetic materials, including energetic ionic liquids, energetic polymers, etc. These research strategies have achieved certain results and greatly enriched the types of energetic materials. However, the complex synthesis steps, yield and cost, crystallization difficulty, dispersion uniformity, etc. have greatly increased the difficulty of research work. At the same time, the coating of non-energetic components will also reduce the energy density and detonation performance of energetic materials.
[0003] Therefore, it is of great scientific significance to explore the design and research ideas of energetic materials with high energy and low sensitivity to promote the development of the field of energetic materials. In recent years, experts and scholars at home and abroad have carried out some research work related to energetic materials around porous materials. Majano et al. loaded the high-density energetic material FOX-7 into the pores of pure silica MFI zeolite nanocrystals, so that FOX-7 did not explode and decompose at about 100°C above the explosion temperature. In 2013, the team of Professor Pang Siping of Beijing Institute of Technology reported for the first time a cationic energetic metal organic framework material with a three-dimensional structure. Its excellent detonation performance makes it have great potential application value in the field of energetic materials. In 2016, Professor Wang Bo's research group and collaborators used the classic MOF (HKUST-1) as a conductive framework precursor, and combined the porous carbon material formed after carbonization with in-situ synthesized copper azide to solve the problem of high electrostatic sensitivity of copper azide, while showing good flame sensitivity, high density, high positive heat of formation and excellent initiation ability. In addition, Titi et al. proposed a strategy to induce the spontaneous combustion behavior of MOFs in 2019. By introducing acetylene or ethylene substituents as triggers for spontaneous combustion in ZIFs, the ability to achieve and adjust the spontaneous combustion performance can be achieved, making spontaneous combustion MOFs promising to become safer and more environmentally friendly propellants. It can be seen that porous materials have played an important role in the development of energetic materials and have great research value.
[0004] Porous aromatic frameworks (PAFs) are a new type of porous material composed of aromatic building blocks, which have experienced rapid development in the past decade. The aromatic building blocks have rich structural types and good chemical reaction activity. By designing the structural units and modifying the PAFs skeleton, the structure and pore properties of PAFs can be regulated, thereby showing different performances and being applied in various fields. For example, the prior art such as CN113278162A has conducted a preliminary exploration of porous aromatic framework energetic materials (EPAFs) and their preparation methods, but the materials prepared therefrom still have room for improvement in terms of specific detonation performance. In addition, how to further improve the preparation process of porous aromatic framework energetic materials to make their production more convenient and quick, so as to be both economical and practical, is also a goal that the industry has always pursued. Summary of the invention
[0005] In view of this, the present invention provides a porous aromatic skeleton energetic material based on tetrazine rings and guanidine salts, and a preparation method and application thereof. Using tetrazine rings and guanidine salts as raw materials, porous aromatic skeleton energetic materials EPAF-8 and / or EPAF-9 are synthesized, and the related products have high energy density and thermal stability, and at the same time have low sensitivity, realizing the preparation of high-energy and low-sensitivity energetic materials, and at the same time optimizing and improving the preparation process, simplifying the preparation process of obtaining the final product, and the whole preparation process has mild conditions and simple process, and has strong industrial application potential.
[0006] To achieve the above-mentioned effects, the first aspect of the present invention provides a method for preparing a porous aromatic skeleton energetic material based on tetrazine rings and guanidine salts, wherein the porous aromatic skeleton energetic material is formed by polymerization of tetrazine rings and guanidine salts, and is characterized in that it comprises the following specific steps: S1: weighing a certain amount of tetrazine rings and guanidine salts into a double-necked bottle, adding a solvent and N,N-diisopropylethylamine to obtain a mixed solution, and ultrasonically treating the mixed solution; S2: under nitrogen protection, in a 60-180°C oil bath, stirring the ultrasonically treated mixed solution obtained in S1 for 2-4 days, and filtering the obtained product; S3: washing and drying the product obtained by filtration in S2 to obtain a porous aromatic skeleton material.
[0007] Optionally, the tetrazine ring in S1 is 3,6-dichloro-1,2,4,5-tetrazine; and the guanidine salt is triaminoguanidine hydrochloride or triaminoguanidine NTO salt.
[0008] Optionally, the guanidine salt is triaminoguanidine hydrochloride, and the mass ratio of the 3,6-dichloro-1,2,4,5-tetrazine to triaminoguanidine hydrochloride is 23:14; or, the guanidine salt is triaminoguanidine NTO salt, and the mass ratio of the 3,6-dichloro-1,2,4,5-tetrazine to triaminoguanidine NTO salt is 23:24.
[0009] Optionally, the solvent in S1 is at least one of toluene, mesitylene, o-dichlorobenzene or N,N-dimethylacetamide.
[0010] Optionally, the solvent in S1 is mesitylene, and in the mixed solution, the volume ratio of mesitylene to N,N-diisopropylethylamine is 5:1.
[0011] Optionally, the washing and drying of the product obtained by filtration in S2 in S3 specifically includes: washing the product obtained by filtration in S2 with dichloromethane, ethanol and purified water in sequence, and vacuum drying at 80° C. overnight.
[0012] The second aspect of the present invention provides a porous aromatic skeleton energetic material based on tetrazine rings and guanidine salts, wherein the porous aromatic skeleton energetic material is EPAF-8, and its specific structure is as follows:
[0013]
[0014] The third aspect of the present invention provides another porous aromatic skeleton energetic material based on tetrazine rings and guanidine salts, wherein the porous aromatic skeleton energetic material is EPAF-9, and its specific structure is as follows:
[0015]
[0016] Optionally, the porous aromatic skeleton energetic material of tetrazine rings and guanidine salts is prepared by the above-mentioned preparation method.
[0017] The fourth aspect of the present invention provides one or more porous aromatic skeleton energetic materials based on tetrazine rings and guanidine salts for use in the field of energetic materials.
[0018] The beneficial effects of the present invention are:
[0019] (1) The porous aromatic framework energetic materials EPAF-8 and / or EPAF-9 based on tetrazine rings and guanidine salts have cationic charge characteristic frameworks, high energy density, high thermal stability and stability, and are energetic materials with great application potential.
[0020] (2) The conditions for preparing the porous aromatic skeleton material are mild, the process is simple, and it is easy to operate, which optimizes the existing preparation process procedures and at the same time ensures a high yield of the final product to meet the actual industrial production requirements.
[0021] In addition, additional advantages, objects, and features of the present invention will be described in part in the following description, and will become apparent to those skilled in the art after studying the following, or may be learned from the practice of the present invention. The objects and other advantages of the present invention may be realized and obtained by the structures and method steps specifically pointed out in the written description and claims and the accompanying drawings.
[0022] Those skilled in the art will appreciate that the objectives and advantages that can be achieved with the present invention are not limited to the above specific description, and the above and other objectives that can be achieved by the present invention will be more clearly understood from the following detailed description. BRIEF DESCRIPTION OF THE DRAWINGS
[0023] The drawings described herein are used to provide a further understanding of the present invention, constitute a part of this application, and do not constitute a limitation of the present invention.
[0024] Figure 1 This is a Fourier infrared spectrum (IR) of the energetic material EPAF-8 prepared in Example 1 of the present invention;
[0025] Figure 2 This is the TG-DSC curve of the energetic material EPAF-8 prepared in Example 1 of the present invention.
[0026] Figure 3 This is a Fourier infrared spectrum (IR) of the energetic material EPAF-9 prepared in Example 5 of the present invention;
[0027] Figure 4 This is the TG-DSC curve of the energetic material EPAF-9 prepared in Example 5 of the present invention. DETAILED DESCRIPTION
[0028] In order to make the purpose, technical scheme and advantages of the present invention more clearly understood, the present invention is further described in detail below in conjunction with the embodiments and the accompanying drawings. The schematic embodiments of the present invention and their descriptions are used to explain the present invention, but are not intended to limit the present invention. It should also be noted that, in order to avoid blurring the present invention due to unnecessary details, only structures and / or processing steps closely related to the solutions according to the present invention are shown in the accompanying drawings, while other details that are not closely related to the present invention are omitted.
[0029] It should be emphasized that the term “include / comprises” when used herein refers to the presence of features, elements, steps or components, but does not exclude the presence or addition of one or more other features, elements, steps or components.
[0030] The embodiment of the present invention provides a first aspect of a method for preparing a porous aromatic skeleton energetic material based on tetrazine rings and guanidine salts, wherein the porous aromatic skeleton energetic material is formed by polymerization of tetrazine rings and guanidine salts, and is characterized in that the method comprises the following specific steps: S1: weighing a certain amount of tetrazine rings and guanidine salts into a double-necked bottle, adding a solvent and N,N-diisopropylethylamine to obtain a mixed solution, and ultrasonically treating the mixed solution; S2: under nitrogen protection, in a 60-180°C oil bath, stirring the ultrasonically treated mixed solution obtained in S1 for 2-4 days, and filtering the obtained product; S3: washing and drying the product obtained by filtration in S2 to obtain a porous aromatic skeleton material.
[0031] Among them, tetrazine ring, as a typical high-nitrogen, low-carbon and hydrogen material, performs well in energy density and combustion efficiency. Tetrazine ring has a variety of synthetic routes, a simple synthesis process, a short reaction time, is green and environmentally friendly, and has a low production cost. In addition, tetrazine ring also has a high reactivity and is easy to covalently bond with other substances, which makes tetrazine ring materials more flexible and diverse when participating in the preparation of energetic materials. The selection of guanidine salts to react with tetrazine rings fully takes into account their high energy characteristics. In the process of preparing the target product of the present invention, a coprecipitation reaction can be fully carried out with the tetrazine ring material, and the composition and structure of the reactants can be better controlled to achieve precise preparation.
[0032] In addition, it should be noted that in the existing preparation technology, a porous aromatic skeleton energetic material is often first obtained by reaction, and then the porous aromatic skeleton energetic material is subjected to a composite reaction with a single explosive (such as NTO) to form a composite energetic material, that is, the porous aromatic skeleton energetic material is an intermediate product, and its preparation purpose is often aimed at improving the high sensitivity and strong corrosion characteristics of the existing single explosive, and it is not the final product. The preparation method proposed in the present invention uses a direct reaction between a tetrazine ring and a guanidine salt, and directly prepares a composite energetic material with similar functions to the existing porous aromatic skeleton energetic material through a more convenient reaction process, and even with better energy density and combustion performance, which undoubtedly simplifies the existing preparation process and is conducive to the industrial application of related materials.
[0033] Optionally, the tetrazine ring in S1 is 3,6-dichloro-1,2,4,5-tetrazine; and the guanidine salt is triaminoguanidine hydrochloride or triaminoguanidine NTO salt.
[0034] Optionally, the guanidine salt is triaminoguanidine hydrochloride, and the mass ratio of 3,6-dichloro-1,2,4,5-tetrazine to triaminoguanidine hydrochloride is 23:14; or, the guanidine salt is triaminoguanidine NTO salt, and the mass ratio of 3,6-dichloro-1,2,4,5-tetrazine to triaminoguanidine NTO salt is 23:24.
[0035] Optionally, the solvent in S1 preferably has a high boiling point and good solubility, and the preparation can be achieved by using a single solvent or a mixture thereof. The solvent component can specifically be at least one of toluene, mesitylene, o-dichlorobenzene or N,N-dimethylacetamide.
[0036] Optionally, the solvent in S1 is mesitylene, and in the mixed solution, the volume ratio of mesitylene to N, N-diisopropylethylamine is 5:1. The N, N-diisopropylethylamine used here as an "acid binding agent" has the main function of neutralizing the acid produced in the reaction, allowing the reaction to proceed in the forward direction to promote the synthesis. Similarly, if one or more of toluene, o-dichlorobenzene or N, N-dimethylacetamide are selected to participate in the reaction, the role played by mesitylene in the reaction process is substantially the same or similar.
[0037] Optionally, washing and drying the product filtered in S2 in S3 specifically includes: washing the product filtered in S2 with dichloromethane, ethanol and purified water in sequence, and vacuum drying at 80° C. overnight.
[0038] It is worth noting that when washing with different solvents, a certain order should be followed. It is reasonable to expect that dichloromethane is used to remove tetrazine monomers, ethanol is used to remove the remaining dichloromethane solvent in the previous procedure, and finally water is used to remove guanidine monomers. Here, dichloromethane and water must be transitioned through ethanol because dichloromethane and water are not miscible. In fact, the order of washing treatment has an unclear effect on the results such as yield. It is more about the effect on product purity after the washing process. Based on what has been mentioned before, the porous aromatic skeleton energetic material prepared by the present invention is a final product rather than an intermediate product. In order to achieve the purpose of industrial production, it is reasonable to have higher requirements for the purity of its product, which makes the washing process in the above order an inevitable requirement.
[0039] The second aspect of the present invention provides a porous aromatic skeleton energetic material based on tetrazine rings and guanidine salts, wherein the porous aromatic skeleton energetic material is EPAF-8, and its specific structure is as follows:
[0040]
[0041] The third aspect of the present invention provides another porous aromatic skeleton energetic material based on tetrazine rings and guanidine salts, wherein the porous aromatic skeleton energetic material is EPAF-9, and its specific structure is as follows:
[0042]
[0043] Optionally, the porous aromatic skeleton energetic material of tetrazine ring and guanidine salt is prepared by the above preparation method.
[0044] The fourth aspect of the present invention provides one or more porous aromatic skeleton energetic materials based on tetrazine rings and guanidine salts for use in the field of energetic materials.
[0045] The present invention is further described in detail below through specific examples. The following examples are only illustrative and not restrictive, and the protection scope of the present invention cannot be limited thereto.
[0046] In addition, the present invention aims to design and synthesize new porous aromatic frameworks (EPAFs) materials. By utilizing the characteristics of PAFs materials, the resulting products have diverse high-porosity structures, ultra-high chemical stability, and can withstand a variety of harsh conditions such as strong acids, strong bases, solvents, heat, and moisture, providing technical and theoretical reserves for the future development of energetic materials and porous materials chemistry, and having great potential application value.
[0047] Example 1
[0048] The present invention uses energetic monomers triaminoguanidine hydrochloride and 3,6-dichloro-1,2,4,5-tetrazine as raw materials to polymerize the synthetic route and structure of the porous aromatic skeleton energetic material EPAF-8:
[0049]
[0050] 2.3 g 3,6-dichloro-1,2,4,5-tetrazine (15.0 mmol) and 1.4 g triaminoguanidine hydrochloride (10.0 mmol) were weighed into a 250 mL two-necked bottle, 50 mL mesitylene and 10 mL N, N-diisopropylethylamine (DIPEA) were added, and the mixed solution was ultrasonicated for a period of time; under nitrogen protection, the mixture was stirred in an oil bath at 180° C. for 2 days, and the product was filtered; the filtered product was washed with dichloromethane, ethanol and purified water respectively, and vacuum dried at 80° C. overnight to obtain a porous aromatic framework EPAF-8 material with a yield of 87.5%.
[0051] The porous aromatic skeleton energetic material EPAF-8 prepared in Example 1 was analyzed by Fourier transform infrared spectroscopy. Figure 1 .
[0052] Depend on Figure 1 It can be seen that the peak at 880cm-1 is related to the stretching vibration of C-Cl on 3,6-dichloro-1,2,4,5-tetrazine, while the peaks at 3320cm-1 and 3200cm-1 are attributed to the characteristic vibration of the amino group on triaminoguanidine hydrochloride. These characteristic peaks disappeared in the product, indicating that the monomers have been fully reacted, proving the successful synthesis of EPAF-8.
[0053] The porous aromatic skeleton energetic material EPAF-8 prepared in Example 1 was subjected to TG-DSC analysis. The results are shown in Figure 2 .
[0054] It can be seen from the TG-DSC curve analysis results that EPAF-8 has excellent thermal stability and presents an obvious exothermic signal peak, and has potential application value in the field of energetic materials.
[0055] Table 1 shows the impact sensitivity and calculated theoretical detonation performance of the energetic material EPAF-8 prepared according to Example 1. It can be seen from the table that the energetic material EPAF-8 exhibits low sensitivity and very good energetic characteristics. Compared with the prior art, the energetic material EPAF-8 produced by the preparation method of the present invention has significant improvements in the main detonation performance, which is due to the excellent performance of the reactants themselves and the effective improvement of the relevant preparation process.
[0056] Table 1. Impact sensitivity and calculated theoretical detonation performance of energetic material EPAF-8 in Example 1
[0057]
[0058] Example 2
[0059] 2.3 g 3,6-dichloro-1,2,4,5-tetrazine (15.0 mmol) and 1.4 g triaminoguanidine hydrochloride (10.0 mmol) were weighed into a 250 mL two-necked bottle, 50 mL mesitylene and 10 mL N, N-diisopropylethylamine (DIPEA) were added, and the mixed solution was ultrasonicated for a period of time; under nitrogen protection, the mixture was stirred in an oil bath at 150° C. for 2 days, and the product was filtered; the filtered product was washed with dichloromethane, ethanol and purified water respectively, and vacuum dried at 80° C. overnight to obtain a porous aromatic framework EPAF-8 material with a yield of 85.5%.
[0060] Example 3
[0061] 2.3 g 3,6-dichloro-1,2,4,5-tetrazine (15.0 mmol) and 1.4 g triaminoguanidine hydrochloride (10.0 mmol) were weighed into a 250 mL two-necked bottle, 50 mL mesitylene and 10 mL N, N-diisopropylethylamine (DIPEA) were added, and the mixed solution was ultrasonicated for a period of time; under nitrogen protection, the mixture was stirred in an oil bath at 180° C. for 3 days, and the product was filtered; the filtered product was washed with dichloromethane, ethanol and purified water respectively, and vacuum dried at 80° C. overnight to obtain a porous aromatic framework EPAF-8 material with a yield of 89.5%.
[0062] Example 4
[0063] 4.6 g 3,6-dichloro-1,2,4,5-tetrazine (30.0 mmol) and 2.8 g triaminoguanidine hydrochloride (20.0 mmol) were weighed into a 250 mL two-necked bottle, 50 mL mesitylene and 10 mL N, N-diisopropylethylamine (DIPEA) were added, and the mixed solution was ultrasonicated for a period of time; under nitrogen protection, the mixture was stirred in an oil bath at 150° C. for 2 days, and the product was filtered; the filtered product was washed with dichloromethane, ethanol and purified water respectively, and vacuum dried at 80° C. overnight to obtain a porous aromatic framework EPAF-8 material with a yield of 83.0%.
[0064] Example 5
[0065] The present invention uses energetic monomers triaminoguanidine NTO and 3,6-dichloro-1,2,4,5-tetrazine as raw materials to polymerize the synthetic route and structure of the porous aromatic skeleton energetic material EPAF-9:
[0066]
[0067] 2.3 g 3,6-dichloro-1,2,4,5-tetrazine (15.0 mmol) and 2.4 g triaminoguanidine NTO salt (10.0 mmol) were weighed into a 250 mL two-necked bottle, 50 mL mesitylene and 10 mL N, N-diisopropylethylamine (DIPEA) were added, and the mixed solution was ultrasonicated for a period of time; under nitrogen protection, the reaction was stirred in an oil bath at 180°C for 2 days, and the product was filtered; it was washed with dichloromethane, ethanol and purified water respectively, and vacuum dried at 80°C overnight to obtain a porous aromatic framework EPAF-9 material with a yield of 84.5%.
[0068] The porous aromatic skeleton energetic material EPAF-9 prepared in Example 5 was analyzed by Fourier transform infrared spectroscopy. Figure 3 .
[0069] Depend on Figure 3 It can be seen that 880cm -1 The peak at 3320 cm is related to the stretching vibration of C-Cl on 3,6-dichloro-1,2,4,5-tetrazine, while the peak at 3320 cm -1 , 3200cm -1 The peaks at are attributed to the characteristic vibrations of the amino groups on the triaminoguanidine NTO salt. These characteristic peaks disappeared in the product, indicating that the monomers have been fully reacted, proving the successful synthesis of EPAF-9.
[0070] The porous aromatic skeleton energetic material EPAF-9 prepared in Example 5 was subjected to TG-DSC analysis. Figure 4 .
[0071] It can be seen from the TG-DSC curve analysis results that EPAF-9 has excellent thermal stability and presents an obvious exothermic signal peak, and has potential application value in the field of energetic materials.
[0072] Table 2 shows the impact sensitivity and calculated theoretical detonation performance of the energetic material EPAF-9 prepared according to Example 5. It can be seen from the table that the energetic material EPAF-9 exhibits low sensitivity and very good energetic characteristics. Compared with the prior art, the energetic material EPAF-9 produced by the preparation method of the present invention has significant improvements in the main detonation performance, which is due to the excellent performance of the reactants themselves and the effective improvement of the relevant preparation process.
[0073] Table 2. Impact sensitivity and calculated theoretical detonation performance of energetic material EPAF-9 in Example 5
[0074]
[0075] Example 6
[0076] 2.3 g 3,6-dichloro-1,2,4,5-tetrazine (15.0 mmol) and 2.4 g triaminoguanidine NTO salt (10.0 mmol) were weighed into a 250 mL two-necked bottle, 50 mL mesitylene and 10 mL N, N-diisopropylethylamine (DIPEA) were added, and the mixed solution was ultrasonicated for a period of time; under nitrogen protection, the reaction was stirred in an oil bath at 150 ° C for 2 days, and the product was filtered; washed with dichloromethane, ethanol and purified water respectively, and vacuum dried at 80 ° C overnight to obtain a porous aromatic framework EPAF-9 material with a yield of 82.0%.
[0077] Example 7
[0078] 2.3 g 3,6-dichloro-1,2,4,5-tetrazine (15.0 mmol) and 2.4 g triaminoguanidine NTO salt (10.0 mmol) were weighed into a 250 mL two-necked bottle, 50 mL mesitylene and 10 mL N, N-diisopropylethylamine (DIPEA) were added, and the mixed solution was ultrasonicated for a period of time; under nitrogen protection, the reaction was stirred in an oil bath at 180°C for 3 days, and the product was filtered; it was washed with dichloromethane, ethanol and purified water respectively, and vacuum dried at 80°C overnight to obtain a porous aromatic framework EPAF-9 material with a yield of 86.0%.
[0079] Example 8
[0080] 4.6 g 3,6-dichloro-1,2,4,5-tetrazine (30.0 mmol) and 4.8 g triaminoguanidine NTO salt (20.0 mmol) were weighed into a 250 mL two-necked bottle, 50 mL mesitylene and 10 mL N, N-diisopropylethylamine (DIPEA) were added, and the mixed solution was ultrasonicated for a period of time; under nitrogen protection, the reaction was stirred in an oil bath at 150 ° C for 2 days, and the product was filtered; washed with dichloromethane, ethanol and purified water respectively, and vacuum dried at 80 ° C overnight to obtain a porous aromatic framework EPAF-9 material with a yield of 81.0%.
[0081] The aromatic building blocks have rich structural types and good chemical reaction activity. By designing the structural units and modifying the PAFs skeleton, the PAFs structure and pore properties can be regulated, thereby showing different performances for application in various fields. Therefore, the design and synthesis of new porous aromatic skeleton energetic (energetic porous aromatic frameworks, EPAFs) materials can provide technical and theoretical reserves for the future development of energetic materials and porous material chemistry. The EPAFs materials provided by the present invention have a variety of high-porosity structures and ultra-high chemical stability, and can withstand strong acids, strong bases, solvents, heat, humidity and other harsh conditions. The improved preparation process is simpler and easier to operate, and can more conveniently and quickly obtain energetic materials that meet the purity standards. The yield is in line with expectations and can meet the actual requirements of industrial production. In addition, the synthesized materials have significantly improved Hanergy properties and have great potential application value.
[0082] The specific description above further illustrates the purpose, technical solutions and beneficial effects of the invention in detail. It should be understood that the above is only a specific embodiment of the present invention and is not intended to limit the scope of protection of the present invention. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention should be included in the scope of protection of the present invention.
Claims
1. A method for preparing a porous aromatic skeleton energetic material based on tetrazine rings and guanidine salts, wherein the porous aromatic skeleton energetic material is formed by polymerization of tetrazine rings and guanidine salts, characterized in that: The specific steps include: S1: weighing a certain amount of tetrazine ring and guanidine salt into a double-necked bottle, adding a solvent and N,N-diisopropylethylamine to obtain a mixed solution, and subjecting the mixed solution to ultrasonic treatment; S2: Under nitrogen protection, in an oil bath at 60-180° C., stirring the mixed solution obtained in S1 after ultrasonic treatment for 2-4 days, and filtering the obtained product; S3: washing and drying the product obtained by filtration in S2 to obtain a porous aromatic skeleton material.
2. The preparation method according to claim 1, characterized in that: The tetrazine ring in S1 is 3,6-dichloro-1,2,4,5-tetrazine; the guanidine salt is triaminoguanidine hydrochloride or triaminoguanidine NTO salt.
3. The preparation method according to claim 2, characterized in that: The guanidine salt is triaminoguanidine hydrochloride, and the mass ratio of 3,6-dichloro-1,2,4,5-tetrazine to triaminoguanidine hydrochloride is 23:14; or, The guanidine salt is triaminoguanidine NTO salt, and the mass ratio of the 3,6-dichloro-1,2,4,5-tetrazine to triaminoguanidine NTO salt is 23:
24.
4. The preparation method according to any one of claims 1 to 3, characterized in that: The solvent in S1 is at least one of toluene, mesitylene, o-dichlorobenzene or N,N-dimethylacetamide.
5. The preparation method according to claim 4, characterized in that: The solvent in S1 is mesitylene, and in the mixed solution, the volume ratio of mesitylene to N,N-diisopropylethylamine is 5:
1.
6. The preparation method according to any one of claims 1 to 3, characterized in that: The washing and drying treatment of the product obtained by filtration in S2 in S3 specifically includes: The product obtained by filtering in S2 was washed with dichloromethane, ethanol and purified water in sequence, and dried under vacuum at 80° C. overnight.
7. A porous aromatic framework energetic material based on tetrazine rings and guanidine salts, characterized in that: The porous aromatic skeleton energetic material is EPAF-8, and its specific structure is as follows:
8. A porous aromatic framework energetic material based on tetrazine rings and guanidine salts, characterized in that: The porous aromatic skeleton energetic material is EPAF-9, and its specific structure is as follows:
9. The porous aromatic skeleton energetic material according to claim 7 or 8, characterized in that: The porous aromatic skeleton energetic material of tetrazine rings and guanidine salts is prepared by the preparation method according to any one of claims 1-6.
10. Use of the porous aromatic skeleton energetic material based on tetrazine ring and guanidine salt according to claim 8 or 9 in the field of energetic materials.
Citation Information
Patent Citations
Porous aromatic skeleton EPAF-4 material and NTO composite salt energetic material and preparation methods
CN113278162A
Porous aromatic framework EPAF-5 material and NTO@EPAF-5 composite salt energetic material, and preparation methods thereof
CN113444246A
Porous aromatic framework EPAF-1 material, CL-20@EPAF-1 composite energetic material and preparation method
CN113501955A
Porous aromatic skeleton EPAF-3 material and NTO@ EPAF-3 composite energetic material and preparation method thereof
CN113527607A
Energetic compounds and compositions
US20170226270A1