Yarn-dyed fabric post-treatment textile auxiliary agent and preparation process thereof
By using specific composition textile additives and finishing processes in colored fabrics, a protective film is formed and double-sided opposite-sex finishing is achieved, which solves the problem that fabric friction is prone to hairballs and water pollution, and improves the smoothness and comfort of the fabric. Spend.
Patent Information
- Application Number
- CN202411402112.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-10-09
- Publication Date
- 2024-11-15
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Colored fabrics are prone to hairballs during wearing and cleaning, resulting in a decrease in aesthetics and comfort. The use of chemical dyes during printing and dyeing leads to water pollution, and the waterproofing and finishing of the inner layer of the fabric causes the wearer to sweat and feel uncomfortable.
Using a colored fabric post-treatment textile auxiliary agent, consisting of penetrating agent, emulsifier, dispersing agent, anionic surfactant, stabilizer, antioxidant, finishing agent, crosslinking agent and thickening agent, through anionic aqueous polyurethane The finishing agent forms a protective film, and the single-sided waterproof and stain-proof finish is carried out by screen printing to achieve double-sided opposite-sex finishing.
Reduce fiber friction, improve fabric smoothness and anti-fouling resistance, avoid water pollution, maintain the hydrophilicity of the inner layer of the fabric, and improve wear comfort.
Smart Images

Figure FT_1 
Figure FT_2 
Figure FT_3
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of yarn-dyed fabric technology, in particular to a yarn-dyed fabric post-treatment textile auxiliary agent and a preparation process thereof. Background Art
[0002] Yarn-dyed fabric is a kind of fabric woven with dyed yarn, which has the characteristics of rich colors, various patterns and comfortable feel. The post-processing of yarn-dyed fabric refers to a series of processing on the yarn-dyed fabric after it is woven to improve its appearance, feel, performance and other aspects.
[0003] The processing of yarn-dyed fabrics mainly includes the following aspects: 1. Desizing: Remove the sizing on the fabric to make the fabric softer and more breathable.
[0004] 2. Scouring: Remove impurities and pigments on the fabric to make the fabric whiter and cleaner.
[0005] 3. Bleaching: Make the fabric whiter and brighter.
[0006] 4. Dyeing: Make the fabric more vivid and rich in color.
[0007] 5. Printing: Print various patterns and designs on the fabric to make the fabric more beautiful and fashionable.
[0008] 6. Finishing: The fabric is treated with shaping, anti-wrinkle, waterproofing, anti-static and other treatments to give the fabric better performance and feel.
[0009] The post-processing of yarn-dyed fabrics is a very important link in the production process of yarn-dyed fabrics, which directly affects the quality and added value of the fabrics. Therefore, when post-processing yarn-dyed fabrics, it is necessary to select appropriate processes and equipment according to the characteristics and uses of the fabrics to ensure the effect and quality of the post-processing.
[0010] Current problems: 1. During wearing and washing, the surface of textiles is prone to produce pilling due to friction, which reduces the appearance and comfort, and thus affects its performance; 2. The use of various chemical dyes and auxiliaries in the printing and dyeing process leads to serious water pollution, energy waste, air pollution and other environmental problems; 3. The waterproof finishing of textiles is usually achieved by dipping and padding waterproofing agents. This finishing method makes both sides of the fabric waterproof. When used for close-fitting clothing such as T-shirts and shirts, the inner layer of the fabric does not absorb moisture, causing discomfort to the wearer when sweating. Therefore, a double-sided anisotropic finishing technology is proposed. Summary of the invention
[0011] In view of the deficiencies in the prior art, the present invention provides a textile auxiliary agent for post-treatment of yarn-dyed fabrics and a preparation process thereof, which solves the problems of hair balls easily generated on the surface of textiles due to friction, energy waste and air pollution, and discomfort caused by the wearer's sweating caused by the inner layer of the fabric not absorbing moisture.
[0012] In order to achieve that the glass powder can maintain a dehumidified state for a long time and has the characteristics of high dispersion performance, the present invention provides the following technical solution: a textile auxiliary agent for post-treatment of yarn-dyed fabrics, composed of the following raw materials in the following mass proportions: Penetrant 10-30%, emulsifier 10-15%, dispersant 2-5%, anionic surfactant 10-15%, stabilizer 1-5%, antioxidant 1-3%, finishing agent 5-10%, cross-linking agent 1-3% and thickener 5-10%, defoamer 0.5-1%, deionized water to 100%; The finishing agent, crosslinking agent and thickener are the main raw materials of post-treatment printing and dyeing auxiliaries. The finishing agent is anionic waterborne polyurethane, with polyester polyol, polyether polyol and diphenylmethane diisocyanate as raw materials, dimethylol propionic acid as a hydrophilic chain extender, the crosslinking agent is methyltriethoxysilane, and the thickener is associative polyurethane.
[0013] Preferably, the preparation conditions of the finishing agent are: the mass fraction of dimethylolpropionic acid is 5%; the mass concentration of the finishing agent is 60g / L, the pH of the finishing solution is 6-7, the baking temperature is 150°C, and the baking time is 3min.
[0014] Preferably, the preparation method of the finishing agent is as follows: add dehydrated polyester polyol and diphenylmethane diisocyanate in a flask in an oil bath at 50°C, heat to 70°C, and react for 2h; add polyether polyol and continue to react for 1h; add measured dimethylol propionic acid and solvent, heat to 80°C, and react for 2h; cool to 45°C in a cold water bath, add solvent and then add deionized water after 30s for high-speed emulsification; when the emulsion can be dissolved in water by itself, slowly add ethylenediamine aqueous solution within 1min, and continue to stir at a low speed for 30min after the addition is completed to obtain a water-based polyurethane finishing agent.
[0015] Preferably, the penetrant is nonylphenol polyoxyethylene ether, the emulsifier is sorbitan oleate, the dispersant is sodium polyacrylate, the anionic surfactant is fatty alcohol polyoxyethylene ether, the stabilizer is polyvinyl alcohol, the antioxidant is 2,6-di-tert-butyl-p-cresol, and the defoamer is a silicone defoamer.
[0016] Preferably, the post-treatment printing and dyeing auxiliary agent is selected from 70g / L of finishing agent, 15% of associative polyurethane thickener (total mass of finishing liquid) and 10g / L of cross-linking agent, baked at 150-170°C for 90s, and the fabric is subjected to single-sided waterproof and antifouling finishing by screen printing.
[0017] Preferably, the preparation process of a textile auxiliary agent for post-treatment of a yarn-dyed fabric as claimed in any one of claims 1 to 5 is characterized in that it comprises the following steps: S1: Add deionized water into a stirring kettle under stirring conditions, slowly add thickener, heat to 60-80°C, stir at a stirring speed of 100-150rpm and a pressure of 0.2-0.4MPa until completely dissolved; S2: After the thickener solution is cooled to 40-50°C, gradually add the finishing agent and continue to stir evenly at a stirring speed of 100-150rpm and a pressure of 0.2-0.4MPa; S3: While stirring, add the cross-linking agent, stir evenly, and then increase the temperature to 150-170°C and bake for reaction for 90 seconds; S4; pulverizing and granulating: After cooling to room temperature, pulverizing and granulating, passing through a 200 mesh sieve, to obtain a mixed powder, S5: The penetrant, emulsifier, anionic surfactant, dispersant, stabilizer, defoamer and mixed powder are fully mixed at a stirring speed of 100-150 rpm; S6: After the solution is cooled naturally, an antioxidant and N,N-dimethylacetamide are added, and then triethylamine is added. After reacting for 30 seconds, deionized water is added for high-speed emulsification, and then the solution is filtered to remove insoluble matter and impurities and the pH value is adjusted; S7: After testing the viscosity, pH value, solid content and other indicators of the final product, package it and store it at 8-20℃.
[0018] Preferably, the fabric is cotton fabric.
[0019] Preferably, when used, the textile auxiliary agent is made into a 20-40 g / L aqueous solution, the fabric is immersed in the prepared solution, dipped and rolled (liquid carrying rate 60%-75%), and baked at 150° C. for 3 minutes for process finishing.
[0020] Compared with the prior art, the present invention provides a textile auxiliary agent for post-treatment of yarn-dyed fabrics and a preparation process thereof, which has the following beneficial effects: 1. Use anionic water-based polyurethane finishing agent, polyester polyol, polyether polyol and diphenylmethane diisocyanate as raw materials, dimethylol propionic acid as hydrophilic chain extender, and use a certain amount of anionic water-based polyurethane finishing agent. It can better adhere to the surface of the fabric and form a protective film, thereby increasing the smoothness and elasticity of the fabric, reducing the friction between fibers, and improving the fabric's anti-pilling and anti-pilling properties.
[0021] 2. Post-processing printing and dyeing auxiliaries include finishing agents, associative polyurethane thickeners and cross-linking agents. The fabric is treated with single-sided waterproof and anti-fouling finishing by screen printing. The double-sided heterosexual dyeing and finishing gives the two sides of the fabric different functions. The inner layer of the same fabric is treated with hydrophilic finishing, and the outer layer is treated with waterproof finishing, that is, waterproof / hydrophilic heterogeneous finishing, which can not only protect against external stains, but also maintain the hydrophilicity of the close-fitting fabric layer, thereby improving wearing comfort. BRIEF DESCRIPTION OF THE DRAWINGS
[0022] Figure 1 is a particle size analysis diagram of the emulsion of the present invention; Figure 2 This is an infrared spectrum analysis diagram of the adhesive film of the present invention; Figure 3 It is the heat resistance analysis diagram of the adhesive film of the present invention. DETAILED DESCRIPTION
[0023] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention. Embodiment 1:
[0024] A textile auxiliary agent for post-treatment of yarn-dyed fabrics, characterized in that it is composed of the following raw materials in the following mass proportions: Penetrant 10-30%, emulsifier 10-15%, dispersant 2-5%, anionic surfactant 10-15%, stabilizer 1-5%, antioxidant 1-3%, finishing agent 5-10%, cross-linking agent 1-3% and thickener 5-10%, defoamer 0.5-1%, deionized water to 100%; The finishing agent, crosslinking agent and thickener are the main raw materials of post-processing printing and dyeing auxiliaries. The finishing agent is an anionic waterborne polyurethane, with polyester polyol, polyether polyol and diphenylmethane diisocyanate as raw materials, dimethylol propionic acid as a hydrophilic chain extender, the crosslinking agent is methyltriethoxysilane, and the thickener is an associative polyurethane. The preparation conditions of the finishing agent are: the mass fraction of dimethylol propionic acid is 5%; the mass concentration of the finishing agent is 60g / L, the pH of the finishing liquid is 6-7, the baking temperature is 150°C, and the baking time is 3min.
[0025] Post-processing printing and dyeing auxiliaries include finishing agents, associative polyurethane thickeners and cross-linking agents. The fabric is treated with single-sided waterproof and anti-fouling finishing by screen printing. The double-sided heterosexual dyeing and finishing gives the two sides of the fabric different functions. The inner layer of the same fabric is treated with hydrophilic finishing and the outer layer is treated with waterproof finishing, that is, waterproof / hydrophilic heterogeneous finishing, which can not only protect against external stains, but also maintain the hydrophilicity of the close-fitting fabric layer, thereby improving wearing comfort.
[0026] The preparation method of the finishing agent is as follows: adding dehydrated polyester polyol and diphenylmethane diisocyanate in a flask in an oil bath at 50°C, heating to 70°C, and reacting for 2h; adding polyether polyol and continuing the reaction for 1h; adding measured dimethylol propionic acid and solvent, heating to 80°C, and reacting for 2h; cooling to 45°C in a cold water bath, adding solvent and then adding deionized water after 30s for high-speed emulsification; when the emulsion can be dissolved in water by itself, slowly adding ethylenediamine aqueous solution within 1min, and continuing to stir at a low speed for 30min after the addition is completed, to obtain a water-based polyurethane finishing agent.
[0027] Anionic water-based polyurethane finishing agent is used, with polyester polyol, polyether polyol and diphenylmethane diisocyanate as raw materials, dimethylol propionic acid as hydrophilic chain extender, and a certain amount of anionic water-based polyurethane finishing agent. It can better adhere to the surface of the fabric to form a protective film, thereby increasing the smoothness and elasticity of the fabric, reducing the friction between fibers, and improving the fabric's anti-pilling and anti-pilling properties.
[0028] The penetrant is nonylphenol polyoxyethylene ether, the emulsifier is sorbitan oleate, the dispersant is sodium polyacrylate, the anionic surfactant is fatty alcohol polyoxyethylene ether, the stabilizer is polyvinyl alcohol, the antioxidant is 2,6-di-tert-butyl-p-cresol, and the defoamer is an organosilicon defoamer.
[0029] The post-treatment printing and dyeing auxiliary agent is selected from finishing agent 70g / L, associative polyurethane thickener 15% (total weight of finishing liquid) and cross-linking agent 10g / L, baked at 150-170℃ for 90s, and the single-sided waterproof and antifouling finishing of the fabric is carried out by screen printing.
[0030] A process for preparing a textile auxiliary agent for post-treatment of yarn-dyed fabrics according to any one of claims 1 to 5, characterized in that it comprises the following steps: S1: Add deionized water into a stirring kettle under stirring conditions, slowly add thickener, heat to 60-80°C, stir at a stirring speed of 100-150rpm and a pressure of 0.2-0.4MPa until completely dissolved; S2: After the thickener solution is cooled to 40-50°C, gradually add the finishing agent and continue to stir evenly at a stirring speed of 100-150rpm and a pressure of 0.2-0.4MPa; S3: While stirring, add the cross-linking agent, stir evenly, and then increase the temperature to 150-170°C and bake for reaction for 90 seconds; S4; pulverizing and granulating: After cooling to room temperature, pulverizing and granulating, passing through a 200 mesh sieve, to obtain a mixed powder, S5: The penetrant, emulsifier, anionic surfactant, dispersant, stabilizer, defoamer and mixed powder are fully mixed at a stirring speed of 100-150 rpm; S6: After the solution is cooled naturally, an antioxidant and N,N-dimethylacetamide are added, and then triethylamine is added. After reacting for 30 seconds, deionized water is added for high-speed emulsification, and then the solution is filtered to remove insoluble matter and impurities and the pH value is adjusted; S7: After testing the viscosity, pH value, solid content and other indicators of the final product, the final product is packaged and stored at 8-20° C. The fabric is cotton fabric.
[0031] When in use, the textile auxiliaries are made into a 20-40g / L aqueous solution, the fabric is immersed in the prepared solution, dipped and rolled (liquid carrying rate 60%-75%), and baked at 150°C for 3 minutes for process finishing. Embodiment 2:
[0032] Fabric performance testing 1. Performance of emulsion (1) Centrifugal stability Take 5 mL of the emulsion into a 10 mL centrifuge tube, centrifuge at 3000 r / min for 15 min, and observe the stability of the emulsion.
[0033] (2) Viscosity Add an appropriate amount of waterborne polyurethane emulsion to a 250 mL beaker and keep the temperature at 25°C. Select an appropriate rotor and set the appropriate speed to read the viscosity value.
[0034] (3) Particle size analysis, reference Figure 1 Heat the emulsion in water at 60°C for 30 min and stir to fully disperse it. Take 1 mL of the emulsion in a 100 mL measuring cylinder and add deionized water to dilute it to 100 mL. Use a nanoparticle size and Zeta potential analyzer to test the emulsion particle size.
[0035] 2. Film performance Pour the emulsion into a polytetrafluoroethylene mold, let it stand in a ventilated place for 24 hours, then vacuum dry it for 24 hours, take it out and let it stand to room temperature.
[0036] (1) Water absorption Weigh a film with a mass of m1, soak it in deionized water for 24 hours, take it out and wipe off the surface moisture, weigh its mass as m2, and calculate the water absorption rate according to the formula.
[0037] Water absorption rate = (m2-m1) / m1 × 100% (2) Contact angle The water contact angle of the prepared film was tested using a JY-82C video contact angle tester. Three different positions of each film were measured and the average value was taken.
[0038] (3) Infrared spectroscopy analysis, reference Figure 2 The structure was characterized by a Nicolet iS20 infrared spectrometer.
[0039] (4) TG and DTG analysis, reference Figure 3 The heat resistance of the film was tested using a TG209 F3 Tarsus thermogravimetric analyzer in a nitrogen atmosphere with a heating rate of 10°C / min and a heating range of 30 to 600°C.
[0040] 3. Fabric performance (1) Scanning electron microscopy The surface morphology of the fabrics was observed using a Sigma 300 scanning electron microscope.
[0041] (2) Anti-pilling performance The pilling resistance of fabrics is tested according to GB / T4802.1-1997 "Textile Fabric Pilling Test Method with Pilling Box".
[0042] (3) Feel Use the Smart Style Tester to test the softness, stiffness and smoothness of fabrics.
[0043]
[0044] Embodiment three: Finishing process Finishing agent 30-110 g / L, thickener 5%-20%, cross-linking agent 0-20 g / L, baking temperature 110-190℃, baking time 90s.
[0045] When the amount of finishing agent is 80g / L, the effect of the amount of thickener on the moisture resistance and stain resistance of the treated surface of the fabric and the hygroscopicity of the untreated surface is investigated;
[0046] From the perspective of finishing effect and cost, the appropriate dosage of thickener is determined to be 15% (total mass of finishing liquid).
[0047] 2. The dosage of thickener is 15%, the baking process temperature is 170℃, and the time is 90s. Explore the dosage of finishing agent Impact on finishing effect;
[0048] The hygroscopicity of the untreated surface of the fabric does not change with the amount of finishing agent used. Therefore, the appropriate amount of finishing agent is 70g / L.
[0049] In order to improve the washing resistance of the finishing effect, it is necessary to use a cross-linking agent in combination, using 15% thickener, 170g / L finishing agent, and baking at 170℃ for 90s to explore the effect of the amount of cross-linking agent on the washing resistance of the finishing effect;
[0050] Since the surface tension of the cross-linking agent is higher than that of the finishing agent, a too high ratio will affect the protective effect on corn oil. Therefore, the appropriate amount of cross-linking agent is determined to be 10g / L.
[0051] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.
Claims
1. A textile auxiliary agent for post-treatment of yarn-dyed fabrics, characterized in that: It is composed of the following raw materials in the following mass proportions: Penetrant 10-30%, emulsifier 10-15%, dispersant 2-5%, anionic surfactant 10-15%, stabilizer 1-5%, antioxidant 1-3%, finishing agent 5-10%, cross-linking agent 1-3% and thickener 5-10%, defoamer 0.5-1%, deionized water to 100%; The finishing agent, crosslinking agent and thickener are the main raw materials of post-treatment printing and dyeing auxiliaries. The finishing agent is anionic waterborne polyurethane, with polyester polyol, polyether polyol and diphenylmethane diisocyanate as raw materials, dimethylol propionic acid as a hydrophilic chain extender, the crosslinking agent is methyltriethoxysilane, and the thickener is associative polyurethane.
2. A textile auxiliary agent for post-treatment of yarn-dyed fabrics according to claim 1, characterized in that: The preparation conditions of the finishing agent are as follows: the mass fraction of dimethylol propionic acid is 5%; the mass concentration of the finishing agent is 60 g / L, the pH value of the finishing solution is 6-7, the baking temperature is 150° C., and the baking time is 3 min.
3. A textile auxiliary agent for post-treatment of yarn-dyed fabrics according to claim 1, wherein the preparation method of the finishing agent is as follows: add dehydrated polyester polyol and diphenylmethane diisocyanate in a flask in an oil bath at 50°C, heat to 70°C, and react for 2 hours; add polyether polyol and continue to react for 1 hour; add measured dimethylol propionic acid and solvent, heat to 80°C, and react for 2 hours; cool to 45°C in a cold water bath, add solvent and then add deionized water after 30 seconds for high-speed emulsification; when the emulsion can dissolve in water by itself, slowly add ethylenediamine aqueous solution within 1 minute, and continue to stir at a low speed for 30 minutes after the addition is completed to obtain a water-based polyurethane finishing agent.
4. The textile auxiliary agent for post-treatment of yarn-dyed fabrics according to claim 1, characterized in that: The penetrant is nonylphenol polyoxyethylene ether, the emulsifier is sorbitan oleate, the dispersant is sodium polyacrylate, the anionic surfactant is fatty alcohol polyoxyethylene ether, the stabilizer is polyvinyl alcohol, the antioxidant is 2,6-di-tert-butyl-p-cresol, and the defoamer is an organosilicon defoamer.
5. The textile auxiliary agent for post-treatment of yarn-dyed fabrics according to claim 1, characterized in that: The post-treatment printing and dyeing auxiliary agent is selected from finishing agent 70g / L, associative polyurethane thickener 15% (total weight of finishing liquid) and cross-linking agent 10g / L, baked at 150-170℃ for 90s, and the single-sided waterproof and antifouling finishing of the fabric is carried out by screen printing.
6. A process for preparing a textile auxiliary agent for post-treatment of yarn-dyed fabrics according to any one of claims 1 to 5, characterized in that: The following steps are involved: S1: Add deionized water into a stirring kettle under stirring conditions, slowly add thickener, heat to 60-80°C, stir at a stirring speed of 100-150rpm and a pressure of 0.2-0.4MPa until completely dissolved; S2: After the thickener solution is cooled to 40-50°C, gradually add the finishing agent and continue to stir evenly at a stirring speed of 100-150rpm and a pressure of 0.2-0.4MPa; S3: While stirring, add the cross-linking agent, stir evenly, and then increase the temperature to 150-170°C and bake for reaction for 90 seconds; S4; pulverizing and granulating: After cooling to room temperature, pulverizing and granulating, passing through a 200 mesh sieve, to obtain a mixed powder, S5: The penetrant, emulsifier, anionic surfactant, dispersant, stabilizer, defoamer and mixed powder are fully mixed at a stirring speed of 100-150 rpm; S6: After the solution is cooled naturally, an antioxidant and N,N-dimethylacetamide are added, and then triethylamine is added. After reacting for 30 seconds, deionized water is added for high-speed emulsification, and then the solution is filtered to remove insoluble matter and impurities and the pH value is adjusted; S7: After testing the viscosity, pH value, solid content and other indicators of the final product, package it and store it at 8-20℃.
7. The textile auxiliary agent for post-treatment of yarn-dyed fabrics and the preparation process thereof according to claim 1, characterized in that: The fabric is cotton fabric.
8. The use of a textile auxiliary agent for post-treatment of yarn-dyed fabrics as claimed in any one of claims 1 to 6, characterized in that: When in use, the textile auxiliaries are made into a 20-40g / L aqueous solution, the fabric is immersed in the prepared solution, dipped and rolled (liquid carrying rate 60%-75%), and baked at 150°C for 3 minutes for process finishing.
Citation Information
Patent Citations
Preparation technology of soft highly-elastic fabric anti-fluffing anti-pilling finishing agent
CN101302276A
Anti-wrinkling finishing agent of garment fabric
CN104894853A
Preparation method of printing and dyeing auxiliary for leather
CN107905002A
Printing and dyeing auxiliary agent and preparation method thereof
CN109056382A
Anti-pilling overcoat and treatment process thereof
CN109736091A