Array substrate, preparation method thereof and flexible electronic paper display panel

By designing a layered protection structure on the array substrate of the flexible electronic paper display panel, the problems of pixel failure and black line failure in the bent area are solved, and the service life and stability of the equipment are improved.

CN118963035APending Publication Date: 2024-11-15HKC CORP LTD

Patent Information

Application Number
CN202411444537.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-10-16
Publication Date
2024-11-15

AI Technical Summary

Technical Problem

The single pixel failure and black line failure of the flexible electronic paper display panel in the bent area lead to high failure rate and short service life.

Method used

An array substrate is designed, including a flexible substrate, an active switching layer, a protective layer and a pixel electrode layer. The protective layer is divided into a first passivation layer, a spacer layer and a second passivation layer, and a specific recess is provided on the bending area. and raised structure to disperse stress and prevent cracks from forming.

Benefits of technology

It effectively reduces the failure rate of the flexible electronic paper display panel, improves service life, prevents the connection stability of the pixel electrode layer and the active switching layer, and adapts to various bending situations.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118963035A_ABST
    Figure CN118963035A_ABST
Patent Text Reader

Abstract

The invention discloses an array substrate and a preparation method thereof and a flexible electronic paper display panel, the array substrate comprises a flexible substrate, an active switch layer, a protection layer and a pixel electrode layer, the active switch layer, the protection layer and the pixel electrode layer are sequentially deposited on the flexible substrate, and the array substrate comprises a bending area and an unfolding area; the protection layer comprises a first passivation layer, a spacer layer and a second passivation layer, the first passivation layer in the corresponding bending area comprises a plurality of first concave parts and a plurality of first convex parts, the first concave parts and the first convex parts are arranged at intervals, the second passivation layer comprises a plurality of second concave parts and a plurality of second convex parts, and the second concave parts and the second convex parts are arranged at intervals. The second concave parts and the second convex parts are arranged at intervals, the first convex parts are located in the second concave parts, and the second convex parts are located in the first concave parts. Through the design, the failure rate of the flexible electronic paper display panel is reduced, and the service life of the flexible electronic paper display panel is prolonged.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the field of display technology, and in particular to an array substrate and a preparation method thereof, and a flexible electronic paper display panel. Background Art

[0002] With the development of digital technology, more and more display devices have entered people's lives, such as electronic paper (EP) display panels. Since electronic paper display panels can maintain display for a long time in the case of power failure, and have the advantages of lightness, thinness, low power consumption, and simple process, they are becoming more and more popular.

[0003] The current flexible electronic paper display panels can be rolled up and folded at will by using a flexible substrate made of polyimide film. However, during use, individual pixels in the bending area of ​​the flexible electronic paper display panel may fail to participate in the display. Even worse, black line failures may appear in the length direction of the bending area. Summary of the invention

[0004] The purpose of the present application is to provide an array substrate and a preparation method thereof and a flexible electronic paper display panel, so as to reduce the failure rate of the flexible electronic paper display panel and increase the service life of the flexible electronic paper display panel.

[0005] The present application discloses an array substrate for use in a flexible electronic paper display panel; the array substrate comprises a flexible substrate, an active switch layer, a protective layer and a pixel electrode layer, the active switch layer, the protective layer and the pixel electrode layer are sequentially deposited on the flexible substrate, and the array substrate comprises a bending region and an unfolding region; The protective layer includes a first passivation layer, a spacer layer and a second passivation layer, the first passivation layer, the spacer layer and the second passivation layer are sequentially deposited on the active switch layer, the spacer layer is at least located between the first passivation layer and the second passivation layer in the bending area, the first passivation layer corresponding to the bending area includes a plurality of first recessed portions and a plurality of first protruding portions, the first recessed portions and the first protruding portions are arranged at intervals, the second passivation layer includes a plurality of second recessed portions and a plurality of second protruding portions, the second recessed portions and the second protruding portions are arranged at intervals, the first protruding portion is located in the second recessed portion, and the second protruding portion is located in the first recessed portion.

[0006] Optionally, in the protective layer in the expansion area, the first passivation layer and the second passivation layer are in contact with each other; in the protective layer only in the bending area, the first passivation layer includes a plurality of first recessed portions and a plurality of first raised portions, the first recessed portions and the first raised portions are arranged at intervals, and the second passivation layer includes a plurality of second recessed portions and a plurality of second raised portions, the second recessed portions and the second raised portions are arranged at intervals, the first raised portion is located in the second recessed portion, and the second raised portion is located in the first recessed portion, and the spacing layer is only located between the first raised portion and the second recessed portion and between the first recessed portion and the second raised portion in the bending area.

[0007] Optionally, in the protective layer in the expansion area, the first passivation layer includes a plurality of first recessed portions and a plurality of first raised portions, the first recessed portions and the first raised portions are spaced apart, the second passivation layer includes a plurality of second recessed portions and a plurality of second raised portions, the second recessed portions and the second raised portions are spaced apart, the first raised portion is located in the second recessed portion, the second raised portion is located in the first recessed portion, and the spacing layer is also located between the first raised portion and the second recessed portion and between the first recessed portion and the second raised portion in the expansion area.

[0008] Optionally, the length direction of the bending area is the first direction, and the width direction of the bending area is the second direction; Along the first direction, the first protruding portion is adjacent to the first concave portion on both upper and lower sides, and the first concave portion is adjacent to the first protruding portion on both upper and lower sides; Along the second direction, both the first protruding portion and the first concave portion are adjacent to each other on both the left and right sides of the first protruding portion, and both the first protruding portion and the first concave portion are adjacent to each other on both the left and right sides of the first concave portion.

[0009] Optionally, the length direction of the bending area is the first direction, and the width direction of the bending area is the second direction; Along the second direction, the first protruding portion is adjacent to the first concave portion on both sides thereof, and the first concave portion is adjacent to the first protruding portion on both sides thereof; Along the first direction, the first protrusion is adjacent to the first recessed portion and the first protrusion on both sides above and below, and the first protrusion is located between the first recessed portion and the first protrusion; the first recessed portion and the first protrusion are adjacent to the first recessed portion and the first protrusion on both sides above and below, and the first recessed portion is located between the first recessed portion and the first protrusion.

[0010] Optionally, the array substrate further includes data lines and scan lines, the data lines and the scan lines are arranged on the flexible substrate, and the data lines and the scan lines are arranged in a criss-cross pattern to divide a plurality of pixel unit areas; the active switch layer includes a plurality of active switches, each of the active switches corresponds one-to-one to each of the pixel unit areas; the orthographic projection of the first recessed portion on the flexible substrate covers the orthographic projection of the active switch on the flexible substrate.

[0011] The present application also discloses a method for preparing an array substrate, which is used to prepare the array substrate described above, wherein the array substrate includes a bending area and an unfolding area, and comprises the following steps: forming an active switching layer on the flexible substrate; A first passivation layer is formed on the active switch layer; and a plurality of first recessed portions and a plurality of first raised portions are formed on the first passivation layer in the bending region, wherein the first recessed portions and the first raised portions are arranged at intervals; a spacing layer is formed at least on the first passivation layer in the bending region; and a second passivation layer is formed on the spacing layer, wherein a plurality of second recessed portions and a plurality of second raised portions are formed on a side of the second passivation layer corresponding to the bending region close to the first passivation layer, wherein the second recessed portions and the second raised portions are arranged at intervals, wherein the first raised portion is located in the second recessed portion, and the second raised portion is located in the first recessed portion, so as to form a protective layer; A pixel electrode layer is formed on the protection layer.

[0012] Optionally, a first passivation layer is formed on the active switch layer; and a plurality of first recessed portions and a plurality of first raised portions are formed on the first passivation layer in the bending region, and the first recessed portions and the first raised portions are arranged at intervals; a spacing layer is formed on at least the first passivation layer in the bending region; and a second passivation layer is formed on the spacing layer, and a plurality of second recessed portions and a plurality of second raised portions are formed on a side of the second passivation layer corresponding to the bending region close to the first passivation layer, and the second recessed portions and the second raised portions are arranged at intervals, and the first raised portion is located in the second recessed portion, and the second raised portion is located in the first recessed portion, so that the step of forming a protective layer includes: forming a first passivation layer on the active switching layer; forming a plurality of first recessed portions and a plurality of first raised portions only on the first passivation layer in the bending region, wherein the first recessed portions and the first raised portions are arranged at intervals; forming a spacer layer only on the first passivation layer in the bending region; A second passivation layer is formed on the spacer layer, wherein a plurality of second recessed portions and a plurality of second raised portions are formed on a side of the second passivation layer corresponding to the bending region and close to the first passivation layer, wherein the second recessed portions and the second raised portions are arranged at intervals, the first raised portion is located in the second recessed portion, and the second raised portion is located in the first recessed portion, so as to form a protective layer; Among them, in the protective layer in the development area, the adjacent surfaces of the first passivation layer and the second passivation layer are flush.

[0013] Optionally, a first passivation layer is formed on the active switch layer; and a plurality of first recessed portions and a plurality of first raised portions are formed on the first passivation layer in the bending region, and the first recessed portions and the first raised portions are arranged at intervals; a spacing layer is formed on at least the first passivation layer in the bending region; and a second passivation layer is formed on the spacing layer, and a plurality of second recessed portions and a plurality of second raised portions are formed on a side of the second passivation layer corresponding to the bending region close to the first passivation layer, and the second recessed portions and the second raised portions are arranged at intervals, and the first raised portion is located in the second recessed portion, and the second raised portion is located in the first recessed portion, so that the step of forming a protective layer includes: forming a first passivation layer on the active switching layer; forming a plurality of first recessed portions and a plurality of first raised portions on the first passivation layer in the bending region and the unfolding region, wherein the first recessed portions and the first raised portions are arranged at intervals; forming a spacer layer on the first passivation layer in the bending area and the unfolding area; A second passivation layer is formed on the spacing layer, and a plurality of second recessed portions and a plurality of second raised portions are formed on the second passivation layer corresponding to the bending area and the unfolding area, the second recessed portions and the second raised portions are arranged at intervals, the first raised portion is located in the second recessed portion, and the second raised portion is located in the first recessed portion to form a protective layer.

[0014] The present application also discloses a flexible electronic paper display panel, which includes an electronic paper film layer and the array substrate, wherein the electronic paper film layer is attached to the array substrate.

[0015] Compared with the existing flexible electronic paper display panel solutions, the present application divides the protective layer into a first passivation layer, a spacer layer and a second passivation layer, and arranges a first protrusion and a first recessed portion arranged at intervals on the first passivation layer in the bending area to disperse the stress on the first passivation layer; and also arranges a second protrusion and a second recessed portion arranged at intervals on the second passivation layer in the bending area. It is important that the second protrusion is located in the first recessed portion, and the first protrusion is located in the second recessed portion. In this way, when cracks occur due to excessive stress, they will not appear at the same position of the first passivation layer and the second passivation layer at the same time, so that the entire protective layer will not be completely cracked, thereby not destroying the connection stability between the pixel electrode layer and the active switch layer, so as to reduce the failure rate of the flexible electronic paper display panel and improve the service life of the flexible electronic paper display panel. BRIEF DESCRIPTION OF THE DRAWINGS

[0016] The included drawings are used to provide a further understanding of the embodiments of the present application, which constitute a part of the specification, are used to illustrate the implementation methods of the present application, and together with the text description, explain the principles of the present application. Obviously, the drawings described below are only some embodiments of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without creative work. In the drawings: Figure 1 is a schematic diagram of a flexible electronic paper display panel according to an embodiment of the present application; Figure 2 is a plan view of an array substrate according to a first embodiment of the present application; Figure 3 is a cross-sectional schematic diagram of an array substrate according to a first embodiment of the present application; Figure 4 is a cross-sectional schematic diagram of a pixel unit region in a first embodiment of the present application; Figure 5 is a plan view of a pixel unit area in the first embodiment of the present application; Figure 6 is a plan view schematically showing another arrangement of the first recessed portion and the first raised portion of the first embodiment of the present application; Figure 7 is a schematic diagram of an array substrate according to a second embodiment of the present application; Figure 8 It is a schematic diagram of a process of preparing an array substrate according to an embodiment of the present application; Figure 9a-9b is a schematic diagram of a process of a method for preparing an array substrate according to an embodiment of the present application; Fig.10 It is a schematic diagram of a process of preparing an array substrate according to an embodiment of the present application; Figure 11a-Figure 11b It is a schematic diagram of a process of preparing a method for an array substrate according to an embodiment of the present application.

[0017] Among them, 10, flexible electronic paper display panel; 20, bending area; 21, first direction; 22, second direction; 30, unfolding area; 100, electronic paper film layer; 110, particle layer; 111, partition wall; 112, chamber; 120, common electrode layer; 200, array substrate; 210, flexible substrate; 300, active switch layer; 310, active switch; 400, protective layer; 410, first passivation layer; 411, first recessed portion; 412, first protruding portion; 420, spacing layer; 430, second passivation layer; 431, second recessed portion; 432, second protruding portion; 500, pixel electrode layer; 610, data line; 620, scan line; 630, pixel unit area. DETAILED DESCRIPTION

[0018] It should be understood that the terms used herein, the specific structures and functional details disclosed are only for describing specific embodiments and are representative, but the present application can be implemented in many alternative forms and should not be construed as being limited to only the embodiments described herein.

[0019] In the description of this application, the terms "first" and "second" are used for descriptive purposes only and should not be understood as indicating relative importance or implicitly indicating the number of technical features indicated. Therefore, unless otherwise specified, features defined as "first" and "second" may explicitly or implicitly include one or more of the features; "plurality" means two or more. The term "including" and any variation thereof means non-exclusive inclusion, and one or more other features, integers, steps, operations, units, components and / or combinations thereof may exist or be added.

[0020] In addition, terms indicating orientation or positional relationships, such as “center,” “lateral,” “up,” “down,” “left,” “right,” “vertical,” “horizontal,” “top,” “bottom,” “inside,” and “outside,” are described based on the orientation or relative positional relationships shown in the accompanying drawings and are merely simplified descriptions for the convenience of describing the present application. They do not indicate that the devices or elements referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as limitations on the present application.

[0021] In addition, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be indirectly connected through an intermediate medium, or it can be internally connected between two components. For ordinary technicians in this field, the specific meanings of the above terms in this application can be understood according to specific circumstances.

[0022] The present application is described in detail below with reference to the accompanying drawings and optional embodiments.

[0023] Figure 1 is a schematic diagram of a flexible electronic paper display panel according to an embodiment of the present application, such as Figure 1 As shown, the present application discloses a flexible electronic paper display panel 10 , which includes an electronic paper film layer 100 and an array substrate 200 , wherein the electronic paper film layer 100 is attached to the array substrate 200 .

[0024] The flexible electronic paper display panel 10 can be folded or rolled into a tube when in use.

[0025] The electronic paper film layer 100 includes a particle layer 110 and a common electrode layer 120. The particle layer 110 includes a capsule structure and a microcup structure. The present application is described using the microcup structure. Electrophoretic particles and partition walls 111 are arranged in the particle layer 110. The partition walls 111 form a plurality of chambers 112. The electrophoretic particles are arranged in the chambers 112. One chamber 112 corresponds to one pixel unit area 630.

[0026] The electrophoretic particles include black electrophoretic particles and white capacitor particles, and of course may also include colored electrophoretic particles, such as red electrophoretic particles, blue electrophoretic particles and green electrophoretic particles. The common electrode layer 120 is located on the side of the particle layer 110 away from the array substrate 200. An electric field is formed between the common electrode and the pixel electrode layer 500 on the array substrate 200 to drive the electrophoretic particles to move to display the picture.

[0027] The present application also discloses an array substrate 200, which can be used in the flexible electronic paper display panel 10 described above. For the array substrate 200, the present application provides the following design, which is specifically introduced through several embodiments: Embodiment 1: During the use of the flexible electronic paper display panel 10, the problem of pixels in the pixel unit area 630 failing to participate in the display may occur, and in severe cases, black lines may appear in the length direction of the bending area 20. The electronic paper film layer 100 of the existing electronic paper display panel is covered on the display area of ​​the array substrate 200, and the non-display area at the edge is exposed, so a thicker passivation layer is required to be set on the array substrate 200 to protect the metal wires below. The same is true for the flexible electronic paper display panel 10 of the present application.

[0028] On the flexible electronic paper display panel 10 where the problem occurs, for example, the pixel electrode layer 500 at the position where the black line appears is disconnected from the active switch layer 300 below, and when the flexible electronic paper display panel 10 is bent, it is observed that cracks appear in the thick passivation layer. Therefore, the present application further improves the existing passivation layer. The details are as follows: Figure 2 is a plan view of an array substrate of the first embodiment of the present application, Figure 3 is a cross-sectional schematic diagram of an array substrate of the first embodiment of the present application, Figure 4 is a cross-sectional schematic diagram of a pixel unit region of the first embodiment of the present application, combined with Figures 2 to 4 As shown, the present application discloses an array substrate 200 for use in a flexible electronic paper display panel 10; the array substrate 200 includes a flexible substrate 210, an active switching layer 300, a protective layer 400 and a pixel electrode layer 500, and the active switching layer 300, the protective layer 400 and the pixel electrode layer 500 are sequentially deposited on the flexible substrate 210.

[0029] The array substrate 200 includes a bending area 20 and an unfolding area 30. The exemplary flexible electronic paper display panel 10 can be folded left and right. At this time, the left and right sides of the array substrate 200 are defined as the unfolding area 30 and the middle is defined as the bending area 20. During the folding or unfolding process, the unfolding areas 30 on the left and right sides are close to or away from each other.

[0030] The protection layer 400 includes a first passivation layer 410 , a spacer layer 420 , and a second passivation layer 430 , wherein the spacer layer 420 may be made of polyvinyl chloride.

[0031] The first passivation layer 410 , the spacer layer 420 , and the second passivation layer 430 are sequentially deposited on the active switch layer 300 , and the spacer layer 420 is at least located between the first passivation layer 410 and the second passivation layer 420 in the bending region 20 .

[0032] The first passivation layer 410 corresponding to the bending area 20 includes a plurality of first recessed portions 411 and a plurality of first raised portions 412, and the first recessed portions 411 and the first raised portions 412 are arranged at intervals. The second passivation layer 430 includes a plurality of second recessed portions 431 and a plurality of second raised portions 432, and the second recessed portions 431 and the second raised portions 432 are arranged at intervals. The first raised portion 412 is located in the second recessed portion 431, and the second raised portion 432 is located in the first recessed portion 411.

[0033] In short, the present application changes the existing passivation layer into a three-layer protective layer 400 , and sets a first protrusion 412 and a first recess 411 on the first passivation layer 410 in the bending area 20 , and then sets a second protrusion 432 and a second recess 431 on the corresponding second passivation layer 430 .

[0034] Compared with the existing flexible electronic paper display panel solution, the present application divides the protective layer 400 into a first passivation layer 410, a spacer layer 420 and a second passivation layer 430, and arranges a first protrusion 412 and a first recessed portion 411 arranged at intervals on the first passivation layer 410 of the bending region 20 to disperse the stress on the first passivation layer 410; and also arranges a second protrusion 432 and a second recessed portion 431 arranged at intervals on the second passivation layer 430 of the bending region 20 to disperse the stress on the second passivation layer 430. It is important that the second protrusion 432 is located in the first recessed portion 411, and the first protrusion 412 is located in the second recessed portion 431. In this way, when cracks occur due to excessive stress, they will not appear at the same position of the first passivation layer 410 and the second passivation layer 430 at the same time, so that the entire protection layer 400 will not be completely cracked, thereby not destroying the connection stability of the pixel electrode layer 500 and the active switching layer 300, thereby reducing the failure rate of the flexible electronic paper display panel 10 and improving the service life of the flexible electronic paper display panel.

[0035] Among them, the cross-sectional shape of the first protrusion 412 is a right trapezoid, the cross-sectional shape of the first recessed portion 411 is an inverted trapezoid, the cross-sectional shape of the second protrusion 432 is an inverted trapezoid, and the cross-sectional shape of the second recessed portion 431 is a right trapezoid, thereby further reducing stress concentration.

[0036] In order to enable the flexible electronic paper display panel 10 to be folded according to the user's usage, the bending area 20 is not fixed. Therefore, in this embodiment, a first recessed portion 411 and a first raised portion 412 are also provided on the first passivation layer 410 of the unfolding area 30, and correspondingly, a second recessed portion 431 and a second raised portion 432 are also provided on the second passivation layer 430 of the unfolding area 30. In simple terms, the first recessed portion 411 and the first raised portion 412 are provided on the entire surface of the first passivation layer 410, and the second recessed portion 431 and the second raised portion 432 are also provided on the entire surface of the second passivation layer 430.

[0037] Specifically, in the protective layer 400 of the expansion area 30, the first passivation layer 410 includes a plurality of first recessed portions 411 and a plurality of first raised portions 412, and the first recessed portions 411 and the first raised portions 412 are arranged at intervals, and the second passivation layer 430 includes a plurality of second recessed portions 431 and a plurality of second raised portions 432, and the second recessed portions 431 and the second raised portions 432 are arranged at intervals, the first raised portions 412 are located in the second recessed portions 431, and the second raised portions 432 are located in the first recessed portions 411, and the spacer layer 420 is also located between the first raised portions 412 and the second recessed portions 431 in the expansion area 30, and the spacer layer 420 is also located between the first recessed portions 411 and the second raised portions 432 in the expansion area 30.

[0038] In this way, the flexible electronic paper display panel 10 can be more adaptable to the user's various bending options, thereby further improving the service life of the flexible electronic paper display panel 10, and the first protrusion 412 and the first recessed portion 411 are arranged on the entire first passivation layer 410, and there is no need to use different mask plates for array substrates 200 of different sizes, which can save costs.

[0039] Figure 5 is a plan view of a pixel unit region in the first embodiment of the present application. Figure 5 As shown, when bending, the stress on the first passivation layer 410 will be concentrated on the relatively thick first protrusion 412, and the stress on the second passivation layer 430 will be concentrated on the relatively thick second protrusion 432. Since the first passivation layer 410 is relatively close to the active switch 310 below, the present application also arranges the active switch 310 below the first recessed portion 411. Specifically: The array substrate 200 further includes a first metal layer, a first insulating layer, a semiconductor layer, a second metal layer, and a second insulating layer. The first metal layer, the first insulating layer, the first semiconductor layer, the second metal layer, and the second insulating layer are sequentially deposited on the flexible substrate 210 .

[0040] The array substrate 200 further includes a data line 610 and a scan line 620, which are disposed on the flexible substrate 210, and the data line 610 and the scan line 620 are arranged in a crisscross pattern to divide a plurality of pixel unit regions 630; the active switch layer 300 includes a plurality of active switches 310, and each active switch 310 corresponds to each pixel unit region 630 one by one; and the orthographic projection of the first recessed portion 411 on the flexible substrate 210 covers the orthographic projection of the active switch 310 on the flexible substrate 210.

[0041] In this way, when cracks appear in the first passivation layer 410 due to bending, the cracks will not appear directly above the active switch 310 , thus preventing the active switch 310 from being damaged.

[0042] Exemplarily, the scan line 620 can be set in the first metal layer, the data line 610 can be set in the second metal layer, the gate of the active switch 310 can be set in the first metal layer, the semiconductor structure of the active switch 310 can be set in the semiconductor layer, and the source and drain of the active switch 310 can be set in the second metal layer.

[0043] Furthermore, the length direction of the bending area 20 is the first direction 21, and the width direction of the bending area 20 is the second direction 22; along the first direction 21, the first protrusion 412 is adjacent to the first recessed portion 411 on both sides, and the first protrusion 412 is adjacent to the first recessed portion 411 on both sides.

[0044] Along the second direction 22 , the first protruding portion 412 is adjacent to the first recessed portion 411 on both sides thereof, and the first protruding portion 412 is adjacent to the first recessed portion 411 on both sides thereof.

[0045] In simple terms, the four adjacent upper, lower, left and right portions of the first raised portion 412 are all first recessed portions 411, and the four adjacent upper, lower, left and right portions of the first recessed portion 411 are all first raised portions 412. Correspondingly, the four adjacent upper, lower, left and right portions of the second raised portion 432 are all second recessed portions 431, and the four adjacent upper, lower, left and right portions of the second recessed portion 431 are all second raised portions 432. In this way, it can be ensured that each of the first raised portion 412 and the second raised portion 432 is relatively independent. Even if cracks occur on the first raised portion 412 and the second raised portion 432, the cracks will not be further expanded, thereby avoiding aggravating the display problem of the flexible electronic paper display panel 10.

[0046] Figure 6 is a plan view of another arrangement of the first recessed portion and the first raised portion of the first embodiment of the present application, such as Figure 6 As shown, the length direction of the bending area 20 is the first direction 21, and the width direction of the bending area 20 is the second direction 22; along the second direction 22, the first protrusion 412 is adjacent to the left and right sides thereof with the first recessed portions 411, and the first protrusion 412 is adjacent to the left and right sides thereof with the first recessed portions 411.

[0047] Along the first direction 21, the first recessed portion 411 and the first raised portion 412 are adjacent to the first raised portion 412 on the upper and lower sides, and the first raised portion 412 is located between the first recessed portion 411 and the first raised portion 412; the first recessed portion 411 and the first raised portion 412 are adjacent to the first recessed portion 411 on the upper and lower sides, and the first recessed portion 411 is located between the first recessed portion 411 and the first raised portion 412.

[0048] In simple terms, the boundary line between the first raised portion 412 and the first recessed portion 411 of the previous row is located in the middle of the first raised portion 412 of the current row, or in the middle of the first recessed portion 411, that is, the boundary line between the first raised portion 412 and the first recessed portion 411 of the previous row and the boundary line between the first raised portion 412 and the first recessed portion 411 of the current row are not on the same straight line. In this way, when cracking occurs at the boundary line between the first recessed portion 411 and the first raised portion 412, a longer crack can be avoided, thereby preventing the problem of black lines appearing on the display of the flexible electronic paper display panel 10 after bending.

[0049] Embodiment 2: Figure 7 is a schematic diagram of an array substrate according to a second embodiment of the present application. Figure 7 As shown, different from the first embodiment, in this embodiment, the first protrusion 412 and the first recess 411 are only provided on the first passivation layer 410 in the bending area 20, and no spacing layer 420 is provided between the first passivation layer 410 and the second passivation layer 430 in the unfolding area 30.

[0050] Specifically, in the protective layer 400 of the expansion area 30, the first passivation layer 410 and the second passivation layer 430 are in contact with each other; only in the protective layer 400 within the bending area 20, the first passivation layer 410 includes a plurality of first recessed portions 411 and a plurality of first raised portions 412, and the first recessed portions 411 and the first raised portions 412 are arranged at intervals; the second passivation layer 430 includes a plurality of second recessed portions 431 and a plurality of second raised portions 432, and the second recessed portions 431 and the second raised portions 432 are arranged at intervals, the first raised portion 412 is located in the second recessed portion 431, and the second raised portion 432 is located in the first recessed portion 411; the spacing layer 420 is only located between the first raised portion 412 and the second recessed portion 431 and between the first recessed portion 411 and the second raised portion 432 in the bending area 20.

[0051] Compared with the solution of the first embodiment, in this embodiment, the first protrusion 412 and the first recessed portion 411 are only provided on the first passivation layer 410 in the bending area 20, and the corresponding second passivation layer 430 is also only provided with the second protrusion 432 and the second recessed portion 431 in the bending area 20, so that the fit between the first passivation layer 410 and the second passivation layer 430 in the expansion area 30 is tighter, thereby preventing water vapor from entering the surface from between the first passivation layer 410 and the second passivation layer 430.

[0052] Figure 8 is a schematic flow chart of a method for preparing an array substrate according to an embodiment of the present application. Figure 9a-9b FIG. 1 is a schematic diagram of a process for preparing an array substrate according to an embodiment of the present application. Figure 8-9b As shown, the present application also discloses a method for preparing an array substrate 200, which is used to prepare the array substrate 200 described above, wherein the array substrate 200 includes a bending area 20 and an unfolding area 30, and comprises the following steps: S1: forming an active switching layer on a flexible substrate; S2: forming a first passivation layer on the active switch layer; and forming a plurality of first recessed portions and a plurality of first raised portions on the first passivation layer in the bending region, wherein the first recessed portions and the first raised portions are arranged at intervals; forming a spacing layer at least on the first passivation layer in the bending region; forming a second passivation layer on the spacing layer, wherein a plurality of second recessed portions and a plurality of second raised portions are formed on a side of the second passivation layer corresponding to the bending region close to the first passivation layer, wherein the second recessed portions and the second raised portions are arranged at intervals, wherein the first raised portion is located in the second recessed portion, and the second raised portion is located in the first recessed portion, so as to form a protective layer; S3: forming a pixel electrode layer on the protective layer.

[0053] Compared with the existing flexible electronic paper display panel solution, the present application divides the protective layer 400 into a first passivation layer 410, a spacer layer 420 and a second passivation layer 430, and arranges a first protrusion 412 and a first recessed portion 411 arranged at intervals on the first passivation layer 410 of the bending region 20 to disperse the stress on the first passivation layer 410; and also arranges a second protrusion 432 and a second recessed portion 431 arranged at intervals on the second passivation layer 430 of the bending region 20 to disperse the stress on the second passivation layer 430. It is important that the second protrusion 432 is located in the first recessed portion 411, and the first protrusion 412 is located in the second recessed portion 431. In this way, when cracks occur due to excessive stress, they will not appear at the same position of the first passivation layer 410 and the second passivation layer 430 at the same time, so that the entire protection layer 400 will not be completely cracked, thereby not destroying the connection stability of the pixel electrode layer 500 and the active switching layer 300, thereby reducing the failure rate of the flexible electronic paper display panel 10 and improving the service life of the flexible electronic paper display panel.

[0054] It is possible that the first protrusion 412 and the first recessed portion 411 are only provided on the first passivation layer 410 of the bending region 20, and the second protrusion 432 and the second recessed portion 431 are also provided on the bending region 20 corresponding to the second passivation layer 430. Specifically, step S2: forming a first passivation layer on the active switch layer; and forming a plurality of first recessed portions and a plurality of first protrusions on the first passivation layer in the bending region, and the first recessed portions and the first protrusions are arranged at intervals; forming a spacing layer at least on the first passivation layer in the bending region; forming a second passivation layer on the spacing layer, and a plurality of second recessed portions and a plurality of second protrusions are formed on the side of the second passivation layer corresponding to the bending region close to the first passivation layer, and the second recessed portions and the second protrusions are arranged at intervals, and the first protrusion is located in the second recessed portion, and the second protrusion is located in the first recessed portion, so as to form a protective layer including: S211: forming a first passivation layer on the active switching layer; S212: forming a plurality of first recessed portions and a plurality of first raised portions only on the first passivation layer in the bending region, wherein the first recessed portions and the first raised portions are arranged at intervals; S213: forming a spacer layer only on the first passivation layer in the bending area; S214: forming a second passivation layer on the spacer layer, wherein a plurality of second recessed portions and a plurality of second raised portions are formed on a side of the second passivation layer corresponding to the bending region and close to the first passivation layer, wherein the second recessed portions and the second raised portions are arranged at intervals, the first raised portion is located in the second recessed portion, and the second raised portion is located in the first recessed portion, so as to form a protective layer; Among them, in the protection layer 400 of the expansion area 30, the first passivation layer 410 and the second passivation layer 430 are attached to each other. After the first recessed portion 411 is etched, the first convex portion 412 is directly formed in the unetched area, and the spacer layer 420 is uniformly arranged on the first passivation layer 410. When the second passivation layer 430 is arranged, the second recessed portion 431 can be directly formed at the position corresponding to the first convex portion 412, and the second convex portion 432 can be directly formed at the position corresponding to the first recessed portion 411. The second passivation layer 430 is flush with the surface away from the first passivation layer 410.

[0055] This makes the first passivation layer 410 and the second passivation layer 430 in the development area 30 more closely attached to each other, thereby preventing water vapor from entering the surface from between the first passivation layer 410 and the second passivation layer 430 .

[0056] Fig.10 is a schematic flow chart of a method for preparing an array substrate according to an embodiment of the present application. Figure 11a-Figure 11b FIG. 1 is a schematic diagram of a process for preparing an array substrate according to an embodiment of the present application. Figure 10-11b As shown, of course, the first protrusion 412 and the first recessed portion 411 can also be set on the entire surface of the first passivation layer 410, and the second protrusion 432 and the second recessed portion 431 can be set on the entire surface of the second passivation layer 430. Specifically, the step S2: forming a first passivation layer on the active switch layer; and forming a plurality of first recessed portions and a plurality of first protrusions on the first passivation layer in the bending area, and the first recessed portions and the first protrusions are arranged at intervals; forming a spacing layer at least on the first passivation layer in the bending area; forming a second passivation layer on the spacing layer, and a plurality of second recessed portions and a plurality of second protrusions are formed on the side of the second passivation layer corresponding to the bending area close to the first passivation layer, and the second recessed portions and the second protrusions are arranged at intervals, the first protrusion is located in the second recessed portion, and the second protrusion is located in the first recessed portion, so as to form a protective layer including: S221: forming a first passivation layer on the active switching layer; S222: forming a plurality of first recessed portions and a plurality of first raised portions on the first passivation layer in the bending area and the unfolding area, wherein the first recessed portions and the first raised portions are arranged at intervals; S223: forming a spacer layer on the first passivation layer in the bending area and the unfolding area; S224: A second passivation layer is formed on the spacing layer, and a plurality of second recessed portions and a plurality of second raised portions are formed on a side of the second passivation layer close to the first passivation layer corresponding to the bending area and the unfolding area, and the second recessed portions and the second raised portions are arranged at intervals, and the first raised portion is located in the second recessed portion, and the second raised portion is located in the first recessed portion, so as to form a protective layer.

[0057] Compared with only setting the first protrusion 412 and the first recessed portion 411 on the first passivation layer 410 in the bending area 20, the second protrusion 432 and the second recessed portion 431 are also set on the bending area 20 of the corresponding second passivation layer 430; the first protrusion 412 and the first recessed portion 411 are set on the entire surface of the first passivation layer 410, and the second protrusion 432 and the second recessed portion 431 are set on the entire surface of the second passivation layer 430, so that the flexible electronic paper display panel 10 can be more adaptable to the user's various bending options, thereby further improving the service life of the flexible electronic paper display panel 10, and the first protrusion 412 and the first recessed portion 411 are set on the entire surface of the first passivation layer 410, so that there is no need to use different mask plates for array substrates 200 of different sizes, which is more cost-saving.

[0058] It should be noted that the limitations on the various steps involved in this solution, without affecting the implementation of the specific solution, are not deemed to limit the order of the steps. The steps written in front can be executed first, or later, or even simultaneously. As long as this solution can be implemented, it should be deemed to fall within the scope of protection of this application.

[0059] It should be noted that the inventive concept of the present application can form a large number of embodiments, but the length of the application document is limited and it is impossible to list them one by one. Therefore, under the premise of no conflict, the embodiments or technical features described above can be arbitrarily combined to form new embodiments. After the embodiments or technical features are combined, the original technical effects will be enhanced.

[0060] The above content is a further detailed description of the present application in combination with specific optional implementation methods, and it cannot be determined that the specific implementation of the present application is limited to these descriptions. For ordinary technicians in the technical field to which the present application belongs, several simple deductions or substitutions can be made without departing from the concept of the present application, which should be deemed to fall within the scope of protection of the present application.

Claims

1. An array substrate, characterized in that: Used in a flexible electronic paper display panel; the array substrate comprises a flexible substrate, an active switch layer, a protective layer and a pixel electrode layer, the active switch layer, the protective layer and the pixel electrode layer are sequentially deposited on the flexible substrate, and the array substrate comprises a bending area and an unfolding area; The protective layer includes a first passivation layer, a spacer layer and a second passivation layer, the first passivation layer, the spacer layer and the second passivation layer are sequentially deposited on the active switch layer, the spacer layer is at least located between the first passivation layer and the second passivation layer in the bending area, the first passivation layer corresponding to the bending area includes a plurality of first recessed portions and a plurality of first protruding portions, the first recessed portions and the first protruding portions are arranged at intervals, the second passivation layer includes a plurality of second recessed portions and a plurality of second protruding portions, the second recessed portions and the second protruding portions are arranged at intervals, the first protruding portion is located in the second recessed portion, and the second protruding portion is located in the first recessed portion.

2. The array substrate according to claim 1, characterized in that: In the protective layer in the expansion area, the first passivation layer and the second passivation layer are in contact with each other; in the protective layer only in the bending area, the first passivation layer includes a plurality of first recessed portions and a plurality of first protruding portions, the first recessed portions and the first protruding portions are arranged at intervals, the second passivation layer includes a plurality of second recessed portions and a plurality of second protruding portions, the second recessed portions and the second protruding portions are arranged at intervals, the first protruding portion is located in the second recessed portion, the second protruding portion is located in the first recessed portion, and the spacing layer is only located between the first protruding portion and the second recessed portion and between the first recessed portion and the second protruding portion in the bending area.

3. The array substrate according to claim 1, characterized in that: In the protective layer in the expansion area, the first passivation layer includes a plurality of first recessed portions and a plurality of first convex portions, the first recessed portions and the first convex portions are arranged at intervals, the second passivation layer includes a plurality of second recessed portions and a plurality of second convex portions, the second recessed portions and the second convex portions are arranged at intervals, the first convex portion is located in the second recessed portion, the second convex portion is located in the first recessed portion, and the spacing layer is also located between the first convex portion and the second recessed portion and between the first recessed portion and the second convex portion in the expansion area.

4. The array substrate according to claim 2 or 3, characterized in that: The length direction of the bending area is taken as the first direction, and the width direction of the bending area is taken as the second direction; Along the first direction, the first protruding portion is adjacent to the first concave portion on both upper and lower sides, and the first concave portion is adjacent to the first protruding portion on both upper and lower sides; Along the second direction, both the first protruding portion and the first concave portion are adjacent to each other on both the left and right sides of the first protruding portion, and both the first protruding portion and the first concave portion are adjacent to each other on both the left and right sides of the first concave portion.

5. The array substrate according to claim 2 or 3, characterized in that: The length direction of the bending area is taken as the first direction, and the width direction of the bending area is taken as the second direction; Along the second direction, the first protruding portion is adjacent to the first concave portion on both sides thereof, and the first concave portion is adjacent to the first protruding portion on both sides thereof; Along the first direction, the first protrusion is adjacent to the first recessed portion and the first protrusion on both sides above and below, and the first protrusion is located between the first recessed portion and the first protrusion; the first recessed portion and the first protrusion are adjacent to the first recessed portion and the first protrusion on both sides above and below, and the first recessed portion is located between the first recessed portion and the first protrusion.

6. The array substrate according to claim 2 or 3, characterized in that: The array substrate further comprises data lines and scan lines, wherein the data lines and the scan lines are arranged on the flexible substrate, and the data lines and the scan lines are arranged in a crisscross pattern to divide a plurality of pixel unit areas; The active switch layer includes a plurality of active switches, each of the active switches corresponds to each of the pixel unit regions one by one; the orthographic projection of the first recessed portion on the flexible substrate covers the orthographic projection of the active switch on the flexible substrate.

7. A method for preparing an array substrate, characterized in that: The method for preparing the array substrate according to any one of claims 1 to 6, wherein the array substrate comprises a bending area and an unfolding area, comprises the steps of: forming an active switching layer on the flexible substrate; forming a first passivation layer on the active switch layer; and forming a plurality of first recessed portions and a plurality of first raised portions on the first passivation layer in the bending region, wherein the first recessed portions and the first raised portions are arranged at intervals; forming a spacer layer at least on the first passivation layer in the bending region; A second passivation layer is formed on the spacer layer, wherein a plurality of second recessed portions and a plurality of second raised portions are formed on a side of the second passivation layer corresponding to the bending region and close to the first passivation layer, wherein the second recessed portions and the second raised portions are arranged at intervals, the first raised portion is located in the second recessed portion, and the second raised portion is located in the first recessed portion, so as to form a protective layer; A pixel electrode layer is formed on the protective layer.

8. The method for preparing an array substrate according to claim 7, characterized in that: forming a first passivation layer on the active switch layer; and forming a plurality of first recessed portions and a plurality of first raised portions on the first passivation layer in the bending region, wherein the first recessed portions and the first raised portions are arranged at intervals; forming a spacer layer at least on the first passivation layer in the bending region; A second passivation layer is formed on the spacer layer, a plurality of second recessed portions and a plurality of second raised portions are formed on a side of the second passivation layer corresponding to the bending region close to the first passivation layer, the second recessed portions and the second raised portions are arranged at intervals, the first raised portion is located in the second recessed portion, and the second raised portion is located in the first recessed portion, so that the step of forming a protective layer includes: forming a first passivation layer on the active switching layer; forming a plurality of first recessed portions and a plurality of first raised portions only on the first passivation layer in the bending region, wherein the first recessed portions and the first raised portions are arranged at intervals; forming a spacer layer only on the first passivation layer in the bending region; A second passivation layer is formed on the spacer layer, wherein a plurality of second recessed portions and a plurality of second raised portions are formed on a side of the second passivation layer corresponding to the bending region and close to the first passivation layer, wherein the second recessed portions and the second raised portions are arranged at intervals, the first raised portion is located in the second recessed portion, and the second raised portion is located in the first recessed portion, so as to form a protective layer; Among them, in the protective layer in the development area, the adjacent surfaces of the first passivation layer and the second passivation layer are flush.

9. The method for preparing an array substrate according to claim 7, characterized in that: forming a first passivation layer on the active switch layer; and forming a plurality of first recessed portions and a plurality of first raised portions on the first passivation layer in the bending region, wherein the first recessed portions and the first raised portions are arranged at intervals; forming a spacer layer at least on the first passivation layer in the bending region; A second passivation layer is formed on the spacer layer, a plurality of second recessed portions and a plurality of second raised portions are formed on a side of the second passivation layer corresponding to the bending region close to the first passivation layer, the second recessed portions and the second raised portions are arranged at intervals, the first raised portion is located in the second recessed portion, and the second raised portion is located in the first recessed portion, so that the step of forming a protective layer includes: forming a first passivation layer on the active switching layer; forming a plurality of first recessed portions and a plurality of first raised portions on the first passivation layer in the bending region and the unfolding region, wherein the first recessed portions and the first raised portions are arranged at intervals; forming a spacer layer on the first passivation layer in the bending area and the unfolding area; A second passivation layer is formed on the spacing layer, and a plurality of second recessed portions and a plurality of second raised portions are formed on the second passivation layer corresponding to the bending area and the unfolding area, the second recessed portions and the second raised portions are arranged at intervals, the first raised portion is located in the second recessed portion, and the second raised portion is located in the first recessed portion to form a protective layer.

10. A flexible electronic paper display panel, characterized in that: The flexible electronic paper display panel comprises an electronic paper film layer and an array substrate as claimed in any one of claims 1 to 6, wherein the electronic paper film layer is attached to the array substrate.

Citation Information

Patent Citations

  • Array substrate and display device

    CN103700322A

  • Array substrate and flexible display device

    CN109449163A

  • Flexible display panel and preparation method thereof

    CN114677918A

  • Display panel, preparation method of display panel and display device

    CN118151461A

  • Flexible display component

    TW201914002A

Cited By

  • Array substrate and preparation method therefor, and flexible electronic paper display panel

    WO2026081836A1