Back etching method for shallow trench isolation process
By adding the hydrogen fluoride purge step in the shallow trench isolation process, the etching speed in different areas of the device is balanced, the problem of the difference in the height of STI oxide after back etching is solved, and the morphology retention and selection ratio of the process is improved.
Patent Information
- Application Number
- CN202411019155.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-26
- Publication Date
- 2024-11-15
AI Technical Summary
During the back etching process of shallow trench isolation process, the height of STI oxides in different areas of the device varies greatly, resulting in uneven etching speed, especially the diffusion difficulty of etching gas in the ISO region and Dense region is different. , affects the morphology preservation and selection ratio of the process.
After the back etching, the hydrogen fluoride purge step is added. By controlling the duration, pressure and flow of hydrogen fluoride, the height difference of oxides in the trench in different regions is reduced. The etching rate of the Dense region is higher than that of the ISO region during the hydrogen fluoride purge process. , balance the oxide height difference caused by the main etching.
The height difference between the STI oxides in the ISO region and the Dense region after the back etching is effectively reduced, the morphological retention and selection ratio of the process is improved, and the problem of uneven etching speed is solved.
Smart Images

Figure CN118969714A_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the field of semiconductor technology, and in particular to an etch-back method for a shallow trench isolation process. Background Art
[0002] In the shallow trench isolation (STI) manufacturing process of advanced technology, Certas Etch technology is used to complete the back etching for the shallow trench isolation process for the consideration of selectivity and retaining good morphology. The back etching is used to remove part of the oxide filled in the silicon groove of the substrate (hereinafter referred to as STI oxide). Certas etch uses NH3 and HF gas as etching sources to etch STI oxide, which has the advantages of high selectivity and fewer defects in the wafer.
[0003] The small feature size (CD) of the device structure manufactured using advanced technology will affect the diffusion of Certas Etch etching gas. The width and density of shallow trench isolation in different device regions are different. The shallow trench isolation in the single-line region (ISO region) of the device is relatively scattered and has a larger width. NH3 and HF gases can diffuse in more easily to etch the STI oxide, and the etching speed is faster. The shallow trench isolation in the multi-line region (Dense region) of the device is relatively dense and narrow. NH3 and HF gases are not easy to diffuse in to etch the STI oxide, and the etching speed is slower. When the amount of STI oxide etching is large, due to the different degree of difficulty of etching gas diffusion in the ISO region and the Dense region, there is a difference in etching rate. After the back etching is completed, there will be a large difference in the height of the STI oxide in the ISO region and the Dense region (such as Figure 1 shown). Summary of the invention
[0004] In view of the above-mentioned shortcomings of the prior art, the purpose of the present application is to provide an etch-back method for shallow trench isolation process, which is used to solve the problem of large differences in STI oxide heights in different device regions after etch-back in the prior art.
[0005] To achieve the above-mentioned purpose and other related purposes, the present application provides an etch-back method for a shallow trench isolation process, comprising:
[0006] Step 1, providing a substrate, wherein a plurality of grooves are formed in the substrate;
[0007] Step 2, filling the trench with oxide;
[0008] Step 3, etching back the oxide to remove part of the oxide in the trench;
[0009] In step 4, hydrogen fluoride purge is performed to reduce the height difference of oxides in the trenches located in different areas of the substrate.
[0010] Preferably, the process conditions of hydrogen fluoride purging include: duration of 10s-15s, and pressure and flow rate being the same as the pressure and flow rate of hydrogen fluoride in step three.
[0011] Preferably, the back etching in step three is Certas Etch using NH3 and HF gases as etching sources.
[0012] Preferably, in step 2, an oxide is first formed on the substrate by a deposition process, and then the oxide outside the groove is removed by a grinding process.
[0013] Preferably, the deposition process is high density plasma deposition.
[0014] Preferably, the oxide comprises silicon oxide.
[0015] Preferably, the step of forming the groove includes: forming a mask layer having a groove pattern on the substrate by photolithography and etching processes; using the mask layer as a mask, forming the groove in the substrate by etching processes; and removing the mask layer by ashing processes.
[0016] Preferably, the mask layer is a photoresist layer.
[0017] Preferably, the region includes an ISO region and a Dense region.
[0018] Preferably, in step 4, the etching rate of the Dense area is higher than that of the ISO area.
[0019] As described above, the back etching method for shallow trench isolation process provided by the present application has the following beneficial effects: a hydrogen fluoride purge (HF purge) step is added after the main etching, and the etching rate of the oxide in the Dense area trench is higher than that in the ISO area during the hydrogen fluoride purge process, which can balance the problem of higher etching rate of the oxide in the ISO area trench caused by the previous main etching, and reduce the height difference of the STI oxide in the ISO area and the Dense area after the back etching is completed. BRIEF DESCRIPTION OF THE DRAWINGS
[0020] In order to more clearly illustrate the specific implementation methods of the present application or the technical solutions in the prior art, the drawings required for use in the specific implementation methods or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are some implementation methods of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying any creative work.
[0021] Figure 1 A schematic diagram showing a cross-sectional structure showing that STI oxide heights in different device regions are greatly different after the conventional back etching is implemented;
[0022] Figure 2 A flow chart of an etch-back method for a shallow trench isolation process provided in an embodiment of the present application is shown. DETAILED DESCRIPTION
[0023] The following describes the implementation of the present application through specific examples, and those skilled in the art can easily understand other advantages and effects of the present application from the contents disclosed in this specification. The present application can also be implemented or applied through other different specific implementations, and the details in this specification can also be modified or changed in various ways based on different viewpoints and applications without departing from the spirit of the present invention.
[0024] The following will be combined with the accompanying drawings to clearly and completely describe the technical solutions in this application. Obviously, the described embodiments are part of the embodiments of this application, not all of them. Based on the embodiments in this application, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of this application.
[0025] In the description of the present application, it should be noted that the terms "center", "upper", "lower", "left", "right", "vertical", "horizontal", "inner", "outer", etc., indicating directions or positional relationships, are only for the convenience of describing the present application and simplifying the description, and do not indicate or imply that the devices or elements referred to must have a specific direction, be constructed and operated in a specific direction, and therefore cannot be understood as limiting the present application. In addition, the terms "first", "second", and "third" are only used for descriptive purposes and cannot be understood as indicating or implying relative importance.
[0026] In the description of this application, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be indirectly connected through an intermediate medium, it can also be the internal connection of two components, it can be a wireless connection, or it can be a wired connection. For ordinary technicians in this field, the specific meanings of the above terms in this application can be understood according to specific circumstances.
[0027] In addition, the technical features involved in the different embodiments of the present application described below can be combined with each other as long as they do not conflict with each other.
[0028] See also Figure 2 , which shows a flow chart of an etch-back method for a shallow trench isolation process provided in an embodiment of the present application.
[0029] like Figure 2 As shown, the back etching method for shallow trench isolation process includes the following steps:
[0030] Step 1, providing a substrate, wherein a plurality of grooves are formed in the substrate;
[0031] Step 2, filling the trench with oxide;
[0032] Step 3, etching back the oxide to remove part of the oxide in the trench;
[0033] In step 4, hydrogen fluoride purge is performed to reduce the height difference of oxides in the trenches located in different areas of the substrate.
[0034] In step 1, optionally, the substrate is a silicon substrate, a germanium substrate, or a silicon-on-insulator substrate, etc.; or the material of the substrate may also include other materials, such as III-V compounds such as gallium arsenide. Those skilled in the art can select the constituent material of the substrate according to the type of device structure formed on the substrate, so the type of the substrate should not limit the protection scope of the present invention.
[0035] As an example, the step of forming the groove includes: forming a mask layer having a groove pattern on the substrate by photolithography and etching processes; using the mask layer as a mask, forming the groove in the substrate by etching processes; and removing the mask layer by ashing processes.
[0036] The substrate has different device regions, and the width and density of the trenches in the different device regions are different. For example, the trenches in the ISO region are more dispersed and have a larger width, while the trenches in the Dense region are more dense and have a smaller width.
[0037] In step 2, an oxide is formed on the substrate by a deposition process, and then the oxide outside the trench is removed by a grinding process. Exemplarily, the deposition process is preferably high density plasma deposition (HDP).
[0038] As an example, the oxide includes silicon oxide.
[0039] In step 3, the oxide in the trench is etched back to make the oxide thickness meet the preset requirements of the shallow trench isolation height. In consideration of selectivity and retaining a good morphology, the Certas Etch technology using NH3 and HF gases as etching sources is used to complete the back etching.
[0040] In step 4, after the main etching of the back etching is completed, hydrogen fluoride purging is performed to delay the diffusion of residual NH3 in the trench. As an example, the process conditions of hydrogen fluoride purging include: duration of 10s-15s, pressure and flow rate are the same as the pressure and flow rate of hydrogen fluoride in step 3.
[0041] Since the groove width in the Dense area is smaller, it is more difficult for the residual NH3 to diffuse out. During the hydrogen fluoride purge, the NH3 content in the groove in the Dense area is higher than that in the ISO area. Therefore, the etching rate of the oxide in the groove in the Dense area is higher than that in the ISO area, which can balance the problem of higher etching rate of the oxide in the ISO area caused by the previous main etching, thereby reducing the height difference of the oxide in the ISO area and the Dense area after the back etching.
[0042] It should be noted that the illustrations provided in this embodiment are only used to illustrate the basic concept of the present application in a schematic manner. Therefore, the drawings only show components related to the present invention rather than being drawn according to the number, shape and size of components in actual implementation. In actual implementation, the type, quantity and proportion of each component may be changed arbitrarily, and the component layout may also be more complicated.
[0043] In summary, the back-etching method for shallow trench isolation process provided by the present application adds a hydrogen fluoride purge step after the main etching. During the hydrogen fluoride purge process, the etching rate of the oxide in the trench of the dense area is higher than that of the ISO area, which can balance the problem of the higher etching rate of the oxide in the trench of the ISO area caused by the previous main etching, and reduce the height difference of the STI oxide in the ISO area and the dense area after the back-etching is completed. Therefore, the present application effectively overcomes various shortcomings in the prior art and has a high industrial utilization value.
[0044] The above embodiments are merely illustrative of the principles and effects of the present application and are not intended to limit the present application. Anyone familiar with the technology may modify or change the above embodiments without violating the spirit and scope of the present application. Therefore, all equivalent modifications or changes made by a person of ordinary skill in the art without departing from the spirit and technical ideas disclosed by the present invention shall still be covered by the claims of the present application.
Claims
1. A back etching method for shallow trench isolation process, characterized in that: The method comprises: Step 1, providing a substrate, wherein a plurality of grooves are formed in the substrate; Step 2, filling the groove with oxide; Step 3, etching back the oxide to remove a portion of the oxide in the trench; Step 4: Perform hydrogen fluoride purge to reduce the height difference of oxides in the trenches located in different areas of the substrate.
2. The method according to claim 1, characterized in that The process conditions of the hydrogen fluoride purging include: duration of 10s-15s, and pressure and flow rate are the same as the pressure and flow rate of hydrogen fluoride in step three.
3. The method according to claim 1, characterized in that The back etching in step 3 is Certas Etch using NH3 and HF gases as etching sources.
4. The method according to claim 1, characterized in that: In the step 2, the oxide is first formed on the substrate by a deposition process, and then the oxide outside the groove is removed by a grinding process.
5. The method according to claim 4, characterized in that The deposition process is high density plasma deposition.
6. The method according to claim 1 or 4, characterized in that: The oxide includes silicon oxide.
7. The method according to claim 1, characterized in that The steps of forming the grooves include: forming a mask layer having the groove pattern on the substrate by photolithography and etching processes; using the mask layer as a mask, forming the grooves in the substrate by etching processes; and removing the mask layer by ashing processes.
8. The method according to claim 7, characterized in that The mask layer is a photoresist layer.
9. The method according to claim 1, characterized in that: The region includes an ISO region and a Dense region.