Adsorbent for trapping carbon dioxide from air flow or industrial air flow, application method and mosquito trap

By reacting platinum/alumina catalyst with cycloethylamine in the supported amine adsorbent to generate grafted short-chain primary amines and loading them on a specific support, the problem of reduced capture effect of supported amine adsorbent under high humidity conditions is solved. , efficient carbon dioxide capture is achieved, and excellent performance stability and capture effect are shown in small-scale scenarios.

CN118988255AActive Publication Date: 2024-11-22DAQIU NEW MATERIALS (SHANDONG) CO LTD
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
CN202411476349.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-10-22
Publication Date
2024-11-22
Estimated Expiration
2044-10-22

AI Technical Summary

Technical Problem

The existing loaded amine adsorbents have reduced carbon dioxide capture effect under high humidity conditions and are difficult to be suitable for small-scale carbon dioxide capture scenarios. In addition, the performance degradation of the loaded amine polymers during repeated heating and desorption, and it is difficult to adopt. Support material of conventional dimensions.

Method used

Grafted short chain primary amines are generated by reacting platinum/alumina catalyst and cycloethylamine with phenyl monochlorosilane in anhydrated reactor, supported on gamma-alumina, silica gel or hydrogen 13X molecular sieve support , an adsorbent with high thermal oxidation resistance and hydrophobicity is formed, and carbon dioxide capture is carried out by vacuum thermal desorption or normal pressure thermal desorption.

Benefits of technology

It is realized efficiently trapping carbon dioxide in air flow or industrial air flow with a relative humidity of 30-100%, to obtain carbon dioxide-rich air flow with CO2 content of more than 5v%, more than 30v%, more than 80v% or even more than 95v%, and the adsorbent is used for a long time. It is stable in use and is suitable for small and medium-sized carbon dioxide capture scenarios.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure SMS_1
    Figure SMS_1
Patent Text Reader

Abstract

The invention belongs to the technical field of gas adsorption separation, and particularly relates to an adsorbent for trapping carbon dioxide from air flow or industrial air flow, an application method and a mosquito trap. The adsorbent is prepared by the following steps: (1) taking methyl ethyl ketone as a reaction solvent, adding a platinum / aluminum oxide catalyst, enabling anhydrous cycloethylamine and phenyl chlorosilane to react, carrying out vacuum distillation on feed liquid to remove 10-15wt% of the feed liquid, and filtering; (2) treating a formed gamma-aluminum oxide, silica gel or hydrogen type 13X molecular sieve carrier at 160-180 DEG C, transferring the carrier to a rotary drum while the carrier is hot, performing nitrogen displacement and cooling, filling ammonia gas, atomizing and spraying the filtrate in the step (1) to the carrier, standing, spraying a methyl ethyl ketone solution containing 3-5wt% of methyl trichlorosilane, filling ammonia gas, and standing; and washing to obtain the adsorbent. The adsorbent is a supported amine adsorbent grafted with short-chain primary amine, is used in a fixed bed and TVSA, TSA and VSA modes, can capture carbon dioxide with high efficiency, and has application prospects.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention belongs to the technical field of gas adsorption and separation, and in particular relates to an adsorbent for capturing carbon dioxide from air flow or industrial air flow, an application method and a mosquito trap. Background Art

[0002] Through pressure swing adsorption technology and amine liquid absorption technology, high-concentration CO2-containing gas streams including pure CO2 gas streams are separated and further utilized from industrial gas streams (CO2 content above 8v%) such as natural gas boiler flue gas, chemical plants such as synthetic ammonia, intermediate gas from natural gas or methanol hydrogen production, etc. This is a mature method that has been scaled up and widely used. In recent years, carbon capture technology has been developed to separate carbon dioxide from air streams (CO2 content of about 430ppmv) to obtain gas streams with a CO2 concentration of more than 1v%, which is used in some special scenarios or regions, or to provide gas source conditions for further enrichment and utilization.

[0003] In the technology of capturing carbon dioxide from air flow or industrial air flow, adsorbing carbon dioxide through solid adsorbents and then desorbing it by heating and reducing pressure (TVSA or VSA) is an effective and feasible way; optional solid adsorbents include molecular sieves, loaded carbonates, loaded amines, etc. Among them, the main principle of capturing carbon dioxide by molecular sieve adsorbents is physical adsorption and desorption. It is suitable for capturing carbon dioxide from industrial air flows with high CO2 content, but not for capturing carbon dioxide from air flows. It usually requires pre-dehydration facilities because it is easier to adsorb moisture in the air flow, and is not suitable for smaller-scale carbon dioxide capture scenarios.

[0004] The main principle of carbonate-loaded adsorbents for capturing carbon dioxide is that under normal temperature conditions in the presence of water (including carbonate aqueous solutions in the inner pores of the adsorbent), carbonates (such as alkaline potassium carbonate and lithium carbonate) absorb carbon dioxide and react to form bicarbonate (the reaction effect is better when a small amount of solution is formed in the inner pores of the adsorbent). The adsorbent is then heated and depressurized, and the bicarbonate decomposes into carbonate while releasing carbon dioxide. The performance of the adsorbent is restored after cooling. US2021187480A1 provides an adsorbent material of this type, which is made by loading alkali metal carbonates such as K2CO3 onto macroporous granular activated carbon by an impregnation method, adsorbing carbon dioxide from an air flow at normal temperature and pressure, and then desorbing it under conditions such as 100-300 mbar (absolute pressure) and 90-135°C. This type of carbonate-loaded adsorbent can be used to capture carbon dioxide from industrial gas streams with a certain CO2 content, and can also be used to capture carbon dioxide from air streams. It is particularly suitable for smaller-scale carbon dioxide capture scenarios; however, it has the following disadvantages: a. The carbon dioxide capture effect is significantly deteriorated when the air flow humidity is too high or too low (when the air flow humidity is too high, such as when the relative humidity is above 90%, the amount of liquid filled in the inner pores of the adsorbent after moisture absorption is too high; when the air flow humidity is too low, such as when the relative humidity is below 30%, the adsorbent does not absorb enough moisture or loses water rapidly; both situations result in a decrease in the rate of carbon dioxide adsorption); b. It is impossible to desorb carbon dioxide through steam or boiling water (resulting in water-soluble loss of carbonates and bicarbonates).

[0005] The main principle of carbon dioxide capture by loaded amine adsorbents is that the primary and secondary amine groups of the loaded organic amines adsorb CO2 and undergo certain reactions to generate amine-CO2 conjugates, thereby achieving carbon dioxide adsorption. When the gas stream contains an appropriate amount of water vapor, it is usually conducive to the adsorption of carbon dioxide. The adsorbent is then heated (about 100°C) and depressurized, and some amine-CO2 conjugates decompose, the amine groups are released, and carbon dioxide is discharged. The performance of the adsorbent is restored after cooling. Loaded amine adsorbents can be used to capture carbon dioxide from industrial gas streams with a certain CO2 content, and can also be used to capture carbon dioxide from air streams. At present, based on the combination of the amine functional group and the carrier, the loaded amine carbon dioxide capture agent, which is recognized to have overall advantages and application potential, is prepared by bonding the amine-containing monomer to the carrier by in-situ polymerization (Type III).

[0006] For example, US2024024849A1 discloses a renewable CO2 capture agent loaded with an amine polymer, wherein the CO2 raw gas includes flue gas or air emitted from a coal-fired power plant containing more than 10% O2; in the amine polymer loaded with the CO2 capture agent, the main adsorption site is a primary amine group; the amine polymer is preferably a linear polymer based on polyallylamine (PAA) or polyvinylamine (PVAm), and its derivatives (further grafting amine-containing groups on some amine groups to generate more amine groups, preferably citrullinated and cross-linked polyallylamine); the carrier includes mesoporous silica foam (MCF), mesoporous γ-alumina, and MCF with γ-alumina coated on the inner pore surface, and preferably a carrier with an integral structure is used.

[0007] US20070149398A1 discloses an amine-loaded carbon dioxide adsorbent, a preparation method and an application method thereof. The adsorbent is composed of 10-70% organic components and 30-90% inorganic components (i.e., carriers, such as powdered silica molecular sieve SBA-15), the inner pore surface of the carrier has hydroxyl groups, and the organic component, i.e., a hyperbranched polymer, is covalently connected to the carrier surface through oxygen provided by the hydroxyl groups; the hyperbranched polymer can be a vinylamine hyperbranched polymer generated by polymerization of cycloethylamine (also known as ethyleneimine), or a hyperbranched polymer having R W A polymer of N-CR2-CR2-structure (wherein R=H or a functional group, W=0, 1 or 2, and the functional group may contain F, Cl, Br, I, N, P, S, O); the hyperbranched polymer may also be connected to the surface of the carrier via a -Si-O- covalent bond, preferably, Si is also connected to a -OCH3 to form a methoxy short branch, and Si is further covalently connected to the surface of the carrier via one O or two Os.

[0008] The carbon dioxide adsorbent loaded with amine polymers disclosed in the above-mentioned US2024024849A1 and US20070149398A1 has the advantages of large amine loading, high CO2 equilibrium adsorption capacity, and low loss of loaded amine. The CO2 equilibrium adsorption capacity in a gas stream containing 400ppmv of CO2 and a gas stream containing 10v% of CO2 can exceed 0.8mol / kg of adsorbent and 1.8mol / kg of adsorbent, respectively, and the amine nitrogen utilization rate is lower than 0.2mol CO2 / mol N and 0.4mol CO2 / mol N, respectively. N (with many tertiary amine groups, which are difficult to adsorb carbon dioxide due to large steric hindrance), the CO2 equilibrium adsorption capacity is significantly reduced when the air flow humidity is too high, such as when the relative humidity is above 90%; in the actual carbon dioxide capture application cycle, since the loading amount of amine polymers usually exceeds 30wt%, it occupies a large proportion of the space in the inner pores, and there is a significant internal diffusion problem. Limited by the internal diffusion of the adsorbent and the generation rate of amine-CO2 conjugates, the dynamic adsorption amount of CO2 is generally about 50% of the equilibrium adsorption amount, the utilization rate of amine nitrogen is correspondingly reduced, and the CO2 adsorption stage is relatively long. The loaded amine polymer also has the problem of performance degradation during the repeated temperature-raising desorption process. The reasons may include: (1) some amine groups will react with certain active centers on the surface of the carrier, such as after strong adsorption, they basically lose the ability to adsorb carbon dioxide, and are easily oxidized by residual O2 during temperature-raising desorption; and (2) some amine groups that do not react with the surface of the carrier are oxidized by O2 in the residual CO2-containing airflow and gradually lose the ability to adsorb carbon dioxide. At the same time, conventional carrier materials with conventional dimensions, easy purchase or preparation, low cost, spherical or strip-shaped are not used. Therefore, these two prior arts are difficult to apply.

[0009] Therefore, it is necessary to develop an easier-to-use loaded amine adsorbent that can adsorb carbon dioxide from air flows or industrial air flows with a relative humidity of 50-100% with high efficiency. The loaded amine is basically not oxidized or lost during desorption by TVSA or TSA. It has advantages in CO2 capture output, operating costs and service life, and can be applied to both small-scale and large-scale carbon dioxide capture scenarios. It is best to use steam or boiling water as the desorption heat source.

[0010] In recent years, it has been found that air conditions containing a certain concentration of CO2 (such as above 0.2v%) have a strong inducing effect on female mosquitoes. Properly designed carbon dioxide induced mosquito traps have better use effects, but when using miniature carbon dioxide liquid cylinders with a volume of 2L, there are troubles in filling, replacing cylinders and purchasing carbon dioxide. It is also not suitable for semi-enclosed scenes such as indoors, which limits the application of such mosquito traps. When using carbonate-loaded adsorbents or amine-loaded adsorbents in the existing technology, using ambient air as the CO2 gas source and TVSA desorption, when the air humidity is too high, such as when the relative humidity is above 90%, the carbon dioxide capture and mosquito catching effect are significantly reduced, and the adsorbent life is affected. Summary of the invention

[0011] To solve the above technical problems, the present invention provides an adsorbent for capturing carbon dioxide from an air flow or an industrial air flow, an application method and a mosquito trap.

[0012] The adsorbent for capturing carbon dioxide from air stream or industrial gas stream of the present invention is prepared by the following steps: (1) The reactor and its attached condensation reflux system and evacuation condensation system are subjected to anhydrous treatment and nitrogen replacement; anhydrous methyl ethyl ketone is injected into the reactor as a reaction solvent, a powdered platinum / alumina catalyst is added, and the stirring is continued. Anhydrous cycloethylamine is injected, and the reactor feed liquid temperature is controlled to be 35-40°C and the condensation temperature of the condensation reflux system is controlled to be -15 to -20°C; phenyl monochlorosilane is continuously injected and the injection time is controlled to be 3-5h, and then the feed liquid continues to react for 4-5h; the reactor feed liquid temperature is then controlled to be 25-40°C, the condensation temperature of the condensation reflux system is controlled to be 0 to 5°C, the condensation temperature of the evacuation condensation system is controlled to be -15 to -20°C and the required vacuum degree, and the reactor feed liquid is distilled for 0.5-1h and the distillation removal amount of the feed liquid is controlled to be 10-15wt%; the distilled feed liquid in the reactor is filtered under water-free and air-tight conditions, and the filtrate is used as the spray impregnation liquid of the adsorbent in step (2); The condensation reflux system and the vacuum condensation system are used in series, and the air inlet end of the condensation reflux system is connected to a top opening of the reactor; the condensate of the condensation reflux system flows back to the reactor, and the condensate of the vacuum condensation system flows into the vacuum liquid storage tank through the pipeline; In the feed of the reactor, the weight ratio of the total amount of methyl ethyl ketone, platinum / alumina catalyst, cycloethylamine and phenylmonochlorosilane is 100:(0.7-1):(15-30), and the molar ratio of cycloethylamine to phenylmonochlorosilane is (2.2-2.3):1; (2) The formed γ-alumina, silica gel or hydrogen-type 13X molecular sieve carrier is placed in an oven and treated at 160-180°C for 4-6 hours, and while hot, it is transferred to a vacuum-evacuable, atomizing nozzle-equipped, anhydrous rotary drum, and the drum is sealed, replaced with nitrogen, maintained at a positive pressure, and cooled to room temperature, and further replaced with high-purity nitrogen and maintained at a positive pressure, and filled with high-purity ammonia until the pressure increases by 3-10 kPa, and maintained for 2-4 hours until the pressure does not decrease; the drum is started to rotate, and the filtrate of step (1) is sprayed onto the carrier by atomization, and the spraying volume of the filtrate is 75-85% of the saturated water absorption volume of the carrier. The spraying time is 3-4 hours, and the mixture is allowed to stand for 20-40 hours for homogenization and reaction. Then, a methyl ethyl ketone solution containing 3-5 wt% of methyl trichlorosilane is sprayed, and the spraying volume of the methyl ethyl ketone solution of methyl trichlorosilane is 5-10% of the saturated water absorption volume of the carrier. The spraying time is 0.5-1 hour, and high-purity ammonia is charged until the pressure increases by 5-10 kPa. Then, the rotation of the drum is stopped, and the mixture is allowed to stand for 10-20 hours for homogenization and reaction. Finally, methyl ethyl ketone is injected for washing 2-3 times, and the pressure is released. Water is injected to a positive pressure of 0.25-0.3 MPa for washing for more than 5 times, and the adsorbent is discharged after drainage and pressure release to obtain the adsorbent. Wherein, the specific surface area of ​​the carrier is higher than 280m 2 / g, pore volume 0.7-1.0mL / g, surface hydroxyl density higher than 4 / nm 2 .

[0013] The adsorbent of the present invention, wherein the carrier in step (2) is preferably a spherical γ-alumina with a diameter of Φ2.5-3 mm or a strip-shaped γ-alumina with a diameter of Φ(1.5-2)x(3-8) mm, a hydrogen-type 13X molecular sieve, or a granular silica gel with an outer size of 3-4 mm, so as to obtain a higher air velocity under the use conditions of the adsorbent in a fixed bed without requiring an excessively high bed inlet air flow pressure or bed pressure drop; further preferably, the carrier has an equivalent pore volume of 15-30 nm in diameter of 0.15 mL / g or more, an equivalent pore volume of 30-100 nm in diameter of 0.1 mL / g or more, and an equivalent pore volume of 100 nm or more in diameter of 0.06 mL / g or more, so that the adsorbent has a lower internal diffusion resistance and a relatively shorter carbon dioxide adsorption time; the surface hydroxyl density is preferably 4.5-5.5 / nm 2 ; Other indicators include: the compressive strength of the spherical carrier is higher than 60N / particle, the compressive strength of the strip carrier is higher than 120N / cm, and the abrasion is lower than 0.4wt%. The production of the carrier is a known technology in this field or related fields and can be purchased on the market or customized. The surface hydroxyl density is detected by the reactive gas chromatography method in the T / FSI049-2020 test method for the content of silanol on the surface of fumed silica. The spherical and strip carriers are first crushed, sheared with high-speed blades, and sieved to obtain fine powder with a particle size of 44-75μm (+325 mesh to -200 mesh), and the drying conditions are changed to 180℃ for 6h.

[0014] In step (1), the condensation reflux system and the vacuum condensation system have air inlet ends a and c and air outlet ends b and d, respectively; the air inlet end a of the condensation reflux system is connected to the top interface of the reactor, and the condensate flows back to the reactor through the air inlet end a and the top interface, and the air outlet end b is connected to the air inlet end c of the vacuum condensation system; the air outlet end d of the vacuum condensation system is connected to a three-way valve and further connected to an oil-free vacuum pump.

[0015] In step (1), the platinum / alumina catalyst contains 0.1-0.2 wt% platinum and can be prepared by the following method: a catalyst preparation container is purged and replaced with a nitrogen flow saturated with isopropanol vapor, and a catalyst having a specific surface area of ​​4-10 m 2 / g, a pore volume of 0.35-0.4mL / g, and an outer diameter of 44-75μm, continue to purge and replace with a nitrogen flow saturated with isopropanol vapor, add an isopropanol solution containing chloroplatinic acid and ethylene glycol of the required concentration during stirring, the amount of the isopropanol solution containing chloroplatinic acid and ethylene glycol added is 25-30wt% of the saturated water absorption of the alumina carrier, after the isopropanol solution is completely absorbed by the carrier (the surface of the carrier becomes dry and the fluidity is restored), the container is sealed and placed for 6-10h, then the temperature is raised to 70-80℃ and dried under the condition of high-purity nitrogen flow purging at this temperature range until all the isopropanol is evaporated, the temperature is raised to 130-150℃ and kept at a constant temperature for 0.5-1h, and then dried under the temperature range of 130-150℃ and high-purity nitrogen flow purging until all the ethylene glycol is evaporated, cooled to room temperature, and the container is sealed to obtain a platinum / alumina catalyst.

[0016] In step (1), the filtered catalyst is washed with methyl ethyl ketone for more than 3 times, and methyl ethyl ketone is added to form a slurry, which is transferred into a sealable container replaced with nitrogen and stored for later use.

[0017] In step (2), it is preferred to maintain a positive pressure of 15-30 kPa (gauge pressure) in the drum during the spraying, homogenization, reaction and methyl ethyl ketone washing to prevent oxygen and water vapor in the ambient air from penetrating into the drum and adversely affecting the grafting reaction process and effect.

[0018] The adsorbent of the present invention is suitable for use in the application of capturing carbon dioxide from air streams or industrial gas streams in a fixed bed manner.

[0019] When the air flow with CO2 content of more than 400ppmv is used as the source of carbon dioxide, it is generally at 0-30℃, normal pressure or low positive pressure below 50kPa (gauge pressure), and the air flow velocity is higher than 2000h -1The adsorption is carried out under the conditions of , and then the adsorbed CO2 is removed by vacuum thermal desorption or atmospheric pressure thermal desorption. After the bed is cooled down, air flow is passed through to carry out the next cycle of carbon dioxide capture operation. The desorption temperature is 90-120°C. The heating and cooling operations can be carried out by indirect heat exchange of heat exchange components such as coils arranged in the adsorbent bed. For example, hot water or steam is circulated in the coils during heating, and cold water is circulated during cooling. Steam, hot water including boiling water, can also be introduced into the adsorbent bed alone or on the basis of indirect heat exchange as a heating source during desorption. When cooling, air flow below room temperature can also be introduced into the adsorbent bed alone or on the basis of indirect heat exchange. Due to the low CO2 content in the air, the adsorption process takes several hours.

[0020] When air flow is used as the source of carbon dioxide and vacuum thermal desorption is adopted after adsorption, the adsorbent bed can be first heated to 90-100°C by indirect heat exchange and evacuated to an absolute pressure below 50kPa, more preferably below 30kPa. Alternatively, the bed can be evacuated to an absolute pressure below 50kPa, more preferably below 30kPa, and then heated to 90-110°C by indirect heat exchange, and finally air or steam is introduced for purging. The exhaust gas during the heating and insulation process of the adsorbent bed and the exhaust gas during purging can be cooled by indirect heat exchange and then collected after passing through a vacuum pump, so as to obtain a carbon dioxide-rich gas flow with a CO2 content of more than 5v% or even more than 30v%.

[0021] When air flow is used as the source of carbon dioxide and normal pressure thermal desorption is adopted after adsorption, the adsorbent bed can be heated to 100-120°C by indirect heat exchange and then air or steam is introduced for purging. Alternatively, 100-120°C steam (which may contain CO2) can be introduced into the adsorbent bed to heat it to 100-120°C and purged. The exhaust gas during the heating and insulation process of the adsorbent bed and the exhaust gas during purging can be collected to obtain a carbon dioxide-rich gas stream with a CO2 content of more than 3v% or even more than 15v%. When steam is used for direct heating and heating, condensed water (including condensed water during the heating of the adsorbent bed and condensed water during the cooling of the removed hot gas stream) should be recycled for steam generation to avoid the dissolution loss of CO2. The exhausted hot gas stream is cooled by indirect heat exchange and / or by spraying low-temperature circulating condensed water to remove most of the water vapor and reuse the condensed water. The CO2 content in the obtained carbon dioxide-rich gas stream can be more than 60v% or even more than 80v%. When using the atmospheric pressure thermal desorption method, circulating boiling water (which may contain CO2 bubbles) can also be introduced into the adsorbent bed to raise the temperature to 90-100°C and immerse the bed. The discharged hot air flow is cooled by indirect heat exchange and / or by spraying low-temperature circulating condensed water to remove most of the water vapor. The CO2 content in the obtained carbon dioxide-rich air flow can also be above 80v%. The advantage of using steam and boiling water as the heat source for atmospheric pressure thermal desorption is that the air in the adsorbent bed including the adsorbent inner pores can be discharged faster, and the oxidation of the loaded amine is lighter than other methods; especially when using steam, the height difference between the adsorbent bed and the steam generator can be used to automatically complete the thermal desorption process without additional mechanical driving force, and the steam condensed water can be reused for steam production; and the small amount of water adsorbed by the adsorbent when adsorbing CO2 from the air can also be thermally desorbed, condensed and reused and is sufficient to supplement the normal consumption of steam generation water or boiling water. For details, see the steam heating and circulation method in the mosquito trap below.

[0022] When an industrial gas stream with a CO2 content of more than 8% by volume is used as the source of carbon dioxide, the gas stream temperature in the adsorption stage should be lower than 40°C, preferably 10-30°C, and the gas stream pressure can be normal pressure or positive pressure. After adsorption, the pressure is reduced to an absolute pressure below 3 kPa, more preferably below 1 kPa, for desorption, and then purged with air and the next cycle of carbon dioxide capture operation is carried out, so as to obtain a carbon dioxide-rich gas stream with a CO2 content of more than 80% by volume or even more than 95% by volume.

[0023] In the application of the adsorbent of the present invention in capturing carbon dioxide from air flow or industrial air flow, the overall process design is determined according to the air flow conditions and the requirements for the CO2 content in the resulting carbon dioxide-rich air flow, especially the selection of the desorption method and the segmentation and collection logic of the CO2-rich gas. When air flow is used as the adsorption gas source, more attention should be paid to the CO2 removal utilization rate in the desorption stage.

[0024] The beneficial effects of the present invention include: the adsorbent is a loaded amine adsorbent grafted with short-chain primary amine, the primary amine loading amount is 0.8-1.3 mol / kg and is grafted on the surface of the carrier through silicon-oxygen covalent bonds, the heat-resistant oxidation performance is good, the loaded amine is basically not easy to be oxidized and lost, it has good hydrophobicity, stable performance, and can be used in a fixed bed and TVSA, TSA, VSA mode. It can capture carbon dioxide with high efficiency from an air flow or industrial air flow with a relative humidity of 30-100%, and a carbon dioxide-rich air flow with a CO2 content of more than 5v%, more than 30v%, more than 80v% or even more than 95v% can be obtained; in an air flow containing more than 400ppmv of CO2 at a relative humidity of 60-100% and an air flow containing 10v% of CO2, the CO2 release and capture amount of a single cycle can exceed 0.54mol / kg adsorbent and 0.70mol / kg adsorbent, respectively, and the amine nitrogen utilization rate is higher than 0.67mol CO2 / mol N and 0.84molCO2 / mol N, respectively. N; It is suitable for small and medium-scale carbon dioxide capture scenarios. It has advantages in CO2 capture output, operating costs and service life. Its overall performance is better than existing technologies and has certain application prospects.

[0025] From the effects of the following embodiments, it is believed that the main principles of the adsorbent of the present invention are as follows, and the above beneficial effects are also the result of the combined effects of the following principles and factors: 1. The main reaction in step (1) is that cycloethylamine reacts with phenylmonochlorosilane (C6H5ClSiH2) to generate C6H5ClSi(C2H4NH2)2 under the conditions of anhydrous methyl ethyl ketone as reaction solvent and platinum / alumina catalyst. The yield of C6H5ClSi(C2H4NH2)2 based on phenylmonochlorosilane can reach more than 95%, and phenylmonochlorosilane is completely converted. The vacuum distillation of the feed liquid is then used to remove the remaining cycloethylamine in the reaction. The filtrate has almost no amine odor and has improved stability. If the distillation step is omitted, the filtrate has a strong amine odor. Cycloethylamine will polymerize and block pores during the grafting and loading reaction of step (2). The filtered catalyst is washed with methyl ethyl ketone for more than 3 times, and methyl ethyl ketone is added to make a slurry, which is transferred into a sealable container and filled with nitrogen to a positive pressure such as 15-30 kPa. After storage, it can be repeatedly used and has stable performance. If the filtrate is pre-processed to complete the reaction of chlorine to hydroxyl (generating C6H5OH(C2H4NH2)2), the generated ammonium chloride is difficult to remove and dehydration dimerization between the hydroxyl groups of C6H5OHSi(C2H4NH2)2 is likely to occur, and the dimerization product cannot be grafted onto the carrier.

[0026] 2. The main reaction in step (2) is that the C6H5ClSi(C2H4NH2)2 contained in the filtrate reacts with the hydroxyl groups of the γ-alumina, silica gel or hydrogen-type 13X molecular sieve carrier through Cl, under the neutralization of sufficient ammonia, and the C6H5Si(C2H4NH2)2 group is grafted to the inner and outer surfaces of the carrier in the form of Si-O-Si or Si-O-Al covalent bonds, and the hydroxyl density on the carrier surface is higher than 4 / nm 2 The grafting amount depends on the mutual steric hindrance of C6H5Si(C2H4NH2)2 groups. The grafting is uniform and the loading is relatively large (the density of surface hydroxyl groups is low, such as less than 1.5 / nm). 2 The grafting is sometimes uneven, and some positions cannot be grafted, resulting in a decrease in the total loading amount). The actual grafting amount is close to the theoretical grafting amount. When a hydrogen-type 13X molecular sieve carrier is used, it is basically grafted in the "cage" of its structure rather than in the pores between cages (no significant internal diffusion restriction is found); the remaining hydroxyl groups of the carrier react with methyltrichlorosilane under the neutralization of sufficient ammonia, and the CH3Si group is grafted to a large proportion of the remaining inner and outer surfaces of the carrier in the form of covalent bonds of Si-O-Si or Si-O-Al; in the subsequent washing process with methyl ethyl ketone solution, a small amount of organic silicon that has not been grafted is basically removed, eliminating the problem of accumulation and pore blocking in the subsequent preparation and application of the adsorbent; in the process of washing methyl ethyl ketone with water injection to a positive pressure of 0.2-0.3MPa and generating ammonium chloride in the grafting reaction, the adsorbent gradually has It has a certain hydrophobicity (but water with a positive pressure of more than 0.2MPa can be pressed into the inner pores), and the obtained adsorbent does not wet and absorb pressureless water at 20-40℃; it only absorbs a small amount of moisture (2-3wt%) in an airflow of saturated water vapor at 20-40℃, and it is believed that basically no aqueous solution is formed in the inner pores. This is the basis for the adsorbent to adsorb carbon dioxide in an airflow with a relative humidity of 90-100% without decreasing its adsorption performance; in the heating or constant temperature process of thermal desorption using normal pressure 100-120℃ steam or boiling water, it is found that its hydrophobicity can still be maintained, otherwise it is easy to cause the adsorbent to gradually pulverize or break; steam can be used for CO2 desorption, which is an important reason for being able to capture a carbon dioxide-rich airflow with a CO2 content of more than 80v% or even more than 95v% from the air flow.

[0027] 3. In the adsorbent prepared in step (2), the C6H5Si(C2H4NH2)2 group and CH3Si group are grafted and loaded by covalent bonding of Si-O-Si or Si-O-Al. The former (C6H5Si(C2H4NH2)2 group) is a short-chain organic amine with good thermal stability and oxidation resistance (stable under conventional hydrothermal conditions below 150°C), small steric hindrance when adsorbing CO2, distributed on the surface of the inner pores, easy to play a role, and less impact on the diffusion of CO2. Therefore, compared with the prior art (including modified MOF), the adsorbent of the present invention can adsorb CO2 faster by 50% or even more than 100% in the adsorption process, and can desorb CO2 faster by more than 30% in the desorption process; The CH3Si group occupies less space, has better thermal stability and oxidation resistance, and has almost no effect on the internal diffusion of CO2; the carrier is not easy to undergo changes such as recrystallization under steam conditions because the surface is basically shielded by the two, especially the silica gel carrier, which is usually not easy to avoid this problem; because the CH3Si group eliminates a large proportion of the remaining hydroxyl groups and has a shielding effect, the primary amine group of the loaded amine cannot or is difficult to contact the surface of the carrier, that is, it cannot or is difficult to react with certain remaining active centers on the surface of the carrier, such as adsorption, and can exert the adsorption capacity of CO2 to a greater extent, and is not easily oxidized by residual O2 during temperature increase desorption. At the same time, the C2H4NH2 group in the C6H5Si(C2H4NH2)2 group is a primary amine group, which has moderate binding strength with CO2 and H2O, strong adsorption and binding ability but still easy to desorb (compared with secondary amine groups). Therefore, the adsorbent has good performance and is very stable in the application of capturing carbon dioxide, and has a long life.

[0028] The present invention also provides a mosquito trap that adopts the adsorbent and uses air flow as a carbon dioxide gas source; the mosquito trap has a carbon dioxide capture system, a mosquito catching system and a control system; the carbon dioxide capture system includes an adsorbent tank and related components, the adsorbent of the present invention is filled in the adsorbent tank in a fixed bed manner, and a carbon dioxide-rich gas flow is generated by the above-mentioned carbon dioxide capture method; the carbon dioxide-rich gas flow generated by the carbon dioxide capture system is continuously or intermittently sent to the mosquito catching system for use; the control system controls the operation of the carbon dioxide capture system and the mosquito catching system according to a set program.

[0029] The carbon dioxide capture system, whose adsorbent tank can be filled with adsorbent, for example, 2-10L, and related components are arranged according to the carbon dioxide capture method.

[0030] The mosquito catching system may have or adopt a mosquito catching structure and operation mode in the prior art. Preferably, the structure of the mosquito catching system includes a mosquito attracting module, a switch-type electric damper (damper), a mosquito catching and killing storage module and a rear suction fan. The mosquito catching and killing storage module has a mosquito catching net box. The mosquito catching principle is to suck mosquitoes attracted by a mixture of carbon dioxide-rich gas and air into the mosquito catching net box with the strong wind generated by the suction fan.

[0031] The mosquito trap has a good mosquito catching effect in summer and autumn when the relative humidity of the air is above 40%, including hot and humid days when the relative humidity is 90-100%. That is, the capture amount and capture concentration of carbon dioxide required for catching mosquitoes do not change significantly with the change of the relative humidity of the air. The mosquito trap is suitable for semi-enclosed places such as indoors and open places outdoors. DETAILED DESCRIPTION

[0032] The technical solution of the present invention is specifically described and illustrated below in conjunction with embodiments. Example 1

[0033] The adsorbent for capturing carbon dioxide from air or industrial gas streams of this embodiment is prepared by following the steps below: (1) A 1500 mL glass reactor (three-necked flask) and its attached condensation reflux system and evacuation condensation system were anhydrous and replaced with 99.9% nitrogen; anhydrous methyl ethyl ketone was injected into the reactor as a reaction solvent, a powdered platinum / aluminum oxide hydrosilylation reaction catalyst was added, and the mixture was stirred continuously. Anhydrous cycloethylamine was injected, and the reactor feed liquid temperature was controlled to be 35-40°C and the condensation temperature of the condensation reflux system was controlled to be -15 to -20°C; phenyl monochlorosilane was continuously injected and the injection time was controlled to be 4 hours, and then the feed liquid continued to react for 4 hours; the reaction was then controlled to The feed liquid temperature in the reactor is 35-40°C, the condensation temperature of the condensation reflux system is 0°C, the condensation temperature of the evacuation condensation system is -20°C and the required vacuum degree is maintained. The reactor feed liquid is distilled for 0.5h and the distillation removal amount of the feed liquid is controlled to be 12-13wt% to evaporate the remaining cycloethylamine; the distilled feed liquid in the reactor is filtered under anhydrous and air-tight conditions, and the filtrate is used as the spray impregnation liquid of the adsorbent in step (2); the filtered catalyst is washed with methyl ethyl ketone for more than 3 times, methyl ethyl ketone is added to prepare a slurry, and the slurry is transferred into a nitrogen-substituted sealed container and stored for later use; The condensation reflux system and the vacuum condensation system have air inlet ends a and c and air outlet ends b and d, respectively; the air inlet end a of the condensation reflux system is connected to a top interface of the reactor, and the condensate flows back to the reactor through the air inlet end a and the top interface, and the air outlet end b is connected to the air inlet end c of the vacuum condensation system; the condensate of the vacuum condensation system flows into the vacuum liquid storage tank through a pipeline, and the air outlet end d is connected to a three-way valve and further connected to an oil-free vacuum pump; In the feed of the reactor, the total amount of methyl ethyl ketone, platinum / alumina catalyst, cycloethylamine and phenylmonochlorosilane is 924 g (800 g, 6.0 g, 140 g, respectively), the weight ratio is 100:0.75:17.5, and the molar ratio of cycloethylamine to phenylmonochlorosilane is 2.25:1; (2) Spherical γ-alumina carrier (Φ2.6-2.8 mm, specific surface area 283 m 2 / g, pore volume 0.74mL / g, 15-30nm equivalent diameter pore volume 0.17mL / g, 30-100nm equivalent diameter pore volume 0.10mL / g, 100nm equivalent diameter pore volume 0.07mL / g, surface hydroxyl density 4.6 / nm 2 , compressive strength 88N / particle, abrasion 0.29wt%) 1308g, put it on a stainless steel plate and spread it into a thin layer, put it in an oven and treat it at 170℃ for 5h, weigh 1000g while it is hot and transfer it to a vacuum-evacuable, atomizing nozzle, and anhydrous rotary drum (content 9.6L), seal the rotary drum, evacuate it to an absolute pressure of 10kPa and fill it with 99.5% nitrogen to a positive pressure of 10kPa and repeat the operation 3 times to replace (remove air and water vapor), maintain positive The pressure was 10 kPa and cooled to room temperature, evacuated to an absolute pressure of 10 kPa and filled with 99.9% nitrogen to a positive pressure of 10 kPa for further replacement (deoxygenation) and maintained at a positive pressure of 10 kPa, and filled with 99.9% ammonia to a positive pressure of 16 kPa (an increase of 6 kPa relative to before ammonia filling), and the pressure was maintained for 3 hours (the drum was started to rotate for 5 minutes every 30 minutes), until the pressure did not decrease and dropped to room temperature (part of the ammonia introduced was adsorbed on the inner and outer surfaces of the carrier to combine with The HCl generated in the amine grafting reaction was loaded below); the drum was started to rotate, and 689 mL of the filtrate of step (1) was sprayed onto the carrier (the spray volume of the filtrate was 85% of the saturated water absorption volume of the carrier, 810 mL). The spraying time was 3.3 h. After standing for 30 h for homogenization and reaction, 65 mL of a methyl ethyl ketone solution containing 4 wt% of methyl trichlorosilane was sprayed. The spray volume of the methyl ethyl ketone solution of methyl trichlorosilane was 8% of the saturated water absorption volume of the carrier. The spraying time was 0.5 h. High-purity ammonia is added until the pressure rises to 8kPa, then the rotation of the drum is stopped and allowed to stand for 15 hours for homogenization and reaction; finally, methyl ethyl ketone (3500-3600g each time) is injected for washing 3 times (try to remove a small amount of ungrafted silicone and eliminate its accumulation and pore blocking problem), the pressure is released, and pure water is injected until the positive pressure in the drum is 0.25MPa, the drum is started to rotate for 0.5h, the water is drained, and the drum is washed 5 times with water (to wash away the ammonium chloride generated by the reaction), and the material is discharged after drainage and pressure release to obtain the adsorbent.

[0034] In step (1), the platinum / alumina catalyst used contains 0.15 wt% platinum and is prepared by the following method: the catalyst preparation container is a 100 mL three-necked glass flask, which is fixed on an electric heating magnetic stirrer with precise temperature control, a stirrer is placed, a mercury thermometer is installed, and a 99.9% nitrogen mixed gas saturated with isopropanol is introduced for replacement (60 mL / min, 30 min), the gas is stopped, and a flask with a specific surface area of ​​6.7 m is added. 2 / g, pore volume 0.38mL / g, outer diameter 44-75μm alumina carrier (+325 mesh to -200 mesh) 10g, then introduce 99.9% nitrogen mixed gas saturated with isopropanol to replace (30mL / min, 10min, the distance between the gas outlet and the bottom of the flask is 30mm), stop the gas, seal the flask, start stirring, use a 2mL syringe and a microporous needle to uniformly add chloroplatinic acid (H2PtCl6) 26.3g / L, ethylene glycol 350g / L 1.2mL of isopropanol solution (dropping time 0.5min) The temperature was raised to 75°C and dried for 3 h, then raised to 145°C and kept at this temperature for 0.5 h, and then dried at 145°C for 3 h (all ethylene glycol was evaporated), cooled to room temperature, nitrogen was stopped, and the flask was sealed to obtain a platinum / alumina catalyst.

[0035] The adsorbent prepared in this embodiment for capturing carbon dioxide from air flow or industrial air flow can float on the surface of pure water at room temperature and 0-106kPa (positive pressure), and can float on the surface of pure water at 100℃ and 0-73kPa (positive pressure), and has good overall hydrophobicity; the total weight loss is 2.3wt% when baked at 130℃ for 4h under air conditions, and the total weight loss is 2.4wt% when continued to be baked for 100h; the odor is very small, and the odor is completely eliminated after purging with air at room temperature for 6h; therefore, the water content is less than 2.4wt%. The nitrogen content detected by chemical method is 0.81mol / kg. Example 2

[0036] The preparation conditions and other raw materials of Example 1 were used and the operations of steps (1) to (2) of Example 1 were basically repeated to prepare the adsorbent for capturing carbon dioxide from air flow or industrial gas flow of this example. The main differences were as follows: in step (1), the total amount of methyl ethyl ketone, platinum / alumina catalyst, cycloethylamine and phenylmonochlorosilane in the feed of the glass reactor was 1048 g (800 g, 8.0 g and 240 g, respectively), the weight ratio was 100:1:30, and the molar ratio of cycloethylamine to phenylmonochlorosilane was 2.20:1; the platinum / alumina catalyst 8.0 g used was obtained by weighing 2.0 g of the unused 4 g of the 10 g catalyst prepared in Example 1, and adding 6.0 g of the catalyst in the methyl ethyl ketone filtered out and preserved in step (1); in step (2), the carrier treated in an oven at 170° C. was a Φ mm spherical hydrogen-type 13X molecular sieve (Φ2.7-3.0 mm, specific surface area 583 m 2 / g, pore volume 0.77mL / g, 15-30nm equivalent diameter pore volume 0.15mL / g, 30-100nm equivalent diameter pore volume 0.10mL / g, 100nm equivalent diameter pore volume 0.06mL / g, surface hydroxyl density 4.8 / nm 2 , compressive strength 72N / particle, abrasion 0.33wt%) 1400g; filled with 99.9% ammonia to a positive pressure of 20kPa (increased by 10kPa relative to before ammonia filling), and sprayed with 672mL of the filtrate prepared in step (1) (the filtrate spraying volume is 80% of the saturated water absorption volume of the carrier 840mL).

[0037] The adsorbent prepared in this embodiment for capturing carbon dioxide from air flow or industrial air flow can float on the surface of pure water at room temperature and 0-92kPa (positive pressure), and can float on the surface of pure water at 100℃ and 0-65kPa (positive pressure), and has good overall hydrophobicity; the total weight loss is 2.6wt% when baked at 130℃ for 4h under air conditions, and the total weight loss is 2.7wt% when continued to be baked for 100h; the odor is very small, and the odor is completely eliminated after purging with air at room temperature for 6h; therefore, the water content is less than 2.7wt%. The nitrogen content detected by chemical method is 1.22mol / kg. Example 3

[0038] The preparation conditions and other raw materials of Example 1 were used and the operations of steps (1) to (2) of Example 2 were basically repeated to prepare the adsorbent for capturing carbon dioxide from air flow or industrial gas flow of this example. The main differences were as follows: in step (1), the total amount of methyl ethyl ketone, platinum / alumina catalyst, cycloethylamine and phenylmonochlorosilane in the feed of the glass reactor was 968 g (800 g, 8.0 g and 200 g, respectively), the weight ratio was 100:1:25, and the molar ratio of cycloethylamine to phenylmonochlorosilane was 2.20:1; the platinum / alumina catalyst 8.0 g was the catalyst in the methyl ethyl ketone filtered out and preserved in step (1) of Example 2; the carrier used in step (2) was granular silica gel (spherical, with a specific surface area of ​​392 m2) with an outer size of 3.2-3.8 mm. 2 / g, pore volume 0.93mL / g, 15-30nm equivalent diameter pore volume 0.20mL / g, 30-100nm equivalent diameter pore volume 0.13mL / g, 100nm equivalent diameter pore volume 0.08mL / g, surface hydroxyl density 5.5 / nm 2 , compressive strength 64N / particle, abrasion 0.25wt%) 1500g; 735mL of the filtrate prepared in the spraying step (1) (the spraying volume of the filtrate is 75% of the saturated water absorption volume of the carrier 980mL).

[0039] The adsorbent prepared in this embodiment for capturing carbon dioxide from air flow or industrial air flow can float on the surface of pure water at room temperature and 0-117kPa (positive pressure), and can float on the surface of pure water at 100℃ and 0-89kPa (positive pressure), and has good overall hydrophobicity; the total weight loss is 2.0wt% when baked at 130℃ for 4h under air conditions, and the total weight loss is 2.1wt% when baked for 100h; the odor is very small, and the odor is completely eliminated after purging with air at room temperature for 6h; therefore, the water content is less than 2.1wt%. The nitrogen content detected by chemical method is 1.04mol / kg. Example 4

[0040] 300 mL of the adsorbent prepared in Examples 1-3 were taken respectively, and carbon dioxide capture experiments were carried out in a small laboratory evaluation device in turn; the adsorbent was filled in a vertical, transparent hard glass tube (with a glass jacket for water insulation) with a height of 320 mm and an inner diameter of 40 mm, and the adsorbent bed height was about 240 mm (height-to-diameter ratio of about 6), and the airflow during adsorption and desorption was upward and downward; simulated air flow and simulated industrial air flow were prepared by the gas distribution system respectively, and the exhaust gas after adsorption was pressurized by a circulating fan and returned to the gas distribution system for utilization; each adsorbent was used to adsorb CO2 in the manner shown in Table 1 below.

[0041] During the capture cycle 0-4, the desorption process after the CO2 gas source adsorption with simulated air flow, a sufficient flow of 100°C atmospheric pressure steam different from the source of the steam in the tube is passed through the jacket, and the tube is purged with 100-103°C atmospheric pressure steam for 10-15 minutes (occurring by the complete vaporization of pure water at a flow rate of 15g / min). The gas and airflow discharged from the tube are cooled to 23-25°C through the condenser, and the condensed water is separated and removed, and then collected in a latex bag. When the gas volume in the latex bag does not increase, it is maintained for 5 minutes and then the latex bag inlet is sealed to terminate the desorption process. The dead volume of the air flow path in the condenser is 110mL; during the bed cooling process, a sufficient flow of 25°C water is passed through the jacket, and 25°C atmospheric pressure air is purged through the tube at a flow rate of 25L / min for 30-60 minutes, and the cooling process is terminated when the exhaust temperature is lower than 30°C.

[0042] In the capture cycle 6-9, the desorption process after the adsorption of CO2 gas source using simulated industrial airflow, the jacket is still empty (water-free), and the tube is evacuated to an absolute pressure of 2-3 kPa (without heating) by a micro oil-free vacuum pump. The exhausted gas and airflow are cooled to 23-25°C by the above-mentioned condenser, and the condensed water is separated and removed, and then collected in a latex bag. When the gas volume in the latex bag does not increase, a room temperature and normal pressure air flow of 50 mL / min is passed through the tube to purge for 10 minutes and continue to evacuate to maintain an absolute pressure of 5-10 kPa. The latex bag inlet is sealed and the vacuum pump is turned off at the same time. After the pressure in the tube rises to normal pressure, the purge air is turned off to end the desorption process. After the desorption process is completed, the next cycle of carbon dioxide capture operation is carried out directly.

[0043] After the capture cycles 0-9 of each adsorbent are completed, the capture cycles 1-9 are repeated once, and then the capture cycle 4 is repeated ten times, for a total of 29 capture cycles, and finally the adsorbent is discharged.

[0044] The volume and CO2 content of the carbon dioxide-rich gas stream collected by the latex bag in each capture cycle were measured, and the CO2 capture capacity (mol CO2 / kg adsorbent) and amine nitrogen utilization rate (mol CO2 / mol N) of the adsorbent were calculated respectively.

[0045] Table 1 Adsorption conditions for CO2 capture experiments

[0046] The results of the carbon dioxide capture experiments of the above adsorbents are as follows: when the simulated air flows are used as the carbon dioxide source, the CO2 content in the carbon dioxide-rich gas flow collected by the latex bags in each capture cycle of each adsorbent is above 95v% (dry basis), the CO2 capture amount of a single capture cycle is more than 0.57mol / kg adsorbent, the amine nitrogen utilization rate is higher than 0.70mol CO2 / mol N, and the relative difference in CO2 capture amount and amine nitrogen utilization rate of each adsorbent under the different relative humidity air flow conditions of 60%, 75%, 90% and 100% is less than 4.5%; when the industrial air flows are used as the carbon dioxide source, the CO2 content in the carbon dioxide-rich gas flow collected by the latex bags in each capture cycle of each adsorbent is more than 90v% (dry basis), the CO2 capture amount of a single capture cycle is more than 0.72mol / kg adsorbent, and the amine nitrogen utilization rate is higher than 0.85molCO2 / mol N, and the relative differences of CO2 capture and amine nitrogen utilization rate of each adsorbent under the different relative humidity airflow conditions of 60%, 75%, 90%, and 100% were all less than 6.3%. Each adsorbent could achieve the capture effects of the first capture cycles 1-9 again in the repeated capture cycles 1-9; each adsorbent could also repeatedly achieve the capture effects of the first and second capture cycles 4 in the last ten repeated capture cycles 3; each adsorbent was unloaded and flattened in a plastic tray for inspection, and no fragmentation or powdering was found, and the appearance did not change from before use.

[0047] Afterwards, 300 mL of the adsorbent of Example 3 (granular silica gel grafted with short-chain organic amine and hydrophobically treated) which had a good overall effect and had been discharged after 29 capture cycles was refilled into the glass tube of the above evaluation device, and the capture cycle 3 was repeated 31 times, for a total of 60 capture cycles, and the adsorbent was finally discharged. In the 30th to 60th capture cycles, the adsorbent was able to repeatedly achieve the carbon dioxide capture effect of the first and second capture cycles 3; the adsorbent was discharged and flattened in a plastic tray for inspection, and no fragmentation or powdering was found, and the appearance was unchanged from before use.

[0048] The experimental results of carbon dioxide capture in this embodiment show that the three adsorbents mentioned above have good heat-oxidation resistance, the loaded amine is basically not prone to oxidation and loss, the moisture absorption is low, the hydrophobicity is good, the performance is stable, the CO2 adsorption rate is fast and the adsorption amount is less affected by humidity, the gas production concentration is high, the gas production in the same time is not low, the carbon dioxide capture effect is good, and it has advantages in CO2 capture output (unit time and unit adsorption tower volume combined), operating costs and service life. The overall performance is better than the existing technology and has certain application prospects. Example 5

[0049] Three commercially available mosquito traps that use air flow as a carbon dioxide gas source were modified by replacing the adsorbents in the fixed beds of their adsorbent tanks with an equal volume of the adsorbent of Example 3 (newly prepared) (each mosquito trap has two adsorbent tanks, and each adsorbent tank contains about 1.1 L of adsorbent). No other changes were made, and the desorption method of carbon dioxide was still normal pressure heating and air purge desorption, as the mosquito trap of this example.

[0050] The mosquito trap before and after modification has a carbon dioxide capture system, a mosquito catching system and a control system; the carbon dioxide capture system includes an adsorbent tank and related components, the adsorbent is filled in the adsorbent tank in a fixed bed manner, and a carbon dioxide-rich gas flow is generated by normal pressure heating and desorption; the carbon dioxide-rich gas flow generated by the carbon dioxide capture system is intermittently sent to the mosquito catching system for use; the control system controls the operation of the carbon dioxide capture system and the mosquito catching system according to a set program; the structure of the mosquito catching system includes a mosquito attracting module, a switch-type electric damper, a mosquito killing and storage module and a rear suction fan, and the mosquito killing and storage module has a mosquito net box; the mosquito catching system sucks mosquitoes attracted by the mixture of rich carbon dioxide gas and air into the mosquito net box along with the strong wind generated by the suction fan.

[0051] The modified mosquito trap has a good mosquito catching effect when placed in semi-enclosed indoor and outdoor open places in summer and autumn when the relative humidity of the air is above 40%, including hot and humid days with a relative humidity of 90-100%. That is, the capture amount and capture concentration of carbon dioxide required for catching mosquitoes do not change significantly with changes in the relative humidity of the air.

[0052] The mosquito traps before modification had a good mosquito catching effect when the relative humidity of the air was 50-85%, and the mosquito catching effect decreased slightly when the relative humidity of the air was above 85%, and decreased sharply when the relative humidity of the air was above 95%. Judging from the records of the use conditions in the mosquito trap manual, the chemical composition analysis results of the removed adsorbents, and the actual mosquito catching effect, the adsorbent tank of one mosquito trap was filled with an adsorbent loaded with carbonate, and the adsorbent tanks of the other two mosquito traps were filled with adsorbents loaded with organic amine polymers. The maximum moisture absorption rate of these adsorbents in the air at 25°C and 90% relative humidity was more than 7wt%, and they were all hydrophilic, and the saturated water absorption rate measured in a 250mL beaker of water was more than 12wt%.

[0053] In the present invention, the unit of CO2 content ppmv is one millionth by volume, and v% is one percent by volume; the specific surface area of ​​the carrier is determined by the low-temperature nitrogen adsorption BET method, and the pore volume and its distribution are obtained by coupling the measurement results of the low-temperature nitrogen adsorption BET method and the mercury injection method.

Claims

1. An adsorbent for capturing carbon dioxide from an air stream or an industrial gas stream, prepared by the following steps: (1) The reactor and its attached condensation reflux system and evacuation condensation system are subjected to anhydrous treatment and nitrogen replacement; anhydrous methyl ethyl ketone is injected into the reactor as a reaction solvent, a powdered platinum / alumina catalyst is added, and the mixture is continuously stirred, and anhydrous cycloethylamine is injected, and the feed liquid temperature in the reactor is controlled to be 35-40°C, and the condensation temperature of the condensation reflux system is controlled to be -15 to -20°C; phenyl monochlorosilane is continuously injected and the injection time is controlled to be 3-5h, and then the feed liquid continues to react for 4-5h; the feed liquid temperature in the reactor is then controlled to be 25-40°C, the condensation temperature of the condensation reflux system is controlled to be 0 to 5°C, the condensation temperature of the evacuation condensation system is controlled to be -15 to -20°C, and the required vacuum degree is controlled, and the reactor feed liquid is distilled for 0.5-1h and the distillation removal amount of the feed liquid is controlled to be 10-15wt%; the distilled feed liquid in the reactor is filtered under water-free and air-tight conditions, and the filtrate is used as the spray impregnation liquid of the adsorbent in step (2); in, The condensation reflux system and the vacuum condensation system are used in series, and the air inlet end of the condensation reflux system is connected to a top opening of the reactor; the condensate of the condensation reflux system flows back to the reactor, and the condensate of the vacuum condensation system flows into the vacuum liquid storage tank through the pipeline; In the feed of the reactor, the weight ratio of the total amount of methyl ethyl ketone, platinum / alumina catalyst, cycloethylamine and phenylmonochlorosilane is 100:(0.7-1):(15-30), and the molar ratio of cycloethylamine to phenylmonochlorosilane is (2.2-2.3):1; (2) The formed γ-alumina, silica gel or hydrogen-type 13X molecular sieve carrier is placed in an oven and treated at 160-180°C for 4-6 hours, and while hot, is transferred to a vacuum-evacuable, atomizing nozzle-equipped, anhydrous rotary drum, and the drum is sealed, replaced with nitrogen, maintained at a positive pressure, and cooled to room temperature, and further replaced with nitrogen and maintained at a positive pressure, and ammonia is filled until the pressure increases by 3-10 kPa, and maintained for 2-4 hours until the pressure does not decrease; the drum is started to rotate, and the filtrate of step (1) is sprayed onto the carrier in an atomized manner, and the spraying volume of the filtrate is 75-85% of the saturated water absorption volume of the carrier, and the spraying The time is 3-4 hours, and the drum is allowed to stand for 20-40 hours for homogenization and reaction, and then a methyl ethyl ketone solution containing 3-5wt% of methyl trichlorosilane is sprayed, and the spraying volume of the methyl ethyl ketone solution of methyl trichlorosilane is 5-10% of the saturated water absorption volume of the carrier. The spraying time is 0.5-1 hour, and ammonia is charged until the pressure increases by 5-10kPa, and then the rotation of the drum is stopped, and the drum is allowed to stand for 10-20 hours for homogenization and reaction; finally, methyl ethyl ketone is injected for washing 2-3 times, and the pressure is released, and water is injected to a positive pressure of 0.25-0.3MPa and washed for more than 5 times, and the material is discharged after drainage and pressure release to obtain an adsorbent; Wherein, the specific surface area of ​​the carrier is higher than 280m 2 / g, pore volume 0.7-1.0mL / g, surface hydroxyl density higher than 4 / nm 2 .

2. The adsorbent according to claim 1, characterized in that The carrier in step (2) is a spherical material with a diameter of 2.5-3 mm or a strip-shaped material with a diameter of (1.5-2) x (3-8) mm, a hydrogen-type 13X molecular sieve, or a granular silica gel with an outer size of 3-4 mm.

3. The adsorbent according to claim 2, characterized in that The carrier in step (2) has an equivalent pore volume of 15-30 nm in diameter of more than 0.15 mL / g, an equivalent pore volume of 30-100 nm in diameter of more than 0.1 mL / g, and an equivalent pore volume of more than 100 nm in diameter of more than 0.06 mL / g, and a surface hydroxyl density of 4.5-5.5 / nm 2 The compressive strength of the spherical carrier is higher than 60N / particle, the compressive strength of the strip carrier is higher than 120N / cm, and the abrasion is lower than 0.4wt%.

4. The adsorbent according to claim 1, characterized in that In step (1), the platinum / alumina catalyst contains 0.1-0.2 wt% platinum and is prepared by the following method: a catalyst preparation container is purged and replaced with a nitrogen flow saturated with isopropanol vapor, and a catalyst having a specific surface area of ​​4-10 m 2 / g, a pore volume of 0.35-0.4mL / g, and an outer diameter of 44-75μm, continue to purge and replace with a nitrogen flow saturated with isopropanol vapor, add an isopropanol solution containing chloroplatinic acid and 300-400g / L of ethylene glycol at the required concentration during stirring, the amount of the isopropanol solution containing chloroplatinic acid and ethylene glycol added is 25-30wt% of the saturated water absorption of the alumina carrier, after the isopropanol solution is completely absorbed by the carrier, the container is sealed and placed for 6-10h, then the temperature is raised to 70-80℃ and dried under the condition of purging with high-purity nitrogen flow at this temperature range until all the isopropanol is evaporated, the temperature is raised to 130-150℃ and kept at a constant temperature for 0.5-1h, and then dried under the temperature range of 130-150℃ and purging with high-purity nitrogen flow until all the ethylene glycol is evaporated, cooled to room temperature, and the container is sealed to obtain a platinum / alumina catalyst.

5. The method for using the adsorbent according to claim 1, characterized in that: When capturing carbon dioxide from air flow in a fixed bed, the adsorption stage is at 0-30°C, atmospheric pressure or low positive pressure below 50kPa, and air flow velocity of 2000-5000h -1 The process is carried out under the conditions of vacuum thermal desorption or atmospheric pressure thermal desorption to remove the adsorbed CO2 at a desorption temperature of 90-120°C to obtain a carbon dioxide-rich gas stream; finally, the bed is cooled to carry out the next cycle of carbon dioxide capture operation.

6. The adsorbent application method according to claim 5, characterized in that: During the vacuum thermal desorption operation, the adsorbent bed is first heated to 90-100°C by indirect heat exchange and evacuated to an absolute pressure below 50 kPa, or first evacuated to an absolute pressure below 50 kPa and then heated to 90-110°C by indirect heat exchange, and then air or steam is introduced for purging; the exhaust gas during the heating and insulation process of the adsorbent bed and the exhaust gas during purging are collected, cooled by indirect heat exchange, and then fed into a vacuum pump to obtain a carbon dioxide-rich gas flow at the outlet of the vacuum pump.

7. The adsorbent application method according to claim 5, characterized in that: During the atmospheric pressure thermal desorption operation, 100-120°C steam is introduced into the adsorbent bed alone or on the basis of indirect heat exchange as a heating heat source and a purge gas; the exhaust gas during the heating and insulation process of the adsorbent bed and the exhaust gas during the purge are collected, the temperature is lowered by indirect heat exchange, the condensed water is separated, and a carbon dioxide-rich gas flow is obtained. The condensed water is recycled for steam generation, and the excess condensed water is discharged.

8. The method for using the adsorbent according to claim 1, characterized in that: When capturing carbon dioxide from an industrial gas stream with a CO2 content of more than 8% by volume in a fixed bed mode, the gas stream temperature in the adsorption stage is 10-30°C, and the gas stream pressure is normal pressure or positive pressure. After adsorption, the pressure is reduced to an absolute pressure below 3kPa for desorption to obtain a carbon dioxide-rich gas stream with a CO2 content of more than 80% by volume, which is then purged with air and the next cycle of carbon dioxide capture operation is carried out.

9. A mosquito trap, comprising a carbon dioxide capture system, a mosquito trap system and a control system; the carbon dioxide capture system comprises an adsorbent tank and related components, and generates a carbon dioxide-rich gas flow by any method as described in claims 5-7, the adsorbent tank is filled with any adsorbent as described in claims 1-3 in a fixed bed manner, and related components are arranged according to the carbon dioxide capture method; the carbon dioxide-rich gas flow generated by the carbon dioxide capture system is continuously or intermittently sent to the mosquito trap system for use; the control system controls the operation of the carbon dioxide capture system and the mosquito trap system according to a set program.

10. The mosquito trap according to claim 9, characterized in that: The mosquito catching system structurally comprises a mosquito attracting module, a switch type electric damper, a mosquito catching and killing storage module and a rear suction fan. The mosquito catching and killing storage module has a mosquito catching net box. The mosquito catching system attracts mosquitoes attracted by a mixture of carbon dioxide-rich gas and air into the mosquito catching net box along with the strong wind generated by the suction fan.

Citation Information

Patent Citations

  • Structures for capturing CO2, methods of making the structures, and methods of capturing CO2

    US20070149398A1

  • Materials for the direct capture of carbon dioxide from atmospheric air

    US20210187480A1

  • Supported Poly(allyl)amine and Derivatives for CO2 Capture from Flue Gas or Ultra-Dilute Gas Streams Such as Ambient Air or Admixtures Thereof

    US20240024849A1

  • Novel linear polymer as well as preparation method and application thereof

    CN115322368A

  • Application of amine-tethered solid sorbents to co2 fixation from air

    US20110179948A1