High-directivity optical fiber transducer based on hollow optical fiber and manufacturing method of high-directivity optical fiber transducer

By using hollow fibers to weld and fill the composite PDMS material in the photo-ultrasonic transducer, the problems of poor structural complexity and stability in the prior art are solved, and high directional photoacoustic response and low maintenance costs are achieved. Effect, suitable for extreme environments.

CN118988694APending Publication Date: 2024-11-22HARBIN ENG UNIV
View PDF 8 Cites 0 Cited by

Patent Information

Application Number
CN202411154910.5
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-22
Publication Date
2024-11-22

AI Technical Summary

Technical Problem

Existing photoelectric ultrasonic transducers have problems of complexity, high cost and poor stability in structural design and manufacturing, especially in applications in extreme environments, which show instability and high maintenance costs.

Method used

采用基于空心光纤的高方向性光纤换能器设计,利用石英光纤与空心光纤焊接,填充复合PDMS材料,通过光热转换和热声转换实现高效的光声响应,并通过简单的制备工艺降低成本和维护要求。

Benefits of technology

It realizes photo-induced ultrasonic effect with fast photoacoustic response speed, high directionality and low loss. It is suitable for a variety of special environments, reduces maintenance costs and improves the anti-interference ability of the equipment.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118988694A_ABST
    Figure CN118988694A_ABST
Patent Text Reader

Abstract

The invention belongs to the technical field of photoinduced ultrasound, and particularly relates to a high-directivity optical fiber transducer based on a hollow optical fiber and a manufacturing method thereof.The optical fiber transducer comprises a silica optical fiber, the tubular hollow optical fiber is fixed to one end of the silica optical fiber, the hollow optical fiber is filled with a composite PDMS material, and a gap is reserved between the composite PDMS material and the silica optical fiber; the manufacturing method comprises the following steps: S1 to S5, mixing an MWCNT / xylene solution and a PDMS / xylene solution, carrying out ultrasonic oscillation treatment to obtain a composite PDMS material, filling the composite PDMS material into the cavity of the hollow optical fiber, and heating the composite PDMS material to cure the composite PDMS material; and fixedly connecting the hollow optical fiber filled with the composite PDMS material with the silica optical fiber. The optical path design is simplified, the loss is small, the directivity is high, the photoacoustic response speed is high, the preparation is simple, and the method is suitable for various special environments.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of photo-induced ultrasound, and in particular relates to a high-directional optical fiber transducer based on a hollow optical fiber and a manufacturing method thereof. Background Art

[0002] The photoacoustic process involves a complex energy conversion mechanism, which mainly includes two consecutive stages: photothermal conversion and thermoacoustic conversion. In this process, the realization of the photoacoustic effect first depends on photothermal conversion, that is, light energy is absorbed by the light absorbing material and converted into thermal energy. Subsequently, the thermal energy further generates ultrasonic waves through the thermoacoustic conversion process. Ultrasonic transducers based on optical fiber platforms have many advantages over non-optical fiber platforms, such as high sensitivity, wide frequency band distribution, excellent long-distance transmission capability, and lightweight. These characteristics make optical fiber ultrasonic transducers widely used in many fields such as medical imaging, structural health monitoring, industrial process control, acoustic sensing, and ocean detection.

[0003] At present, different structures of photoacoustic ultrasonic transducers have been proposed in domestic and foreign patents. Their structures and designs have their own advantages and disadvantages:

[0004] For example, in the prior art "Optomechanical Effects Occurring in a Hybrid Metal-Halide Perovskite Single Crystal Based on Photoinduced Resonant Ultrasound Spectroscopy", Tisdale Jeremy T et al. from the University of Tennessee in the United States used RUS (resonant ultrasonic spectroscopy) to measure the photoinduced ultrasonic effect in a hybrid metal halide perovskite single crystal under CW (continuous wave) laser irradiation. However, in this study, the RUS measurement technology requires high-precision instruments and complex data analysis, which increases the difficulty and cost of the experiment, while the experimental construction process in this patent content is simple and low-cost.

[0005] For another example, in the prior art "Hybrid optical fiber for light-induced superconductivity.", Evgeny Sedov and others from Vladimir University in Russia designed a superconducting optical fiber with light-induced superconductivity mediated by exciton-polariton Bose-Einstein condensate. However, the stability and durability of the new material used in practical applications still need to be verified, and it may face environmental impact and degradation problems in long-term use. The optical fiber material in this patent content is mature in use and suitable for measurement in a variety of extreme environments such as underwater and plateau areas.

[0006] In addition, after searching related technologies, the following are found:

[0007] First, the Chinese patent with patent application number CN116299837B uses micro-nano optical technology to etch the core on the end face of the optical fiber to form a 45° tilted grating, and uses sputtering and dip coating to manufacture an FP resonant cavity on the end face of the optical fiber to detect the photo-induced ultrasonic echo signal. The graphene array and polystyrene composite material are coated on the multi-mode optical fiber tilted grating pulse laser output as a photo-induced ultrasonic transducer to generate a photo-induced ultrasonic signal for endoscopic imaging. This design involves multiple complex processes such as core etching, sputtering, and dip coating. The manufacturing process is cumbersome and has high requirements for equipment and processes. The optical fiber connection operation in this patent is simple and not easy to damage the optical fiber structure.

[0008] Second, the Chinese patent with patent application number CN107050673A provides a focused photo-induced ultrasound material and its preparation method and an endoscopic photo-induced ultrasound probe. However, the 3D printing technology based on mask image projection stereolithography technology in this design is complex, and the high-precision 3D printing equipment and preparation process have high requirements on the accuracy and stability of the equipment, which increases the manufacturing and maintenance costs. The design structure in this patent content is simple and reduces the use and maintenance costs.

[0009] Based on various studies, the main structures of optical fiber used in the field of photo-induced ultrasound include chemical etching to form an air chamber, thick coating of annular cavity composite PDMS material, etc. The above methods all have corresponding defects, such as chemical etching to form an air chamber is complicated, and the structure is unstable after welding; the direct filling of the annular cavity with composite PDMS material has poor directionality and more heat loss.

[0010] In contrast, the hollow fiber structure for high-directional photoacoustic effect proposed in the present invention has achieved significant improvements in the design and function of the fiber optic transducer. The internal cavity of the hollow fiber is conducive to its filling with composite materials, providing a photoacoustic conversion space. The tube wall of the hollow fiber can naturally guide the propagation direction of the ultrasound after it is generated, improving the directionality of ultrasound transmission, so that it can propagate a longer distance in a specified direction. Secondly, in the method of making the fiber optic transducer, the hollow fiber is welded with the quartz fiber to further enhance the directionality of the system structure. The hollow fiber can also protect the internal composite PDMS material from falling off in the complex environment of the bottom of the water. The overall structure preparation process is simple, which is more conducive to photoacoustic applications with low loss and high directionality requirements. Summary of the invention

[0011] The purpose of the present invention is to provide a high-directivity fiber optic transducer based on hollow fiber and a method for making the same, which simplifies the optical path design, has low loss, high directivity, fast photoacoustic response speed, is easy to prepare, and is suitable for a variety of special environments.

[0012] The technical solution adopted by the present invention is as follows:

[0013] A high-directional fiber optic transducer based on a hollow-core fiber comprises a quartz fiber, a hollow-core fiber is fixed at one end of the quartz fiber, a composite PDMS material is filled inside the hollow-core fiber, a spacing is left between the composite PDMS material and the quartz fiber, when working, the quartz fiber transmits an optical signal, and the composite PDMS material is filled into the air chamber inside the hollow-core fiber for photothermal conversion and thermoacoustic conversion. Compared with traditional thermosensitive materials and thermosensitive circuits, the high-directional fiber optic transducer has rapid response, high photoacoustic conversion efficiency, good mechanical properties, obvious sound frequency vibration, and easy signal collection. The outer wall of the hollow-core fiber plays a certain guiding role in the conduction process after the sound wave is generated, so that the propagation direction of the sound wave is more concentrated, thereby enhancing the effective propagation distance.

[0014] The quartz optical fiber is a single-mode optical fiber or a multi-mode optical fiber.

[0015] The quartz optical fiber includes an outer sheath tube and a fiber core located inside the outer sheath tube;

[0016] Wherein, the diameter of the outer sheath is 60-2000 μm, and the diameter of the fiber core is greater than 5 μm.

[0017] The thickness of the composite PDMS material filled inside the hollow optical fiber is 40-200 μm.

[0018] A method for manufacturing a high-directional fiber optic transducer based on a hollow fiber comprises the following steps:

[0019] S1: Mix MWCNT, 1-pyrenebutyric acid and thionyl chloride, transfer the mixed solution into a round-bottom flask, reflux at 100°C for 30 min to obtain pyrenebutyric acid chloride and remove unreacted thionyl chloride;

[0020] Next, the product from which unreacted thionyl chloride was removed was allowed to stand overnight with oleylamine and triethylamine in tetrahydrofuran;

[0021] Then, the product is washed with ether to remove unreacted tetrahydrofuran, sodium sulfate is added to the washed product, and the product is placed in a vacuum drying oven to dry the MWCNT to a constant weight, thereby obtaining a pyrenebutyryl-functionalized MWCNT product;

[0022] The functionalized MWCNTs are dissolved in xylene, stirred evenly, and then placed in an ultrasonic oscillator for oscillation to obtain a stable MWCNT / xylene solution;

[0023] S2: Mixing the PDMS prepolymer and the PDMS cross-linking agent, weighing xylene as a solvent, pouring the mixed PDMS prepolymer and cross-linking agent mixture into the solvent, and stirring until the PDMS is completely dissolved in the xylene to form a uniform solution;

[0024] S3: taking the MWCNT / xylene solution obtained in step S1, mixing it with the PDMS / xylene solution obtained in step S2, and subjecting it to ultrasonic oscillation treatment to obtain a composite PDMS material;

[0025] S4: filling the composite PDMS material into the hollow optical fiber cavity and then heating the composite PDMS material to solidify it;

[0026] S5: The hollow optical fiber filled with the composite PDMS material is fixedly connected to the quartz optical fiber.

[0027] In the step S1, MWCNT, 1-pyrenebutyric acid and thionyl chloride are mixed in a mass ratio of 1:3:5, and oleylamine and triethylamine are mixed in a mass ratio of 35:71.

[0028] In step S1, the ultrasonic oscillator uses 1 kHz, 5 W ultrasonic oscillation for 1 hour.

[0029] In the step S2, the prepolymer and the PDMS cross-linking agent are mixed in a mass ratio of 10:1.

[0030] The fixed connection in step S5 is to connect the quartz optical fiber and the hollow optical fiber together by fusion welding using an optical fiber welding piece.

[0031] The fixed connection in step S5 is to connect the quartz optical fiber and the hollow optical fiber together by fusion welding using a PI adhesive.

[0032] The technical effects achieved by the present invention are:

[0033] The high-directivity optical fiber transducer based on hollow optical fiber of the present invention simplifies the optical path design, has low loss, high directivity, fast photoacoustic response speed, is simple to prepare, and is suitable for a variety of special environments.

[0034] The invention discloses a high-directional fiber optic transducer based on a hollow-core fiber. The outer wall of the hollow-core fiber plays a certain guiding role in the conduction process of the sound wave after it is generated, so that the propagation direction of the sound wave is more concentrated, thereby enhancing the effective propagation distance.

[0035] The present invention discloses a method for manufacturing a high-directional fiber optic transducer based on a hollow fiber. The single-mode fiber and the hollow fiber are welded to form a relatively sealed air chamber, thereby forming a certain physical wrapping protection for the internal composite PDMS material, further preventing the material from falling off, having strong anti-interference ability, and being able to be flexibly used in special extreme environments, thereby reducing maintenance costs.

[0036] The present invention discloses a method for manufacturing a high-directional fiber optic transducer based on a hollow optical fiber. The composite PDMS material is filled into an air chamber to perform photothermal conversion and thermoacoustic conversion. Compared with traditional thermosensitive materials and thermosensitive circuits, the method has rapid response, high photoacoustic conversion efficiency, good mechanical properties, obvious sound frequency vibration, and easy signal collection.

[0037] The invention discloses a method for manufacturing a high-directional optical fiber transducer based on a hollow optical fiber, which combines PDMS material with a high light absorption material, thereby improving the photosensitivity and thermosensitivity of the PDMS material itself, enhancing the photoacoustic conversion efficiency of the material, and optimizing its mechanical properties so that it can perform photoacoustic conversion better. BRIEF DESCRIPTION OF THE DRAWINGS

[0038] Figure 1 is a cross-sectional view of a high-directivity optical fiber transducer based on a hollow-core optical fiber according to a first embodiment of the present invention;

[0039] Figure 2 is a flow chart of the preparation of the composite PDMS material of Example 2 of the present invention;

[0040] Figure 3 Schematic diagram of the capillary process filling composite PDMS material according to the second embodiment of the present invention;

[0041] Figure 4 This is a schematic diagram of welding a high-directional fiber optic transducer based on a hollow-core fiber according to a second embodiment of the present invention;

[0042] Figure 5 This is a schematic diagram of bonding a high-directional fiber optic transducer based on a hollow-core fiber according to a fourth embodiment of the present invention;

[0043] Figure 6 It is a schematic structural diagram of a hollow-core optical fiber reserved air cavity according to a fifth embodiment of the present invention.

[0044] In the accompanying drawings, the components represented by the reference numerals are listed as follows:

[0045] 1. Quartz optical fiber; 2. Hollow optical fiber; 3. Composite PDMS material; 4. Optical fiber welding parts; 5. PI adhesive parts. DETAILED DESCRIPTION

[0046] In order to make the purpose and advantages of the present invention more clearly understood, the present invention is specifically described below in conjunction with embodiments. It should be understood that the following text is only used to describe one or several specific embodiments of the present invention, and does not strictly limit the scope of protection of the specific claims of the present invention.

[0047] Embodiment 1:

[0048] like Figure 1As shown, a high-directional fiber optic transducer based on hollow-core fiber comprises a quartz fiber 1, a hollow-core fiber 2 is fixed at one end of the quartz fiber 1, a composite PDMS material 3 is filled inside the hollow-core fiber 2, and a gap is left between the composite PDMS material 3 and the quartz fiber 1. When working, the quartz fiber 1 transmits optical signals, and the composite PDMS material 3 is filled into the air chamber inside the hollow-core fiber 2 for photothermal conversion and thermoacoustic conversion. Compared with traditional thermosensitive materials and thermosensitive circuits, it has rapid response, high photoacoustic conversion efficiency, good mechanical properties, obvious sound frequency vibration, and easy signal collection. The outer wall of the hollow-core fiber 2 plays a certain guiding role in the conduction process after the sound wave is generated, so that the propagation direction of the sound wave is more concentrated, thereby enhancing the effective propagation distance.

[0049] like Figure 1 As shown, the quartz optical fiber 1 is a single-mode optical fiber or a multi-mode optical fiber, which can transmit multiple groups of optical signals when working, and change the rate of photothermal conversion and thermoacoustic conversion of the composite PDMS material 3.

[0050] like Figure 1 As shown, the quartz optical fiber 1 includes an outer sheath tube and a fiber core located inside the outer sheath tube. The diameter of the outer sheath tube is 60-2000 μm, and the diameter of the fiber core is greater than 5 μm. A thicker outer sheath tube is used to strictly protect the fiber core to reduce the possibility of damage to the fiber core.

[0051] like Figure 1 As shown, the thickness of the composite PDMS material 3 filled inside the hollow optical fiber 2 is 40-200 μm, and the cross-sectional area of ​​the composite PDMS material 3 is much larger than the cross-sectional area of ​​the fiber core, and can transmit all the optical signals transmitted by the fiber core as much as possible.

[0052] Embodiment 2:

[0053] like Figure 2 As shown, a method for preparing a high-directional optical fiber transducer based on a hollow fiber, step S1: the functionalization method of MWCNT pyrenebutyric acid is as follows: 1g MWCNT, 3g 1-pyrenebutyric acid and 5g thionyl chloride are mixed, and the mixed solution is transferred to a 25ml round-bottom flask, and refluxed at 100°C for 30min to obtain pyrenebutyric chloride and remove unreacted thionyl chloride;

[0054] Next, the product was allowed to stand overnight with 3.5 mg of oleylamine and 7.1 mg of triethylamine in 15 ml of tetrahydrofuran;

[0055] Then, the product was washed with 20 ml of ether to remove unreacted tetrahydrofuran, sodium sulfate was added to the washed product, and the product was placed in a vacuum drying oven to dry the MWCNT at 60° C. to a constant weight, thereby obtaining a pyrenebutyryl-functionalized MWCNT product;

[0056] The functionalized MWCNT was dissolved in 90 g of xylene, stirred evenly, and then placed in an ultrasonic oscillator and subjected to ultrasonic oscillation at 1 kHz and 5 W for 1 h to obtain a stable MWCNT / xylene solution;

[0057] Step S2: in the process of preparing the composite material, PDMS and the functionalized MWCNT are mixed in a xylene solution to achieve uniform dispersion of the MWCNT in the PDMS material;

[0058] 10 mg of PDMS prepolymer and 1 mg of PDMS cross-linking agent were mixed in a ratio of 10:1, and 89 g of xylene was weighed as a solvent. The weighed PDMS prepolymer and cross-linking agent mixture was poured into the xylene solution and stirred with a magnetic stirrer until PDMS was completely dissolved in the xylene to form a uniform solution;

[0059] Step S3: 90 g of the MWCNT / xylene solution obtained in step S1 is mixed with the PDMS / xylene solution obtained in step S2 and subjected to ultrasonic oscillation treatment;

[0060] After ultrasonic vibration, the solution was stirred for 10 min using a high-speed stirrer to ensure that the MWCNTs were evenly dispersed in the PDMS xylene solution and to further improve the uniformity;

[0061] If, during the stirring process, bubbles exist in the solution, the mixed solution can be placed in a vacuum degassing device for degassing;

[0062] During the operation, it is necessary to check the distribution of MWCNT in the solution to ensure that it is evenly dispersed;

[0063] Step S4: According to the hollow-core optical fiber 2, the composite PDMS material solution 3 should be filled into the inner cavity of the hollow-core optical fiber, and the hollow-core optical fiber is cleaned to ensure that the inside of the optical fiber is clean and free of dust and impurities; ethanol or other suitable solvents are used to clean the hollow-core optical fiber;

[0064] After standing and drying, the prepared liquid composite PDMS material 3 is placed in a clean reagent tube; one end of the hollow core optical fiber 2 is directly and gently inserted into the solution, such as Figure 3 As shown, due to the capillary phenomenon, the liquid will naturally fill into the cavity of the hollow-core optical fiber 2 along the hollow-core optical fiber 2. When a certain amount of liquid is introduced into the hollow-core optical fiber 2, the hollow-core optical fiber 2 is immediately lifted to observe the height of the composite PDMS material 3 entering the cavity of the hollow-core optical fiber 2. Generally, the photo-induced ultrasonic efficiency of the polymer composite PDMS material 3 with a thickness between 40 and 200 μm is the best. Therefore, it is necessary to repeatedly use the capillary phenomenon to make the liquid composite PDMS material 3 enter the internal cavity of the hollow-core optical fiber 2 until the hollow-core optical fiber 2 is filled to a predetermined length.

[0065] Afterwards, the position of the composite PDMS material 3 is further adjusted so that the end of the material is 30 to 50 μm away from the end of the hollow-core optical fiber 2. The hollow-core optical fiber 2 is horizontally placed in a high-temperature drying oven for heating at 80° C. for 40 min to cure the composite PDMS material 3 to form a composite PDMS material layer.

[0066] Step S5: Connect the hollow optical fiber 2 filled with the composite PDMS material 3 to the quartz optical fiber 1 by fusion splicing to achieve high-precision alignment and low-loss connection, and place the optical fibers at both ends in a precision optical fiber cutter for cutting to ensure that the cut surface is flat and smooth without notches or bevels;

[0067] After cutting, use a high-power microscope to check the fiber section to ensure that it is perfectly flat to ensure welding quality. Place the fiber in the fixed groove of the fiber fusion splicer, align the fiber core center axis, and start the fusion splicer for welding.

[0068] During the fusion splicing process, the end face of the optical fiber is melted by electric arc heating, and the two ends of the optical fiber are butt-jointed in the molten state. Figure 4 As shown, the optical fiber welding part 4 is matched and coated at the welding position, wherein the optical fiber welding part 4 can use 353ND optical fiber curing glue;

[0069] After the fusion splicing is completed, the strength test function of the fusion splicer is used to perform a tensile test on the fusion point to ensure a firm connection, thus completing the preparation of a composite PDMS material-filled air-gap double-core optical fiber for triggering a highly directional photo-induced ultrasonic effect.

[0070] The dosage of materials used in this method is shown in Table 1 below:

[0071] Ingredients Table 1

[0072]

[0073]

[0074] Embodiment three:

[0075] The design and production process is the same as that of Example 2. For similarities, please refer to Example 2. Figure 2 As shown, the difference is that after preparing the composite PDMS material 3 in step S3, 0.5 mg of powdered AuNP material is additionally added, and the ultrasonic oscillator is used to perform ultrasonic oscillation at 1 kHz and 5 W for 30 min to disperse the AuNP in the composite material solution to form a composite.

[0076] PDMS-MWCNT-AuNP materials;

[0077] The introduction of AuNP material will further enhance the absorption efficiency of the composite PDMS material itself for light in a specific band. The size of AuNP is usually between 1 and 100 nm and can have different shapes, such as sphere, rod, star, etc. Changes in shape and size will lead to changes in the local surface LSPR (plasmon resonance) effect. The LSPR of spherical AuNP usually appears in the visible light range. As the particle size increases, the LSPR peak red-shifts, further enhancing the absorption efficiency of this band, thereby further improving the photo-induced ultrasound efficiency of the system.

[0078] Embodiment 4:

[0079] The design and production process is the same as that of Example 2. For similarities, please refer to Example 2. Figure 5 As shown, the difference is that: the method of connecting the single-mode optical fiber and the hollow-core optical fiber in step S5 is to use PI adhesive 5 (polyimide) to bond the optical fiber, and before connecting the single-mode optical fiber and the hollow-core optical fiber, use an optical fiber cutter to cut the optical fiber end face to make it flat and smooth, and clean the optical fiber end face with alcohol and a dust-free cloth to ensure that there is no dirt or grease;

[0080] Preferably, the 0.5mgPI adhesive 5 is evenly coated on the end faces of the single-mode optical fiber and the hollow optical fiber, and aligned with the optical fiber end face again after coating;

[0081] Then, the welding point is initially dried, the temperature of the bonding point is controlled to be 80-120°C, and the drying time is 30 minutes, so that the PI film gradually hardens;

[0082] The temperature of the bonding point is increased to 150-200°C, the pre-curing time is 20 minutes, the temperature of the bonding point is increased to 300-500°C, and the full curing time is 2 hours. The performance of the PI adhesive 5 is further enhanced through the full curing process. After cooling, the optical fiber bonding condition is verified, and the mechanical properties and light transmission conditions of the optical fiber bonding point are verified.

[0083] Since the composite PDMS material may decompose at a high temperature, and the temperature of the welding end of the optical fiber welding machine is 1500-1700°C, there is a potential problem of denaturing the components of the composite PDMS material when directly using the optical fiber welding machine for welding.

[0084] Therefore, in Example 4, PI adhesive 5 is selected for bonding single-mode optical fiber and hollow optical fiber. The curing temperature of PI adhesive 5 is 700°C, and there is no problem of decomposition and denaturation of the composite PDMS material. PI adhesive 5 is resistant to aging and solvents, and has stable chemical properties, and can be used for bonding silicon-based materials.

[0085] Embodiment five:

[0086] The design and production process are the same as those in Example 2. The similarities can be referred to in Example 2. The difference is that in step S4: in the process of introducing the composite PDMS material into the hollow optical fiber by using the capillary phenomenon, an air chamber is reserved at the end, such as Figure 6 As shown;

[0087] After using capillary phenomenon to introduce the composite PDMS material into the hollow-core optical fiber, a micro-injection pump is used to blow the composite PDMS material in the hollow-core optical fiber to the other end face of the hollow-core optical fiber until an air chamber with a width of 40 μm is reserved at the end face of the welding side of the hollow-core optical fiber, and then the composite PDMS material is cured.

[0088] Embodiment six:

[0089] like Figure 5 As shown, the design and production process is the same as that of Example 2, except that in step S1, step S2, and step S3: the composite PDMS material is prepared by mixing a PDMS material solution with 0.1 mg of spherical AuNP material;

[0090] 0.5 mg of powdered AuNP material was added, and the AuNP was dispersed in the composite material solution by ultrasonic oscillation at 1 kHz and 5 W for 30 min.

[0091] Embodiment seven:

[0092] like Figure 5 As shown, the design and production process are the same as that of Example 2, except that in step S1, step S2, and step S3: the composite PDMS material is prepared by mixing 10 ml of PDMS material solution and Sudan red solution material, and Sudan red type II is preferred in this embodiment.

[0093] For detailed description, the applicant lists the following Table 2 for explanation:

[0094] Table 2

[0095] Sudan red dye parameter Preference or range Example Reference Dosage Sudan Red Type I 0.625~10(ng / mL) 5.00ml 6ml Sudan Red Type II 0.625~10(ng / mL) 8.00ml 8ml Sudan red type III 0.625~10(ng / mL) 10.00ml 10ml Sudan IV 0.625~10(ng / mL) 10.00ml 10ml 2-AA 0.75~10(ng / mL) 8.00ml 8ml

[0096] When using:

[0097] The experimental process is the same as that of Example 2, except that: 10 g of PDMS prepolymer and 1 g of cross-linking agent are weighed and added into 89 g of xylene;

[0098] Then use a magnetic stirrer to stir until PDMS is completely dissolved to form a uniform solution;

[0099] Then, 8 ml of Sudan Red Type II material was added to the solution. After the addition, the mixed solution was placed in an ultrasonic oscillator and treated with 1 kHz, 5 W ultrasonic oscillation for 30 minutes until a uniform and stable solution was formed to form a composite PDMS material.

[0100] The above is only a preferred embodiment of the present invention. It should be noted that, for those skilled in the art, several improvements and modifications can be made without departing from the principles of the present invention, and these improvements and modifications should also be considered as the protection scope of the present invention. The structures, devices and operating methods not specifically described and explained in the present invention shall be implemented according to the conventional means in the art unless otherwise specified and limited.

Claims

1. A highly directional fiber optic transducer based on hollow-core fiber, Features: The invention comprises a quartz optical fiber (1), wherein a hollow optical fiber (2) is fixed at one end of the quartz optical fiber (1), a composite PDMS material (3) is filled inside the hollow optical fiber (2), and a distance is left between the composite PDMS material (3) and the quartz optical fiber (1).

2. A high-directivity fiber optic transducer based on hollow-core fiber according to claim 1, Features: The quartz optical fiber (1) is a single-mode optical fiber or a multi-mode optical fiber.

3. A high-directivity fiber optic transducer based on hollow-core fiber according to claim 1, Features: The quartz optical fiber (1) comprises an outer sheath tube and a fiber core located inside the outer sheath tube; Wherein, the diameter of the outer sheath is 60-2000 μm, and the diameter of the fiber core is greater than 5 μm.

4. A high-directivity fiber optic transducer based on hollow-core fiber according to claim 1, Features: The thickness of the composite PDMS material (3) filled inside the hollow optical fiber (2) is 40 to 200 μm.

5. A method for manufacturing a high-directional fiber optic transducer based on hollow-core fiber, Features: A highly directional fiber optic transducer based on a hollow-core fiber as described in any one of claims 1 to 4, comprising the following steps: S1: Mix MWCNT, 1-pyrenebutyric acid and thionyl chloride, transfer the mixed solution into a round-bottom flask, reflux at 100°C for 30 min to obtain pyrenebutyric acid chloride and remove unreacted thionyl chloride; Next, the product from which unreacted thionyl chloride was removed was allowed to stand overnight with oleylamine and triethylamine in tetrahydrofuran; Then, the product is washed with ether to remove unreacted tetrahydrofuran, sodium sulfate is added to the washed product, and the product is placed in a vacuum drying oven to dry the MWCNT to a constant weight, thereby obtaining a pyrenebutyryl-functionalized MWCNT product; The functionalized MWCNTs are dissolved in xylene, stirred evenly, and then placed in an ultrasonic oscillator for oscillation to obtain a stable MWCNT / xylene solution; S2: Mixing the PDMS prepolymer and the PDMS cross-linking agent, weighing xylene as a solvent, pouring the mixed PDMS prepolymer and cross-linking agent mixture into the solvent, and stirring until the PDMS is completely dissolved in the xylene to form a uniform solution; S3: taking the MWCNT / xylene solution obtained in step S1, mixing it with the PDMS / xylene solution obtained in step S2, and subjecting it to ultrasonic oscillation treatment to obtain a composite PDMS material (3); S4: filling the composite PDMS material (3) into the cavity of the hollow optical fiber (2), and then heating the composite PDMS material (3) to solidify it; S5: The hollow optical fiber (2) filled with the composite PDMS material (3) and the quartz optical fiber (1) are fixedly connected together.

6. The method for manufacturing a high-directional fiber optic transducer based on a hollow fiber according to claim 5, Features: In the step S1, MWCNT, 1-pyrenebutyric acid and thionyl chloride are mixed in a mass ratio of 1:3:5, and oleylamine and triethylamine are mixed in a mass ratio of 35:

71.

7. The method for manufacturing a high-directional fiber optic transducer based on a hollow fiber according to claim 5, Features: In step S1, the ultrasonic oscillator uses 1 kHz, 5 W ultrasonic oscillation for 1 hour.

8. The method for manufacturing a high-directional fiber optic transducer based on a hollow fiber according to claim 5, Features: In the step S2, the prepolymer and the PDMS cross-linking agent are mixed in a mass ratio of 10:

1.

9. The method for manufacturing a high-directional fiber optic transducer based on a hollow fiber according to claim 5, Features: The fixed connection in step S5 is achieved by connecting the quartz optical fiber (1) and the hollow optical fiber (2) together by fusion welding using an optical fiber welding piece (4).

10. The method for manufacturing a high-directional fiber optic transducer based on a hollow fiber according to claim 9, Features: The fixed connection in step S5 is achieved by using a PI adhesive (5) to connect the quartz optical fiber (1) and the hollow optical fiber (2) together by fusion welding.

Citation Information

Patent Citations

  • Focusing photoinduced ultrasound material, preparation method thereof and endoscopic photoinduced ultrasound probe

    CN107050673A

  • A method for preparing an all-optical lateral photo-induced ultrasound self-generating and self-retracting fiber optic endoscope

    CN116299837B

  • Double-C-type cavity-based sensitive membrane embedded optical fiber hydrogen sensor

    CN108152220A

  • Distributed optical fiber laser ultrasonic transduction device based on no-core fiber

    CN108927314A

  • Sensitivity-enhanced composite multi-cavity FPI temperature sensor, preparation method and application

    CN115638894A