Horizontal structure LED chip and preparation method thereof
By etching the P-type contact layer in the LED chip to form a protrusion and a dielectric layer, and combining the hot press bonding technology, the problems of low light extraction efficiency and poor reliability in the prior art are solved, and high-efficiency light extraction and reliability are achieved promote.
Patent Information
- Application Number
- CN202411162498.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-23
- Publication Date
- 2024-11-26
- Estimated Expiration
- 2044-08-23
AI Technical Summary
In the process of improving the light extraction efficiency, existing LED chips are prone to damage the active layer and have low reliability, especially in the process of solid crystal and wire bonding, there is a risk of epitaxial layer fragmentation.
Using the horizontal structure LED chip preparation method, the protrusion is formed by etching the P-type contact layer, and a dielectric layer and a metal reflective layer are formed on the top of it. The protrusion height and the refractive index of the dielectric layer are controlled to form a micro-reflective mirror to reduce the P-type contact. The layer absorbs light and fills the gap by hot press bonding to avoid cavity formation.
It effectively improves the light extraction efficiency, avoids active layer damage, improves chip reliability, reduces production costs, and reduces the risk of epitaxial layer fragmentation during crystal solidification and wire bonding.
Smart Images

Figure CN119029104A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of semiconductor optoelectronic devices, and in particular to a horizontal structure LED chip and a preparation method thereof. Background Art
[0002] At present, the ODR reflective structure formed by the composite of the DBR layer and the metal layer is a relatively new way to improve the light extraction rate of LED chips. It is mainly divided into three types: one is a horizontal structure of the dielectric layer + a horizontal structure of the metal reflective layer. The reflector area of this ODR reflective structure is small, and it is difficult to effectively increase the reflective area, and the effect of improving the light extraction efficiency is poor. The other is to etch away part of the active area to form a reflector with a certain angle. Although this solution effectively increases the area of the ODR reflector and changes the angle of the reflector, this solution requires etching away part of the active area. On the one hand, it reduces the area of the effective light-emitting area. On the other hand, the damage caused by etching the active area may cause reliability problems such as leakage. Another solution is to form a micro-vacuum structure with hemispherical grooves to improve the light reflectivity, but this structure has a cavity of the quasi-vacuum layer inside the chip. When the solid crystal, welding wire, etc. are subjected to external pressure, the risk of epitaxial layer fragmentation will be greatly increased. Summary of the invention
[0003] The technical problem to be solved by the present invention is to provide a horizontal structure LED chip and a preparation method thereof, which can effectively improve the light extraction efficiency without damaging the active layer and has higher reliability.
[0004] In order to solve the above technical problems, the present invention provides a method for preparing a horizontal structure LED chip, which comprises the following steps:
[0005] S1. Providing an epitaxial wafer, wherein the epitaxial wafer comprises a first substrate and an N-type semiconductor layer, an active layer, and a P-type semiconductor layer sequentially arranged on the first substrate; the P-type semiconductor layer comprises a first preset region and a second preset region;
[0006] S2, etching the P-type contact layer to form a plurality of protrusions in a first preset area, and providing grooves between adjacent protrusions; the height of the protrusions is less than or equal to 50% of the thickness of the P-type contact layer;
[0007] S3, forming a dielectric layer on the epitaxial wafer obtained in step S2, wherein the thickness of the dielectric layer is less than the depth of the groove, and the refractive index of the dielectric layer is less than the refractive index of the P-type contact layer;
[0008] S4, etching the dielectric layer to form a plurality of first through holes exposing the protrusions on the tops of the protrusions;
[0009] S5, forming a metal reflective layer on the epitaxial wafer obtained in step S4, wherein the metal reflective layer fills the groove;
[0010] S6, forming a bonding layer on the metal reflective layer;
[0011] S7, bonding the epitaxial wafer obtained in step S6 to the second substrate;
[0012] S8, removing the first substrate to expose the N-type semiconductor layer;
[0013] S9, forming an N electrode on the N-type semiconductor layer to obtain an intermediate;
[0014] S10, forming a plurality of second through holes etched to the P-type contact layer on the intermediate body; the second through holes are arranged in the second preset area;
[0015] S11, forming a P electrode on the intermediate obtained in step S10 to obtain an LED wafer; the P electrode is electrically connected to the P electrode through the second through hole;
[0016] S12, cutting the LED wafer to obtain horizontal structure LED chips.
[0017] As an improvement of the above technical solution, step S10 includes:
[0018] S101: forming a plurality of second through holes etched to the P-type contact layer on the intermediate body, wherein the second through holes are arranged in the second preset area;
[0019] S102: forming a plurality of third through holes etched to the metal reflective layer in the second through hole; the P electrode is electrically connected to the metal reflective layer through the third through holes.
[0020] As an improvement of the above technical solution, the bonding layer is an Au layer or an Ag layer, and its thickness is 300nm to 800nm;
[0021] In step S8, a Ag layer or an Au layer is provided on the surface of the second substrate; the epitaxial wafer obtained in step S7 is bonded to the second substrate by thermal compression bonding, and during bonding, the metal reflective layer and the bonding layer are pressed against each other to fill the gap on the surface of the epitaxial wafer;
[0022] The bonding temperature is 200° C. to 360° C., and the bonding pressure is 8000 kgf to 15000 kgf.
[0023] As an improvement of the above technical solution, step S5 includes:
[0024] S51: forming a metal reflective layer on the epitaxial wafer obtained in step S4;
[0025] S52: Annealing the epitaxial wafer obtained in step S51 so that the metal reflective layer forms an ohmic contact with the P-type contact layer.
[0026] As an improvement of the above technical solution, the thickness of the P-type contact layer is 1 μm to 10 μm, and its doping concentration is ≥ 1×10 18 cm -3 ; and / or
[0027] The protrusions are in the shape of a truncated cone, an ellipsoidal crown or a prism, the height of the protrusions is 0.5 μm to 5 μm, and the distance between adjacent protrusions is 0.5 μm to 10 μm; and / or
[0028] The height of the protrusion is 20% to 35% of the thickness of the P-type contact layer; and / or
[0029] The dielectric layer is one or more of a SiO2 layer, a MgF2 layer, a TiO2 layer, and a Ti2O5 layer; the thickness of the dielectric layer is 0.2 μm to 4 μm; and / or
[0030] The metal reflective layer is one or more of an Au layer, an Ag layer, and an Al layer, and the thickness of the metal reflective layer is 0.5 μm to 10 μm.
[0031] As an improvement of the above technical solution, the thickness of the P-type contact layer is 2 μm to 4 μm, and its doping concentration is 2×10 18 cm -3 ~5×10 20 cm -3 ; and / or
[0032] The protrusions are truncated cone-shaped, the height of the protrusions is 0.5 μm to 1.8 μm, and the distance between adjacent protrusions is 0.5 μm to 3 μm; and / or
[0033] The dielectric layer is a SiO2 layer with a thickness of 0.3 μm to 1 μm; and / or
[0034] The metal reflective layer is an Au layer, and the thickness thereof is 0.8 μm to 2 μm.
[0035] As an improvement of the above technical solution, the doping concentration of the P-type contact layer increases gradually from the side close to the active layer to the side close to the dielectric layer.
[0036] As an improvement of the above technical solution, the epitaxial wafer includes a first substrate, an N-type GaAs buffer layer, an N-type GaInP etching stop layer, an N-type semiconductor layer, an active layer, a P-type semiconductor layer and a P-type contact layer sequentially arranged on the first substrate;
[0037] The first substrate is a GaAs substrate;
[0038] The second substrate is a sapphire substrate;
[0039] The N-type semiconductor layer includes an N-type GaAs ohmic contact layer, an N-type AlGaInP roughening layer and an N-type AlGaInP current spreading layer, which are arranged on the N-type GaInP etching stop layer in sequence;
[0040] The P-type semiconductor layer is a P-type AlGaInP confinement layer;
[0041] The P-type contact layer is a P-type GaP window layer.
[0042] As an improvement of the above technical solution, in step S9, the first substrate and the N-type GaInP etching stop layer are removed to expose the N-type GaAs ohmic contact layer, and the N-type GaAs ohmic contact layer is etched to form a contact pattern;
[0043] In step S9, an N electrode is formed on the contact pattern, and the N-type AlGaInP roughening layer is roughened;
[0044] In step S11, a P electrode is first formed on the intermediate body obtained in step S10, and then a passivation protection layer is formed, and then etching is performed to expose the N electrode and the P electrode, so as to obtain an LED wafer.
[0045] Correspondingly, the present invention also discloses a horizontal structure LED chip, which is prepared by the above-mentioned preparation method of the horizontal structure LED chip.
[0046] The implementation of the present invention has the following beneficial effects:
[0047] 1. In the preparation method of the horizontal structure LED chip of the present invention, a process of etching the P-type contact layer to form a protrusion - forming a dielectric layer - etching the dielectric layer to form a first through hole - forming a metal reflective layer is adopted to form a micro-reflector. Based on this process: First, by controlling the height of the protrusion to be less than or equal to 50% of the thickness of the P-type contact layer, it is avoided that the MQW active area is damaged by etching too deep, and the effective light-emitting area is not lost. Second, etching thins the P-type contact layer and reduces the light absorption of the P-type contact layer. Third, by controlling the refractive index of the dielectric layer to be less than the refractive index of the P-type contact layer, and the composite metal reflective layer, a micro-reflector structure is formed, which greatly increases the reflection area of the micro-reflector, changes the reflection angle, improves the light reflectivity, and thus improves the light extraction efficiency. Fourth, the layers are tightly combined without gaps, which avoids damage to the LED chip during later solid crystal and wire bonding, thereby improving reliability.
[0048] 2. In the preparation method of the horizontal structure LED chip of the present invention, the P electrode is electrically connected to the metal reflective layer through the third through hole, and the metal reflective layer is connected to the P-type contact layer through the first through hole of the array. Through this structure, the uniformity of current injection is greatly improved, the thickness of the P-type contact layer is reduced, the light absorption is reduced, the light extraction efficiency is further improved, and the production cost is also reduced.
[0049] 3. In the method for preparing the horizontal structure LED chip of the present invention, the shape of the protrusion is controlled to be an ellipsoid crown, a truncated cone, or a prism, so that the top is small and the bottom is large, and the protrusion has an inclined surface, which can effectively increase the reflection area and change the reflection angle.
[0050] 4. In the preparation method of the horizontal structure LED chip of the present invention, by controlling the materials of the metal reflective layer and the bonding layer and selecting the hot pressing bonding process, during the bonding process, the ductile metal is squeezed to fill the pits without leaving any gaps, that is, there is no cavity inside the chip. During the processes of solid crystal and wire bonding, the risk of the epitaxial layer being broken due to pressure can be greatly reduced. BRIEF DESCRIPTION OF THE DRAWINGS
[0051] Figure 1 is a schematic structural diagram of an epitaxial wafer in one embodiment of the present invention;
[0052] Figure 2 is a schematic diagram of the structure of the epitaxial wafer after step S2 in one embodiment of the present invention;
[0053] Figure 3 is a schematic diagram of the structure of the epitaxial wafer after step S4 in one embodiment of the present invention;
[0054] Figure 4 is a schematic diagram of the structure of the epitaxial wafer after step S6 in one embodiment of the present invention;
[0055] Figure 5 is a schematic diagram of the structure of the epitaxial wafer after step S7 in one embodiment of the present invention;
[0056] Figure 6 is a schematic diagram of the structure of the epitaxial wafer after step S8 in one embodiment of the present invention;
[0057] Figure 7 is a schematic diagram of the structure of the intermediate after step S9 in one embodiment of the present invention;
[0058] Figure 8 is a schematic diagram of the structure of a horizontal structure LED chip after step S12 in one embodiment of the present invention;
[0059] Fig. 9 is a schematic diagram of a top view of a horizontal structure LED chip in one embodiment of the present invention;
[0060] In the figure, 1 is an epitaxial wafer, 11 is a first substrate, 12 is an N-type semiconductor layer, 121 is an N-type GaAs ohmic contact layer, 122 is an N-type AlGaInP roughening layer, 123 is an N-type AlGaInP current spreading layer, 124 is an N-type AlGaInP limiting layer, 13 is an active layer, 14 is a P-type semiconductor layer, 15 is a P-type contact layer, 151 is a first preset area, 152 is a second preset area, 153 is a protrusion, 154 is a groove, 155 is a third through hole, 16 is an N-type GaAs buffer layer, 17 is an N-type GaInP corrosion stop layer, 2 is a dielectric layer, 21 is a first through hole, 3 is a metal reflective layer, 5 is a second substrate, 51 is a sub-bonding layer, 6 is an N-electrode, 61 is an N-electrode extension strip, 7 is an intermediate, 71 is a second through hole, 8 is a P-electrode, and 9 is a passivation protection layer. DETAILED DESCRIPTION
[0061] In order to make the purpose, technical solutions and advantages of the present invention more clear, the present invention is described in further detail below.
[0062] The present invention provides a method for preparing a horizontal structure LED chip, which comprises the following steps:
[0063] S1: Provide epitaxial wafers;
[0064] Ginseng Figure 1 , the epitaxial wafer 1 includes a first substrate 11, and an N-type semiconductor layer 12, an active layer 13, a P-type semiconductor layer 14 and a P-type contact layer 15 sequentially arranged on the first substrate 11. Specifically, the LED chip of the present invention can be a red light, green light, yellow light or purple light LED chip, and different types of semiconductor layers, active layers and contact layers can be selected based on the control of the emission wavelength. Exemplarily, in one embodiment, when the LED chip is a blue light LED chip or a green light LED chip, the N-type semiconductor layer 12 can be an N-type GaN layer, the active layer 13 can be an InGaN-GaN type multi-quantum well layer, the P-type semiconductor layer 14 can be a P-type GaN layer, and the P-type contact layer 15 can be a P-type InGaN layer or a highly doped P-type GaN layer, but is not limited thereto. In another embodiment, when the LED chip is a purple LED chip, the N-type semiconductor layer 12 may be an N-type AlGaN layer, the active layer 13 may be an AlGaN-AlGaN type multi-quantum well layer, the P-type semiconductor layer 14 may be a P-type AlGaN layer, and the P-type contact layer 15 may be a P-type GaN layer, but is not limited thereto.
[0065] Preferably, in one embodiment, the LED chip is a red LED chip, and the epitaxial wafer 1 includes an N-type GaAs buffer layer 16, an N-type GaInP etching stop layer 17, an N-type semiconductor layer 12, an active layer 13, a P-type semiconductor layer 14 and a P-type contact layer 15 sequentially arranged on a first substrate 11. Among them, the first substrate 11 is a GaAs substrate. The N-type semiconductor layer 12 includes an N-type GaAs ohmic contact layer 121, an N-type AlGaInP roughening layer 122, an N-type AlGaInP current spreading layer 123 and an N-type AlGaInP limiting layer 124 sequentially arranged on the N-type GaInP etching stop layer 17; the P-type semiconductor layer is a P-type AlGaInP limiting layer; and the P-type contact layer 15 is a P-type GaP window layer. The following steps are described with reference to a red LED chip, but the technical solution of the present invention is not limited to the red LED chip described herein.
[0066] Specifically, the thickness of the P-type contact layer 15 is 1 μm to 10 μm. If the thickness is too small, the active layer 13 is easily damaged when etching to form the protrusion 153, thereby reducing the luminous efficiency. At the same time, it also affects the current expansion function of the P-type contact layer 15. In addition, the height of the formed protrusion 153 is small, and the effect of improving the light extraction efficiency is weak. If the thickness is greater than 10 μm, too much light is absorbed, thereby reducing the light extraction efficiency. Preferably, the thickness of the P-type contact layer 15 is 1 μm to 5 μm, and more preferably 1.5 μm to 4 μm.
[0067] The P-type contact layer 15 includes a first preset region 151 and a second preset region 152 . The first preset region is subsequently etched to form a protrusion 153 and a groove 154 . The P-type contact layer 15 in the second preset region 152 is not etched to form a protrusion 153 .
[0068] Specifically, the P-type doping concentration of the P-type contact layer 15 is ≥ 1×10 18 cm -3 Preferably, the P-type doping concentration of the P-type contact layer 15 is 2×10 18 cm -3 ~5×10 20 cm -3 . More preferably, the doping concentration of the P-type contact layer 15 increases from the side 13 close to the active layer to the side close to the dielectric layer 2, that is, the doping concentration of the surface layer is greater than the doping concentration of the bottom layer. Based on the above-mentioned doping concentration control, on the one hand, the P-type contact layer with a high doping concentration in the subsequent second preset area is retained, thereby improving the ohmic contact with the metal reflective layer; on the other hand, a lower doping concentration in the bottom layer can reduce defects, reduce light absorption, and reduce the adverse effects of leakage channels formed by etching when forming protrusions 153 and grooves 154.
[0069] S2: etching the P-type contact layer to form a plurality of protrusions in the first preset area;
[0070] Among them, reference Figure 2 The protrusion 153 is small at the top and large at the bottom, and its side has an inclined surface, a curved surface or a spherical surface, which can effectively increase the reflection area, change the reflection angle, and improve the light extraction efficiency. Preferably, the protrusion 153 is in the shape of a truncated cone, an ellipsoid crown or a prism, but is not limited thereto. More preferably, it is in the shape of a truncated cone.
[0071] Specifically, the height of the protrusion 153 is less than or equal to 50% of the thickness of the P-type contact layer 15 to prevent the active layer 13 from being damaged by excessive etching, without losing the effective light-emitting area, and also weakening the adverse effect on the current expansion function of the P-type contact layer 15. Preferably, the height of the protrusion 153 is 20% to 40% of the thickness of the P-type contact layer 15, and more preferably 20% to 35%.
[0072] Specifically, the height of the protrusion 153 is 0.5 μm to 5 μm, preferably 0.5 μm to 1.8 μm.
[0073] The protrusions 153 are arranged in an array, and the distance between adjacent protrusions 153 is 0.5 μm to 10 μm. If the distance is too small, the ohmic contact function of the P-type contact layer 15 is affected. If the distance is too large, less light is reflected, and the effect of improving the light extraction efficiency is limited. Preferably, the distance between adjacent protrusions 153 is 0.5 μm to 4 μm, and more preferably 0.5 μm to 3 μm. A groove 154 is provided between adjacent protrusions 153. Preferably, in one embodiment, reference Fig. 9 The protrusions 153 cover the entire first preset area (ie, the light-emitting area), which can improve the light-emitting efficiency and further optimize the current distribution.
[0074] Specifically, the P-type contact layer 15 can be etched by dry etching or wet etching, but is not limited thereto. Preferably, the P-type contact layer 15 is etched by dry etching, which has high etching accuracy and can better control the distribution and shape of the protrusions 153.
[0075] S3: forming a dielectric layer on the epitaxial wafer obtained in step S2;
[0076] The refractive index of the dielectric layer 2 is less than that of the P-type contact layer 15, so as to be combined with the protrusion 153 to improve the reflectivity of light. Specifically, the dielectric layer 2 is one or more of a SiO2 layer, a MgF2 layer, a TiO2 layer, and a Ti2O5 layer, but is not limited thereto. The above dielectric layer 2 can not only improve the reflectivity of light, but also effectively passivate the damage formed by etching to avoid leakage. More preferably, the dielectric layer 2 is a SiO2 layer.
[0077] Among them, see Figure 3The thickness of the dielectric layer 2 is smaller than the depth of the groove 154 . Specifically, the thickness of the dielectric layer 2 is 0.2 μm to 4 μm, preferably 0.3 μm to 1 μm.
[0078] S4: etching the dielectric layer to form a plurality of first through holes exposing the protrusions on the top of the protrusions;
[0079] The first through hole 21 can be formed on the top of the protrusion 153 by dry etching or wet etching, but is not limited thereto. Preferably, the dielectric layer 2 is etched by dry etching to form the first through hole 21, and the etching precision is high.
[0080] S5: forming a metal reflective layer on the epitaxial wafer obtained in step S4;
[0081] Among them, see Figure 4 The metal reflective layer 3 is one or more of an Au layer, an Ag layer, and an Al layer, but is not limited thereto. The Au layer is preferred, which has better adhesion, a reflectivity close to that of Ag, and can form a good ohmic contact with the protrusion 153. Meanwhile, the reflectivity of the Au layer decreases minimally after high-temperature annealing.
[0082] Specifically, the thickness of the metal reflective layer 3 is 0.5 μm to 10 μm. The metal reflective layer 3 in the present invention fills the groove 154 of the P-type contact layer 15. Preferably, the thickness of the metal reflective layer 3 is 0.8 μm to 2 μm
[0083] Preferably, in one embodiment, step S5 includes:
[0084] S51: forming a metal reflective layer on the epitaxial wafer obtained in step S4;
[0085] S52: Annealing the epitaxial wafer obtained in step S51.
[0086] Among them, the annealing temperature is 360℃~500℃. Through annealing, the ohmic contact between the metal reflective layer 2 and the P-type contact layer 15 can be greatly optimized. The current injected through the P electrode can be evenly distributed to the entire ohmic P-type contact layer 15 through the metal reflective layer 2, which greatly optimizes the current expansion uniformity, thereby reducing the thickness of the P-type contact layer 15, reducing light absorption, and improving luminous efficiency. It should be noted that in conventional horizontally structured LED chips, the increase in the size of the LED chip makes the current expansion more uneven. The commonly used solutions are to prepare P-electrode extension strips and to increase the thickness of the P-type contact layer, which can usually reach 8μm~12μm. The present invention distributes the current through the metal reflective layer, so there is no need to prepare P-electrode extension strips, and the thickness of the P-type contact layer can also be reduced.
[0087] S6: forming a bonding layer on the metal reflective layer;
[0088] According to different later bonding processes, a bonding layer 4 of different materials can be formed on the metal reflective layer 3. For example, when a eutectic bonding process is adopted, an Au layer, a Cu layer, an In layer, a Pb layer or a Sn layer can be adopted, but it is not limited thereto. For another example, when a hot pressing bonding process is adopted, an Au layer, a Cu layer, an Ag layer or an Al layer can be used as the bonding layer 4, but it is not limited thereto.
[0089] Preferably, in one embodiment, a hot compression bonding process is adopted for bonding, that is, the bonding layer 4 is selected from an Au layer or an Ag layer. The bonding layer 4 can assist the metal reflective layer 3 to improve the reflectivity of light; secondly, low-temperature hot compression bonding can be adopted. During hot compression bonding, the metal reflective layer 3 and the bonding layer 4 have ductility under the combined action of temperature and pressure, so that the metal is squeezed to fill the gaps on the surface of the epitaxial wafer, that is, the resulting chip has no cavity and can withstand higher pressure without breaking during the later process of solid crystal and wire bonding, thereby greatly improving the yield rate. At the same time, it also further optimizes the ohmic contact between the metal reflective layer 3 and the P-type contact layer 15, further improving the uniformity of current distribution.
[0090] The thickness of the bonding layer 4 is 300 nm to 800 nm, preferably 300 nm to 500 nm.
[0091] S7: bonding the epitaxial wafer obtained in step S6 to the second substrate;
[0092] Specifically, the epitaxial wafer and the second substrate 5 may be bonded by eutectic bonding, thermal compression bonding or other bonding methods, but are not limited thereto. Preferably, thermal compression bonding is used. The bonding temperature is 200°C to 360°C, and the bonding pressure is 8000kgf to 15000kgf. The epitaxial wafer structure obtained after bonding is as follows: Figure 5 shown.
[0093] Specifically, when the thermal compression bonding process is adopted, a sub-bonding layer 51 is disposed on the surface of the second substrate 5 , which is an Ag layer or an Au layer, to complete the bonding.
[0094] The second substrate 5 is a common substrate in the art, such as a silicon substrate, a sapphire substrate or a silicon carbide substrate, but is not limited thereto. Preferably, in one embodiment, the second substrate 5 is a sapphire substrate.
[0095] S8: removing the first substrate to expose the N-type semiconductor layer;
[0096] Specifically, the first substrate may be removed by an alkali polishing process or a laser lift-off process, but is not limited thereto. Preferably, the first substrate is removed by a laser lift-off process.
[0097] In the process of removing the first substrate, the buffer layer, intrinsic GaN layer, etc. disposed on the surface are also removed. In one embodiment of the present invention, when the LED is a red LED chip, the first substrate (GaAs substrate), N-type GaAs buffer layer 16 and N-type GaInP etching stop layer 17 are removed.
[0098] S9: forming an N electrode on the N-type semiconductor layer to obtain an intermediate;
[0099] The N electrode 7 may be formed by evaporation, sputtering or other processes, and the N electrode 7 may be one or more of Cr layer, Al layer, Pt layer, Au layer, AuBe composite layer, AuZn composite layer, etc. commonly used in the art, but is not limited thereto.
[0100] Preferably, when the LED is a red LED chip, the N-type GaAs ohmic contact layer is first patterned by a photolithography and etching process, and then the N electrode 7 is formed, and then the N-type AlGaInP roughening layer is roughened 122 .
[0101] S10: forming a plurality of second through holes etched to the P-type contact layer on the intermediate body;
[0102] The intermediate body can be etched by dry etching or wet etching to form a plurality of second through holes 71 . The second through holes 71 are arranged in the second preset area 152 and etched to the P-type contact layer 15 . The second through holes 71 are used to subsequently form the P-electrode 8 .
[0103] Preferably, in one embodiment, step S10 includes:
[0104] S101: forming a plurality of second through holes etched to the P-type contact layer on the intermediate body;
[0105] S102: forming a plurality of third through holes etched to the metal reflective layer in the second through hole;
[0106] Specifically, the P-type contact layer 15 in the second through hole 71 is further etched to form a third through hole 155 etched to the metal reflective layer. The P electrode can be electrically connected to the metal reflective layer 3 through the third through hole 155, and the current injected by the P electrode 8 can be distributed to various parts of the P-type contact layer 15 through the metal reflective layer 3, thereby greatly improving the current expansion uniformity.
[0107] S11: forming a P electrode on the intermediate obtained in step S10 to obtain an LED wafer;
[0108] Among them, the P electrode 8 can be formed by evaporation, sputtering and other processes. The P electrode 8 uses one or more of the Cr layer, Al layer, Pt layer, Au layer, AuBe composite layer, AuZn composite layer and the like commonly used in the art, but is not limited thereto.
[0109] Preferably, in one embodiment, in step S11, a P electrode is first formed on the intermediate obtained in step S10, and then a passivation protection layer is formed, and then etching is performed to expose the N electrode and the P electrode, so as to obtain an LED wafer.
[0110] S12: Cut the LED wafer to obtain horizontal structure LED chips
[0111] Specifically, the second substrate is first ground and thinned, and then laser cut and split to obtain a horizontal structure LED chip. The structure of the horizontal structure LED chip is as follows: Figure 8 shown.
[0112] The above is a preferred embodiment of the invention. It should be pointed out that a person skilled in the art can make several improvements and modifications without departing from the principle of the invention. These improvements and modifications are also considered to be within the scope of protection of the invention.
Claims
1. A method for preparing a horizontal structure LED chip, characterized in that: The following steps are involved: S1. Providing an epitaxial wafer, wherein the epitaxial wafer comprises a first substrate and an N-type semiconductor layer, an active layer, and a P-type semiconductor layer sequentially arranged on the first substrate; the P-type semiconductor layer comprises a first preset region and a second preset region; S2, etching the P-type contact layer to form a plurality of protrusions in a first preset area, and providing grooves between adjacent protrusions; the height of the protrusions is less than or equal to 50% of the thickness of the P-type contact layer; S3, forming a dielectric layer on the epitaxial wafer obtained in step S2, wherein the thickness of the dielectric layer is less than the depth of the groove, and the refractive index of the dielectric layer is less than the refractive index of the P-type contact layer; S4, etching the dielectric layer to form a plurality of first through holes exposing the protrusions on the tops of the protrusions; S5, forming a metal reflective layer on the epitaxial wafer obtained in step S4, wherein the metal reflective layer fills the groove; S6, forming a bonding layer on the metal reflective layer; S7, bonding the epitaxial wafer obtained in step S6 to the second substrate; S8, removing the first substrate to expose the N-type semiconductor layer; S9, forming an N electrode on the N-type semiconductor layer to obtain an intermediate; S10, forming a plurality of second through holes etched to the P-type contact layer on the intermediate body; the second through holes are arranged in the second preset area; S11, forming a P electrode on the intermediate obtained in step S10 to obtain an LED wafer; the P electrode is electrically connected to the P electrode through the second through hole; S12, cutting the LED wafer to obtain horizontal structure LED chips.
2. The method for preparing a horizontal structure LED chip according to claim 1, characterized in that: Step S10 includes: S101: forming a plurality of second through holes etched to the P-type contact layer on the intermediate body, wherein the second through holes are arranged in the second preset area; S102: forming a plurality of third through holes etched to the metal reflective layer in the second through hole; the P electrode is electrically connected to the metal reflective layer through the third through holes.
3. The method for preparing a horizontal structure LED chip according to claim 1, characterized in that: The bonding layer is an Au layer or an Ag layer, and its thickness is 300nm to 800nm; In step S8, a Ag layer or an Au layer is provided on the surface of the second substrate; the epitaxial wafer obtained in step S7 is bonded to the second substrate by thermal compression bonding, and during bonding, the metal reflective layer and the bonding layer are pressed against each other to fill the gap on the surface of the epitaxial wafer; The bonding temperature is 200° C. to 360° C., and the bonding pressure is 8000 kgf to 15000 kgf.
4. The method for preparing a horizontal structure LED chip according to any one of claims 1 to 3, characterized in that: Step S5 includes: S51: forming a metal reflective layer on the epitaxial wafer obtained in step S4; S52: Annealing the epitaxial wafer obtained in step S51 so that the metal reflective layer forms an ohmic contact with the P-type contact layer.
5. The method for preparing a horizontal structure LED chip according to any one of claims 1 to 3, characterized in that: The thickness of the P-type contact layer is 1 μm to 10 μm, and its doping concentration is ≥ 1×10 18 cm -3 ; and / or The protrusions are in the shape of a truncated cone, an ellipsoidal crown or a prism, the height of the protrusions is 0.5 μm to 5 μm, and the distance between adjacent protrusions is 0.5 μm to 10 μm; and / or The height of the protrusion is 20% to 35% of the thickness of the P-type contact layer; and / or The dielectric layer is one or more of a SiO2 layer, a MgF2 layer, a TiO2 layer, and a Ti2O5 layer; the thickness of the dielectric layer is 0.2 μm to 4 μm; and / or The metal reflective layer is one or more of an Au layer, an Ag layer, and an Al layer, and the thickness of the metal reflective layer is 0.5 μm to 10 μm.
6. The method for preparing a horizontal structure LED chip according to any one of claims 1 to 3, characterized in that: The thickness of the P-type contact layer is 2 μm to 4 μm, and the doping concentration is 2×10 18 cm -3 ~5×10 20 cm -3 ; and / or The protrusions are truncated cone-shaped, the height of the protrusions is 0.5 μm to 1.8 μm, and the distance between adjacent protrusions is 0.5 μm to 3 μm; and / or The dielectric layer is a SiO2 layer with a thickness of 0.3 μm to 1 μm; and / or The metal reflective layer is an Au layer, and the thickness thereof is 0.8 μm to 2 μm.
7. The method for preparing a horizontal structure LED chip according to claim 2, characterized in that: The doping concentration of the P-type contact layer increases gradually from the side close to the active layer to the side close to the dielectric layer.
8. The method for preparing a horizontal structure LED chip according to claim 1, characterized in that: The epitaxial wafer comprises a first substrate, an N-type GaAs buffer layer, an N-type GaInP etching stop layer, an N-type semiconductor layer, an active layer, a P-type semiconductor layer and a P-type contact layer which are sequentially arranged on the first substrate; The first substrate is a GaAs substrate; The second substrate is a sapphire substrate; The N-type semiconductor layer includes an N-type GaAs ohmic contact layer, an N-type AlGaInP roughening layer and an N-type AlGaInP current spreading layer, which are arranged on the N-type GaInP etching stop layer in sequence; The P-type semiconductor layer is a P-type AlGaInP confinement layer; The P-type contact layer is a P-type GaP window layer.
9. The method for preparing a horizontal structure LED chip according to claim 8, characterized in that: In step S9, the first substrate and the N-type GaInP etching stop layer are removed to expose the N-type GaAs ohmic contact layer, and the N-type GaAs ohmic contact layer is etched to form a contact pattern; In step S9, an N electrode is formed on the contact pattern, and the N-type AlGaInP roughening layer is roughened; In step S11, a P electrode is first formed on the intermediate body obtained in step S10, and then a passivation protection layer is formed, and then etching is performed to expose the N electrode and the P electrode, so as to obtain an LED wafer.
10. A horizontal structure LED chip, characterized in that: The LED chip is prepared by the method for preparing a horizontal structure LED chip as described in any one of claims 1 to 9.
Citation Information
Patent Citations
Horizontal-electrode inverted red-light LED chip and preparation method thereof
CN106129224A
AlGaInP light-emitting diode thin-film chip structure and preparation method thereof
CN106684220A
Diode chip and preparation method thereof
CN109873066A
Semiconductor light emitting element
JP2009252860A
Semiconductor light emitting element, LED lamp, and method of manufacturing the semiconductor light emitting element
JP2011142231A