Hydrogen sulfide treatment catalyst with high catalytic efficiency

By using catalysts composed of rare earth oxides, transition metal oxides, cocatalysts and support in a high concentration of CO2 environment, the problems of low efficiency and high by-products of traditional catalysts are solved, and efficient H2S treatment and environmental protection requirements are met.

CN119034754AInactive Publication Date: 2024-11-29PINJIANG JIANGHUA ENVIRONMENTAL PROTECTION EQUIP FILLING MATERIAL
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411147581.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-21
Publication Date
2024-11-29
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

The traditional H2S treatment catalyst is less efficient in a high concentration CO2 environment and has more by-products, making it difficult to meet environmental protection requirements.

Method used

The catalyst consisting of rare earth oxides, transition metal oxides, cocatalysts and support is prepared through mixing, stirring, drying and calcining steps to ensure uniform distribution of active components and cocatalysts, form a stable catalyst structure, and improve catalytic efficiency. and stability.

Benefits of technology

In a high concentration of CO2 environment, the conversion efficiency of H2S reaches more than 90%, the by-product generation amount is extremely low, meets environmental protection requirements, and has good stability and reusability.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119034754A_ABST
    Figure CN119034754A_ABST
Patent Text Reader

Abstract

The present invention discloses a hydrogen sulfide treatment catalyst with high catalytic efficiency, and relates to the technical field of hydrogen sulfide treatment catalysts, and the hydrogen sulfide treatment catalyst comprises the following raw materials by mass: 10-30% of an active component, 1-10% of a promoter, and 60-80% of a carrier. The catalyst promoter is used for adjusting the acid-base property of the catalyst for hydrogen sulfide treatment and improving the adsorption and conversion capacity of hydrogen sulfide, and the carrier with high specific surface area and good pore structure is used for effectively dispersing active components and improving the active surface area of the catalyst for hydrogen sulfide treatment. The catalyst for hydrogen sulfide treatment with high catalytic efficiency can be successfully prepared by reasonably combining the rare earth oxide, the transition metal oxide, the cocatalyst and the carrier, and the catalyst not only has high catalytic efficiency in the environment of high-concentration carbon dioxide, but also has good stability and few byproducts, can be repeatedly used, and is suitable for industrial production. The environment-friendly requirement can be met.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of catalysts for treating hydrogen sulfide, in particular to a catalyst for treating hydrogen sulfide with high catalytic efficiency. Background Art

[0002] Coal chemical industry is a long-term strategy for energy development. With the increasingly tight supply of oil and natural gas, the development of coal chemical industry is of great significance to sustainable development, future energy construction and energy technology. However, pollution discharge from coal chemical enterprises is inevitable. In the field of coal chemical industry, its waste gas emissions are often huge, and its hourly waste gas emissions can reach hundreds of thousands of cubic meters. Although the H2S concentration in the waste gas is low, the total emission volume is very large. Direct emission into the atmosphere not only aggravates the greenhouse effect, but also poses a serious threat to the environment and human health.

[0003] In the chemical industry, the H2S emission standard is 5mg / m 3 , and there is a trend of further tightening. At present, the traditional catalysts for H2S treatment are inefficient in high-concentration CO2 environments, produce more by-products, and are difficult to meet environmental protection requirements. Therefore, the development of a catalyst that can efficiently convert H2S in a high-concentration CO2 environment has important practical application value and environmental significance. Summary of the invention

[0004] The purpose of the present invention is to provide a catalyst for treating hydrogen sulfide with high catalytic efficiency, so as to solve the technical problems proposed in the above background technology that the traditional H2S treatment catalyst has low efficiency in a high concentration CO2 environment, produces more by-products, and is difficult to meet environmental protection requirements.

[0005] To achieve the above object, the present invention provides the following technical solution: a catalyst for treating hydrogen sulfide with high catalytic efficiency, comprising the following raw materials in mass percentage: 10%-30% active component, 1%-10% promoter, and 60%-80% carrier.

[0006] Preferably, the active component consists of rare earth oxide and transition metal oxide, and the mass percentage is: 5%-15% rare earth oxide and 5%-15% transition metal oxide.

[0007] Preferably, the rare earth oxide is selected from lanthanum dioxycarbonate La2O3, cerium oxide CeO2, praseodymium oxide Pr6O 11 At least one of .

[0008] Preferably, the transition metal oxide is selected from at least one of copper oxide CuO, cobalt oxide CoO and nickel oxide NiO.

[0009] Preferably, the promoter is a metal oxide, and the metal oxide is selected from at least one of potassium oxide K2O, sodium oxide Na2O, calcium oxide CaO, and magnesium oxide MgO.

[0010] Preferably, the carrier is selected from at least one of activated carbon C, aluminum oxide Al2O3, silicon oxide SiO2, and titanium oxide TiO2.

[0011] Preferably, the rare earth oxide and transition metal oxide of the active components are mixed in a desired ratio to obtain a mixture A, the carrier is placed in a suitable amount of solvent, and stirred to form a suspension, and the solvent is selected from water or an organic solvent.

[0012] Preferably, mixture A is gradually added to the suspension, and metal oxides of the promoter are added simultaneously, and stirred continuously to obtain mixture B, so as to ensure that the active components and the promoter are evenly distributed on the surface of the carrier.

[0013] Preferably, the mixture B is filtered to remove excess solvent, and the filtered solid is placed in a drying oven and dried at a temperature of 80-120° C. to completely remove residual solvent.

[0014] Preferably, the dried solid is placed in a calcination furnace and calcined at a temperature of 400-600°C to allow the active components and the co-catalyst to interact with the carrier to form a stable catalyst structure. The calcined catalyst is sieved to remove particles that are too large or too small to obtain a catalyst with uniform particle size.

[0015] Compared with the prior art, the present invention has the following beneficial effects:

[0016] The present invention uses a co-catalyst, and the co-catalyst is selected from at least one of potassium oxide K2O, sodium oxide Na2O, calcium oxide CaO, and magnesium oxide MgO, so that the acidity and alkalinity of the catalyst for hydrogen sulfide treatment can be adjusted, and the adsorption and conversion capabilities of hydrogen sulfide can be improved. By using a carrier with a high specific surface area and a good pore structure, and the carrier is selected from at least one of activated carbon C, aluminum oxide Al2O3, silicon oxide SiO2, and titanium oxide TiO2, the active components can be effectively dispersed, and the active surface area of ​​the catalyst for hydrogen sulfide treatment can be improved. By reasonably combining rare earth oxides, transition metal oxides, co-catalysts and carriers, a catalyst for hydrogen sulfide treatment with high catalytic efficiency can be successfully prepared. The catalyst not only has high catalytic efficiency in an environment with high concentration of carbon dioxide, but also has good stability, less by-products, can be reused, and can meet environmental protection requirements. BRIEF DESCRIPTION OF THE DRAWINGS

[0017] Figure 1 Schematic diagram of raw materials of the catalyst for treating hydrogen sulfide of the present invention. DETAILED DESCRIPTION

[0018] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0019] Embodiment 1

[0020] See also Figure 1 The present invention provides a technical solution: a catalyst for treating hydrogen sulfide with high catalytic efficiency, comprising the following raw materials in percentage by mass: 10%-30% active component, 1%-10% promoter, and 60%-80% carrier.

[0021] The active components are composed of rare earth oxides and transition metal oxides, and the mass percentages are: 5%-15% of rare earth oxides and 5%-15% of transition metal oxides.

[0022] The rare earth oxide is selected from lanthanum dioxycarbonate La2O3, cerium oxide CeO2, praseodymium oxide Pr6O 11 At least one of .

[0023] The transition metal oxide is selected from at least one of copper oxide CuO, cobalt oxide CoO and nickel oxide NiO.

[0024] The co-catalyst is a metal oxide, and the metal oxide is selected from at least one of potassium oxide K2O, sodium oxide Na2O, calcium oxide CaO, and magnesium oxide MgO, so that it can be used to adjust the acidity and alkalinity of the catalyst for hydrogen sulfide treatment and improve the adsorption and conversion capacity of hydrogen sulfide.

[0025] The carrier is selected from at least one of activated carbon C, aluminum oxide Al2O3, silicon oxide SiO2, and titanium oxide TiO2. By using a carrier with a high specific surface area and a good pore structure, the active components can be effectively dispersed and the active surface area of ​​the catalyst for hydrogen sulfide treatment can be increased.

[0026] The active component rare earth oxide La2O3 and transition metal oxide CuO are mixed in a desired proportion to obtain a mixture A, the carrier SiO2 is placed in an appropriate amount of solvent and stirred to form a suspension, and the solvent is selected from water or an organic solvent, the mixture A is gradually added to the suspension, and the metal oxide K2O of the co-catalyst is added and continuously stirred to obtain a mixture B, which is used to ensure that the active component and the co-catalyst are evenly distributed on the surface of the carrier, the mixture B is filtered to remove excess solvent, and the filtered solid is placed in a drying oven and dried at a temperature of 80-120°C to completely remove residual solvent, the dried solid is placed in a calcining furnace and calcined at a temperature of 400-600°C to allow the active component and the co-catalyst to interact with the carrier to form a stable catalyst structure, and during the calcination process, the heating rate and calcination time need to be controlled to ensure that the performance of the catalyst is optimal, and the calcined catalyst is sieved to remove the part with too large or too small particles to obtain a catalyst A with uniform particle size.

[0027] The catalyst A has a H2S conversion efficiency of more than 90% in a high-concentration CO2 environment, and the amount of by-products generated is extremely low, which can meet environmental protection requirements and has good stability and reusability.

[0028] Embodiment 2

[0029] See also Figure 1 The present invention provides a technical solution: a catalyst for treating hydrogen sulfide with high catalytic efficiency, comprising the following raw materials in percentage by mass: 10%-30% active component, 1%-10% promoter, and 60%-80% carrier.

[0030] The active components are composed of rare earth oxides and transition metal oxides, and the mass percentages are: 5%-15% of rare earth oxides and 5%-15% of transition metal oxides.

[0031] The rare earth oxide is selected from lanthanum dioxycarbonate La2O3, cerium oxide CeO2, praseodymium oxide Pr6O 11 At least one of .

[0032] The transition metal oxide is selected from at least one of copper oxide CuO, cobalt oxide CoO and nickel oxide NiO.

[0033] The co-catalyst is a metal oxide, and the metal oxide is selected from at least one of potassium oxide K2O, sodium oxide Na2O, calcium oxide CaO, and magnesium oxide MgO, so that it can be used to adjust the acidity and alkalinity of the catalyst for hydrogen sulfide treatment and improve the adsorption and conversion capacity of hydrogen sulfide.

[0034] The carrier is selected from at least one of activated carbon C, aluminum oxide Al2O3, silicon oxide SiO2, and titanium oxide TiO2. By using a carrier with a high specific surface area and a good pore structure, the active components can be effectively dispersed and the active surface area of ​​the catalyst for hydrogen sulfide treatment can be increased.

[0035] The active component rare earth oxide Pr6O 11 and transition metal oxides CoO and NiO in a desired proportion to obtain a mixture A, the carrier SiO2 is placed in an appropriate amount of solvent and stirred to form a suspension, and the solvent is selected from water or an organic solvent, the mixture A is gradually added to the suspension, and the metal oxides Na2O and CaO of the co-catalyst are added at the same time, and the stirring is continued to obtain a mixture B, which is used to ensure that the active components and the co-catalyst are evenly distributed on the surface of the carrier, the mixture B is filtered to remove excess solvent, and the filtered solid is placed in a drying oven and dried at a temperature of 80-120°C to completely remove the residual solvent, the dried solid is placed in a calcining furnace and calcined at a temperature of 400-600°C to allow the active components and the co-catalyst to interact with the carrier to form a stable catalyst structure, and during the calcination process, the heating rate and the calcination time need to be controlled to ensure that the performance of the catalyst is optimal, the calcined catalyst is sieved to remove the part of the particles that are too large or too small to obtain a catalyst B with uniform particle size.

[0036] The catalyst B has a H2S conversion efficiency of more than 90% in a high-concentration CO2 environment, and the amount of by-products generated is extremely low, which can meet environmental protection requirements and has good stability and reusability.

[0037] In summary, when preparing a catalyst for treating hydrogen sulfide with high catalytic efficiency, the rare earth oxide and transition metal oxide of the active components are mixed in a desired proportion to obtain a mixture A, the carrier is placed in an appropriate amount of solvent, and stirred to form a suspension, and the solvent is selected from water or an organic solvent, the mixture A is gradually added to the suspension, and the metal oxide of the promoter is added at the same time, and the stirring is continued to obtain a mixture B, the mixture B is filtered, and the filtered solid is placed in a drying oven and dried at a temperature of 80-120° C. The dried solid is placed in a calcining furnace and calcined at a temperature of 400-600° C. The calcined catalyst is sieved to remove the part with excessively large or small particles to obtain a catalyst for treating hydrogen sulfide with uniform particle size and high catalytic efficiency. The contents not described in detail in this specification belong to the prior art known to professional and technical personnel in this field.

[0038] Although the present invention has been described in detail with reference to the aforementioned embodiments, it is still possible for those skilled in the art to modify the technical solutions described in the aforementioned embodiments, or to make equivalent substitutions for some of the technical features therein. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention should be included in the protection scope of the present invention.

Claims

1. A catalyst for treating hydrogen sulfide with high catalytic efficiency, It is characterized in that The raw materials include the following mass percentages: 10%-30% active component, 1%-10% co-catalyst, and 60%-80% carrier.

2. A catalyst for treating hydrogen sulfide with high catalytic efficiency according to claim 1, Features: The active components are composed of rare earth oxides and transition metal oxides, and the mass percentages are: 5%-15% of rare earth oxides and 5%-15% of transition metal oxides.

3. A catalyst for treating hydrogen sulfide with high catalytic efficiency according to claim 2, Features: The rare earth oxide is selected from lanthanum dioxycarbonate La 2 O 3 、Cerium Oxide CeO 2 、Pr 6 O 11 At least one of .

4. A catalyst for treating hydrogen sulfide with high catalytic efficiency according to claim 2, Features: The transition metal oxide is selected from at least one of copper oxide CuO, cobalt oxide CoO and nickel oxide NiO.

5. A catalyst for treating hydrogen sulfide with high catalytic efficiency according to claim 1, Features: The co-catalyst is a metal oxide, and the metal oxide is selected from potassium oxide K 2 O, sodium oxide Na 2 O, at least one of calcium oxide (CaO) and magnesium oxide (MgO).

6. A catalyst for treating hydrogen sulfide having high catalytic efficiency according to claim 1, Features: The carrier is selected from activated carbon C, alumina Al 2 O 3 、Silicon oxide SiO 2 , titanium oxide TiO 2 At least one of .

7. A method for preparing a catalyst for treating hydrogen sulfide with high catalytic efficiency according to claims 1-6, Features: The rare earth oxide and transition metal oxide of the active components are mixed in a desired ratio to obtain a mixture A, and the carrier is placed in a suitable amount of solvent and stirred to form a suspension, and the solvent is selected from water or an organic solvent.

8. A method for preparing a catalyst for treating hydrogen sulfide with high catalytic efficiency according to claim 7, Features: The mixture A is gradually added to the suspension, and the metal oxide of the promoter is added at the same time, and stirred continuously to obtain the mixture B, which is used to ensure that the active components and the promoter are evenly distributed on the surface of the carrier.

9. A method for preparing a catalyst for treating hydrogen sulfide with high catalytic efficiency according to claim 8, Features: The mixture B is filtered to remove excess solvent, and the filtered solid is placed in a drying oven and dried at a temperature of 80-120° C. to completely remove residual solvent.

10. A method for preparing a catalyst for treating hydrogen sulfide with high catalytic efficiency according to claim 9, Features: The dried solid is placed in a calcining furnace and calcined at a temperature of 400-600°C to allow the active components and the co-catalyst to interact with the carrier to form a stable catalyst structure. The calcined catalyst is sieved to remove particles that are too large or too small to obtain a catalyst with uniform particle size.