Method for producing crystal oscillators on whole board
Through the method of producing crystal oscillators in the whole plate, the processing technology of SMD quartz crystal resonators is simplified by using ceramic materials and glue sizing systems, solving the problems of complex structures and environmental pollution in the existing technology, and achieving a low-cost and high-efficiency production process. Improve product stability and yield.
Patent Information
- Application Number
- CN202411050458.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-01
- Publication Date
- 2024-11-29
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
The processing technology of existing SMD quartz crystal resonators has problems such as complex structure, high processing difficulty, and environmental pollution. In particular, additional anti-corrosion coating is required during welding and cutting of metal cover plates, which increases production costs and processes.
The method of producing crystal oscillators in the whole plate is adopted, and the cover plate is made using ceramic materials, and connected to the base through the glue sizing system, pre-curing heating and vacuum treatment are performed, and the division is combined with a lobster to avoid laser welding and cutting, and simplify the process flow.
It reduces processing costs and environmental pollution, improves product stability and yield, simplifies process flow, reduces electroplating and anti-corrosion treatment, and improves production efficiency and product quality.
Smart Images

Figure CN119035042A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of production and processing of electronic components, and specifically to a method for producing crystal oscillators using a whole board. Background Art
[0002] SMD quartz crystal resonators are commonly used electronic devices, and their usage is increasing with the development of digital technology. However, there are technical barriers to improving processing efficiency and quality in terms of device structure and processing technology. In addition, there are also environmental pollution problems in the processing technology.
[0003] The overall structure of a quartz crystal oscillator is that a quartz crystal wafer with one end suspended in the air is provided in a chamber, and a conductive structure is provided. In order to ensure the working stability of the crystal oscillator, the chamber of the current quartz crystal oscillator is vacuumed. The existing whole plate cover of the quartz crystal oscillator mostly adopts a metal cover welding method. A metal kovar ring is provided on the whole plate base and at the connection with the whole plate cover. After the crystal oscillator chamber is vacuumed, the whole plate cover and the kovar ring are laser welded in a vacuum environment to achieve the sealing of the cavity. This whole plate metal cover welding still has many disadvantages. For example, a metal kovar ring must be provided on the upper surface of the base, and the kovar ring needs to be provided with a conductive hole to achieve electrical connection with other conductive areas for unified electroplating operations, which increases the processing difficulty of the whole plate base. In addition, during the whole plate processing process, the metal cover is cut with the help of laser after laser sealing. Whether it is the sealing position or the cutting position, an additional anti-corrosion coating needs to be applied to avoid oxidation and rust at the welding and cutting positions, which increases the production process and production cost. Summary of the invention
[0004] The technical problem to be solved by the present invention is to provide a method for producing a crystal oscillator in a whole plate.
[0005] The specific technical solution of the present invention to solve the above technical problems is:
[0006] The whole-board production crystal oscillator method based on the whole-board cover plate for whole-board production of crystal oscillators described above comprises the following steps:
[0007] SS1. Provide a whole-plate resonator semi-finished product, wherein the whole-plate resonator semi-finished product includes a whole-plate base, wafers fixed on each base, and the whole-plate cover plate described above;
[0008] SS2, applying glue to the connection position between the whole cover plate and the base by using a glue application system;
[0009] SS3, covering the whole plate cover plate on the whole plate base, and performing pre-curing heating, wherein the pre-curing heating is used to make the colloid on the whole plate cover plate reach a semi-cured state;
[0010] SS4, evacuate the semi-finished resonator in the vacuum chamber;
[0011] SS5. Continue to heat the semi-finished resonator product in a vacuum environment until the colloid is completely solidified, so that the connection between each single sub-cover plate and the base is airtight, and ensure that the cavity of the resonator containing the wafer is kept in a vacuum state;
[0012] SS6. Obtain a whole-plate resonator, split the whole-plate resonator into pieces, and obtain a single SMD quartz crystal resonator.
[0013] Compared with the prior art, this solution has the following technical effects:
[0014] There is no need to set a kovable ring and related electrical connection structure on the whole board base, so the structure is simple, the processing steps are few, the processing technology requirements are low, and the processing cost is low; the cancellation of the kovable ring also reduces the material used in the electroplating process, which reduces the cost and is also beneficial to environmental protection; the assembly process of the crystal oscillator does not need to consider the corrosion protection problem of the cover plate welding and cutting parts, and does not need a laser cutting process. The cover plate can be split using a ready-made splitting machine, so there are fewer processing steps, fewer processing equipment, and low processing costs; the energy consumption of the link based on the spray valve gluing is lower than that of the laser welding link, so the energy consumption is lower; the insulating cover plate will not cause a short circuit between the two electrodes of the chip, so the finished product crystal oscillator has a higher yield rate, and even based on this structure, in the case of traditional metal cover plates, the glue point of the fixed electrode is high enough to contact the cover plate, which will inevitably lead to waste, while in this process, the glue point of the fixed electrode is high enough to contact the cover plate, which can improve the stability of the product, because the fixing effect of the chip is no longer solely dependent on the glue point, and the cover plate that contacts the glue point also further exerts a certain pressure on the glue point, thereby improving the fixation of the chip and avoiding poor chip fixation.
[0015] Furthermore, a whole plate cover plate is provided for producing a crystal oscillator, the whole plate cover plate is made of ceramic, the whole plate cover plate is divided into a plurality of sub-cover plates arranged in a matrix, pre-breaking lines are provided between adjacent sub-cover plates, and the pre-breaking lines are non-through-cut pre-breaking lines.
[0016] Compared with the prior art, this solution uses ceramic material to make the cover plate. Since ceramic is insulating, even if the glue point connecting the two electrodes of the chip is too high and touches the cover plate, a short circuit will not occur. On the other hand, since it is made of ceramic material and uses colloid connection instead of laser welding, there is no need to set a kovar ring on the corresponding base, and there is no need to set a structure electrically connected to the kovar ring, which simplifies the structure of the crystal oscillator and reduces the difficulty of processing the quartz crystal oscillator. Finally, since ceramic is hard and brittle, it can be mechanically split using a splitting machine by setting a pre-breaking line, and the ceramic material itself has strong corrosion resistance. After splitting, there is no need to spray an anti-corrosion layer like a metal cover plate, which further simplifies the processing procedures of the crystal oscillator and reduces processing costs.
[0017] Furthermore, the pre-fracture line is a V-shaped groove.
[0018] The technical effect of adopting the above further technical solution is that, on the one hand, the V-shaped groove is easy to process and the processing cost is reduced; on the other hand, the stress of the V-shaped groove is concentrated at the bottom of the groove, which facilitates the splitting operation.
[0019] Furthermore, pre-breaking lines are provided on both the front and back sides of the whole cover plate.
[0020] The technical effect of adopting the above further technical solution is that pre-breaking lines are set at corresponding positions on both sides, and the breaking position is accurate when splitting, the breaking surface is neat, and the surface quality is good.
[0021] Furthermore, at least two measuring holes are provided on the whole plate cover.
[0022] The technical effect of adopting the above-mentioned further technical solution is that, especially when the two measuring holes are located at relatively far positions on the whole plate cover, such as at the two ends of the longer sides, or at the diagonal positions of the quadrilateral, based on measuring the distance between the two measuring holes and then converting it into the size of the adjacent sub-cover plate on the whole plate cover, the measurement error will be evenly dispersed and the measured size will be more accurate.
[0023] Furthermore, the semi-cured state means that the whole plate cover and the whole plate base have achieved a preliminary bonding connection, the relative positions in the horizontal direction are fixed, but the bonding point has not reached an airtight state.
[0024] The beneficial effect of adopting the above further solution is that it realizes the fixing of the initial position of the cover plate, and at the same time reserves holes for vacuuming the base cavity, thereby avoiding one-time complete solidification resulting in the air in the cavity being unable to be extracted, affecting the quality of the product.
[0025] Furthermore, the step SS5 also includes a step of applying pressure to the cover plate in a vertical direction, so as to enhance the strength of the connection between the cover plate and the base and improve the air tightness.
[0026] The beneficial effect of adopting the above further solution is to further enhance the connection strength and improve the product quality.
[0027] Furthermore, the step SS1 also includes a step of confirming whether the size difference between the whole plate cover and the whole plate base is within a set threshold.
[0028] The beneficial effect of adopting the above further solution is to ensure that the colloid applied on the cover plate is adapted to the connection between the base, especially the width of the applied rubber strip is generally only about 0.2mm. If the size deviation is large, it is very likely to cause the glue point to deviate from the base, resulting in defective products. Because ceramic products have different expansion coefficients during the firing process, the prior art cannot achieve absolute size consistency, so from batches of bases and batches of cover plates, find bases and cover plates whose relative size differences are within the allowable threshold, which can ensure that the base and cover plate of the product are adapted, and ensure that the applied rubber strip is just located at the connection of the base and will not deviate due to deviations in processing dimensions.
[0029] Furthermore, in step SS2, the glue application system is a spray valve, and the spray valve sprays glue reciprocatingly in a straight line along the length and width directions of the entire cover plate. For example, the spray valve first sprays glue reciprocatingly in a straight line intermittently along a first direction of the entire cover plate (for example, the length direction is defined as the first direction), and then sprays glue reciprocatingly in a straight line intermittently along a second direction perpendicular to the first direction (i.e., the width direction), and finally realizes a closed rubber ring on a single cover plate. During the whole process, the nozzle has fewer turning times and fewer positioning times, so the gluing efficiency is high.
[0030] The beneficial effect of adopting the above further scheme is that, compared with the circular gluing method of each bead, the linear reciprocating glue spraying has the highest efficiency and is the easiest to control, thereby improving the production efficiency of the product and reducing the production cost.
[0031] Furthermore, the confirmation of whether the size difference between the whole plate cover and the whole plate base is within the set threshold specifically refers to pre-measuring the size of each whole plate base, marking it with a unique base identifier, and binding the size information with the unique base identifier in the system; pre-measuring the size of each whole plate cover, marking it with a unique cover identifier, and binding the size information with the unique cover identifier in the system; the system obtains the unique identifier of the whole plate base, finds the whole plate cover of matching size in the system, and the system informs the storage location, and the robot takes it from the corresponding storage location to form a whole plate resonator semi-finished product together with the whole plate base and the chips fixed on each base.
[0032] The beneficial effect of adopting the above-mentioned further scheme is that the dimensions of the whole board base and the whole board cover are measured in advance and entered into the system. The system can perform preliminary matching work. In actual production, based on the identification of the whole board base obtained by scanning the code or other means, the matching whole board cover can be quickly matched to improve work efficiency. At the same time, the adaptability of the whole board base and the whole board cover is ensured, thereby improving the quality of the final product. BRIEF DESCRIPTION OF THE DRAWINGS
[0033] Figure 1 It is a plan view of the whole cover plate of the present invention;
[0034] Figure 2 for Figure 1 A partial enlarged view of the middle part;
[0035] Figure 3 It is a three-dimensional schematic diagram of the whole cover plate of the present invention;
[0036] Figure 4 This is a cross-sectional view of the crystal oscillator where the glue point contacts the upper cover;
[0037] Figure 5 This is a schematic diagram of the route for spraying glue through the spray valve on the entire cover plate;
[0038] Figure 6 for Figure 5 Enlarged view of point B in the middle.
[0039] In the accompanying drawings, the component names represented by the reference numerals are listed as follows:
[0040] 1. Sub-cover plate; 2. Pre-fracture line; 4. Positioning hole; 5. Through hole; 6. Glue dot; 7. Wafer; 8. Upper electrode dispensing station; 9. Lower electrode dispensing station; 10. Upper electrode; 11. Lower electrode; 12. Glue strip; 12-1. First horizontal colloid; 12-2. Second horizontal colloid; 12-(n+1), first vertical colloid; 12-(n+2), second vertical colloid. DETAILED DESCRIPTION
[0041] The principles and features of the present invention are described below in conjunction with the accompanying drawings. The examples given are only used to explain the present invention and are not used to limit the scope of the present invention.
[0042] like Figure 1 As shown, a whole plate cover for producing a crystal oscillator is made of ceramic. The whole plate cover is divided into a plurality of sub-covers 1 arranged in a matrix. Pre-break lines 2 are provided between adjacent sub-covers 1. Figure 3As shown, the pre-fracture line 2 is a non-through V-shaped groove, and the front and back sides of the whole cover plate are provided with pre-fracture lines 2, and the pre-fracture lines on both sides are on the preset fracture surface. When producing the whole cover plate, the pre-fracture line 2 is first engraved on the raw embryo of the whole cover plate, and then fired, because the hardness of the ceramic is particularly high after firing, and the pre-fracture line cannot be engraved. Each sub-cover plate is provided with a through hole 5 at the four corners. The setting of the through hole 5 can reduce the stress during the splitting, making it easier to split.
[0043] Positioning holes 4 are arranged around the entire cover plate. The positioning holes 4 can be in various forms such as circular and triangular, so as to facilitate clamping and fixing with a workpiece.
[0044] The through holes 5 located at the four top corners of the whole cover are used as measuring holes. The whole cover is photographed with a fixed focus and distance based on the camera system. The size of the whole cover can be accurately calculated based on the number of pixels between the two positioning holes in the obtained photo, and the average size of each sub-cover can be further calculated. When this method is based on measuring the distance between the two measuring holes and then converting it into the size of the adjacent sub-cover on the whole cover, the measurement error will be evenly dispersed, the measured size will be more accurate, and it is beneficial to the control of subsequent processing technology.
[0045] For example, in this example, the length of the entire cover plate (sub-cover plate area) is 43.6 cm, and it is divided into 22 sub-cover plates in the length direction. The two measuring holes are located at both ends of the length direction. The measured value is, and the calculated width of each sub-cover plate is 1.98 mm.
[0046] When SMD quartz crystal oscillators are produced based on the whole plate cover, there is no need to set a kovar ring on the corresponding ceramic base, and there is no need to set a structure electrically connected to the kovar ring, which simplifies the structure of the crystal oscillator base and reduces the difficulty of processing the quartz crystal oscillator base. Of course, it also means that the processing difficulty of the crystal oscillator itself is reduced and the processing cost is reduced.
[0047] Compared with the prior art, this solution uses ceramic material to make the cover plate. Since ceramic is insulating, even if the glue point connecting the two electrodes of the chip is too high and touches the cover plate, a short circuit will not occur. Moreover, even if the glue point connecting the two electrodes of the chip is so high that it touches the cover plate, the cover plate will play an additional auxiliary role in fixing the chip, so that the scrapped products in the traditional process are turned into high-quality products in this process. On the other hand, since it is a ceramic material, colloid connection is used instead of laser welding, which reduces energy consumption. Finally, since ceramic is hard and brittle, it can be mechanically split using a splitting machine by setting a pre-breaking line. In addition, the ceramic material itself has strong corrosion resistance, so there is no need to spray an anti-corrosion layer after splitting like a metal cover plate, which further simplifies the processing procedures of the crystal oscillator and reduces processing costs.
[0048] The whole-board production crystal oscillator method based on the whole-board cover plate for whole-board production of crystal oscillators described above comprises the following steps:
[0049] SS1. Provide a whole-plate resonator semi-finished product, wherein the whole-plate resonator semi-finished product includes a whole-plate base, wafers fixed on each base, and the whole-plate cover plate described above;
[0050] SS2, applying glue to the connection position between the whole cover plate and the base by using a glue application system;
[0051] SS3, covering the whole plate cover plate on the whole plate base, and performing pre-curing heating, wherein the pre-curing heating is used to make the colloid on the whole plate cover plate reach a semi-cured state;
[0052] SS4, placing the semi-finished resonator into the vacuum chamber for vacuuming;
[0053] SS5. Continue to heat the semi-finished resonator product in a vacuum environment until the colloid is completely solidified, so that the connection between each sub-cover plate and the base is airtight, and ensure that the cavity of the resonator containing the wafer is kept in a vacuum state;
[0054] SS6. Obtain a whole-plate resonator, split the whole-plate resonator into pieces, and obtain a single SMD quartz crystal resonator.
[0055] Based on the process of this scheme, there is no need to set a cuttable ring and related electrical connection structure on the base of the whole board, so the structure is simple, the processing steps are few, the processing technology requirements are low, and the processing cost is low; the cancellation of the cuttable ring also reduces the materials used in the electroplating process, which reduces costs and is also beneficial to environmental protection; the assembly process of the crystal oscillator does not need to consider the anti-corrosion problems at the welding and cutting points of the cover plate, and does not require a laser cutting process. The cover plate can be split using a ready-made splitting machine, so there are few processing steps, fewer processing equipment, and low processing costs; the energy consumption of the link based on the spray valve glue application is lower than that of the laser welding link, so the energy consumption is lower; even if it produces Figure 4 In the situation shown, that is, the glue point 6 abuts against the sub-cover 1, the insulating sub-cover 1 will not cause a short circuit between the upper electrode 10 and the lower electrode 11 of the chip, so the finished product crystal oscillator yield is higher. Even based on this structure, in the case of traditional metal cover plates, the glue point of the fixed electrode is so high that it contacts the cover plate, which will inevitably lead to scrap. In this process, the glue point of the fixed electrode is so high that it contacts the cover plate, which can improve the stability of the product, because the fixing effect of the chip is no longer solely dependent on the glue point, and the cover plate that contacts the glue point also further exerts a certain pressure on the glue point, thereby improving the fixation degree of the chip and avoiding poor chip fixation.
[0056] Furthermore, the semi-cured state means that the whole plate cover and the whole plate base have achieved preliminary bonding connection, and the relative position in the horizontal direction is fixed, but the bonding part has not reached the airtight state. That is, the initial position of the cover is fixed, and at the same time, a gap is reserved for vacuuming the base cavity, so as to avoid one-time complete curing that makes it impossible to extract the air in the cavity, affecting the quality of the product.
[0057] Furthermore, the step SS5 also includes a step of applying pressure to the cover plate in a vertical direction, so as to enhance the strength of the connection between the cover plate and the base and improve the air tightness.
[0058] Further strengthen the connection strength and improve product quality.
[0059] Furthermore, the size difference between the whole plate cover and the whole plate base in step SS1 is within a set threshold.
[0060] Ensure that the colloid applied on the cover plate fits the connection between the sub-cover plate and the base. As mentioned in the previous example, the size of a single sub-cover plate is 1.98mm, and the width of the top edge of the base connected to the sub-cover plate is only about 0.2mm. The width of the applied rubber strip is about 0.1-0.2mm. If the size deviation exceeds 0.2mm, the rubber strip will deviate from the base, causing the rubber strip to be applied to a place other than the connection between the sub-cover plate 1 and the base, resulting in defective products. Because ceramic products have different expansion coefficients during the firing process, the existing technology cannot achieve absolute dimensional consistency. Therefore, finding bases and cover plates whose relative size differences are within the allowable threshold from batches of bases and batches of cover plates can ensure that the base and cover plate of the product are compatible, and ensure that the applied rubber strip is just located at the connection of the base and will not deviate due to deviations in processing dimensions.
[0061] Furthermore, in step SS2, the glue application system is a spray valve, and the spray valve reciprocates linearly along the length and width directions of the entire cover plate, spraying glue intermittently. The intermittent glue spraying is to avoid the pre-fracture line position and finally realize a closed rubber ring on a single cover plate.
[0062] like Figure 5 As shown (please note that in order to show the gluing direction more clearly, Figure 5The pre-break lines on the whole plate cover are hidden in the figure). The first step is to start from the upper left corner of the whole plate cover and apply the first horizontal glue 12-1 intermittently along a straight line from left to right. The interruption is to avoid the pre-break line. The second step is to move downward by the width of a sub-cover (based on the glue application position), and then apply glue intermittently along a straight line from right to left to obtain the second horizontal glue 12-2. The above operations are carried out in sequence until all places where glue is required in the left and right directions are applied. Then change to applying glue in the up and down directions. In this example, first apply glue intermittently along a straight line from the upper left corner to the lower left corner to obtain the first vertical glue 12-(n+1). Then, move to the right by the length of a sub-cover (based on the glue application position), and then apply glue intermittently along a straight line from bottom to top to obtain the second vertical glue 12-(n+2). Repeat this process until all places where glue is required in the up and down directions are applied. Figure 6 One circle of rubber ring is shown.
[0063] The linear reciprocating glue spraying is the simplest and most efficient to control, which can improve the production efficiency of the product and reduce the production cost.
[0064] Furthermore, the whole board base and the whole board cover plate pre-measure the size of each whole board base, mark it with a unique base identifier, and bind the size information with the unique base identifier in the system; pre-measure the size of each whole board cover plate, mark it with a unique cover identifier, and bind the size information with the unique cover identifier in the system; obtain the unique identifier of the whole board base, and match the whole board cover plates whose size differences are within the set threshold range in the system to form a whole board resonator semi-finished product.
[0065] The dimensions of the whole board base and the whole board cover are measured in advance and entered into the system. The system can perform preliminary matching work. In actual production, based on the identification of the whole board base obtained by scanning the code or other means, the system can quickly match the appropriate whole board cover to improve work efficiency. At the same time, it ensures the adaptability of the whole board base and the whole board cover and improves the quality of the final product.
[0066] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principle of the present invention should be included in the protection scope of the present invention.
Claims
1. A method for producing crystal oscillators from a whole board. It is characterized in that The following steps are involved: SS1. Provide a whole-plate resonator semi-finished product, wherein the whole-plate resonator semi-finished product includes a whole-plate base, wafers fixed on each base, and a whole-plate cover; SS2, applying glue to the connection position between the whole cover plate and the base by using a glue application system; SS3, covering the whole plate cover plate on the whole plate base, and performing pre-curing heating, wherein the pre-curing heating is used to make the colloid on the whole plate cover plate reach a semi-cured state; SS4, vacuum the semi-finished resonator; SS5. Continue heating in a vacuum environment until the colloid is completely solidified, so that the connection between the cover plate and the base is airtight, and ensure that the cavity of the resonator containing the wafer is in a vacuum state; SS6. Obtain a whole-plate resonator, split the whole-plate resonator into pieces, and obtain a single SMD quartz crystal resonator.
2. The method for producing a crystal oscillator from a whole plate according to claim 1, It is characterized in that The whole cover plate is made of ceramics and is divided into a plurality of sub-cover plates arranged in a matrix. Pre-fracture lines are arranged between adjacent sub-cover plates, and the pre-fracture lines are non-through-cut pre-fracture lines.
3. The method for producing a crystal oscillator from a whole plate according to claim 2, It is characterized in that The pre-fracture line is a V-shaped groove.
4. The method for producing a crystal oscillator from a whole plate according to claim 2 or 3, It is characterized in that Pre-breaking lines are arranged on both the front and back sides of the whole cover plate.
5. The method for producing a crystal oscillator from a whole plate according to claim 4, It is characterized in that At least two measuring holes are arranged on the whole plate cover.
6. The method for producing a crystal oscillator from a whole plate according to claim 1, It is characterized in that The semi-cured state means that the whole plate cover and the whole plate base have achieved a preliminary bonding connection, the relative positions in the horizontal direction are fixed, but the bonding point has not reached an airtight state.
7. The method for producing a crystal oscillator from a whole plate according to claim 1, It is characterized in that The step SS5 also includes a step of applying pressure to the cover plate in a vertical direction, so as to enhance the strength of the connection between the cover plate and the base and improve the air tightness.
8. The method for producing a crystal oscillator from a whole plate according to any one of claims 5 to 7, It is characterized in that The step SS1 also includes a step of confirming whether the size difference between the whole plate cover and the whole plate base is within a set threshold.
9. The method for producing a crystal oscillator from a whole plate according to any one of claims 5 to 7, It is characterized in that In step SS2, the glue application system is a spray valve, which first sprays glue reciprocatingly in a linear manner along a first direction of the entire cover plate, and then sprays glue reciprocatingly in a linear manner along a second direction perpendicular to the first direction.
10. The method for producing a crystal oscillator from a whole plate according to claim 8, It is characterized in that The confirming whether the size difference between the whole plate cover and the whole plate base is within the set threshold specifically refers to measuring the size of each whole plate base in advance, marking it with a unique base identifier, and binding the size information with the unique base identifier in the system; measuring the size of each whole plate cover in advance, marking it with a unique cover identifier, and binding the size information with the unique cover identifier in the system; The unique identifier of the whole-board base is obtained, and the whole-board cover with a matching size difference within the set threshold range is searched in the system, and the corresponding whole-board cover is taken by a robot to form a whole-board resonator semi-finished product.
Citation Information
Patent Citations
Quartz-crystal resonator
CN101662270A
Ultrathin ceramic-packaged quartz crystal resonator
CN101873112A
Resonator with resistor-capacitor loop, base, base group and base preparation method
CN106100604A
Glue spraying technology of flexible circuit board
CN106102335A
Production process of LED flexible lamp strips
CN106195695A
Cited By
Surface crystal wafer and processing method of surface crystal oscillator
CN119995540A