Preparation method of semiconductor structure and semiconductor structure
By introducing graphene film as a stress release structure in semiconductor devices and combining silicon nitride films, the device deformation and performance inconsistency caused by the stress of silicon nitride films is solved, and higher mechanical performance and thermal stability are achieved, which improves the Reliability of semiconductor devices.
Patent Information
- Application Number
- CN202411146702.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-20
- Publication Date
- 2024-11-29
AI Technical Summary
The stress characteristics of silicon nitride thin films in semiconductor devices lead to device deformation, inconsistent performance, and thermal stability problems. The existing relief methods have limitations, making it difficult to meet the high precision and performance requirements of deep submicron processes.
The graphene film is used as the stress release structure, and a graphene film is formed on one side of the substrate by chemical vapor deposition or transfer method. Combined with the silicon dioxide film, a stress release structure is formed, and a silicon nitride film is formed on the side of the substrate. Etching and chemical mechanical grinding remove stress relief structures to achieve stress relief.
Effectively alleviate the internal stress of silicon nitride film, enhance process compatibility, prevent wafer warping and deformation, improve mechanical and thermal stability, optimize electrical performance, and improve the reliability of semiconductor devices.
Smart Images

Figure CN119049958A_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the field of semiconductor technology, and in particular to a method for preparing a semiconductor structure and a semiconductor structure. Background Art
[0002] With the development of semiconductor technology, the characteristic size of semiconductor devices is getting smaller and smaller. Especially after the semiconductor process enters the deep submicron stage, many new methods are applied to the device manufacturing process to achieve high integration and high performance devices. For example, the application of silicon nitride film has become more important and widespread. Silicon nitride (Si3N4, SiN) is a chemical compound. In the crystal structure of silicon nitride, each silicon atom is combined with four nitrogen atoms in the form of a tetrahedron, and each nitrogen atom is also combined with four silicon atoms in the form of a tetrahedron. This structure makes the crystal lattice of silicon nitride extremely stable and not easy to deform.
[0003] Silicon nitride has excellent insulation properties, with a resistivity of up to 10^14Ω·cm, far exceeding some common insulating materials such as silicon oxide (SiO2). Its low dielectric constant makes it an ideal isolation layer in microwave and radio frequency applications. The silicon nitride layer also plays a role in blocking the diffusion of impurities in the chip. It can prevent dopants such as boron and phosphorus from changing device characteristics through diffusion. In addition, it can also prevent the diffusion of metal ions to prevent faults such as short circuits. Silicon nitride has excellent thermal stability, which is determined by its special chemical properties and crystal structure. It can remain stable in high temperature environments without chemical decomposition or physical shape changes like other materials.
[0004] Silicon nitride films are widely used in deep submicron processes due to their high dielectric strength, high temperature resistance, corrosion resistance and stress management capabilities, such as electrical insulation layer, hard mask layer, stress engineering, etch stop layer, diffusion barrier layer, high K / metal gate (HKMG), insulation layer in multi-layer interconnect structure, etc. Although silicon nitride films are widely used in semiconductors, their stress characteristics also bring many limitations and challenges. These limitations mainly come from the following effects of internal stress in the film on the performance and reliability of semiconductor devices:
[0005] (1) Device deformation caused by film stress: Excessive compressive and tensile stresses generated during the deposition process may cause wafer warping, film cracking or peeling, affecting subsequent processes and device performance. At the same time, in complex multi-layer structures, stress is concentrated in certain areas, which may lead to excessive local stress, causing microcracks or interlayer separation.
[0006] (2) Impact on transistor performance: Uneven stress distribution will lead to inconsistent transistor performance and affect the overall performance of the chip.
[0007] (3) Thermal stability and stress changes: Semiconductor devices undergo multiple thermal cycles during manufacturing and operation. The stress of silicon nitride films may change at different temperatures, leading to stress accumulation and stress relaxation, affecting the long-term reliability of the device.
[0008] (4) Manufacturing difficulty: During the multi-layer manufacturing process, the stress of the silicon nitride film needs to be precisely controlled to ensure stress balance between each layer. This increases the complexity and cost of the manufacturing process. The window for controlling the stress of the silicon nitride film is narrow, and a slight deviation may cause the stress to exceed the standard, affecting the stability of the overall process.
[0009] At present, there are several technical methods to relieve the stress of silicon nitride films:
[0010] (1) Doping: Doping other elements (such as hydrogen, oxygen, etc.) into silicon nitride films can effectively improve the stress state of the film.
[0011] (2) Thermal annealing: Annealing can rearrange the atoms in the film, thereby reducing internal stress.
[0012] (3) Surface treatment: Before depositing silicon nitride film, surface treatment of the substrate (such as roughening, etching, chemical modification, etc.) can improve the adhesion and stress distribution of the film, thereby relieving stress.
[0013] (4) Film thickness control: By precisely controlling the thickness of the silicon nitride film, the accumulation of stress can be reduced.
[0014] (5) Use of buffer layer: Introducing a buffer layer (such as silicon dioxide) between the silicon nitride film and the substrate can alleviate stress concentration at the interface.
[0015] These solutions all have some limitations. For example, the non-uniformity of doping concentration can lead to local stress concentration, and impurities can also affect the electrical properties of the film; thermal budget and oxidation issues during thermal annealing; damage risks and precision requirements of surface treatment; the influence of the film's extreme thickness. Too thin silicon nitride films may experience mechanical and thermal stress instability and be prone to cracking and failure; the buffer layer may bring additional stress and interface problems, leading to the introduction of new stress concentration and defects.
[0016] Therefore, it is necessary to develop new process methods and thin film structures to meet the high precision and performance requirements of deep submicron processes in order to achieve effective stress relief. Summary of the invention
[0017] In view of the problems in the prior art, the purpose of the present application is to provide a method for preparing a semiconductor structure and a semiconductor structure, so as to effectively alleviate the internal stress of the second film and improve the performance and reliability of the semiconductor structure.
[0018] The present invention provides a method for preparing a semiconductor structure, comprising:
[0019] providing a substrate;
[0020] forming at least one stress release structure on one side of the substrate, each of the stress release structures comprising a first film and a graphene film, wherein the graphene film is located on a side of the first film away from the substrate;
[0021] A second film is formed on a side of the stress release structure away from the substrate.
[0022] In some embodiments, the stress release structure includes a first film and a plurality of graphene films, and the plurality of graphene films are sequentially formed on a side of the first film facing away from the substrate.
[0023] In some embodiments, forming at least one stress relief structure on one side of the substrate comprises the following steps:
[0024] A plurality of stress release structures are sequentially formed on one side of the substrate, and the plurality of stress release structures are sequentially superimposed on one side of the substrate.
[0025] In some embodiments, the stress relief structure is formed by the following steps:
[0026] forming a first thin film on one side of the substrate;
[0027] A graphene film is formed on the side of the first film facing away from the substrate by using a chemical vapor deposition method or a transfer method.
[0028] In some embodiments, when a graphene film is formed on the side of the first film facing away from the substrate by chemical vapor deposition, methane is used as the carbon source, hydrogen is used as the auxiliary gas, the carrier is an inert gas or nitrogen, the deposition temperature is 600-1200°C, the methane flow rate is 10-100sccm, and the hydrogen flow rate is 100-500sccm.
[0029] In some embodiments, the first film is a silicon dioxide film, and is formed on one side of the substrate by using a furnace thermal oxidation method or a chemical vapor deposition method.
[0030] In some embodiments, the graphene film has a thickness of 0.34 nm to 5 nm.
[0031] In some embodiments, forming a second film on a side of the stress release structure away from the substrate comprises the following steps:
[0032] A second film is formed on a side of the stress release structure away from the substrate by using a plasma enhanced chemical vapor deposition method.
[0033] In some embodiments, the second film is a silicon nitride film, and after the second film is formed on the side of the stress release structure away from the substrate, the following steps are further included:
[0034] forming a photoresist layer on a side of the second film away from the stress release structure;
[0035] Etching the photolithography window to form a groove structure;
[0036] After the groove structure is filled, chemical mechanical polishing is used to remove the stress release structure and the second film.
[0037] The embodiment of the present application also provides a semiconductor structure, which is prepared using the semiconductor structure preparation method described above.
[0038] The semiconductor structure preparation method and semiconductor structure provided in this application have the following advantages:
[0039] The preparation method of the present application and the resulting semiconductor structure can effectively alleviate the internal stress of the second film, achieve the release of the internal stress of the second film by introducing a graphene film layer, alleviate the atomic mismatch phenomenon at the joint interface of heterogeneous film layers, enhance process compatibility, prevent wafer warping and deformation, improve mechanical properties and thermal stability, optimize electrical properties, and improve the performance and reliability of the second film in semiconductor manufacturing applications. BRIEF DESCRIPTION OF THE DRAWINGS
[0040] Other features, objects and advantages of the present application will become more apparent by reading the detailed description of non-limiting embodiments made with reference to the following drawings.
[0041] Figure 1 is a flow chart of a method for preparing a semiconductor structure according to an embodiment of the present application;
[0042] Figure 2 It is a schematic diagram of the structure of two-dimensional graphene;
[0043] Figure 3 is a schematic diagram of the structure of two-dimensional graphene nitride;
[0044] Figure 4 is a schematic diagram of a semiconductor structure according to an embodiment of the present application;
[0045] Figures 5 to 9 is a schematic diagram of a process of removing a thin film layer on a substrate in a semiconductor structure according to an embodiment of the present application; wherein, Figure 5 is a schematic diagram of forming a photoresist on the second film; Figure 6 A schematic diagram of forming a photolithography window; Figure 7 A schematic diagram of forming a shallow trench etching window; Figure 8Schematic diagram of etching a window to fill a shallow trench; Fig. 9 A schematic diagram of forming a shallow trench after etching away each film layer on the substrate;
[0046] Fig.10 is a schematic diagram of a semiconductor structure according to another embodiment of the present application;
[0047] Fig.11 is a schematic diagram of a semiconductor structure according to yet another embodiment of the present application. DETAILED DESCRIPTION
[0048] Example embodiments will now be described more fully. However, example embodiments can be implemented in a variety of forms and should not be construed as limited to the embodiments set forth herein; on the contrary, these embodiments are provided so that the present application will be comprehensive and complete, and the concept of the example embodiments will be fully conveyed to those skilled in the art. "Or" and "or" in the specification may both mean "and" or "or". Although the terms "upper", "lower", "between", etc. may be used in this specification to describe different exemplary features and elements of the present application, these terms are used herein only for convenience, such as according to the directions of the examples described in the accompanying drawings. Nothing in this specification should be construed as requiring a specific three-dimensional direction of the structure to fall within the scope of the present application. Although "first" or "second" etc. are used in this specification to represent certain features, they are only used to represent the function, and are not used as a limitation on the number and importance of specific features.
[0049] The present application provides a method for preparing a semiconductor structure and a semiconductor structure prepared by the preparation method. The preparation method comprises: providing a substrate; forming at least one stress release structure on one side of the substrate, each of the stress release structures comprising a first film and a graphene film, the graphene film being located on the side of the first film away from the substrate; and forming a second film on the side of the stress release structure away from the substrate. The preparation method of the present application and the obtained semiconductor structure can effectively relieve the internal stress of the second film, release the internal stress of the second film by introducing a graphene film layer, relieve the atomic mismatch phenomenon at the joint surface of heterogeneous film layers, enhance process compatibility, prevent wafer warping and deformation, improve mechanical properties and thermal stability, optimize electrical properties, and improve the performance and reliability of the second film in semiconductor manufacturing applications.
[0050] The following is a detailed description of the method for preparing the semiconductor structure and the semiconductor structure in several embodiments in conjunction with the accompanying drawings. The same reference numerals in the figures represent the same or similar structures, and thus their repeated descriptions will be omitted. The sizes and proportions of the various film layers shown in the figures are only examples and are not intended to represent the sizes and proportions of the actual film layers.
[0051] Figure 11 is a flow chart of a method for preparing a semiconductor structure according to an embodiment of the present application. Figure 1 As shown, the method for preparing the semiconductor structure includes:
[0052] S100: providing a substrate; in this embodiment, the substrate is a silicon substrate;
[0053] S200: forming at least one stress release structure on one side of the substrate, each of the stress release structures comprising a first film and a graphene film, wherein the graphene film is located on a side of the first film away from the substrate;
[0054] In this embodiment, the first film is a silicon dioxide (SiO2) film, which can be used as a buffer layer for a silicon nitride film. In the prior art, silicon oxide films and silicon nitride films are directly superimposed on each other, and there are differences in their thermal expansion coefficients and lattice matching, which will cause stress accumulation when the temperature changes or under the action of the inherent stress of the silicon nitride film. When the silicon oxide film is thin, cracks between the film layers or stress transfer to the silicon substrate may occur, resulting in a decrease in device performance. When the silicon oxide film is thick, the film deposition efficiency may be reduced.
[0055] The present application further adds a graphene film on the basis of the first film, such as Figure 2 As shown, graphene has a honeycomb crystal structure, and the carbon-carbon covalent bonds between carbon atoms are very strong, so that graphene can maintain its structure without being destroyed when stretched. When subjected to external forces, its unique crystal structure can effectively disperse local stress.
[0056] S300: forming a second film on a side of the stress release structure away from the substrate; in this embodiment, the second film is a silicon nitride film.
[0057] In the present application, a graphene film is added between the silicon nitride film and the first film, and the graphene film forms a flexible transition layer between the silicon nitride film and the first film. Graphene has high strength and flexibility, can absorb the stress in the silicon nitride film, reduce the stress concentration between the silicon dioxide film and the silicon nitride film, and thus relieve the overall stress level. Figure 3 As shown, the graphene film can form a good bond with the silicon nitride film through van der Waals force and covalent bonding (CN bond). By arranging one or more layers of graphene film on the lower surface or upper surface of the silicon nitride film, the stress distribution of the overall structure can be changed.
[0058] Therefore, the present application provides a process method that can effectively relieve the internal stress of silicon nitride film. The internal stress of silicon nitride film is released by introducing a graphene film layer. The high strength and elasticity, ultra-thin thickness, excellent thermal conductivity, good interface bonding and excellent process compatibility of the graphene film layer are utilized to improve the mechanical properties of silicon nitride film, reduce the internal stress of the film, improve the mechanical stability, provide good heat dissipation capability, maintain the stability of silicon nitride film during thermal cycling, and achieve improved device performance and reliability.
[0059] Figure 4 Schematic diagram of a semiconductor structure according to an embodiment of the present application. The semiconductor structure includes:
[0060] Substrate 100; in this embodiment, the substrate 100 is a silicon substrate;
[0061] A first film 200 is formed on one side of the substrate 100; in this embodiment, the first film 200 is a silicon dioxide film;
[0062] A graphene film 300 is formed on the side of the first film 200 away from the substrate 100; in this embodiment, the thickness of the graphene film is 0.34 nm to 5 nm, and the thickness of the graphene film here is only an example and is not intended to limit the scope of protection of the present application; the graphene film 300 and the first film 200 form a stress release structure;
[0063] The second film 400 is formed on a side of the graphene film 300 away from the first film 200 ; in this embodiment, the second film 400 is a silicon nitride film.
[0064] In this embodiment, the number of layers and thickness of the graphene film 300 can be selected as needed. The elastic modulus and mechanical properties of the graphene film 300 can be regulated by regulating its thickness, number of layers and lattice structure to achieve the regulation of stress distribution. By optimizing the thickness of the graphene film 300, a more effective stress relief effect can be achieved. When a single-layer graphene film 300 is used, it has an extremely low thickness and does not increase the thickness of the overall film structure. In this embodiment, a stress release structure is provided, which includes a first film 200 and a graphene film 300. In another embodiment, two or more stress release structures superimposed in sequence can be formed between the substrate 100 and the second film 400. Each stress release structure may include two or more graphene films 300. Various deformations are within the scope of protection of this application.
[0065] In this embodiment, in step S200, the stress release structure is formed by the following steps:
[0066] forming a silicon dioxide film on one side of the substrate;
[0067] Specifically, a silicon dioxide film is formed on one side of the substrate by a furnace thermal oxidation method or a chemical vapor deposition (CVD) method;
[0068] A graphene film is formed on the side of the silicon dioxide film away from the substrate by using a chemical vapor deposition method or a transfer method.
[0069] In one embodiment, when a graphene film is formed on the side of the silicon dioxide film away from the substrate by chemical vapor deposition, methane (CH4) is used as a carbon source (reaction precursor), hydrogen (H2) is used as an auxiliary gas to promote graphene growth, the carrier is an inert gas (helium or argon) or nitrogen, the deposition temperature is 600-1200°C, the methane flow rate is 10-100sccm, and the hydrogen flow rate is 100-500sccm. The process pressure can be low pressure (10-3Pa~105Pa) and ultra-low pressure (<10-3Pa). The thickness of the graphene film is 0.34nm (single layer)~5nm (multilayer).
[0070] In another embodiment, a transfer method is used to form a graphene film on the side of the silicon dioxide film facing away from the substrate, that is, the graphene film is transferred to the surface of the target silicon dioxide film by the transfer method, and the interface bonding strength is improved by post-processing.
[0071] In this embodiment, the step S300 of forming a second film on a side of the stress release structure away from the substrate includes the following steps:
[0072] Plasma enhanced chemical vapor deposition (PECVD) is used to form a silicon nitride film of a certain target thickness on the side of the stress release structure away from the substrate. When forming the silicon nitride film, the flow rate of the precursor gas ammonia (NH3) is 10-100sccm, the flow rate of silane (SiH4) is 150sccm, the deposition temperature is 300-400°C, and the film thickness range is 400-2000A. The graphene film obtained by chemical vapor deposition can form a good bond with the silicon nitride film through van der Waals force and covalent bonding (CN bond). By growing one or more layers of graphene film by CVD on the lower surface or upper surface of the silicon nitride film, the stress distribution of the overall structure can be changed.
[0073] In this embodiment, the silicon nitride film can be used for electrical insulation layers, hard mask layers, stress engineering, etch stop layers, diffusion barrier layers, high-K / metal gate (HKMG), and insulation layers in multi-layer interconnect structures in semiconductor devices. The following uses the silicon nitride film as an active area etch barrier layer and a shallow trench isolation chemical mechanical polishing stop layer as an example to illustrate the formation of Figure 4After the semiconductor structure is shown, a shallow trench isolation (STI) process is formed in the substrate.
[0074] like Figure 5 As shown, after forming the second film 400 on the side of the stress release structure (including the first film 200 and the graphene film 300) away from the substrate 100, a photoresist layer 500 is formed on the side of the second film 400 away from the stress release structure (200, 300). Figure 6 and Figure 7 As shown, etching is performed on the photolithography window 510 to form a shallow trench etching window 600. The photoresist layer 500 may be a positive photoresist or a negative photoresist. Figure 8 As shown, the shallow trench etching window 600 is filled with deposited oxide. Fig. 9 As shown, plasma dry etching or chemical mechanical polishing (CMP) is used to remove the silicon nitride film / graphene film / silicon dioxide film at the shallow trench etching window, and finally a shallow trench 110 is formed at the substrate 100. After the process is completed, a substrate 100 without warpage and lattice defects can be obtained, providing excellent prerequisites for subsequent processes. At the same time, a defect-free substrate 100 can ensure the reliability of semiconductor devices, improve the service life of semiconductor devices, and reduce the risk of failure.
[0075] Fig.10 A schematic diagram of a semiconductor structure of another embodiment of the present application is shown. Figure 4 The difference between the semiconductor structure shown in FIG. 1 is that a multilayer graphene film is formed between the first film 200 (silicon dioxide film) and the second film 400 (silicon nitride film), that is, the stress release structure includes a first film 200 and a multilayer graphene film. Fig.10 Two layers of graphene films 310 and 320 are shown exemplarily. However, the present application is not limited thereto. In other alternative embodiments, the number and subsequent steps of the graphene films can be set according to actual needs. In this embodiment, the synergistic effect of the multilayer graphene film structure is achieved, and in the multilayer graphene film, the interaction between different layers (van der Waals force) helps to relieve stress. The multilayer graphene film can share and relieve external stress through relative slip and interlayer interaction. Fig.10 The semiconductor structure can be applied, for example, to a situation where a single-layer graphene film is difficult to effectively alleviate the inherent stress of a silicon nitride film when the silicon oxide film is thin, but the present application is not limited thereto.
[0076] Fig.11 Schematic diagram of a semiconductor structure of another embodiment of the present application. Figure 4The difference between the semiconductor structure shown in is that: a plurality of stress release structures are formed between the substrate 100 and the second film 400, and each stress release structure includes a first film and a graphene film. In this embodiment, corresponding to the above step S200: at least one stress release structure is formed on one side of the substrate, including the following steps: a plurality of stress release structures are sequentially formed on one side of the substrate, and the plurality of stress release structures are sequentially superimposed on one side of the substrate. When the process requires a thicker silicon nitride film, it is difficult for the silicon oxide film + multi-layer graphene film to release the inherent stress of the silicon nitride film. It can be achieved by depositing a film such as Fig.11 The stacked graphene structure shown is formed by alternately depositing silicon dioxide films and graphene auxiliary layers. The number of stacked layers can be adjusted according to the stress state of the silicon nitride film to maximize stress relief. Fig.11 exemplarily shows a structure having two stress release structures, wherein the lower stress release structure includes a first film 210 and a graphene film 310, and the upper stress release structure includes a second film 220 and a graphene film 320. The present application is not limited thereto, and in other alternative embodiments, three stress release structures or more stress release structures may be formed as required, all of which fall within the protection scope of the present application.
[0077] In this embodiment, the graphene film is introduced to achieve crack protection, improve thermal stability, and improve mechanical stability and process compatibility. At the same time, the preparation process of the graphene film is relatively mature and easy to integrate into the existing semiconductor manufacturing process. Studies have shown that the surface flatness of the film prepared with the assistance of graphene is improved by 20% and the crack density is reduced by nearly 50% compared with a single film; another study shows that the graphene film as a stress buffer layer can significantly improve the thermal stability of the device and can effectively reduce the thermal stress caused by temperature changes. Experimental data show that in a high temperature environment, the stability of the device using graphene to relieve film stress is 30% higher than that of the traditional device.
[0078] In the above embodiments, the second film is a silicon nitride film as an example, that is, a graphene film is used to relieve the internal stress of the silicon oxide film. However, the present application is not limited to this. In other alternative embodiments, the second film can also be a gallium nitride film, a silicon carbide film, etc., and a graphene film is used to relieve the internal stress of the gallium nitride film, the silicon carbide film, etc., relieve the thermal stress and mechanical stress of the film layer, and improve the thermal management capability and reliability of semiconductor devices using these film layers.
[0079] In summary, by adopting the preparation method of the semiconductor structure of the present application, the internal stress of the second film can be effectively relieved, and the internal stress of the second film can be released by introducing a graphene film layer, thereby alleviating the atomic mismatch phenomenon at the joint interface of the heterogeneous film layers, enhancing process compatibility, preventing wafer warping and deformation, improving mechanical properties and thermal stability, optimizing electrical properties, and improving the performance and reliability of the second film in semiconductor manufacturing applications.
[0080] The above content is a further detailed description of the present application in combination with specific preferred implementation methods, and it cannot be determined that the specific implementation of the present application is limited to these descriptions. For ordinary technicians in the technical field to which the present application belongs, several simple deductions or substitutions can be made without departing from the concept of the present application, which should be deemed to fall within the scope of protection of the present application.
Claims
1. A method for preparing a semiconductor structure, It is characterized in that include: providing a substrate; forming at least one stress release structure on one side of the substrate, each of the stress release structures comprising a first film and a graphene film, wherein the graphene film is located on a side of the first film away from the substrate; A second film is formed on a side of the stress release structure away from the substrate.
2. The method for preparing a semiconductor structure according to claim 1, It is characterized in that The stress release structure includes a first film and a plurality of graphene films, wherein the plurality of graphene films are sequentially formed on a side of the first film away from the substrate.
3. The method for preparing a semiconductor structure according to claim 1, It is characterized in that Forming at least one stress release structure on one side of the substrate comprises the following steps: A plurality of stress release structures are sequentially formed on one side of the substrate, and the plurality of stress release structures are sequentially superimposed on one side of the substrate.
4. The method for preparing a semiconductor structure according to claim 1, It is characterized in that The stress release structure is formed by the following steps: forming a first thin film on one side of the substrate; A graphene film is formed on the side of the first film facing away from the substrate by using a chemical vapor deposition method or a transfer method.
5. The method for preparing a semiconductor structure according to claim 4, It is characterized in that When a graphene film is formed on the side of the first film away from the substrate by chemical vapor deposition, methane is used as a carbon source, hydrogen is used as an auxiliary gas, an inert gas or nitrogen is used as a carrier, the deposition temperature is 600-1200°C, the methane flow rate is 10-100sccm, and the hydrogen flow rate is 100-500sccm.
6. The method for preparing a semiconductor structure according to claim 4, It is characterized in that The first film is a silicon dioxide film, and is formed on one side of the substrate by using a furnace thermal oxidation method or a chemical vapor deposition method.
7. The method for preparing a semiconductor structure according to claim 1, It is characterized in that The thickness of the graphene film is 0.34nm-5nm.
8. The method for preparing a semiconductor structure according to claim 1, It is characterized in that The second film is a silicon nitride film, and forming the second film on a side of the stress release structure away from the substrate comprises the following steps: A second film is formed on a side of the stress release structure away from the substrate by using a plasma enhanced chemical vapor deposition method.
9. The method for preparing a semiconductor structure according to claim 1, It is characterized in that After forming a second film on a side of the stress release structure away from the substrate, the method further includes the following steps: forming a photoresist layer on a side of the second film away from the stress release structure; Etching the photolithography window to form a groove structure; After the groove structure is filled, chemical mechanical polishing is used to remove the stress release structure and the second film.
10. A semiconductor structure, It is characterized in that The semiconductor structure is prepared by the method for preparing the semiconductor structure according to any one of claims 1 to 8.