Water-stimuli-responsive room-temperature phosphorescent material, film, preparation method and application
By using the core and shell spinning technology of water-stimulated response room temperature phosphorescence materials in inorganic long afterglow luminescent materials, the high cost and biotoxicity problems of inorganic materials are solved, and a pure, low-toxicity and high-efficiency phosphorescence display in water environment is constructed. Organic flexible fiber films have expanded their application scenarios.
Patent Information
- Application Number
- CN202411175516.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-26
- Publication Date
- 2024-12-03
AI Technical Summary
The existing inorganic long-term afterglow luminescent materials have high cost, potential biotoxicity and water environment instability. The construction of pure organic long-term afterglow luminescent materials is difficult to build and have poor flexibility, which limits its application scenarios.
Using water-stimulated response room temperature phosphorescence materials, including core and shell materials, polyvinylpyrrolidone and polyacrylonitrile as spinning materials, N,N'-di-2-naphthyl-1,4-phenylenediamine and As a luminescent material, 4-methoxydipaniline is used to prepare a flexible fiber film through coaxial electrospinning technology, and the luminescent material is released in a water environment using the hygroscopicity of the core layer and the water-insoluble properties of the shell layer.
It realizes low-cost, low-toxicity, and efficient phosphorescence display in water environments, expands the application scenarios of stimulus response materials, especially in the fields of water writing, water leakage detection and information encryption, which has high practical value.
Smart Images

Figure CN119061524A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of room temperature phosphorescent (RTP) materials, in particular to a room temperature phosphorescent material responsive to water stimulation, a film, and a preparation method and application thereof. Background Art
[0002] As a type of smart material, stimuli-responsive organic light-emitting materials have attracted much attention in recent years due to their wide applications in biosensing, information encryption, data storage, and anti-counterfeiting. Compared with traditional fluorescent materials, RTP materials show longer emission lifetimes, which can even be captured by the naked eye. Therefore, the changes in emission lifetime, emission color, and intensity of RTP materials under external stimuli are potential monitoring parameters. This has greatly promoted the practical application of stimuli-responsive organic light-emitting materials.
[0003] So far, RTP materials are generally limited to inorganic materials containing metals, especially rare earth phosphors. Typical inorganic long afterglow materials include aluminates, silicates and sulfides. Since Matsuzawa in 1996 in strontium aluminate SrAl2O4:Eu 2 + After Dy doping in the nanostructured carbon nanotubes to achieve a 2000 min afterglow emission (J. Electrochem. Soc. 1996, 143, 2670-2673), inorganic long afterglow luminescent materials have made great progress. Their emission is controlled by the slow release of captured charge carriers from isolated traps of impurities, defects or ions through thermal stimulation with low luminescence efficiency. However, these materials have some inherent disadvantages, including high cost, potential biotoxicity and instability in aqueous environments.
[0004] In contrast to inorganic long afterglow luminescent materials, organic long afterglow luminescent materials have attracted much attention due to their good compatibility, photostability, thermal stability and chemical inertness, as well as excellent flexibility, low toxicity, material diversity, and diverse molecular structures. Purely organic long afterglow luminescent materials with special stimulus responses have become a research difficulty because they are difficult to construct. The RTP of some pure organic materials depends on the crystal structure and has poor flexibility, which greatly limits their application scenarios; the other part uses amorphous polymer molecules to construct a stimulus response system, but its RTP performance is poor and its flexibility is average.
[0005] In order to expand the application scenarios of pure organic long afterglow luminescent materials, we urgently need to combine other process technologies to prepare materials with good flexibility and stimulus responsiveness. Summary of the invention
[0006] In view of the deficiencies in the prior art, the object of the present invention is to provide a water stimulus responsive room temperature phosphorescent material, film, preparation method and application.
[0007] The present invention provides a room temperature phosphorescent material responsive to water stimulation.
[0008] Another object of the present invention is to provide a pure organic flexible fiber film that responds to water stimulation and exhibits room temperature phosphorescence properties.
[0009] Another object of the present invention is to provide a method for preparing a pure organic flexible fiber film that responds to water stimulation and exhibits room temperature phosphorescence properties.
[0010] Another object of the present invention is to provide a pure organic flexible fiber film that responds to water stimulation and displays room temperature phosphorescence properties for use in water writing and in-situ detection of water leakage.
[0011] Another object of the present invention is to provide a pure organic flexible fiber film that responds to water stimulation and displays room temperature phosphorescence properties for use in anti-counterfeiting and information encryption.
[0012] The purpose of the present invention is achieved through the following technical solutions.
[0013] A water stimulus responsive room temperature phosphorescent material, characterized in that it is a spinning process, comprising a core layer material and a shell material, and luminescent materials are added to both the core layer material and the shell layer material.
[0014] The water stimulus responsive room temperature phosphorescent material is characterized in that:
[0015] ⑤The core material has good hygroscopic properties, ensuring that the fiber can release the luminescent material when it comes into contact with water;
[0016] ⑥ The shell material has good water insolubility and can provide attachment and support for the luminescent material to prevent the spinning membrane from dissolving;
[0017] ⑦ The viscosity of the core material and the shell material should be compatible and have good solubility in the same spinning solvent;
[0018] ⑧The luminescent material has good solubility in the spinning solvent.
[0019] The water stimulus responsive room temperature phosphorescent material is characterized in that the core layer material and the shell layer material are selected from polyvinyl pyrrolidone PVP and polyacrylonitrile PAN respectively.
[0020] The water stimulus responsive room temperature phosphorescent material is characterized in that the luminescent material constitutes a long afterglow luminescent system: N,N'-di-2-naphthyl-1,4-phenylenediamine DBNPD is selected as the guest molecule and 4-methoxydiphenylamine MO-DPA is selected as the host molecule; the molar ratio of the host and guest molecules is 80-100:1.
[0021] A pure organic flexible fiber film that responds to water stimulation and exhibits room temperature phosphorescence properties is characterized in that the film is made of the water stimulation responsive room temperature phosphorescence material.
[0022] The method for preparing the pure organic flexible fiber film that responds to water stimulation and exhibits room temperature phosphorescence characteristics is characterized in that:
[0023] S1: Weigh appropriate amounts of core layer and shell layer materials, add appropriate amounts of luminescent materials respectively, and then add appropriate amounts of solvent to dissolve and prepare core layer and shell layer precursor solutions;
[0024] S2: extracting the precursor solution, adjusting the spinning parameters and spinning using a coaxial electrospinning device.
[0025] The method for preparing a pure organic flexible fiber film that responds to water stimulation and displays room temperature phosphorescence properties is characterized in that the core layer material and shell layer material are respectively selected from polyvinyl pyrrolidone and polyacrylonitrile; the mass percentage of polyvinyl pyrrolidone in the core layer and shell layer precursor solutions is 8%, and the mass percentage of polyacrylonitrile is 12%; the mass percentage of the luminescent material accounts for 33% of the spinning material.
[0026] The method for preparing a pure organic flexible fiber film that responds to water stimulation and shows room temperature phosphorescence characteristics is characterized in that the spinning solution stirring temperature is 50°C, the time is 12 hours, and the rotation speed is 10rpm; the spinning voltage is 20kV, the inner layer spinning solution pushing speed is 0.4mL / h, and the outer layer spinning solution pushing speed is 0.5mL / h.
[0027] Pure organic flexible fiber films that display room-temperature phosphorescence in response to water stimulation are used in water writing and in-situ detection of water pipeline leakage.
[0028] Pure organic flexible fiber films that display room-temperature phosphorescence properties in response to water stimulation are used in anti-counterfeiting and information encryption.
[0029] Mechanism of organic flexible fiber film showing room temperature phosphorescence in response to water stimulation
[0030] Since the carbon and hydrogen atoms in the nitrile group of PAN are connected by a σ bond and two π bonds, this structure can absorb high-energy ultraviolet light and convert it into heat energy. The RTP material receives less excitation light, which leads to poor luminescence performance of the flexible film directly obtained by coaxial electrospinning. The TEM images of the flexible film before and after contacting water show that the ratio of the core layer diameter to the overall fiber diameter is about 48%, proving that the fiber has a good coaxial structure. When the fiber is exposed to water, uneven voids appear inside the fiber. This shows that after the fiber is exposed to water, the internal PVP is partially dissolved, exposing more luminescent materials, thereby enhancing the luminescence performance.
[0031] The prepared pure organic flexible fiber film that responds to water stimulation and shows room temperature phosphorescence characteristics is used as a writable film, and text or pattern information is input on the film through processes such as water coating or water writing. After being excited by ordinary ultraviolet light, the water-coated or water-written area shows bright phosphorescence emission.
[0032] The prepared pure organic flexible fiber film that responds to water stimulation and shows room temperature phosphorescence properties is wrapped around a water pipe. When a local trace water leakage occurs, the spun membrane absorbs moisture and shows phosphorescence emission in situ after being excited by ordinary ultraviolet light.
[0033] The beneficial effects of the present invention are as follows:
[0034] 1. The luminescent material selected by the present invention uses cheap raw materials and shows bright green room temperature phosphorescence after being excited by ordinary ultraviolet light;
[0035] 2. The pure organic flexible fiber film prepared by the present invention that responds to water stimulation and exhibits room temperature phosphorescence characteristics has a simple preparation method, and the materials used are all organic materials with good flexibility. This is a new idea and strategy for constructing stimulus-responsive phosphorescent materials using coaxial electrospinning technology. Based on the water stimulation response characteristics and good flexibility, the design ideas and application prospects of stimulus-responsive materials are greatly expanded.
[0036] 3. The pure organic flexible fiber film prepared by the present invention has sensitive water stimulus response and room temperature phosphorescence characteristics, and has high practical value in information input, in-situ detection system of water pipeline leakage, etc. This strategy for preparing a pure organic flexible fiber film with stimulus response and room temperature phosphorescence characteristics is reported for the first time in the world.
[0037] 4. The pure organic flexible fiber film prepared by the present invention also has good applications in the fields of information encryption and anti-counterfeiting. BRIEF DESCRIPTION OF THE DRAWINGS
[0038] Figure 1 is a schematic diagram of preparing a flexible film in Example 1 and a schematic diagram of its water stimulus response;
[0039] Figure 2 are SEM images of the flexible film prepared in Example 1 before and after contact with water;
[0040] Figure 3 are TEM images of the flexible film prepared in Example 1 before and after contact with water;
[0041] Figure 4 are fluorescence microscope images of the flexible film prepared in Example 1 before and after contact with water;
[0042] Figure 5is a schematic diagram of the mechanism by which the flexible film prepared in Example 1 has a water stimulus response;
[0043] Figure 6 This is a display diagram of Example 2 after water writing and information coating;
[0044] Figure 7 This is a performance display diagram of the flexible film after high humidity environment interference in Example 3;
[0045] Figure 8 It is a schematic diagram and actual display diagram of the application of water leakage detection in the water delivery system according to Example 4. DETAILED DESCRIPTION
[0046] The technical solution of the present invention is further described below in conjunction with specific embodiments.
[0047] In the following examples, N,N'-di-2-naphthyl-1,4-phenylenediamine (DBNPD) was purchased from Tianjin Xiensi Biochemical Technology Co., Ltd. 4-Methoxydiphenylamine (MO-DPA) was purchased from Sane Chemical Technology (Shanghai) Co., Ltd. Polyacrylonitrile (PAN, molecular weight: 250K) was purchased from DuPont, USA. Polyvinylpyrrolidone (PVP) was purchased from Shandong Yousuo Chemical Technology Co., Ltd. N,N-dimethylformamide (DMF) was purchased from Tianjin Dengke Chemical Reagent Co., Ltd.
[0048] The instruments and models involved in the tests in the following embodiments are:
[0049] Ocean Optics multi-band spectrometer, FlexSEM 1000 scanning electron microscope, F-7000 fluorescence spectrometer;
[0050] Room temperature: 20~25℃.
[0051] The power of the UV lamp in the following examples is 20W (365nm).
[0052] Example 1
[0053] The luminescent material selected N,N'-di-2-naphthyl-1,4-phenylenediamine (DBNPD) as the guest molecule and 4-methoxydiphenylamine (MO-DPA) as the host molecule; the core layer material and the shell layer material were polyvinyl pyrrolidone (PVP) and polyacrylonitrile (PAN), respectively.
[0054] 1) Weigh 7 mL of reagent N,N-dimethylformamide and place it in clean and dry containers A and B respectively; weigh 0.0072 g of N,N'-di-2-naphthyl-1,4-phenylenediamine and 0.3986 g of 4-methoxydiphenylamine and place it in container A; weigh 0.0113 g of N,N'-di-2-naphthyl-1,4-phenylenediamine and 0.6251 g of 4-methoxydiphenylamine and place it in container B; start and adjust the stirrer speed to 10 rpm at room temperature. Under room temperature stirring, add 0.6087 g of polyvinylpyrrolidone (PVP) to container A and 0.9545 g of polyacrylonitrile (PAN) to container B. Seal containers A and B and transfer them to a heat-collecting constant temperature heating magnetic stirrer, adjust the temperature to 50°C, keep the speed at 10 rpm, and stir for 12 hours.
[0055] 2) Transfer the stirred A and B liquids to syringes ① and ② respectively. Place syringes ① and ② at the core and shell positions of the coaxial electrospinning jet device. The spinning conditions are as follows: the distance between the needle and the receiver is 15 cm, the voltage is 20.00 KV, and the core layer syringe push speed is 0.40 mL·h -1 The shell syringe push speed is 0.50 mL·h -1 , the spinning time is 8h.
[0056] Figure 1 Schematic diagram of the preparation of the flexible film in Example 1 and its water stimulus response.
[0057] Figure 2 The SEM images of the flexible film prepared in Example 1 before and after contact with water are shown in Figure 1. As can be seen from the figure, there are some bead-like sites inside the flexible film. According to the general particle size of the luminescent material, the initial weak RTP of the flexible film comes from these bead-like areas. After contact with water, a large number of irregular substances appear between the fibers, which are the source of the enhanced RTP.
[0058] Figure 3 TEM images of the flexible film prepared in Example 1 before and after contact with water. As can be seen from the figure, when the fiber is exposed to water, uneven cavities appear inside the fiber. This is because the internal PVP is partially dissolved, exposing more luminescent materials, thereby enhancing the luminescent performance.
[0059] Figure 4 The following are fluorescence microscope images of the flexible film prepared in Example 1 before and after contact with water. As can be seen from the figure, the initial weak RTP of the flexible film originates from these beaded regions. After contact with water, a large number of other luminescent sites appear between the fibers, which enhances the RTP performance of the film.
[0060] Figure 5Schematic diagram of the mechanism of the flexible film prepared in Example 1 having a water stimulus response. When the flexible film contacts water, the fiber has a certain water absorption due to the presence of the core layer PVP. When water enters the interior of the fiber, the core layer PVP is partially destroyed, thereby releasing the luminescent material in the core layer, and thus the luminescent performance of the wet water area is enhanced.
[0061] Example 2
[0062] Take the film material obtained in Example 1, lay it flat on a hard plane, and assemble a water writing pen core. Use the water writing pen core to write text or input encrypted information. The written content can show bright green room temperature phosphorescence after being excited by ordinary ultraviolet light. After that, the encrypted information film can be soaked in water to achieve information coverage.
[0063] Figure 6 This is a display diagram after water writing and information coating in Example 2. As can be seen from the figure, the film has good information input and reading capabilities and has good application prospects in the fields of information encryption and anti-counterfeiting.
[0064] Example 3
[0065] The film material obtained in Example 1 was used to write with water using the water writing pen prepared in Example 2 to input information. The film was placed in an environment with a humidity of 60%, 70%, and 80% for one week to test its water stimulus response resistance to high humidity interference.
[0066] Figure 7 This is a performance display diagram of the flexible film after being subjected to high humidity environment interference in Example 3. As can be seen from the figure, in a high humidity environment, the film still has good water stimulus response characteristics, indicating that the film has good practical application prospects.
[0067] Example 4
[0068] Take the film material obtained in Example 1, cut it into 1 cm wide strips, and wrap it around a water pipeline. When a leak occurs in the water pipeline, the spinning membrane absorbs water and can show phosphorescence emission in situ after being excited by ordinary ultraviolet light. Further, a marine fiber optic spectrometer is used to convert the optical signal into an electrical signal. Whether there is an abnormality in the signal attenuation is determined to realize a water leakage monitoring system.
[0069] Figure 8It is a schematic diagram and actual display diagram of the application of water leakage detection in the water delivery system in Example 3. The spinning membrane tape is evenly wrapped around the water delivery pipe. Among them, due to the superior flexibility of the spinning membrane, it can fit tightly with the water delivery pipe. When the spinning membrane wrapped on the outside of the pipeline is excited by 365nm ultraviolet light, if an obvious LPL emission area appears, it means that a leak has occurred at that location, and the size of the LPL emission area can be used to judge the degree of leakage. Furthermore, when the attenuation of the light signal intensity is abnormal, it means that a leak has occurred at that location. This visual in-situ monitoring of leaks shows its excellent commercial application value in special water delivery systems.
Claims
1. A water-stimulus-responsive room-temperature phosphorescent material, characterized in that: The invention relates to a spinning method, which comprises a core material and a shell material, and luminescent materials are added to both the core material and the shell material.
2. The water stimulus responsive room temperature phosphorescent material according to claim 1, characterized in that: ①The core material has good moisture absorption properties, ensuring that the fiber can release the luminescent material when it comes into contact with water; ②The shell material has good water insolubility and can provide attachment and support for the luminescent material to prevent the spinning membrane from dissolving; ③The viscosity of the core material and the shell material should be compatible and have good solubility in the same spinning solvent; ④The luminescent material has good solubility in the spinning solvent.
3. The water stimulus responsive room temperature phosphorescent material according to claim 1 or 2, characterized in that: The core layer material and shell layer material are selected from polyvinyl pyrrolidone PVP and polyacrylonitrile PAN respectively.
4. The water stimulus responsive room temperature phosphorescent material according to claim 1, characterized in that: The luminescent material constitutes a long afterglow luminescent system: N,N'-di-2-naphthyl-1,4-phenylenediamine DBNPD is selected as the guest molecule and 4-methoxydiphenylamine MO-DPA is the host molecule; the molar ratio of the host molecule to the guest molecule is 80-100:
1.
5. A pure organic flexible fiber film that exhibits room temperature phosphorescence in response to water stimulation, characterized in that: A film is made using the water stimulus responsive room temperature phosphorescent material described in any one of claims 1 to 4.
6. The method for preparing the pure organic flexible fiber film showing room temperature phosphorescence characteristics in response to water stimulation according to claim 6, characterized in that: S1: Weigh appropriate amounts of core layer and shell layer materials, add appropriate amounts of luminescent materials respectively, and then add appropriate amounts of solvent to dissolve and prepare core layer and shell layer precursor solutions; S2: extracting the precursor solution, adjusting the spinning parameters and spinning using a coaxial electrospinning device.
7. The method for preparing the pure organic flexible fiber film showing room temperature phosphorescence characteristics in response to water stimulation according to claim 7, characterized in that: The core layer material and shell layer material are selected from polyvinyl pyrrolidone and polyacrylonitrile respectively; the mass percentage of polyvinyl pyrrolidone in the core layer and shell layer precursor solution is 8%, and the mass percentage of polyacrylonitrile is 12%; the mass percentage of the luminescent material accounts for 33% of the spinning material.
8. The method for preparing the pure organic flexible fiber film that responds to water stimulation and exhibits room temperature phosphorescence properties according to claim 6, characterized in that: The stirring temperature of the spinning solution is 50°C, the time is 12h, and the rotation speed is 10rpm; the spinning voltage is 20kV, the pushing speed of the inner layer spinning solution is 0.4mL / h, and the pushing speed of the outer layer spinning solution is 0.5mL / h.
9. Application of pure organic flexible fiber film that displays room temperature phosphorescence properties in response to water stimulation in water writing and in-situ detection of water pipeline leakage.
10. Application of pure organic flexible fiber films that display room temperature phosphorescence properties in response to water stimulation in anti-counterfeiting and information encryption.
Citation Information
Cited By
Light printing LPL flexible thin film material as well as preparation method and application thereof
CN120520016A
Optical printing LPL flexible film material and preparation method and application thereof
CN120520016B
Universal method for preparing water vapor response type LPL intelligent thin film
CN120625263A
A general method for preparing water vapor responsive LPL smart film
CN120625263B