Radiation-proof flame-retardant body armor and manufacturing method thereof
Through the body armor that blends polyethylene fiber and polyimide fiber and coats aluminum foil, the existing body armor has solved the problem of insufficient radiation and flame retardant performance, and achieved efficient electromagnetic wave shielding and flame retardant effects. Simple, suitable for mass production.
Patent Information
- Application Number
- CN202411485157.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-10-23
- Publication Date
- 2024-12-03
AI Technical Summary
The existing body armor has insufficient performance in radiation protection and flame retardant, and the manufacturing process is complex and costly. In particular, the radiation protection performance is less studied, and the commonly used silver plating process is expensive and complex.
Using composite materials made of polyethylene fiber and polyimide fiber, and coated with aluminum foil on the outer layer, the body armor is manufactured through cross-laminated structure and hot pressing composite process to achieve multiple properties of radiation, flame retardant and bulletproof .
It has achieved effective shielding of electromagnetic radiation in battlefield environments, reducing radiation hazards, and has efficient flame retardant properties to avoid harmful gases. It has a simple process, reduces production costs, and is suitable for large-scale production.
Smart Images

Figure CN119063577A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to a radiation-proof flame-retardant bulletproof vest and a manufacturing method thereof. Background Art
[0002] The combat environment on the battlefield is complex, and certain types of bullets, such as depleted uranium armor-piercing bullets, are indeed radioactive, so radiation may be generated when using these ammunition. Depleted uranium armor-piercing bullets are a special type of ammunition that is made of hard alloy containing depleted uranium 238, which has weaker radioactivity. This material has strong penetrating power and is often used to attack tanks and armored vehicles. Although the radioactivity of depleted uranium bullets is lower than other types of uranium, they still cause great harm to the human body. When depleted uranium bullets burn, aerosolized uranium oxide and depleted uranium particles can enter the human body, causing severe internal irradiation, which may cause serious damage to human organs.
[0003] In addition, general bulletproof vests mainly focus on the bulletproof effect, and pay less attention to radiation protection, flame retardancy and other properties. For example, flame retardancy mainly relies on adding flame retardants such as halogens to the fabric, but when the clothes burn, they will produce gases that are harmful to the human body and endanger health. There is less research on radiation-proof bulletproof vests, so safe and environmentally friendly fabric flame retardant methods and radiation protection are urgently needed. At present, the radiation protection on the market mainly adopts silver plating technology, which is expensive and the silver plating process is complicated.
[0004] Therefore, those skilled in the art are in urgent need of a radiation-proof and flame-retardant bulletproof vest with simple materials and simple manufacturing process. Summary of the invention
[0005] The purpose of the present invention is to solve the deficiencies of the above prior art and provide a radiation-proof flame-retardant bulletproof vest and a method for manufacturing the same. A new composite material is made by blending in a reasonable proportion, and aluminum foil is coated on the outer layer of the protective clothing. The bulletproof vest made of this material can achieve radiation-proof flame retardancy at the same time, and its structure and manufacturing process are simple. This purpose of the present invention is achieved as follows:
[0006] On the one hand, a radiation-proof flame-retardant bulletproof vest is provided, wherein the bulletproof vest is formed by cross-laminating at least two layers of UD cloth, wherein the cross-angle is 90°, wherein the UD cloth comprises polyethylene fiber and polyimide fiber, wherein the UD cloth is composed of polyethylene and polyimide in a mass ratio of (1 to 8): 1, wherein the polyethylene fiber is 400-800D, and the polyimide fiber is 1-7D, and the outer surface of the UD cloth is coated with aluminum foil, wherein the thickness of the aluminum foil is 80 μm-200 μm.
[0007] Polyethylene fiber has extremely high tensile strength and impact resistance. Its tensile strength is about 15 times that of steel, but its density is extremely low. This fiber can not only provide effective physical protection against the impact of high-speed projectiles, but also has excellent chemical resistance and wear resistance. The low thermal conductivity and low water absorption of polyethylene fiber enable it to maintain good mechanical properties in a humid environment.
[0008] Polyimide fiber is a polymer material with excellent flame retardant properties. Its notable features are high temperature resistance, no melting and dripping, self-extinguishing when away from fire, and no release of toxic gases when burning. In addition, polyimide fiber has excellent radiation resistance and can effectively protect against radiation hazards from specific weapons and ammunition on the battlefield. Due to its excellent mechanical and chemical resistance, polyimide fiber can still maintain dimensional stability and long-term durability in high temperature and complex environments.
[0009] Aluminum foil has good electromagnetic wave shielding properties and can reflect and absorb most of the electromagnetic radiation. When wrapped on the outer layer of the bulletproof vest, the aluminum foil reflects and absorbs electromagnetic radiation and converts it into heat energy, thereby reducing the impact of radiation on the human body. The aluminum foil itself is non-flammable, which not only improves the radiation protection performance, but also enhances the flame retardancy, ensuring the safety of the bulletproof vest in various fire or high temperature environments.
[0010] Through blending, the multiple properties of the material are balanced, making the protective clothing bulletproof, flame retardant and radiation proof.
[0011] Furthermore, the UD cloth further comprises a substrate film, and the polyethylene and polyimide are fixed on the substrate film by an adhesive.
[0012] Furthermore, the adhesive is epoxy resin.
[0013] On the other hand, a method for manufacturing a radiation-proof flame-retardant bulletproof vest comprises the following steps: a) blending polyethylene fiber and polyimide fiber in a ratio of (1-8):1; b) spreading a substrate film flat, impregnating an adhesive and evenly spreading it on the film, spreading the blended fibers, pressing the blended fibers onto the adhesive surface, and drying them in an oven; c) placing UD cloths that are in contact with each other crosswise at a crossing angle of 90°; d) hot-pressing and compounding the product of c; and e) wrapping the product of d as a whole with aluminum foil, and fixing the four corners of the aluminum foil on the product by sewing.
[0014] Furthermore, in step b), the drying temperature is 50° C.-80° C., and the drying time is 10-30 minutes.
[0015] Furthermore, in step c), the compounding temperature is 90-140° C., the compounding pressure is 1-10 MPa, and the compounding speed is 1-10 m / min.
[0016] Beneficial effects: The present invention adopts aluminum foil as the covering material, and utilizes the reflection and absorption characteristics of aluminum foil on electromagnetic waves, so that the bulletproof vest can effectively shield electromagnetic radiation, and is particularly suitable for dealing with the radiation hazards brought by weapons such as depleted uranium armor-piercing bullets on the battlefield. Experimental results show that within the frequency range of 10MHz to 3000MHz, the shielding effectiveness can reach 96.2% to 98.5%, effectively reducing the damage of radiation to the wearer;
[0017] Due to its high heat resistance and flame retardancy, the bulletproof vest of the present invention can self-extinguish in high temperature and fire environments without generating harmful gases, thus ensuring the safety of the wearer. The fiber material does not require the addition of additional flame retardants, thus avoiding the generation of toxic gases when conventional flame retardant materials are burned, thus having the advantages of environmental protection and safety.
[0018] The manufacturing method of the present invention has a simple process flow, and the preparation of the bulletproof material can be achieved mainly through the steps of blending, bonding, hot pressing and compounding. Compared with complex radiation protection processes such as traditional silver plating, the aluminum foil coating method of the present invention is more economical, reduces production costs, and is suitable for large-scale production. BRIEF DESCRIPTION OF THE DRAWINGS
[0019] Figure 1 It is a structural schematic diagram of a single-layer UD cloth for radiation-proof and flame-retardant bulletproof vest;
[0020] Figure 2 It is a schematic diagram of the structure of the interlaced UD cloth of a radiation-proof and flame-retardant bulletproof vest;
[0021] Figure 3 It is a schematic diagram of the structure of a radiation-proof and flame-retardant bulletproof vest with UD cloth coated with aluminum foil;
[0022] In the figure: 1. polyethylene fiber, 2. polyimide fiber, 3. aluminum foil, 4. suture. DETAILED DESCRIPTION
[0023] In order to deepen the understanding of the present invention, the present invention will be further described in detail below in conjunction with embodiments and drawings. The embodiments are only used to explain the present invention and do not constitute a limitation on the protection scope of the present invention.
[0024] The present invention provides a radiation-proof flame-retardant bulletproof vest on one hand. The bulletproof vest is formed by cross-stacking at least two layers of UD cloth, the cross-angle of which is 90°, the UD cloth comprises polyethylene fiber 1 and polyimide fiber 2, the UD cloth is composed of polyethylene and polyimide in a mass ratio of (1-8):1, the polyethylene fiber 1 is 400-800D, the polyimide fiber 2 is 1-7D, the outer surface of the UD cloth is coated with aluminum foil 3, the thickness of the aluminum foil 3 is 80μm-200μm, the UD cloth also comprises a substrate film, the polyethylene and polyimide are fixed on the substrate film by an adhesive, and the adhesive is an epoxy resin.
[0025] On the other hand, the present invention provides a method for manufacturing a radiation-proof flame-retardant bulletproof vest, comprising the following steps: a) blending polyethylene fiber 1 and polyimide fiber 2 in a ratio of (1-8):1; b) spreading a substrate film, impregnating an adhesive and evenly spreading it on the film, spreading the blended fiber, pressing the blended fiber onto the surface of the adhesive, and drying in an oven; c) placing UD cloths that are in contact with each other crosswise at a crossing angle of 90°; d) hot-pressing and laminating the product of c; e) wrapping the product of d as a whole with aluminum foil 3, and fixing the four corners of the aluminum foil 3 on the product by sewing with sutures 4; the drying temperature in step b) is 50°C-80°C, and the drying time is 10-30 minutes; the laminating temperature in step c) is: 90-140°C; the laminating pressure is 1-10MPa; and the laminating speed is 1-10m / min.
[0026] For the purpose of greater clarity, the invention is described in detail through the following examples.
[0027] Embodiment 1:
[0028] The polyethylene fiber 1 and the polyimide fiber 2 are blended in a ratio of 1:1. The specification of the polyethylene fiber 1 is 600D, and the specification of the polyimide fiber 2 is 3D. This embodiment has two layers of UD cloth.
[0029] The following are the manufacturing steps:
[0030] Step a): blending polyethylene fiber 1 and polyimide fiber 2 in a ratio of 1:1 to form a blended yarn;
[0031] Step b): Spread the substrate film flat, use epoxy resin as an adhesive, evenly apply it on the substrate film, and evenly press the blended fiber on the adhesive surface after unfolding. The drying temperature of the adhesive is set to 60° C. and the drying time is 20 minutes;
[0032] Step c): stacking two layers of UD cloth crosswise at a crossing angle of 90°, wherein each layer of UD cloth is made of blended yarn;
[0033] Step d): hot pressing and laminating, the hot pressing temperature is 100° C., the pressure is 5 MPa, and the laminating speed is 5 m / min;
[0034] Step e): Wrap the composite UD cloth with 120 μm thick aluminum foil 3, and fix the aluminum foil 3 to the four corners of the material by a sewing machine to form a bulletproof inner core.
[0035] Embodiment 2:
[0036] The polyethylene fiber 1 and the polyimide fiber 2 are blended in a ratio of 4:1. The specification of the polyethylene fiber 1 is 800D, and the specification of the polyimide fiber 2 is 5D. This embodiment has three layers of UD cloth.
[0037] The following are the manufacturing steps:
[0038] Step a): blending polyethylene fiber 1 and polyimide fiber 2 in a ratio of 4:1;
[0039] Step b): Spread the substrate film flat, use epoxy resin as an adhesive, evenly apply it on the substrate film, press the blended fiber to the adhesive surface, and dry it at 70° C. for 15 minutes;
[0040] Step c): stacking three layers of UD fabric crosswise at a cross angle of 90° to form a cross fiber structure;
[0041] Step d): hot pressing and laminating, the hot pressing temperature is 120° C., the pressure is 7 MPa, and the laminating speed is 8 m / min;
[0042] Step e): Wrap the composited UD cloth with 150 μm thick aluminum foil 3, and sew and fix the four corners of the aluminum foil 3.
[0043] Embodiment three:
[0044] The polyethylene fiber 1 and the polyimide fiber 2 are blended in a ratio of 8:1. The specification of the polyethylene fiber 1 is 400D, and the specification of the polyimide fiber 2 is 2D. This embodiment has four layers of UD cloth.
[0045] The following are the manufacturing steps:
[0046] Step a): blending polyethylene fiber 1 and polyimide fiber 2 in a ratio of 8:1;
[0047] Step b): After the substrate film is unfolded, epoxy resin is used as an adhesive, the adhesive is evenly coated on the substrate film, the blended fiber is pressed to the surface, and then dried at 50° C. for 30 minutes;
[0048] Step c): placing four layers of UD fabrics crosswise at a crossing angle of 90° to form a composite structure;
[0049] Step d): hot pressing and laminating, the hot pressing temperature is 90° C., the pressure is 3 MPa, and the laminating speed is 3 m / min;
[0050] Step e): Wrap the composited UD cloth with 200 μm thick aluminum foil 3, and fix the four corners of the aluminum foil 3 by sewing.
[0051] The polyethylene composite material prepared according to the above method is compared with the bulletproof inner core made of pure PE fiber. The shielding effectiveness is tested according to GB / T 22583-2009, the electromagnetic wave frequency range is 10MHz~3000MHz, and the afterburning time (the time the material continues to burn with flames after the ignition source is removed under the specified experimental conditions) is tested according to GB 8965.1-2009. PE polyethylene, PI is polyimide, the results are as follows:
[0052]
[0053] From the above results, it can be seen that as the amount of polyimide fiber 2 added increases, the shielding effectiveness of the inner core also increases accordingly, and the flame retardant effect also improves accordingly. On the basis of blending, a comparison is made between whether the aluminum foil 3 is coated or not, and it is found that adding aluminum foil 3 also has a beneficial effect on the shielding effectiveness.
[0054] Polyimide fiber 2 has good spinnability and can be made into textiles for various special occasions. Due to its high and low temperature resistance, flame retardancy, no melting droplets, self-extinguishing when away from fire, and excellent heat insulation, radiation resistance and wear resistance, polyimide fiber 2 thermal insulation protective clothing is comfortable to wear, has good skin adaptability, is permanently flame retardant, and has stable dimensions, good safety and long service life. Compared with other fibers, due to the low thermal conductivity of the material itself, it is also an excellent thermal insulation material. Aluminum foil uses the reflection and absorption characteristics of electromagnetic radiation to reflect most of the electromagnetic radiation and absorb part of the electromagnetic radiation and convert it into heat energy, thereby reducing the impact of electromagnetic radiation on the human body.
[0055] The present invention aims to blend polyimide fiber 2 with PE fiber to form a mixed fiber as the main material of a bulletproof vest. The application of polyimide fiber 2 in clothing fabrics fully demonstrates the flame retardancy, radiation resistance, high temperature resistance and wear resistance of polyimide fiber 2. It does not require the addition of flame retardants, has self-flame retardancy, self-extinguishes when away from fire, and does not produce toxic gases when burned. It can also prevent radiation in a complex battlefield environment, is safe and environmentally friendly, and is wrapped with aluminum foil 3 on the outside of the bulletproof vest to further improve the radiation protection performance.
[0056] Finally, it should be noted that the above embodiments are only used to illustrate the technical solution of the present invention rather than to limit it. Although the present invention has been described in detail with reference to the preferred embodiments, those skilled in the art should understand that the technical solution of the present invention can be modified or replaced by equivalents without departing from the purpose and scope of the technical solution of the present invention, which should be included in the scope of the claims of the present invention.
Claims
1. A radiation-proof and flame-retardant bulletproof vest, It is characterized in that The bulletproof vest is formed by cross-stacking at least two layers of UD cloth, the cross-angle is 90°, the UD cloth comprises polyethylene fiber and polyimide fiber, the UD cloth is composed of polyethylene and polyimide in a mass ratio of (1-8):1, the polyethylene fiber is 400-800D, the polyimide fiber is 1-7D, and the outer surface of the UD cloth is covered with aluminum foil, the thickness of the aluminum foil is 80μm-200μm.
2. The radiation-proof flame-retardant bulletproof vest according to claim 1, Features The UD cloth also includes a substrate film, and the polyethylene and polyimide are fixed on the substrate film by an adhesive.
3. The radiation-proof and flame-retardant bulletproof vest according to claim 2, It is characterized in that The adhesive is epoxy resin.
4. A method for manufacturing the radiation-proof flame-retardant bulletproof vest according to any one of claims 1 to 3, It is characterized in that The method comprises the following steps: a) blending polyethylene fiber and polyimide fiber in a ratio of (1-8):1; b) spreading a substrate film flatly, impregnating an adhesive and evenly spreading the film flatly, spreading the blended fiber, pressing the blended fiber onto the adhesive surface, and drying in an oven; c) placing UD cloths that are in contact with each other crosswise at a crossing angle of 90 degrees; d) performing hot pressing compounding on the product of c; and e) wrapping the product of d as a whole with aluminum foil, and fixing the four corners of the aluminum foil on the product by sewing.
5. The method for manufacturing a radiation-proof and flame-retardant bulletproof vest according to claim 1, It is characterized in that The drying temperature in step b) is 50° C.-80° C., and the drying time is 10-30 minutes.
6. The method for manufacturing a radiation-proof flame-retardant bulletproof vest according to claim 1, It is characterized in that In step c), the compounding temperature is 90-140° C., the compounding pressure is 1-10 MPa, and the compounding speed is 1-10 m / min.
Citation Information
Patent Citations
Multifunctional nuclear radiation protective garment
CN103778986A
Bulletproof composite material and preparation method thereof
CN114957989A
Fireproof flame-retardant wearable fabric and preparation method thereof
CN117507522A
High-flame-retardant glass fiber composite fabric
CN220564821U