Method for preparing different-surface-layer metal titanium / steel composite plate under atmospheric pressure
By rolling galvanized aluminum-magnesium steel plates and titanium plates directly under atmospheric pressure, zinc/steel/zinc/titanium four-layer composite plates were prepared, which solved the problem of interface reaction of titanium/steel composite plates at high temperatures, and achieved simple and low Cost preparation process, suitable for high corrosion environments.
Patent Information
- Application Number
- CN202411318551.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-20
- Publication Date
- 2024-12-06
AI Technical Summary
The existing titanium/steel composite panels have interface reactions at high temperatures to generate brittle phases, resulting in poor binding performance, and the existing preparation process is complex and costly, making it difficult to produce thin composite layers on a large scale.
Directly roll galvanized aluminum-magnesium steel plates and titanium plates under atmospheric pressure. Through the preparation, surface treatment, online heating and rolling process, a titanium steel composite plate with zinc/steel/zinc/titanium layer is prepared to avoid welding and High-temperature rolling, medium-temperature rolling and hydraulic cylinder thrust are used to achieve reversible rolling.
It realizes efficient preparation of titanium steel composite board, with steel support strength and corrosion-resistant anti-corrosion layer, simple process and low cost, suitable for corrosion environments, and the use of titanium is reduced, reducing production costs.
Smart Images

Figure HDA0005052927350000011 
Figure HDA0005052927350000012
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of composite plate preparation, and in particular relates to a method for preparing a composite plate with different surface layers of titanium / steel under atmospheric pressure. Background Art
[0002] Titanium / steel composite plate has both the corrosion resistance of titanium and the excellent weldability, formability and thermal conductivity of steel, and greatly saves the use of titanium. It has high economic value and good application prospects and is widely used in petrochemical, energy transmission, salt making equipment, medical equipment, aerospace, shipbuilding industry and marine engineering. Galvanized aluminum-magnesium steel plate is a new type of highly corrosion-resistant coated steel plate. Its excellent flat corrosion resistance and cut corrosion resistance are particularly important for downstream industries; it also has good friction resistance, alkali resistance, ammonia resistance, high surface hardness and excellent laser welding performance. Generally speaking, the composition of zinc-aluminum-magnesium coating is mainly zinc, which is composed of zinc and aluminum with a content of 1.5% to 11.0%, magnesium with a content of 1.5% to 3.0% and a trace amount of silicon; it is widely used in solar thermal, photovoltaic, animal husbandry, electrical cabinets, special steel for door industry, high corrosion-resistant color-coated plate for construction, home appliances, automobile structure and other fields.
[0003] For titanium / steel composite materials, due to the serious interface reaction between titanium and steel at high temperature, if titanium and steel are directly rolled and composited, the composite interface is prone to produce brittle phases such as Ti-Fe intermetallic compounds and TiC, which affects the bonding performance of titanium-steel composite plates. In order to inhibit the generation of interfacial brittle phases and block the combination of Ti and C or Ti and Fe, Al, Cu, V, Ni, Mo, Fe, etc. are usually added between titanium and steel as an intermediate layer, or an anti-oxidation coating is used to enhance the bonding strength of the titanium-steel composite interface. The above-mentioned intermediate layers are all made of pure metals, and there are few reports on alloys as intermediate layers of titanium / steel composite plates. At present, scientific research work is mainly focused on titanium-steel composite plates with two layered structures of titanium / steel and titanium / steel / titanium; but there are few reports on titanium / steel / corrosion-resistant metal layer or titanium / steel / decorative metal layer composite plates. This type of titanium-steel composite plate with different surface metals can not only provide the functions of other metals, but also further reduce the use of titanium and save costs.
[0004] At present, there are few studies on the TiO2-ZnO system. Steinike's research shows that during the mixing of ZnO and TiO2 powders, compounds Zn2TiO4, ZnTiO3 and Zn2Ti3O8 can be formed through solid-state reactions. The main preparation methods of titanium steel composite plates are explosion composite method, explosion-rolling composite method and vacuum rolling composite method. The explosion composite method has many disadvantages such as low interface bonding efficiency, environmental pollution and small product size, and is not easy to mass produce. The vacuum rolling composite method is a production process that achieves good metallurgical bonding between the substrate and the cladding through vacuum welding, heating and rolling, which has attracted much attention; but its process flow is long and the rolling cost is high; if the heating is uneven during the rolling process or the hot rolling temperature is not enough, the yield rate will be affected, and it is even difficult to prepare titanium steel composite plates with thin composite layers. Summary of the invention
[0005] In order to overcome the above-mentioned defects of the prior art, the present invention directly rolls and compounds titanium plates and galvanized products (galvanized plates for automobiles, steel for photovoltaic brackets) under atmospheric pressure to prepare a four-layer titanium-steel composite plate of zinc / steel / zinc / titanium. It has both the supporting strength of steel and a corrosion-resistant anti-corrosion layer, and can be used in working environments with large corrosion concentration gradients.
[0006] In order to achieve the above-mentioned purpose of the invention, the present invention provides a method for preparing a titanium / steel composite plate with different surface layers under atmospheric pressure, including plate preparation and surface treatment, clamping and installation, online heating, rolling and other processes, and the method specifically includes the following steps:
[0007] ① Plate preparation and surface treatment: The galvanized aluminum-magnesium steel plate and the titanium plate are processed into the same size, the titanium plate is polished, and then treated with an acid solution for 10s to 20s; then the galvanized aluminum-magnesium steel plate and the titanium plate are cleaned with ethanol respectively, and blown dry for use; this can remove oil stains or other surface contaminants on the titanium strip.
[0008] The titanium plate is polished to a surface roughness Ra of 3.2 μm. The acid solution is composed of hydrofluoric acid with a concentration of 40.0%, nitric acid with a concentration of 65.0% to 68.0%, and water, with a volume ratio of hydrofluoric acid: nitric acid: water = 2:5:93.
[0009] ② Align the edges of the galvanized aluminum-magnesium steel plate and the titanium plate and stack them, clamp them on a heated hydraulic fixture, and apply a certain tension until the steel plate and the titanium plate are straightened and tightly together; the tension is 10kN to 20kN.
[0010] ③ The galvanized aluminum-magnesium steel plate and the titanium plate are heated online simultaneously, and the heating temperature is controlled to be 30° C. to 50° C. lower than the melting point of the galvanized layer;
[0011] ④ Start the rollers for rolling, and the thrust hydraulic cylinder moves left and right repeatedly to achieve reversible rolling; the reduction amount for each pass is 16% to 20%, and the total reduction amount is ≥50%; then air-cool to room temperature to obtain a different surface layer of metal titanium / steel composite plate.
[0012] Compared with the prior art, the invention has the following beneficial effects: At present, titanium / steel composite plates are prepared by adding other pure metals between titanium and steel and rolling them at high temperature in vacuum, and welding is required before rolling. The technical solution of the present invention is to prepare the titanium / steel composite plates at medium temperature by direct rolling under atmospheric pressure, without welding or vacuuming, with lower heating temperature, simpler process and lower cost.
[0013] The present invention directly rolls and compounds titanium plates and galvanized products (galvanized plates for automobiles and steel for photovoltaic brackets) under atmospheric pressure to prepare a zinc / steel / zinc / titanium four-layer titanium-steel composite plate, which has both the supporting strength of steel and a corrosion-resistant anticorrosive layer, and can be widely used in working environments with large corrosion concentration gradients. The middle layer of the titanium-steel composite plate is a zinc-aluminum-magnesium alloy, and the heating temperature is reduced to prepare a composite plate of galvanized layer / steel / galvanized layer / titanium by medium-temperature rolling; the process is simple, the manufacturing cost is low, and it can be widely promoted and applied. BRIEF DESCRIPTION OF THE DRAWINGS
[0014] Figure 1 The present invention is a schematic diagram of the rolling process and device of the galvanized aluminum-magnesium steel plate / titanium composite plate; in the figure: 1-galvanized aluminum-magnesium steel plate; 2-titanium plate; 3-roller; 4-temperature measuring device; 5-heating hydraulic clamp; 6-thrust hydraulic cylinder.
[0015] Figure 2 Schematic diagram of the microstructure of the composite interface of the galvanized aluminum-magnesium steel plate / titanium composite plate prepared in the embodiment; in the figure, section A is the galvanized layer; section B is the steel layer; section C is the zinc layer; and section D is the titanium layer. DETAILED DESCRIPTION
[0016] The present invention is further described below in conjunction with specific examples, but the present invention is not limited in any way. To avoid redundant description, the raw materials in the following examples are all commercially available products unless otherwise specified, and the methods used are all conventional methods unless otherwise specified.
[0017] A method for preparing a titanium / steel composite plate with different surface layers under atmospheric pressure comprises the following steps:
[0018] ① Plate preparation and surface treatment: The galvanized aluminum-magnesium steel plate and the titanium plate are processed into the same size, the titanium plate is polished, and then treated with an acid solution for 10s to 20s; then the galvanized aluminum-magnesium steel plate and the titanium plate are cleaned with ethanol, respectively, and blown dry for later use.
[0019] ② Align the edges of the steel plate and the titanium plate and stack them, clamp them on a heated hydraulic fixture, and apply tension to straighten and tighten the steel plate and the titanium plate.
[0020] ③ The galvanized aluminum-magnesium steel plate and the titanium plate are heated online simultaneously, and the heating temperature is controlled to be 30° C. to 50° C. lower than the melting point of the galvanized layer.
[0021] ④ Start the rollers for rolling, and the thrust hydraulic cylinder moves left and right repeatedly to achieve reversible rolling; the reduction amount for each pass is 16% to 20%, and the total reduction amount is ≥50%; then air-cool to room temperature to obtain a different surface layer of metal titanium / steel composite plate.
[0022] The matters not described in the following embodiments are the same as the description of the above specific implementation methods.
[0023] Example
[0024] A method for preparing a titanium / steel composite plate with different surface layers under atmospheric pressure, the specific process flow (refer to Figure 1 The flowchart shown is:
[0025] A certain brand of galvanized aluminum-magnesium coated steel plate 1 is selected. The chemical composition of the steel base is: C content is 0.19%, Si content is 0.26%, Mn content is 1.1%, P content is 0.019%, S content is 0.04%, Als content is 0.054%, Ti content is 0.050%; mechanical properties: yield strength ReH is 480MPa, elongation after fracture is 15%; the weight of the galvanized layer is 270g / m 2 The coating composition is 10% Al, 2.6% Mg, 0.25% Si, and the rest is zinc. The titanium plate 2 is selected as model TA2.
[0026] ① Process a galvanized aluminum-magnesium steel plate 1 with a size of 600×80×0.6mm and a titanium plate 2 with a size of 600×80×0.6mm; clean the steel plate 1 with alcohol; polish the titanium plate 2 appropriately (polished to a surface roughness Ra of 3.2μm), then clean it with 2ml HF+5ml HNO3+93ml H2O solution for 15s, clean it with ethanol, blow dry it and set it aside.
[0027] ② Align the edges of the steel plate 1 and the titanium plate 2 and stack them. Fix and tighten the two ends with the online heating hydraulic clamp 5, adjust the distance of the thrust hydraulic cylinder 6, and apply a tension of 10kN to the left and right ends respectively;
[0028] ③ Simultaneously, the steel plate 1 and the titanium plate 2 are subjected to online resistance heating, and the heating temperature is measured to 400° C. by a contact temperature measuring device 4;
[0029] ④ Rolling 4 times, with a reduction of 16% to 20% in each time and a total reduction of 50%; then cooling to room temperature to obtain a titanium-steel composite plate with a different surface layer and a thickness of 0.6 mm.
[0030] After the metallographic sample of the composite plate obtained in the embodiment was prepared, it was detected on a scanning electron microscope. Figure 2 As shown, the titanium / steel bond is good, the bonding surface is continuous and smooth, and there are no defects such as pores, inclusions, microcracks and unwelded parts.
[0031] For any technician familiar with the art, without departing from the scope of the technical solution of the present invention, the technical content disclosed above can be used to make many possible changes and modifications to the technical solution of the present invention, or modified into equivalent embodiments with equivalent changes. Therefore, any simple modification, equivalent change and modification made to the above embodiments according to the technical essence of the present invention without departing from the content of the technical solution of the present invention should still fall within the scope of protection of the technical solution of the present invention.
Claims
1. A method for preparing a titanium / steel composite plate with different surface layers under atmospheric pressure, characterized in that: The method comprises the following steps: ① Plate preparation and surface treatment: Process the galvanized aluminum-magnesium steel plate and the titanium plate into the same size, grind the titanium plate, and treat it with an acid solution for 10s to 20s; then wash the galvanized aluminum-magnesium steel plate and the titanium plate with ethanol, blow dry and set aside; ② Align the edges of the steel plate and the titanium plate and stack them, clamp them on a heated hydraulic fixture, and apply tension to straighten and tighten the steel plate and the titanium plate; ③ The galvanized aluminum-magnesium steel plate and the titanium plate are heated online simultaneously, and the heating temperature is controlled to be 30° C. to 50° C. lower than the melting point of the galvanized layer; ④ Start the rollers for rolling, and the thrust hydraulic cylinder moves left and right repeatedly to achieve reversible rolling; the reduction amount for each pass is 16% to 20%, and the total reduction amount is ≥50%; then air-cool to room temperature to obtain a different surface layer of metal titanium / steel composite plate.
2. The method according to claim 1, characterized in that Step ① The titanium plate is polished to a surface roughness Ra of 3.2 μm.
3. The method according to claim 2, characterized in that Step ① The acid solution is composed of hydrofluoric acid with a concentration of 40.0%, nitric acid with a concentration of 65.0% to 68.0%, and water, with a volume ratio of hydrofluoric acid: nitric acid: water = 2:5:
93.
4. The method according to claim 3, characterized in that The tension in step ② is 10 to 20 kN.
Citation Information
Patent Citations
Preparation method of hot dip galvanized steel tube / titanium bimetal composite tube
CN104043673A
Manufacturing method for rolling titanium-steel composite plate
CN104138903A
Preparation method for multilayer dissimilar metal composite ultra-thin strip
CN105170652A
Method for preparing titanium / steel composite plate through hot rolling in atmospheric environment
CN115156330A
Titanium bimetallic clad plate
CN201297010Y
Cited By
Metal composite plate laser manufacturing equipment
CN119870981A
High-thermal-conductivity titanium steel cold-rolled composite board and preparation method thereof
CN120838875A
High-thermal-conductivity titanium steel cold-rolled clad plate and preparation method thereof
CN120838875B