Non-ionic surfactant as well as preparation method and application thereof
Through the non-ionic surfactant with an amphiphilic polyoxyethylene polyoxypropylene ether structure, the problem of insufficient emulsification performance in the prior art is solved, and the excellent emulsification effect on paraffin or dimethyl silicone oil is achieved, which significantly improves emulsification ability.
Patent Information
- Application Number
- CN202411186066.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-27
- Publication Date
- 2024-12-06
AI Technical Summary
The emulsification performance of existing non-ionic surfactants is poor, making it difficult to effectively emulsify paraffin or dimethyl silicone oil.
Nonionic surfactant with amphiphilic polyoxyethylene polyoxypropylene ether structure was prepared by multi-step reaction of C8-C18 fatty alcohol, catalyst, epoxy propylene alcohol, ethylene oxide and propylene oxide, combined with cooling , neutralization and degassing treatments to form a product with excellent emulsification properties.
The emulsification ability of paraffin or dimethyl silicone oil is significantly improved, forming a stable emulsification layer, and enhancing the adsorption and dispersion properties of surfactants at the oil-water interface.
Smart Images

Figure CN119080591A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of surfactants, and in particular relates to a nonionic surfactant and a preparation method and application thereof. Background Art
[0002] Surfactants are widely used in various fields as a kind of "industrial MSG". According to their ionicity, they can be divided into anionic surfactants, nonionic surfactants, cationic surfactants and amphoteric surfactants. Nonionic surfactants are increasingly used in various fields due to their excellent degreasing, wetting, emulsification and dispersion properties. The hydrophilic and lipophilic groups determine the application performance of nonionic surfactants.
[0003] In the prior art, non-ionic surfactants still have the problem of poor emulsification performance. Therefore, developing a non-ionic surfactant with excellent emulsification performance is a technical problem that needs to be solved urgently. Summary of the invention
[0004] The main purpose of the present invention is to provide a nonionic surfactant, which has excellent emulsifying properties.
[0005] The present invention also provides a method for preparing a nonionic surfactant, which can prepare the nonionic surfactant with simple process and low cost.
[0006] The present invention also provides a functional composition. Since the functional composition includes the nonionic surfactant, the functional composition has excellent emulsifying properties.
[0007] The present invention also provides a method for emulsifying paraffin or dimethyl silicone oil. Since the method uses the above-mentioned non-ionic surfactant or functional composition to emulsify paraffin or dimethyl silicone oil, the emulsification method can improve the emulsification ability of paraffin or dimethyl silicone oil.
[0008] In a first aspect, the present invention provides a nonionic surfactant having a structure shown in Formula 1:
[0009]
[0010] Wherein, R represents at least one of C8-C18 hydrocarbon groups; a+b is 3-12, and m+n is 1-5.
[0011] As above nonionic surfactant, said R is C 18 H 35 , having the structure shown in Formula 2:
[0012]
[0013] The nonionic surfactant as described above, wherein a+b is 6-12, and m+n is 2-4.
[0014] The nonionic surfactant as described above is prepared by a method comprising the following process:
[0015] To a system including C8-C18 fatty alcohol and a catalyst, propylene oxide, ethylene oxide and propylene oxide are sequentially added to carry out a reaction, and the reaction product is subjected to post-treatment including cooling treatment, neutralization treatment and degassing treatment to obtain the nonionic surfactant.
[0016] In a second aspect, the present invention provides a method for preparing the nonionic surfactant as described above, comprising the following steps:
[0017] 1) reacting a first system including a C8-C18 fatty alcohol, a catalyst, and glycidol to obtain a first intermediate;
[0018] 2) performing a secondary reaction on a second system including the first intermediate and ethylene oxide to obtain a second intermediate;
[0019] 3) reacting the third system including the second intermediate and propylene oxide three times to obtain a third intermediate;
[0020] 4) performing post-treatment including cooling treatment, neutralization treatment and degassing treatment on the third intermediate to obtain the nonionic surfactant.
[0021] In the preparation method as described above, the mass of the catalyst is 0.02-1% of the total mass of the fatty alcohol, propylene oxide, ethylene oxide and propylene oxide.
[0022] The preparation method as described above, wherein the molar ratio of the fatty alcohol to the glycidol is 1:1-1.2;
[0023] The temperature of the primary reaction is 120-160° C. and the time is 0.5-4 h.
[0024] The preparation method as described above, wherein the molar ratio of the fatty alcohol to ethylene oxide is 1:3-12;
[0025] The temperature of the secondary reaction is 120-160° C. and the time is 1-4 hours.
[0026] The preparation method as described above, wherein the molar ratio of the fatty alcohol to propylene oxide is 1:1-5;
[0027] The temperature of the three reactions is 110-160° C. and the time is 0.5-4 h.
[0028] In a third aspect, the present invention provides a functional composition, comprising the nonionic surfactant as described above, and the nonionic surfactant obtained by the preparation method as described above.
[0029] In a fourth aspect, the present invention provides a method for emulsifying paraffin or dimethicone oil, using the nonionic surfactant as described above, the nonionic surfactant obtained by the preparation method as described above, and the functional composition as described above to emulsify paraffin or dimethicone oil.
[0030] The nonionic surfactant provided by the present invention is a double hydrophilic polyoxyethylene polyoxypropylene ether, so that the nonionic surfactant has excellent emulsifying properties. DETAILED DESCRIPTION
[0031] In order to make the purpose, technical solutions and advantages of the present invention clearer, the technical solutions in the embodiments of the present invention will be clearly and completely described below in combination with the embodiments of the present invention. Obviously, the described embodiments are part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0032] In a first aspect, the present invention provides a nonionic surfactant having a structure shown in Formula 1:
[0033]
[0034] Wherein, R represents at least one of C8-C18 hydrocarbon groups; a+b is 3-12, and m+n is 1-5.
[0035] The nonionic surfactant provided by the present invention has the structure shown in the above formula 1, that is, the structure of a double hydrophilic polyoxyethylene polyoxypropylene ether, and the substituent represented by R, a+b, and m+n are limited. This structural characteristic enables the nonionic surfactant to have excellent emulsifying properties. It is speculated that this may be because the presence of the double hydrophilic group makes the adsorption of the nonionic surfactant molecule on the interface between the water phase and the oil phase more stable, which can better reduce the tension of the liquid / liquid interface and make the oil agent less likely to agglomerate; the alternating arrangement of the polyoxyethylene and polyoxypropylene segments in the molecule can increase the hydrophilic and lipophilic balance of the molecule, and this structure is conducive to the orderly arrangement of the surfactant molecules on the oil-water interface to form a stable emulsified layer.
[0036] The nonionic surfactant provided by the present invention is a double hydrophilic polyoxyethylene polyoxypropylene ether, so that the nonionic surfactant has excellent emulsifying properties.
[0037] In some embodiments of the present invention, R is C 18 H 35 , having the structure shown in Formula 2:
[0038]
[0039] In the present invention, when R represents C 18 H 35 , and having the structure shown in the above formula 2, can further improve the emulsification performance of the non-ionic surfactant.
[0040] In some embodiments of the present invention, a+b is 6-12, and m+n is 2-4.
[0041] In the present invention, when a+b is 6-12 and m+n is 2-4, as a preferred embodiment, the emulsifying performance of the nonionic surfactant can be further improved.
[0042] In some embodiments of the present invention, the nonionic surfactant is prepared by a method comprising the following process:
[0043] To a system including C8-C18 fatty alcohol and a catalyst, propylene oxide, ethylene oxide and propylene oxide are sequentially added to carry out a reaction, and the reaction product is subjected to post-treatment including cooling treatment, neutralization treatment and degassing treatment to obtain the nonionic surfactant.
[0044] The raw materials for preparing the nonionic surfactant in the present invention include C8-C18 fatty alcohol, catalyst, glycidol, ethylene oxide and propylene oxide. Specifically, the C8-C18 fatty alcohol and the catalyst can be mixed, nitrogen replacement is carried out, dehydration and heating are carried out, glycidol is slowly added, ethylene oxide is slowly introduced after the reaction is completed, propylene oxide is added after the reaction is completed, cooling, neutralization and degassing are carried out after the reaction to obtain the nonionic surfactant.
[0045] In the present invention, glycidol is used to modify C8-C18 fatty alcohol to form dihydroxy fatty alcohol ether, which is then reacted with ethylene oxide and propylene oxide to obtain dihydrophilic polyoxyethylene polyoxypropylene ether, so that the nonionic surfactant has excellent emulsifying properties.
[0046] In a second aspect, the present invention provides a method for preparing the nonionic surfactant as described above, comprising the following steps:
[0047] 1) reacting a first system including a C8-C18 fatty alcohol, a catalyst, and glycidol to obtain a first intermediate;
[0048] 2) performing a secondary reaction on a second system including the first intermediate and ethylene oxide to obtain a second intermediate;
[0049] 3) reacting the third system including the second intermediate and propylene oxide three times to obtain a third intermediate;
[0050] 4) performing post-treatment including cooling treatment, neutralization treatment and degassing treatment on the third intermediate to obtain the nonionic surfactant.
[0051] The method for preparing the nonionic surfactant of the present invention comprises continuously adding raw materials during the reaction process to finally prepare the nonionic surfactant of the first aspect of the present invention.
[0052] Specifically, in step 1), the catalyst can be at least one of potassium hydroxide, sodium methoxide, phosphazene catalyst, and sodium hydroxide, preferably sodium methoxide and phosphazene catalyst. The C8-C18 fatty alcohol and the catalyst can be mixed, nitrogen replacement can be performed, dehydration and temperature can be increased, and glycidol can be slowly added to perform a reaction to obtain the first intermediate.
[0053] In step 2), ethylene oxide is slowly introduced into the first intermediate obtained in step 1) to carry out a secondary reaction to obtain a second intermediate.
[0054] In step 3), propylene oxide is slowly introduced into the second intermediate obtained in step 2) to carry out three reactions to obtain a third intermediate.
[0055] In step 4), the third intermediate obtained in step 3) is sequentially subjected to cooling, neutralization, and degassing treatment to obtain a hydrophilic polyoxyethylene polyoxypropylene ether. The cooling temperature may be 80-90° C., and the neutralizer used in the neutralization treatment may be at least one of lactic acid, phosphoric acid, and acetic acid, preferably lactic acid and acetic acid, which are used to neutralize the alkaline catalyst added in step 1) and reduce the pH value of the system.
[0056] The invention provides a method for preparing a nonionic surfactant, which comprises modifying C8-C18 fatty alcohols with propylene oxide to form dihydroxy fatty alcohol ethers, and then reacting the modified fatty alcohols with ethylene oxide and propylene oxide to obtain dihydrophilic polyoxyethylene polyoxypropylene ethers, so that the nonionic surfactant has excellent emulsifying properties.
[0057] In some embodiments of the present invention, the mass of the catalyst is 0.02-1% of the total mass of the fatty alcohol, propylene oxide, ethylene oxide and propylene oxide.
[0058] The mass of the catalyst in the present invention is 0.02-1%, preferably 0.05-0.3%, of the total mass of the fatty alcohol, propylene oxide, ethylene oxide, and propylene oxide. The mass of the catalyst is within a suitable range so that the catalyst can fully exert its catalytic effect, accelerate the reaction rate, reduce the occurrence of side reactions, and promote the formation of the target product.
[0059] In some embodiments of the present invention, the molar ratio of the fatty alcohol to glycidol is 1:1-1.2;
[0060] The temperature of the primary reaction is 120-160° C. and the time is 0.5-4 h.
[0061] In the present invention, the molar ratio of fatty alcohol to glycidol is 1:1-1.2, preferably 1:1-1.1, so that the two reactants can fully contact and react, which can improve the reaction efficiency, and appropriately increase the amount of glycidol to ensure that the fatty alcohol is completely reacted.
[0062] The temperature of the primary reaction is 120-160° C., preferably 120-140° C. A suitable reaction temperature is beneficial to improving the selectivity of the reaction, promoting the formation of the target product, and reducing the occurrence of side reactions.
[0063] The time of one reaction is 0.5-4h, preferably 1-3h, which can make the reaction fully proceed and improve the production efficiency.
[0064] In some embodiments of the present invention, the molar ratio of the fatty alcohol to ethylene oxide is 1:3-12;
[0065] The temperature of the secondary reaction is 120-160° C. and the time is 1-4 hours.
[0066] In the present invention, the molar ratio of fatty alcohol to ethylene oxide is 1:3-12, preferably 1:6-12, so that a proper amount of ethylene oxide molecules can react with the first intermediate, and a proper amount of ethylene oxide groups can be introduced into the first intermediate.
[0067] The temperature of the secondary reaction is 120-160° C., preferably 130-150° C., which can make the reaction rate moderate, facilitate the ring-opening addition reaction of the first intermediate and ethylene oxide, improve the selectivity of the reaction, promote the formation of the target product, and reduce the occurrence of side reactions.
[0068] The secondary reaction time is 1-4 hours, preferably 2-4 hours, which can achieve a higher conversion rate, ensure that the hydroxyl group on the first intermediate can fully react with ethylene oxide, and improve production efficiency.
[0069] In some embodiments of the present invention, the molar ratio of the fatty alcohol to propylene oxide is 1:1-5;
[0070] The temperature of the three reactions is 110-160° C. and the time is 0.5-4 h.
[0071] In the present invention, the molar ratio of fatty alcohol to propylene oxide is 1:1-5, preferably 1:2-4, so that a proper amount of propylene oxide molecules can react with the second intermediate, and a proper amount of propylene oxide groups can be introduced into the second intermediate.
[0072] The temperature of the tertiary reaction is 110-160° C., preferably 110-140° C., which can make the reaction rate moderate, is conducive to the ring-opening addition reaction of the second intermediate and propylene oxide, improves the selectivity of the reaction, promotes the formation of the target product, and reduces the occurrence of side reactions.
[0073] The time of the three reactions is 0.5-4 hours, preferably 1.5-3 hours, which can achieve a higher conversion rate, ensure that the hydroxyl group on the second intermediate can fully react with propylene oxide, and improve production efficiency.
[0074] In a third aspect, the present invention provides a functional composition, comprising the nonionic surfactant as described above, and the nonionic surfactant obtained by the preparation method as described above.
[0075] The functional composition provided by the present invention comprises the above nonionic surfactant, or the nonionic surfactant prepared by the above preparation method, and therefore, the functional composition has excellent emulsifying properties.
[0076] In a fourth aspect, the present invention provides a method for emulsifying paraffin or dimethicone oil, using the nonionic surfactant as described above, the nonionic surfactant obtained by the preparation method as described above, and the functional composition as described above to emulsify paraffin or dimethicone oil.
[0077] In the paraffin or dimethicone oil emulsification method provided by the present invention, the paraffin or dimethicone oil is emulsified using the nonionic surfactant or functional composition. Therefore, the emulsification method can improve the emulsification ability of paraffin or dimethicone oil.
[0078] The technical solution of the present invention is further described below in conjunction with specific embodiments.
[0079] Example 1
[0080] The preparation method of the nonionic surfactant of this embodiment comprises the following steps:
[0081] Add 536g of oleyl alcohol (M=268) and 4.0g of sodium hydroxide to the reactor, heat to 120°C, vacuum dehydrate for 1h, and control the moisture content in the reactor to be below 50ppm; heat to 160°C, slowly add 148g of propylene oxide (M=74) to the reactor, control the pressure to 0.1-0.4MPa, and carry out a primary reaction for 1h; maintain the reaction temperature at 160°C, slowly add 528g of ethylene oxide (M=44), control the pressure to 0.1-0.4MPa, and carry out a secondary reaction for 2h; continue to maintain the reaction temperature at 160°C, slowly add 116g of propylene oxide (M=58), control the pressure to 0.1-0.4MPa, and carry out a tertiary reaction for 1.0h. After the reaction is completed, cool to 85°C, add lactic acid to neutralize to pH=6.5, vacuum degas, and obtain product 1. The mass of the catalyst is 0.3% of the total mass of oleyl alcohol, propylene oxide, ethylene oxide, and propylene oxide. The molar ratio of oleyl alcohol to propylene oxide is 1:1, the molar ratio of oleyl alcohol to ethylene oxide is 1:6, and the molar ratio of oleyl alcohol to propylene oxide is 1:1. The hydroxyl value of the obtained product 1 is 170.3 mgKOH / g, and the calculated molecular weight is about 658.9 g / mol. Through carbon spectrum ( 13 C-NMR) characterization showed carbon atom absorption peaks after ring opening of propylene oxide at δ (64.3, 71.1, 79.3).
[0082] The structural formula of product 1 is:
[0083]
[0084] Where R is C 18 H 35 , a+b is 6, m+n is 1.
[0085] Example 2
[0086] The preparation method of the nonionic surfactant of this embodiment comprises the following steps:
[0087] Add 268g of oleyl alcohol (M=268) and 2.1g of sodium methoxide to the reactor, heat to 120°C, vacuum dehydrate for 1h, and control the moisture content in the reactor to be below 50ppm; heat to 140°C, slowly add 81g of propylene oxide (M=74) to the reactor, control the pressure to 0.1-0.4MPa, and carry out a primary reaction for 0.5h; maintain the reaction temperature at 140°C, slowly add 528g of ethylene oxide (M=44), control the pressure to 0.1-0.4MPa, and carry out a secondary reaction for 4h; maintain the reaction temperature at 140°C, slowly add 174g of propylene oxide (M=58), control the pressure to 0.1-0.4MPa, and carry out a tertiary reaction for 2h. After the reaction is completed, cool to 85°C, add lactic acid to neutralize to pH=6.5, vacuum degas, and obtain product 2. The mass of the catalyst is 0.2% of the total mass of oleyl alcohol, propylene oxide, ethylene oxide, and propylene oxide. The molar ratio of oleyl alcohol to propylene oxide is 1:1.09, the molar ratio of oleyl alcohol to ethylene oxide is 1:12, and the molar ratio of oleyl alcohol to propylene oxide is 1:3. The 2-hydroxyl value of the obtained product is 107.9 mgKOH / g, and the calculated molecular weight is about 1039.8 g / mol. Through carbon spectrum ( 13 C-NMR) characterization showed carbon atom absorption peaks after ring opening of propylene oxide at δ (64.3, 71.1, 79.3).
[0088] The structural formula of product 2 is:
[0089]
[0090] Where R is C 18 H 35 , a+b is 12, m+n is 3.
[0091] Example 3
[0092] The preparation method of the nonionic surfactant of this embodiment comprises the following steps:
[0093] Add 402g of oleyl alcohol (M=268) and 3.1g of potassium hydroxide to the reactor, heat to 120°C, vacuum dehydrate for 1h, and control the moisture content in the reactor to be below 50ppm; heat to 140°C, slowly add 116g of propylene oxide (M=74) to the reactor, control the pressure to 0.1-0.4MPa, and carry out a primary reaction for 2h; cool to 130°C, slowly add 396g of ethylene oxide (M=44), control the pressure to 0.1-0.4MPa, and carry out a secondary reaction for 3h; heat to 140°C, slowly add 348g of propylene oxide (M=58), control the pressure to 0.1-0.4MPa, and carry out a tertiary reaction for 4h. After the reaction is completed, cool to 80°C, add lactic acid to neutralize to pH=6, vacuum degas, and obtain product 3. The mass of the catalyst is 0.25% of the total mass of oleyl alcohol, propylene oxide, ethylene oxide, and propylene oxide. The molar ratio of oleyl alcohol to propylene oxide is 1:1.05, the molar ratio of oleyl alcohol to ethylene oxide is 1:6, and the molar ratio of oleyl alcohol to propylene oxide is 1:4. The 3-hydroxyl value of the obtained product is 134.6 mgKOH / g, and the calculated molecular weight is about 833.6 g / mol. Through carbon spectrum ( 13 C-NMR) characterization showed carbon atom absorption peaks after ring opening of propylene oxide at δ (64.3, 71.1, 79.3).
[0094] The structural formula of product 3 is:
[0095]
[0096] Where R is C 18 H 35, a+b is 6, m+n is 4.
[0097] Example 4
[0098] The preparation method of the nonionic surfactant of this embodiment comprises the following steps:
[0099] Add 321g of oleyl alcohol (M=268) and 1g of phosphazene catalyst to the reactor, heat to 120°C, vacuum dehydrate for 1h, and control the moisture content in the reactor to be below 50ppm; heat to 150°C, slowly add 93g of propylene oxide (M=74) to the reactor, control the pressure to 0.1-0.4MPa, and carry out a primary reaction for 3h; cool to 130°C, slowly add 528g of ethylene oxide (M=44), control the pressure to 0.1-0.4MPa, and carry out a secondary reaction for 4h; heat to 135°C, slowly add 208g of propylene oxide (M=58), control the pressure to 0.1-0.4MPa, and carry out a tertiary reaction for 3h. After the reaction is completed, cool to 90°C, add lactic acid to neutralize to pH=7, vacuum degas, and obtain product 4. The mass of the catalyst is 0.09% of the total mass of oleyl alcohol, propylene oxide, ethylene oxide, and propylene oxide. The molar ratio of oleyl alcohol to propylene oxide is 1:1.05, the molar ratio of oleyl alcohol to ethylene oxide is 1:10, and the molar ratio of oleyl alcohol to propylene oxide is 1:3. The 4-hydroxyl value of the obtained product is 118.7 mgKOH / g, and the calculated molecular weight is about 945.2 g / mol. Through carbon spectrum ( 13 C-NMR) characterization showed carbon atom absorption peaks after ring opening of propylene oxide at δ (64.3, 71.1, 79.3).
[0100] The structural formula of product 4 is:
[0101]
[0102] Where R is C 18 H 35 , a+b is 10, m+n is 3.
[0103] Example 5
[0104] The preparation method of the nonionic surfactant of this embodiment comprises the following steps:
[0105] Add 482g of oleyl alcohol (M=268) and 0.88g of phosphazene catalyst to the reactor, heat to 120°C, vacuum dehydrate for 1.5h, and control the moisture content in the reactor to be below 50ppm; heat to 160°C, slowly add 159g of propylene oxide (M=74) to the reactor, control the pressure to 0.1-0.4MPa, and carry out a primary reaction for 4h; maintain the temperature at 160°C, slowly add 712g of ethylene oxide (M=44), control the pressure to 0.1-0.4MPa, and carry out a secondary reaction for 2h; cool to 110°C, slowly add 418g of propylene oxide (M=58), control the pressure to 0.1-0.4MPa, and carry out a tertiary reaction for 4h. After the reaction is completed, cool to 85°C, add acetic acid to neutralize to pH=6.5, vacuum degas, and obtain product 5. The mass of the catalyst is 0.05% of the total mass of oleyl alcohol, propylene oxide, ethylene oxide, and propylene oxide. The molar ratio of oleyl alcohol to propylene oxide is 1:1.19, the molar ratio of oleyl alcohol to ethylene oxide is 1:9, and the molar ratio of oleyl alcohol to propylene oxide is 1:4. The 5-hydroxyl value of the obtained product is 116.4 mgKOH / g, and the calculated molecular weight is about 963.9 g / mol. Through carbon spectrum ( 13 C-NMR) characterization showed carbon atom absorption peaks after ring opening of propylene oxide at δ (64.3, 71.1, 79.3).
[0106] The structural formula of product 5 is:
[0107]
[0108] Where R is C 18 H 35 , a+b is 9, m+n is 4.
[0109] Example 6
[0110] The preparation method of the nonionic surfactant of this embodiment comprises the following steps:
[0111] Add 268g of oleyl alcohol (M=268) and 2.1g of potassium hydroxide to the reactor, heat to 120°C, vacuum dehydrate for 1h, and control the moisture content in the reactor to be below 50ppm; heat to 135°C, slowly add 77g of propylene oxide (M=74) to the reactor, control the pressure to 0.1-0.4MPa, and carry out a primary reaction for 2h; heat to 145°C, slowly add 132g of ethylene oxide (M=44), control the pressure to 0.1-0.4MPa, and carry out a secondary reaction for 1h; heat to 160°C, slowly add 232g of propylene oxide (M=58), control the pressure to 0.1-0.4MPa, and carry out a tertiary reaction for 3h. After the reaction is completed, cool to 80°C, add acetic acid to neutralize to pH=6, vacuum degas, and obtain product 6. The mass of the catalyst is 0.3% of the total mass of oleyl alcohol, propylene oxide, ethylene oxide, and propylene oxide. The molar ratio of oleyl alcohol to propylene oxide is 1:1.04, the molar ratio of oleyl alcohol to ethylene oxide is 1:3, and the molar ratio of oleyl alcohol to propylene oxide is 1:4. The 6-hydroxyl value of the obtained product is 159.5 mgKOH / g, and the calculated molecular weight is about 703.4 g / mol. Through carbon spectrum ( 13 C-NMR) characterization showed carbon atom absorption peaks after ring opening of propylene oxide at δ (64.3, 71.1, 79.3).
[0112] The structural formula of product 6 is:
[0113]
[0114] Where R is C 18 H 35 , a+b is 3, m+n is 4.
[0115] Example 7
[0116] The preparation method of the nonionic surfactant of Example 7 is basically the same as that of Example 4, except that the amount of the phosphazene catalyst added is changed to g, so that the mass of the catalyst is 0.02% of the total mass of oleyl alcohol, propylene oxide, ethylene oxide, and propylene oxide, and finally the product 7 is prepared. The hydroxyl value of the obtained product 7 is 119.1 mgKOH / g, and the calculated molecular weight is about 942.1 g / mol. Through carbon spectrum ( 13 C-NMR) characterization showed carbon atom absorption peaks after ring opening of propylene oxide at δ (64.3, 71.1, 79.3).
[0117] The structural formula of product 7 is:
[0118]
[0119] Where R is C 18 H 35 , a+b is 10, m+n is 3.
[0120] Example 8
[0121] The preparation method of the nonionic surfactant of Example 8 is basically the same as that of Example 1, except that the amount of sodium hydroxide added as the catalyst is changed to 13.28 g, so that the mass of the catalyst is 1% of the total mass of oleyl alcohol, propylene oxide, ethylene oxide, and propylene oxide. Finally, product 8 is prepared. The hydroxyl value of the obtained product 8 is 169.5 mgKOH / g, and the calculated molecular weight is about 661.9 g / mol. Through carbon spectrum ( 13 C-NMR) characterization showed carbon atom absorption peaks after ring opening of propylene oxide at δ (64.3, 71.1, 79.3).
[0122] The structural formula of product 8 is:
[0123]
[0124] Where R is C 18 H 35 , a+b is 6, m+n is 1.
[0125] Comparative Example 1
[0126] The preparation method of the nonionic surfactant of Comparative Example 1 comprises the following steps:
[0127] Add 474g of 2-propylheptanol and 3g of potassium hydroxide to the reactor, heat to 110°C, vacuum dehydrate for 1h, and control the moisture content in the reactor to be below 50ppm; then continue to heat to 140°C, slowly add 222g of propylene oxide to the reactor, feed time for 2h, control the pressure at 0.1-0.3MPa, and age for 0.5h; then slowly add 660g of ethylene oxide, feed time for 3.0h, control the pressure at 0.1-0.3Mpa, and age for 1.0h. After aging, cool to 85°C, add lactic acid to neutralize to pH=6.5, vacuum degas, and obtain product 9. The obtained product 9 has a hydroxyl value of 247.3mgKOH / g and a calculated molecular weight of about 453.7g / mol, which is determined to be a difunctional product. Through carbon spectrum ( 13 C-NMR) characterization showed carbon atom absorption peaks after ring opening of propylene oxide at δ (64.6, 64.4, 79.5).
[0128] The structural formula of product 9 is:
[0129]
[0130] Where R is C 12 H 25 , c+d is 5.
[0131] Comparative Example 2
[0132] The preparation method of the nonionic surfactant of Comparative Example 2 comprises the following steps:
[0133] Add 536g of oleyl alcohol (M=268) and 4.0g of sodium hydroxide to the reactor, heat to 120°C, vacuum dehydrate for 1h, and control the moisture content in the reactor to be below 50ppm; heat to 130°C, slowly add 148g of propylene oxide (M=74) to the reactor, control the pressure to 0.1-0.4MPa, and carry out a primary reaction for 1h; heat to 140°C, slowly add 528g of ethylene oxide (M=44), control the pressure to 0.1-0.4Mpa, and carry out a secondary reaction for 4h. After the reaction is completed, cool to 85°C, add lactic acid to neutralize to pH=6.5, vacuum degas, and obtain product 10. The hydroxyl value of the obtained product 10 is 186.4mgKOH / g, and the calculated molecular weight is about 601.9g / mol. Through carbon spectrum ( 13 C-NMR) characterization showed carbon atom absorption peaks after ring opening of propylene oxide at δ (64.3, 71.1, 79.3).
[0134] The structural formula of product 10 is:
[0135]
[0136] Where R is C 18 H 35 , c+d is 6.
[0137] Test example
[0138] Emulsifying ability: Tested by paraffin or dimethyl silicone oil emulsification phase separation method, 40mL of liquid paraffin or dimethyl silicone oil and 40mL of 1g / L non-ionic surfactant aqueous solution were poured into a beaker, stirred and emulsified at 1000rpm for 1min, and then quickly poured into a measuring cylinder, and the time taken to separate 10mL of aqueous phase was recorded. The longer the time, the better the emulsifying ability. See Table 1 for specific results.
[0139] Table 1
[0140]
[0141] It can be seen from Table 1 that, compared with the comparative example, the nonionic surfactant provided by the present invention is a double hydrophilic polyoxyethylene polyoxypropylene ether, so that the nonionic surfactant has excellent emulsifying properties.
[0142] From the comparison between Examples 1-2 and Comparative Example 1, it can be seen that after the nonionic surfactant provided by the present invention emulsifies paraffin and dimethyl silicone oil, it takes a long time to separate 10 mL of water phase, and has excellent emulsification performance.
[0143] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention, rather than to limit it. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or replace some or all of the technical features therein with equivalents. However, these modifications or replacements do not cause the essence of the corresponding technical solutions to deviate from the scope of the technical solutions of the embodiments of the present invention.
Claims
1. A nonionic surfactant, It is characterized in that It has the structure shown in Formula 1: Wherein, R represents at least one of C8-C18 hydrocarbon groups; a+b is 3-12, and m+n is 1-5.
2. The nonionic surfactant according to claim 1, It is characterized in that The R is C 18 H 35 , having the structure shown in Formula 2:
3. The nonionic surfactant according to claim 1 or 2, It is characterized in that The a+b is 6-12, and the m+n is 2-4.
4. The nonionic surfactant according to any one of claims 1 to 3, It is characterized in that The nonionic surfactant is prepared by a method comprising the following steps: To a system including C8-C18 fatty alcohol and a catalyst, propylene oxide, ethylene oxide and propylene oxide are sequentially added to carry out a reaction, and the reaction product is subjected to post-treatment including cooling treatment, neutralization treatment and degassing treatment to obtain the nonionic surfactant.
5. A method for preparing the nonionic surfactant according to any one of claims 1 to 4, It is characterized in that The following steps are involved: 1) reacting a first system including a C8-C18 fatty alcohol, a catalyst, and glycidol to obtain a first intermediate; 2) performing a secondary reaction on a second system including the first intermediate and ethylene oxide to obtain a second intermediate; 3) reacting the third system including the second intermediate and propylene oxide three times to obtain a third intermediate; 4) performing post-treatment including cooling treatment, neutralization treatment and degassing treatment on the third intermediate to obtain the nonionic surfactant.
6. The preparation method according to claim 5, It is characterized in that The mass of the catalyst is 0.02-1% of the total mass of the fatty alcohol, propylene oxide, ethylene oxide and propylene oxide.
7. The preparation method according to claim 5 or 6, It is characterized in that The molar ratio of the fatty alcohol to glycidol is 1:1-1.2; The temperature of the primary reaction is 120-160° C. and the time is 0.5-4 h.
8. The preparation method according to any one of claims 5 to 7, It is characterized in that The molar ratio of the fatty alcohol to ethylene oxide is 1:3-12; The temperature of the secondary reaction is 120-160° C. and the time is 1-4 hours.
9. The preparation method according to any one of claims 5 to 8, It is characterized in that The molar ratio of the fatty alcohol to propylene oxide is 1:1-5; The temperature of the three reactions is 110-160° C. and the time is 0.5-4 h.
10. A functional composition, It is characterized in that The invention comprises the nonionic surfactant described in any one of claims 1 to 4 and the nonionic surfactant prepared by the preparation method described in any one of claims 5 to 9.
11. A method for emulsifying paraffin or dimethyl silicone oil, It is characterized in that Paraffin or dimethyl silicone oil is emulsified using the nonionic surfactant described in any one of 1-4, the nonionic surfactant prepared by the preparation method described in any one of claims 5-9, and the functional composition described in claim 10.
Citation Information
Cited By
Non-ionic surfactant as well as preparation method and application thereof
CN119798052A
A nonionic surfactant, its preparation method and use
CN119798052B