Buckling-resistance brace
By using alloy steel materials and specific microstructural structures in anti-buckling supports, combined with end restraint sections and casing design, the problem of poor low-cycle fatigue performance in the existing technology is solved, and the problem of poor low-cycle fatigue performance in high-intensity earthquakes and long-term Important role under vibration and improved seismic performance.
Patent Information
- Application Number
- CN201811436554.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2018-11-28
- Publication Date
- 2024-10-22
- Estimated Expiration
- 2038-11-28
AI Technical Summary
Existing anti-buckling supports cannot effectively function due to poor low-cycle fatigue performance under high-severity earthquakes and long-term vibrations, resulting in material fatigue fracture.
Made of alloy steel, the microstructural structure is composed of metastable austenite and thermally induced epsilon martensite with a volume fraction of no more than 10%. Combined with a specific chemical composition and organizational structure, it enhances hysteretic characteristics and low-cycle fatigue performance. And through the design of the end restraint section and casing, it is ensured that the buckling section can fully exert its hysteretic energy dissipation effect under high-severity vibration.
It plays an important role in high-intensity earthquakes and long-term vibrations, improves the seismic performance of buildings, and extends fatigue life and fatigue resistance by optimizing materials and connection methods.
Smart Images

Figure CN109339545B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to an anti-buckling energy dissipation brace, belonging to the technical field of civil engineering structures. Background Art
[0002] Large-scale earthquakes and long-term, long-period external vibrations can cause great damage to high-rise buildings and structures. Energy dissipation and shock absorption devices and technologies can effectively absorb external vibration energy and minimize damage to buildings and structures. Buckling-resistance braces are a common energy dissipation and shock absorption element that are widely used in civil engineering structures. Under small earthquakes, buckling-resistance braces can provide additional stiffness to beam-column structures and reduce structural deformation; under large earthquakes, buckling-resistance braces can yield when subjected to tension or compression, showing good hysteretic energy dissipation capacity.
[0003] At present, buckling-resistance braces mainly use mild steel and low-yield carbon steel (such as industrial pure iron, low-yield steel for shock absorption with a yield strength of 100-225MPa, Q235 steel, etc.) as energy-absorbing core materials. Although the above-mentioned core steels have low yield strength, relatively stable hysteresis characteristics and full hysteresis curves, their low-cycle fatigue performance is poor. Under a large earthquake, the material will suffer fatigue fracture after a few cycles of tension-compression cyclic loads. Therefore, buckling-resistance braces made of the above-mentioned core materials cannot play an important role under high-intensity earthquakes and long-term vibrations. Summary of the invention
[0004] The object of the present invention is to provide a buckling-resistance energy dissipation brace.
[0005] Different from the existing buckling-resistance brace, the core material of the buckling-resistance brace of the present invention not only has stable hysteresis characteristics and a full hysteresis curve, but also has excellent low-cycle fatigue performance. Therefore, the buckling-resistance brace of the present invention has stronger cumulative plastic deformation capacity and hysteresis energy dissipation capacity, and can still play an important role under high-intensity earthquakes and long-term vibrations.
[0006] The purpose of the present invention can be achieved by the following technical solutions:
[0007] The present invention provides an anti-buckling energy dissipation support, comprising an end restraint section, a buckling section and a sleeve; the end restraint section is located at both ends of the buckling section and plays a role in transferring loads, one side of the end restraint section is connected to the buckling section, and the other side is used to connect with a beam, a column member or a node; the sleeve is fixed to the outside of the buckling section by grouting concrete, and a layer of non-bonding material is provided between the concrete and the outside of the buckling section; the buckling section plays an energy dissipation role, and is made of alloy steel, the microstructure of the alloy steel consists of metastable austenite and heat-induced ε martensite with a volume fraction not exceeding 10%, and when entering the yield stage, the microstructure of the alloy steel undergoes ε martensite phase transformation under the action of stress / strain, and undergoes reversible phase transformation between the metastable austenite and the stress / strain-induced ε martensite under the action of tension-compression alternating loads.
[0008] The present invention limits the microstructure of the alloy steel material used in the buckling section to austenite and ε martensite (formed by heat induction) with a volume fraction not exceeding 10%. The purpose is to promote the stress / strain induced formation of lamellar ε martensite with single variant crystallographic characteristics under tensile-compression alternating loads, avoid strong interaction between the heat-induced ε martensite in the original matrix structure and the stress / strain induced ε martensite, thereby promoting the reversible phase transformation between austenite and stress / strain induced ε martensite, reducing the generation of alloy steel matrix crystal defects and delaying the expansion of fatigue cracks, so that the alloy steel has excellent room temperature low-cycle fatigue life.
[0009] Furthermore, the mass percentage of the chemical composition of the buckling section alloy steel is: 20.0%≤Mn≤34.0%, 3.5%≤Si≤6.0%, 0.1%≤Ni≤5.0%, 0.005%≤C<0.15%, P≤0.02%, S≤0.03%, N≤0.02%, and the rest is Fe and unavoidable impurity elements, wherein the mass percentage of Mn, Ni and C also satisfies the following relationship: Mn+1.6Ni+52C≥32% and Mn+2Ni≤37%. The yield strength of the above alloy steel is between 200 and 360 MPa; under cyclic tension-compression loading conditions, when the strain amplitude, strain ratio and loading frequency are 1%, -1.0 and 0.1-0.2 Hz respectively, the stress amplitude is <530 MPa, and the room temperature fatigue life of the alloy steel is >2000 cycles.
[0010] Furthermore, the mass percentages of the chemical components of the alloy steel in the buckling section are as follows: 24% ≤ Mn ≤ 32%, 3.5% ≤ Si ≤ 6.0%, 1.0% < Al < 2.5%, 0.005% ≤ C < 0.14%, P ≤ 0.02%, S ≤ 0.03%, N ≤ 0.02%, and the balance is Fe and inevitable impurity elements, where the mass percentage contents of Si and Al satisfy the relationship: 2.0 < Si / Al ≤ 4.5. The yield strength of the above alloy steel is between 200 and 380 MPa; under the condition of cyclic tension-compression loading, when the strain amplitude, strain ratio, and loading frequency are 1%, -1.0, and 0.1 - 0.2 Hz respectively, the stress amplitude < 550 MPa, and the room-temperature fatigue life of the steel plate > 2000 cycles.
[0011] In the present invention, the buckling section serves as an energy-dissipating core material, and the cross-section of the buckling section has any type of axisymmetric geometric shape, and its axis of symmetry is in the axial direction of the support. The cross-sectional forms with any type of axisymmetric geometric shape mainly include the I-shaped, cross-shaped, H-shaped, double-T-shaped, circular-shaped, etc. Generally, the core materials with complex symmetric cross-sections such as the cross-shaped, H-shaped, and double-T-shaped can be formed by welding alloy steel plates with high fatigue performance.
[0012] In order to make the plastic deformation of the buckling-restrained energy-dissipating brace only concentrate in the buckling section (so that the buckling section can fully play the role of hysteretic energy dissipation) and avoid obvious yield deformation or even failure at the connection between the buckling section and the two-side end restraint sections during the service of the brace, the buckling section adopts a cross-sectional form that is narrow in the middle and wide at both ends. The reasonable selection of the ratio of the cross-sectional area of the middle part to that of the two ends of the buckling section mainly depends on the connection strength between the buckling section and the end restraint section and the (yield) strength of the alloy steel of the buckling section. In principle, the yield limit force when the connection between the buckling section and the end restraint section yields needs to be greater than the yield limit force when the buckling section yields.
[0013] The end restraint section is usually a structural elastic connector composed of units such as square steel plates (steel blocks), angle steels, short T-shaped steel beams, or reserved connecting plates of beam-column members, and the units are connected into one body by welding or high-strength bolts. The material of the end restraint section is usually selected from Q235 steel, Q345 steel, 45# steel, etc.
[0014] One side of the end restraint section and the buckling section can be combined by means of welding, bolt connection, or threaded connection.
[0015] When the buckling section is connected to one side of the end restraint section by welding, the welding material can be selected from austenitic stainless steel welding wires such as ER309MoL or duplex stainless steel welding wires such as ER2209, so that the (yield) strength at the weld is similar to or not less than the (yield) strength of the buckling section material, thereby satisfying that the yield limit force when yielding occurs at the weld is greater than the yield limit force when yielding occurs in the buckling section.
[0016] Furthermore, the ratio of the cross-sectional area of the middle part and the two end parts of the buckling section is reasonably selected so that the yield limit force when the weld yields is not less than 1.5 to 1.8 times the yield limit force when the buckling section yields, so as to fully ensure that plastic deformation and hysteresis energy dissipation occur only in the middle part of the supported buckling section.
[0017] The buckling section and one side of the end restraining section can also be connected by a threaded joint. The buckling section is processed with external threads at both ends, and one side of the end restraining section adjacent thereto is processed with internal threads. The specification size of the thread and the thread connection depth are reasonably selected so that the yield limit force when the thread connection yields is greater than the yield limit force when the buckling section yields.
[0018] The buckling section and one side of the end restraint section can also be connected by high-strength bolts. The number and position of the bolt connection joints are reasonably selected so that the yield limit force when all bolt connections yield is greater than the yield limit force when the buckling section yields.
[0019] The sleeve is made of steel and has a round tube shape or a square tube shape.
[0020] The buckling-resistance energy-dissipation support of the present invention is installed in buildings and structures, and is connected with beams, column components or nodes of the buildings or structures to form a whole. The support has the energy-dissipation function of a metal damper, and can significantly improve the seismic performance of buildings and structures.
[0021] Compared with the prior art, the present invention has the following beneficial effects:
[0022] The alloy steel material used in the buckling section of the buckling-resistant energy-dissipating support of the present invention has metastable austenite and heat-induced ε martensite with a volume fraction not exceeding 10%. Under the action of tension-compression alternating loads, the internal microstructure of the material undergoes a reversible phase transformation between austenite and stress / strain-induced ε martensite, so that the alloy steel material has excellent room temperature low-cycle fatigue performance and hysteresis energy dissipation characteristics. The energy-dissipating support of the present invention can play an important role even in frequent and high-intensity vibration environments. In addition, compared with traditional energy-dissipating core materials (yield strength is usually less than 235MPa), the new energy-dissipating alloy steel core material also has higher strength (yield strength is between 200 and 380MPa), which helps to achieve lightweight energy-dissipating support. BRIEF DESCRIPTION OF THE DRAWINGS
[0023] Figure 1 Schematic diagram of the three-dimensional structure of the bolt-connected buckling-resistance energy-absorbing support in Example 1.
[0024] Figure 2 for Figure 1 Schematic diagram of the exploded structure of the components of the bolted buckling-resistance brace shown.
[0025] Figure 3 for Figure 1 Schematic diagram of the cross-sectional structure of the bolt-connected buckling-resistance energy-absorbing brace shown.
[0026] Figure 4 This is a schematic diagram of the cross-sectional structure of the welded joint type buckling-resistance energy-absorbing support in Example 2.
[0027] Figure 5 for Figure 4 Schematic diagram of the BB section structure.
[0028] Figure 6 for Figure 4 Schematic diagram of the CC cross-section structure.
[0029] Figure 7 This is a schematic diagram of the cross-sectional structure of the threaded joint type buckling-resistance energy-absorbing brace in Example 3.
[0030] Figure 8 for Figure 7 Schematic diagram of the AA section structure.
[0031] Numbers in the figure: 1, end restraint section, 2, buckling section, 3, casing. DETAILED DESCRIPTION
[0032] The present invention is described in detail below with reference to the accompanying drawings and specific embodiments.
[0033] Embodiment 1:
[0034] like Figure 1 , Figure 2 and Figure 3 As shown, a new type of bolt-connected buckling-resistance energy dissipation support consists of three parts: an end restraint section 1, a buckling section 2 and a sleeve 3; the end restraint section 1 is located at both ends of the buckling section 2, plays a role in transferring load, and one side of the end restraint section 1 is connected to the buckling section 2; the buckling section 2 bears the role of plastic deformation and hysteresis energy dissipation; the sleeve 3 is fixed to the outside of the buckling section 2 by grouting concrete, and there is a layer of non-bonding material between the concrete and the outside of the buckling section.
[0035] The cross-sectional shape of the buckling section 2 is a straight line, and the cross-sectional area is narrow in the middle and wide at both ends along the axial direction, and the ratio of the cross-sectional area between the middle part and the two ends is 2:1. The material of the buckling section 2 is alloy steel, and the chemical composition and mass percentage of the alloy steel are: 29.8% Mn, 4.97% Si, 1.74% Al, 0.008% C, 0.009% P, 0.023% S, 0.005% N, and the rest are Fe and unavoidable impurity elements. The yield strength of the alloy steel is 328MPa; under cyclic tension-compression loading conditions, when the strain amplitude, strain ratio and loading frequency are 1%, -1.0 and 0.2Hz respectively, the stress amplitude is 468MPa, and the room temperature fatigue life of the steel plate is 7991 cycles. The microstructure of the alloy steel is a single austenite structure; when entering the yield stage, the austenite structure of the alloy steel undergoes an ε martensite phase transformation under stress / strain, and a reversible phase transformation between austenite and stress / strain-induced ε martensite occurs under the action of tension-compression alternating loads. Bolt holes are processed at both ends of the buckling section 2. In this embodiment, the sleeve is square.
[0036] The end restraint section 1 is welded from three Q345 steel plates, two parallel steel plates are vertically welded to the third steel plate, and the interval between the two parallel steel plates is the thickness of the steel plate of the flexure section 2. Bolt holes are processed at the corresponding positions of the two parallel steel plates. The two ends of the flexure section 2 (the corresponding positions are also processed with bolt holes) are inserted between the two parallel steel plates of the end restraint section 1, and then firmly connected with bolts. In this way, the end restraint section 1 is connected to the flexure section 2.
[0037] The design of the geometric shapes and connection modes of the end restraining section 1 and the buckling section 2 ensures that the buckling section 2 bears all the plastic deformation and fully exerts the hysteresis energy dissipation function.
[0038] The buckling-resistance energy dissipation support is connected to the beam, column member or node at the end restraint section 1 by bolts.
[0039] Embodiment 2:
[0040] refer to Figure 4 , Figure 5 and Figure 6 A welded joint type buckling restrained brace is composed of three parts: an end restraint section 1, a buckling section 2 and a sleeve 3; the end restraint section 1 is located at both ends of the buckling section 2, and one side of the end restraint section 1 is connected to the buckling section 2; the buckling section 2 bears the role of plastic deformation and hysteresis energy dissipation; the sleeve 3 is fixed to the outside of the buckling section 2 by grouting concrete, and there is a layer of non-bonding material between the concrete and the outside of the buckling section. In this embodiment, the sleeve is square.
[0041] The cross-sectional shape of the buckling section 2 is a cross-shaped cross-sectional shape, which is narrow in the middle and wide at both ends along the axial direction, and the cross-sectional area ratio of the middle part to the two ends is 2:1. The cross-shaped cross-sectional shape is obtained by welding, and the welding material is ER307Si austenitic stainless steel welding wire. The material of the buckling section 2 is alloy steel, and the chemical composition and mass percentage of the alloy steel are: 30.8% Mn, 4.58% Si, 2.77% Ni, 0.08% C, 0.01% P, 0.018% S, 0.008% N, and the rest are Fe and unavoidable impurity elements. The yield strength of the alloy steel is 279MPa; under cyclic tension-compression loading conditions, when the strain amplitude, strain ratio and loading frequency are 1%, -1.0 and 0.2Hz respectively, the stress amplitude is 460MPa, and the room temperature fatigue life of the steel plate is 7819 cycles. The microstructure of the alloy steel is single austenite; when entering the yield stage, the microstructure of the alloy steel undergoes a reversible phase transformation between austenite and stress / strain induced ε martensite under the action of tension-compression alternating loads.
[0042] The cross-sectional shape of the end restraint section 1 is also cross-shaped and is welded from Q345 steel plates. The cross-sectional shape of the end restraint section 1 is opposite to that of the buckling section 2 and is connected together by CO2 gas shielded welding, and the welding material is ER307Si austenitic stainless steel welding wire.
[0043] The design of the geometric shapes and connection modes of the end restraining section 1 and the buckling section 2 ensures that the buckling section 2 bears all the plastic deformation and fully exerts the hysteresis energy dissipation function.
[0044] The buckling-resistance energy dissipation support is connected to the beam, column member or node at the end restraint section 1.
[0045] Embodiment 3:
[0046] refer to Figure 7 and Figure 8 A threaded joint type buckling-resistance energy dissipation brace, consisting of an end restraint section 1, a buckling section 2 and a sleeve 3; the end restraint section 1 is located at both ends of the buckling section 2, and one side of the end restraint section 1 is connected to the buckling section 2; the buckling section 2 bears the role of plastic deformation and hysteresis energy dissipation; the sleeve 3 is fixed to the outside of the buckling section 2 by grouting concrete, and there is a layer of non-bonding material between the concrete and the outside of the buckling section. In this embodiment, the sleeve is a circular tube.
[0047] The cross-sectional shape of the buckling section 2 is circular, and the circular cross-section is narrow in the middle and wide at both ends along the axial direction, and the cross-sectional area ratio of the middle part to the two ends is 2.5:1. The material of the buckling section 2 is alloy steel, and the chemical composition and mass percentage of the alloy steel are: 28.1% Mn, 4.40% Si, 2.92% Ni, 0.1% C, 0.01% P, 0.02% S, 0.009% N, and the rest are Fe and unavoidable impurity elements. The yield strength of the alloy steel is 291MPa; under cyclic tension-compression loading conditions, when the strain amplitude, strain ratio and loading frequency are 1%, -1.0 and 0.2Hz respectively, the stress amplitude is 482MPa, and the room temperature fatigue life of the steel is 6899 cycles. The microstructure of the alloy steel is single austenite; when entering the yield stage, the microstructure of the alloy steel undergoes a reversible phase transformation between austenite and stress / strain induced ε martensite under the action of tension-compression alternating loads. Both ends of the buckling section 2 are processed with external threads.
[0048] The end restraint section 1 is made of a Q345 steel block, and an internal assembly thread is processed on one side thereof connected to the buckling section 2. The end restraint section 1 is connected to the buckling section 2 through a threaded joint.
[0049] The design of the geometric shapes and connection modes of the end restraining section 1 and the buckling section 2 ensures that the buckling section 2 bears all the plastic deformation and fully exerts the hysteresis energy dissipation function.
[0050] The buckling-resistance energy dissipation support is connected to the beam, column member or node at the end restraint section 1 by bolts.
[0051] The above description of the embodiments is to facilitate the understanding and use of the invention by those skilled in the art. It is obvious that those skilled in the art can easily make various modifications to these embodiments and apply the general principles described herein to other embodiments without creative work. Therefore, the present invention is not limited to the above embodiments, and improvements and modifications made by those skilled in the art based on the disclosure of the present invention without departing from the scope of the present invention should be within the scope of protection of the present invention.
Claims
1. A buckling-resistance energy dissipation brace, characterized in that: It comprises an end restraint section, a buckling section and a sleeve; the end restraint section is located at both ends of the buckling section and plays a role in transferring loads, one side of the end restraint section is connected to the buckling section, and the other side is used to connect to a beam, a column member or a node; the sleeve is fixed to the outside of the buckling section by grouting and filling concrete, and there is a layer of non-bonding material between the concrete and the outside of the buckling section; The buckling section plays an energy dissipation role and is made of alloy steel. The microstructure of the alloy steel consists of metastable austenite and heat-induced ɛ martensite with a volume fraction not exceeding 10%. When entering the yield stage, the microstructure of the alloy steel undergoes a ɛ martensite phase transformation under the action of stress / strain, and a reversible phase transformation between the metastable austenite and the stress / strain-induced ɛ martensite occurs under the action of tension-compression alternating loads; The alloy steel is composed of the following chemical components in mass percentage: 20.0%≤Mn≤34.0%, 3.5%≤Si≤6.0%, 0.1%≤Ni≤2.92%, 0.005%≤C<0.15%, P≤0.02%, S≤0.03%, N≤0.02%, and the rest are Fe and unavoidable impurity elements, wherein the mass percentage contents of Mn, Ni and C also satisfy the following relationship: Mn+1.6Ni+52C≥32% and Mn+2Ni≤37%; The yield strength of the alloy steel material of the buckling section is between 200 and 360 MPa; under cyclic tension-compression loading conditions, when the strain amplitude, strain ratio and loading frequency are 1%, -1.0 and 0.1-0.2 Hz respectively, the stress amplitude is less than 530 MPa, and the room temperature fatigue life of the alloy steel is greater than 2000 cycles; The buckling section adopts a cross-section form that is narrow in the middle and wide at both ends; the ratio of the cross-sectional area of the middle part of the buckling section to the two end parts is such that the yield limit force when the connection between the buckling section and one side of the end constraint section yields is greater than the yield limit force when the buckling section yields, so as to fully ensure that plastic deformation and hysteresis energy dissipation occur only in the middle part of the supported buckling section; The connection method between the buckling section and one side of the end restraining section is selected from one of welding, threaded joint connection, and high-strength bolt connection.
2. A buckling-resistance brace according to claim 1, characterized in that: The cross section of the buckling section has any type of axisymmetric geometry, with the axis of symmetry being the axis direction of the support.
3. The buckling-resistance brace according to claim 1, characterized in that: The buckling section is connected to one side of the end restraining section by welding, and the yield limit force of the welding point when yielding is not less than 1.5 to 1.8 times the yield limit force of the buckling section when yielding.