A VCP electroplating device
By using the main tank body with upper and lower openings and spoiler baffle in the electroplating device, the turbulence effect of the electroplating solution is achieved, the problems of uneven thickness of the electroplating layer, large equipment volume and high cost are solved, and the electroplating efficiency and compact equipment are improved. type.
Patent Information
- Application Number
- CN201910214456.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2019-03-20
- Publication Date
- 2024-11-08
- Estimated Expiration
- 2039-03-20
AI Technical Summary
Due to the complex structure and large equipment volume, the existing electroplating devices have large spacing between the cathode and anode plates, which affects the uniformity of the distribution of power lines, causing inconsistent thickness of the electroplating layer, and high equipment costs and high energy consumption.
The main groove body design with upper and lower openings is designed, and the spoiler baffle is set between the anode plate and the cathode plate, and the jet device is omitted, so that the plating solution enters from the upper opening, and flows out from the lower opening under the action of gravity, increasing the turbulence effect and passing through the The flow rate adjustment device adjusts the flow rate of the plating solution.
The distance between the cathode and anode plates is significantly reduced, the uniformity of the electroplating layer is improved, the equipment volume and cost is reduced, the electroplating efficiency is enhanced, and the problem of uneven thickness of the electroplating layer is solved.
Smart Images

Figure CN109735892B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of electroplating, and in particular to a VCP electroplating device. Background Art
[0002] Currently, the commonly used electroplating equipment for PCB workpieces generally consists of a tank body, an anode plate, a cathode plate (PCB workpiece to be electroplated) and a jet device to promote the flow of electrolyte. This system has a complex structure and a large volume. Since the distance between the anode and cathode plates is large, the uniformity of the distribution of the electric lines is affected, resulting in uneven current distribution on the PCB workpiece to be electroplated, which makes the thickness of the electroplating layer inconsistent, affecting product quality.
[0003] CN207672141U discloses an electroplating device with a movable jet rod, which includes: an electroplating tank, an anode, a cathode, an electroplating solution jet system and a power device. The electroplating solution jet system includes a first liquid inlet pipe, a second liquid inlet pipe, a pump, a three-way valve and two jet main rods; the electroplating device of the utility model has a movable jet rod that adjusts the relative position between the nozzle and the printed circuit board by horizontally reciprocating left and right, and enhances the solution exchange of the electroplating solution on the surface of the printed circuit board, through holes and blind holes without affecting the overall solution circulation, thereby effectively improving the uniformity of the electroplating coating and the through-hole capacity of the solution. Although the above device improves the solution exchange between the electrolyte and the surface of the cathode plate by improving the jet device, there are still problems such as large equipment volume, high device cost and high energy consumption of the jet device.
[0004] CN106350841A discloses an electroplating device, which includes an electroplating tank, a conveying mechanism and multiple groups of jet components arranged in the electroplating tank, wherein the jet components include two resin jet tubes arranged side by side, a gap is left between the two jet tubes for the circuit board to pass through, at least one row of spray hole groups distributed along the axial direction of the jet tube is arranged along the inner side of each of the jet tubes, the spray hole groups in each row of the two jet tubes are arranged opposite to each other, each of the spray hole groups includes a plurality of spray holes, and the spray holes in the spray hole groups in the opposite rows are staggered along the axial direction of the spray tube; the above device has the problems of complex device structure, high equipment cost and large equipment volume.
[0005] CN207468763U discloses a mobile stirring electroplating device, which includes an electroplating tank containing electroplating parts, wherein the electroplating tank is provided with an electroplating solution; a jet pipe arranged on the electroplating tank for spraying the electroplating solution; a clamping device for clamping a workpiece to be electroplated; a first power device arranged above the electroplating tank for driving the workpiece to move horizontally; and a second power device arranged on one side of the electroplating tank for driving the workpiece to move up and down. The above-mentioned device has a large equipment volume, complex operation and high operating cost.
[0006] Although the above documents disclose some electroplating devices, there are still problems such as large equipment size, high cost, and uneven electroplating layer thickness due to the large distance between the anode and cathode plates. Therefore, it is still of great significance to develop an electroplating device with small equipment size and uniform electroplating layer thickness. Summary of the invention
[0007] The object of the present invention is to provide a VCP electroplating device, which omits the jet device in the traditional device by setting a spoiler baffle between the conductive space accommodating the cathode plate and the anode plate, so that during the electroplating process, the distance between the anode plate and the cathode plate is significantly reduced, thereby fundamentally solving the problem of inconsistent thickness of the electroplating layer. The reduction in the distance between the anode and cathode plates significantly reduces the volume of the main tank body of the electroplating tank, thereby improving the compactness of the device and reducing the cost of the equipment.
[0008] In order to achieve the purpose of the invention, the present invention adopts the following technical solutions:
[0009] The present invention provides a VCP electroplating device, which includes a main tank body 1, which is a shell with upper and lower openings; two anode plates 2 are arranged in the shell along the opening direction, and an electroplating space for accommodating a cathode plate 3 is provided between the two anode plates 2; a spoiler baffle 4 is provided between the anode plate 2 and the electroplating space for accommodating the cathode plate 3.
[0010] The electroplating space for accommodating the cathode plate in the VCP electroplating device of the present invention is used to place the cathode plate during the electroplating process; during the electroplating process, the cathode plate is placed in the electroplating space between the two anode plates. Since the upper and lower openings of the shell are parallel to the ground, the electroplating solution enters the shell from the upper opening of the shell, and then flows through the anode plate and the cathode plate under the action of gravity, thereby achieving the electroplating effect. A spoiler baffle is arranged between the anode plate and the cathode plate, which can prevent the cathode plate from short-circuiting when in contact with the anode plate, and on the other hand, it can play a stirring role in the process of the electroplating solution flowing from top to bottom, thereby generating turbulence in the electroplating solution. In addition, this device reduces the jet device in the traditional electroplating device, thereby greatly reducing the distance between the anode plate and the cathode plate, so that the width of the shell is significantly reduced, reducing the footprint of the equipment, and the reduction in the width of the shell can significantly increase the flow rate of the electroplating solution from top to bottom, thereby producing a jet-like effect.
[0011] The device of the present invention simplifies the jet device in the traditional device, so that the distance between the two anode plates can be significantly reduced, which on the one hand reduces the footprint of the device, and on the other hand makes the layout of the power lines more convenient.
[0012] The spoiler baffle of the present invention may be any spoiler baffle having any shape that can produce a spoiler effect, for example, a louver shape.
[0013] Preferably, the two anode plates 2 are arranged in parallel.
[0014] Preferably, the two anode plates 2 are arranged opposite to each other.
[0015] Preferably, the housing comprises a rectangular parallelepiped housing.
[0016] Preferably, the anode plate 2 extends along the length direction of the shell.
[0017] Preferably, the length of the shell is 2-100m, for example, 2m, 10m, 15m, 20m, 30m, 40m, 50m, 60m, 70m, 80m, 90m or 100m, etc.
[0018] Preferably, the shell is formed by splicing n segments along the length direction.
[0019] Preferably, the length of the segment is 1-4 m, for example, 1 m, 1.2 m, 1.5 m, 1.8 m, 2 m, 2.5 m, 3 m, 3.5 m or 4 m.
[0020] Preferably, n≥1, for example, 1, 3, 5, 7, 9, 10, 20 or 30, etc.
[0021] The shell of the present invention is formed by splicing n segments with a length of 1-4m; for example, the total length of the shell is 21m, the length of each segment is 3m, and 7 segments are required according to actual requirements.
[0022] Preferably, the width of the shell is 5.5-10 cm, for example, 5.5 cm, 6 cm, 6.5 cm, 7 cm, 7.5 cm, 8 cm, 8.5 cm, 9 cm, 9.5 cm or 10 cm, etc., preferably 5.5-6.5 cm, and more preferably 5.5 cm.
[0023] The width of the shell used in the present invention is significantly smaller than that of the traditional electroplating device, which significantly reduces the floor space and facilitates the layout of the power lines. At the same time, the narrow shell width can accelerate the flow speed of the fluid, which cooperates with the spoiler baffle to increase the turbulence of the solution, thereby maintaining a high electroplating efficiency. There is no need to use a jet device, saving equipment costs.
[0024] Preferably, the height of the shell is 20-90 cm, for example, 20 cm, 30 cm, 40 cm, 50 cm, 60 cm, 70 cm, 80 cm or 90 cm, etc., preferably 60-80 cm, and more preferably 70 cm.
[0025] Preferably, the distance between the two anode plates is 1-6 cm, such as 1 cm, 2 cm, 3 cm, 4 cm, 5 cm or 6 cm, etc., preferably 2 cm.
[0026] The present invention controls the distance between the two anode plates to be 1-6 cm, which is significantly reduced compared with the anode plate spacing (15-20 cm) of traditional equipment, making the arrangement of the power lines between the anode plate and the cathode plate more convenient and fundamentally solving the problem of poor consistency of the electroplating layer thickness.
[0027] Preferably, a plating space for accommodating a cathode plate is provided at a middle position between the two anode plates.
[0028] Preferably, the electroplating space accommodating the cathode plate is arranged in parallel with the anode plate 2 .
[0029] Preferably, the electroplating space accommodating the cathode plate is arranged opposite to the anode plate 2 .
[0030] The thickness of the electroplating space for accommodating the cathode plate is determined according to the thickness of the cathode plate, and the thickness needs to be such that after the cathode plate is placed, the cathode plate can move along the conductive track.
[0031] Preferably, the spoiler baffle 4 is symmetrically arranged between the anode plate 2 and the electroplating space accommodating the cathode plate 3 .
[0032] The device of the present invention can adjust the flow rate of the electroplating solution at the shell outlet through the flow regulating device, thereby effectively adjusting the electroplating process parameters.
[0033] Preferably, the lower end opening of the shell is connected to the auxiliary groove 5.
[0034] Preferably, the sub-tank stores electroplating solution.
[0035] Preferably, the lower end of the auxiliary tank is connected to the centrifugal pump 6.
[0036] Preferably, a flow regulating device is provided at the lower opening of the shell.
[0037] Preferably, the flow regulating device comprises a leakage flow regulating plate 7.
[0038] Preferably, the upper opening of the shell is connected to the liquid collecting device.
[0039] Preferably, the liquid collecting device comprises a liquid collecting tray 8 .
[0040] Preferably, the liquid collecting tray 8 is in communication with the centrifugal pump 6 .
[0041] The lower end opening of the shell of the main tank body of the present invention is connected to the auxiliary tank, and the plating liquid flows out from the lower end of the shell and enters the auxiliary tank. The auxiliary tank is used to store the plating liquid, and the upper end opening of the shell is connected to the liquid collecting device; the plating liquid can be transferred from the auxiliary tank to the liquid collecting device via a centrifugal pump, and the plating liquid in the liquid collecting device enters the main tank body through the upper end opening of the shell to participate in the electroplating reaction.
[0042] Preferably, the cathode plate 3 comprises a plate-shaped workpiece to be electroplated.
[0043] Preferably, the device further comprises a conductive track, wherein the conductive track is used to place the cathode plate into the electroplating space accommodating the cathode plate.
[0044] Preferably, the conductive track comprises a conductive clamp, and the conductive clamp is used to connect the cathode plate.
[0045] During the electroplating process, the cathode plate is connected to the conductive track through a conductive clamp, and the cathode plate moves along the length direction of the shell with the conductive track, thereby completing the electroplating process and realizing the continuous operation of the electroplating process. The conductive clamp and the conductive track are common settings in the electroplating process in the art and are not limited here.
[0046] The method of using the device of the present invention is as follows:
[0047] During the electroplating process, the cathode plate (the plate-shaped workpiece to be electroplated) is placed between two anode plates (denoted as anode plate A and anode plate B), and spoiler baffles are arranged between anode plate A and the cathode plate and between anode plate B and the cathode plate; the electroplating liquid is added from the upper opening of the shell, and due to the action of gravity, it flows out from the lower opening of the shell; thus completing the electroplating process.
[0048] Compared with the prior art, the present invention has the following beneficial effects:
[0049] (1) The device of the present invention adopts a shell with upper and lower openings as the main tank body, eliminating the jet device, and at the same time, a spoiler baffle is set between the anode plate and the electroplating space accommodating the cathode plate, so that the electroplating liquid enters the shell from the upper opening, and then flows out from the lower opening under the action of gravity. The elimination of the jet device significantly reduces the distance between the cathode plate and the anode plate, and significantly increases the flow rate of the fluid from top to bottom. The presence of the spoiler baffle plays a stirring role on the electroplating liquid, increases the turbulence of the electroplating liquid, and ensures the quality of electroplating;
[0050] (2) The distance between the anode plate and the cathode plate of the device described in the present invention is significantly reduced, which fundamentally solves the problem of uneven electroplating and facilitates the layout of power lines. The volume of the main tank is also significantly reduced, saving floor space, improving the compactness of the electroplating device, and saving equipment costs. BRIEF DESCRIPTION OF THE DRAWINGS
[0051] Figure 1 is a schematic diagram of a VCP electroplating device described in the specific implementation mode of the present invention;
[0052] Figure 2 It is a schematic diagram of the method for selecting measurement points of the 85-point copper thickness measurement method described in the application example of the present invention.
[0053] 1-main tank body, 2-anode plate, 3-cathode plate, 4-spoiler baffle, 5-auxiliary tank, 6-centrifugal pump, 7-leakage flow regulating plate, 8-liquid collecting tray. DETAILED DESCRIPTION
[0054] The technical solution of the present invention is further described below by specific implementation methods. It should be understood by those skilled in the art that the embodiments are only to help understand the present invention and should not be regarded as specific limitations of the present invention.
[0055] This embodiment provides a VCP electroplating device. Figure 1 As shown, the electroplating device includes a main tank body 1, which is a rectangular shell structure, and its upper and lower surfaces are open designs (that is, it does not include the upper and lower surfaces); two anode plates 2 are arranged in parallel and opposite to each other in the shell along the opening direction, and the two anode plates 2 extend along the length direction of the shell; a plating space for accommodating a cathode plate 3 is arranged between the two anode plates 2, which is used to place the cathode plate 3, and the electroplating space for accommodating the cathode plate 3 is arranged in parallel and opposite to each other in the middle position of the two anode plates 2; spoiler baffles 4 are symmetrically arranged between the two anode plates 2 and the electroplating space for accommodating the cathode plate 3; the lower opening of the shell is connected to the auxiliary tank 5, and the auxiliary tank 5 is connected to the liquid collecting tray 8 through a centrifugal pump 6, and the centrifugal pump 6 is used to transfer the electroplating liquid from the auxiliary tank to the liquid collecting tray, and a leakage flow regulating plate 7 is arranged at the lower end opening of the shell to control the flow rate of the electroplating liquid.
[0056] The method of using the device described in this embodiment is as follows:
[0057] During the electroplating process, the cathode plate (plate-shaped workpiece to be electroplated) connected to the conductive track by a conductive fixture follows the conductive track into the electroplating space provided between the two anode plates for accommodating the cathode plate;
[0058] The plating liquid in the auxiliary tank enters the liquid collecting tray through a centrifugal pump, and the plating liquid in the liquid collecting tray enters the main tank body through the upper opening of the main tank body, and contacts the anode plate and the cathode plate. Under the action of the spoiler baffle, the plating liquid generates turbulence, which increases its contact with the anode and cathode plates, and then flows into the auxiliary tank through the lower opening of the main tank body; a leakage flow regulating plate is arranged at the lower end of the shell of the main tank body, which is used to regulate the flow through the main tank body.
[0059] During the electroplating process, the cathode plate moves along the length direction of the main tank shell along with the conductive guide rail, thereby realizing continuous operation of the above process.
[0060] Application Example 1
[0061] This application example adopts the device described in the above embodiment: wherein, the height of the main tank body is 70cm and the width is 4.5cm. The material of the main tank body is PP material, the total thickness of the PP plate in the width direction is 1cm, the inner cavity width of the main tank body is 3.5cm, the length of the main tank body is 80cm, the anode plate is a diamond mesh coated titanium electrode with a thickness of 1.5mm, and the distance between the anode plate and the inner wall of the main tank body is 1.5mm. The spoiler baffle adopts a baffle, and the baffle is installed in fit with the anode plate on the same side. The baffle adopts a louver structure, and a gap of 3mm is left between the two baffles (for accommodating the cathode plate). The cathode plate used in the test is a circuit board, and the length of the circuit board is 60cm, the width is 50cm, and the thickness is 1.5mm. During the electroplating process, the circuit board is placed between the two baffles and reciprocates along the length direction of the main tank body.
[0062] The electroplating solution used in this application example is SkyPlate 628 acid copper electroplating solution from Tiancheng Technology Co., Ltd. The current density during electroplating is 2.5ASD and the electroplating time is 40min. After the electroplating is completed, the copper thickness tester is used to measure the thickness of the copper surface after electroplating; the test method is the copper thickness 85-point measurement method, which measures the copper thickness at each point on the board surface and then uses the formula to calculate the uniformity of the copper thickness.
[0063] The method for calculating the uniformity of copper thickness using the formula is as follows:
[0064] Use a copper thickness gauge to measure the copper thickness at designated points on the copper surface, and then use the corresponding statistical formula to calculate the CoV value. Generally, CoV≤10% is required, and the surface uniformity of the copper surface is acceptable.
[0065] CoV is defined as follows:
[0066]
[0067]
[0068]
[0069] Among them, X i is the measured value of each measuring point, is the average value of each measurement, and n is the number of measurement points.
[0070] The method for selecting the measuring points of the 85-point copper thickness measurement method described in this application example is as follows: Figure 2As shown in the figure, the length of the circuit board is L and the width is W. In the longitudinal direction of the circuit board: 15mm, L / 16, L / 8, 3L / 16, L / 4, 5L / 16, 3L / 8, 7L / 16, L / 2, 9L / 16, 5L / 8, 11L / 16, 3L / 4, 13L / 16, 7L / 8, 15L / 16 and L-15 respectively represent the distances between the selected measuring points and the top of the circuit board; along the transverse direction of the circuit board: 15mm, W / 4, W / 2, 3W / 4 and W-15 respectively represent the distances between the selected measuring points and the left side of the circuit board. The copper thickness measurement values of each point are shown in Table 1:
[0071] Table 1 (unit, μm)
[0072] 15mm W / 4 W / 2 3W / 4 W-15 15mm 37.44 37.41 37.37 37.43 37.47 L / 16 37.23 37.11 36.51 36.73 37.35 L / 8 37.24 36.73 36.19 36.53 37.36 3L / 16 37.25 36.55 36.13 36.48 37.29 L / 4 37.21 36.48 35.37 36.27 37.25 5L / 16 37.22 36.31 35.41 35.32 37.23 3L / 8 37.21 35.69 35.33 35.77 37.24 7L / 16 37.23 35.33 35.12 35.37 37.22 L / 2 37.19 35.27 35.02 35.27 36.91 9L / 16 37.29 35.39 35.14 35.44 37.3 5L / 8 37.24 35.47 35.35 35.41 37.31 11L / 16 37.25 35.45 35.34 35.46 37.34 3L / 4 37.22 36.44 35.34 35.98 37.33 13L / 16 37.31 36.53 35.67 36.35 37.36 7L / 8 37.27 36.73 36.29 36.51 37.41 15L / 16 37.21 37.35 36.61 36.67 37.46 L-15 37.46 37.43 37.44 37.47 37.85
[0073] It can be calculated from the above table that σ = 0.83, average copper thickness = 36.58 μm, and CoV = 2.3%, which meets the requirements for electroplating uniformity.
[0074] The electroplating device of the present invention is provided with a main tank body of the electroplating device as a shell with upper and lower openings, wherein the electroplating solution enters the shell from the upper opening of the shell and flows out from the lower opening of the shell under the action of gravity, and a spoiler device is provided between the anode plate and the electroplating space accommodating the cathode plate, so that the electroplating solution flowing through the shell under the action of gravity generates turbulence, thereby achieving the technical effect of jet flow; the device of the present invention uses a spoiler baffle to replace the jet flow device, so that the distance between the cathode plate and the anode plate can be significantly reduced, and the narrow flow channel increases the flow rate of the electroplating solution, further enhancing the effect of turbulence. Moreover, the reduction in the distance between the anode and cathode plates makes the distribution of the electric lines more uniform, thereby making the current on the cathode plate more uniform, fundamentally solving the problem of uneven thickness of the electroplating layer on the cathode plate.
[0075] The applicant declares that the above is only a specific implementation mode of the present invention, but the protection scope of the present invention is not limited thereto. Those skilled in the art should understand that any changes or substitutions that can be easily thought of by those skilled in the art within the technical scope disclosed by the present invention shall fall within the protection scope and disclosure scope of the present invention.
Claims
1. A VCP electroplating device, It is characterized in that The device comprises a main tank body (1), the main tank body (1) being a shell with upper and lower openings; two anode plates (2) are arranged in the shell along the opening direction, and an electroplating space for accommodating a cathode plate is provided between the two anode plates; a spoiler baffle (4) is provided between the anode plate (2) and the electroplating space for accommodating the cathode plate (3); The lower end opening of the shell is connected to the auxiliary groove (5); The secondary tank (5) stores the electroplating solution; The lower end of the auxiliary tank (5) is connected to a centrifugal pump (6); A flow regulating device is provided at the lower opening of the shell; The flow regulating device comprises a leakage flow regulating plate (7); The upper opening of the shell is connected to the liquid collecting device; The liquid collecting device comprises a liquid collecting tray (8); The liquid collecting tray (8) is in communication with the centrifugal pump (6); The method of using the VCP electroplating device is as follows: During the electroplating process, the cathode plate is placed between two anode plates, which are denoted as anode plate A and anode plate B. Meanwhile, spoiler baffles are provided between anode plate A and cathode plate and between anode plate B and cathode plate. The electroplating solution is added from the upper opening of the shell and flows out from the lower opening of the shell due to gravity. Thereby completing the electroplating process.
2. The device according to claim 1, It is characterized in that The two anode plates (2) are arranged in parallel.
3. The device as claimed in claim 2, It is characterized in that The two anode plates (2) are arranged opposite to each other.
4. The device according to claim 1, It is characterized in that The housing comprises a rectangular parallelepiped housing.
5. The device according to claim 1, It is characterized in that The anode plate (2) extends along the length direction of the shell.
6. The device according to claim 1, It is characterized in that The length of the shell is 2-100m.
7. The device according to claim 1, It is characterized in that The shell is formed by splicing n segments along the length direction.
8. The device according to claim 7, It is characterized in that The length of the segments is 1-4 m.
9. The device according to claim 7, It is characterized in that Said n≥1.
10. The device according to claim 1, It is characterized in that The width of the shell is 5.5-10 cm.
11. The device according to claim 10, It is characterized in that The width of the shell is 5.5-6.5 cm.
12. The device according to claim 11, It is characterized in that The width of the housing is 5.5 cm.
13. The device according to claim 1, It is characterized in that The height of the shell is 20-90 cm.
14. The device according to claim 13, It is characterized in that The height of the shell is 60-80 cm.
15. The device according to claim 14, It is characterized in that The height of the shell is 70 cm.
16. The device according to claim 1, It is characterized in that The distance between the two anode plates is 1-6 cm.
17. The device according to claim 16, It is characterized in that The distance between the two anode plates is 2 cm.
18. The device according to claim 1, It is characterized in that An electroplating space for accommodating a cathode plate is provided in the middle of the two anode plates (2).
19. The device according to claim 18, It is characterized in that The electroplating space accommodating the cathode plate is arranged in parallel with the anode plate (2).
20. The device according to claim 19, It is characterized in that The electroplating space accommodating the cathode plate is arranged directly opposite to the anode plate (2).
21. The device according to claim 1, It is characterized in that The spoiler baffle (4) is symmetrically arranged between the anode plate (2) and the electroplating space accommodating the cathode plate (3).
22. The device according to claim 1, It is characterized in that The device also includes a conductive track, which is used to place the cathode plate (3) into the electroplating space accommodating the cathode plate.
23. The device according to claim 22, It is characterized in that A conductive clamp is provided on the conductive track, and the conductive clamp is used to connect the cathode plate (3).