On-site testing device for bonding strength between shotcrete and surrounding rock

By designing the assembled steel mold and reaction frame device, the problem of inconsistent fixation and stress of the specimen during the bond strength testing of shotcrete and surrounding rock was solved, achieving more accurate and efficient bond strength testing, which is suitable for vertical rock walls. on-site inspection.

CN109959606BActive Publication Date: 2024-10-29SINOHYDRO BUREAU 12 CO LTD
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
CN201910354257.X
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2019-04-29
Publication Date
2024-10-29
Estimated Expiration
2039-04-29

AI Technical Summary

Technical Problem

The existing bonding strength testing method between shotcrete and surrounding rock has problems such as specimen molding, inconsistent stress, base surface requirements, and unsuitable testing instruments, which causes the testing results to deviate from the true value and cannot accurately reflect the actual bonding strength, affecting the project. Quality acceptance.

Method used

Design a device that includes an assembled steel mold, a reaction frame and a dowel rod. The dowel rod is fixed at the center of the specimen by assembling the steel mold, ensuring that the dowel rod is perpendicular to the bonding surface, and the reaction frame and jack are used to achieve normal alignment. Force transmission solves the problems of specimen fixation and force deviation.

Benefits of technology

It improves the success rate and accuracy of bond strength testing, is suitable for testing on vertical rock walls, and reduces labor intensity and equipment operation complexity.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN109959606B_ABST
    Figure CN109959606B_ABST
Patent Text Reader

Abstract

The present invention relates to a device for testing the bonding strength between shotcrete and surrounding rock on site, comprising an assembled steel mold, a reaction frame, a force transfer rod, and a jack. One end of the force transfer rod is fixed in the assembled steel mold, and the reaction frame and the center of the jack pass through the other end of the force transfer rod and are sequentially sleeved on the force transfer rod. The test device and test method for testing the bonding strength between shotcrete and surrounding rock on site of the present invention overcome the problem that there is no fixed support on site and it is difficult to set up the force transfer rod, so that the test can be carried out smoothly and effectively. The test method is particularly suitable for vertical rock walls where supports cannot be set up. In addition, the reaction frame and the steel mold structure provided in the present invention enable the force transfer rod to be located at the center of the test piece and perpendicular to the bonding surface. The positive force is transmitted between the force transfer rod and the bonding test piece, ensuring that the bonding test piece is subjected to positive force, thereby ensuring the success rate and accuracy of the bonding strength test.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the field of engineering construction, and specifically relates to a device and a test method for testing the bonding strength of shotcrete and surrounding rock on site in water conservancy and hydropower, highway, railway engineering and the like. Background Art

[0002] Shotcrete is a common construction method for tunnel and cavern support, and the bond strength test of shotcrete is an important means of shotcrete quality inspection. At present, the Technical Specifications for Anchor and Shotcrete Support of Water Conservancy and Hydropower Engineering (SL377-2007), the Technical Specifications for Rock and Soil Anchor and Shotcrete Support Engineering (GB50086-2015), and the Construction Specifications for Anchor and Shotcrete Support of Hydropower and Water Conservancy Engineering (DL / T 5181-2017) all have corresponding provisions for the test methods of shotcrete bond strength. The bond strength test methods in these specifications are roughly the same. After summarization, there are three main test methods: 1. Reserved specimen pull-out method, 2. Drill core pull-out method, and 3. Indoor splitting method of shotcrete slab. The test objectives are mainly two points: 1. The force is basically consistent with the bond force of on-site shotcrete, and 2. The test viscosity meets the requirements. However, the three methods currently have defects in specimen molding, specimen force, base surface requirements, test instruments, and test methods.

[0003] 1) On-site core drilling and pulling method

[0004] When drilling cores in the field, the swing of the drill disturbs and damages the concrete specimens; it is difficult to ensure that the loading is not eccentric when drilling holes and burying tie rods or using epoxy resin to stick the pull heads; insufficient thickness of the spray layer can easily cause stress concentration. The above factors will cause the axial tensile bond strength obtained by the field core pulling method to be too small, so the test results of this method cannot truly reflect the bonding between the shotcrete and the surrounding rock. In addition, when the surrounding rock integrity of the random core drilling on site is poor, the core sample is prone to breakage during the core drilling, resulting in a low success rate of the field core drilling method.

[0005] 2) Spraying large plate splitting method

[0006] There is shearing phenomenon during the splitting test, which leads to a higher splitting bond strength obtained by the shotcrete splitting method. In addition, the selection of rock blocks for shotcrete at the construction site cannot fully reflect the actual situation on site, and is inconsistent with the actual bonding situation between shotcrete and surrounding rock.

[0007] 3) Reserved specimen pulling method

[0008] Shotcrete is mixed with an accelerator, and the strength of concrete develops very quickly after spraying. It is difficult to dig a 50mm wide annular groove, which is labor-intensive and time-consuming, and may also damage the reserved specimen. Moreover, it is difficult to ensure that the steel tie rod is not eccentric when the steel tie rod is embedded before spraying concrete and fixed on the rock surface. When the spray layer is thicker, the reserved specimen is heavier, and the bonding strength between the newly sprayed concrete and the surrounding rock is low, so it is likely that the specimen cannot be supported, resulting in test failure and no bonding strength test results.

[0009] In summary, the three current detection methods all have some problems to a greater or lesser extent. The test values ​​deviate from the true values, and the bonding strength test values ​​cannot truly reflect the actual bonding strength conditions. As a result, the project quality cannot pass the acceptance due to the test errors based on the actual situation on site, and the data is falsified in order to pass the acceptance.

[0010] In addition, the main difficulties of on-site bonding tests are:

[0011] 1 Most of them are installed on vertical rock walls, and it is difficult to fix the specimens.

[0012] 2. There is no fixed support on site, and it is difficult to erect the force transfer rod. Even if it is installed with difficulty, it will be deflected by the high-speed sprayed concrete during spraying.

[0013] 3 It is difficult to find a test surface with good flatness on site. The flatness is poor after spraying, and it is difficult to align the reaction frame.

[0014] 4. The jacks and reaction frames are heavy and require multiple people to support the equipment during on-site operation, which is labor-intensive. Summary of the invention

[0015] In order to overcome the above-mentioned problems, the present invention provides a new device and test method for on-site testing of the bond strength of shotcrete and surrounding rock. A new reaction frame is designed to fix the force transfer rod, so that the force transfer rod is located at the center of the specimen and perpendicular to the bonding surface, and a new steel mold is designed to fix the bonding strength specimen. This solves the problem of difficulty in fixing the specimen and overcomes the problem of test failure caused by the specimen being unable to accept the positive force.

[0016] Specifically, the present invention provides the following technical solutions:

[0017] A device for testing the bonding strength of shotcrete and surrounding rock on site comprises an assembled steel mold, a reaction frame, a force transfer rod and a jack. One end of the force transfer rod is fixed in the assembled steel mold, and the reaction frame and the center of the jack pass through the other end of the force transfer rod and are sleeved on the force transfer rod in sequence.

[0018] Some preferred implementations further include a ball joint and a nut sleeved on the force transmission rod; the reaction frame and the jack are fixedly locked on the force transmission rod through the ball joint and the nut.

[0019] In some preferred embodiments, the assembled steel mold includes two semi-cylindrical templates and a sleeve, and the outer wall of the sleeve is connected to a cross-symmetrical wing plate; the two semi-cylindrical templates are spliced ​​into a cylindrical steel mold, and a connecting plate with thread holes is welded to the outer side of the cross-symmetrical wing plate, and the cross-symmetrical wing plate is connected to the inner wall of the cylindrical template through the connecting plate; the semi-cylindrical template has an installation hole corresponding to the connecting plate.

[0020] In some preferred embodiments, after the semi-cylindrical templates are spliced ​​into a cylindrical steel mold, a sleeve with a cross-wing plate is placed in the cylindrical steel mold, the thread holes of the connecting plate are docked with the mounting holes on the cylindrical steel mold, and the mounting holes and thread holes are locked with countersunk screws.

[0021] In a specific implementation manner, the spliced ​​cylindrical steel mold is fixed by locking the mounting holes and the thread holes with countersunk screws.

[0022] In some preferred embodiments, the sleeve has a slot, and one end of the force transmission rod is inserted into the slot and fixedly connected with the sleeve. In a specific embodiment, the slot is provided with an internal thread; one end of the force transmission rod is a threaded structure; the force transmission rod is fixed in the slot through the internal thread and the threaded structure.

[0023] The assembled steel mold is suitable for on-site assembly and is easy to operate. In addition, the steel mold can make the force transmission rod perpendicular to the rock and concrete specimens, ensuring the success and efficiency of the on-site bond strength test.

[0024] In some preferred embodiments, the reaction frame includes a base plate, a bearing plate, a plurality of screw rods connecting the base plate and the bearing plate, and an upper nut and a lower nut sleeved on the screw rods and respectively located above and below the bearing plate.

[0025] In some preferred implementations, the base plate and the load-bearing plate are annular structures; the centers of the annular structures of the base plate and the load-bearing plate pass through the force transmission rod.

[0026] In some preferred embodiments, a groove is provided at the center of the bearing plate, and the diameter of the groove is larger than the inner diameter of the bearing plate ring; the bottom of the jack is located in the groove of the bearing plate to fix the jack to the reaction frame.

[0027] The reaction frame can make the jack and the force transmission rod installed on the reaction frame coaxial, thereby ensuring that the force of the bonding strength test does not deviate; and the reaction frame can be disassembled into several parts, which is easy to carry and install.

[0028] On the other hand, the present invention also provides a test method for on-site detection of the bonding strength between shotcrete and surrounding rock, comprising the following steps:

[0029] 1) Make an assembled steel mold for forming the shotcrete specimen, and a reaction frame for connecting the specimen and the force transfer rod;

[0030] 2) Select the field test area: select a rock surface with an area of ​​500mm×500mm as the test area; select the 300mm×300mm range in the center of the test area as the test point; remove the dust, slag and loose rock blocks on the surface of the surrounding rock in the test area, so that the flatness of the test point is no more than 10mm, and the flatness outside the test point is no more than 30mm;

[0031] 3) Make at least three test specimens of shotcrete and surrounding rock bonding at the test site;

[0032] 4) The specimens were naturally cured for 28 days;

[0033] 5) Conduct tensile bond strength tests on the three specimens respectively;

[0034] 6) Test result determination:

[0035] (1) The average value of the tensile bond strength test of the three specimens is taken as the test result of the tensile bond strength;

[0036] (2) When the difference between the strength test value of one of the specimens and the average value is greater than 20% of the average value, the average strength value of the remaining two specimens shall be taken as the test result;

[0037] (3) The arithmetic mean of the bond strength test values ​​of the three specimens shall be taken as the test result. When the difference between the bond strength test values ​​of two specimens and the average value is greater than 20% of the average value, three more specimens shall be added and the test results of the six specimens shall be calculated together. When the difference between the bond strength test values ​​of no more than two specimens and the average value is greater than 20% of the average value, the two test values ​​shall be eliminated and the average strength value of the remaining specimens shall be taken as the test result. When the difference between the bond strength test values ​​of more than two specimens and the average value is greater than 20% of the average value, the test is invalid. The reason shall be analyzed and the test site shall be re-selected for re-testing.

[0038] In some preferred embodiments, the assembled steel mold includes two semi-cylindrical templates and a sleeve, and the outer wall of the sleeve is connected to a cross-symmetrical wing plate; the two semi-cylindrical templates are spliced ​​into a cylindrical steel mold, and a connecting plate with thread holes is welded to the outer side of the cross-symmetrical wing plate, and the cross-symmetrical wing plate is connected to the inner wall of the cylindrical template through the connecting plate; the semi-cylindrical template has an installation hole corresponding to the connecting plate.

[0039] In some preferred embodiments, the reaction frame includes a base plate, a bearing plate, a plurality of screw rods connecting the base plate and the bearing plate, and an upper nut and a lower nut sleeved on the screw rods and respectively located above and below the bearing plate.

[0040] In some preferred embodiments, the test piece preparation in step 3) specifically includes the following steps:

[0041] (1) Align and close the two semi-cylindrical templates to form a cylindrical template, then place the sleeve with the cross wing plate in the cylindrical steel mold, so that the thread holes of the connecting plate are connected with the mounting holes on the cylindrical steel mold, and lock the mounting holes and thread holes with countersunk screws to complete the assembly of the assembled steel mold;

[0042] (2) Paste a circle of 20mm thick extruded board or pearl cotton board or other isolation materials on the outside of the cylindrical template;

[0043] (3) Fill the pits on the surface of the surrounding rock at the test point;

[0044] (4) Drive an expansion bolt at each end of the central axis of the test point, and use steel wire to fix the assembled steel mold at the test point. The steel wire is clamped on the upper surface of the assembled steel mold, and the steel wire is tightened to ensure that the steel mold will not loosen;

[0045] (5) Screw the blind screw into the socket of the sleeve to prevent the shotcrete from entering the sleeve;

[0046] (6) When spraying concrete into the assembled steel formwork, stop spraying when the spraying thickness reaches the outer edge of the assembled steel formwork. Scrape the concrete in the test area with a scraper to make it level. The thickness should be flush with the outer edge of the assembled steel formwork.

[0047] In some preferred embodiments, the tensile bond strength test in step 5) specifically comprises the following steps:

[0048] (1) After the specimen is cured, remove the isolation material pasted on the outside of the assembled steel mold, cut the steel wire that fixes the assembled steel mold, and unscrew the blind screws in the socket;

[0049] (2) Insert one end of the force transmission rod into the socket of the sleeve and fix it;

[0050] (3) Drill a hole on the sprayed concrete surface at the distance from the center of the reaction frame bottom plate to the hanging hole at the position just above the force transmission rod, insert the steel bar, pass the reaction frame bottom plate through the other end of the force transmission rod and hang the hanging hole of the bottom plate on the steel bar at the same time; install four screws on the bottom plate, put the upper and lower nuts on the screws, pass the pressure plate through the other end of the force transmission rod, and put the pressure plate on the four screws at the same time, and finally put the upper nuts on the screws; press the reaction frame lightly to make the bottom plate of the reaction frame close to the concrete surface in the assembly formwork, use a T-square to lean against the pressure plate, adjust the upper and lower nuts of the screws, make the pressure plate perpendicular to the force transmission rod, and then tighten the upper and lower nuts;

[0051] (4) Install the jack, pass the other end of the force transmission rod through the center hole of the jack, gently push the jack in, make the bottom of the jack fall into the groove on the pressure plate, support the jack with a lute support, make the force transmission rod be located at the center of the center hole of the jack;

[0052] (5) Put the hollow ball joint and nut on the other end of the force transmission rod, tighten the nut, and fix the reaction frame, jack, and ball joint on the force transmission rod in sequence;

[0053] (6) Slowly apply a tensile force to the force transfer rod at a rate of 10 kN / min until the specimen in the steel mold is destroyed and record the failure load.

[0054] In some preferred implementations, in order to ensure safety and prevent objects from falling and injuring people after the specimen is destroyed, the steel bars and the force transmission rods of the hanging holes are connected by steel ropes.

[0055] Beneficial Effects

[0056] The test device and test method for on-site detection of the bonding strength between shotcrete and surrounding rock of the present invention overcome the problem of difficulty in setting up the force transfer rod due to the lack of fixed support on site, so that the test can be carried out smoothly and effectively. The test method is particularly suitable for vertical rock walls where support cannot be set up. In addition, the reaction frame and steel mold structure provided in the present invention enable the force transfer rod to be located at the center of the specimen and perpendicular to the bonding surface, and the positive force is transmitted between the force transfer rod and the bonding specimen, ensuring that the bonding specimen is subjected to positive force, thereby ensuring the success rate and accuracy of the bonding strength test. BRIEF DESCRIPTION OF THE DRAWINGS

[0057] Figure 1 It is a schematic diagram of the cylindrical steel mold of the present invention.

[0058] Figure 2 It is a schematic diagram of a sleeve with a cross wing plate according to the present invention.

[0059] Figure 3 It is a schematic diagram of the cross section BB of the sleeve with the cross wing plate of the present invention.

[0060] Figure 4 It is a structural schematic diagram of the assembled steel mold of the present invention.

[0061] Figure 5 It is a schematic diagram of the AA section of the assembled steel mold of the present invention.

[0062] Figure 6 This is a top view of the steel formwork fixed on the surrounding rock (experimental surface).

[0063] Figure 7 It is a structural schematic diagram of the reaction frame of the present invention.

[0064] Figure 8 It is a schematic diagram of the base of the present invention.

[0065] Fig. 9 It is a side view of the base of the present invention.

[0066] Fig.10 It is a schematic diagram of the bearing plate of the present invention.

[0067] Fig.11 It is a side view of the bearing plate of the present invention.

[0068] Fig.12 It is a schematic diagram of the steel formwork of the present invention being fixed on the surrounding rock.

[0069] Fig.13 The schematic diagram of the device for testing the bonding strength between shotcrete and surrounding rock on site according to the present invention is that the steel formwork and surrounding rock are fixed and then the concrete is shotcreted.

[0070] Fig.14 The present invention is a schematic diagram of a device for testing the bonding strength between shotcrete and surrounding rock on site after the steel mold and shotcrete are separated and the blind bolts are unscrewed.

[0071] Fig.15 The present invention is a schematic diagram of the connection between the steel mold and the force transmission rod of the device for on-site testing of the bonding strength between shotcrete and surrounding rock.

[0072] Fig.16 The present invention is a schematic diagram of a device for testing the bonding strength between shotcrete and surrounding rock on site.

[0073] Fig.17A and Fig. 17B This is a schematic diagram of the ball joint seat.

[0074] Fig.18A and Fig.18B Schematic diagram of the ball joint lower seat.

[0075] Reference numerals

[0076] Assembled steel mold 200, semi-cylindrical template 210, edge 211 on one side of the template, edge 212 on the other side of the template, wire groove 213, sleeve 220, cross-symmetrical wing plate 221, socket 222, isolation material 240, expansion bolt 270, steel wire 260, blind screw 280, reaction frame 100, base 110, connector 111, base hanging part 112, hanging hole 113, load-bearing plate 120, groove 121, through hole 122, stiffening rib 123, screw 130, concrete 300, concrete specimen 320, concrete and concrete specimen spacer 310, surrounding rock 400, force transmission rod 500, jack 600, ball joint 700, ball joint upper seat 710, ball joint lower seat 720, nut 900 DETAILED DESCRIPTION

[0077] The following further describes the structures or technical terms used in the present invention. In the following detailed description, the reference text attached to the legend is a part of this part, which is described in the way of illustrating the specific specific scheme that the present invention may be implemented. We do not exclude that the present invention can also implement other specific schemes and change the structure of the present invention without violating the scope of use of the present invention.

[0078] like Figure 1-5 As shown, the spliced ​​steel mold 200 for on-site testing of the bonding strength between shotcrete and rock of the present invention comprises two semi-cylindrical templates 210, which are enclosed into a cylindrical steel mold. The cylindrical steel mold is used to receive shotcrete and form a test piece after curing.

[0079] The splicing steel mold 200 also includes a sleeve 220, which is used to receive the dowel rod, so there is a socket 222 inside the sleeve 220, and the socket is provided with an internal thread for connecting the dowel rod with threaded threads. In a specific embodiment, the bottom of the sleeve 220 has an enlarged head 226 with a diameter of 50-56 mm, specifically 52 mm. The sleeve has a diameter of 40 mm, the socket has a diameter of 25 mm, and a depth of 58 mm.

[0080] A cross-symmetrical wing plate 221 is connected to the outer wall of the sleeve 220, and the cross-symmetrical wing plate 221 is used to fix the sleeve 220 to the cylindrical steel mold. In a specific embodiment, two semi-cylindrical templates 210 are butt-jointed to form the outer wall of the steel mold 200, and the mounting hole 211 of the outer wall 200 is aligned with the thread hole 224 of the connecting plate 223 at the end of the cross-wing plate 221, and the countersunk screw 225 is screwed on to complete the assembly.

[0081] In the present invention, the outer wall of the steel mold is provided with a mounting hole 211, which can be fixed to the connecting plate 223 of the wing plate 221. Once assembled, the force direction of the pull rod is fixed and is no longer disturbed by the impact force of the shotcrete during the construction process.

[0082] In some embodiments, the diameter of the spliced ​​cylindrical template 200 is Φ200 mm, and the height of the cylindrical template 200 is between 70-100 mm.

[0083] When in use, firstly, the two semi-cylindrical templates 210 are correspondingly spliced ​​together to enclose the cylindrical template 200. The cross-symmetrical wing plate 221 is placed in the cylindrical template 200, and the thread hole 224 on the connecting plate 223 of the wing plate 221 is aligned with the mounting hole 211 of the cylindrical template 200, and the countersunk screw 226 is screwed on to complete the assembly. When used to fix on the test surface, Figure 6As shown, two expansion bolts 270 are installed on both sides of the steel mold 200, and the expansion bolts 270 are connected with steel wires 260 to press the steel mold 200, so that the steel mold 200 can be fixed to the test surface.

[0084] like Figure 7-11 As shown, the reaction frame 100 for on-site testing of the bonding strength between shotcrete and rock of the present invention includes a base plate 110 and a bearing plate 120, and the base plate 110 and the bearing plate 120 are connected by screws 130 and nuts. Among them, there are multiple screws 130, which are connected at the edges of the base plate 110 and the bearing plate 120. Specifically, there are multiple screw bases 111 on the base plate 110 for plugging and fixing the screws, and the multiple screw bases 111 are evenly distributed around the base plate 110. In a specific embodiment, there are 4 screws, and the corresponding screw bases are also 4. The screw 130 is fixed after being inserted into the screw base 111. A plurality of through holes 122 for sleeve screws are evenly distributed around the bearing plate 120, wherein the position of the through hole 122 corresponds to the position of the screw base 111 on the base plate, so as to ensure that the screw 130 is in a vertical state after connecting the base plate 110 and the bearing plate 120. In a specific embodiment, the number of through holes is 4. After the lower nut 140 is first sleeved on the screw rod 130, the load-bearing plate 120 is sleeved through the through hole 122, and finally the upper nut 150 is sleeved on the screw rod 130. In this way, by adjusting the position of the upper and lower nuts 140 / 150 on each screw rod 130, the upper and lower positions of the load-bearing plate 120 on the screw rod 130 can be adjusted, and the angle of the load-bearing plate 120 relative to the vertically erected screw rod 130 can be slightly adjusted, so that the jack and the force transmission rod located on the load-bearing plate 120 can be coaxially stressed.

[0085] In some specific embodiments, the bottom plate 110 is a circular ring structure, and the screw base 111 is evenly located on the ring. The screw base 111 has a depression in the middle, and the depression is used to receive and fix the bottom of the screw 130.

[0086] In one embodiment of the present invention, there are four screw rods 130, screw rod base 111 and through holes 122, and these components correspond to each other and are connected. In some embodiments, the screw rod 130 has a size of Φ25×140 mm.

[0087] The bearing plate 120 is also a circular ring structure. The outer diameter of the ring of the bottom plate 110 and the bearing plate 120 is the same, and the inner diameter of the ring of the bearing plate 120 is smaller than the inner diameter of the ring of the bottom plate 110. In some specific embodiments, the outer diameter of the ring of the bottom plate 110 and the bearing plate 120 is Φ320mm; the inner diameter of the ring of the bearing plate 120 is Φ50mm, and the inner diameter of the ring of the bottom plate 110 is Φ260mm. The through holes 122 are evenly distributed at the edge of the circular ring bearing plate 120.

[0088] A groove 121 is provided at the center of the bearing plate 120, and the diameter of the groove 121 is larger than the inner diameter of the ring of the bearing plate 120. In one embodiment, the diameter of the groove 121 is Φ100 mm.

[0089] In a specific embodiment, a plurality of stiffening ribs 123 are evenly fixed on the upper surface of the bearing plate 120 . The stiffening ribs 123 are located between the grooves 121 and the through holes 122 .

[0090] The bottom plate 110 is also provided with an ear plate 112 protruding from the edge of the bottom plate, and a hanging hole 113 is provided in the middle of the ear plate. The hanging hole 112 is used for hanging on the concrete specimen during the initial process of installing the reaction frame 100 during the bonding strength test.

[0091] When in use, a hole with a depth of 150mm and a diameter of Φ20 is made on the surface of the concrete specimen, and a steel bar is inserted. The hanging hole 113 of the bottom plate of the reaction frame is hung on the steel bar, four pressure-bearing screws 130 are installed on the bottom plate 110, and the pressure plate 120 is put on. The reaction frame 100 is gently pressed by hand to make it close to the concrete surface, and a T-square is leaned against the pressure plate 120. The nuts 140 and 150 of the pressure-bearing screw are adjusted to make the pressure plate 120 perpendicular to the force transmission rod and then the nuts are tightened. The jack is installed, and the force transmission rod passes through the center hole of the jack. The jack is gently pushed in so that the bottom of the jack falls into the circular groove 121 on the pressure plate. The jack is supported by a lute support so that the force transmission rod is located at the center of the center hole of the jack.

[0092] The device for testing the bonding strength between shotcrete and surrounding rock on site of the present invention is as follows: Figure 12-16As shown, in addition to the assembly template 200 and the reaction frame 100, it also includes a force transmission rod 500 and a jack 600. The force transmission rod 500 is used to transmit force to the test piece 320. Therefore, one end of the force transmission rod 500 is inserted into the splicing steel mold 200 and forms an integral body with the test piece 320 in the steel mold 200. Specifically, one end of the force transmission rod is inserted into the socket 222 of the sleeve of the splicing steel mold and fixed. In some specific embodiments, the socket 222 is provided with an internal thread, and one end of the force transmission rod 500 has a thread. The force transmission rod 500 is inserted into the socket 222, and the force transmission rod 500 is fixed on the sleeve 220 through the engagement of the thread and the internal thread. Then, the bottom plate 110 and the bearing plate 120 of the reaction frame 100 pass through the force transmission rod 500 through the center of the ring. The jack 600 is sleeved on the force transmission rod 500 and is fixedly connected to the reaction frame 100 at the same time. Specifically, after the other end of the force transmission rod 500 passes through the center hole of the jack 600, the bottom of the jack 600 falls into the groove 121 of the pressure plate, and the jack 600 is supported by a lute support, and the force transmission rod 500 is adjusted so that the force transmission rod 500 is located at the center of the center hole of the jack 600. If necessary, the upper and lower nuts 140 and 150 on each screw 130 are adjusted to adjust the upper and lower positions of the bearing plate 120 on the screw 130, and the angle of the bearing plate 120 relative to the vertically erected screw 130 can be slightly adjusted, so that the jack 600 and the force transmission rod 500 located on the bearing plate 120 can be coaxially stressed. The force transmission rod 500 is also sleeved with a ball joint 700 and a nut 900. The ball joint 700 is placed on the other end of the jack 600, and the nut 900 located on the outermost side is tightened to lock the force transmission rod 500 and all parts connected to the force transmission rod. In some embodiments, the ball joint 700 is composed of two parts: a ball joint upper seat 710 and a ball joint lower seat 720, respectively. Fig.17A , Fig. 17B and Fig.18A , Fig.18B As shown, the upper seat of the ball joint falls into the arc surface of the lower seat of the ball joint and can rotate freely, so that the force transmission rod and the pulling force of the jack are automatically aligned.

[0093] In the present invention, the bonding strength test is carried out by using a device for testing the bonding strength of shotcrete and surrounding rock on site. Figure 1-1 8 to describe the specific operation method as follows:

[0094] 1. Preparation of the test device, including the production of an assembled steel mold 200 for forming a shotcrete specimen, and a reaction frame 100 for connecting the specimen 320 and the force transmission rod 500.

[0095] 2. Select the on-site test area, and choose a rock surface with an area of ​​500mm×500mm as the test area; select the 300mm×300mm range in the center of the test area as test point 400; remove the dust, slag and loose rocks on the surface of the surrounding rock in the test area, so that the flatness of the test point is not more than 10mm, and the flatness outside the test point is not more than 30mm.

[0096] 3. Make the shotcrete and surrounding rock bonding test piece 320 on site at the test point 400. The specific operation is as follows:

[0097] (1) Align and close two semi-cylindrical templates 210 to form a cylindrical template 200, then place the sleeve 220 with the cross wing plate 221 in the cylindrical steel mold 200, so that the thread hole 224 of the connecting plate 223 is connected with the mounting hole 211 on the cylindrical steel mold, and the mounting hole 211 and the thread hole 224 are locked with the countersunk screw 226 to complete the assembly of the assembled steel mold 200;

[0098] (2) Paste a circle of 20 mm thick extruded board or pearl cotton board or other insulating material 240 on the outside of the cylindrical template 200;

[0099] (3) Fill the pits on the surface of the surrounding rock at the test point; because the surface of the surrounding rock is undulating after the blasting operation, filling the pits will make the sprayed concrete surface smooth and will not affect the installation of the reaction frame;

[0100] (4) Drive an expansion bolt 270 mm at each end of the central axis of the test point. Figure 7 , fix the assembled steel mold 200 at the test point 400 with a steel wire 260, clamp the upper surface of the assembled steel mold 200 with the steel wire 260, and tighten the steel wire 260 to ensure that the steel mold 200 will not loosen;

[0101] (5) Screw the blind screw 280 into the socket 222 of the sleeve 220 to prevent the sprayed concrete from entering the sleeve 220. Fig.12 ;

[0102] (6) When spraying concrete in the assembled steel mold 200, stop spraying when the spraying thickness reaches the outer edge of the assembled steel mold 200. Use a scraper to scrape the concrete 300 in the test area in time. The thickness should be flush with the outer edge of the steel mold 200. Fig.13 shown.

[0103] 4. Repeat step 3 twice to make two more test pieces 320.

[0104] 5. The specimens were naturally cured for 28 days.

[0105] 6. Conduct tensile bond strength tests on the three test pieces 320 respectively. The specific operation method is:

[0106] (1) After the curing of the test piece 320 is completed, the isolation material 240 pasted on the outside of the assembled steel mold 200 is removed to form a space 310 between the concrete and the concrete test piece, thereby separating the test piece 320 from the rest of the concrete 300 to form a separate test piece 320; the steel wire 260 fixing the assembled steel mold 200 is cut off, and the blind screw 280 in the connecting slot 222 is unscrewed. Fig.14 As shown;

[0107] (2) Insert one end of the force transmission rod 500 into the socket 222 of the sleeve and fix it. Fig.15 As shown;

[0108] (3) At the position directly above the force transmission rod 500, a hole (not shown in the figure) is drilled on the surface of the sprayed concrete 300 according to the distance from the center of the reaction frame bottom plate 110 to the hanging hole 113, and the steel bar is inserted. The reaction frame bottom plate 110 is passed through the other end of the force transmission rod 500 and the hanging hole 113 of the bottom plate is hung on the steel bar; four screw rods 130 are installed on the bottom plate 110, and the upper and lower nuts 140 are put on the screw rods 130. The pressure plate 120 is passed through the other end of the force transmission rod 500, and the pressure plate 120 is sleeved on the four screw rods 130. Finally, the upper nuts 150 are put on the screw rods 130; lightly press the reaction frame 10 0 Make the bottom plate 110 of the reaction frame close to the surface of the concrete 300 and the test piece 320, use a T-square to lean against the pressure plate 120, adjust the upper and lower nuts 140, 150 of the pressure screw 130, make the pressure plate 120 and the force transmission rod 500 perpendicular, and then tighten the upper and lower nuts 140, 150; (4) Install the jack 600, make the other end of the force transmission rod 500 pass through the center hole of the jack 600, gently push the jack 600, make the bottom of the jack 600 fall into the groove 121 on the pressure plate, support the jack 600 with a lute support, and adjust it so that the force transmission rod 500 is located at the center of the center hole of the jack 600;

[0109] (5) Put the hollow ball joint 700 and the nut 900 on the force transmission rod 500, tighten the nut 900, so that the reaction frame 100, the jack 600, and the ball joint 700 are all fixed on the force transmission rod 500; Fig.16 As shown;

[0110] (6) The steel bars of the hanging hole and the force transmission rod 500 are connected by a steel rope (not shown in the figure) to prevent the specimen 320 from falling and injuring people after being damaged;

[0111] (7) Slowly apply a tensile force to the force transmission rod 500 at a speed of 10 kN / min until the test piece 320 in the steel mold 200 connected to the force transmission rod 500 is destroyed, and record the failure load.

[0112] 7. Test result determination:

[0113] (1) The average value of the tensile bond strength test of three specimens 320 should be taken as the test result of the tensile bond strength;

[0114] (2) When the difference between the strength test value of one of the specimens 320 and the average value is greater than 20% of the average value, the average strength value of the remaining two specimens shall be taken as the test result;

[0115] (3) The arithmetic mean of the bond strength test values ​​of the three specimens shall be taken as the test result. When the difference between the bond strength test values ​​of two specimens and the average value is greater than 20% of the average value, three more specimens shall be added and the test results of the six specimens shall be calculated together. When the difference between the bond strength test values ​​of no more than three or two specimens and the average value is greater than 20% of the average value, the two test values ​​shall be eliminated and the average strength value of the remaining specimens shall be taken as the test result. Conversely, when the difference between the bond strength test values ​​of more than two specimens and the average value is greater than 20% of the average value, the test is invalid. The reason shall be analyzed and the test site shall be re-selected for re-testing.

[0116] 8. The experiment is over.

Claims

1. A device for testing the bonding strength between shotcrete and surrounding rock on site, characterized in that: It includes an assembly steel mold, a reaction frame, a force transmission rod, and a jack. One end of the force transmission rod is fixed in the assembly steel mold, and the reaction frame and the center of the jack pass through the other end of the force transmission rod and are sequentially sleeved on the force transmission rod; the reaction frame includes a base plate, a bearing plate, a plurality of screws connecting the base plate and the bearing plate, and an upper nut and a lower nut sleeved on the screws and respectively located above and below the bearing plate; the base plate and the bearing plate are circular ring structures; the center of the ring of the base plate and the bearing plate passes through the force transmission rod; a recess is provided at the center of the bearing plate The groove has a diameter larger than the inner diameter of the bearing plate ring; the bottom of the jack is located in the groove of the bearing plate to fix the jack to the reaction frame; the assembled steel mold includes two semi-cylindrical templates and a sleeve, and the outer wall of the sleeve is connected with a cross-symmetrical wing plate; the two semi-cylindrical templates are spliced ​​into a cylindrical steel mold, and a connecting plate with a thread hole is welded on the outer side of the cross-symmetrical wing plate, and the cross-symmetrical wing plate is connected to the inner wall of the cylindrical template through the connecting plate; the semi-cylindrical template is provided with a mounting hole corresponding to the connecting plate.

2. The device for testing the bonding strength between shotcrete and surrounding rock on site according to claim 1 is characterized in that: It also includes a ball joint and a nut which are sleeved on the force transmission rod; the reaction frame and the jack are fixed and locked on the force transmission rod through the ball joint and the nut.

3. The device for testing the bonding strength between shotcrete and surrounding rock on site according to claim 1 is characterized in that: After the semi-cylindrical templates are spliced ​​into a cylindrical steel mold, the sleeve with the cross wing plate is placed in the cylindrical steel mold, the thread holes of the connecting plate are connected to the mounting holes on the cylindrical steel mold, and the mounting holes and thread holes are locked with countersunk screws.

4. The device for testing the bonding strength between shotcrete and surrounding rock on site according to claim 3 is characterized in that: A connecting slot is provided in the sleeve, and one end of the force transmission rod is inserted into the connecting slot and fixedly connected with the sleeve.

5. The device for testing the bonding strength between shotcrete and surrounding rock on site according to claim 1 is characterized in that: The bottom plate of the reaction frame is also provided with an ear plate protruding from the edge of the bottom plate, and a hanging hole is provided in the middle of the ear plate.

6. The device for testing the bonding strength between shotcrete and surrounding rock on site according to claim 5 is characterized in that: Screw bases for receiving screws are evenly distributed on the bottom plate, and a depression is provided in the middle of the screw bases.

7. The device for testing the bonding strength between shotcrete and surrounding rock on site according to claim 1 is characterized in that: The sleeve is provided with a connecting slot inside, and an internal thread is arranged in the connecting slot; and an enlarged head is arranged at the bottom of the sleeve.

Citation Information

Patent Citations

  • Contact surface bonding strength measurement system

    CN104198374A

  • Hard pull structural piece of steel pipe scaffold

    CN204266573U

  • Device for testing bonding strength of sprayed concrete and surrounding rock on site