A low temperature plasma waste gas treatment device
By adopting a longitudinally arranged anode plate and cooling tube structure in the low-temperature plasma exhaust gas treatment device, and using modified graphite fiber and kaolin fillers, the problems of short device life and insufficient adsorption effect are solved, and efficient exhaust gas treatment and energy consumption reduction are achieved.
Patent Information
- Application Number
- CN201910530303.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2019-06-19
- Publication Date
- 2024-10-22
- Estimated Expiration
- 2039-06-19
AI Technical Summary
The existing low-temperature plasma waste gas treatment device has a short life and is inconvenient to use, and the dielectric constant and adsorption effect of the filler are insufficient, which affects the treatment efficiency and energy consumption.
A low-temperature plasma exhaust gas treatment device including longitudinally arranged anode plates and cooling tubes is designed. Modified graphite fiber and kaolin are used as fillers. The adsorption capacity of the fillers is improved through acidification and surfactant treatment, and the adsorption capacity of the fillers is improved through urea and sodium bicarbonate. Pore agents increase pore size and specific surface area.
It effectively extends the service life of the device, improves waste gas treatment efficiency, reduces energy consumption, enhances the adsorption capacity of organic matter, and reduces the generation of harmful by-products.
Smart Images

Figure CN110180340B_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of environmental protection equipment, relates to sewage treatment, and specifically relates to a low-temperature plasma waste gas treatment device. Background Art
[0002] Low-temperature plasma waste gas treatment is a process in which a large number of energetic electrons generated by dielectric discharge under the action of an external electric field bombard pollutant molecules, causing them to ionize, dissociate and excite, and then triggering a series of complex physical and chemical reactions, which transform complex large molecular pollutants into simple small molecular safe substances, or transform toxic and harmful substances into non-toxic or low-toxic substances, thereby degrading and removing pollutants.
[0003] At present, low-temperature plasma waste gas treatment devices include plasma tubes, which are covered with sleeves on the outside, and cathode and anode electrodes are formed between the plasma tube and the sleeves, and ions are generated through high-voltage discharge. Since the temperature of industrial waste gas is high when it is discharged, the plasma tube and the sleeve cannot be effectively cooled down, and they are easily burned out due to long-term high-temperature operation, and their service life is short; over time, particulate pollutants are easily accumulated in the sleeve, affecting the discharge effect, and it is not convenient to clean, which makes it very inconvenient to use.
[0004] The discharge strength of the plasma waste gas treatment device can affect the removal efficiency and energy utilization of harmful gases. The dielectric constant and adsorption effect of the filler in the reactor have a corresponding relationship with the discharge characteristics. Therefore, fillers with high relative dielectric constant and good adsorption effect can improve the treatment rate and inhibit the generation of harmful by-products. At present, commonly used fillers include microporous γ-Al2O3 spherical particle adsorbents, ceramic adsorbents, barium titanate adsorbents, and negative nano-TiO2 adsorbents. Summary of the invention
[0005] The purpose of the present invention is to solve the technical problems of short life and inconvenient use of low-temperature plasma waste gas treatment devices in the prior art, and to provide a low-temperature plasma waste gas treatment device to solve the shortcomings of the prior art.
[0006] In order to achieve the above object, the present invention adopts the following technical solutions:
[0007] A low-temperature plasma waste gas treatment device comprises a box body; a chamber is arranged in the middle of the box body, and an air inlet and an air outlet connected to the chamber are respectively arranged at two ends of the box body; a plurality of longitudinally parallel anode plates are arranged in the chamber; the two ends of the anode plate are respectively opposite to the air inlet and the air outlet; a plurality of groups of evenly distributed plug holes are arranged on the anode plate; a plasma tube is vertically penetrated through the plug hole; one end of the plasma tube is arranged in the box body, and the other end is fixed by a fixing plate; a high-voltage generator is arranged in the box body; the two poles of the high-voltage generator are respectively connected to the plasma tube and the anode plate by wires and high-voltage connectors.
[0008] Furthermore, the anode plate is made of aluminum plate, and a cooling coil is arranged inside, and the cooling coil is provided with a group of circulation joints on the anode plate.
[0009] Furthermore, the anode plate is a double-layer plate in a sealed arrangement, and the cooling coil is arranged in the middle of the double-layer plate; the anode plate corresponding to the plug-in hole of the plasma tube is sealed with the double-layer plate through a cylindrical collar.
[0010] Furthermore, a conical opening is provided between the air inlet and the air outlet and the chamber respectively; and an air guide plate is provided at the end of the conical opening corresponding to the air inlet.
[0011] Furthermore, a cooling box sleeved on the plasma tube is provided in the chamber; the cooling box is arranged close to the inner wall of the chamber, and is arranged at one end or both ends of the plasma tube; and circulation joints are respectively provided at both ends of the cooling box.
[0012] As another technical solution of the present invention, the chamber is equipped with a filler, which has a high dielectric constant and good adsorption effect, and can improve the waste gas treatment efficiency, reduce the energy consumption of the reactor, and avoid the generation of secondary pollutants;
[0013] Specifically, the filler is prepared according to the following process:
[0014] Step 1) adding chitosan to 5-15 times the weight of acetic acid, stirring and dispersing the chitosan uniformly, and then mixing the chitosan with graphite fiber in a mass ratio of 1-2:2-3, and then placing the mixture at a temperature of 50° C. for 30 minutes to obtain modified graphite fiber;
[0015] Step 2) Filter the kaolin through a 100-mesh sieve, collect the sieve residue, add 3-5 times the weight of 10% hydrochloric acid, stir at 200 rpm for 10-20 min, add 1% by weight of a cationic surfactant, continue stirring at 200 rpm for 10-20 min, and then collect the precipitate by centrifugation to obtain modified kaolin;
[0016] Step 3) adding modified graphite fiber, modified kaolin, urea and ammonium bicarbonate into a reaction kettle in a mass ratio of 20-30:10-20:1-2:1-2, stirring at 300 rpm for 15 min, then entering a drum granulator for granulation, and then drying at 80-90° C. for 30 min to obtain granules;
[0017] Step 4) The particles obtained in step 3) are put into a sintering furnace for sintering at a temperature of 700-800°C, kept at this temperature for 30 minutes, taken out, and naturally cooled to room temperature to obtain a filler.
[0018] Preferably, the chitosan is chitosan with a deacetylation rate of 55-70%.
[0019] Preferably, the concentration of acetic acid is 1%;
[0020] The cationic surfactant is stearamidopropyl dimethylamine lactate or dodecyl trimethyl ammonium chloride.
[0021] Compared with the prior art, the beneficial effects achieved by the present invention mainly include but are not limited to the following aspects:
[0022] The present invention has a reasonable structure. The anode plate is in the shape of a longitudinally arranged plate and is provided with a cooling pipe. The exhaust gas passes through the middle and is not easy to remain. It effectively solves the technical problems of short life and inconvenient use in the prior art. Graphite fiber has properties such as heat resistance, corrosion resistance, high conductivity and non-toxicity. It is modified by chitosan to improve the interfacial bonding strength and provide a plastic interface that can eliminate interfacial internal stress. The tissue compatibility and adsorption capacity are greatly improved. The present invention increases the interlayer spacing of kaolin through acidification and surfactant treatment. At the same time, some cations are adsorbed on the surface, which improves the hydrophobicity and the ability to adsorb organic matter. The present invention uses urea and sodium bicarbonate as pore-forming agents. Through the calcination process, the number of pores and specific surface area are increased, and the adsorption capacity is improved. BRIEF DESCRIPTION OF THE DRAWINGS
[0023] Figure 1 It is a schematic diagram of the top view of the structure of the present invention;
[0024] Figure 2 It is a schematic diagram of the structure of the anode plate of the present invention;
[0025] Figure 3 : Effect of different fillers on toluene removal rate.
[0026] In the figure, 1, box body 2, conical mouth 3, air guide plate 4, anode plate 5, circulation joint 6, fixing plate 7, plasma tube 8, chamber 9, air inlet 10, air outlet 11, cooling box 12, high voltage generator 13, high voltage joint 14, wire 15, plug hole 16, cooling coil. DETAILED DESCRIPTION
[0027] The technical solution of the present invention will be described clearly and completely below in conjunction with the accompanying drawings. In the description of the present invention, it is obvious that the embodiments described below are part of the embodiments of the present invention, rather than all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0028] Example 1
[0029] according to Figure 1 and Figure 2 A low-temperature plasma waste gas treatment device comprises a box body 1; a chamber 8 is arranged in the middle of the box body, and an air inlet 9 and an air outlet 10 connected to the chamber are respectively arranged at two ends of the box body; a plurality of longitudinally parallel anode plates 4 are arranged in the chamber; the two ends of the anode plate are respectively opposite to the air inlet and the air outlet; a plurality of groups of evenly distributed plug holes 15 are arranged on the anode plate; a plasma tube 7 is vertically penetrated on the plug hole; one end of the plasma tube is arranged in the box body, and the other end is fixed by a fixing plate 6; a high-voltage generator 12 is arranged in the box body; the two poles of the high-voltage generator are respectively connected to the plasma tube 7 and the anode plate 4 through a wire 14 and a high-voltage connector 13.
[0030] High-energy electrons are generated between the plasma tube 7 and the anode plate 4. During the operation of the exhaust gas, the pollutant molecules in the exhaust gas are broken down by the electrons and decomposed in a very short time, so that the pollutants can be degraded and removed.
[0031] The anode plate 4 is made of aluminum plate, and a cooling coil 16 is arranged inside. The cooling coil is provided with a group of circulation joints 5 on the anode plate.
[0032] The cooling coil 16 and the circulation joint 5 are made of glass and rubber hose respectively.
[0033] The spacing between adjacent anode plates is 25-35 mm, and the distance between the plasma tube 7 and the side wall of the plug hole 15 is 5-10 mm.
[0034] The anode plate adopts a double-layer plate which is arranged in a sealed manner, and the cooling coil is arranged in the middle of the double-layer plate; the plug-in hole of the anode plate corresponding to the plasma tube is sealed with the double-layer plate through a cylindrical sleeve ring.
[0035] Conical openings 2 are respectively provided between the air inlet and the air outlet and the chamber; and an air guide plate 3 is provided at the end of the conical opening corresponding to the air inlet.
[0036] The chamber is provided with a cooling box 11 sleeved on the plasma tube; the cooling box is arranged close to the inner wall of the chamber and is arranged at one end or both ends of the plasma tube; and circulation joints are respectively arranged at both ends of the cooling box.
[0037] The cooling box is provided with a glass inner wall, and the circulation joint adopts a rubber hose.
[0038] A cleaning channel is provided on the bottom surface of the chamber 8 corresponding to the anode plate.
[0039] The invention has a reasonable structure, the anode plate is in the shape of a longitudinally arranged plate and is provided with a cooling pipe, the exhaust gas passes through the middle and is not prone to residue, which effectively solves the technical problems of short life and inconvenient use in the prior art.
[0040] Example 2
[0041] A filler for a low-temperature plasma waste gas treatment device is prepared according to the following process:
[0042] Step 1) adding chitosan with a deacetylation rate of 55-70% to 10 times the weight of 1% acetic acid, stirring and dispersing the mixture evenly, and then mixing the mixture with graphite fiber at a mass ratio of 1:1, and placing the mixture at 50° C. for 30 minutes to obtain modified graphite fiber;
[0043] Step 2) Filter the kaolin through a 100-mesh sieve, collect the sieve residue, add 3 times the weight of 10% hydrochloric acid, stir at 200 rpm for 10 min, add 1% by weight of stearamidopropyl dimethylamine lactate, continue stirring at 200 rpm for 10 min, and then collect the precipitate by centrifugation to obtain modified kaolin;
[0044] Step 3) adding modified graphite fiber, modified kaolin, urea and ammonium bicarbonate into a reactor in a mass ratio of 20:10:1:1, stirring at 300 rpm for 15 min, and then entering a drum granulator for granulation, controlling the particle size to be 1 mm, and then drying at 90° C. for 30 min to obtain particles;
[0045] Step 4) The particles obtained in step 3) are put into a sintering furnace for sintering at a temperature of 750° C., kept at this temperature for 30 minutes, taken out, and naturally cooled to room temperature to obtain a filler.
[0046] Example 3
[0047] A filler for a low-temperature plasma waste gas treatment device is prepared according to the following process:
[0048] Chitosan with a deacetylation rate of 55-70% is added to 8 times the weight of 1% acetic acid, stirred and dispersed evenly, and then mixed with graphite fiber at a mass ratio of 2:3, and then placed at 50°C for 30 minutes to obtain modified graphite fiber;
[0049] Pass kaolin through a 100-mesh sieve, collect the sieve residue, then add 5 times the weight of 10% hydrochloric acid, stir at 200 rpm for 10 minutes, then add 1% by weight of dodecyltrimethylammonium chloride, continue stirring at 200 rpm for 20 minutes, and then collect the precipitate by centrifugation to obtain modified kaolin;
[0050] The modified graphite fiber, modified kaolin, urea and ammonium bicarbonate were added to the reactor in a mass ratio of 30:15:2:1, stirred at 300 rpm for 15 min, and then put into a drum granulator for granulation, with the particle size controlled to be 2 mm, and then placed at 85°C and dried for 30 min to obtain particles;
[0051] The obtained particles were put into a sintering furnace for sintering at a temperature of 800° C., kept warm for 30 minutes, taken out, and naturally cooled to room temperature to obtain a filler.
[0052] Example 4
[0053] Conventional γ-Al2O3 particles, ceramics, and 4A molecular sieves were used as control fillers, and the filler of the present invention was the filler prepared in Example 2; the performance of the filler of the present invention was verified.
[0054] Toluene gas was used as the test pollutant, and the experimental conditions were: the inlet concentration of toluene was 600 mg / m3, the flow rate was 50 L / h, and the humidity was 10%.
[0055] Select the voltage strength to be 16-22kV, such as Figure 3 As shown, the test conditions of each group are exactly the same. When toluene gas is introduced and voltage is applied at the same time, the influence of voltage and filler on the removal rate is detected. It can be seen that under the same voltage, the removal effect of the filler of the present invention is the best. This is because, compared with conventional fillers, the present invention not only has better adsorption effect, can make organic molecules relatively enriched on its surface, can increase the residence time of toluene in the reaction zone to a certain extent, but also has a higher dielectric constant, strengthens the external electric field, generates a large number of active particles such as strong oxidizing free radicals, and can promote the degradation of pollutants.
[0056] It should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention, rather than to limit it. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that the technical solutions described in the aforementioned embodiments may still be modified, or some of the technical features thereof may be replaced by equivalents. However, these modifications or replacements do not deviate the essence of the corresponding technical solutions from the spirit and scope of the technical solutions of the embodiments of the present invention.
Claims
1. A low-temperature plasma waste gas treatment device, comprising a box; a chamber is provided in the middle of the box, and an air inlet and an air outlet are provided at both ends of the box respectively, which are connected to the chamber; wherein: The chamber is provided with a plurality of anode plates distributed in parallel in the longitudinal direction; the two ends of the anode plate are respectively opposite to the air inlet and the air outlet; the anode plate is provided with a plurality of groups of evenly distributed plug holes; the plug holes are provided with a plasma tube vertically penetrating; one end of the plasma tube is arranged in the box body, and the other end is fixed by a fixing plate; a high-voltage generator is arranged in the box body; the two poles of the high-voltage generator are respectively connected to the plasma tube and the anode plate through wires and high-voltage connectors; The chamber is provided with a filler; The filler is prepared according to the following process: Step 1) adding chitosan to 5-15 times the weight of acetic acid, stirring and dispersing the chitosan uniformly, and then mixing the chitosan with graphite fiber in a mass ratio of 1-2:2-3, and then placing the mixture at a temperature of 50° C. for 30 minutes to obtain modified graphite fiber; Step 2) Filter the kaolin through a 100-mesh sieve, collect the sieve residue, then add 3-5 times the weight of 10% hydrochloric acid, stir at 200 rpm for 10-20 min, then add 1% by weight of a cationic surfactant, continue stirring at 200 rpm for 10-20 min, and then collect the precipitate by centrifugation to obtain modified kaolin; Step 3) adding modified graphite fiber, modified kaolin, urea and ammonium bicarbonate into a reaction kettle in a mass ratio of 20-30:10-20:1-2:1-2, stirring at 300 rpm for 15 min, then entering a drum granulator for granulation, and then placing at 80-90° C. and drying for 30 min to obtain granules; Step 4) putting the particles obtained in step 3) into a sintering furnace for sintering at a temperature of 700-800° C., keeping the temperature for 30 minutes, taking out, and naturally cooling to room temperature to obtain a filler; The chitosan is chitosan with a deacetylation rate of 55-70%, the concentration of acetic acid is 1%, and the cationic surfactant is stearamidopropyl dimethylamine lactate or dodecyl trimethyl ammonium chloride.
2. The low-temperature plasma waste gas treatment device according to claim 1, characterized in that: The anode plate is made of aluminum plate, and a cooling coil is arranged inside. The cooling coil is provided with a group of circulation joints on the anode plate.
3. The low-temperature plasma waste gas treatment device according to claim 1, characterized in that: The anode plate adopts a double-layer plate which is arranged in a closed manner, and the cooling coil is arranged in the middle of the double-layer plate; the plug-in hole of the anode plate corresponding to the plasma tube is sealed with the double-layer plate through a cylindrical sleeve ring.
4. The low-temperature plasma waste gas treatment device according to claim 1 is characterized in that: Conical openings are respectively arranged between the air inlet and the air outlet and the chamber; and an air guide plate is arranged at the end of the conical opening corresponding to the air inlet.
5. The low-temperature plasma waste gas treatment device according to claim 1, characterized in that: A cooling box sleeved on the plasma tube is arranged in the chamber; the cooling box is arranged close to the inner wall of the chamber and is arranged at one end or both ends of the plasma tube; and circulation joints are respectively arranged at both ends of the cooling box.