Plasticized rubber powder forced mixer
By using a forced mixer with extrusion pins and bevel mixing trays in the production of recycled glue, combined with internal and external cooling systems and automatic feeding mechanism, the problems of low efficiency and uneven glue are solved, and high efficiency is achieved. Stable recycled glue production.
Patent Information
- Application Number
- CN201911202556.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2019-11-29
- Publication Date
- 2024-11-19
- Estimated Expiration
- 2039-11-29
AI Technical Summary
Traditional recycled glue refiners have low efficiency, uneven glue materials, difficult to remove glue in the machine, and poor cooling effect, resulting in unstable recycled glue performance, and manual handling leads to high labor intensity and unstable quality.
A forced mixer of plasticized rubber powder is designed, which uses a combination of extrusion pins and inclined mixing plates for cutting, extrusion and mixing. Combined with internal and external cooling systems, the glue can be uniformly cooled and automatically controlled to ensure that the glue can be It operates continuously in a closed state, and realizes continuous feeding and sealing conveying of materials through an automatic feeding mechanism.
It realizes efficient shear, extrusion and mixing of rubber, improves the performance and production efficiency of recycled rubber, reduces energy consumption and labor intensity, and ensures the uniformity and quality stability of rubber.
Smart Images

Figure CN110774473B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to a plasticized rubber powder refining device, in particular to a plasticized rubber powder forced mixing device. Background Art
[0002] The production process of reclaimed rubber is a systematic processing and conversion process for the recycling of waste rubber, which mainly includes a series of complex manufacturing processes such as the crushing of waste tires, grinding and screening, mixing and premixing of rubber powder and auxiliary materials, plasticization (desulfurization) treatment, refining of rubber powder, sheeting and coiling, packaging, storage and transportation of finished rubber. Among them, the refining process of plasticized (desulfurized) rubber powder is an important link in the production process of reclaimed rubber. The refining of traditional reclaimed rubber is completed by a refiner. The rubber powder after plasticization (desulfurization) is repeatedly rolled by multiple refiners to achieve the purpose of refinement and refining.
[0003] The main disadvantages of the refiner in the traditional reclaimed rubber production process are as follows: (1) In order to ensure the refining effect, the refiner needs to be repeatedly extruded 5-7 times to ensure that the reclaimed rubber can reach a good quality. However, this multi-pass processing method has low efficiency, large investment and high energy consumption; (2) There is always a part of the rubber that cannot be discharged in the refiner in the prior art. In order to ensure the quality of the reclaimed rubber during the next operation, it is necessary to discharge the remaining rubber after the machine is shut down. However, due to the complexity of equipment dismantling, the internal rubber temperature decreases after the machine is shut down and dismantled, making it difficult to clean the rubber in the machine, affecting the performance of the equipment; (3) Since the refiner cannot be emptied during use, there is always overlapping rubber in each pass, which makes it difficult to ensure uniformity of the rubber. , which ultimately leads to uneven and unstable performance of the recycled rubber; (4) Due to the requirements of the refining machine on the roller in terms of strength, rigidity, surface hardness and smoothness, the wall thickness of the cast iron roller in the prior art is usually thicker, and the heat conduction of cast iron is poor, and the cooling effect cannot be achieved well; in order to achieve the cooling effect, the line speed must be reduced, which reduces production efficiency and increases production costs; (5) The existing traditional feeding method is to transport the desulfurized rubber powder to the machine next to the on-site rubber refining operation for storage (directly stacked on the ground) waiting for the rubber refining operation, and then the operator uses a shovel or other tools to add it to the rubber refining machine for rolling. During this process, the rubber powder is easily scattered in the workshop and is easily mixed with other impurities, which can easily lead to unstable rubber refining quality, and the labor intensity of manual handling is high. Summary of the invention
[0004] The technical problem to be solved by the present invention is to provide a plasticized rubber powder forced mixer which has good cooling effect and good sealing, solves the problems of uneven rubber material and low efficiency existing in the existing refining machine through one-time refining, and is also convenient for removing the plasticized rubber material in the machine.
[0005] In order to solve the above technical problems, the technical solution of the present invention is: a plasticized rubber powder forced mixer comprises a mixing frame, a mixing barrel is installed on the mixing frame, and a mixing inlet and a mixing outlet are correspondingly arranged at both ends of the mixing barrel, a mixing shaft is rotatably installed in the mixing barrel, one end of the mixing shaft close to the mixing inlet extends out of the mixing barrel and is connected to a mixing driving device, a feeding chamber and a mixing chamber are arranged in the mixing barrel, the outer periphery of the mixing shaft is located in the feeding chamber and a feeding device is installed, the outer periphery of the mixing shaft is located in the mixing chamber and a mixing device is installed, the mixing inlet is arranged above the feeding end of the feeding device, the discharging end of the feeding device is arranged at the feeding end of the mixing device, the mixing outlet is arranged at the discharging end of the mixing device, and the end of the mixing shaft close to the mixing outlet extends out of the mixing barrel and is correspondingly installed with a discharging rotary cutting device.
[0006] As a preferred technical solution, the mixing device includes inclined mixing disks evenly spaced around the outer circumference of the mixing shaft, and a group of pin assemblies are respectively arranged between two adjacent inclined mixing disks. The pin assemblies include extrusion pins evenly installed on the wall of the mixing barrel, and the bottom ends of the extrusion pins extend into the mixing chamber.
[0007] As a preferred technical solution, the extrusion pin includes a mounting portion fixedly mounted on the wall of the mixing barrel, an extrusion stirring portion is provided at the lower end of the mounting portion, the bottom of the extrusion stirring portion extends into between two adjacent inclined mixing disks, and an extrusion plane for receiving and extruding plasticized rubber powder is provided on the extrusion stirring portion; side gaps are respectively provided between the two ends of the extrusion stirring portion and the ends of the inclined mixing disks on both sides, and a bottom gap is provided between the bottom end of the extrusion stirring portion and the outer periphery of the mixing shaft, and both the side gap and the bottom gap gradually increase from the extrusion plane to the rear.
[0008] As a preferred technical solution, the discharging and peeling device includes a split discharging disk that blocks the discharging end of the mixing barrel, the outer end of the split discharging disk is correspondingly provided with a peeling knife installed on the mixing shaft, the mixing shaft is provided with a locking nut that abuts against the outside of the peeling knife, and the mixing shaft is also provided with a positioning block that abuts against the inside of the peeling knife, and the outer circumferential surface of the positioning block cooperates with the inner annular surface of the annular disk body.
[0009] As a preferred technical solution, the split discharge tray includes at least two discharge plates, all of which are spliced together to form a circular tray body, and the surface of any of the discharge plates is evenly distributed with a number of material holes, and all of the material holes are together enclosed to form a circular structure; the edge of any of the discharge plates is evenly distributed with a number of bolt mounting holes, and all of the bolt mounting holes are together enclosed to form a circle.
[0010] As a preferred technical solution, it also includes a cooling system, which includes an external cooling system coated on the outer wall of the mixing barrel and / or an internal cooling system arranged inside the mixing shaft. The heat in the mixing barrel is transferred to the external cooling system through the outer wall of the mixing barrel for external heat exchange and / or the heat in the mixing barrel is transferred to the internal cooling system through the outer wall of the mixing shaft for internal heat exchange.
[0011] As a preferred technical solution, the internal cooling system includes a liquid return chamber which is arranged at the center of the axis of the mixing shaft and is open at one end. The liquid return chamber extends from the feeding end of the mixing barrel to the discharging end of the mixing barrel to the end of the mixing shaft. A liquid inlet pipe with two ends opening is also installed in the liquid return chamber. A liquid gap is provided between the inner end of the liquid inlet pipe and the inner end of the liquid return chamber. A heat conversion joint is installed at the end of the mixing shaft. A liquid inlet port connected to the outer end of the liquid inlet pipe is provided in the heat conversion joint. A liquid return port connected to the liquid return chamber is also provided in the heat conversion joint. An internal circulation pipeline is connected between the liquid inlet port and the liquid return port.
[0012] As an optimal technical solution, the internal circulation pipeline includes an internal cooling water inlet pipeline and an internal cooling water return pipeline. The internal cooling water inlet pipeline is provided with an internal circulation water pump, the internal cooling water return pipeline is provided with an internal circulation electromagnetic throttle valve, and the internal cooling water return pipeline is also provided with an internal circulation temperature sensor.
[0013] As a preferred technical solution, the external cooling system includes an external cooling jacket coated on the outer peripheral wall of the mixing barrel, and a water inlet nozzle and a water return nozzle are respectively provided at both ends of the external cooling jacket, and an external circulation pipeline is connected between the water inlet nozzle and the water return nozzle.
[0014] As an optimal technical solution, the external circulation pipeline includes an external cooling water inlet pipeline and an external cooling water return pipeline. The external cooling water inlet pipeline is provided with an external circulation water pump, the external cooling water return pipeline is provided with an external circulation electromagnetic throttle valve, and the external cooling water return pipeline is also provided with an external circulation temperature sensor.
[0015] Due to the adoption of the above technical scheme, the plasticized rubber powder forced mixer comprises a mixing frame, a mixing barrel is installed on the mixing frame, and a mixing inlet and a mixing outlet are correspondingly arranged at two ends of the mixing barrel, a mixing shaft is rotatably installed in the mixing barrel, and one end of the mixing shaft close to the mixing inlet extends out of the mixing barrel and is connected to a mixing driving device, a feeding chamber and a mixing chamber are arranged in the mixing barrel, the outer periphery of the mixing shaft is located in the feeding chamber and a feeding device is installed, the outer periphery of the mixing shaft is located in the mixing chamber and a mixing device is installed, the mixing inlet is arranged above the feeding end of the feeding device, the discharging end of the feeding device is arranged at the feeding end of the mixing device, the mixing outlet is arranged at the discharging end of the mixing device, and the end of the mixing shaft close to the mixing outlet extends out of the mixing barrel and a discharging rotary cutting device is correspondingly installed; the beneficial effects of the present invention are:
[0016] (1) The extrusion pin is an important component for completing damping, shearing and mixing. Under the joint action of the inclined mixing disk and the extrusion pin, the plasticized rubber powder is cut, rubbed, extruded, mixed and produces a plasticizing physical reaction. At the same time, the temperature rises rapidly under the strong extrusion pressure. The extrusion pin and the inclined mixing disk form a suitable spatial kinetic energy state, which prompts the plasticized rubber powder to further fully complete the plasticizing reduction reaction. Compared with the cylindrical pin, the trapezoidal extrusion pin has a reasonable design, large resistance, large extrusion force, small kinetic energy, high output, etc., and can better achieve the shearing, extrusion and mixing of the rubber.
[0017] (2) Since the split discharge tray is detachable and can be detachably mounted on the mixer frame by bolts, when the machine is shut down due to power outage or special circumstances, the locking nut can be withdrawn and the rotary cutter and the split discharge tray can be quickly removed. During the cleaning process, it is no longer necessary to remove the bearing seat. Instead, the hardened rubber material can be automatically discharged by rotating the mixing shaft. In this way, no full-time operator is required, which saves time and effort. It is also easier to remove the hardened rubber material in the machine, avoiding problems such as difficult and unclean removal. The machine has a reasonable design, is easy to assemble, and has a low cost.
[0018] (3) The heat in the mixing barrel is transferred outwards through the external cooling system, and the heat in the mixing barrel is transferred inwards through the internal cooling system. The external cooling system is combined with the internal cooling system, and the rubber powder in the mixing barrel can achieve heat transfer in two directions, ensuring that the rubber in the mixing barrel can be fully and evenly cooled, effectively avoiding the phenomenon of only local cooling. It can be seen that the internal cooling system and the external cooling system are important links to ensure the continuous and uniform plasticization reaction of the plasticized rubber. Too high or too low temperature is not conducive to the plasticization mixing reaction, and may even make it impossible. The external cooling system and the internal cooling system are both connected to the automatic control system, and the temperature inside the mixing barrel is controlled in real time by the automatic control system to ensure a suitable temperature environment and ensure that the rubber completes the physical plasticization reaction at 150-160°C. Compared with a cooling device without cooling or only using one direction, the cooling effect is significantly better. The performance of the recycled rubber can be significantly improved under the expected temperature, time, and shear mixing of the plasticized rubber powder, and energy consumption is reduced;
[0019] (4) The setting of the mixing system ensures that the plasticized rubber powder works continuously in a fully enclosed state. The plasticized rubber powder runs in a closed state from beginning to end, so no dust, waste gas or waste water is generated. Continuous and efficient operation is achieved under the effective and appropriate control of the automatic control system;
[0020] (5) The automatic feeding mechanism can not only realize automatic transportation of materials, but also effectively ensure continuous feeding, and no longer need regular loading and unloading. The energy consumption is stable, energy-saving and environmentally friendly, labor-saving, and requires fewer operators to improve efficiency. In addition, the automatic feeding mechanism can realize sealed transportation to prevent rubber powder from scattering in the workshop and prevent the unstable rubber refining quality caused by impurities mixed into the rubber powder. BRIEF DESCRIPTION OF THE DRAWINGS
[0021] The following drawings are intended only to illustrate and explain the present invention, and do not limit the scope of the present invention.
[0022] Figure 1 It is a structural schematic diagram of a forced mixer according to an embodiment of the present invention;
[0023] Figure 2 yes Figure 1 Cross-section along the AA direction;
[0024] Figure 3 yes Figure 1 Cross-section along the middle BB direction;
[0025] Figure 4 It is a schematic diagram of the structure of the split discharging tray according to an embodiment of the present invention;
[0026] Figure 5 is a schematic structural diagram of a rotary cutter according to an embodiment of the present invention;
[0027] Figure 6 is a schematic structural diagram of an extrusion pin according to an embodiment of the present invention;
[0028] Figure 7 This is a schematic diagram of the side material transfer of the extrusion pin according to an embodiment of the present invention;
[0029] Figure 8 This is a schematic diagram of the bottom feeding of the extrusion pin according to an embodiment of the present invention;
[0030] Fig. 9 Schematic diagram of the material passing side gap and the material passing bottom gap of the extrusion pin in an embodiment of the present invention;
[0031] Fig.10 is a schematic diagram of a cooling system according to an embodiment of the present invention;
[0032] Fig.11 is a schematic diagram of a cooling system in an embodiment of the present invention;
[0033] Fig.12 is a partial schematic diagram of a forced mixer according to an embodiment of the present invention;
[0034] Fig.13 is a schematic structural diagram of a hybrid system according to an embodiment of the present invention;
[0035] In the figure: 1-mixing frame; 2-mixing barrel; 3-mixing shaft; 4-mixing drive device; 41-mixing motor; 42-elastic pin coupling; 43-mixing reducer; 44-cross slider coupling; 5-feeding device; 6-mixing device; 61-inclined mixing plate; 62-extrusion pin; 63-mounting part; 64-extrusion stirring part; 65-extrusion plane; 66-inclined plane; 67-mounting flange; 68-stirring teeth; 69-mixing push surface; 7-discharging rotary cutting device; 71-split discharging plate; 72-rotary cutting knife; 7 3-locking nut; 74-discharging plate; 75-material hole; 76-bolt mounting hole; 77-ejection hole; 78-positioning block; 79-peeling tooth; 710-peeling guide surface; 711-discharging nozzle; 8-internal cooling system; 81-return liquid chamber; 82-liquid inlet pipe; 83-heat conversion joint; 84-liquid inlet; 85-return liquid port; 9-external cooling system; 91-external cooling jacket; 92-water inlet nozzle; 93-water return nozzle; 94-external cooling chamber; 10-main machine hopper; 11-storage hopper; 12-feeding mechanism; 13-belt conveyor. DETAILED DESCRIPTION
[0036] The present invention is further described below in conjunction with the accompanying drawings and examples. In the following detailed description, certain exemplary embodiments of the present invention are described only by way of illustration. Needless to say, those of ordinary skill in the art will recognize that the described embodiments may be modified in various ways without departing from the spirit and scope of the present invention. Therefore, the drawings and description are illustrative in nature and are not intended to limit the scope of protection of the claims.
[0037] like Figures 1 to 12 As shown, the plasticized rubber powder forced mixer comprises a mixing machine frame 1, which serves as a bearing base for supporting the entire device; a mixing barrel 2 is installed on the mixing frame 1, and the mixing barrel 2 is an important part for accommodating the main functional components and completing mixing and reduction reactions; a mixing shaft 3 is rotatably installed in the mixing barrel 2, and the mixing shaft 3 is a key part for power transmission and a basis for the installation and positioning of functional components. The two ends of the mixing shaft 3 are supported by bearing seats respectively; one end of the mixing shaft 3 close to the mixing inlet extends out of the mixing barrel 2 and is connected to a mixing drive device 4; a feeding chamber and a mixing chamber are arranged in the mixing barrel 2, and the mixing shaft 3 is located in the feeding cavity and a feeding device 5 is installed on the periphery of the mixing shaft 3. A mixing device 6 is installed on the periphery of the mixing shaft 3. The mixing inlet is arranged above the feeding end of the feeding device 5. The discharging end of the feeding device 5 is arranged at the feeding end of the mixing device 6. The mixing outlet is arranged at the discharging end of the mixing device 6. The end of the mixing shaft 3 close to the mixing outlet extends out of the mixing barrel 2 and a discharging rotary cutting device 7 is installed thereon. An internal cooling system 8 is arranged inside the mixing shaft 3. An external cooling system 9 is arranged on the outer periphery of the mixing barrel 2. The present invention also includes an external cooling system 9 and an internal cooling system 8. An automatic control system is also installed on the mixing frame 1. The mixing drive device 4, the internal cooling system 8 and the external cooling system 9 are all connected to the automatic control system. The automatic control system includes a PLC automatic control box, which implements appropriate control of the entire set of equipment at all times and real-time control of the spindle speed and water temperature. The mixing rack 1 is also equipped with a power distribution system, which includes an electrical box serving as a power distribution source for the entire equipment.
[0038] A main machine hopper 10 is installed on the mixing barrel 2 at the mixing material inlet. The main machine hopper 10 serves as a receiving port, and the feeding end of the feeding device 5 is correspondingly arranged below the main machine hopper 10 .
[0039] See also Fig.12In this embodiment, the feeding mechanism is a feeding agitator installed on the periphery of the mixing shaft 3. The feeding mechanism serves as a key component for forcefully conveying the plasticized rubber powder. It is used to forcibly convey the plasticized rubber powder into the mixing chamber for mixing, and push the plasticized rubber powder to move to the rear end, thereby ensuring the continuous mixing process.
[0040] See also Figure 2 and Fig.12 The mixing device 6 includes inclined mixing disks 61 evenly spaced around the mixing shaft 3, the inclined mixing disks 61 are connected to the mixing shaft 3 via a key, the inclined mixing disks 61 are arranged in a straight line on the mixing shaft 3, and a group of pin assemblies are respectively provided between two adjacent inclined mixing disks 61, the pin assemblies include extrusion pins 62 evenly mounted on the wall of the mixing barrel 2, and the bottom ends of the extrusion pins 62 extend into the mixing cavity.
[0041] See also Figure 6 The extrusion pin 62 includes a mounting portion 63 fixedly mounted on the wall of the mixing barrel 2, and an extrusion stirring portion 64 is provided at the lower end of the mounting portion 63. The bottom of the extrusion stirring portion 64 extends between the two adjacent inclined mixing discs 61, and an extrusion plane 65 for receiving and extruding the plasticized rubber powder is provided on the extrusion stirring portion 64; and a material passing side gap is respectively provided between the two ends of the extrusion stirring portion 64 and the ends of the inclined mixing discs 61 on both sides, namely Fig. 9 In S1, a gap is provided between the bottom end of the extrusion stirring portion 64 and the outer periphery of the mixing shaft 3, that is, Fig. 9 The function of the side gap and the bottom gap is to provide a movement space for the plasticized rubber powder to flow through and to ensure that the extrusion stirring part 64 does not interfere with the movement of the mixing disk below and the mixing shaft 3.
[0042] The working principle of the extrusion pin 62 is:
[0043] See also Figure 7 and Figure 8 Since the extrusion plane 65 is a planar structure, when the plasticized rubber powder is driven by the inclined mixing disk 61 to rotate, the resistance is relatively large when passing through the extrusion plane 65. At this time, the extrusion plane 65 will hinder the rubber material from moving backward quickly, and the plasticized rubber powder will stay in front of the extrusion plane 65 for a longer time, and then the rubber material will slowly pass through the side gaps on both sides and the bottom gap of the material passing. During the process of passing through the gaps, the rubber material passing through the side gaps will be sheared and extruded between the end of the extrusion stirring part 64 and the end of the inclined mixing disk 61. The flow route of the rubber material is shown in FIG. Figure 7 In the direction of the arrow, from Figure 7It can be seen that the rubber material will not easily pass through the side gaps on both sides, and the shearing, extrusion and mixing effects are better at this time, and the mechanical properties of the rubber material produced are poor, but the product quality is higher; due to the better shearing, extrusion and mixing effects, that is, continuous mixing can be achieved in one device to achieve the required finished product quality, which can effectively replace the process of repeated extrusion 5-7 times in the refiner in the prior art;
[0044] The extrusion pin 62 is an important component for completing damping, shearing and mixing. Under the joint action of the inclined mixing disk 61 and the extrusion pin 62, the plasticized rubber powder is cut, rubbed, extruded, mixed and produces a plasticizing physical reaction. At the same time, the temperature rises rapidly under the strong extrusion pressure. The extrusion pin 62 and the inclined mixing disk 61 form a suitable spatial kinetic energy state, which prompts the plasticized rubber powder to further fully complete the plasticizing reduction reaction. Compared with the cylindrical pin, the extrusion pin 62 with a trapezoidal structure is reasonably designed and has the advantages of large resistance, large extrusion force, small kinetic energy, and high output, and can better achieve the shearing, extrusion and mixing of the rubber.
[0045] The side gap and the bottom gap of the material passing material are gradually increased from the extrusion plane 65 to the rear. Figure 7 S1 and Figure 8 Medium S2.
[0046] Further, see Figure 7 In this embodiment, the cross section of the extrusion stirring portion 64 is a trapezoidal structure, the large end surface of the trapezoidal structure is the extrusion plane 65, and the gaps on the material passing side between the waists on both sides of the trapezoidal structure and the ends of the inclined mixing disks 61 on both sides gradually increase. As the gaps on the material passing side gradually increase, when the rubber material passes through the gaps on the material passing side, the space suddenly increases after shearing and extrusion. Figure 7 In the flow direction of the middle arrow, the rubber can flow backward quickly and not accumulate between the side gaps. In this way, more rubber can pass through the side gaps in a short time to complete the shearing and extrusion of the materials, thereby improving the performance of the rubber in a short time. Therefore, the gradual increase of the side gap has three advantages. First, it can prevent the accumulation of materials at the side gaps and prevent the materials from being blocked between the inclined mixing disk 61 and the extrusion stirring part 64 after passing through, affecting the performance of the equipment; second, it can make the subsequent rubber pass through the side gaps stably, ensuring that the performance of more rubber is improved in a short time; third, in the process of passing through the side gaps, due to the small gap, the rubber becomes tight at this time, and after passing through, the space suddenly becomes larger, and the rubber becomes loose at this time. Through the change of loose and tight, intermittent extrusion, the quality of the rubber can be better improved.
[0047] Further, see Figure 8In this embodiment, the bottom end of the extrusion stirring portion 64 is an inclined plane 66, and the gap between the inclined plane 66 and the outer periphery of the mixing shaft 3 gradually increases. The advantage of the gradual increase in the gap at the bottom of the material passing is the same as the advantage of the gradual increase in the gap at the side of the material passing. When the rubber passes through the gap at the bottom of the filter, the space suddenly increases after shearing and extrusion. Figure 8 In the flow direction of the middle arrow, the rubber can flow backward quickly and not accumulate between the gaps at the bottom of the material transfer. In this way, more rubber can pass through the gap at the bottom of the material transfer in a short time to complete the shearing and extrusion of the material, thereby improving the performance of the rubber in a short time. Therefore, the gradual increase in the gap at the bottom of the material transfer has two advantages. First, it can prevent material accumulation at the gap at the bottom of the material transfer, and prevent the material from being blocked between the mixing shaft 3 and the extrusion stirring part 64 after passing through, affecting the performance of the equipment; second, it can make the subsequent rubber pass through the gap at the bottom of the material transfer stably, ensuring that the performance of more rubber is improved in a short time; third, in the process of passing through the side gap of the material transfer, due to the small gap, the rubber becomes tight at this time, and after passing through, the space suddenly becomes larger, and the rubber becomes loose at this time. Through the change of loose and tight, intermittent extrusion, the quality of the rubber can be better improved.
[0048] The mounting portion 63 is configured as a cylindrical body, and a mounting flange 67 is mounted on the top of the cylindrical body. Figure 6 The mixing barrel 2 is provided with a barrel wall mounting hole for inserting the cylindrical column, and the mounting flange 67 is mounted on the barrel wall of the mixing barrel 2 by bolts. During installation, the extrusion pin 62 is inserted from the outside to the inside into the barrel wall mounting hole, and then the mounting flange 67 is fixed to the barrel wall of the mixing barrel 2 by bolts.
[0049] The extrusion pin 62 is made of 42CrMo, which is ultra-high strength steel and has high strength and toughness, as well as high fatigue limit and multiple impact resistance.
[0050] See also Figure 2In the present embodiment, the inclined mixing disk 61 is an inclined triangular disk having three stirring teeth 68. Of course, an inclined quadrangular disk or an inclined two-corner disk may also be selected as required. An inclined mixing pushing surface 69 is provided on the stirring teeth 68. Due to the inclined structure, the mixing pushing surface 69 can, on the one hand, reduce the resistance of the plasticized rubber powder to the inclined mixing disk 61 during mixing, and can effectively mix the plasticized rubber powder in the mixing barrel 2, and improve the service life of the inclined mixing disk 61 and the mixing shaft 3; on the other hand, because the material can be effectively pushed from the front side to the back side through the mixing pushing surface 69, it has the effect of promoting the backward movement of the plasticized rubber powder. Correspondingly, a group of the pin assemblies includes three extrusion pins 62, and the three extrusion pins 62 are evenly distributed on the wall of the mixing barrel 2. The top of the extrusion pin 62 is fixedly mounted on the wall of the mixing barrel 2 through a mounting flange 67. The bottom end of the extrusion pin 62 extends into the mixing chamber close to the surface of the mixing shaft 3, but there is a gap between the bottom end of the extrusion pin 62 and the mixing shaft 3, which will not affect the rotation of the mixing shaft 3. There is a gap between the outer end of the inclined mixing disk 61 and the inner wall of the mixing shaft 3, which will not affect the rotation of the inclined mixing disk 61.
[0051] See also Figure 3 and Fig.10 The discharging rotary cutting device 7 includes a split discharging disc 71 sealed at the discharging end of the mixing barrel 2, and the outer end of the split discharging disc 71 is correspondingly provided with a rotary cutter 72 installed on the mixing shaft 3, and the rotary cutter 72 is connected to the mixing shaft 3 by a key and can rotate with the mixing shaft 3. A locking nut 73 is installed on the mixing shaft 3 to abut against the outer side of the rotary cutter 72, and a threaded section 1 cooperating with the locking nut 73 is provided on the mixing shaft 3. The locking nut 73 is threadedly connected to the mixing shaft 3, and the locking nut 73 is used to position the outer side of the rotary cutter 72.
[0052] See also Figure 4The split discharge tray 71 includes at least two discharge plates 74, all of which are spliced together to form a circular disk body. The structure of the spliced circular disk body is the same as the appearance of the whole discharge tray in the prior art, except that the spliced circular disk body is not an integral structure, but a detachable structure with a connecting seam, wherein the connecting seam is very small and will not affect the overall strength of the split discharge tray 71; a plurality of material holes 75 are evenly distributed on the surface of any of the discharge plates 74, and the material holes 75 are used as mixing discharge ports for passing the rubber material, and all of the material holes 75 are together enclosed to form a circular structure, which is the same as the distribution method of the material holes 75 in the prior art; a plurality of bolt mounting holes 76 are evenly distributed on the edge of any of the discharge plates 74, and all of the bolt mounting holes 76 are together enclosed to form a circle, which is the same as the distribution method of the material holes 75 in the prior art, and the cross-section of the bolt mounting holes 76 is "T"-shaped. The material hole 75 is an arc-shaped hole, a circular hole or an anisotropic hole. In the present embodiment, the material hole 75 is an arc-shaped hole. Of course, the material hole 75 can be selected according to the material forming shape.
[0053] In this embodiment, the split discharge tray 71 includes two discharge plates 74, and adopts a two-piece structure. Of course, three, four or more pieces can also be adopted. However, compared with other pieces, the use of two pieces has the advantages of easy processing, simple installation and positioning, and high strength. Since the split discharge tray 71 adopts a multi-piece setting, when disassembling, it is not necessary to pass the split discharge tray 71 through the mixing shaft 3 as a whole as in the prior art, but only to remove each single piece of the discharge plate 74 separately. The bolt mounting holes 76 are used to install the discharge plates 74, and are arranged in a uniform manner, so that when the spliced split discharge tray 71 is installed, it is not necessary to be restricted by the installation direction.
[0054] The edge of any of the discharge plates 74 is uniformly provided with a plurality of ejection holes 77, and all the ejection holes 77 are enclosed together to form a circle. The ejection holes 77 are provided to facilitate the disassembly of the discharge plate 74. When disassembling, the bolts installed in the bolt installation holes 76 are first screwed out, and then the screws are screwed into the ejection holes 77 to slowly eject the discharge plate 74, which facilitates the disassembly of the discharge plate 74.
[0055] The mixing shaft 3 is also provided with a positioning block 78 which abuts against the inner side of the rotary cutter 72. The mixing shaft 3 is also provided with a second threaded section which cooperates with the positioning block 78. The positioning block 78 is threadedly connected to the mixing shaft 3. The positioning block 78 is used to position the inner side of the rotary cutter 72. The outer peripheral surface of the positioning block 78 cooperates with the inner ring surface of the annular disk body. The positioning block 78 is located in the inner ring of the annular disk body. The outer end of the positioning block 78 extends out of the surface of the split discharge disk 71, so that there is a certain gap between the outer surface of the annular disk body and the inner surface of the rotary cutter 72, so as to provide space for the discharge of the rubber material. The molding length of the discharged rubber material is controlled by this gap to adapt to the different states and sizes of the material. The outer circumferential surface of the positioning block 78 is clearance-matched with the inner annular surface of the annular disk body, and together they seal the outside of the mixing barrel 2. A clearance fit is adopted between the two to prevent the internal rubber material from being discharged from the fitting point. The positioning block 78 and the locking nut 73 position the rotary cutter 72, and are correspondingly installed on the outer side of the split discharge disk 71 to achieve the fit between the split discharge disk 71 and the rotary cutter 72.
[0056] See also Figure 5 The outer periphery of the rotary cutter 72 is provided with a plurality of rotary cutting teeth 79 corresponding to the material hole 75, and the inner end of the rotary cutting tooth 79 is provided with a rotary cutting blade, and the rotary cutting blade is provided with a rotary cutting guide surface 710 inclined toward the rear of the rotation direction; during the rotation of the rotary cutter 72, the rotary cutting blade will cut off the rubber material extruded from the material hole 75, and the rotary cutting guide surface 710 serves as a discharge port. During the cutting process, the rubber material will move along the rotary cutting guide surface 710, which can ensure the stability, sharpness and molding state of the cutting. A discharge nozzle 711 is also fixedly installed on the outside of the mixing barrel 2. The discharge nozzle 711 is located below the split discharge tray 71, that is, below the mixing discharge port, and is also located above the discharge port of the blanking conveying mechanism, which is used to receive the cut rubber material and guide the rubber material to the blanking conveying mechanism.
[0057] The rotary cutter 72 is a double-edged disc rotary cutter 72, a three-edged disc rotary cutter 72 or a four-edged disc rotary cutter 72. In this embodiment, the rotary cutter 72 is a four-edged disc rotary cutter 72. Of course, a double-edged disc rotary cutter 72 or a three-edged disc rotary cutter 72 can also be selected according to needs; among them, the output of the four-edged disc rotary cutter 72 is fine and broken; the output of the double-edged disc rotary cutter 72 is relatively coarse; the output of the three-edged disc rotary cutter 72 is centered, and the appropriate one can also be selected according to actual use needs.
[0058] The bearing seat is connected to the mixer frame 1 through a bearing bracket, and an escape zone is provided on the bearing bracket to facilitate the operation of the locking nut 73, the rotary cutter 72, and the split discharge tray 71. The setting of the escape zone can facilitate the operator to extend his hand to operate the split discharge tray 71.
[0059] The working principle of the discharging peeling device 7 is:
[0060] The split material discharging tray 71 and the rotary cutter 72 are a set of components to achieve the desired material state. When working, the mixing shaft 3 rotates, which drives the rotary cutter 72 to rotate, and cuts off the rubber material discharged from the material hole 75 on the split material discharging tray 71, completing the discharging process.
[0061] During installation, the gap between the rotary cutter 72 and the split discharge tray 71 can be adjusted through the locking nut 73 and the positioning block 78. The locking nut 73 and the positioning block 78 are used as parts to meet the positioning of the cutter and the gap adjustment. The gap can be adjusted to adapt to different states and sizes of materials to achieve a suitable rotary cutting gap.
[0062] Since the split discharge tray 71 is detachable and detachably mounted on the mixer frame 1 by bolts, when the machine is shut down in case of power failure or special circumstances, the locking nut 73 is first unscrewed backwards, and then the rotary cutter 72 is pushed backwards to withdraw the locking nut 73 and the rotary cutter 72 from the split discharge tray 71. At this time, each of the discharge plates 74 is removed from the mixer frame 1, and the machine is restarted after power is restored. At this time, the hardened rubber material will be discharged through the discharge end of the mixing barrel 2 under the push of the inclined mixing tray 61. When all the hardened rubber material is discharged After completion, each of the discharge plates 74 is installed respectively, and the rotary cutter 72 and the locking nut 73 are installed at the same time. After the installation is completed, new plasticized rubber powder can be added for mixing; during the cleaning process, it is no longer necessary to disassemble the bearing seat, but the hardened rubber is automatically discharged by rotating the mixing shaft 3. In this way, no full-time operator is required, which saves time and effort, and it is easier to remove the hardened rubber in the machine, avoiding problems such as difficult and unclean removal; it has a simple structure, reasonable design, convenient assembly, low cost, and is worth promoting and using.
[0063] See also Figure 1 and Fig.13The mixing drive device 4 includes a mixing motor 41, the power end of the mixing motor 41 is connected to a mixing reducer 43 through an elastic pin coupling 42, and the output end of the mixing reducer 43 is connected to the mixing shaft 3 through a cross slider coupling 44. The mixing motor 41 and the mixing reducer 43 are both fixedly mounted on the mixing frame 1, and the function of the mixing reducer 43 is to increase the torque and meet the speed requirements; the elastic pin coupling 42 is a buffer connection; the mixing motor 41 is a prime mover; the mixing motor 41, the mixing reducer 43, the elastic pin coupling 42, and the cross slider coupling 44 are all prior art, which are well known to ordinary engineers and technicians in this field, and will not be repeated here. When working, the mixing motor 41 transmits power to the mixing shaft 3 through the elastic pin coupling 42, the mixing reducer 43, and the cross slider coupling 44 to achieve mixing of rubber powder.
[0064] See also Figure 1 The present invention also includes a cooling system, which includes an external cooling system 9 coated on the outer wall of the mixing barrel 2 and / or an internal cooling system 8 arranged inside the mixing shaft 3. The heat in the mixing barrel 2 is transferred to the external cooling system 9 through the outer wall of the mixing barrel 2 for external heat exchange and / or the heat in the mixing barrel 2 is transferred to the internal cooling system 8 through the outer wall of the mixing shaft 3 for internal heat exchange.
[0065] The cooling system can be used in three ways: one is to use the internal cooling system 8 alone, and the heat in the mixing barrel 2 is transferred to the internal cooling system 8 through the outer wall of the mixing shaft 3 for internal heat exchange; the second is to use the external cooling system 9 alone, and the heat in the mixing barrel 2 is transferred to the external cooling system 9 through the outer wall of the mixing barrel 2 for external heat exchange; the third is to use the internal cooling system 8 and the external cooling system 9 in combination, and the heat inside the mixing barrel 2 is exchanged both externally and internally.
[0066] When used in combination, the heat in the mixing barrel 2 is transferred outward through the external cooling system 9, and the heat in the mixing barrel 2 is transferred inward through the internal cooling system 8. The external cooling system 9 is combined with the internal cooling system 8, and the rubber powder in the mixing barrel 2 can achieve heat transfer in two directions, ensuring that the rubber in the mixing barrel 2 can be fully and evenly cooled, effectively avoiding the phenomenon of only local cooling. It can be seen that the internal cooling system 8 and the external cooling system 9 are important links to ensure the continuous and uniform plasticization reaction of the plasticized rubber. Too high or too low temperature is not conducive to the plasticization mixing reaction, and it may even be impossible to carry out. The external cooling system 9 and the internal cooling system 8 are both connected to the automatic control system, which controls the temperature inside the mixing barrel 2 in real time to ensure a suitable temperature environment and ensure that the rubber completes the physical plasticization reaction at 150-160°C. Compared with a cooling device without cooling or only using one direction of cooling, the cooling effect of the present invention is significantly better. The performance of the recycled rubber can be significantly improved under the expected temperature, time, and shear mixing of the plasticized rubber powder, and the energy consumption is reduced.
[0067] See also Fig.11 The internal cooling system 8 includes a liquid return chamber 81 which is arranged at the center of the axis of the mixing shaft 3 and is open at one end. The liquid return chamber 81 extends from the feeding end of the mixing barrel 2 to the discharging end of the mixing barrel 2 and to the end of the mixing shaft 3. The length of the liquid return chamber 81 corresponds to the mixing chamber, which is used to ensure that the cooling liquid in the liquid return chamber 81 can cool the rubber material in the mixing chamber. A liquid inlet pipe 82 with openings at both ends is also installed in the liquid return chamber 81, and a liquid gap is provided between the inner end of the liquid inlet pipe 82 and the inner end of the liquid return chamber 81. A heat conversion joint 83 is installed at the end of the mixing shaft 3, and a liquid inlet port 84 connected to the outer end of the liquid inlet pipe 82 is provided in the heat conversion joint 83. A liquid return port 85 connected to the liquid return chamber 81 is also provided in the heat conversion joint 83, and an internal circulation pipeline is connected between the liquid inlet port 84 and the liquid return port 85. The inner circulation pipeline includes an inner cooling water inlet pipeline and an inner cooling water return pipeline. The inner cooling water inlet pipeline is provided with an inner circulation water pump, the inner cooling water return pipeline is provided with an inner circulation electromagnetic throttle valve, and the inner cooling water return pipeline is also provided with an inner circulation temperature sensor. The inner circulation electromagnetic throttle valve and the inner circulation temperature sensor are both electrically connected to the automatic control system. The inner circulation electromagnetic throttle valve, the inner circulation temperature sensor, and the automatic control system are all prior art, which are well known to ordinary engineering and technical personnel in the field and will not be described in detail here.
[0068] See also Fig.11The internal circulation flow route is: the coolant enters the liquid inlet pipe 82 through the internal cooling water inlet pipeline and the liquid inlet port 84, then flows to the inner end of the liquid inlet pipe 82, finally flows into the liquid return chamber 81 through the liquid gap, finally flows to the outer end through the liquid return chamber 81, and returns to the internal cooling water return pipeline through the liquid return pipe. As the coolant continuously flows from the inner end to the outer end of the liquid return chamber 81, the heat inside the mixing barrel 2 is transferred inwardly to the liquid return chamber 81 through the mixing shaft 3, and heat is exchanged with the coolant to achieve internal cooling of the mixing barrel 2.
[0069] The inner water circulation pipeline is also provided with an inner circulation electromagnetic throttle valve for controlling the return flow of the coolant, a plurality of inner circulation temperature sensors for measuring the temperature, and a PLC control board. The inner circulation electromagnetic throttle valve and the inner circulation temperature sensor are connected to the PLC control board, and the PLC control board is connected to the automatic control system. The inner circulation temperature sensor transmits the measured temperature signal to the PLC control board, and then transmits the signal to the automatic control system, and then the automatic control system uses the temperature signal to feedback control the opening, closing and opening size of the inner circulation electromagnetic throttle valve. When the temperature of the inner circulation temperature sensor is higher than the set value, it means that the temperature in the mixing barrel 2 is higher. At this time, the inner circulation electromagnetic throttle valve is controlled to open a little wider, speeding up the flow of the coolant, realizing rapid circulation, and rapid cooling; when the temperature of the inner circulation temperature sensor is lower than the set value, it means that the temperature in the mixing barrel 2 is lower. The inner circulation electromagnetic throttle valve is controlled to open a little smaller to reduce energy loss. Of course, if the return liquid chamber 81 is filled with heat medium, the mixing barrel 2 can be heated.
[0070] See also Figure 1 and Figure 2 The external cooling system 9 includes an external cooling jacket 91 coated on the outer peripheral wall of the mixing barrel 2, and a water inlet nozzle 92 and a water return nozzle 93 are respectively provided at both ends of the external cooling jacket 91, and an external circulation pipeline is connected between the water inlet nozzle 92 and the water return nozzle 93. The external circulation pipeline includes an external cooling water inlet pipeline and an external cooling water return pipeline, an external circulation water pump is provided on the external cooling water inlet pipeline, an external circulation electromagnetic throttle valve is provided on the external cooling water return pipeline, and an external circulation temperature sensor is also provided on the external cooling water return pipeline. The external circulation electromagnetic throttle valve and the external circulation temperature sensor are both electrically connected to the automatic control system. The external circulation electromagnetic throttle valve, the external circulation temperature sensor, and the automatic control system are all prior art, which are well known to ordinary engineering and technical personnel in this field and will not be repeated here.
[0071] Specifically, three outer cooling sleeves 91 are evenly distributed on the outer wall of the mixing barrel 2. The outer cooling sleeves 91 are arc-shaped structures and are welded on the outer wall of the mixing barrel 2. Figure 2 The extrusion pins 62 are all located outside the outer cooling sleeve 91, and a closed outer cooling cavity 94 is formed between the outer cooling sleeve 91 and the outer wall of the mixing barrel 2. The outer cooling cavity 94 is filled with coolant, and both ends of the outer cooling sleeve 91 are provided with a water inlet nozzle 92 and a water return nozzle 93 connected to the outer cooling cavity 94, and the water inlet nozzle 92 and the water return nozzle 93 are connected to the external water circulation pipeline.
[0072] The external water circulation pipeline is also provided with an external circulation electromagnetic throttle valve for controlling the reflux flow of the coolant, a plurality of external circulation temperature sensors for measuring temperature, and a PLC control board. The external circulation electromagnetic throttle valve and the external circulation temperature sensor are connected to the PLC control board, and the PLC control board is connected to the automatic control system. The coolant continuously circulates in the external cooling cavity 94, and the heat in the mixing barrel 2 is transferred outwardly to the external cooling cavity 94 through the barrel wall, and heat is exchanged with the coolant to achieve the cooling of the mixing barrel 2; the external circulation temperature sensor transmits the measured temperature signal to the PLC control board, and then transmits the signal to the automatic control system, and then the automatic control system uses the temperature signal to feedback control the opening, closing and opening size of the external circulation electromagnetic throttle valve. When the temperature of the external circulation temperature sensor is higher than the set value, it means that the temperature inside the mixing barrel 2 is high. At this time, the external circulation electromagnetic throttle valve is controlled to open a little wider to speed up the flow of the coolant, achieve rapid circulation, and quickly cool down; when the temperature of the external circulation temperature sensor is lower than the set value, it means that the temperature inside the mixing barrel 2 is low. The external circulation electromagnetic throttle valve is controlled to open a little smaller to reduce energy loss. Of course, if the external cooling chamber 94 is filled with heat medium, the mixing barrel 2 can be heated.
[0073] See also Fig.13The plasticized rubber powder forced mixing system includes a forced mixer, an automatic feeding mechanism is installed at the mixing inlet of the forced mixer, and a blanking conveying mechanism is installed at the mixing outlet of the forced mixer; the automatic feeding mechanism and the blanking conveying mechanism are both connected to the automatic control system. The automatic control system implements appropriate control over the entire set of equipment at all times, and controls the feeding supply, spindle speed, water temperature control, and belt output speed in real time, so that the forced mixer can achieve the optimal working parameters and improve the working efficiency of the forced mixer. In addition, the setting of the mixing system ensures that the plasticized rubber powder works continuously under full closure. The plasticized rubber powder runs in a closed state from beginning to end, so no dust, waste gas, or wastewater is generated, and continuous and efficient operation is achieved under the effective and appropriate control of the automatic control system.
[0074] The automatic feeding mechanism includes a storage hopper 11, and a feeding mechanism 12 is installed at the discharge port of the storage hopper 11, and the discharge port of the feeding mechanism 12 corresponds to the mixing feed port. The storage hopper 11 serves as a feed hopper for the feeding mechanism 12. In this embodiment, the feeding mechanism 12 is a spiral feeding auger, and a feeding motor is installed at the top of the feeding auger. The feeding motor serves as the power source of the feeding mechanism 12. The upper part of the feeding auger is located at the discharge port and is provided with a discharge nozzle. The discharge nozzle is located above the main hopper 10 and corresponds to the mixing feed port. When working, the feeding mechanism 12 lifts the material in the storage hopper 11 and discharges it through the discharge nozzle, which just falls into the main hopper 10 and enters the mixing shaft 3. The automatic feeding mechanism can not only realize automatic transportation of materials, but also effectively ensure continuous feeding, and no longer need regular loading and unloading, with stable energy consumption, energy saving and environmental protection, saving labor, requiring fewer operators, and improving efficiency. In addition, the automatic feeding mechanism can realize sealed transportation, which is used to prevent rubber powder from scattering in the workshop and prevent the unstable rubber mixing quality caused by impurities mixed into the rubber powder.
[0075] In this embodiment, the material delivery mechanism is a belt conveyor 13, and the mixing outlet is located above the material delivery outlet of the belt conveyor 13, so that the material dropped from the mixing outlet can be transported to a designated location by the belt conveyor 13, which is easy to operate, reduces labor intensity, and saves a lot of labor. The belt conveyor 13 is a prior art, which is well known to ordinary engineers and technicians in this field and will not be described here. Of course, a screw conveyor auger can be selected as the material delivery mechanism according to the working site conditions.
[0076] Working principle of the present invention:
[0077] After the plasticized rubber powder enters the storage hopper 11, it is distributed to the feeding mechanism by the loading mechanism 12. After forced feeding by the feeding mechanism, the plasticized rubber powder is cut, rubbed, extruded, mixed and produces a plasticized physical reaction under the joint action of the inclined mixing disk 61 and the extrusion pin 62, and the temperature rises rapidly under the strong extrusion pressure. Under the joint action of the internal cooling system 8 and the external cooling system 9, the temperature is controlled in real time by the automatic control system; it is ensured that the rubber material completes the physical plasticization reaction at 150-160°C, so that the plasticized rubber material has higher mechanical properties and is easier to realize automation. Due to the feeding device 5 at the front end, the plasticized rubber powder slowly moves forward under the action of the multiple inclined mixing disks 61 (the reason for the slowness is related to the multiple extrusion pins 62). When the plasticized rubber powder reaches the split discharge disk 71 at the end, it is chopped under the action of the rotary cutter 72, falls into the blanking conveying mechanism through the mixing discharge port and is discharged; the discharge temperature is ≤90°C, and the working cycle is completed.
[0078] The above shows and describes the basic principles, main features and advantages of the present invention. It should be understood by those skilled in the art that the present invention is not limited to the above embodiments. The above embodiments and descriptions are only for explaining the principles of the present invention. Without departing from the spirit and scope of the present invention, the present invention may have various changes and improvements, which fall within the scope of the present invention. The scope of protection of the present invention is defined by the attached claims and their equivalents.
Claims
1. A plasticized rubber powder forced mixer, comprising a mixing frame, a mixing barrel mounted on the mixing frame, a mixing inlet and a mixing outlet correspondingly arranged at both ends of the mixing barrel, a mixing shaft rotatably mounted in the mixing barrel, one end of the mixing shaft close to the mixing inlet extending out of the mixing barrel and connected to a mixing drive device, characterized in that: A feeding cavity and a mixing cavity are arranged in the mixing barrel, a feeding device is installed in the feeding cavity on the periphery of the mixing shaft, a mixing device is installed in the mixing cavity on the periphery of the mixing shaft, a mixing inlet is arranged above the feeding end of the feeding device, a discharging end of the feeding device is arranged at the feeding end of the mixing device, a mixing outlet is arranged at the discharging end of the mixing device, and an end of the mixing shaft close to the mixing outlet extends out of the mixing barrel and a discharging rotary cutting device is installed correspondingly; The mixing device comprises inclined mixing disks evenly spaced on the periphery of the mixing shaft, a group of pin assemblies are respectively arranged between two adjacent inclined mixing disks, the pin assemblies comprise extrusion pins evenly mounted on the wall of the mixing cylinder, the bottom ends of the extrusion pins extend into the mixing cavity; The extrusion pin includes a mounting portion fixedly mounted on the wall of the mixing barrel, an extrusion stirring portion is provided at the lower end of the mounting portion, the bottom of the extrusion stirring portion extends into between two adjacent inclined mixing disks, and an extrusion plane for receiving and extruding plasticized rubber powder is provided on the extrusion stirring portion; side gaps for feeding are respectively provided between the two ends of the extrusion stirring portion and the ends of the inclined mixing disks on both sides, and a bottom gap for feeding is provided between the bottom end of the extrusion stirring portion and the outer periphery of the mixing shaft, and both the side gap for feeding and the bottom gap for feeding gradually increase from the extrusion plane to the rear.
2. The plasticized rubber powder forced mixer according to claim 1, characterized in that: The discharging and peeling device includes a split discharging disk that blocks the discharging end of the mixing barrel, the outer end of the split discharging disk is correspondingly provided with a peeling knife installed on the mixing shaft, the mixing shaft is provided with a locking nut that abuts against the outer side of the peeling knife, and the mixing shaft is also provided with a positioning block that abuts against the inner side of the peeling knife, and the outer peripheral surface of the positioning block cooperates with the inner ring surface of the circular disk body.
3. The plasticized rubber powder forced mixer according to claim 2, characterized in that: The split discharge tray includes at least two discharge plates, all of which are spliced together to form a circular tray body, and the surface of any of the discharge plates is evenly distributed with a number of material holes, and all of the material holes are together enclosed to form a circular structure; the edge of any of the discharge plates is evenly distributed with a number of bolt mounting holes, and all of the bolt mounting holes are together enclosed to form a circle.
4. The plasticized rubber powder forced mixer according to claim 1, characterized in that: It also includes a cooling system, which includes an external cooling system coated on the outer wall of the mixing barrel and / or an internal cooling system arranged inside the mixing shaft. The heat in the mixing barrel is transferred to the external cooling system through the outer wall of the mixing barrel for external heat exchange and / or the heat in the mixing barrel is transferred to the internal cooling system through the outer wall of the mixing shaft for internal heat exchange.
5. The plasticized rubber powder forced mixer according to claim 4, characterized in that: The internal cooling system includes a liquid return chamber which is arranged at the center of the axis of the mixing shaft and is open at one end. The liquid return chamber extends from the feeding end of the mixing barrel to the discharging end of the mixing barrel and to the end of the mixing shaft. A liquid inlet pipe with two ends opening is also installed in the liquid return chamber. A liquid gap is provided between the inner end of the liquid inlet pipe and the inner end of the liquid return chamber. A heat conversion joint is installed at the end of the mixing shaft. A liquid inlet port connected to the outer end of the liquid inlet pipe is provided in the heat conversion joint. A liquid return port connected to the liquid return chamber is also provided in the heat conversion joint. An internal circulation pipeline is connected between the liquid inlet port and the liquid return port.
6. The plasticized rubber powder forced mixer according to claim 5, characterized in that: The internal circulation pipeline includes an internal cooling water inlet pipeline and an internal cooling water return pipeline. The internal cooling water inlet pipeline is provided with an internal circulation water pump, the internal cooling water return pipeline is provided with an internal circulation electromagnetic throttle valve, and the internal cooling water return pipeline is also provided with an internal circulation temperature sensor.
7. The plasticized rubber powder forced mixer according to claim 4, characterized in that: The external cooling system comprises an external cooling jacket coated on the outer peripheral wall of the mixing barrel, and a water inlet nozzle and a water return nozzle are respectively arranged at two ends of the external cooling jacket, and an external circulation pipeline is connected between the water inlet nozzle and the water return nozzle.
8. The plasticized rubber powder forced mixer according to claim 7, characterized in that: The external circulation pipeline includes an external cooling water inlet pipeline and an external cooling water return pipeline. The external cooling water inlet pipeline is provided with an external circulation water pump, the external cooling water return pipeline is provided with an external circulation electromagnetic throttle valve, and the external cooling water return pipeline is also provided with an external circulation temperature sensor.
Citation Information
Patent Citations
Multi cutter-head extruder and assembling method thereof
CN101508168A
Device and method for directly preparing regenerated rubber sheet by continually cooling and mixing desulfurized rubber powder
CN102344592A
Surface shear plasticization method and device
CN106808664A
Waste tyre rubber recycling desulfuration refining treatment system
CN109054078A
Natural rubber primary processing wet stirring and extrusion washing all-in-one machine
CN109366788A