Secondary battery and electrode component thereof

By designing a combined structure of strip grooves and a second conductive layer on the first conductive layer of the secondary battery electrode component, combined with the protective layer, the problem of the conductive layer falling off is solved, and the performance and safety of the electrode component are improved.

CN111048791BActive Publication Date: 2024-10-29CONTEMPORARY AMPEREX TECHNOLOGY CO LTD
View PDF 11 Cites 0 Cited by

Patent Information

Application Number
CN201811183466.4
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2018-10-11
Publication Date
2024-10-29
Estimated Expiration
2038-10-11

AI Technical Summary

Technical Problem

During the rolling process of secondary battery electrode components, due to insufficient connection force between the insulating matrix and the conductive layer, the conductive layer may fall off, affecting the performance of the electrode component.

Method used

An electrode component is designed, in which the first conductive layer is provided with a strip groove extending in the height direction on the surface of the insulating base, the second conductive layer is located in the strip groove, and a protective layer is provided on the protrusion to relieve stress. And enhance the connection force and reduce the risk of the conductive layer falling off.

Benefits of technology

It effectively reduces the risk of the conductive layer falling off, improves the performance and safety of the electrode component, and ensures the stability and overcurrent capability of the electrode component during the rolling process.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN111048791B_ABST
    Figure CN111048791B_ABST
Patent Text Reader

Abstract

The present invention provides a secondary battery and an electrode component thereof. The electrode component comprises an insulating substrate, a first conductive layer and an active material layer; the first conductive layer is arranged on the surface of the insulating substrate, and the active material layer is arranged on a side of the first conductive layer away from the insulating substrate; the first conductive layer is provided with a strip groove extending in the height direction, and the strip groove is used to release the stress of the first conductive layer. The secondary battery comprises an electrode assembly, and the electrode assembly comprises the electrode component.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of batteries, and in particular to a secondary battery and an electrode component thereof. Background Art

[0002] The electrode components of secondary batteries generally include a current collector and an active material layer coated on the surface of the current collector. In order to improve the safety performance of secondary batteries, some electrode components select a current collector with a multi-layer structure. Figures 1 to 3 The current collector includes an insulating substrate 11 and a conductive layer 12 connected to the surface of the insulating substrate 11 , and the active material layer 13 is coated on the surface of the conductive layer 12 .

[0003] In the production process of the electrode component, it is necessary to roll the active material layer 13 to thin the active material layer 13 and improve the energy density. The insulating substrate 11 is a relatively soft material (such as PET plastic), and the conductive layer 12 is usually made of metal. The elastic modulus of the insulating substrate 11 is smaller than the elastic modulus of the conductive layer 12, so the ductility of the insulating substrate 11 is higher than the ductility of the conductive layer 12. In the process of extending the insulating substrate 11, the insulating substrate 11 will exert a force on the conductive layer 12, and because the connection force between the insulating substrate 11 and the conductive layer 12 is small, when the conductive layer 12 is extended to a certain extent, it may cause the conductive layer 12 to fall off from the surface of the insulating substrate 11, thereby affecting the performance of the electrode component. Summary of the invention

[0004] In view of the problems existing in the background technology, an object of the present invention is to provide a secondary battery and an electrode component thereof, which can reduce stress concentration, reduce the risk of conductive layer falling off, and ensure the performance of the electrode component.

[0005] In order to achieve the above objective, the present invention provides a secondary battery and an electrode component thereof.

[0006] The electrode component includes an insulating substrate, a first conductive layer and an active material layer; the first conductive layer is arranged on the surface of the insulating substrate, and the active material layer is arranged on a side of the first conductive layer away from the insulating substrate; the first conductive layer is provided with a strip groove extending in the height direction.

[0007] The electrode member further includes a second conductive layer having a first portion located within the stripe-shaped groove.

[0008] The second conductive layer also includes a second portion, which is disposed on a surface of the first conductive layer away from the insulating substrate and connected to the first portion, and the active material layer is disposed on a surface of the second portion away from the first conductive layer.

[0009] The first conductive layer includes a main body and a protrusion extending from the main body, the main body is coated with an active material layer, and the protrusion is not coated with an active material layer. The strip groove includes a first groove formed in the protrusion, and the second part is at least partially located on a surface of the protrusion away from the insulating substrate.

[0010] The strip-shaped groove further includes a second groove formed in the main body, and the first groove is communicated with the second groove.

[0011] The electrode component further includes a protective layer, which is disposed on a surface of the second portion away from the protrusion and connected to the active material layer, and the first groove does not extend beyond the protective layer.

[0012] The second conductive layer has a stiffness smaller than that of the first conductive layer.

[0013] The strip-shaped groove penetrates the first conductive layer along the thickness direction, and the first part of the second conductive layer is connected to the insulating substrate.

[0014] There are a plurality of strip-shaped grooves, and the plurality of strip-shaped grooves are arranged at intervals along the width direction.

[0015] The secondary battery includes an electrode assembly, and the electrode assembly includes the electrode member.

[0016] The beneficial effects of the present invention are as follows: In the present application, strip grooves are formed on the first conductive layer, and the strip grooves can effectively release the force on the first conductive layer, reduce stress concentration, effectively reduce the risk of the first conductive layer falling off the surface of the insulating substrate, and ensure the performance of the electrode component. BRIEF DESCRIPTION OF THE DRAWINGS

[0017] Figure 1 Schematic diagram of an electrode component in the prior art.

[0018] Figure 2 for Figure 1 Schematic diagram of the electrode component during the roller pressing process.

[0019] Figure 3 for Figure 1 Schematic diagram of the insulating substrate and conductive layer of the electrode component before rolling.

[0020] Figure 4 for Figure 1 Schematic diagram of the insulating substrate and the conductive layer of the electrode component after rolling.

[0021] Figure 5 is a schematic diagram of a secondary battery according to the present invention.

[0022] Figure 6 is a cross-sectional view of an electrode assembly according to the present invention.

[0023] Figure 7FIG. 1 is a schematic diagram of a first embodiment of an electrode component according to the present invention.

[0024] Figure 8 for Figure 7 Section view along line AA.

[0025] Fig. 9 for Figure 7 A schematic diagram of an electrode component during the forming process.

[0026] Fig.10 for Figure 7 Another schematic diagram of an electrode component during the forming process.

[0027] Fig.11 for Fig.10 Schematic diagram of the first conductive layer after rolling.

[0028] Fig.12 for Figure 7 Another schematic diagram of the electrode component during the forming process.

[0029] Fig.13 for Figure 7 Schematic diagram of the electrode component after winding.

[0030] Fig.14 FIG. 1 is a schematic diagram of a second embodiment of an electrode component according to the present invention.

[0031] Fig.15 for Fig.14 Section view along line BB.

[0032] Fig.16 for Fig.15 Schematic diagram of the insulating substrate and the first conductive layer.

[0033] Fig.17 FIG. 4 is a schematic diagram of a third embodiment of an electrode component according to the present invention.

[0034] Fig.18 for Fig.17 Section view along line CC.

[0035] Fig.19 FIG. 4 is a schematic diagram of a fourth embodiment of an electrode component according to the present invention.

[0036] Fig. 20 for Fig.19 Sectional view along line DD.

[0037] Fig.21 for Fig.19 Schematic diagram of the first conductive layer of the electrode member.

[0038] Fig. 22FIG. 5 is a schematic diagram of a fifth embodiment of an electrode component according to the present invention.

[0039] Fig.23 for Fig. 22 Section view along line EE.

[0040] Fig.24 for Fig. 22 Schematic diagram of the first conductive layer of the electrode member.

[0041] The reference numerals are described as follows:

[0042] 1 electrode component 5 housing

[0043] 11 Insulation base 6 Top cover

[0044] 12 first conductive layer 7 electrode terminal

[0045] 121 main body 8 adapter

[0046] 122 protrusion 9 roller

[0047] 13 Active material layer G strip groove

[0048] 14 second conductive layer G1 first groove

[0049] 141 first part G2 second groove

[0050] 142 second part G3 third groove

[0051] 15 protective layer G4 fourth groove

[0052] 16 Conductive structure P electrical guide

[0053] 2Positive electrode component X width direction

[0054] 3. Thickness direction of negative electrode component Y

[0055] 4 Diaphragm Z height direction DETAILED DESCRIPTION

[0056] The following will be combined with the drawings in the embodiments of the present application to clearly and completely describe the technical solutions in the embodiments of the present application. Obviously, the described embodiments are only part of the embodiments of the present application, rather than all of the embodiments. The following description of at least one exemplary embodiment is actually only illustrative and is by no means intended to limit the present application and its application or use. Based on the embodiments in the present application, all other embodiments obtained by ordinary technicians in this field without carrying out creative work are within the scope of protection of this application.

[0057] In the description of the present application, it should be understood that the use of terms such as "first" and "second" to limit components is only for the convenience of distinguishing the corresponding components. Unless otherwise stated, the above terms have no special meaning and therefore cannot be understood as limiting the scope of protection of the present application.

[0058] The secondary battery of the present invention includes an electrode assembly, referring to Figure 6 The electrode assembly includes a positive electrode component 2, a negative electrode component 3 and a separator 4, and the separator 4 is arranged between the positive electrode component 2 and the negative electrode component 3. The positive electrode component 2, the separator 4 and the negative electrode component 3 are stacked and wound into a flat shape. The electrode assembly is a core component for realizing the charging and discharging functions of the secondary battery.

[0059] The secondary battery of the present invention can be a soft pack battery, and the electrode assembly formed by winding the positive electrode component 2, the separator 4 and the negative electrode component 3 is directly packaged in a packaging bag. The packaging bag can be an aluminum-plastic film.

[0060] Of course, the secondary battery of the present application may also be a hard shell battery. Figure 5 The secondary battery mainly includes an electrode assembly, a shell 5, a top cover plate 6, an electrode terminal 7 and a switching plate 8.

[0061] The housing 5 may have a hexahedral shape or other shapes. A cavity is formed inside the housing 5 to accommodate the electrode assembly and the electrolyte. The housing 5 has an opening at one end, and the electrode assembly can be placed in the receiving cavity of the housing 5 through the opening. The housing 5 may be made of a conductive metal material such as aluminum or aluminum alloy, or may be made of an insulating material such as plastic.

[0062] The top cover plate 6 is disposed on the housing 5 and covers the opening of the housing 5, thereby enclosing the electrode assembly in the housing 5. The electrode terminal 7 is disposed on the top cover plate 6, the upper end of the electrode terminal 7 protrudes to the upper side of the top cover plate 6, and the lower end can pass through the top cover plate 6 and extend into the housing 5. The adapter 8 is disposed in the housing 5 and fixed to the electrode terminal 7. There are two electrode terminals 7 and two adapters 8, the positive electrode component 2 is electrically connected to one electrode terminal 7 via one adapter 8, and the negative electrode component 3 is electrically connected to the other electrode terminal 7 via the other adapter 8.

[0063] In the secondary battery, at least one of the positive electrode member 2 and the negative electrode member 3 employs an electrode member 1 described later.

[0064] Figures 7 to 13 FIG. 1 is a schematic diagram of a first embodiment of an electrode component 1 of the present invention. Figure 7 and Figure 8 The electrode component 1 of the first embodiment includes an insulating substrate 11, a first conductive layer 12 and an active material layer 13. The first conductive layer 12 is disposed on both surfaces of the insulating substrate 11, and the active material layer 13 is disposed on one side of the first conductive layer 12 away from the insulating substrate 11.

[0065] The insulating substrate 11 may be made of PET (polyethylene terephthalate) film or PP (polypropylene) film.

[0066] The material of the first conductive layer 12 is selected from at least one of a metal conductive material and a carbon-based conductive material; the metal conductive material is preferably at least one of aluminum, copper, nickel, titanium, silver, nickel-copper alloy, and aluminum-zirconium alloy; the carbon-based conductive material is preferably at least one of graphite, acetylene black, graphene, and carbon nanotubes.

[0067] The first conductive layer 12 may be formed on the surface of the insulating substrate 11 by at least one of vapor deposition and electroless plating. The vapor deposition method is preferably physical vapor deposition (PVD), such as thermal evaporation deposition.

[0068] The active material layer 13 can also be provided on the surface of the first conductive layer 12 by coating. The active material (such as lithium manganese oxide, lithium iron phosphate), a binder, a conductive agent and a solvent can be made into a slurry, and then the slurry is coated on the outer surfaces of the two first conductive layers 12, and the active material layer 13 is formed after the slurry is cured.

[0069] Reference Fig. 9 , the first conductive layer 12 is provided with a strip groove G, which extends substantially along the height direction Z and is used to release the stress of the first conductive layer 12. The length of the strip groove G along the width direction X is 0.001 mm to 1 mm, and is much smaller than the length of the strip groove G extending along the height direction Z. The strip groove G can be straight or curved, and from a general perspective, the strip groove G only needs to extend approximately along the height direction Z; that is, there can be a small angle between the extension direction of the strip groove G and the height direction Z (for example, the angle can be less than 10°).

[0070] The thickness of the insulating substrate 11 can be 1 μm to 20 μm, and the thickness of the first conductive layer 12 can be 0.1 μm to 10 μm. Since the first conductive layer 12 is relatively thin, the burrs generated by the first conductive layer 12 are relatively small during the cutting process of the electrode component 1, and it is difficult to pierce the diaphragm 4 of more than ten microns, thereby avoiding short circuits and improving safety performance. In addition, when a foreign object pierces the electrode component 1 of the secondary battery, since the thickness of the first conductive layer 12 is relatively small, the burrs generated by the first conductive layer 12 at the part pierced by the foreign object are relatively small, and it is difficult to pierce the diaphragm 4, thereby avoiding short circuits and improving safety performance.

[0071] The first conductive layer 12 includes a main body 121 and a protrusion 122 extending from the main body 121, the main body 121 is coated with an active material layer 13, and the protrusion 122 is not coated with the active material layer 13. The active material layer 13 can be directly coated on the surface of the main body 121. Of course, alternatively, other materials can also be provided between the main body 121 and the active material layer 13.

[0072] The portion of the insulating base 11 corresponding to the protrusion 122 and the protrusion 122 form an electric lead P. The electric lead P may be plural and arranged at intervals along the width direction X. Fig.13 When the electrode component 1 is wound and formed, the multiple electrical conductors P are stacked along the thickness direction Y.

[0073] The electrode member 1 further includes a protective layer 15 , which is provided on a side of the protrusion 122 away from the insulating substrate 11 and connected to the active material layer 13 .

[0074] The protective layer 15 includes a binder and an insulating material. The insulating material includes at least one of aluminum oxide and aluminum oxyhydroxide. The binder, the insulating material and the solvent are mixed together to prepare a slurry, which is coated on the surface of the protrusion 122 and forms the protective layer 15 after curing. The hardness of the protective layer 15 is greater than the hardness of the protrusion 122.

[0075] The electrode component 1 further includes a conductive structure 16, which is welded to the area of ​​the protrusion 122 that is not covered by the protective layer 15. Figure 7 and Figure 8 , conductive structures 16 are fixed on both sides of each electrical guide portion P along the thickness direction Y. Fig.13 After the electrode component 1 is wound, all the conductive structures 16 are stacked and welded to the adapter sheet 8 at the same time. Figure 5 The current in the electrode component 1 can be output to the outside through the adapter 8 and the electrode terminal 7.

[0076] The electrode component 1 of the first embodiment can be formed according to the following steps:

[0077] (i) forming a first conductive layer 12 on the surface of an insulating substrate 11 by vapor deposition or chemical plating, thereby preparing a composite strip; Fig. 9 During the molding process, a strip-shaped groove G is reserved on the first conductive layer 12 .

[0078] (II) Reference Fig.10 , the active material layer 13 and the protective layer 15 are simultaneously coated on the surface of the first conductive layer 12 .

[0079] (iii) rolling the active material layer 13 to compact the active material layer 13 and increase its density.

[0080] (IV) Reference Fig.12 After rolling, a metal foil (such as aluminum foil) is welded on the first conductive layer 12, and then Fig.12 The dotted lines in the figure cut out multiple electrical guides P and multiple conductive structures 16, thereby obtaining Figure 7 The electrode component 1 is shown.

[0081] In step (a), the first conductive layer 12 can be formed on the surface of the insulating substrate 11 by vapor deposition or chemical plating, so the connection force between the first conductive layer 12 and the insulating substrate 11 is relatively small. Under the action of external force, the first conductive layer 12 may easily fall off from the surface of the insulating substrate 11.

[0082] Since the elastic modulus of the insulating substrate 11 is smaller than the elastic modulus of the first conductive layer 12, the ductility of the insulating substrate 11 is higher than the ductility of the first conductive layer 12. In step (iii), the insulating substrate 11 is compressed and stretched. Since the ductility of the insulating substrate 11 is high, the insulating substrate 11 will exert a force on the first conductive layer 12. In the prior art, the force on the first conductive layer 12 cannot be released, so when the first conductive layer 12 is stretched to a certain extent, the force on the first conductive layer 12 will be greater than the connection force between the insulating substrate 11 and the first conductive layer 12, causing the insulating substrate 11 and the first conductive layer 12 to slide relative to each other, so that the first conductive layer 12 falls off from the surface of the insulating substrate 11, affecting the performance of the electrode component 1.

[0083] In the present application, a strip groove G is formed on the first conductive layer 12, and the strip groove G can effectively release the force on the first conductive layer 12, reduce stress concentration, avoid excessive force on the first conductive layer 12, and effectively reduce the risk of the first conductive layer 12 falling off the surface of the insulating substrate 11, thereby ensuring the performance of the electrode component 1.

[0084] Specifically, Fig.11 The state of the first conductive layer 12 after rolling is shown, wherein the dotted line shows the state of the strip groove G before rolling. During the rolling process of step (iii), the force on the first conductive layer 12 is gradually concentrated on the strip groove G; when the force on the first conductive layer 12 is too large, the first conductive layer 12 will crack along the strip groove G under the action of the force, thereby releasing the stress in time, avoiding the force on the first conductive layer 12 being greater than the connection force between the insulating substrate 11 and the first conductive layer 12, reducing the probability of relative slip between the insulating substrate 11 and the first conductive layer 12, and ensuring the performance of the electrode component 1.

[0085] During the use of the secondary battery, the current generated by the active material layer 13 flows to the protrusion 122 via the main body 121, that is, on the first conductive layer 12, the current generally flows along the height direction Z, and therefore, the flow area of ​​the first conductive layer 12 depends on the area of ​​the cross section of the first conductive layer 12 perpendicular to the height direction Z. In the present application, the strip groove G generally extends along the height direction Z, and its length in the width direction X is very small, that is, the size of the strip groove G along the height direction Z is greater than the size of the strip groove G along the width direction X. Therefore, when the first conductive layer 12 is cracked along the strip groove G during the rolling process, the strip groove G has little effect on the flow area of ​​the first conductive layer 12, thereby ensuring that the flow capacity of the first conductive layer 12 meets the requirements.

[0086] In step (iii), as the rolling progresses, the force acting on the first conductive layer 12 will gradually increase; Fig.11 When the electrode component 1 is rolled along the width direction X for a certain length, the force on the first conductive layer 12 will drive the first conductive layer 12 to crack along the strip groove G, thereby releasing the stress in time. Since the first conductive layer 12 has a large length in the width direction X, preferably, there are multiple strip grooves G, and the multiple strip grooves G are arranged at intervals along the width direction X. The multiple strip grooves G can release stress in stages during the rolling process, avoid the force on the first conductive layer 12 being greater than the connection force between the insulating substrate 11 and the first conductive layer 12, reduce the probability of relative slip between the insulating substrate 11 and the first conductive layer 12, and ensure the performance of the electrode component 1.

[0087] Reference Figure 8 and Fig. 9 , the strip groove G penetrates the first conductive layer 12 along the thickness direction Y, that is, along the thickness direction Y, the depth of the strip groove G is equal to the thickness of the first conductive layer 12. At this time, the first conductive layer 12 is more likely to crack along the strip groove G during the rolling process, thereby releasing stress in time.

[0088] In step (ii), the active material layer 13 can be filled into the strip grooves G, so the current on the active material layer 13 can flow to the first conductive layer 12 through the peripheral wall of the strip grooves G, thereby improving the current collecting capacity of the first conductive layer 12. In step (iii), even if the first conductive layer 12 is cracked along the strip grooves G, the active material layer 13 will be filled into the cracked part under the action of the roller pressure.

[0089] Since the elastic modulus of the insulating matrix 11 is relatively small, in step (iii), the insulating matrix 11 corresponding to the main body 121 will extend toward the lower side of the protrusion 122, causing the insulating matrix 11 inside the protrusion 122 to bulge and deform, and the protrusion 122 is easily deformed under the force of the insulating matrix 11, thereby generating cracks. In the present application, the protective layer 15 has a relatively high strength, and can provide support for the protrusion 122 during the rolling process of the electrode component 1, limit the deformation of the protrusion 122, reduce the probability of cracks in the protrusion 122, and improve the current carrying capacity of the electrode component 1.

[0090] During the operation of the secondary battery, the protrusion 122 may fall off due to factors such as vibration; therefore, the protective layer 15 is preferably connected to the active material layer 13, so that the protective layer 15 can be fixed to the active material layer 13, increase the bonding force of the protective layer 15 on the electrode component 1, improve the anti-vibration ability, and prevent the protective layer 15 from falling off together with the protrusion 122. At the same time, the protrusion 122 is most likely to bulge near the root of the active material layer 13 (that is, the junction of the protrusion 122 and the main body 121), so when the protective layer 15 is connected to the active material layer 13, the deformation of the protrusion 122 can be reduced, and the probability of cracking can be reduced, thereby improving the current capacity of the electrode component 1.

[0091] In order to simplify the description, only the differences between the other four embodiments and the first embodiment are mainly introduced below, and the parts not described can be understood with reference to the first embodiment.

[0092] Figures 14 to 16 Schematic diagram of a second embodiment of the electrode component of the present invention. Fig.14 and Fig.16 , along the thickness direction Y, the depth of the strip groove G is less than the thickness of the first conductive layer 12. Compared with the first embodiment, the flow area of ​​the first conductive layer 12 of the second embodiment is larger. The cross section of the strip groove G can be U-shaped or V-shaped.

[0093] Fig.17 and Fig.18 FIG. 1 is a schematic diagram of a third embodiment of an electrode component of the present invention. Fig.17 and Fig.18 Compared with the first embodiment, the electrode component 1 of the third embodiment further includes a second conductive layer 14, and the second conductive layer 14 has a first portion 141 located in the strip groove G. The first portion 141 is filled into the strip groove G, and the current around the strip groove G can be transmitted through the first portion 141; in other words, the first portion 141 can repair the conductive network of the first conductive layer 12, increase the flow area, and ensure the overall flow capacity of the electrode component 1.

[0094] In the first embodiment, the active material layer 13 is filled into the strip groove G, so the distribution of the active material layer 13 is not uniform, that is, the thickness of the active material layer 13 at the strip groove G is greater than the thickness at other positions. During the operation of the secondary battery, the active material layer 13 may deposit lithium at the position corresponding to the strip groove G. In the third embodiment, the first portion 141 is filled into the strip groove G, thereby ensuring the flatness of the first conductive layer 12, improving the uniformity of the distribution of the active material layer 13, and reducing the risk of lithium deposition.

[0095] The second conductive layer 14 further includes a second portion 142 , which is disposed on a surface of the first conductive layer 12 away from the insulating substrate 11 and connected to the first portion 141 . The active material layer 13 is disposed on a surface of the second portion 142 away from the first conductive layer 12 .

[0096] The second conductive layer 14 can be a metal material or a non-metal material. In order to reduce the burrs generated when foreign matter pierces the electrode member 1, the second conductive layer 14 is preferably a non-metal material that is not easy to generate burrs. Specifically, the conductive carbon, the binder and the solvent can be made into a slurry, and then the slurry can be applied to the first conductive layer 12. After the slurry is cured, the second conductive layer 14 is formed. During the coating process, the slurry fills the strip groove G and forms the first part 141.

[0097] In step (ii), the slurry of the second conductive layer 14 may be first applied onto the first conductive layer 12 , and then the slurry of the active material layer 13 and the slurry of the protective layer 15 may be applied onto the surface of the second conductive layer 14 .

[0098] In step (three), even if the first conductive layer 12 is cracked along the strip groove G, the second part 142 will be filled into the cracked part under the action of roller pressure, thereby repairing the conductive network of the first conductive layer 12, increasing the flow area, and ensuring the overall flow capacity of the electrode component 1.

[0099] If the second conductive layer 14 is only provided on the surface of the first conductive layer 12, the current of the second conductive layer 14 can only be conducted to the first conductive layer 12 through the surface of the first conductive layer 12. In the present application, the first portion 141 of the second conductive layer 14 is embedded in the strip groove G on the first conductive layer 12, so that the current can be conducted not only to the first conductive layer 12 through the surface of the first conductive layer 12, but also through the peripheral wall of the strip groove G, thereby increasing multiple conduction paths, forming a multi-point conductive network, improving the conductive performance of the electrode component 1, reducing the polarization of the electrode component 1 and the secondary battery, and improving the high-rate charge and discharge performance of the secondary battery.

[0100] The second portion 142 is at least partially located on the surface of the protrusion 122 away from the insulating substrate 11. The protection layer 15 may be disposed on the surface of the second portion 142 away from the protrusion 122. The conductive structure 16 is welded to the area of ​​the protrusion 122 not covered by the second portion 142.

[0101] In step (three), the main body 121 extends under the influence of the insulating substrate 11, while the protrusion 122 is almost not extended. The main body 121 and the insulating substrate 11 apply a force to the protrusion 122 when extending, and because the protrusion 122 is thin, microcracks will appear in the protrusion 122 under the action of the force. In the present application, the second part 142 is arranged on the surface of the protrusion 122, so even if the protrusion 122 is cracked during the rolling process, the current at the crack can be transmitted to the outside through the second part 142, thereby realizing the repair of the conductive network and ensuring the overall current capacity of the electrode component 1.

[0102] The rigidity of the second conductive layer 14 is less than that of the first conductive layer 12. That is, when subjected to force, the second conductive layer 14 is more likely to deform. When the protrusion 122 deforms, the second portion 142 also deforms with the protrusion 122; even if the protrusion 122 cracks due to excessive deformation, the second portion 142 is unlikely to break, thereby ensuring the transmission of current.

[0103] The strip groove G penetrates the first conductive layer 12 along the thickness direction Y, and the first portion 141 of the second conductive layer 14 is connected to the insulating substrate 11. The first portion 141 is embedded in the strip groove G and adhered to the insulating substrate 11, thereby increasing the connection strength among the first conductive layer 12, the second conductive layer 14 and the insulating substrate 11.

[0104] Figures 19 to 21 FIG. 4 is a schematic diagram of a fourth embodiment of an electrode component of the present invention. Figures 19 to 21 Compared with the third embodiment, the strip-shaped groove G of the fourth embodiment includes a first groove G1 formed in the protrusion 122 .

[0105] In step (three), the portion of the insulating base 11 corresponding to the main body 121 is compressed and stretched, and the portion of the insulating base 11 corresponding to the main body 121 will apply a force to the portion of the insulating base 11 corresponding to the protrusion 122, thereby driving the portion of the insulating base 11 corresponding to the protrusion 122 to extend. The protrusion 122 is restricted by the protective layer 15 and is therefore almost inextensible; the portion of the insulating base 11 corresponding to the protrusion 122 will apply a force to the protrusion 122 when extending. If the force is greater than the connection force between the insulating base 11 and the protrusion 122, the protrusion 122 is easy to fall off from the insulating base 11. In the present application, the first groove G1 can effectively release the force on the protrusion 122, reduce stress concentration, avoid excessive force on the protrusion 122, effectively reduce the probability of the protrusion 122 falling off, and ensure the performance of the electrode component 1.

[0106] Preferably, the first groove G1 does not extend beyond the protective layer 15 in the direction away from the active material layer 13. The area of ​​the protrusion 122 covered by the protective layer 15 is subjected to the greatest stress, so the first groove G1 only needs to be provided in the area of ​​the protrusion 122 covered by the protective layer 15. The area of ​​the protrusion 122 not covered by the protective layer 15 is subjected to less force and does not have the risk of falling off. If the first groove G1 extends to the area of ​​the protrusion 122 not covered by the protective layer 15, the flow capacity of the protrusion 122 will be reduced.

[0107] The strip-shaped groove G further includes a second groove G2 formed in the main body 121 , and the first groove G1 is connected to the second groove G2 .

[0108] In step (three), the main body 121 extends under the force applied by the insulating base 11. Since the protrusion 122 is restricted by the protective layer 15, the protrusion 122 is almost inextensible. Therefore, the area of ​​the main body 121 close to the protrusion 122 will be subject to the reaction force of the protrusion 122. In other words, the area of ​​the main body 121 close to the protrusion 122 is simultaneously subjected to the forces of the insulating base 11 and the protrusion 122. Therefore, the area of ​​the main body 121 close to the protrusion 122 can easily fall off from the insulating base 11. In the present application, the second groove G2 extends to the area of ​​the main body 121 close to the protrusion 122, thereby effectively releasing the force on the main body 121, reducing stress concentration, and effectively reducing the probability of relative slip between the insulating base 11 and the main body 121, thereby ensuring the performance of the electrode component 1.

[0109] The strip groove G also includes a plurality of third grooves G3 arranged at intervals along the width direction X, and the third grooves G3 are formed in the main body 121. In the width direction X, each third groove G3 is located between two adjacent second grooves G2; in the height direction Z, the third grooves G3 and the second grooves G2 are staggered from each other.

[0110] Figure 22 to Figure 24 FIG. 5 is a schematic diagram of a fifth embodiment of an electrode component of the present invention. Figure 22 to Figure 24 The strip groove G of the fifth embodiment includes a third groove G3 and a fourth groove G4 formed in the main body 121. The third groove G3 is multiple and arranged at intervals along the width direction X, and the fourth groove G4 is multiple and arranged at intervals along the width direction X.

[0111] In the width direction X, each third groove G3 is located between two adjacent fourth grooves G4. In the height direction Z, the third grooves G3 and the fourth grooves G4 are staggered from each other. The third grooves G3 and the fourth grooves G4 are dispersedly arranged in the width direction X and the height direction Z, which can improve the stress release effect and improve uniformity.

Claims

1. An electrode component (1) of a secondary battery, comprising an insulating substrate (11), a first conductive layer (12) and an active material layer (13); The first conductive layer (12) is arranged on the surface of the insulating substrate (11), and the active material layer (13) is arranged on a side of the first conductive layer (12) away from the insulating substrate (11); The first conductive layer (12) is provided with a strip-shaped groove (G) extending along a height direction (Z); The thickness of the insulating substrate (11) is 1 μm to 20 μm, and the thickness of the first conductive layer (12) is 0.1 μm to 10 μm; The electrode member (1) further comprises a second conductive layer (14), the second conductive layer (14) having a first portion (141) located in the strip-shaped groove (G).

2. The electrode component (1) according to claim 1, characterized in that The second conductive layer (14) further comprises a second portion (142), the second portion (142) being arranged on a surface of the first conductive layer (12) away from the insulating substrate (11) and connected to the first portion (141), and the active material layer (13) being arranged on a surface of the second portion (142) away from the first conductive layer (12).

3. The electrode component (1) according to claim 2, characterized in that The first conductive layer (12) includes a main body (121) and a protrusion (122) extending from the main body (121), the main body (121) is coated with an active material layer (13), and the protrusion (122) is not coated with the active material layer (13); The strip-shaped groove (G) comprises a first groove (G1) formed on the protrusion (122), and the second portion (142) is at least partially located on a surface of the protrusion (122) away from the insulating substrate (11).

4. The electrode component (1) according to claim 3, characterized in that The strip-shaped groove (G) further includes a second groove (G2) formed in the main body (121), and the first groove (G1) is connected to the second groove (G2).

5. The electrode component (1) according to claim 3, characterized in that The electrode component (1) further comprises a protective layer (15), which is arranged on a surface of the second portion (142) away from the protrusion (122) and connected to the active material layer (13), and the first groove (G1) does not extend beyond the protective layer (15).

6. The electrode component (1) according to claim 1, characterized in that The second conductive layer (14) has a stiffness smaller than that of the first conductive layer (12).

7. The electrode component (1) according to claim 1, characterized in that The strip-shaped groove (G) penetrates the first conductive layer (12) along the thickness direction (Y), and the first portion (141) of the second conductive layer (14) is connected to the insulating base (11).

8. The electrode component (1) according to claim 1, characterized in that There are a plurality of strip-shaped grooves (G), and the plurality of strip-shaped grooves (G) are arranged at intervals along the width direction (X).

9. A secondary battery, characterized in that: The invention comprises an electrode assembly, wherein the electrode assembly comprises the electrode component (1) according to any one of claims 1 to 8.

Citation Information

Patent Citations

  • A dye-sensitized solar cell including a composite substrate

    CN106847515A

  • Electrode member, electrode assembly and rechargeable battery

    CN108428848A

  • Secondary battery and pole piece thereof

    CN108598491A

  • Secondary battery and electrode component thereof

    CN110660956A

  • Secondary batteries and their electrode components

    CN113224316B